Method for reconditioning a wear part of a mineral processing plant
The method addresses uneven wear in mineral processing parts by using a detection unit to apply hard material coatings via additive manufacturing, ensuring optimal performance and reducing downtime.
Patent Information
- Application Number
- DE102021103694
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-02-17
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2041-02-17
AI Technical Summary
Wear parts in mineral processing plants, such as blow bars and crushing cones, experience uneven wear leading to decreased crushing performance and increased energy consumption, necessitating frequent and time-consuming replacements.
A method using a detection unit to assess the wear contour of these parts and apply a controlled coating of hard material via additive manufacturing to restore them to optimal condition, even out wear, and extend maintenance intervals.
The method extends the service life of wear parts by maintaining optimal performance and reducing downtime through precise and timely application of hard material coatings, even wear distribution, and consistent energy consumption.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[0001] The invention relates to a method for preparing a wear part of a mineral processing plant, wherein the wear part has a working area which is exposed to tool wear during the operation of the mineral processing plant in such a way that a wear area with a wear contour results, wherein a coating plant is provided and wherein a repair coating, made of repair material, in particular of hard material or in particular comprising a hard material, is applied to the wear area by means of the coating plant.
[0002] The invention further relates to a wear part for a mineral processing plant.
[0003] Mineral processing plants, as defined in the invention, can be crushing plants or screening plants used to process mineral material. Crushing plants, as defined in the invention, can be, in particular, mobile or stationary. Specifically, they can be impact crushers, jaw crushers, roller crushers, or cone crushers.
[0004] Wear parts according to the invention can be components of the aforementioned mineral processing plants. In particular, these can be a striking bar of an impact crusher, a crushing jaw of a jaw crusher, a crushing cone, a cone crusher (especially an inner or outer cone), or a crushing roller of a roller crusher.
[0005] It is also conceivable that a wear part according to the invention is a component of a screening plant for screening mineral material. It is conceivable that the wear part is a feed hopper or a screen surface.
[0006] The wear parts known from the prior art wear down to a certain degree during operation. They then need to be replaced with new wear parts. A disadvantage of this is that replacing the wear parts is time-consuming and results in longer machine downtimes. With increasing wear, especially on impact bars, crushing jaws, crushing cones, or crushing rollers in crushing plants, the crushing performance and crushing quality decrease. In addition, energy consumption increases.
[0007] Furthermore, wear parts do not wear uniformly across their entire wear area. For example, the wear on impact bars of crushers is almost always uneven. Even if such an impact bar only reaches its wear limit at a specific point (for example, in the middle or at the edge), the entire impact bar must still be replaced.
[0008] EP 0 192 972 A1 discloses a mill for crushing coal. The mill has a grinding table which forms a grinding surface within its working area. A conical roller rolls on this grinding surface. Both the conical roller and the grinding table can be set in rotary motion. The contact area on which the conical roller rolls is coated with a hard material coating that can be applied by welding.
[0009] GB 2 559 422 A discloses a method for repairing the outer contour of a grinding roller used in a roller mill. Repair materials with varying wear resistance are applied to the worn outer contour. The material with the highest wear resistance is applied where the wear is greatest.
[0010] CN 1 10 449 765 A discloses a method for repairing a crusher used for shredding waste. For this purpose, the surface of a cutting tool of the crusher is first scanned to create a 3D model of the cutting tool. A repair unit is then used to apply a weld to the worn surface of the cutting tool.
[0011] US 2007 / 0 187 537 A1 discloses a roller crusher having two counter-rotating crushing rollers. A crushing gap is formed between the two crushing rollers. Each crushing roller is assigned a welding device by means of which a hardfacing can be applied to the surface of the crushing rollers.
[0012] US 2014 O 215 787 A1 describes a repair method for regenerating a cutting blade. In this process, a cutting area of the blade is measured. Then, depending on the measurement result, a weld overlay is applied to the cutting blade.
[0013] The object of the invention is to provide a method for the preparation of a wear part of a mineral processing plant, with which the wear part can be maintained in a condition that enables optimized machine operation throughout its entire service life.
[0014] The task is solved by capturing the wear contour in the wear area, at least partially, by means of a detection unit, by storing or being able to store a reference contour in a processing unit, by comparing the wear contour with the reference contour in the processing unit, and by controlling the coating system from the processing unit in such a way that it applies a refill volume of the repair order to the wear contour.
[0015] With the method according to the invention, the wear part can be easily and quickly refurbished even with minimal wear. The repair can be carried out using an additive manufacturing process in which the hard material is applied. A weld overlay process is conceivable as the additive manufacturing method. Preferably, the refurbishment of the wear part is performed at regular intervals. For example, it can be provided that the refurbishment is carried out after each work shift (e.g., after 8 to 10 operating hours) or after a specific number of work shifts.
[0016] The processing is carried out by first using the detection unit to detect the worn zone of the working area. Based on a reference contour, the processing unit can then determine the required refill volume from the measurement result. This volume is necessary to restore the worn part to its optimal operating condition. According to the invention, the detection unit can be formed by suitable sensors that enable the detection of a three-dimensional surface, namely at least a portion of the worn area. In particular, it is conceivable that an optical, non-contact detection unit is used. Such a detection unit can, in particular, be a 3D scanner, for example, a laser scanner.Within the scope of the invention, the processing unit can be a suitable computing unit that exchanges data with the acquisition unit and the coating system.
[0017] Within the scope of the invention, the reference contour can correspond, in particular, to the condition of the wear part in an unworn state, thus representing, for example, the new condition of the wear part. However, it is also conceivable that any other suitable contour, differing from the new condition, is used as the reference contour.
[0018] One conceivable embodiment of the invention is such that, taking into account the wear contour and the reference contour in the processing unit, the filling volume is determined. Based on the filling volume, the processing unit can then control the coating system in such a way that the area to be regenerated is coated with the repair material in an optimal manner.
[0019] According to a preferred embodiment of the invention, it is provided that the processing device compares the wear contour with a maximum permissible wear contour, and that, if the maximum permissible wear contour is exceeded, the processing device controls the coating system to initiate the coating process for coating the repair order.
[0020] Here, the wear contour is detected by the measuring device, and, taking into account a maximum permissible wear contour, it is determined whether the wear part is still in a condition suitable for the upcoming machining task or whether the maximum permissible wear contour has already been exceeded, at least in some areas. This inspection can be carried out manually or automatically with a suitable measuring device. In particular, it may be intended that the inspection takes place during operation of the material processing equipment or at least with the wear part installed in the machine.
[0021] Particularly preferably, the wear part in the working area may have a theoretically maximum wear contour that defines a theoretically maximum wear of 100% compared to the wear part in its new condition, and the processing equipment may initiate the coating of the repair order when wear reaches a maximum of 5%, preferably a maximum of 2.5%, and particularly preferably a maximum of 1% of the theoretically maximum wear. It has been shown that in the prior art, the maximum available wear range, for example in the case of impact bars, can only be utilized to a maximum of 30% to 40% in order to achieve sufficiently good processing results. As already mentioned above, with increasing wear, the processing result also decreases and energy consumption increases.In contrast to the usual approach known from the prior art, the invention takes a different approach by no longer allowing the theoretically maximum wear, but rather applying the repair coating after relatively minor wear. It has been shown that when the actual wear is 5% of the maximum possible wear, a relatively constant energy consumption can be achieved, particularly for the crushing plant, over the entire service life. If a value of 2.5% is chosen, a consistent performance result is also achieved for crushing tools. It is particularly advantageous if regeneration is carried out after reaching only 1% of the theoretically maximum wear.
[0022] Additionally or alternatively, particularly in the case of impact strips, it may be provided that the processing equipment initiates the coating of the repair order if the wear contour deviates from the reference contour by a maximum of 10 millimeters at at least one point, in order to achieve the effects described above.
[0023] Within the scope of the invention, it can be provided that the filling volume corresponds to the wear volume. In other words, the repair order restores the wear part to its original condition or to an almost new condition.
[0024] Alternatively, the filling volume can be designed to differ from the wear volume, and in particular, the filling volume can be designed to deviate from the wear volume by a tolerance of ±10%, at least in a partial area. It is conceivable that the repair process creates a tool contour that differs from the new condition of the wear part. For certain applications, the resulting tool contour can be set back from the new condition contour of the wear part. However, it is particularly preferred that the tool contour created by the repair process extends beyond the new condition tool contour, at least in certain areas. If the wear part experiences uneven wear, a protruding contour can be applied with the wear coating in areas of increased wear.In this way, a more uniform available wear volume can be achieved, thus extending the maintenance interval. It has been shown that, particularly with impact bars, it is advantageous if, in at least one area of increased wear, a repair contour extending beyond the original contour by a maximum of 5–10 millimeters is built up during the repair process. Especially with impact bars, it is preferable that this protrusion is built up in the tangential direction (relative to the rotational movement of the rotor).
[0025] In practical application, the method according to the invention can be carried out such that the processing device identifies at least one special wear zone in the wear contour which has an increased state of wear compared to a wear area directly or indirectly adjacent to the special wear zone, in particular with respect to the reference contour, and that a repair coating with a greater thickness is applied in the special wear zone than in the adjacent wear area.
[0026] A particularly preferred embodiment of the invention is such that the repair coating has a layered structure with several layers, preferably between 1 and 20 layers. The repair coating is applied layer by layer using the coating system. The process can be configured such that the required fill volume is first determined by the sensing unit. The processing unit then determines the number of required layers and their respective thicknesses. Subsequently, the processing unit controls the coating system so that the individual layers are produced by the coating system to generate the desired fill volume.
[0027] Any suitable additive coating process that enables the creation of a repair layer, in particular a hard coating layer, on a steel material can be used to produce the repair structure. It is particularly preferred that the repair layer be designed as a weld overlay.
[0028] According to the invention, a control device is used to shut down the mineral processing equipment, at least in the area carrying the wear part, and to coat the wear part with the repair material while it is installed in the mineral processing equipment. This allows the wear part to be repaired in situ, i.e., without removing it. This approach is particularly suitable when removing the wear part is time-consuming or not possible. In such cases, maintenance time can be minimized. Alternatively, a regeneration unit could be located outside the mineral processing equipment. The wear part could then be removed and processed centrally in this regeneration unit using the inventive method, for example, at a service center.
[0029] According to the invention, the coating system is further provided that it is connected to the mineral processing unit by means of a connecting section, and that the coating system has a kinematic mechanism in the area between the connecting section and the coating system by means of which it is held outside the working area of the wear part during the operation of the mineral processing unit and by means of which it can be moved into and within the working area of the wear part for the generation of the repair order. In this case, the coating system can be part of the mineral processing unit. The generation of the repair order can therefore be automated in the machine, particularly during downtime.
[0030] In such a system, it may be provided that the control unit of the mineral processing equipment or a separate control unit controls the movement of the kinematics. However, it is also conceivable that the kinematics are controlled by an operator.
[0031] If a cleaning device, preferably a water jet cleaning device or a mechanical cleaning device, for example with brushes, or a sandblasting device, is used to clean the working area of the wear part while installed in the mineral processing equipment, and if the wear contour is then detected by the detection unit, then the wear part can preferably be cleaned in the machine for the purpose of precise measurement using the detection unit. Preferably, the cleaning device is part of the mineral processing equipment.
[0032] The wear part for the material processing device can in particular be a crushing tool, a striking bar, a crushing bar, a crushing jaw, a crushing cone, a crushing roller or a feed hopper, with at least one working area which has a wear area which forms a wear contour, wherein a repair layer made of repair material, in particular of hard material or in particular comprising a hard material, is arranged on the wear area, and wherein the repair layer forms a filling volume which is designed as a layer structure with one or more layers.
[0033] As described above, the wear part can be designed such that the filling volume corresponds to the wear volume, or that the filling volume differs from the wear volume, in particular that the filling volume differs from the wear volume by a tolerance of ±10%.
[0034] If the wear part according to the invention is a striking bar, then the working area can have a breaking edge which is arranged in the transition between a front breaking surface and a free surface extending from the breaking edge to the rear of the wear part, and the repair order can at least partially form the breaking edge.
[0035] The invention will be explained in more detail below with reference to an embodiment illustrated in the drawings. The drawings show: Fig. 1. A crushing rotor for an impact crusher in perspective view, Fig. 2A a striking bar of the crushing rotor according to Fig. 1 in side view, Fig. 2B the impact bar according to Fig. 2A front view, Fig. 3 in combination the striking bar according to the Fig. 2A and Fig. 2B together with a coating system, Fig. 4 the striking bar according to the Fig. 2A and Fig. 2B in a regenerated state, Fig. 5 in combination a striking bar with a modified coating system, Fig. 6 a schematic representation of a striking bar according to the invention with a repair order in exploded view, Fig. 7 one of the Fig. 6. Detail taken from the image in enlarged view, Fig. 8 a schematic representation of an enlarged section of a striking bar according to Fig. 7, together with a coating system, Fig. 9 a striking bar according to the state of the art in a maximum wear condition and Fig. 10 A striking bar prepared according to the invention in two views.
[0036] Fig. Figure 1 shows a schematic representation of a crushing rotor 10, as typically used in an impact crusher. The crushing rotor 10 has several disc-shaped segments 13 connected to each other by a shaft 11. The shaft 11 can be connected to the machine frame of a mineral processing plant via bearings 12 such that the crushing rotor 10 can rotate about the longitudinal axis of the shaft 11 during operation. Several wear parts 20, which in this case form impact bars, can be interchangeably connected to the crushing rotor 10. For this purpose, abutments 14 are mounted on the crushing rotor, against which the wear parts 20 are supported from the rear. Clamping elements are provided in the area of the abutments 14, by means of which the wear parts 20 can be clamped to the crushing rotor 10.
[0037] The method of fastening the wear parts 20 is known from the prior art and does not need to be explained in more detail here.
[0038] How Fig. 2A and Fig. As shown in 2B, the wear part 20 is preferably symmetrical to its position in Fig. 2B is formed in a central transverse plane extending horizontally from left to right. However, within the scope of the invention, it is also conceivable that the wear part 20 is formed asymmetrically.
[0039] The wear part 20 has at least one working area 22. In the present embodiment, two working areas 22, 23 are provided on opposite sides of the wear part 20. The working areas 22, 23 are connected to each other in one piece via a central part 21.
[0040] The working area 22 forms a breaking edge 22.1 at the transition from a front-facing breaking surface 22.2 to a rearward-facing free surface 22.3. The breaking edge 22.1 runs in Fig. 2B in a horizontal direction from left to right.
[0041] The working area 23 forms a breaking edge 23.1 at the transition from a front-side breaking surface 23.2 to a rearward-adjoining free surface 23.3; the breaking edge 23.1 runs in Fig. 2B in a horizontal direction from left to right.
[0042] The wear part 20 has a rear support surface 24 opposite the front breaking surfaces 22.2, 23.2. A fixing projection 25 is preferably formed in the central region of the support surface 24. The wear part 20 can be supported against the abutment 14 by means of the support surface 24. The fixing projection 25 engages in a fixing receptacle of the abutment 14 to create a positive fit in the radial direction.
[0043] As mentioned above, the wear part 20 can be constructed symmetrically with respect to its central transverse plane. Accordingly, the wear part 20 can be mounted on the crushing rotor 10 in either of two mounting positions rotated 180° relative to each other. In each mounting position, either the first working area 22 or the second working area 23 can be located radially outside the crushing rotor 10.
[0044] How Fig. Figure 1 shows that, in the assembled state, the working area 22 is arranged radially outside the crushing rotor 10. During operation, the working area 22 wears in the region of the crushing edge 22.1, resulting in a wear zone V. This wear zone V is bounded by a wear contour 22.4.
[0045] Fig. Figure 5 illustrates that the wear zone V can develop unevenly in the direction of the central longitudinal axis of the wear part 20. Accordingly, distinct wear zones 27 can form in the region of the longitudinal ends of the wear part 20, which exhibit increased wear compared to an adjacent wear zone 28 in the wear zone V. This is shown in the illustration according to Figure 5. Fig. 7 clearly visible.
[0046] Fig. Figure 9 shows a wear part, namely a striking bar, which has the structure described above. This drawing illustrates how this wear part 20 is used according to the prior art. A reference contour R is shown in the working area 22 in dashed lines. This reference contour corresponds to the new condition of the wear part 20.
[0047] Due to wear, the wear contour 22.4 develops during operation. The theoretically maximum wear contour Vmaxtheor is defined by the central longitudinal plane of the wear part 20. Thus, the distance from the reference contour R to the theoretically maximum wear contour Vmaxtheor in the direction perpendicular to the central transverse plane results in a theoretically maximum wear V0 of 100%. Typically, the wear parts 20 are replaced when they exhibit wear in the range between 30% and 40% of the theoretically maximum wear V0, as the remaining area is required for mounting the impact bar. This illustrates Fig. 9. 20 is the number of wear parts shown.
[0048] As described above, the wear parts 20, in the form of impact bars, can be designed to allow for reverse mounting. Therefore, when the wear limit is reached, these impact bars can be mounted rotated by 180° so that a working area is again available in an unworn state. When the second working area is also worn, replacement of the wear parts 20 is indicated.
[0049] In Fig. Figure 10 now illustrates that the wear part 20 can again have a theoretically maximum wear volume V0 of 100%, which correlates with the distance between the central transverse plane of the wear part 20 and the reference contour R.
[0050] In Fig. Figure 10 illustrates that a wear zone V has formed in the working area 22 due to operational factors. Accordingly, a wear contour 22.4 results below the reference contour R. According to one embodiment of the invention, the wear part 20 should be operated for a maximum of until the actual wear is less than 5%, preferably less than 2.5%, particularly preferably less than 1% of the theoretically maximum wear volume V0. In other words, a maximum permissible wear contour Vmax is defined. If the actual wear contour 22.4 touches or exceeds the maximum permissible wear contour Vmax, a repair process for the wear part 20 should be initiated.
[0051] Preferably, it is provided that for this purpose the wear contour 22.4 is continuously or in intervals recorded and compared with the maximum permissible wear contour Vmax.
[0052] For example, the wear contour 22.4 can be detected contactlessly using an optical scanner. In a processing unit, the wear contour 22.4 can be compared with the maximum permissible wear contour Vmax.
[0053] Fig. Figure 5 shows an example where the wear contour 22.4 in the wear area V can be measured using a detection unit 33, which includes an optical scanner 33.1. This optical scanner 33.1 can be moved over the wear contour 22.4 by means of a handling device 30 in order to detect it.
[0054] According to one embodiment, the measurement result of the detection unit 33 can be compared with a reference contour R (for example, the reference contour is the geometric shape of the wear part 20 in its new condition). The difference between the reference contour R and the wear contour 22.4 yields a refill volume FV.
[0055] The refill volume FV can contain information about local wear along the working area 22.
[0056] In Fig. Figure 6 illustrates the refill volume FV.
[0057] After the filling volume FV has been detected by the processing device, the processing device can initiate the application of a repair layer 26 to the wear area V. According to the invention, the repair layer 26 can be applied using an additive manufacturing process, for example, a weld overlay process.
[0058] According to Fig. For this purpose, a coating system 35 may be provided, which, for example, includes a welding attachment unit. A material reservoir 34 is assigned to the coating system 35, through which a filler material 36 is supplied to the coating system 35. This filler material 36 may be a welding filler material 36.
[0059] According to the invention, both the coating system 35 and the detection unit 33 can be guided and supported by a handling device 30. The handling device 30 has a connecting section 31. The handling device 30 is rigidly connected to the material processing equipment by means of this connecting section 31. The connecting section 31 carries a kinematic mechanism 32, which supports the detection unit 33 and / or the coating system 35. According to the invention, the handling device 30 can be an industrial robot.
[0060] When the processing unit initiates the coating process, control data is transmitted from the processing unit to the handling device 30. How Fig. Figure 8 shows that the repair order 26 is then applied using the additive manufacturing process. Preferably, the repair order 26 is applied in layers 26.1 in the wear area. Preferably, the entire fill volume FV is filled with the repair order 26.
[0061] It is also conceivable that the repair coating 26 is applied beyond the determined fill volume FV. It is particularly preferred that, at least in a specific wear zone 27, a repair coating 26 is applied beyond the reference contour R and thus beyond the fill volume FV. In this way, a coating is created in the particularly wear-prone specific wear zone 27 that protrudes beyond the reference contour R. Preferably, the overall wear can be more uniform across the working area 22 in this way.
[0062] In Fig.Figure 7 illustrates the repair order 26 in exploded view with its individual layers 26.1 for better illustration.
[0063] After the repair order 26 has been applied, the handling device 30 moves away from the wear part 20 into a waiting position, in which it is located outside the working area of the rotor 10.
[0064] Preferably, the repair order 26 is applied to the wear part 20 while it is installed in the material processing unit. This way, the wear part 20 does not need to be removed and can be regenerated in situ while the crushing rotor 10 is at a standstill.
[0065] Within the scope of the invention, it is conceivable that the regeneration of the wear part 20 is carried out at predetermined intervals. For example, the regeneration of the wear part 20 can be carried out at the end of a work shift (i.e., after, for example, 8 to 10 hours of operation).
[0066] According to the invention, a method is proposed for reconditioning a wear part 20 of a mineral processing plant. The wear part 20 has at least one working area 22, 23 which, during operation of the mineral processing plant, is subject to tool wear such that a wear area V with a wear contour 22.4 results. For regenerating the wear part 20, a coating system 35 is provided by means of which a repair coating 26, consisting of repair material, in particular a hard material or, more specifically, comprising a hard material, is applied to the wear area V. The wear contour 22.4 is detected at least partially in the wear area V by means of a detection unit 33. The measurement result thus obtained is then compared in a processing unit with a reference contour R, which is stored or can be stored in the processing unit.Subsequently, the coating system 35 is controlled by the processing unit in such a way that it applies a filling volume FV of the repair order 26 to the wear contour 22.4.
[0067] If the coating is carried out in situ in the mineral processing facility with the repair order 26, the mineral processing facility may be equipped with a cleaning device, for example a water jet cleaning device, cleaning brushes, a sandblasting device or similar, with which the wear part 20 is cleaned in the wear area V before the detection unit 33 measures the wear contour 22.4 in order to obtain the most accurate measurement result possible.
[0068] While regeneration should preferably take place in the crushing chamber of the machine (i.e., without removing the wear part 20), it is also conceivable that the wear part 20 is regenerated outside the machine if it can be replaced quickly. In that case, the actual processing can be carried out in a separate processing plant, which would then include, for example, the prescribed handling device 30.
Claims
[1] Method for processing a wearing part (20) of a mineral processing plant, wherein the wearing part (20) has a working area (22, 23) which is exposed to tool wear during operation of the mineral processing device in such a way that a wear area (V) with a wear contour (22.4) is produced, wherein a coating system (35) is provided and wherein by means of the coating system (35) a repair application (26) consisting of repair material, in particular of hard material or in particular comprising a hard material, is applied to the wear area (V), wherein the wear contour (22.4) in the wear area (V) is detected at least in regions by means of a detection unit (33), wherein a reference contour (R) is stored or can be stored in a processing device, wherein the wear contour (22.4) is compared with the reference contour (R) in the processing device, wherein the coating system (35) is controlled by the processing device in such a way that it applies a filling volume (FV) of the repair order (26) to the wear contour (22.4), wherein the mineral processing device is stopped by means of a control device at least in the area which carries the wearing part (20), wherein the wearing part (20) is coated with the repair order (26) in the installed state in the mineral processing device, wherein the coating system (35) is connected to the mineral processing device by means of a connecting section (31), and wherein the coating system (35) has, in the area between the connecting section (31) and the coating system (35), a kinematics (32) by means of which it is held outside the working area of the wearing part (20) during the working operation of the mineral processing device and with which it can be adjusted into the working area of the wearing part (20) and moved within this for the generation of the repair order (26). [2] Method according to claim 1 characterized bythat the filling volume (FV) is determined taking into account the wear contour (22.4) and the reference contour (R) in the processing device. [3] Method according to claim 1 or 2, characterized by that the processing device compares the wear contour (22.4) with a maximum permissible wear contour (VMAX), and that if the maximum permissible wear contour (VMAX) is exceeded, the processing device controls the coating system (35) in order to initiate the coating process for coating the repair order (26). [4] Method according to claim 3, characterized bythat the wearing part (20) in the working area (22, 23) has a theoretically maximum wear contour which defines a theoretical maximum wear of 100% compared to the wearing part (20) in the new state, and that the processing device initiates the coating of the repair order (26) when there is wear of a maximum of 5%, preferably a maximum of 2.5%, particularly preferably a maximum of 1% of the theoretical maximum wear, and / or that the processing device initiates the coating of the repair order (26) when the wear contour deviates from the reference contour by a maximum of 10 millimeters at least at one point. [5] Method according to one of claims 1 to 4, characterized bythat the filling volume (FV) corresponds to the wear volume, or that the filling volume (FV) deviates from the wear volume, wherein in particular it is provided that the filling volume (FV) deviates from the wear volume with a tolerance of ±10%. [6] Method according to one of claims 1 to 5, characterized by that the processing device determines at least one special wear zone (27) in the wear contour (22.4), which has an increased state of wear, in particular with respect to the reference contour, compared to a wear region directly or indirectly adjoining the special wear zone (27), and that in the special wear zone (27) a repair application (26) is coated with a greater application height than in the adjoining wear region (28). [7] Method according to one of claims 1 to 6, characterized bythat the repair order (26) has a layer structure with several layers (26.1), preferably with in the range between 1 and 20 layers (26.1). [8] Method according to one of claims 1 to 7, characterized by that the repair order (26) is designed as a build-up welding. [9] Method according to one of claims 1 to 8, characterized by that a control device of the mineral processing device controls the movement of the kinematics (32). [10] Method according to one of claims 1 to 9, characterized by that a cleaning device, preferably a water jet cleaning device, is provided, by means of which the working area (22, 23) of the wearing part (20) can be cleaned in the installed state in the mineral processing device, and that the wear contour is then detected by means of the detection unit (33).
Citation Information
Patent Citations
Surfacing welding repair system and repair method for breaking machine, computer equipment and readable storage medium
CN110449765A
Highly abrasive resistant material
EP0192972A1
A method of repairing a grinding parts used in a roller mill and to grinding parts so repaired
GB2559422A
Repairing crusher rolls
US20070187537A1
Regenerating method of cutting blade, its regenerating equipment, and cutting blade for shearing type grinding machine
US20140215787A1
Cited By
A method for repairing a cutting tool component
EP4751840A1