METHOD FOR PRODUCING A NANOSTRUCTURE FIELD EFFECT TRANSISTOR DEVICE
The use of a multilayer spacer film with a two-stage annealing process addresses the challenge of parasitic capacitance and electrical shorts in miniaturized semiconductor devices by creating seamless internal spacers with balanced dielectric and etch resistance, enhancing device performance.
Patent Information
- Application Number
- DE102022103105
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-02-07
- Filing Date
- 2022-02-10
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2042-02-10
AI Technical Summary
As semiconductor devices continue to shrink in size, challenges arise in reducing parasitic capacitance and preventing electrical shorts due to the formation of seams in internal spacers, which are difficult to fill and etch-resistant materials often lack the necessary dielectric properties.
A multilayer spacer film is formed with a first dielectric layer having a higher dielectric constant and etch resistance, followed by a two-stage annealing process to remove seams, and then trimmed to create seamless internal spacers with a balanced dielectric constant and etch resistance, ensuring no electrical shorts occur.
The method achieves reduced parasitic capacitance and prevents electrical shorts by forming seamless internal spacers with a balanced dielectric constant and etch resistance, improving device performance in advanced processing nodes.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
BACKGROUND
[0001] Semiconductor devices are used in a wide variety of electronic applications, such as personal computers, mobile phones, digital cameras, and other electronic devices. Semiconductor devices are typically manufactured by depositing insulating or dielectric layers, conductive layers, and semiconductor layers of material onto a semiconductor substrate, and by lithography to structure the various material layers and create circuit components and elements.
[0002] The semiconductor industry continues to improve the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.) by continuously reducing the minimum feature size, thus enabling the integration of more components into a given area. However, as minimum feature sizes decrease, additional problems arise that need to be addressed.
[0003] US 2021 / 0 234 017 A1 describes a semiconductor structure comprising a stack of semiconductor layers arranged over a substrate, a metal gate stack with an upper section arranged over the stack of semiconductor layers and a lower section nested within the stack of semiconductor layers, an inner spacer arranged on sidewalls of the lower section of the metal gate stack, an air gap enclosed in the inner spacer, and an epitaxial source / drain (S / D) feature arranged over the inner spacer and adjacent to the metal gate stack. Further prior art is known from US 2021 / 0 126 106 A1 and US 2020 / 0 105 929 A1. The invention is specified in the claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0004] Aspects of this disclosure are best understood with reference to the detailed description below in conjunction with the accompanying drawings. It should be noted that, in accordance with common industry practice, various features are not drawn to scale. Rather, for the sake of clarity of discussion, the dimensions of the various features may be enlarged or reduced as desired. Fig. Figure 1 shows an example of a nanostructured field-effect transistor (NSFET) device in a three-dimensional view according to some embodiments. The Fig. 2, Fig. 3A, Fig. 3B, Fig. 4A, Fig. 4B, Fig. 5A, Fig. 5B, Fig. 6 to Fig. 13 and Fig. 15 to Fig. Figure 19 shows cross-sectional views of a nanostructured field-effect transistor (NSFET) device at various stages of fabrication according to one embodiment. Fig. Figure 14 shows the chemical reaction during the process in Fig. 13 Processing shown in one embodiment. Fig. Figure 20 shows a cross-sectional view of a nanostructured field-effect transistor (NSFET) device according to another embodiment. Fig. Figure 21 shows a cross-sectional view of a nanostructured field-effect transistor (NSFET) device according to yet another embodiment. Fig. Figure 22 is a flowchart of a process for manufacturing a semiconductor device in some embodiments. DETAILED DESCRIPTION
[0005] The following disclosure provides many different embodiments or examples for implementing various features of the invention. Specific examples of components and arrangements are described below to simplify the present disclosure. For example, the fabrication of a first feature over or on top of a second feature in the following description may include embodiments in which the first and second features are formed in direct contact, and it may also include embodiments in which additional features can be formed between the first and second features, so that the first and second features may not be in direct contact.
[0006] Furthermore, spatially relative terms, such as "located below," "under," "lower," "located above," "upper," and the like, can be used here to simply describe the relationship of an element or structure to one or more other elements or structures depicted in the figures. These spatially relative terms are intended to encompass various orientations of the device in use or operation, in addition to the orientation shown in the figures. The device can be oriented differently (rotated by 90 degrees or in a different orientation), and the spatially relative descriptors can be interpreted accordingly.In this entire discussion, unless otherwise stated, the same or similar reference numerals in different figures refer to the same or a similar component formed by the same or similar process using one or more of the same or similar materials.
[0007] According to some embodiments, a multilayer spacer film is formed to create the internal spacers of a nanostructured field-effect transistor (NSFET) device by filling the sidewall depressions in a first semiconductor material. The first semiconductor material is contained in a stack of layers consisting of alternating layers of the first semiconductor material and a second semiconductor material. The multilayer spacer film includes a first dielectric layer that lines the sidewall depressions and a second dielectric layer on top of the first dielectric layer. The first dielectric layer has a higher dielectric constant than the second dielectric layer. After the second dielectric layer is formed, a multi-stage annealing process is performed to remove seams (e.g., air gaps) in the multilayer spacer film.The multilayered spacer film is then trimmed to form the internal spacers of the NSFET device. The multilayered internal spacers achieve a good balance between dielectric constant and etch resistance, resulting in a lower parasitic capacitance for the NSFET device, while the internal spacers themselves exhibit high etch resistance to prevent electrical short circuits (e.g., caused by etching through the internal spacers) between the source / drain regions and the gate structure of the NSFET device.
[0008] Fig. Figure 1 shows an example of a nanostructured field-effect transistor (NSFET) device 30 in a three-dimensional view according to some embodiments. The NSFET device 30 comprises semiconductor fins 90 (also referred to as fins) projecting over a substrate 50. A gate electrode 122 (e.g., a metal gate) is arranged over the fins, and source / drain regions 112 are formed on opposite sides of the gate electrode 122. A plurality of nanostructures 54 (e.g., nanowires or nanosheets) are formed over the fins 90 and between the source / drain regions 112. Insulation regions 96 are formed on opposite sides of the fins 90. A gate dielectric layer 120 is formed around the nanostructures 54. Gate electrodes 122 are located over and around the gate dielectric layer 120.
[0009] Fig. Figure 1 further shows reference cross-sections that are used in later figures. Cross-section AA is along a longitudinal axis of a gate electrode 122 and in a direction, for example, perpendicular to the direction of current flow between the source / drain regions 112 of the NSFET device 30. Cross-section BB is perpendicular to cross-section AA and is along a longitudinal axis of a fin 90 and in a direction of, for example, current flow between the source / drain regions 112 of the NSFET device 30. For clarity, subsequent figures refer to these reference cross-sections.
[0010] The Fig. 2, Fig. 3A, Fig. 3B, Fig. 4A, Fig. 4B, Fig. 5A, Fig. 5B, Fig. 6 to Fig. 13 and Fig. 15 to Fig. Figure 19 are cross-sectional views of a nanostructured field-effect transistor (NSFET) device at various stages of fabrication according to one embodiment. In this discussion, figures with the same number but different letters (e.g., Fig. 5A and Fig. 5B) Different views of the same device at the same manufacturing stages.
[0011] In Fig. 2. A substrate 50 is provided. The substrate 50 can be a semiconductor substrate, such as a bulk semiconductor, a semiconductor-on-insulator (SOI) substrate, or the like, which may be doped (e.g., with a p- or n-type dopant) or undoped. The substrate 50 can be a wafer, such as a silicon wafer. In general, an SOI substrate is a layer of semiconductor material formed on an insulating layer. The insulating layer may be, for example, a buried oxide layer (BOX layer), a silicon oxide layer, or the like. The insulating layer is provided on a substrate, typically a silicon or glass substrate. Other substrates, such as a multilayer or gradient substrate, may also be used.In some embodiments, the semiconductor material of substrate 50 comprises silicon; germanium; a compound semiconductor comprising silicon carbide, gallium arsenic, gallium phosphide, indium phosphide, indium arsenide and / or indium antimonide; an alloy semiconductor comprising SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP and / or GaInAsP; or combinations thereof.
[0012] An epitaxial material stack 64 is formed on the substrate 50. The epitaxial material stack 64 comprises alternating layers of a first semiconductor material 52 and a second semiconductor material 54. Fig. The layers formed by the first semiconductor material 52 are designated 52A, 52B, 52C, and 52D, and the layers formed by the second semiconductor material 54 are designated 54A, 54B, 54C, and 54D. The number of layers formed by the first and second semiconductor materials is given by the number of layers formed by the first and second semiconductor materials. Fig. The figures shown in Figure 2 are merely non-limiting examples. Other numbers of layers are also possible and are intended to be fully included within the scope of protection of this disclosure.
[0013] In some embodiments, the first semiconductor material 52 is an epitaxial material suitable for forming channel regions of, for example, p-FETs, such as silicon germanium (SixGe1-x, where x is in the range of 0 to 1), and the second semiconductor material 54 is an epitaxial material suitable for forming channel regions of, for example, n-FETs, such as silicon. The epitaxial material stacks 64 are structured to form channel regions of an NSFET in a subsequent processing step. In particular, the epitaxial material stacks 64 are structured to form horizontally extending nanostructures, wherein the channel regions of the resulting NSFET comprise multiple horizontally extending nanostructures.
[0014] The epitaxial material stacks 64 can be formed by an epitaxial growth process, which can be carried out in a growth chamber. During the epitaxial growth process, the growth chamber is cyclically exposed to a first set of precursors for the selective growth of the first semiconductor material 52 and then, in some embodiments, to a second set of precursors for the selective growth of the second semiconductor material 54. The first set of precursors includes precursors for the first semiconductor material (e.g., silicon germanium), and the second set of precursors includes precursors for the second semiconductor material (e.g., silicon). In some embodiments, the first set of precursors includes a silicon precursor (e.g., silane) and a germanium precursor (e.g., germanium), and the second set of precursors includes the silicon precursor but omits the germanium precursor.The epitaxial growth process can thus involve continuously allowing a flow of the silicon precursor to the growth chamber, and then cyclically: (1) allowing a flow of the germanium precursor to the growth chamber when the first semiconductor material 52 is grown; and (2) preventing the flow of the germanium precursor to the growth chamber when the second semiconductor material 54 is grown. The cyclical suspension can be repeated until a target number of layers has been formed.
[0015] The Fig. 3A, Fig. 3B, Fig. 4A, Fig. 4B, Fig. 5A, Fig. 5B, Fig. 6 to Fig. 13 and Fig. 15 to Fig. Figure 19 shows cross-sectional views of the NSFET device 100 in subsequent manufacturing stages according to one embodiment. Fig. 3A, Fig. 4A, Fig. 5A, Fig. 6 to Fig. 10 and Fig. 15 to Fig. 19 are cross-sectional views along cross-section BB in Fig. 1. The Fig. 3B, Fig. 4B and Fig. 5B are cross-sectional views along cross-section AA in Fig. 1. The Fig. 11 to Fig. 13 are enlarged views of a section of the Fig. 10 NSFET devices shown. Although one fin and one gate structure are shown in the figures as a non-restrictive example, it should be noted that other numbers of fins and other numbers of gate structures can also be formed.
[0016] In Fig. 3A and Fig. In step 3B, a fin structure 91 is formed, projecting above the substrate 50. The fin structure 91 comprises a semiconductor fin 90 and a layer stack 92 located above the semiconductor fin 90. The layer stack 92 and the semiconductor fin 90 can be formed by etching trenches in the epitaxial material stack 64 and the substrate 50, respectively.
[0017] The fin structure 91 can be structured by any suitable method. For example, the fin structure 91 can be structured using one or more photolithography processes, including dual-structuring or multiple-structuring processes. In general, dual-structuring or multiple-structuring processes combine photolithography and self-alignment processes, thereby producing structures that, for example, have spacings smaller than those that can otherwise be obtained using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed over a substrate and structured using a photolithography process. Spacers are formed adjacent to the structured sacrificial layer using a self-alignment process.The sacrificial layer is then removed, and the remaining spacers can then be used to structure, for example, the fin structure 91.
[0018] In some embodiments, the remaining spacers are used to structure a mask 94, which is then used to structure the fin structure 91. The mask 94 can be a single-layer mask or a multi-layer mask, such as a multi-layer mask comprising a first mask layer 94A and a second mask layer 94B. The first mask layer 94A and the second mask layer 94B can each be formed from a dielectric material, such as silicon oxide, silicon nitride, a combination thereof, or the like, and can be deposited or thermally grown according to suitable techniques. The first mask layer 94A and the second mask layer 94B are different materials with high etch selectivity. For example, the first mask layer 94A can be silicon oxide, and the second mask layer 94B can be silicon nitride.The mask 94 can be formed by structuring the first mask layer 94A and the second mask layer 94B using any acceptable etching process. The mask 94 can then be used as an etching mask to etch the substrate 50 and the epitaxial material stack 64. The etching can be any acceptable etching process, such as reactive ion etching (RIE), neutral beam etching (NBE), the like, or a combination thereof. In some embodiments, the etching is an anisotropic etching process. After the etching process, the structured epitaxial material stack 64 forms the layer stack 92, and the structured substrate 50 forms the semiconductor fin 90, as shown in [Figure]. Fig. 3A and Fig. 3B is shown. Therefore, in the illustrated embodiment, the layer stack 92 also comprises alternating layers of the first semiconductor material 52 and the second semiconductor material 54, and the semiconductor fin 90 is formed from the same material (e.g. silicon) as the substrate 50.
[0019] Next, in Fig. 4A and Fig. 4B Shallow trench insulation (STI) regions 96 are formed over the substrate 50 and on opposite sides of the fin structure 91. As an example of forming the STI regions 96, an insulating material can be formed over the substrate 50. The insulating material can be an oxide, such as silicon dioxide, a nitride, the like, or a combination thereof, and can be formed by high-density plasma chemical vapor deposition (HDP-CVD), flowable chemical vapor deposition (FCVD) (e.g., CVD-based material deposition in a remote plasma system and post-curing to convert it into another material, such as an oxide), the like, or a combination thereof. Other insulating materials formed by any acceptable process can be used. In the illustrated embodiment, the insulating material is silicon dioxide formed by an FCVD process.A tempering process can be carried out after the insulation material has been formed.
[0020] In one embodiment, the insulating material is formed such that excess insulating material covers the fin structure 91. In some embodiments, a lining is first formed along the surfaces of the substrate 50 and the fin structure 91, and a filler material, such as those discussed above, is formed over the lining. In some embodiments, the lining is omitted.
[0021] Next, a removal process is applied to the insulating material to remove excess insulating material above the fin structure 91. In some embodiments, a planarization process, such as chemical-mechanical polishing (CMP), a back-etching process, combinations thereof, or the like, may be used. The planarization process exposes the layer stack 92 such that the upper surfaces of the layer stack 92 and the insulating material are flat after the planarization process is complete. Next, the insulating material is recessed to form the STI regions 96. The insulating material is recessed such that the layer stack 92 protrudes between adjacent STI regions 96. Upper portions of the semiconductor fin 90 may also protrude between adjacent STI regions 96.Furthermore, the upper surfaces of the STI regions 96 can have a flat surface, as illustrated, a convex surface, a concave surface (such as a bulge), or a combination thereof. The upper surfaces of the STI regions 96 can be formed as flat, convex, and / or concave by suitable etching. The STI regions 96 can be recessed using an acceptable etching process, such as one that is selective for the insulating material (e.g., etching the insulating material at a faster rate than the semiconductor fin material 90 and the layer stack material 92). For example, chemical oxide removal with a suitable etchant, such as dilute hydrofluoric acid (dHF acid), can be used.
[0022] Still referring to Fig. 4A and Fig. 4B A dielectric dummy layer 97 is formed over the layer stack 92 and over the STI region 96. The dielectric dummy layer 97 can be, for example, silicon oxide, silicon nitride, a combination thereof, or the like, and can be deposited or thermally grown according to acceptable techniques. In one embodiment, a conformal silicon layer is formed over the layer stack 92 and over the upper surface of the STI regions 96, and a thermal oxidation process is carried out to convert the deposited silicon layer into an oxide layer as the dielectric dummy layer 97.
[0023] Next, in Fig. 5A and Fig. 5B A dummy gate 102 is formed over the fin 90 and over the layer stack 92. To form the dummy gate 102, a dummy gate layer can be formed over the dielectric dummy layer 97 and then planarized, for example by CMP. The dummy gate layer can be a conductive material and can be selected from a group that includes amorphous silicon, polycrystalline silicon (polysilicon), polycrystalline silicon germanium (poly-SiGe), or the like. The dummy gate layer can be deposited by physical vapor deposition (PVD), CVD, sputtering, or other techniques. The dummy gate layer can be made of other materials that exhibit high etch selectivity from the insulating regions 96.
[0024] Masks 104 are then formed over the dummy gate layer. The masks 104 can be formed from silicon nitride, silicon oxynitride, combinations thereof, or the like, and can be structured using acceptable photolithography and etching techniques. In the illustrated embodiment, the mask 104 comprises a first mask layer 104A (e.g., a silicon oxide layer) and a second mask layer 104B (e.g., a silicon nitride layer). The structure of the masks 104 is then transferred to the dummy gate layer by an acceptable etching technique to form the dummy gate 102, and then transferred to the dielectric dummy layer by an acceptable etching technique to form dummy gate dielectrics 97. The dummy gate 102 covers respective channel regions of the layer stack 92. The structure of the masks 104 can be used to physically separate the dummy gate 102 from neighboring dummy gates.The dummy gate 102 can also have a longitudinal direction that is substantially perpendicular to the longitudinal direction of the fins 90. In some embodiments, the dummy gate 102 and the dummy gate dielectric 97 are collectively referred to as a dummy gate structure 106.
[0025] Next, a gate spacer layer 107 is formed by conformally depositing an insulating material over the layer stack 92, the STI regions 96, and the dummy gate 102. The insulating material can be silicon nitride, silicon oxynitride, silicon carbonitride, a combination thereof, or the like. In some embodiments, the gate spacer layer 107 comprises several sublayers. For example, a first sublayer 108 (sometimes referred to as a gate gasket spacer layer) can be formed by thermal oxidation or deposition, and a second sublayer 109 (sometimes referred to as a main gate spacer layer) can be conformally deposited on top of the first sublayer 108. Fig. Figure 5B shows cross-sectional views of the NSFET device 100 in Fig. 5A, but along cross-section AA in Fig. 1.
[0026] Next, in Fig. 6. The gate spacer layer 107 is etched by an anisotropic etching process to form gate spacers 107. The anisotropic etching process can remove horizontal sections of the gate spacer layer 107 (e.g., sections above the layer stack 92, the STI regions 96, and the dummy gate 102), with remaining vertical sections of the gate spacer layer 107 (e.g., along sidewalls of the dummy gate 102 and the dummy gate dielectric 97) forming the gate spacers 107.
[0027] After forming the gate spacers 107, implantation of lightly doped source / drain regions (LDD regions) (not shown) can be performed. Suitable type (e.g., p- or n-type) impurities can be implanted into the exposed layer stack 92 and / or the semiconductor fin 90. The n-type impurities can be any suitable n-type impurities, such as phosphorus, arsenic, antimony, or the like, and the p-type impurities can be any suitable p-type impurities, such as boron, BF₂, indium, or the like. The lightly doped source / drain regions can have an impurity concentration of about 10 15 cm -3 up to about 10 16 cm -3 have. A tempering process can be used to activate the implanted impurities.
[0028] Next, in Fig. Seven openings 110 (which can also be referred to as depressions or source / drain openings) are formed in the layer stack 92. The openings 110 can extend through the layer stack 92 and into the semiconductor fin 90. The openings 110 can be formed by any acceptable etching technique using, for example, the dummy gate 102 and the gate spacers 107 as an etching mask. The openings 110 expose end sections of the first semiconductor material 52 below the dummy gate 102 and expose end sections of the second semiconductor material 54 below the dummy gate 102.
[0029] Next, in Fig. 8. After the openings 110 were formed, a selective etching process (e.g., a wet etching process using an etching chemical) was performed to deepen end sections of the first semiconductor material 52 exposed by the openings 110, without substantially attacking the second semiconductor material 54. Following the selective etching process, depressions 52R were formed in the first semiconductor material 52 at the locations where the removed end sections had been. It should be noted that, due to the depressions 52R, sidewalls of the first semiconductor material 52 are deepened by respective sidewalls 54S of the second semiconductor material 54, and therefore the depressions 52R can also be referred to as sidewall depressions 52R.
[0030] The Fig. 9 to Fig. Figure 15 shows the formation of a multilayer spacer film 59 that fills the sidewall recesses 52R. The multilayer spacer film 59 contains a first dielectric layer 55 and a second dielectric layer 57, which differs from the first dielectric layer 55. Details are discussed below.
[0031] Next, with reference to Fig. 9 The first dielectric layer 55 is conformally formed over the dummy gate structure 106, along the sidewalls of the gate spacers 107, in the openings 110, and in the sidewall recesses 52R. In the illustrated embodiment, the first dielectric layer 55 is formed from a dielectric material such as silicon oxycarbide (SiOC), silicon oxycarbonitride (SiOCN), or the like. The first dielectric layer 55 (also referred to as a first spacer layer) can be formed by a highly conformal deposition process, such as atomic layer deposition (ALD). For example, a thermal ALD process can be carried out at a temperature between about 500°C and about 700°C to form the first dielectric layer 55. As another example, a plasma-assisted ALD process (PEALD process) can be carried out at a temperature between about 200 °C and about 300 °C to form the first dielectric layer 55.The thermal ALD or PEALD deposition process can achieve a conformity of more than approximately 95% in the formation of the first dielectric layer 55. As in . Fig. As shown in Figure 9, the first dielectric layer 55 lines the side wall recess 52R and lines the side walls and bottoms of the openings 110.
[0032] In some embodiments, the first dielectric layer 55 has a dielectric constant between approximately 3.7 and approximately 4.5. The density of the first dielectric layer 55 can be between approximately 2.0 g / cm³. 3 and about 6 g / cm² 3In some embodiments, the first dielectric layer 55 is a carbon-rich layer to provide good etch resistance in subsequent processing. For example, the atomic percentage of carbon in the first dielectric layer 55 is greater than about 5 atomic percent (at%), such as between about 5 at% and about 20 at%. The disclosed range of atomic percentage of carbon (e.g., between about 5 at% and about 20%) provides good etch resistance against a wide variety of etchants (e.g., dilute HF (dHF), H3PO4, a mixture of H2O2 and SC2, or a mixture of NF3 and F2) while keeping the dielectric constant low. If the atomic percentage of carbon is less than about 5 at%, then the etch resistance property of the first dielectric layer 55 may deteriorate below a target resistance level.On the other hand, if the atomic percentage of carbon is greater than about 20 at%, the dielectric constant of the first dielectric layer 55 may be too high (e.g. greater than about 4.5), which can increase the parasitic capacitance.
[0033] Next, in Fig. 10. A second dielectric layer 57 is formed conformally over the first dielectric layer 55. The second dielectric layer 57 is formed from a dielectric material such as silicon nitride (SiN), silicon carbonitride (SiCN), silicon oxynitride (SiON), silicon oxycarbonitride (SiOCN), or the like. The second dielectric layer 57 (also referred to as a second spacer layer) can be formed by a highly conformal deposition process, such as ALD. For example, a thermal ALD process with a conformance greater than 99% can be performed to form the second dielectric layer 57. As shown in Fig. As shown in Figure 10, the second dielectric layer 57 extends along the first dielectric layer 55, lines the sidewall recesses 52R, and lines the sidewalls and bottoms of the openings 110. The first dielectric layer 55 and the second dielectric layer 57 are collectively referred to in this discussion as a multilayer spacer film 59. In particular, the multilayer spacer film 59 fills in Fig. 10 the side wall recesses 52R not completely (see Fig. 9) Instead, a seam 56 (e.g., an air gap) may exist in each sidewall recess 52R due to, for example, the high aspect ratio of the sidewall recess 52R in advanced processing nodes and the difficulty of filling high aspect ratio openings. The sizes of the seams 56 in Fig. 10 may be an exaggeration to clearly show the seams 56.
[0034] In some embodiments, the second dielectric layer 57 has a dielectric constant between approximately 3.0 and approximately 4.2. The density of the second dielectric layer 57 can be between approximately 1.0 g / cm³. 3 and about 2.5 g / cm² 3 In the illustrated embodiment, the dielectric constant of the first dielectric layer 55 is higher than or equal to the dielectric constant of the second dielectric layer 57. Furthermore, in some embodiments, the density of the first dielectric layer 55 is higher than the density of the second dielectric layer 57. The higher dielectric constant and / or the higher density of the first dielectric layer 55 is chosen to achieve a higher etch resistance, so that in a subsequent etching process to remove the first semiconductor material 52 (see Fig. 18), the first dielectric layer 55 and the second dielectric layer 57 would not be etched through to expose the source / drain regions 112, thereby creating an electrical short circuit between the subsequently produced replacement gate structure 123 (see Fig. 19) and the Source / Drain Regions 112 are avoided. Further details are discussed below.
[0035] The Fig. 11 to Fig. Figure 13 shows a multi-stage tempering process for removing the seams 56 in one embodiment. For the sake of simplicity, the Fig. 11 to Fig. 13 only a section of the second dielectric layer 57 in a sidewall recess 52R. A two-stage tempering process is described below with reference to the Fig. 11 to Fig. 14 described.
[0036] It will now be on Fig. 11 Reference is made to an enlarged view of a section of the second dielectric layer 57 in a sidewall recess and a corresponding seam 56 in Fig. 10 shows. Fig. Figure 11 further shows the different bonds between silicon atoms and different functional groups in the material of the second dielectric layer 57. For example, it shows Fig. 11 bonds between silicon atoms and the hydroxyl group (e.g. -OH group), the amine group (e.g. -NH2 group) and the methyl group (e.g. -CH3 group).
[0037] Next, in Fig. 12 The first step of the two-stage tempering process, referred to as the first tempering process 62, is carried out. In some embodiments, the first tempering process 62 is carried out using a gas source comprising water vapor (e.g., H₂O vapor), and therefore it can also be referred to as the H₂O tempering process. The water vapor is supplied to come into contact with the second dielectric layer 57. The temperature of the first tempering process 62 can range from about 300 °C to about 550 °C. The chemical reactions in the first tempering process can be described by the following chemical equations: Si-NH2+H2O→NH3+Si-OH (1) Si-CH3+H2O→CH4+Si-OH (2)
[0038] From chemical equations (1) and (2) it can be seen that during the first annealing process 62, some of the -NH2 and -CH3 functional groups in the second dielectric layer 57 are replaced by the -OH functional groups to form Si-OH bonds. Volatile products, such as ammonia (NH3) and methane (CH4), are formed and released from the second dielectric layer 57 (e.g., as gases). The release of NH3 and CH4 from the second dielectric layer 57 is also referred to as the degassing process. Since oxygen atoms are larger than nitrogen and carbon atoms, the replacement of the -NH2 and -CH3 functional groups by the -OH functional groups causes the volume of the second dielectric layer 57 (e.g., the amount of space it occupies) to increase in some embodiments.In other words, the volume of the second dielectric layer 57 is increased after the first annealing process 62, which reduces the size of the seam 56. In the example of . Fig. 12. The seam 56, although reduced in size, is not removed (e.g. closed) after the first tempering process 62.
[0039] Next, in Fig. 13 The second step of the two-stage tempering process, referred to as the second tempering process 66, is carried out. In some embodiments, the second tempering process 66 is carried out using a gas source comprising nitrogen gas (e.g., N2), and therefore it can also be referred to as the N2 tempering process. The nitrogen gas is supplied to come into contact with the second dielectric layer 57. The temperature of the second tempering process 66 can be between approximately 400 °C and approximately 600 °C. In some embodiments, the second dielectric layer 57 has hydrophobic surfaces after the second tempering process 66, e.g., due to the chemical reactions induced by the tempering processes, which improves the etch resistance of the second dielectric layer 57.
[0040] Fig. Figure 14 shows the chemical reactions in the second annealing process 66. The high temperature of the second annealing process 66 breaks some of the bonds between the -OH functional groups and the HOH functional groups, and the HOH functional groups release water vapor from the second dielectric layer 57 (e.g., from it). Furthermore, two adjacent Si-OH bonds can form a cross-link (e.g., Si-O-Si) and release an HOH functional group as water vapor due to the cross-link. Therefore, the second annealing process 66 serves to dehumidify the second dielectric layer 57 and to form cross-links (e.g., Si-O-Si) in the second dielectric layer 57. As shown in Figure 14, the second annealing process 66 is characterized by the formation of cross-links (e.g., Si-O-Si) within the second dielectric layer 57. Fig. As shown in Figure 13, after the second tempering process 66 the seam 56 is closed (also referred to as being removed from the second dielectric layer 57). Fig. Figure 13 shows details of the molecular structure of the second dielectric layer 57 in areas previously covered by the seam 56, at the upper right corner and in Fig. 13 shown by the arrow. It is evident that some -NH2 functional groups may still remain in the second dielectric layer 57 after the second annealing process 66.
[0041] Fig. Figure 15 shows the NSFET device 100 after the multi-stage annealing process described above. As in Fig. As shown in Figure 15, the multilayer spacer film 59, comprising the first dielectric layer 55 and the second dielectric layer 57, completely fills the sidewall recesses 52R (see Figure 15). Fig. 8).
[0042] Next, in Fig. 16 A trimming process (also referred to as an internal spacer trimming process) is carried out to remove (e.g., completely remove) sections of the multilayer spacer film 59 that are located outside the sidewall recesses 52R, such as sections along the sidewalls and bottoms of the openings 110 and sections along the upper surface of the dummy gate 102. After the trimming process, the remaining sections of the multilayer spacer film 59 within the sidewall recesses 52R form internal spacers 58.
[0043] In some embodiments, the trimming process is a suitable etching process, such as a dry or wet etching process. In one exemplary embodiment, a dry etching process is performed using a gas source comprising a mixture of CHF3 and O2, a mixture of CF4 and O2, a mixture of NF3, CH3F, and CHF3, or the like, to remove sections of the multilayer spacer film 59 located outside the sidewall recesses 52R. Parameters of the dry etching process, such as the mixing ratio of the gases in the gas source, the pressure, and / or the flow rates of the gases, are adjusted to achieve a lateral etch rate. In the example of Fig. 16. After the trimming process, the sidewalls of the remaining sections of the multilayer spacer film 59 are aligned with the sidewalls 54S of the second semiconductor material 54. In some embodiments, the sidewalls of the remaining sections of the multilayer spacer film 59 are recessed from the sidewalls 54S of the second semiconductor material 54 or extend beyond the sidewalls 54S of the second semiconductor material 54 in the direction of the openings 110. These and other variations are said to be fully included within the scope of protection of the present disclosure. After the trimming process, the remaining sections of the first dielectric layer 55 and the remaining sections of the second dielectric layer 57 form inner spacers 58 in the sidewall recesses 52R. In some embodiments, the average dielectric constant of the inner spacers 58 is between about 3.7 and about 4.5.
[0044] Next, in Fig. 17. An etching process, which can be a pre-cleaning process for the subsequent epitaxial process to form the source / drain regions 112, is carried out. Next, source / drain regions 112 are formed in the openings 110. As in Fig. As shown in Figure 17, the Source / Drain regions 112 fill the openings 110.
[0045] In some embodiments, the source / drain regions 112 are formed from one or more epitaxial materials, and therefore they can also be referred to as epitaxial source / drain regions 112. In some embodiments, the epitaxial source / drain regions 112 are formed in the openings 110 to exert voltage in the respective channel regions of the formed NSFET device 100, thereby improving performance. The epitaxial source / drain regions 112 are formed such that the dummy gate 102 is arranged between adjacent pairs of the epitaxial source / drain regions 112. In some embodiments, the gate spacers 107 are used to separate the epitaxial source / drain regions 112 from the dummy gate 102 by a suitable lateral distance, so that the epitaxial source / drain regions 112 do not short-circuit the subsequently formed gate of the resulting NSFET device.
[0046] In some embodiments, the epitaxial source / drain regions 112 are grown epitaxially within the openings 110. The epitaxial source / drain regions 112 can comprise any acceptable material, such as one suitable for an n-type or p-type device. For example, when forming n-type devices, the epitaxial source / drain regions 112 can comprise materials that exert tensile stress in the channel regions, such as silicon, SiC, SiCP, SiP, or the like. Similarly, when forming p-type devices, the epitaxial source / drain regions 112 can comprise materials that exert compressive stress in the channel regions, such as SiGe, SiGeB, Ge, GeSn, or the like. The epitaxial source / drain regions 112 can have surfaces that are raised above the respective surfaces of the fins and can have facets.
[0047] The epitaxial source / drain regions 112 and / or the fins can be implanted with dopants to form source / drain regions, similar to the process previously discussed for forming lightly doped source / drain regions, followed by annealing. The source / drain regions can accommodate an impurity concentration of between approximately 10 19 cm -3 and about 10 21 cm -3 The n-type and / or p-type impurities for source / drain regions can be any of the impurities discussed previously. In some embodiments, the epitaxial source / drain regions 112 can be doped in situ during growth.
[0048] As a result of the epitaxial processes used to form the epitaxial source / drain regions 112, the upper surfaces of the epitaxial source / drain regions 112 have facets that extend laterally outward beyond the side walls of the fin 90. In some embodiments, adjacent epitaxial source / drain regions 112 arranged over adjacent fins remain separate after the epitaxial process is complete. In other embodiments, these facets cause adjacent epitaxial source / drain regions 112 arranged over adjacent fins of the same NSFET to merge.
[0049] Next, in Fig. 18 A contact etch stop layer (CESL) 116 (e.g., conformal) is formed over the source / drain regions 112 and over the dummy gate 102, and a first interlayer dielectric (ILD) 114 is then deposited over the CESL 116. The CESL 116 is formed from a material having a different etch rate than the first ILD 114 and can be formed from silicon nitride using PECVD, although other dielectric materials, such as silicon oxide, silicon oxynitride, combinations thereof, or the like, and alternative techniques for forming the CESL 116, such as low-pressure CVD (LPCVD), PVD, or the like, could be used.
[0050] The first ILD 114 can be formed from a dielectric material and can be deposited by any suitable process, such as CVD, plasma-enhanced CVD (PECVD), or FCVD. Dielectric materials for the first ILD 114 can include silicon dioxide, phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), or the like. Other insulating materials formed by any acceptable process can be used.
[0051] Next, the dummy gate 102 is removed. To remove the dummy gate 102, a planarization process, such as a CMP, can be performed to flatten the top surfaces of the first ILD 114 and the CESL 116 with the top surfaces of the dummy gate 102 and gate spacers 107. The planarization process can also flatten the masks 104 (see Fig. 5A) on the dummy gates 102 (if the mask 104 was not removed by the anisotropic etching process to form the gate spacers 107) and remove sections of the gate spacers 107 along the sidewalls of the masks 104. After the planarization process, the upper surfaces of the dummy gate 102, gate spacers 107, and the first ILD 114 are flat. Accordingly, the upper surface of the dummy gate 102 is exposed at the upper surface of the first ILD 114.
[0052] Following the planarization process, the dummy gate 102 and the dummy gate dielectric 97 are removed in one or more etching steps, leaving a depression 103 (which may also be referred to as an opening 103) between the gate spacers 107. In some embodiments, the dummy gate 102 is removed by an anisotropic dry etching process. For example, the etching process may involve a dry etching process using reactive gas(es) that selectively etch the dummy gate 102 without etching the first ILD 114 or the gate spacers 107. During the removal of the dummy gate 102, the dummy gate dielectric 97 may be used as an etch stop layer when the dummy gate 102 is etched. The dummy gate dielectric 97 can then be removed after the dummy gate 102 has been removed. The recess 103 exposes the channel regions of the NSFET.The channel regions are arranged between adjacent pairs of the epitaxial source / drain regions 112. After removal of the dummy gate 102 and the dummy gate dielectric 97, the first semiconductor material 52 and the second semiconductor material 54, which were arranged under the dummy gate 102, are exposed through the recess 103.
[0053] Next, the first semiconductor material 52 is removed to expose the second semiconductor material 54. After the first semiconductor material 52 is removed, the second semiconductor material 54 forms a plurality of nanostructures 54 that extend horizontally (e.g., parallel to a top main surface of the substrate 50). The nanostructures 54 can be collectively referred to as the channel regions or channel layers of the formed NSFET device 100. As shown in Fig. As shown in Figure 18, removing the first semiconductor material 52 creates columns 53 (e.g., empty spaces) between the nanostructures 54. Depending on the shape and / or dimensions of the nanostructures 54, the nanostructures 54 can also be referred to as nanowires or nanosheets, and the NSFET device 100 can also be referred to as a gate-all-around device (GAA device) in some embodiments.
[0054] In some embodiments, the first semiconductor material 52 is removed by a selective etching process using an etchant that is selective for the first semiconductor material 52 (e.g., has a higher etch rate for it), such that the first semiconductor material 52 is removed without attacking the second semiconductor material 54. In one embodiment, an isotropic etching process is performed to remove the first semiconductor material 52. The isotropic etching process can be performed using an etching gas and optionally a carrier gas. In some embodiments, the etching gas comprises HF, a mixture of F₂ and HF, or the like, and the carrier gas can be an inert gas such as Ar, He, N₂, combinations thereof, or the like. In some embodiments, an etchant such as dissolved ozone in deionized water (DIO₄) is used to selectively remove the first semiconductor material 52.
[0055] Advantages of the present disclosure will now be discussed. As feature sizes continue to shrink in advanced processing nodes, reducing the parasitic capacitance of the device plays an important role in improving device performance. While low-k materials (e.g., material with a low dielectric constant value, such as less than about 3.0) can be used to reduce parasitic capacitance, low-k materials generally exhibit low etch resistance. For the NSFET device 100, it is advantageous to form the inner spacers 58 with a low dielectric constant to reduce parasitic capacitance. At the same time, the inner spacer 58 should have a high etch resistance so that, during the etching process to form the well 103, the inner spacers 58 would not be etched through to expose the source / drain regions 112.Otherwise, an electrical short circuit can occur between the source / drain regions 112 and the subsequently formed replacement gate structure 123 (see . Fig. 19).
[0056] By filling the sidewall recesses 52R with the multilayer spacer film 59, the disclosed embodiments achieve a balance between dielectric constant and etch resistance. For example, the first dielectric layer 55, which is exposed to the etching chemicals used in the etching process to form the recess 103, is formed from a dielectric material with a relatively high dielectric constant and a relatively high density, thus providing good etch resistance to prevent or reduce the possibility of being etched through. At the same time, the second dielectric layer 57 is formed from a dielectric material with a lower dielectric constant, so that the overall (e.g., average) dielectric constant of the inner spacer 58 is still low (e.g., between about 3.7 and about 4.5).
[0057] A further advantage of using the multilayer spacer film 59 to fill the sidewall recesses 52R, compared to a reference design using a single-layer dielectric material, is that the resulting internal spacers 58 are seamless (e.g., they have no seams 56). In advanced processing nodes, it is becoming increasingly difficult to completely fill openings (e.g., sidewall recesses 52R), especially those with high aspect ratios. Without the methods disclosed so far, the internal spacers formed by a single-layer dielectric material may exhibit seams (e.g., 56).The seams significantly increase the possibility of an electrical short circuit between the source / drain regions 112 and the subsequently formed gate stack 123. This is because, once the etching process for forming the cavity 103 exposes the seams in the inner spacers, the electrically conductive material of the gate stack 123 can fill the seams and form conductive channels connecting the gate stack 123 to the source / drain regions 112. In other words, without the seams, the etching process would have to etch through a larger lateral gap in the inner spacers 58 to expose the source / drain regions 112; however, with the seams, the etching process only needs to expose the seams to cause an electrical short circuit. The disclosed methods achieve improved gap filling capability by forming the second dielectric layer 57 with a deposition process with high conformity (e.g. > 99.99%) in order to better fill the sidewall recess 52R.Furthermore, the multi-stage annealing process, through expansion of the second dielectric layer 57 and cross-linking, among other features, eliminates the seams 56 and achieves seamless internal spacers 58, which significantly reduces the possibility of an electrical short circuit between the source / drain regions 112 and the gate stack 123. Additionally, the surfaces of the second dielectric layer 57 are hydrophobic after the annealing processes, which further increases the etch resistance of the internal spacer 58.
[0058] Next, in Fig. 19 A gate dielectric layer 120 (e.g., conformal) is formed in the recess 103 and in the columns 53. The gate dielectric layer 120 wraps around the nanostructures 54, lines the sidewalls of the inner spacers 58 and the sidewalls of the gate spacers 107, and extends along the upper surface and sidewalls of the fin 90. According to some embodiments, the gate dielectric layer 120 comprises silicon oxide, silicon nitride, or multiple layers thereof. In some embodiments, the gate dielectric layer 120 comprises a high-k dielectric material, and in these embodiments, the gate dielectric layer 120 may have a dielectric constant greater than about 7.0 and may comprise a metal oxide or silicate of Hf, Al, Zr, La, Mg, Ba, Ti, or Pb, or combinations thereof. The formation processes of the gate dielectric layer 120 can include molecular beam deposition (MBD), ALD, PECVD and the like.
[0059] Next, a gate electrode material (e.g., an electrically conductive material) is formed in the well 103 and the columns 53 to form the gate electrode 122. The gate electrode 122 fills the remaining sections of the well 103 and the column 53. The gate electrode 122 can be made of a metal-containing material such as Cu, Al, W, the like, combinations thereof, or multiple layers thereof, and can be formed, for example, by electroplating, electroless plating, or another suitable method. After the gate electrode 122 is filled, a planarization process, such as CMP, can be performed to remove excess sections of the gate dielectric layer 120 and the gate electrode material, with the excess sections located above the top surface of the first ILD 114.The remaining sections of gate electrode material and the gate dielectric layer 120 thus form the substitute gate structure of the resulting NSFET device 100. The gate electrode 122 and the gate dielectric layer 120 can be collectively referred to as a gate stack 123, a substitute gate structure 123, or a metal gate structure 123. Each gate stack 123 extends over and around the respective nanostructures 54.
[0060] Although the gate electrode 122 in Fig. 19 For the sake of simplicity, it is shown as a single layer, but a person skilled in the art will easily recognize that the gate electrode 122 may have a multilayer structure and may comprise a plurality of layers, such as a barrier layer, a work function layer, a seed layer and a filler metal.
[0061] For example, a barrier layer can be conformally formed over the gate dielectric layer 120. The barrier layer can comprise an electrically conductive material, such as titanium nitride, although other materials, such as tantalum nitride, titanium, tantalum, or the like, can be used alternatively. A work function layer can be formed over the barrier layer. Exemplary p-type work function materials (may also be referred to as p-type work function metals) include TiN, TaN, Ru, Mo, Al, WN, ZrSi2, MoSi2, TaSi2, NiSi2, other suitable p-type work function materials, or combinations thereof. Exemplary n-type work-of-flow materials (which may also be referred to as n-type work-of-flow metals) include Ti, Ag, TaAl, TaAlC, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, other suitable n-type work-of-flow materials or combinations thereof.A work function value is associated with the material composition of the work function layer, and thus the work function layer is selected to match its work function value so that a target threshold voltage VTH is achieved in the device to be formed. Next, a nucleation layer can be formed over the work function layer. The nucleation layer can be formed from tungsten, copper, or copper alloys, although other suitable materials may be used alternatively. Once the nucleation layer has been formed, the filler metal can be formed on top of the nucleation layer, filling openings 103 and column 53. The filler metal may include tungsten, although other suitable materials, such as aluminum, copper, tungsten nitride, ruthenium, silver, gold, rhodium, molybdenum, nickel, cobalt, cadmium, zinc, alloys of these, combinations thereof, or the like, may be used alternatively.
[0062] Additional processing can be performed to complete the fabrication of the NSFET device 100, as any person skilled in the art would readily recognize, so details need not be repeated here. For example, a second ILD can be deposited over the first ILD 114. Furthermore, gate contacts and source / drain contacts can be formed extending through the second ILD and / or the first ILD 114 to couple electrically with the gate stack 123 and the source / drain regions 112, respectively.
[0063] Fig. Figure 20 shows a cross-sectional view of a nanostructured field-effect transistor (NSFET) device 100A according to another embodiment. The NSFET device 100A is the NSFET device 100 of Fig. 19 similarly, but during the etching process to form the depression 103, sections of the exposed first dielectric layer 55 are removed by the etching process. As a result, the inner surface of the first dielectric layer 55 of each inner spacer 58, which faces the gate electrode 122, has a different shape than that in Fig. 19. For example, the inner surface of the first dielectric layer 55 of each inner spacer 58 is in Fig. 19 has a curved surface and protrudes towards the gate electrode 122. In the example of Fig. 20 the inner surface of the first dielectric layer 55 of each inner spacer 58 has a straight side wall extending parallel to the gate electrode 122.
[0064] Fig. Figure 21 shows a cross-sectional view of a nanostructured field-effect transistor (NSFET) device 100B according to yet another embodiment. The NSFET device 100B is the NSFET device 100A of Fig. 20 is similar, but during the etching process to form the well 103, the first dielectric layer 55 is etched through and exposed by the second dielectric layer 57. As a result, the gate dielectric layer 120 of the gate stack 123 physically contacts the first dielectric layer 55 and the second dielectric layer 57. It should be noted that due to the seamless structure of the internal spacers 58 and the increased etch resistance of the second dielectric layer 57 (e.g., due to hydrophobic surfaces), no electrical short circuit occurs, and the NSFET device 100B still functions correctly.
[0065] Variations of the disclosed embodiments are possible and are intended to be fully included within the scope of protection of this disclosure. For example, depending on the type of device (e.g., n- or p-type) being formed, the second semiconductor material 54 can be removed, and the first semiconductor material 52 can remain to form the nanostructures that function as the channel regions of the formed NSFET device. In embodiments where the first semiconductor material 52 remains to form the nanostructures, internal spacers 58 are formed along the end sections of the second semiconductor material 54 before the second semiconductor material 54 is removed, as a person skilled in the art would readily recognize.
[0066] Embodiments can achieve advantages. For example, the disclosed methods or structures achieve a good balance between dielectric constant and etch resistance. The internal spacers 58, which comprise the first dielectric layer 55 and the second dielectric layer 57, are seamless, exhibit high etch resistance, and a relatively low overall dielectric constant. As a result, the parasitic capacitance of the formed NSFET device is reduced, while still achieving a high level of etch resistance to prevent an electrical short circuit between source / drain regions 112 and the gate stack 123.
[0067] Fig. Figure 22 shows a flowchart of a method 1000 for manufacturing a semiconductor device according to some embodiments. It is understood that the in Fig. The embodiment shown in Figure 22 is merely one example of many possible embodiments. A person skilled in the art would recognize many variations, alternatives, and modifications. For example, different steps, as shown in Figure 22, can be used. Fig. 22 can be displayed, added, removed, replaced, rearranged or repeated.
[0068] With reference to Fig.In Block 1010, a dummy gate structure is formed over a fin structure projecting from a substrate. The fin structure comprises a fin and a stack of layers above the fin, the stack of layers consisting of alternating layers of a first semiconductor material and a second semiconductor material. In Block 1020, openings are formed in the fin structure on opposite sides of the dummy gate structure, the openings exposing first sections of the first semiconductor material and second sections of the second semiconductor material. In Block 1030, the exposed first sections of the first semiconductor material are recessed to form sidewall depressions in the first semiconductor material. In Block 1040, the sidewall depressions are lined with a first dielectric material. In Block 1050, a second dielectric material is deposited in the sidewall depressions on top of the first dielectric material.In block 1060, the second dielectric material is annealed after its deposition. In block 1070, source / drain regions are formed in the openings after annealing.
[0069] In one embodiment, a method for forming a semiconductor device comprises: forming a dummy gate structure over a fin structure projecting above a substrate, wherein the fin structure comprises a fin and a stack of layers above the fin, the stack of layers comprising alternating layers of a first semiconductor material and a second semiconductor material; forming openings in the fin structure on opposite sides of the dummy gate structure, wherein the openings expose first sections of the first semiconductor material and second sections of the second semiconductor material; deepening the exposed first sections of the first semiconductor material,to form sidewall recesses in the first semiconductor material; lining the sidewall recesses with a first dielectric material; depositing a second dielectric material in the sidewall recesses on top of the first dielectric material; after deposition of the second dielectric material, annealing the second dielectric material; and after annealing, forming source / drain regions in the openings. In one embodiment, the first dielectric material has a first dielectric constant, and the second dielectric material has a second dielectric constant that is smaller than the first dielectric constant. In one embodiment, after deposition of the second dielectric material and before annealing, there are air gaps in the sidewall recesses.wherein the annealing of the second dielectric material removes the air gaps. In one embodiment, after annealing, the volume of the second dielectric material is increased to fill the air gaps. In one embodiment, the annealing of the second dielectric material comprises: performing a first annealing process using a first gas source; and after the first annealing process, performing a second annealing process using a second gas source.which differs from the first gas source. In one embodiment, the first gas source comprises water vapor and the second gas source comprises nitrogen gas. In one embodiment, the first tempering process and the second tempering process are carried out at different temperatures. In one embodiment, the first tempering process replaces -NH2 functional groups and -CH3 functional groups in the second dielectric material with -OH functional groups. In one embodiment, the second tempering process forms Si-O-Si cross-links in the second dielectric material. In one embodiment, deepening the exposed first sections of the first semiconductor material comprises performing an etching process using an etchant that is selective for the first semiconductor material. In one embodiment, the method further comprises: after creating the source / drain regions, removing the dummy gate structure,to expose the first semiconductor material and the second semiconductor material located beneath the dummy gate structure; selectively removing the exposed first semiconductor material, wherein, after the selective removal of the exposed first semiconductor material, the second semiconductor material remains and forms a plurality of nanostructures; and fabricating a replacement gate structure around the plurality of nanostructures. In one embodiment, the removal of the exposed first semiconductor material comprises performing an etching process, wherein the etching process etches through the first dielectric material and exposes the second dielectric material.
[0070] In one embodiment, a method for forming a semiconductor device comprises: forming a first gate structure over a fin structure, wherein the fin structure comprises a fin and a layer stack over the fin, the layer stack comprising layers of a first semiconductor material interleaved with layers of a second semiconductor material; forming source / drain openings in the fin structure on opposite sides of the first gate structure; selectively removing first sections of the first semiconductor material exposed by the source / drain openings to form sidewall depressions in the first semiconductor material;Lining the sidewall recesses with a multilayer spacer film, wherein the multilayer spacer film comprises a first spacer layer and a second spacer layer formed from different materials, wherein air gaps remain in the sidewall recesses after lining; performing a tempering process after lining, wherein the tempering process removes the air gaps in the sidewall recesses;and after the tempering process, formation of source / drain regions in the source / drain openings. In one embodiment, the first spacer layer is formed from a first dielectric material and the second spacer layer is formed from a second dielectric material, wherein the first dielectric constant of the first dielectric material is higher than the second dielectric constant of the second dielectric material. In one embodiment, carrying out the tempering process comprises: carrying out a first tempering process using a first gas source;and after the first annealing process, performing a second annealing process using a second gas source that differs from the first gas source. In one embodiment, a second volume of the second spacer layer after the annealing process is larger than a first volume of the second spacer layer before the annealing process. In one embodiment, the method further comprises: after fabricating the source / drain regions, removing the first gate structure to expose second sections of the first semiconductor material and second sections of the second semiconductor material located beneath the first gate structure; selectively removing the second sections of the first semiconductor material, wherein, after the selective removal of the second sections of the first semiconductor material, the second sections of the second semiconductor material form a plurality of nanostructures;and fabrication of a replacement gate structure around the majority of nanostructures.;
[0071] In one embodiment, a semiconductor device comprises: a fin projecting over a substrate; a gate structure over the fin; source / drain regions over the fin on opposite sides of the gate structure; channel layers under the gate structure and between the source / drain regions, wherein the channel layers are substantially parallel to each other, the gate structure surrounding the channel layers; and inner spacers arranged vertically between end sections of adjacent channel layers and laterally between the gate structure and the source / drain regions, each of the inner spacers comprising a first dielectric layer and a second dielectric layer that is distinct from the first dielectric layer.In one embodiment, the first dielectric layer contacts the gate structure and the second dielectric layer contacts the source / drain regions, wherein the first dielectric constant of the first dielectric layer is higher than the second dielectric constant of the second dielectric layer. In another embodiment, a section of the gate structure extends through the first dielectric layer and contacts the second dielectric layer.
Claims
[1] A method of manufacturing a semiconductor device, the method comprising: Forming a dummy gate structure (106) over a fin structure (91) protruding above a substrate (50), the fin structure (91) comprising a fin (90) and a layer stack (92) over the fin (90), the layer stack (92) comprising alternating layers of a first semiconductor material (52) and a second semiconductor material (54); Forming openings (110) in the fin structure (91) on opposite sides of the dummy gate structure (106), the openings (110) exposing first portions of the first semiconductor material (52) and second portions of the second semiconductor material (54); Deepening the exposed first portions of the first semiconductor material (52) to form sidewall recesses (52R) in the first semiconductor material (52); lining the sidewall recesses (52R) with a first dielectric material; depositing a second dielectric material in the sidewall recesses (52R) on the first dielectric material; after depositing the second dielectric material, annealing the second dielectric material; and after annealing, forming source / drain regions (112) in the openings (110), wherein after deposition of the second dielectric material and before annealing there are air gaps in the sidewall recesses (52R), wherein annealing the second dielectric material removes the air gaps. [2] The method of claim 1, wherein the first dielectric material has a first dielectric constant and the second dielectric material has a second dielectric constant that is less than the first dielectric constant. [3] The method of claim 1 or 2, wherein after annealing, a volume of the second dielectric material is increased to fill the air gaps. [4] A method according to any one of the preceding claims, wherein annealing the second dielectric material comprises: Performing a first annealing process (62) using a first gas source; and after the first annealing process (62), performing a second annealing process (66) using a second gas source different from the first gas source. [5] The method of claim 4, wherein the first gas source comprises water vapor and the second gas source comprises nitrogen gas. [6] The method of claim 5, wherein the first annealing process (62) and the second annealing process (66) are performed at different temperatures. [7] Method according to one of claims 4 to 6, wherein the first annealing process (62) replaces NH2 functional groups and CH3 functional groups in the second dielectric material with OH functional groups. [8] The method of claim 7, wherein the second annealing process forms Si-O-Si cross-links in the second dielectric material. [9] The method of any preceding claim, wherein recessing the exposed first portions of the first semiconductor material (52) comprises performing an etching process using an etchant selective for the first semiconductor material (52). [10] Method according to one of the preceding claims, further comprising: after forming the source / drain regions (112), removing the dummy gate structure (106) to expose the first semiconductor material (52) and the second semiconductor material (54) disposed beneath the dummy gate structure (106); selectively removing the exposed first semiconductor material (52), wherein after the selective removal of the exposed first semiconductor material (52), the second semiconductor material (54) remains and forms a plurality of nanostructures; and Forming a replacement gate structure (123) around the plurality of nanostructures. [11] The method of claim 10, wherein removing the exposed first semiconductor material (52) comprises performing an etching process, the etching process etching through the first dielectric material and exposing the second dielectric material. [12] A method of forming a semiconductor device, the method comprising: Forming a first gate structure over a fin structure (91), the fin structure (91) comprising a fin (90) and a layer stack (92) over the fin (90), the layer stack comprising layers of a first semiconductor material (52) interleaved with layers of a second semiconductor material (54); Forming source / drain openings in the fin structure (91) on opposite sides of the first gate structure; selectively removing first portions of the first semiconductor material (52) exposed through the source / drain openings to form sidewall recesses (52R) in the first semiconductor material (52); lining the sidewall recesses (52R) with a multilayer spacer film (59), the multilayer spacer film (59) comprising a first spacer layer and a second spacer layer formed from different materials, wherein there are air gaps in the sidewall recesses (52R) after the lining; Performing an annealing process after lining, wherein the annealing process (62, 66) removes the air gaps in the sidewall recesses (52R); and after the annealing process (62, 66), forming source / drain regions (112) in the source / drain openings. [13] The method of claim 12, wherein the first spacer layer is formed of a first dielectric material and the second spacer layer is formed of a second dielectric material, wherein a first dielectric constant of the first dielectric material is higher than a second dielectric constant of the second dielectric material. [14] The method of claim 12 or 13, wherein performing the annealing process comprises: Performing a first annealing process (62) using a first gas source; and after the first annealing process (62), performing a second annealing process (66) using a second gas source different from the first gas source. [15] The method of claim 14, wherein a second volume of the second spacer layer after the annealing process (62, 66) is greater than a first volume of the second spacer layer before the annealing process (62, 66). [16] A method according to any one of claims 12 to 15, further comprising: after forming the source / drain regions (112), removing the first gate structure to expose second portions of the first semiconductor material (52) and second portions of the second semiconductor material (54) disposed beneath the first gate structure; selectively removing the second portions of the first semiconductor material (52), wherein after the selective removal of the second portions of the first semiconductor material (52), the second portions of the second semiconductor material (54) form a plurality of nanostructures; and Forming a replacement gate structure (123) around the plurality of nanostructures.
Citation Information
Patent Citations
Gate-all-around field-effect transistor with asymmetric threshold voltage
US20200105929A1
Spacer structure for semiconductor device
US20210126106A1
Air gap in inner spacers and methods of fabricating the same in field-effect transistors
US20210234017A1