Method for producing an electrically conductive channel structure in a substrate

DE102023207522B3Active Publication Date: 2024-10-31FRAUNHOFER GESELLSCHAFT ZUR FORDERUNG DER ANGEWANDTEN FORSCHUNG EV
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
DE102023207522
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-08-04
Publication Date
2024-10-31
Estimated Expiration
2043-08-04

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A method for producing an electrically conductive channel structure in a substrate comprises the following steps: (-) providing a stacked arrangement in a clamping device, wherein the stacked arrangement comprises a substrate provided with a channel structure, a metal foil having an aluminum material (= also an aluminum material alloy) on the substrate, and a compressible sealing element that surrounds the metal foil at least laterally under pressure, (-) applying a surface-acting mechanical process pressure and a process temperature to the stacked arrangement with the clamping device in order to melt the metal foil having the aluminum material at the process temperature and introduce it into the channel structure as metallic filler material by means of the surface-acting mechanical process pressure, and (-) cooling the stacked arrangement.to solidify the introduced metallic filler material and to maintain the electrically conductive channel structure filled with the metallic filler material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical area The present invention relates to a method for producing an electrically conductive channel structure in a substrate, e.g., in a glass substrate or silicon substrate, for example, as an interposer arrangement. The interposer arrangement can be produced using the described manufacturing method. The present invention relates to conductive channel structures (vias, blind vias, 3D structures) made of / with an aluminum material in a substrate that may comprise a glass, quartz, sapphire, ceramic, or semiconductor material. The present invention particularly relates to TGVs (through glass vias) or conductive channel structures (vias or blind vias) made of / with an aluminum material in glass substrates. The present invention further relates to TSVs (through silicon vias) or conductive channel structures (vias or blind vias) made of / with an aluminum material in silicon substrates. An interposer arrangement, for example, comprises an electrically conductive channel structure extending at least partially through a substrate, said channel structure comprising an aluminum material or an aluminum material alloy. Such an interposer arrangement can be manufactured, for example, using the manufacturing method for an electrically conductive channel structure in a substrate. Technical background In semiconductor technology, the term "via-hole plating" through a substrate, e.g. a silicon or glass substrate, or PCB (PCB = printed circuit board) refers to a vertical electrical connection made of metal through the substrate (also wafer or chip) in order to create an electrical connection between two or more metallization levels, e.g. on opposite sides of the substrate. Various competing technologies are known for the production of electrically conductive vias through wafer substrates. These are based either on the use of solder (soft solder) or galvanized copper to fill the vias. Such vias comprise an opening (a hole) through the substrate, which is plated with copper, forming an electrical connection through the substrate layers. Such vias also require an adhesion promoter layer on the via wall, making the resulting manufacturing process relatively complex. Furthermore, the processes used to date in microtechnology have the character of a 2.5D technology, i.e., only 2D structures can be lithographically structured which are extended vertically in depth, e.g., by high-rate etching. This limits the design options to purely vertical vias, whereby the use of adhesion promoters results in relatively poor high-frequency properties due to the skin effect (current displacement effect), since the current through the via concentrates in the surface (in the edge region) with increasing frequency, i.e., in the less conductive adhesion promoter. Furthermore, the limitation to purely vertical vias also results from the fact that the sidewall metallization, which is normally required for the galvanic filling of copper, can only be applied to accessible (i.e.,vertically extending) surfaces, i.e., on surfaces that are not obscured by other structures. Alternative manufacturing processes, for example, use pin vias embedded in glass made of highly conductive silicon, molybdenum, or tungsten, although these materials are not very suitable for high-frequency and quantum technology applications. US 2016 / 0 093 530 A1 relates to a method for forming vias through a substrate. DE 11 2020 002 022 T5 refers to BAVV resonators with antisymmetric thick electrodes. DE 10 2012 208 033 A1 relates to a hybrid integrated component and a method for its production. DE 10 2020 128 994 A1 relates to a semiconductor package and a method for producing the same. US 2013 / 0 115 730 A1 refers to low-temperature wafer-level processing for MEMS components. WO 2009 / 134 838 A2 relates to a system and method for encapsulation. The object underlying the present invention is therefore to provide an improved method for producing electrically conductive channel structures in a substrate. This problem is solved by the subject matter of independent patent claim 1. Specific embodiments, implementations and further developments of the present invention are defined in the dependent claims. Overview of the inventive concept (method and device): According to one embodiment, a method for producing an electrically conductive channel structure in a substrate comprises the following steps: - Providing a stack arrangement in a clamping device, wherein the stack arrangement comprises a substrate provided with a channel structure, a metal foil (or sheet) comprising an aluminum material (= also an aluminum material alloy) on the substrate, and a compressible sealing element designed to surround the metal foil (at least) laterally under pressure, - Applying a surface-acting mechanical process pressure and a process temperature with the clamping device to the stack arrangement in order to melt the metal foil comprising the aluminum material at the process temperature and to introduce it into the channel structure as a metallic filler material by means of the surface-acting mechanical process pressure, and - Cooling the stack arrangement,to solidify the introduced metallic filler material and to maintain the electrically conductive channel structure filled with the metallic filler material. The compressible sealing element can be designed, for example, as an overlapping surface seal or as an enclosing ring seal. The compressible sealing element can also be designed for high-temperature applications at the process temperature (as a compressible high-temperature sealing element). The present invention is therefore based on the finding that a novel, advantageous method for producing electrically conductive channel structures (e.g., in the form of feedthroughs, 3D structures (3D = 3-dimensional), passive components, or blind holes, etc.) in a substrate can be implemented, wherein the channel structures, e.g., through-holes, blind holes, or 3D structures, in a dielectric substrate are pressure-filled with an aluminum melt (based on a metal foil comprising an aluminum material or an aluminum material alloy). Channel structures with different geometries with regard to hole diameter, flank angle, channel inclination, and channel length can be filled. With the method according to the invention for producing electrically conductive channel structures in a substrate, a corresponding interposer arrangement can also be obtained or produced. According to one example, an interposer arrangement comprises a substrate having an electrically and / or thermally conductive channel structure extending at least partially through the substrate, wherein the channel structure comprises an aluminum material or an aluminum material alloy, wherein the electrically and / or thermally conductive channel structure extends from a main surface area of the substrate into the substrate. The aluminum material or aluminum material alloy has at least 80% or 90% aluminum as its main component in order to have a resulting melting point of at least 420°C (or 520°C) or between 420°C (or 520°C) and 850°C as a brazing solder. Short description of the drawings and figures Preferred embodiments of the present invention are explained in more detail below with reference to the accompanying drawings and figures. They show: Fig. 1 a schematic flow diagram of the manufacturing method according to the invention according to one embodiment; Fig. 2a an exemplary basic flow diagram of the manufacturing method according to the invention, e.g. with an overlapping surface seal, according to a further embodiment; Fig. 2b an exemplary basic flow diagram of the manufacturing method according to the invention, e.g. with an enclosing ring seal, according to a further embodiment; Fig. 3a exemplary Al-TGVs (Aluminum Through-Glass Vias) in glass (e.g. quartz glass) produced using the manufacturing method of Fig. 1 or Fig. 2; Fig. 3b a detailed illustration of the interface connection between the conductive Al filling (of the Al-TGV) and glass (e.g. borosilicate glass) produced using the manufacturing method of Fig.1 or Fig. 2; Fig. 4a -b an example of an Al-Cu melt filling in a quartz substrate (manufactured using the manufacturing method according to Fig. 1 or Fig. 2 ) according to an embodiment; Fig. 5a -c an exemplary procedure for obtaining improved electrical properties of the vias (Al-TGVs) according to an embodiment; Fig. 5d a further exemplary procedure for obtaining improved electrical properties of the vias (Al-TGVs) according to an embodiment; Fig. 6a -i exemplary geometries of channel structures with different dimensions and wall angles (for filling using the manufacturing method according to the invention of Fig. 1 or Fig. 2 ); Fig. 7 a schematic representation of further possible substrate topologies for use in the manufacturing method according to the invention of Fig. 1 or Fig. 2;8-12 show exemplary embodiments of an interposer arrangement or of a part of the interposer arrangement according to FIG. 1; FIGS. 8a-e show schematic representations of exemplary interposer arrangements (with possible substrate topologies) according to further exemplary embodiments, which can be obtained, for example, using the inventive manufacturing method of FIG. 1 or FIG. 2; FIG. 9a show exemplary 3D channel structures (e.g., an aluminum-filled 3D coil) produced using the inventive manufacturing method of FIG. 1 or FIG. 2 according to an exemplary embodiment; FIG. 9b shows an enlarged 3D X-ray tomography image of the aluminum-filled 3D coil of FIG. 9a; FIG. 10 shows a perspective view (3D view) of a component (in the form of a metal-filled coil) in a glass substrate produced using the manufacturing method of FIG. 1 or FIG. 2 according to an exemplary embodiment;11 shows a perspective view of a component (in the form of a thin-film getter structure with via contacting) manufactured using the manufacturing method of FIG. 1 or FIG. 2 according to an embodiment; FIGS. 12a-b show a perspective view and a cross-sectional view of a component (in the form of a capacitor structure) manufactured using the manufacturing method of FIG. 1 or FIG. 2 according to an embodiment; FIGS. 13a-c show cross-sectional views of packaged components (e.g., MEMS, sensors, and / or ICs) with the Al-TGVs (manufactured using the manufacturing method of FIG. 1 or FIG. 2) for electrical connection (as an electrical via) and / or thermal connection (for heat dissipation) according to an embodiment; FIG. 14 shows an exemplary basic flow diagram for further processing (at wafer level) of the stack arrangement obtained using the manufacturing method of FIG. 1 or FIG. 2 according to an embodiment; and FIG.15 - 22 exemplary, basic flow diagrams relating to further and alternative procedures for producing an electrically conductive channel structure by introducing a metallic filling material according to further embodiments. Before exemplary embodiments of the present invention are explained in more detail below with reference to the drawings, it is pointed out that identical, functionally equivalent or equivalent elements, objects, functional blocks and / or method steps in the different figures are provided with the same reference numerals, so that the description of these elements, objects, functional blocks and / or method steps (with the same reference numerals) shown in different exemplary embodiments is interchangeable or can be applied to one another. Detailed description of the figures and embodiments In the following description, the description of an element made of a material such as a glass, quartz, sapphire, ceramic or semiconductor material means that the element comprises this material, ie is formed at least partially or completely from the semiconductor material. It is understood that when an element is described as being "connected" or "coupled" to another element, it may be directly connected or coupled to the other element, or intervening elements may be present. Conversely, when an element is described as being "directly connected" or "coupled" to another element, no intervening elements are present. Other terms used to describe the relationship between elements should be interpreted similarly (e.g., "between" versus "directly between," "adjacent" versus "directly adjacent," etc.). To simplify the description of the different exemplary embodiments, at least some of the figures have a Cartesian coordinate system x, y, z, wherein the directions x, y, z are arranged orthogonal to one another. In the exemplary embodiments, the xy plane corresponds to the main surface area of a carrier or substrate (= reference plane = xy plane), wherein the vertical direction upwards relative to the reference plane (xy plane) corresponds to the "+z" direction, and wherein the vertical direction downwards relative to the reference plane (xy plane) corresponds to the "-z" direction. In the following description, the term "lateral" means a direction parallel to the x and / or y direction, i.e. parallel to the xy plane, wherein the term "vertical" indicates a direction parallel to the + / -z direction. In the context of this description, terms and / or text passages placed in brackets are to be understood as examples of further explanations, exemplary embodiments, additions and / or exemplary alternatives (to the preceding term or the preceding text passage). A schematic flow diagram of the method 100 according to the invention for producing an electrically conductive channel structure in a substrate is described below with reference to Fig. 1. The arrangement obtained in the manufacturing method 100, i.e., a substrate with electrically conductive channel structures or vias, can then be used, for example, as a so-called interposer arrangement 50 for electronic components for their rerouting and / or heat dissipation, etc. Referring to the method 100 of Fig. 1, at step 120, a stack arrangement is provided in a clamping device (clamping arrangement), wherein the stack arrangement comprises a substrate provided with a channel structure, a metal foil comprising an aluminum material or an aluminum material alloy on the substrate, and a compressible sealing element which surrounds the metal foil (at least) laterally under surface-acting pressure. The compressible sealing element can be designed, for example, as an overlapping surface seal or as an enclosing ring seal. The compressible sealing element can also be designed for high-temperature applications at the process temperature (as a compressible high-temperature sealing element). In a (subsequent) step 140, a surface-acting mechanical process pressure and a process temperature are now exerted on the stack arrangement with (by means of) the clamping device in order to melt (liquefy) the metal foil comprising the aluminum material at the process temperature and to introduce it into the channel structure as a metallic filler material by means of the surface-acting mechanical process pressure. According to one embodiment, in step 140, for example, the liquefied material of the metal foil is enclosed between the compressible surface sealing element and the substrate provided with the channel structures. The compressible surface sealing element covers the metal foil and overlaps the edge region of the metal foil, thus surrounding the metal foil (covering and laterally surrounding it) under pressure up to the substrate. Thus, lateral leakage / escape of the liquefied / molten material of the metal foil can be prevented by the surrounding surface sealing element. According to a further embodiment, in step 140, for example, the liquefied material of the metal foil is enclosed between a first tool (e.g., press die) of the clamping device and the substrate provided with the channel structures, wherein a compressible ring sealing element (= an enclosing ring seal) surrounds (encloses) the edge region of the metal foil, so that the ring sealing element surrounds the metal foil laterally (between the substrate and the first tool) under pressure. This can prevent the liquefied / molten material of the metal foil from lateral leakage (escape) through the surrounding ring sealing element. In a subsequent step 160, the stack arrangement is cooled in order to resolidify (solidify) the introduced metallic filler material (ie, the metallic filler material melted during introduction) in order to obtain the electrically conductive channel structure filled with the (solidified) metallic filler material. According to one embodiment, the channel structure can be formed as at least one through-hole structure, as at least one blind hole structure or as at least one 3D structure in the substrate. According to one embodiment, the metal foil may comprise the aluminum material as the main component (≥ 80%) for a resulting melting point of at least 420°C (or 520°C) or between 420°C (or 520°C) and 850°C. According to one embodiment, the (elevated) process temperature may be set to a value of at least 10 K or 20 K above the melting temperature of the metal foil comprising the aluminum material. According to one embodiment, the channel structure may have a coating (wall coating) comprising nitride material, e.g., with AIN (aluminum nitride), SiN (silicon nitride) or TiN (titanium nitride) with a thickness in a range of 2 to 100 nm. According to one embodiment, the compressible sealing element can be designed as a compressible surface sealing element. According to one embodiment, the surface sealing element can cover the metal foil and have a lateral projection (extending laterally beyond the metal foil), i.e., overlap the metal foil in order to enclose the metal foil up to the substrate when the mechanical process pressure is applied. According to one embodiment, the compressible sealing element can be designed as a compressible ring sealing element, wherein the ring sealing element surrounds the edge region of the metal foil and laterally encloses the metal foil under the application of pressure. According to one embodiment, the sealing element can be designed as a reusable high-temperature seal. According to one embodiment, the sealing element can comprise or consist of a graphite foil or a structured (annular) graphite foil with a thickness in a range of 0.3 to 1 mm or approximately 0.5 mm. According to one embodiment, the clamping arrangement may comprise a first and a second tool, with the stacking arrangement arranged between the first and second tools. According to one embodiment, the step of exerting mechanical pressure between the first and second tools may be performed with a contact pressure in a range of 10 N / cm2 to 600 N / cm2. According to one embodiment, the first and / or second tool may be configured to heat the stacking arrangement to the process temperature. According to one embodiment, the first tool can be designed as a press stamp and the second tool as a counter substrate, wherein a main surface area of the second tool facing the substrate has a surface roughness with a mean roughness Ra or an average roughness depth RZ between 0.5 to 10 µm or of approximately 3 µm. According to one embodiment, the main surface area of the second tool facing the substrate may have a coating to provide the surface roughness of the main surface area of the second tool facing the substrate. This coating can prevent adhesion of the aluminum melt and, at the same time, adhesion of the hot glass substrate. According to one embodiment, the coating may comprise a boron nitride material. According to one embodiment, the surface roughness of the main surface area of the second tool adjacent to the substrate may be selected to act as a flow stop for the molten metal and to allow lateral escape of a gas present in the channel structure. According to one embodiment, the substrate may comprise or consist of a glass, quartz, sapphire, ceramic or semiconductor material. According to one embodiment, the method 100 may further include removing excess metallic filler material on one side of a main surface region or on both sides of both opposite main surface regions of the substrate. According to one embodiment, the removal of the excess material may be performed by means of a CMP process (CMP = chemical mechanical polishing). According to one embodiment, the method may further comprise removing the stack assembly from the clamping assembly and removing the sealing element from the substrate. According to one embodiment, the method may further comprise performing a single-sided or double-sided metallization by means of a thin-film deposition process in order to obtain, via a lithographic patterning process and a subsequent etching step, a metallization structure electrically connected to the conductive channel structure on one or both main surface regions of the substrate formed with the conductive channel structure. According to the invention, a novel, advantageous method for producing electrically conductive channel structures, e.g., in the form of feedthroughs, 3D structures, passive components, or blind holes, etc., in a substrate is thus obtained. The channel structures, e.g., through-holes in a dielectric substrate, are pressure-filled with an aluminum melt (based on a metal foil comprising an aluminum material or an aluminum material alloy). Channel structures with different geometries regarding hole diameter, flank angle, channel inclination, and channel length can be filled. To achieve this, the method first provides a stacked assembly in a clamping device, wherein the stacked assembly comprises a substrate provided with a channel structure, a metal foil comprising an aluminum material (or an aluminum material alloy) on the substrate, and a compressible sealing element. The compressible sealing element surrounds (encloses) the metal foil under pressure, at least laterally (as a ring seal) or encloses the metal foil up to the substrate (as a surface seal). Subsequently, a surface-acting mechanical process pressure and an (elevated) process temperature are applied to the stack assembly by means of the clamping device in order to melt the metal foil containing the aluminum material at the process temperature and to introduce or press it into the channel structure as a metallic filler material using the surface-acting mechanical process pressure. Finally, the stack assembly is cooled to solidify the introduced metallic filler material and obtain the electrically conductive channel structure filled with the metallic filler material. In this context, it should be noted that aluminum acts as its own adhesion promoter to glass, quartz, ceramic, or sapphire substrates. Bonding to silicon and oxidized silicon substrates is also possible. The provision of an additional adhesion promoter layer can therefore be omitted or is no longer necessary, which not only makes the aluminum via (Al via) significantly easier to manufacture compared to conventional manufacturing processes, but also makes the filling of true 3D structures possible. Sidewall wetting can optionally be improved by dielectric coatings. Conformal deposition (ALD = atomic layer deposition) or LP-CVD (LP-CVD = low-pressure chemical vapor deposition) technology is particularly suitable for this purpose. Suitable dielectric layer materials include aluminum nitride (AIN), aluminum oxide (Al2O3), silicon nitride (SiN), titanium nitride (TiN), etc., e.g., with a thickness in the range of 2 to 100 nm or 30 to 50 nm. The aluminum wettability of the channel structure can be favorably influenced by a pre-coating with SiN, AlN, TiN, etc., using an LP-CVD or ALD process. The layer thicknesses range from 2 nm to 100 nm, or (preferably) from 30 to 50 nm. The (conformal) pre-coating can be used either to fill smaller via diameters (in the range of 5 to 15 µm) at the same process temperature and pressure, or, in particular, to reduce the necessary pressure for larger via diameters. Since aluminum is very ductile (= has the property of plastically deforming under load before it fails), aluminum can be pressed quite easily into the opening(s) in the substrate in molten form using a hot-filling process without the very large differences in the thermal expansion coefficients between the substrate material, e.g. glass, silicon, etc., and the aluminum material or aluminum alloy leading to destruction, cracks in the substrate or detachment at the interface between metal and substrate. The filling process of the hole and / or channel structures can be improved by applying a suction vacuum (= by applying a negative atmospheric pressure) to remove gases in the hole and / or channel structure, or by introducing a protective gas atmosphere to prevent hot oxidation, particularly at the wetting front. For complex-shaped hole and / or channel structures (e.g., 3D structures), undesired gas entrapment along the channel to be filled can be avoided by evacuating the channel structures prior to filling, e.g., from two opposing channel inlets simultaneously. The particularly dense interface connection between the substrate (e.g. a dielectric substrate) and the aluminum filling also opens up the possibility of producing hermetically sealed vias. The method 100 is applicable for the sequential filling of individual hole structures, of groups of hole arrangements (chips / modules) or of all hole structures 12-1 present on a substrate 12 in a common parallel filling process step. Fig. 2a now shows an exemplary basic flow diagram of the method 100 according to the invention for producing an electrically conductive channel structure 12-2 in a substrate 12, wherein, for example, an overlapping surface seal is used. Fig. 2a thus shows a possible implementation of the various method steps of the schematic flow diagram of the manufacturing method 100 illustrated with reference to Fig. 1. The arrangement obtained in the manufacturing method 100, i.e. a substrate with electrically conductive channel structures or vias, can then be used, for example, as a so-called interposer arrangement 50 for electronic components, such as as rewiring (rerouting interposer), as a conductive via, as a (passive) electrical component or for heat dissipation, etc. Referring to the method 100 of Fig. 2a, in step 120, a stack assembly 10 is provided in a clamping device 30 (clamping assembly), wherein the stack assembly 10 comprises a substrate 12 provided with a channel structure 12-1, a metal foil 14 comprising an aluminum material or an aluminum material alloy on the substrate 12, and a compressible surface sealing element 16 covering the metal foil 14 and surrounding the metal foil 14 under (area-acting) pressure application up to the substrate 12. According to the embodiment of the manufacturing method 100 shown in Fig. 2a, the clamping device 30 can have a first and a second tool 32, 34, wherein the stacking arrangement 10 is arranged or clamped (flush) between the first and second tools 32, 34 of the stacking arrangement 30. In a (subsequent) step 140, a surface-acting mechanical process pressure FP and a process temperature TP are now applied to the stack arrangement 10 with (by means of) the clamping device 30 in order to melt (liquefy) the metal foil 14 comprising the aluminum material at the process temperature TP and to introduce it into the channel structure(s) 12-1 as metallic filler material 14-1 by means of the surface-acting mechanical process pressure FP. In step 140, for example, the liquefied material 14-1 of the metal foil 14 is enclosed between the compressible surface sealing element 16 and the substrate 12 provided with the channel structure(s) 12-1, so that lateral leakage (escape) of the liquefied (molten) material 14-1 of the metal foil 14 is prevented by the surrounding surface sealing element 16. The compressible surface sealing element can cover the metal foil at least partially or completely, wherein, for example, at least the (entire) edge region of the metal foil is (completely) overlapped by the compressible surface sealing element 16. According to one embodiment, the surface sealing element can cover the metal foil and have a lateral projection extending beyond the edge of the metal foil. This overlap of the surface sealing element 14 beyond the edge region of the metal foil can, for example, have an annular, circumferential thickening or bulge (curvature) 16-1, which extends (as a depressed edge region of the surface seal) to the substrate. Thus, the surface sealing element can completely enclose the metal foil without exerting a surface-acting mechanical process pressure FP. In a subsequent step 160, the stack arrangement 10 is cooled in order to resolidify (solidify) the introduced metallic (molten) filler material 14-1 in order to obtain the electrically conductive channel structure(s) 12-2 filled with the (solidified) metallic filler material 14-1. In the manufacturing method 100 illustrated by way of example in Fig. 2a, an aluminum pressure melt filling of the channel structures 12-1 in the substrate 12 is carried out. The (second) tool 34 of the clamping device 30 arranged on the substrate 12 serves, for example, as a counter substrate to obtain a flow stop (or a flow stop function) during the melt filling process, wherein the compressible high-temperature seal 16 is provided as an overlapping boundary or enclosure to cause lateral exit or escape of the liquefied (molten) material 14-1 of the metal foil 14 on the side of the substrate 12 adjacent to the first tool 32 of the clamping device 30. According to one embodiment, the step of exerting 140 mechanical pressure FP between the first and second tools 32, 34 of the clamping device 30 can be carried out with a contact pressure (between the first and second tools 32, 34) of greater than 10 N / cm2 or in a range between 10 N / cm2 and 600 N / cm2. According to one embodiment, the first or second tool 32, 34, or both tools 32, 34 of the clamping device 30 can be configured to heat the (clamped) stack assembly 10 to the (elevated) process temperature TP. This process can also be referred to as tempering. In the context of the present description, tempering (applying the process temperature) is understood to mean a temperature treatment, for example, a time-controlled, homogeneous heating of the stack assembly, wherein this temperature treatment is applied, for example, during the application of the planar mechanical pressure FP between the first and second tools 32, 34 of the clamping device 30. The step 140 of applying a process temperature TP to the stack assembly 10 can be performed, for example, with a predetermined temperature profile (or temperature ramp). The application 140 of the process temperature TP (peak temperature) to the stack assembly 10 can be performed, for example (depending on the material of the metal foil 14) for 1 to 30 (e.g., 3 to 15 or 3 to 5) seconds. The heating of the stack assembly 10 and the application of the process temperature TP (peak temperature) to the stack assembly 10 can, for example, be carried out independently of any additional alloying, provided this has already been applied. The production of an AlCu melt can take place during the heating process and does not significantly prolong the process. The extension (due to the additional alloying) can be in the range of 15 to 20 seconds. As shown by way of example in step 120 of Fig. 2a, the stack arrangement 10 comprises, in the vertical direction (from top to bottom in Fig. 2a), the compressible surface sealing element 16 (high-temperature seal), the metal foil 14 comprising the aluminum material (= also an aluminum material alloy), and the substrate 12 provided with the channel structure(s) 12-1, e.g., a perforated glass, quartz, sapphire ceramic, or semiconductor substrate (wafer). In the exemplary embodiment of the manufacturing method 100 shown in Fig. 2a, the first tool 32 is designed, for example, as a press die, and the second tool 34 of the clamping device 30 is designed as a (e.g., coated) counter substrate, wherein the second tool 34 also acts as a flow stop for the liquefied material 14-1 of the metal foil 14 during the filling process. The material of the compressible surface sealing element 16 also prevents contact of the liquid aluminum 14-1 with the pressure or pressing ram 32. Furthermore, the liquefied aluminum 14-1 does not adhere to the material of the compressible surface sealing element (the high-temperature surface seal) 16. Typical suitable materials for the compressible surface sealing element are, for example, graphite or materials such as boron nitride, etc. With regard to the process sequence 100 shown in Fig. 2a, it is further noted that the stacking arrangement 10 may also have an inverted (reverse) sequence between the first and second tools 32, 34 of the clamping device 30 without the process result being (significantly) changed or impaired, since gravity effects (iW) have no influence on the filling process. By applying the surface-acting mechanical process pressure FP and the elevated process temperature TP (annealing process) with the liquefaction (melting) of the material of the metal foil 14, which comprises an aluminum material, the channel structure(s) 12-1 of the substrate 12 are pressurized. The metal foil 14 is surrounded or enclosed by the surface sealing element 16 up to the substrate 12 (also laterally) due to the compression (surface-acting mechanical pressure) of the compressible surface sealing element 16. Due to the flow-stopping effect of the counter-substrate or the surface 34-1 of the counter-substrate 34, the filling process in step 140 takes place up to the surface 34-1 of the second tool 34 of the clamping device 30, which acts as the counter-substrate. According to one embodiment, a main surface region 34-1 of the second tool 34 (the counter substrate) facing the substrate 12 can have a surface roughness with a mean roughness Ra or an average roughness depth RZ of between 0.5 µm and 10 µm or of approximately 3 µm. This surface quality (the roughness) of the main surface region 34-1 of the second tool 34 facing the substrate 12 prevents, on the one hand, adhesion of the molten metal (molten aluminum) to this main surface region 34-1 of the second tool 34 during the pressure filling process and, furthermore, prevents adhesion of the hot substrate 12 (e.g., the glass substrate), which is at the process temperature TP, to this main surface region 34-1 of the second tool 34. According to one embodiment, the main surface region 34-1 of the second tool 34 facing the substrate 12 can have a coating 36 to provide this surface roughness of the main surface region 34-1 of the second tool 34 facing the substrate 12. Thus, the surface texture of the main surface region 34-1 of the second tool 34 facing the substrate 12 can be obtained, for example, by means of the coating 36, wherein the coating 36 can comprise or consist of a boron nitride material. The boron nitride (BN) does not react with the liquefied material (aluminum material) 14-1 of the metal foil 14, since boron nitride is oxidation-resistant up to approximately 800°C and does not react with glass or metal. Furthermore, BN does not adhere to glass, nor does the hot glass mass adhere to the BN. Furthermore, the boron nitride material can achieve the desired surface roughness of the second tool 34, whereby during the filling process it can also be achieved that air / gas can escape laterally from the channel structures 12-1 of the substrate 12, while the surface texture has or provides the desired flow-stopping effect for the molten metal 14-1 on the surface 34-1 of the counter-substrate 34 (second tool). As further illustrated by way of example in Fig. 2a of the manufacturing method 100, the first tool 32 (the press ram) can further have a non-stick coating 38 on its main surface region 32-1 (facing the substrate 12), which enables simplified detachment (removal) of the first tool 32 from the stack arrangement 10, i.e., from the compressible surface sealing element 16, after the filling and cooling process 140, 160 of the method 100. The non-stick coating 36 can, for example, be arranged on (or form) the main surface region 32-1 of the first tool 32 facing the stack arrangement 10. According to one embodiment, the coating 36 of the second tool 34 may comprise a boron nitride material, wherein the surface roughness of the main surface region of the second tool 34 adjacent to the substrate 12 is selected to act as a flow stop for the molten metal and to enable lateral escape of a gas present in the channel structure 12-1 of the substrate 12. Thus, the flow front of the molten material 14-1 of the metal foil 14 can impact a plate 34 (second tool 34) located beneath the substrate 12, which plate is provided with the rough boron nitride coating. The flow front pushes the gas in the channel downwards and stops flat on the substrate 12. The gap formed by the coating roughness is so narrow that the flow front cannot move further laterally between the substrate 12 (e.g. glass substrate) and the second tool (counter substrate plate) 34.In this procedure, a protective gas atmosphere is helpful / possible, but not absolutely necessary. This allows for sufficient control of the flow front. According to one embodiment, the substrate 12 may comprise, for example, a dielectric material, such as glass, quartz, sapphire, ceramic, etc., or a semiconductor material, e.g., silicon (polysilicon). When using silicon (polysilicon) for the substrate 12, it may be necessary, for example, to provide an additional barrier and insulation layer, e.g., made of SiO2, to prevent a possible reaction of the hot liquid aluminum material with the silicon. The step 160 of cooling the stack arrangement 10 can, for example, be carried out with a predetermined temperature profile (or temperature ramp, as in the step of applying the process temperature) in order to ensure, for example, that the cooling of the elements and structures involved is carried out in the most material-friendly manner possible due to different thermal expansion coefficients. The cooling process 160 can, for example, be carried out with a (average) temperature change (cooling) of 20 to 500 K (or 30 to 400 K or 300 to 400 K) per minute (until a normal temperature is reached (e.g., removal temperature of the filled substrate 12, e.g., in a range between the ambient temperature and approximately 200°C). The time required for the cooling process may depend, for example, on the structure of the clamping device 30 and, for example, the stamping unit 32. After step 160 of cooling the stack assembly 10 and the clamping device 30, after the release of the surface-acting mechanical process pressure FP, the stack assembly 10 can be removed from the clamping device 30, wherein the surface sealing element 16 can then also be removed from the substrate 12. After removing the substrate 12 (e.g., glass substrate) equipped, for example, with the aluminum feedthroughs (e.g., aluminum TGVs) 12-2 and the relaxed seal (surface sealing element) 16, the substrate 12 provided with the electrically conductive channel structure(s) 12-2, for example, can now be fed to further processing steps. Thus, in the method 100, excess metallic filler material 14-2 can further (optionally) be removed on one side of a main surface area or on both sides of both opposite main surface areas of the substrate 12, e.g. by means of a CMP process (CMP = chemical mechanical polishing). Furthermore, in the method 100 (optionally), a one-sided or two-sided metallization can be carried out on the substrate 12 by means of a thin-film deposition process in order to obtain, for example, via a lithographic structuring process and a subsequent etching step, a metallization structure electrically connected to the conductive channel structure 12-2 on one or both main surface regions of the substrate 12 formed with the conductive channel structure 12-2. The method 100 according to the invention for producing an electrically conductive channel structure 12-2 in the substrate 12 can thus be used to obtain, for example, an arrangement such as an interposer 50, which has channel structures 12-2 completely filled with metal in the substrate 12 (e.g., a flat substrate), wherein, for example, a chemical bonding zone (interface) of the metal filling 14-1 of the channel structures 12-2 to the channel walls is obtained without, for example, a metallic thin-film adhesion promoter coating being required or used in the method. With regard to the stacking arrangement 10 shown in Fig. 2a in the description of the manufacturing method 100, it should be noted that a plurality of such stacking arrangements 10 can also be arranged between the first and second tools 32, 34 of the clamping device 30 in order to carry out the manufacturing method 100 of Fig. 2a. It should only be noted that either the compressible surface sealing element 16 used in each case or another intermediate layer can be used as the respective counter-substrate 34 to provide the flow-stopping effect. According to one embodiment, the channel structure 12-1 can be formed as at least one through-hole structure, as at least one blind-hole structure or as at least one 3D structure in the substrate 12, so that after carrying out the method 100, an electrically conductive channel structure 12-2 is obtained in the substrate 12 in the form of a conductive through-hole structure, at least one conductive blind-hole structure or at least one conductive 3D structure in the substrate. According to one embodiment, the (elevated) process temperature TP can be set to a value of at least 5 K, 10 K, or 20 K above the melting temperature of the metal foil 14 comprising the aluminum material. The process temperature TP is thus selected to ensure reliable melting of the material of the metal foil 14 with the lowest possible thermal stress on the elements and structures involved. For this purpose, the first or second tool 32, 34, or both tools 32, 34, can be configured to heat the stack arrangement 10 to the desired process temperature TP, i.e., to perform the tempering process at the desired process temperature TP. During the melt filling of the channel structures 12-1 of the substrate 12 defined according to method 100, the process temperature is therefore at least 5 K, 10 K, or 20 K higher than the melting temperature of the metal of the metal foil 14 selected for the filling. The process temperature is, for example, upper limited by the softening temperature of the substrate material. If, for example, glass is used as the substrate material, its viscosity decreases with increasing temperature (e.g., continuously), whereby glass is an amorphous inorganic material. By means of a supporting carrier material 13 (see, for example, Fig. 20) with a high melting temperature or softening temperature, e.g., silicon, even low-melting glass substrates 12 can be filled with aluminum or an aluminum alloy without bending or structural changes to such a glass substrate 12 occurring. According to one embodiment, the metal foil 14 can comprise the aluminum material as its main component, e.g., with a proportion of ≥ 80%, 90%, or 95%, or even pure aluminum (= 100% proportion), for a resulting melting point of at least 420°C or 520°C, or between 420°C (or 520°C) and 850°C. Thus, the material of the metal foil is a brazing material, since the brazing temperature, by definition, is above 420°C or even above 520°C. By adjusting the melting temperature and the "over" temperature above it (process temperature = melting temperature + 5 / 10 / 20 K), the wettability of a pure aluminum melt (without ambient oxygen) in the hole structures 12-1 can be improved by reducing the surface tension of the metal melt 14-1 by approximately 5% (e.g., filling temperature approximately 830 °C), while the density of the melt 14-1 and the viscosity are little affected. In aluminum-copper alloys for the metal foil 14, this effect is pronounced and dependent on the copper content. Since higher alloying proportions (of copper) can increase strength and generally also lead to significantly increased volume resistances, the metal material of the metal foil contains aluminum as its main component, e.g., at least 80%, 90%, 95%, or 99%.While the density, surface tension and viscosity of pure aluminum depend little on temperature, there is a significant effect on aluminum-copper alloys, at least for the viscosity. The metal foil 14, which comprises the aluminum material (as the main component), can have a single-layer or multi-layer foil structure. Thus, the metal foil 14 can comprise a single-layer aluminum material, a two-layer composite comprising an aluminum layer and a copper layer (or foil in each case), a three-layer composite comprising an aluminum layer, a copper layer, and another aluminum layer, etc., as long as the aluminum material represents the main component of the multi-layer foil structure (and rests on the substrate 12). As glass materials for the substrate (glass substrate) 12, for example, a Borofloat® glass (Borofloat 33 from Schott) or another glass, such as Schott AF32, Corning Eagle XG, Hoya SD2, can be used. According to one embodiment, the surface sealing element 16 can cover the metal foil 14 and have a lateral projection (over the metal foil 14) in order to enclose the metal foil 14 (hermetically sealed) up to the substrate 12 when the mechanical process pressure FP and the process temperature TP are applied. According to one embodiment, the compressible surface sealing element 16 can be designed as a reusable high-temperature seal. According to a further embodiment, the surface sealing element 16 may comprise or consist of a graphite foil having a thickness in a range of 0.3 mm to 1 mm or of approximately 0.5 mm. In addition to graphite, other materials that do not adhere to the liquid aluminum material, such as other carbons, SiC, or BN, can be considered as materials for the compressible surface sealing element 16. For example, fabrics made of / with graphite, SiC, and / or BN fibers (each individually or in combination) can also be used. Due to the compressible high-temperature surface seal (e.g., a graphite foil) 16 with the (lateral) overlap over the edge of the applied metal foil (e.g., aluminum or aluminum alloy foil), the molten metal (the molten material 14-1 of the metal foil 14) can be held above the substrate area to be filled (with the channel structures 12-1) of the substrate 12 during the step of applying surface-acting mechanical process pressure FP and the process temperature TP, and lateral squeezing (escape) under pressure FP can be avoided. By using the compressible surface seal element 16, very high yields can be achieved in the manufacturing method 100. The lateral projection of the gasket seal over the metal foil can depend, for example, on the thickness of the metal foil and / or the thickness of the gasket seal. For an aluminum foil of thickness H, a gasket seal 16 of thickness D can have an overlap (lateral projection) or a width of the outer sealing area W in the following ratio: W > 50 x H / D mm, or 100 x H / D mm > W > 50 x H / D mm. In the context of the present description of method 100, filling or the filling process refers to the introduction of molten metal 14-1 for the complete or partial filling of cavities or channel structures 12-1 in a substrate 12, e.g., a ceramic, glass, or silicon substrate. Filling can also be understood as an inner wall lining of cavities or channel structures 12-1 in the substrate 12 with a metal coating or a filling limited to the depth of the channel structure 12-1. A substrate 12 is understood, for example, to be a material body having two opposite parallel main surface areas (sides), regardless of the width-to-height ratio. The opposite sides of the substrate 12 can, but do not have to, be arranged parallel to each other, and may also be arranged non-parallel to each other in some areas. In the context of the present description, a channel, channel structure or cavity 12-1 is referred to as a recess with at least one open side (opening) to an outer side of the substrate 12, whereby this is independent of the geometric shape of the recess 12-1, e.g. in the form of a lateral slot, a pocket, a blind hole or a through-hole, or a channel in any geometric design with at least one opening to a substrate surface. Although reference is often made in the present description to an aluminum filling (based on the metal foil comprising an aluminum material), the method according to the invention can also be applied to filling with ultrapure aluminum or aluminum alloys. For example, alloys with a reduced melting point in relation to ultrapure aluminum can be used, wherein one or more alloying elements from the areas of copper, silicon, germanium and / or magnesium can be used. Furthermore, alloys or aluminum alloys with improved electrical properties, e.g. against electromigration, such as Al-Si or AlCu (each a few % share, e.g. 1 to 5 % share) can be used. This list of alloying elements is only to be regarded as exemplary and not exhaustive. Furthermore, it is pointed out that the term foil in “metal foil, aluminum foil, aluminum alloy foil” 14 in the context of the present description includes the use of stacked individual foils but also thin metal sheets or roll-clad sheets, e.g. made of aluminum-copper, from which alloys are formed, for example, during the filling process and fill the channel structures or perforations 12-1 of the substrate 12 (at least partially). Typical thicknesses of metal foils and metal sheets can range from 20 µm to 1000 µm or between 20 µm and 50 µm and around (typically) 30 µm. According to embodiments, the metal foil comprises the aluminum material as the main component with a volume fraction of >60%, >80%, or even >90%. Furthermore, the manufacturing method 100 according to the invention enables the electrically conductive channel structures 12-2 in the substrate 12 to fill a metal filling 14-1 to a degree of 90% or even between 95% and 98% and up to 100%, i.e., the channel structure 12-2 is completely filled (i.e., at least 90% or 98%), free of pores or inclusions. According to one embodiment, for example, for the purely aluminum melt filling of channel structures 12-1 in low-melting glass substrates 12, e.g., Schott BF33, temperature-resistant temporary carrier substrates 13 (see, e.g., Fig. 18 ), such as, e.g., silicon wafers, can be used. These carrier substrates 13 can, in turn, be equipped with suction hole channels that are aligned with the holes in the glass substrate. Alignment can be achieved by placement, by passive alignment aids (e.g., pins, balls), or by previously performed anodic bonding. The carrier substrate can be discarded after filling or can be provided with a non-stick coating for reuse. According to one embodiment, the filling can also be carried out with a low-melting aluminum-copper alloy in the manufacturing method 100. This alloy can be introduced as a pre-alloyed foil or formed in situ from (at least) one aluminum foil and (at least) one copper foil by forming an aluminum-copper eutectic during the warm-up phase of the pressure stamp 32. The process temperature can be reduced by approximately 100 K (compared to pure aluminum), thereby enabling the filling of low-melting substrates 12, e.g., glass substrates, without deformation. The method 100 can be carried out, for example, in a process chamber with a predetermined (e.g., inert) process atmosphere and a predetermined atmospheric process pressure. Fig. 2b now shows an exemplary basic flow diagram of the method 100 according to the invention for producing an electrically conductive channel structure 12-2 in a substrate 12, wherein, for example, an enclosing ring seal is used as the compressible sealing element 16. In the further exemplary embodiment of the flow diagram of the manufacturing method 100 shown in the following Fig. 2b, the method steps shown in Figs. 1 and 2a are again carried out, with the additions and changes (differences) compared to the previously described manufacturing method 100 being presented below. With the exception of the shape of the compressible sealing element 16 as an enclosing ring seal, the above statements regarding the manufacturing method 100 in Figs. 1 and 2a are equally applicable to the exemplary embodiment of the manufacturing method 100 shown in Fig. 2b. This also applies (in particular) to the materials of the compressible sealing element 16, the process sequence, the process parameters, all other described elements and their properties, etc. According to the embodiment of Fig. 2b, the compressible sealing element 16 comprises, for example, an enclosing ring seal. The compressible sealing element 16 can also be designed for high-temperature applications at the process temperature (as a compressible high-temperature sealing element). Fig. 2b thus shows a possible implementation of the various method steps of the schematic flow diagram of the manufacturing method 100 illustrated with reference to Fig. 1. The arrangement obtained in the manufacturing method 100, i.e. a substrate with electrically conductive channel structures or vias, can then be used, for example, as a so-called interposer arrangement 50 for electronic components, such as as rewiring (rerouting interposer), as a conductive via, as a (passive) electrical component or for heat dissipation, etc. Referring to the method 100 of Fig. 2b, at step 120, a stack assembly 10 is provided in a clamping device 30 (clamping assembly), wherein the stack assembly 10 comprises a substrate 12 provided with a channel structure 12-1, a metal foil 14 comprising an aluminum material or an aluminum material alloy on the substrate 12, and a compressible ring sealing element 16 surrounding the edge region of the metal foil and laterally enclosing the metal foil under pressure. According to the embodiment of the manufacturing method 100 shown in Fig. 2b, the clamping device 30 can have a first and a second tool 32, 34, wherein the stacking arrangement 10 is arranged or clamped (flush) between the first and second tools 32, 34 of the stacking arrangement 30. In a (subsequent) step 140, a surface-acting mechanical process pressure FP and a process temperature TP are now applied to the stack arrangement 10 with (by means of) the clamping device 30 in order to melt (liquefy) the metal foil 14 comprising the aluminum material at the process temperature TP and to introduce it into the channel structure(s) 12-1 as metallic filler material 14-1 by means of the surface-acting mechanical process pressure FP. In step 140, for example, the liquefied material 14-1 of the metal foil 14 is enclosed between a first tool (e.g., press die) of the clamping device and the substrate provided with the channel structures, wherein a compressible ring sealing element (= an enclosing ring seal) surrounds (encloses) the edge region of the metal foil, so that the ring sealing element surrounds (hermetically or tightly encloses) the metal foil laterally (between the substrate and the first tool) under pressure. This prevents lateral leakage (escape) of the liquefied / molten material of the metal foil through the surrounding ring sealing element. The annular sealing element 16 can have an inner peripheral shape (ring shape) that is adapted, for example, to the outer peripheral shape of the metal foil 14. The inner peripheral shape of the annular sealing element 16 can, for example, have a configuration that is flush or conforms to the outer region (the outer peripheral shape) of the metal foil 14. In a subsequent step 160, the stack arrangement 10 is cooled in order to resolidify (solidify) the introduced metallic (molten) filler material 14-1 in order to obtain the electrically conductive channel structure(s) 12-2 filled with the (solidified) metallic filler material 14-1. In the manufacturing method 100 illustrated by way of example in Fig. 2b, an aluminum pressure melt filling of the channel structures 12-1 in the substrate 12 is carried out. The (second) tool 34 of the clamping device 30 arranged on the substrate 12 serves, for example, as a counter substrate to obtain a flow stop (or a flow stop function) during the melt filling process, wherein the compressible high-temperature seal 16 is provided as a lateral boundary or enclosure to cause the liquefied (molten) material 14-1 of the metal foil 14 to emerge or escape laterally on the side of the substrate 12 adjacent to the first tool 32 of the clamping device 30. According to one embodiment, the step of exerting 140 mechanical pressure FP between the first and second tools 32, 34 of the clamping device 30 can be carried out with a contact pressure (between the first and second tools 32, 34) of greater than 10 N / cm2 or in a range between 10 N / cm2 and 600 N / cm2. According to one embodiment, the first or second tool 32, 34, or both tools 32, 34 of the clamping device 30 can be configured to heat the (clamped) stack assembly 10 to the (elevated) process temperature TP. This process can also be referred to as tempering. In the context of the present description, tempering (applying the process temperature) is understood to mean a temperature treatment, for example, a time-controlled, homogeneous heating of the stack assembly, wherein this temperature treatment is applied, for example, during the application of the planar mechanical pressure FP between the first and second tools 32, 34 of the clamping device 30. The step 140 of applying a process temperature TP to the stack assembly 10 can be performed, for example, with a predetermined temperature profile (or temperature ramp). The application 140 of the process temperature TP (peak temperature) to the stack assembly 10 can be performed, for example (depending on the material of the metal foil 14) for 1 to 30 (e.g., 3 to 15 or 3 to 5) seconds. The heating of the stack assembly 10 and the application of the process temperature TP (peak temperature) to the stack assembly 10 can, for example, be carried out independently of any additional alloying, provided this has already been provided. The production of an AlCu melt can take place during the heating process and does not significantly prolong the process. The prolongation can be in the range of 15 to 20 seconds. As shown by way of example in step 120 of Fig. 2b, the stack arrangement 10 comprises, in the vertical direction (from top to bottom in Fig. 2b), the metal foil 14 with the laterally surrounding annular sealing element 16 (high-temperature seal) and the substrate 12 provided with the channel structure(s) 12-1, e.g., a perforated glass-quartz, sapphire, ceramic, or semiconductor substrate (wafer). In the exemplary embodiment of the manufacturing method 100 shown in Fig. 2b, the first tool 32 is designed, for example, as a press die, and the second tool 34 of the clamping device 30 is designed as a (e.g., coated) counter substrate, wherein the second tool 34 also acts as a flow stop for the liquefied material 14-1 of the metal foil 14 during the filling process. With regard to the process sequence 100 shown in Fig. 2b, it is further noted that the stacking arrangement 10 may also have an inverted (reverse) sequence between the first and second tools 32, 34 of the clamping device 30 without the process result being (significantly) changed or impaired, since gravity effects (iW) have no influence on the filling process. By applying the surface-acting mechanical process pressure FP and the elevated process temperature TP (annealing process) with the liquefaction (melting) of the material of the metal foil 14, which comprises an aluminum material, the channel structure(s) 12-1 of the substrate 12 are pressurized. During compression (during the surface-acting mechanical pressure application) of the compressible ring sealing element 16, the metal foil 14 is laterally surrounded or enclosed by the directional sealing element 16. Due to the flow-stopping effect of the counter-substrate or the surface 34-1 of the counter-substrate 34, the filling process in step 140 proceeds up to the surface 34-1 of the second tool 34 of the clamping device 30, which acts as the counter-substrate. According to one embodiment, a main surface region 34-1 of the second tool 34 (the counter substrate) facing the substrate 12 can have a surface roughness with a mean roughness Ra or an average roughness depth RZ of between 0.5 µm and 10 µm or of approximately 3 µm. This surface quality (the roughness) of the main surface region 34-1 of the second tool 34 facing the substrate 12 prevents, on the one hand, adhesion of the molten metal (molten aluminum) to this main surface region 34-1 of the second tool 34 during the pressure filling process and, furthermore, prevents adhesion of the hot substrate 12 (e.g., the glass substrate), which is at the process temperature TP, to this main surface region 34-1 of the second tool 34. According to one embodiment, the main surface region 34-1 of the second tool 34 facing the substrate 12 can have a coating 36 to provide this surface roughness of the main surface region 34-1 of the second tool 34 facing the substrate 12. Thus, the surface texture of the main surface region 34-1 of the second tool 34 facing the substrate 12 can be obtained, for example, by means of the coating 36, wherein the coating 36 can comprise or consist of a boron nitride material. The boron nitride (BN) does not react with the liquefied material (aluminum material) 14-1 of the metal foil 14, since boron nitride is oxidation-resistant up to approximately 800°C and does not react with glass or metal. Furthermore, BN does not adhere to glass, nor does the hot glass mass adhere to the BN. Furthermore, the boron nitride material can achieve the desired surface roughness of the second tool 34, whereby during the filling process it can also be achieved that air / gas can escape laterally from the channel structures 12-1 of the substrate 12, while the surface texture has or provides the desired flow-stopping effect for the molten metal 14-1 on the surface 34-1 of the counter-substrate 34 (second tool). As further illustrated by way of example in Fig. 2b of the manufacturing method 100, the first tool 32 (the press ram) can further have a non-stick coating 38 on its main surface region 32-1 (facing the substrate 12), which enables simplified detachment (removal) of the first tool 32 from the stacking arrangement 10, i.e., from the compressible sealing element 16, after the filling and cooling process 140, 160 of the method 100. The non-stick coating 36 can, for example, be arranged on (or form) the main surface region 32-1 of the first tool 32 facing the stacking arrangement 10. According to one embodiment, the coating 36 of the second tool 34 may comprise a boron nitride material, wherein the surface roughness of the main surface region of the second tool 34 adjacent to the substrate 12 is selected to act as a flow stop for the molten metal and to enable lateral escape of a gas present in the channel structure 12-1 of the substrate 12. Thus, the flow front of the molten material 14-1 of the metal foil 14 can impact a plate 34 (second tool 34) located beneath the substrate 12, which plate is provided with the rough boron nitride coating. The flow front pushes the gas in the channel downwards and stops flat on the substrate 12. The gap formed by the coating roughness is so narrow that the flow front cannot move further laterally between the substrate 12 (e.g. glass substrate) and the second tool (counter substrate plate) 34.In this procedure, a protective gas atmosphere is helpful / possible, but not absolutely necessary. This allows for sufficient control of the flow front. According to one embodiment, the substrate 12 may comprise, for example, a dielectric material, such as glass, quartz, sapphire, ceramic, etc., or a semiconductor material, e.g., silicon (polysilicon). When using silicon (polysilicon) for the substrate 12, it may be necessary, for example, to provide an additional barrier and insulation layer, e.g., made of SiO2, to prevent a possible reaction of the hot liquid aluminum material with the silicon. The step 160 of cooling the stack arrangement 10 can, for example, be carried out with a predetermined temperature profile (or temperature ramp, as in the step of applying the process temperature) in order to ensure, for example, that the cooling of the elements and structures involved is carried out in the most material-friendly manner possible due to different thermal expansion coefficients. The cooling process 160 can, for example, be carried out with an (average) temperature change (cooling) of 20 to 500 K (or 30 to 400 K or 300 to 400 K) per minute (until a normal temperature is reached (e.g., removal temperature of the filled substrate 12, e.g., in a range between the ambient temperature and approximately 200°C). The required time for the cooling process can depend, for example, on the structure of the clamping device 30 and, e.g., the stamping unit 32. After step 160 of cooling the stack assembly 10 and the clamping device 30, after the release of the surface-acting mechanical process pressure FP, the stack assembly 10 can be removed from the clamping device 30, wherein the ring sealing element 16 can then also be removed from the substrate 12. After removing the substrate 12 (e.g., glass substrate) equipped, for example, with the aluminum feedthroughs (e.g., aluminum TGVs) 12-2 and the relaxed seal (ring sealing element) 16, the substrate 12 provided, for example, with the electrically conductive channel structure(s) 12-2 can now be fed to further processing steps. Thus, in the method 100, excess metallic filler material 14-2 can further (optionally) be removed on one side of a main surface area or on both sides of both opposite main surface areas of the substrate 12, e.g. by means of a CMP process (CMP = chemical mechanical polishing). Furthermore, in the method 100 (optionally), a one-sided or two-sided metallization can be carried out on the substrate 12 by means of a thin-film deposition process in order to obtain, for example, via a lithographic structuring process and a subsequent etching step, a metallization structure electrically connected to the conductive channel structure 12-2 on one or both main surface regions of the substrate 12 formed with the conductive channel structure 12-2. The method 100 according to the invention for producing an electrically conductive channel structure 12-2 in the substrate 12 can thus be used to obtain, for example, an arrangement such as an interposer 50, which has channel structures 12-2 completely filled with metal in the substrate 12 (e.g., a flat substrate), wherein, for example, a chemical bonding zone (interface) of the metal filling 14-1 of the channel structures 12-2 to the channel walls is obtained without, for example, a metallic thin-film adhesion promoter coating being required or used in the method. With regard to the stacking arrangement 10 shown in Fig. 2b in the description of the manufacturing method 100, it should be noted that a plurality of such stacking arrangements 10 can also be arranged between the first and second tools 32, 34 of the clamping device 30 in order to carry out the manufacturing method 100 of Fig. 2b. It should only be noted that an additional intermediate layer can be used as the respective counter substrate 34 to provide the flow-stopping effect. According to one embodiment, the channel structure 12-1 can be formed as at least one through-hole structure, as at least one blind-hole structure or as at least one 3D structure in the substrate 12, so that after carrying out the method 100, an electrically conductive channel structure 12-2 is obtained in the substrate 12 in the form of a conductive through-hole structure, at least one conductive blind-hole structure or at least one conductive 3D structure in the substrate. According to one embodiment, the (elevated) process temperature TP can be set to a value of at least 5 K, 10 K, or 20 K above the melting temperature of the metal foil 14 comprising the aluminum material. The process temperature TP is thus selected to ensure reliable melting of the material of the metal foil 14 with the lowest possible thermal stress on the elements and structures involved. For this purpose, the first or second tool 32, 34, or both tools 32, 34, can be configured to heat the stack arrangement 10 to the desired process temperature TP, i.e., to perform the tempering process at the desired process temperature TP. During the melt filling of the channel structures 12-1 of the substrate 12 defined according to method 100, the process temperature is therefore at least 5 K, 10 K, or 20 K higher than the melting temperature of the metal of the metal foil 14 selected for the filling. The process temperature is, for example, upper limited by the softening temperature of the substrate material. If, for example, glass is used as the substrate material, its viscosity decreases with increasing temperature (e.g., continuously), whereby glass is an amorphous inorganic material. By means of a supporting carrier material 13 (see, for example, Fig. 20) with a high melting temperature or softening temperature, e.g., silicon, even low-melting glass substrates 12 can be filled with aluminum or an aluminum alloy without bending or structural changes to such a glass substrate 12 occurring. According to one embodiment, the metal foil 14 can comprise the aluminum material as its main component, e.g., with a proportion of ≥ 80%, 90%, or 95%, or even pure aluminum (= 100% proportion), for a resulting melting point of at least 420°C or 520°C, or between 420°C (or 520°C) and 850°C. Thus, the material of the metal foil is a brazing material, since the brazing temperature, by definition, is above 420°C or even above 520°C. By adjusting the melting temperature and the "over" temperature above it (process temperature = melting temperature + 5 / 10 / 20 K), the wettability of a pure aluminum melt (without ambient oxygen) in the hole structures 12-1 can be improved by reducing the surface tension of the metal melt 14-1 by approximately 5% (e.g., filling temperature approximately 830 °C), while the density of the melt 14-1 and the viscosity are little affected. In aluminum-copper alloys for the metal foil 14, this effect is pronounced and dependent on the copper content. Since higher alloying proportions (of copper) can increase strength and generally also lead to significantly increased volume resistances, the metal material of the metal foil contains aluminum as its main component, e.g., at least 80%, 90%, 95%, or 99%.While the density, surface tension and viscosity of pure aluminum depend little on temperature, there is a significant effect on aluminum-copper alloys, at least for the viscosity. The metal foil 14, which comprises the aluminum material (as the main component), can have a single-layer or multi-layer foil structure. Thus, the metal foil 14 can comprise a single-layer aluminum material, a two-layer composite comprising an aluminum layer and a copper layer (or foil in each case), a three-layer composite comprising an aluminum layer, a copper layer, and another aluminum layer, etc., as long as the aluminum material represents the main component of the multi-layer foil structure (and rests on the substrate 12). As glass materials for the substrate (glass substrate) 12, for example, a Borofloat® glass (Borofloat 33 from Schott) or another glass, such as Schott AF32, Corning Eagle XG, Hoya SD2, can be used. According to one embodiment, the annular sealing element 16 can laterally enclose (surround) the metal foil 14 or the edge region in order to laterally enclose the metal foil 14 when the mechanical process pressure FP and the process temperature TP are applied and to prevent the liquefied / molten material of the metal foil from lateral leakage (escape) through the surrounding annular sealing element. According to one embodiment, the compressible sealing element 16 can be designed as a reusable high-temperature seal. According to a further embodiment, the annular sealing element 16 may comprise or consist of a structured foil, e.g., a structured graphite foil, with a thickness (vertical height) in a range from 0.3 mm to 1 mm or approximately 0.5 mm. The (lateral) width B of the annular sealing element 16 may be in a range from 0.5 mm to 20 mm or from 2 to 5 mm. In addition to graphite, other materials that do not adhere to the liquid aluminum material, such as other carbons, SiC, or BN, can be considered as materials for the compressible surface sealing element 16. For example, fabrics made of / with graphite, SiC, and / or BN fibers (each individually or in combination) can also be used. By applying a compressible high-temperature ring seal (e.g., a structured graphite foil) 16 laterally around the applied metal foil (e.g., aluminum or aluminum alloy foil), the molten metal (the molten material 14-1 of the metal foil 14) can be held above the substrate area to be filled (with the channel structures 12-1) of the substrate 12 during the step of applying a surface-acting mechanical process pressure FP and the process temperature TP, and lateral squeezing (escape) under pressure FP can be prevented. By using the compressible ring seal element 16, very high yields can be achieved in the manufacturing method 100. In the context of the present description of method 100, filling or the filling process refers to the introduction of molten metal 14-1 for the complete or partial filling of cavities or channel structures 12-1 in a substrate 12, e.g., a ceramic, glass, or silicon substrate. Filling can also be understood as an inner wall lining of cavities or channel structures 12-1 in the substrate 12 with a metal coating or a filling limited to the depth of the channel structure 12-1. A substrate 12 is understood, for example, to be a material body having two opposite parallel main surface areas (sides), regardless of the width-to-height ratio. The opposite sides of the substrate 12 can, but do not have to, be arranged parallel to each other, and may also be arranged non-parallel to each other in some areas. In the context of the present description, a channel, channel structure or cavity 12-1 is referred to as a recess with at least one open side (opening) to an outer side of the substrate 12, whereby this is independent of the geometric shape of the recess 12-1, e.g. in the form of a lateral slot, a pocket, a blind hole or a through-hole, or a channel in any geometric design with at least one opening to a substrate surface. Although reference is often made in the present description to an aluminum filling (based on the metal foil comprising an aluminum material), the method according to the invention can also be applied to filling with ultrapure aluminum or aluminum alloys. For example, alloys with a reduced melting point in relation to ultrapure aluminum can be used, wherein one or more alloying elements from the areas of copper, silicon, germanium and / or magnesium can be used. Furthermore, alloys or aluminum alloys with improved electrical properties, e.g. against electromigration, such as Al-Si or AlCu (each a few % share, e.g. 1 to 5 % share) can be used. This list of alloying elements is only to be regarded as exemplary and not exhaustive. Furthermore, it should be noted that the term foil in "metal foil, aluminum foil, aluminum alloy foil" 14 in the context of the present description includes the use of stacked individual foils but also thin metal sheets or roll-clad sheets, e.g., made of aluminum-copper, from which alloys are formed, for example, during the filling process and (at least partially) fill the channel structures or perforations 12-1 of the substrate 12. Typical thicknesses of metal foils and metal sheets can range from 20 µm to 1000 µm, or between 20 µm and 50 µm, and approximately (typically) 30 µm. According to embodiments, the metal foil comprises the aluminum material as the main component with a volume fraction of >60%, >80%, or even >90%. Furthermore, the manufacturing method 100 according to the invention enables the electrically conductive channel structures 12-2 in the substrate 12 to fill a metal filling 14-1 to a degree of 90% or even between 95% and 98% and up to 100%, i.e., the channel structure 12-2 is completely filled (i.e., at least 90% or 98%), free of pores or inclusions. According to one embodiment, for example, for the purely aluminum melt filling of channel structures 12-1 in low-melting glass substrates 12, e.g., Schott BF33, temperature-resistant temporary carrier substrates 13 (see, e.g., Fig. 18 ), such as, e.g., silicon wafers, can be used. These carrier substrates 13 can, in turn, be equipped with suction hole channels that are aligned with the holes in the glass substrate. Alignment can be achieved by placement, by passive alignment aids (e.g., pins, balls), or by previously performed anodic bonding. The carrier substrate can be discarded after filling or can be provided with a non-stick coating for reuse. According to one embodiment, the filling can also be carried out with a low-melting aluminum-copper alloy in the manufacturing method 100. This alloy can be introduced as a pre-alloyed foil or formed in situ from (at least) one aluminum foil and (at least) one copper foil by forming an aluminum-copper eutectic during the warm-up phase of the pressure stamp 32. The process temperature can be reduced by approximately 100 K (compared to pure aluminum), thereby enabling the filling of low-melting substrates 12, e.g., glass substrates, without deformation. The method 100 can be carried out, for example, in a process chamber with a predetermined (e.g., inert) process atmosphere and a predetermined atmospheric process pressure. The surface sealing element described in connection with Fig. 2a and the ring sealing element described in connection with Fig. 2b can easily be provided and / or used as independent structures. However, embodiments of the present invention provide for the two structures, i.e., the surface sealing element and the ring sealing element, to be used together. The joint use can be carried out as the use of both independent or individual structures. Alternatively, it is possible to firmly connect the surface sealing element and the ring sealing element to one another, for example by means of an adhesive or bonding process, and to use the connected structure. As a further advantageous alternative, it is provided for the surface sealing element and the ring sealing element to be provided together as a one-piece or integral component and / or to be used as such. Fig. 3a shows exemplary Al-TGVs (aluminum through-glass vias) in the substrate 12 (e.g., in glass or quartz glass) produced using the manufacturing method of Fig. 1 or Fig. 2. Fig. 3b shows, by way of example, a detailed representation of the interface connection 11 between the conductive Al filling 12-2 (of the Al-TGV) and glass 12 (e.g., borosilicate glass), which were produced using the manufacturing method 100 for high-pressure melt filling according to that shown in Fig. 1 and Fig. 2. As can be seen from Fig. 3a, aluminum acts as its own adhesion promoter to glass-quartz, ceramic or sapphire substrates 12. Since an additional adhesion promoter layer can be omitted, Al vias can not only be produced much more easily according to the manufacturing method according to the invention, but it is also possible to fill true 3D structures, as is also shown by way of example in Fig. 9b. In this context, it should be noted that aluminum acts as its own adhesion promoter to glass, quartz, ceramic, or sapphire substrates, as shown by way of example in Fig. 3b. Bonding to silicon and oxidized silicon substrates is also possible. The provision of an additional adhesion promoter layer can therefore be omitted or is no longer necessary, which not only makes the aluminum via (Al via) significantly easier to manufacture compared to conventional manufacturing processes, but also makes the filling of true 3D structures possible. Sidewall wetting or bonding can optionally be improved by dielectric coatings. Conformal deposition (ALD = atomic layer deposition) or LP-CVD (LP-CVD = low-pressure chemical vapor deposition) technology is particularly suitable for this purpose. Suitable dielectric layer materials include aluminum nitride (AIN), aluminum oxide (Al2O3), silicon nitride (SiN), titanium nitride (TiN), etc., e.g., with a thickness in the range of 5 to 100 nm or 30 to 50 nm. These dielectric layer materials can improve the filling of the openings and allow filling at lower pressures. These layers can also act as additional barrier layers and can help prevent unwanted reactions between the glass and the metallization. The focus here is not (necessarily) on the aluminum material, but (especially) on additives (alloys), such as copper. For example, copper can release monovalent ions that diffuse into the glass and can impair, for example, the insulating properties or transparency of the glass. The aluminum wettability of the channel structure can be favorably influenced by a pre-coating with SiN, AlN, TiN, etc., using an LP-CVD or ALD process. The layer thicknesses range from 5 nm to 100 nm, or (preferably) from 30 to 50 nm. The (conformal) pre-coating can be used either to fill smaller via diameters (in a range of 5 to 15 µm) at the same process temperature and pressure, or, in particular, to reduce the necessary pressure for larger via diameters. Fig. 4a-b now shows an example of an Al-Cu melt filling 14-1 in the channel structure 12-2 in a substrate 12 (e.g., a quartz substrate), which was produced using the manufacturing method 100 of Fig. 1 or Fig. 2 according to an exemplary embodiment. In the example of an Al-Cu melt filling 14-1 in a quartz substrate 12 shown in Fig. 4ab, an Al-Cu roll-clad sheet is used, for example. The aluminum material forms an adhesive coating to the substrate 12, while copper phases are present in the volume body. The alloy is completely formed when the aluminum layer is melted by reaction with the copper layer. The aluminum side of the roll cladding 14 is placed on the substrate 12 facing the (glass) substrate 12. According to one embodiment, the use of ultrapure aluminum (4 N, 5 N, or 6 N) can be considered for applications (e.g., a cryogenically compatible arrangement of microelectrical components for quantum computer applications, e.g., at temperatures below 10 K) that require particularly low volume resistances of the electrically conductive feedthroughs 12-2 through the substrate 12. The electron noise when passing through grain boundaries can be reduced by additional annealing of the substrate 12 (e.g., glass substrate) with the TGVs 12-2. A grain structure as coarse as possible in the TGVs 12-2, with grain diameters in the range of the channel diameters of the channel structures 12-1 or larger, is desirable for the lowest possible volume resistances and low electron noise. This annealing (additional annealing) is carried out, for example, at temperatures in the range of 250 °C to 500 °C in a furnace.A further improvement in the electrical properties of already manufactured TGVs can be achieved by directional solidification of the microstructure, which can produce a columnar grain structure (of TGVs 12-2). In this context, reference is made to Figs. 5a-c, for example, which show an exemplary procedure. In the exemplary procedure illustrated in Figs. 5a-c, the channel structure 12-1 in the substrate 12 is first filled with aluminum (according to method 100). As illustrated in Fig. 5b, an Al recrystallization is performed during further annealing in order to obtain a directional solidification of the Al microstructure 14-1 in the (filled) via 12-2. As illustrated by way of example in Fig. 5c, a thinning of the substrate can be performed in order to emphasize the columnar grain structure in the via 12-2, after which, for example, a metallization 12-3 and passivation 12-4 of contact pads can be performed. This allows a concept of recrystallization by an imposed temperature gradient to generate columnar grain structures of the TGVs produced using method 100 to be obtained. With reference to Fig. 5d, a further exemplary procedure for obtaining improved electrical properties of the vias (Al-TGVs) 12-2 according to a further embodiment is explained by way of example. According to one embodiment, particularly low volume resistances of the electrically conductive feedthroughs 12-2 through the substrate 12 can be achieved, for example, using ultrapure aluminum (4 N, 5 N, or 6 N). As shown by way of example in Fig. 5d, a single-crystal (monocrystalline) via filling 14-1 can be achieved (in situ), however, with different orientations in the vias 12-2, i.e., there are no grain boundaries in the metal material of the vias 12-2. Thus, the electron noise that arises when passing through grain boundaries can be avoided or at least greatly reduced with the single-crystal vias 12-2. This single-crystal via filling 14-1 of the vias 12-2 can be achieved, for example, by using high-purity aluminum (Al content > 98%) or ultrapure aluminum (Al content = 100%) in the pressure filling method 100. Furthermore, the application 140 of the process temperature TP (peak temperature) to the stack arrangement 10 can be carried out, for example, for a (relatively long) time of 5 to 40 seconds or 10 to 30 seconds. Furthermore, the cooling process 160 can be carried out, for example, with a relatively low (average) temperature change (cooling) of 20 to 300 K (or 30 to 200 K) per minute (until a normal temperature of, for example, 290 K to 300 K is reached) (Ostwald ripening). The manufacturing method 100 according to the invention for producing an electrically conductive channel structure 12-2 in a substrate 12 opens up many new application possibilities that are (by far) not limited to the field of radio frequency technology or quantum technology. Compared to previous processes in microtechnology, which implement 2.5D technology (extension of 2D structures into the depth), the inventive procedure, e.g. using SLE processes (SLE = Selective Laser-induced Etching), enables new possibilities for the production of 3D-shaped microstructures or channel structures. The inventive manufacturing method 100 for producing an electrically conductive channel structure 12-2 in a substrate 12 based on the aluminum melt filling of hole and blind hole structures 12-1 in substrates 12, e.g., glass and oxidized silicon substrates, is not limited to (very) specific processing methods for producing the hole structures. Thus, for applications in microelectronics, structuring methods with very high aspect ratios in substrates 12 (e.g., glass substrates), in particular with a thermomechanical expansion coefficient largely adapted to silicon, are of interest. The term glass substrate is understood here to mean technical glasses and IR-transparent ceramics (e.g., in the range around 1 µm wavelength - for laser-induced etching) with a low thermal expansion coefficient of 0 ppm / K < CTE < 6 ppm / K (CTE = Coefficient of Thermal Expansion) (e.g.,Sapphire, AlN, Si3N4, SiC, glass ceramic) to synthetically produced quartz glass (fused silica) with an expansion coefficient of approximately 0.1 ppm / K. A ceramic substrate, for example, can be provided with holes that can also be filled according to the procedure described. Filling hole structures 12-1 is also possible in silicon (in a silicon substrate 12) with and without surface oxidation, e.g., for the production of electrical feedthroughs and heat dissipation vias. In silicon, a barrier can separate the silicon and the hot aluminum. The barrier can be SiO2 or comprise SiO2, although deposited layers, such as Si3N4, are also suitable for this purpose. The substrates 12 (e.g., glass, silicon substrates, etc.) are used, for example, in wafer form with plane-parallel top and bottom surfaces. However, flat (glass) substrates with other dimensions can also be used, for example, to produce metamaterials with specifically adjusted reflection or transmission properties for high-frequency electromagnetic radiation (5G, 6G, radar, THz). Metamaterials are artificially produced materials with optical, electrical, or magnetic properties that do not occur naturally. Possible methods with high detail resolution for hole creation rely, for example, on laser exposure (usually fs to ns pulse duration) to locally increase the glass etching rate and subsequent etching either in KOH, NaOH solution, or in hydrofluoric acid (HF). Other wet-chemical etching methods are conceivable. The various laser processing methods and the different etching properties of the glasses, depending on their chemical composition, also produce different hole geometries, particularly when considering the degree of freedom of double-sided or single-sided etching. The formation of the channel structures 12-1 and wall angles depends on the substrate material, e.g., the glass material, the laser focal resolution, the exposure strategy, the etching chemistry used, the etching time, etc. Fig. 6a-i now show exemplary geometries of channel structures with different dimensions and wall angles for filling with the inventive manufacturing method 100 according to Fig. 1 or Fig. 2. As shown in Fig. 6a, for example, a quartz substrate 12 is etched on both sides using LIDE (Laser Induced Deep Etching) with a structured additional protective mask to obtain both the through-hole geometries 12-1 and the blind-hole geometries 12-1. The protective mask has opposing openings on both sides to obtain the through-hole geometries and only a single-sided opening to obtain the blind-hole geometry of the channel structures 12-1. Fig. 6b shows an example of the substrate 12, e.g. a quartz substrate, which was etched on one side using LIDE, for example, in order to obtain the channel structures 12-1 with blind hole geometry. As shown in Fig. 6c, the substrate 12, e.g. a quartz substrate, can be etched through on one side by means of LIDE in order to obtain the through-hole geometries of the channel structures 12-1. As shown in Fig. 6d, the substrate 12, e.g. a quartz substrate, can be etched on both sides by LIDE in order to obtain the through-hole geometries of the channel structures 12-1. As shown by way of example in Fig. 6e, the substrate 12, e.g. a quartz substrate, can be etched on both sides by means of SLE (SLE = Selective Laser-Induced Etching) in order to obtain different hole geometries (blind hole depths) of the channel structures 12-1. As shown by way of example in Fig. 6f, the substrate 12, e.g., a quartz substrate, can be etched on both sides using SLE to obtain different hole geometries (hole diameters) of the channel structures 12-1. Furthermore, for example, a flow stop for the liquefied metal material 14-1 is created by the constricted hole geometry (constriction) 23. Fig. 6g shows, for example, the substrate 12, e.g., a quartz substrate, which has been etched on both sides using SLE to obtain different hole geometries, ie, different hole diameters of the channel structures 12-1 at different substrate depths. Furthermore, a flow stop for the liquefied metal material 14-1 is created, for example, by the constricted hole geometry (constriction) 23. Fig. 6h shows the substrate 12, e.g. a glass substrate (e.g. Schott AfF2 eco), in which the hole geometries of the channel structures 12-1 were etched on one side using LIDE. Fig. 6i shows the substrate 12, e.g., a glass substrate 12 (e.g., Schott Af32 eco), in which the hole geometries of the channel structures 12-1 were etched on both sides using LIDE (continuous hole geometries). Furthermore, a flow stop for the liquefied metal material 14-1 is created, for example, by the constricted hole geometry (constriction) 23. In summary, it can be stated that the substrates 12 shown in Fig. 6a-i have different hole geometries and flank angles of the channel structures 12-1. Fig. 7 now shows a schematic representation of further possible topologies of the substrate 12 for use in the manufacturing method according to the invention of Fig. 1 or Fig. 2 . For example, during an etching process on substrate 12 to obtain the channel structures 12-1, structured protective masks (e.g., patterned by photolithography) can be used on one or both sides. These masks limit or prevent the etching attack on certain substrate areas and enable / allow access to other areas. This allows, for example, raised areas to be created on substrate 12 or areas to be deep etched after other areas, e.g., after further processing of the wafers, downstream in the manufacturing process. For example, surface region 12-A of substrate 12 has no etching. Surface region 12-B of substrate 12 has, for example, an etched surface without laser exposure. Surface region 12-C of substrate 12 has, for example, an etched pocket depression. Surface region 12-B of substrate 12 has, for example, a circumferential frame elevation. In Figs. 8-12, exemplary embodiments of an interposer arrangement 50 or a part of the interposer arrangement 50 are now described, which can be obtained with the manufacturing method 100, 100-1 - 100-8 according to the invention. The interposer assembly 50 includes a substrate 12 having an electrically and / or thermally conductive channel structure 12-2 extending at least partially through the substrate 12, wherein the channel structure 12-2 comprises an aluminum material or an aluminum material alloy, and wherein the electrically and / or thermally conductive channel structure 12-2 extends from a main surface area of the substrate 12 into the substrate 12. The aluminum material or aluminum material alloy has at least 80% or 90% aluminum as its main component in order to have a resulting melting point of at least 420°C (or 520°C) or between 420°C (or 520°C) and 850°C as a brazing solder. According to an example of the interposer arrangement 50 (see Figs. 8a-d), the conductive channel structure 12-2 extends from one main surface area of the substrate 12 into the substrate 12 and to the opposite main surface area of the substrate 12. According to an example of the interposer arrangement 50 (see Fig. 8b and d), the conductive channel structure 12-2 does not extend, at least in sections, in a direction vertical to the two opposite main surface regions of the substrate. According to an example of the interposer arrangement 50 (see Fig. 8a-c and e), the conductive channel structure 12-2 extends vertically to the two opposite main surface areas of the substrate 12. According to an example of the interposer arrangement 50 (see Fig. 8a-e), the electrically and / or thermally conductive channel structure 12-2 is formed as at least one thermal connection made of aluminum for heat dissipation through the substrate 12 (between the first and second, opposite main surface region). According to an example of the interposer arrangement 50 (see Fig. 8a-e), the conductive channel structure 12-2 is formed as at least one electrical via through the substrate 12 and / or as at least one passive component in the substrate 12. According to an example of the interposer arrangement 50 (see Fig. 8a-e), the at least one via 12-2 through the substrate 12 has an aspect ratio of 50:1 (length to diameter). An interposer or interposer assembly 50, for example, refers to an electrical interface that connects a socket or interconnect level to another interconnect level. The purpose of an interposer is therefore, for example, to distribute an interconnect level across a larger interconnect field or to redirect an interconnect level to another, different interconnect level. Thus, Fig. 8a-e show schematic representations of exemplary interposer arrangements 50 (with further possible substrate topologies) according to further examples, which can be obtained, for example, with the inventive manufacturing method 100 of Fig. 1 or Fig. 2. Fig. 8a-e show various topographies and hole geometries for the interposer arrangement 50, which can be produced by SLE and LIDE laser exposure and subsequent single-sided or double-sided etching in the substrates 12, e.g., glass substrates. Local etch protection allows protected areas to be etched subsequently, e.g., after metallization or via filling. For example, recessed surface recesses 12-1, blind holes 12-1, channel structures 12-1, and open through-holes 12-1 can be introduced into substrates 12 that are otherwise already metallized on one or both sides by protecting the metallizations 12-2 from etching attack with protective masks. Figs. 8a-e show filled vias (fully or partially through-hole openings) in various possible geometries. A via channel 12-2 can also start and end on the same side of the substrate 12. A via channel 12-2 can also split and start or end with a different number of arms between the first and second, opposite main surface areas of the substrate 12 (see Fig. 8d). Fig. 9a now shows an exemplary 3D channel structure 12-2 (e.g., a 3D coil) in the substrate 12, which can be manufactured, for example, using the inventive manufacturing method 100 of Fig. 1 or Fig. 2. As shown in Fig. 9a, the electrical contacts 12-3 can be arranged on the same main surface side of the substrate 12. Fig. 9b shows an enlarged 3D X-ray tomography image of the 3D coil of Fig. 9a. The 3D coil 12-1 can be manufactured, for example, using the manufacturing method 100 of Fig. 1 or Fig. 2 in the substrate 12, e.g., a glass substrate. Fig. 9b shows the channel structure 12-2 produced in quartz or glass by the SLE method with the aluminum pressure filling (via the filling openings 15) according to the method 100 of Fig. 1 or Fig. 2 as a 3D X-ray tomography image. Fig. 10 now shows an exemplary perspective view (3D view) of a component in the form of a metal-filled coil 12-2 in a substrate (e.g., glass substrate) 12, e.g., manufactured using the manufacturing method 100 of Fig. 1 or Fig. 2. As shown in Fig. 10, the electrical contacts 12-3 can be arranged on the same main surface side of the substrate 12. The metal-filled coil 12-2 in the substrate 12 can now, for example, be arranged around a channel 18 in the extension direction, wherein the channel 18 in the substrate 12 can be filled with a ferrite paste in order to generate a higher inductance of the coil (coil) 12-2. The coil (coil) 12-2 can, for example, also be designed to be flat in one plane and to be provided with a coil core. Fig. 11 now shows an exemplary perspective view of a component in the form of a thin-film getter structure 19 with via contact 12-2 through the substrate 12 and manufactured, for example, using the manufacturing method 100 of Fig. 1 or Fig. 2. As shown in Fig. 11, the thin-film getter structure 19 has a via contact 12-2 from the rear side, ie the electrical contacts 12-3 are arranged on the same main surface side of the substrate 12 in order to enable heating of the thin-film getter arrangement 19 (for getter activation) via the via contact 12-2. Fig. 12a-b now show an exemplary perspective view and an exemplary cross-sectional view of a component in the form of a capacitor structure manufactured using the manufacturing method 100 of Fig. 1-2. Using the manufacturing method 100, the capacitor arrangement 60 with opposing contact surfaces 12-3 and pin electrodes 12-2 can be manufactured. 13a-c now show exemplary cross-sectional views of packaged components 70, such as MEMS, sensors and / or ICs, with the Al vias 12-2, e.g. Al-TGVs, in the substrate 12 and manufactured, for example, using the manufacturing method 100 of Fig. 1 or Fig. 2, for electronic connection as electrical vias 12-2 and / or for thermal connection 12-2 (for heat dissipation) according to a further embodiment. As shown by way of example in Fig. 13a, the conductive channel structure 12-2 in the substrate 12 can be used for the mechanical and / or electrical connection of another substrate 13. Furthermore, through-openings 12-1 in the substrate 12 can be provided as fluidic, acoustic, etc. access and / or exit openings to a cavity 72 arranged between the two substrates 12, 13, containing an electrical and / or mechanical component 74. As shown in Fig. 13b, the conductive feedthroughs 12-2 can be provided in the substrate 12 for the electrical connection (rewiring) and / or for the thermal connection (for heat dissipation to a heat sink) of an electronic component 74, wherein the electronic component 74 is arranged in a cavity 72 arranged between the two substrates 12, 13 on the substrate 12. As shown in Fig. 13c, the conductive feedthroughs 12-2 can be provided in the substrate 12 for the electrical connection (rewiring) and / or for the thermal connection (for heat dissipation to a heat sink) of an optoelectronic component 74 (with a plurality of individual elements 74, 74', 74"), wherein the optoelectronic component 74 is arranged in a cavity 72 arranged between the two substrates 12, 13 on the substrate 12. In the arrangement of Fig. 13a-b, the electronic component 74 may comprise a mechanical component (MEMS component), while in Fig. 13c the arrangement may comprise an optoelectronic component (e.g. with a high heat dissipation). Fig. 14 now shows an exemplary, basic (schematic) flow diagram 200 for further processing (e.g., at wafer level) of the stack arrangement 10 obtained with the manufacturing method 100 of Fig. 1 or Fig. 2. As will be described in more detail below, in the method 200, excess metallic filler material 14-2 can further be removed on one side of a main surface region or on both sides of both opposite main surface regions of the substrate 12, for example by means of a CMP process (CMP = chemical mechanical polishing). Furthermore, in the method 200, a one-sided or two-sided metallization can be carried out on the substrate 12 by means of a thin-film deposition process in order to obtain, for example, via a lithographic structuring process and a subsequent etching step, a metallization structure 12-3 electrically connected to the conductive channel structure 12-2 on one or both main surface regions of the substrate 12 formed with the conductive channel structure 12-2. As shown in partial image 1 (step 210) of Fig. 14, the stack arrangement 10 processed / machined according to the method 100 of Fig. 1 or Fig. 2, ie the substrate 12 provided with the electrically conductive channel structure 12-2, forms the starting point for further processing (e.g., at wafer level) according to the method 200. The substrate 12 has, for example, a plurality of conductive channel structures 12-2 with a plurality of conductive feedthroughs and a plurality of blind holes (or passive components). The substrate (wafer) 12 thus comes from the Al filling process 100, wherein the substrate 12 has, for example, channel structures 12-2 filled with an AlGe solder material (solder), wherein all other options described above for the material composition of the metal foil 14 are equally applicable. The following exemplary process steps, as illustrated in the following partial images, can now be applied to obtain an interposer arrangement 50 (e.g., a glass interposer) with integrated passive components and / or active components, e.g., an RF transistor, as part of further wafer processing 200. This component combination is to be regarded merely as an example of the resulting interposer arrangement 50. As shown in sub-step 2 (step 220) of Fig. 14, conditioning or processing of the substrate top side (wafer top side) 12-A of the substrate 12 can be carried out using an etching or grinding and polishing process (CMP process). As shown in sub-step 3 (step 230) of Fig. 14, conditioning of the substrate underside (wafer underside) 12-B of the substrate 12 can further be carried out using an etching or grinding and polishing (CMP) process. As shown in sub-step 4 (step 240) of Fig. 14, processing of the substrate top side (wafer top side) 12-A of the substrate 12, optionally with structured metallizations 12-3 and optional passivation layers 12-4, can now be performed. The process flow can also utilize the substrate top side (wafer top side) 12-A of the substrate 12 in this step. As is now shown in sub-image 5 (step 250) of Fig. 14, the processing carried out in sub-image 4 (step 240) with the substrate top side 12-A can be carried out equally on the substrate bottom side (wafer bottom side) 12-B, optionally with resistance layers 12-5. Part 6a (step 260a) of Fig. 14 now shows an exemplary option in which a solder 17 is applied to corresponding contact pads 12-3 and the active component 74, e.g., a transistor, is mounted / attached. In the optional embodiment illustrated in Part 6a, a cover 76 can be bonded to the top side 12-A (wafer top side) of the substrate 12 (wafer) using a mold compound. Subsequently, the components / assemblies 74 can be separated (at the wafer level) (in step 270a). The separated assembly 74 is shown as an example in Figure 7a. As illustrated by way of example in sub-image 6b (step 260b) of Fig. 14, a solder 17 can be applied to the contact pads 12-3 on the second main surface 12-B of the substrate 12, wherein the (e.g., active) component 74, e.g., a transistor, is further mounted on corresponding contact pads 12-3. In the optional embodiment illustrated in sub-image 6b, a hermetic covering of the substrate top side (wafer top side) can be obtained by means of a further substrate 78 provided with cavities, e.g., a glass or silicon wafer. Subsequently (in step 270b) the components / assemblies 74 can again be separated, with partial image 7b illustrating an example of a separated assembly. As shown by way of example in the partial images of Fig. 14, the passive component, i.e., the channel structure 12-2 formed as a blind hole, can also take any other suitable form to provide the passive component associated with the transistor. Thus, the manufacturing method described with reference to Fig. 1 or Fig. 2 for filling channel structures 12-1 (e.g., 3D channels) in the substrate 12 can be used to manufacture embedded passive components 12-2, such as coils with and without cores, coils with fluid channels for medical applications, antennas, capacitors, etc. In the following, further procedures (schematic flow diagrams 100-# of the method 100) for producing an electrically conductive channel structure 12-2 in a substrate 12 are described with reference to Figs. 15-22, wherein optional configurations of the clamping device 30 and its mode of operation, as well as different configurations of the stacking arrangement 10, can be applied to the manufacturing method 100 described above. These further optional configurations can, for example, support the function of the compressible sealing element (surface sealing or ring sealing element) 16 of Fig. 1 or Fig. 2a-b, although the compressible sealing element 16 is not explicitly shown in some alternatives of the manufacturing method 10 described below. In the further exemplary embodiments 100-1 - 100-8 (100-#) of the flowchart of the manufacturing method 100 shown in the following Figs. 15-22, the method steps shown with reference to Figs. 1 and 2 are again essentially carried out, with the additions and changes (differences) compared to the manufacturing method 100 described above being presented below. Furthermore, identical, functionally equivalent or equivalent elements, objects, functional blocks and / or method steps are provided with the same reference numerals in the different figures, so that the description of these elements, objects, functional blocks and / or method steps (with the same reference numeral) presented in the different exemplary embodiments is interchangeable or can be applied to one another. In the following, exemplary implementations for realizing a suction vacuum are also described (see also the embodiments based on Figs. 15 - 22 ), wherein the vacuum for sucking the melt 14-1 into non-through hole structures (blind holes) 12-1 can be produced in different ways. A vacuum can be applied, particularly for through-holes or blind holes 12-1, with a very thin tapping through a vacuum chuck 34 from the underside of the glass substrate 12 to be filled. Using the vacuum as a controlling variable can be complex in terms of process technology. Nevertheless, it is advantageous to be able to dynamically regulate the vacuum in order to prevent excessive suction of the melt 14-1 through through-holes. A flat cover substrate 32 (with a non-stick coating made of BN, carbon, etc.) under controlled contact pressure FP (e.g., mechanically plus hydraulically by flooding the chamber (= process chamber) with protective gas) prevents the aluminum foil 14 from shrinking during melting and sags toward the substrate 12 to be filled during the filling of the through-holes 12-1. The cover substrate 32 thus forms an overlying mechanical valve to reduce the flow rate of the melt through through holes 12-1.On the other hand, the cover substrate 32 prevents the upper side contact of the melt 14-1 with the ambient atmosphere, whereby the formation of surface nitrides and oxides on the aluminum can be avoided. Fig. 15 now shows an exemplary, basic flow diagram 100-1 relating to an alternative procedure for producing an electrically conductive channel structure 12-2 in the substrate 12 by introducing a metallic filling material 14-1 into the channel structure(s) 12-1 according to a further embodiment (insofar as a compressible sealing element 16 is used). According to the embodiment of flowchart 100-1 of method 100 of Fig. 15, in step 120, a substrate 12 (e.g., a perforated glass wafer) provided with a channel structure 12-1 and an (anodically bonded) aluminum foil 14 is placed onto the second tool 34 (e.g., a vacuum chuck) and sucked onto it. The metal foil 14 comprising the aluminum material can, for example, be anodically bonded to the substrate 12. In order to perform process sequence 100-1 with an anodically pre-bonded aluminum foil (a metal foil comprising aluminum material) 14, an anodically bondable substrate 12 (e.g., a glass substrate) is required. In step 140, in an inert gas environment with atmospheric pressure (e.g., overpressure P1), the metal foil (aluminum foil) 14 can be pressed against the substrate 12 with the upper (coated) stop 32 (first tool) and heated. The metal foil melts, at least partially or completely filling the channel structures (e.g., holes) 12-1 in the substrate 12. The filling of the channel structures 12-1 is assisted by the atmospheric (suction) negative pressure (vacuum) provided by the second tool 34 (vacuum chuck). In step 116, the processed stack arrangement 10 is cooled, wherein after cooling and ventilating the process chamber and switching off the vacuum suction, the substrate 12 provided with the electrically conductive channel structure 12-2 (ie the filled wafer) can be removed. In the following, a further exemplary, basic flow diagram 100-2 of the manufacturing method 100 for producing an electrically conductive channel structure 12-2 in a substrate 12 by introducing a metallic filler material 14-1 according to a further exemplary embodiment will now be described with reference to Fig. 16. The process 100-2 of Fig. 16 differs from the process 100-1 of Fig. 15 in that instead of the anodically pre-bonded aluminum foil 14, an AlCu roll-clad sheet 14 (foil) is now used, wherein this sheet 14 can also optionally be anodically bonded to the substrate 12. Furthermore, since part of the copper of the AlCu sheet 14 melts in step 140, the channel structures (holes) 12-1 can be filled with an AlCu alloy by AlCu eutectic formation in order to obtain the conductive channel structures 12-2 in the substrate. In the following, a further exemplary, basic flow diagram 100-3 of the manufacturing method 100 for producing an electrically conductive channel structure 12-2 in a substrate 12 by introducing a metallic filler material 14-1 according to a further exemplary embodiment will now be described with reference to Fig. 17. In process flow 100-3, for example, an aluminum foil 14 anodically prebonded to a glass wafer (glass substrate) 12 is used, wherein the perforated glass substrate 12 comprises, for example, a "Schott Af32 eco" material. Furthermore, a flow stop for the liquefied metal material 14-1 is created by the centrally narrowed hole geometry 23. The glass substrate 12 of Fig. 17 corresponds, for example, to the substrate 12 described with reference to Fig. 6i. As becomes clear in step 140, the molten aluminum material 14-1 is filled, for example, into the holes (channel structures) 12-1 to a certain degree, wherein the degree of filling can be defined or adjusted by the hole geometry (the hole cross-section) and the provided atmospheric negative pressure (suction vacuum). In the following, a further exemplary, basic flow diagram 100-4 of the manufacturing method 100 for producing an electrically conductive channel structure 12-2 in a substrate 12 by introducing a metallic filler material 14-1 according to a further exemplary embodiment will now be described with reference to Fig. 18. In process sequence 100-4 of Fig. 18, a flow stop is created by two laterally offset substrates (glass substrates) 12, 12'. For this purpose, in step 120, a perforated substrate (glass wafer) 12 is arranged offset on a similarly perforated substrate 12' (e.g., with an intermediate non-stick coating), thereby producing suction channels 12-1 with a flow stop effect at the constrictions 23. In step 140, the liquefied metal (aluminum) 14-1 of the applied metal foil 14 is mechanically pressed flat against the surface of the (e.g., coated upper stop) 32 (first tool). Heating can occur, for example, in a non-reactive gas atmosphere (N2, Ar, etc.). In step 140 (melting the aluminum foil in a non-reactive gas atmosphere with an applied suction vacuum), the channel structure 12-1 of the substrate 12 is filled up to the constriction 23, which acts as a flow stop. In the following, a further exemplary, basic flow diagram 100-5 of the manufacturing method 100 for producing an electrically conductive channel structure 12-2 in a substrate 12 by introducing a metallic filler material 12 according to a further exemplary embodiment will now be described with reference to Fig. 19. In the process sequence 100-5, the channel structures (blind holes) 12-1 in the substrate are evacuated by a procedure with melting spacers 25. In step 120, a perforated substrate (perforated glass wafer) 12 is placed on a vacuum chuck (second tool) 34 and sucked in, wherein the aluminum foil 14 is placed on the substrate 12 with (laterally spaced) spacers 25, wherein the gap / distance between the aluminum foil 14 and the substrate 12 as well as the channel structures 12-1 are evacuated via the chamber vacuum. In step 140, the upper stop (first tool) 32 is pressed flat and heated until the spacers 25 melt in the vacuum. As a result, the vacuum (atmospheric negative pressure) in the channel structures (blind holes) 12-1 remains sealed gas-tight by the pressed-on aluminum foil 14. The process chamber can optionally be flooded with an inert gas to support the pressing of the aluminum foil 14 against the substrate 12. Upon heating to the process temperature, the metal material (aluminum) of the metal foil 14 melts and flows into the evacuated channel structures (hole structures) 12-1. After cooling and ventilating the process chamber and switching off the vacuum suction, the substrate 12 (the filled wafer) provided with the electrically conductive channel structures 12-2 can be removed in step 116. In the following, a further exemplary, basic flow diagram 100-6 of the manufacturing method 100 for producing an electrically conductive channel structure 12-2 in a substrate 12 by introducing a metallic filler material 12 according to a further exemplary embodiment will now be described with reference to Fig. 20. In the process sequence 100-6 illustrated in Fig. 20, the fastening of the aluminum foil 14 can be carried out by a thin-film soldering process. In step 120, a substrate 12 (perforated glass wafer) provided with the channel structures 12-1, for example, with an AlGe solder coating 27 facing upwards, is placed onto the second tool (vacuum chuck) 34 and sucked in, whereupon the aluminum foil 14 is placed onto the coated substrate 12. In step 140, a pressing (mechanical pressure) is created with the upper coated stop (first tool) 32 in the vacuum environment, and the upper stop 32 is heated to create a eutectic AlGe solder bond between the AlGe solder coating 27 and the Al foil 14. When heated to the process temperature TP, the aluminum foil is then completely melted and introduced (flowed) into the (optionally stepped) channel structures (blind holes) 12-1 in the substrate 12. In step 160, after the process chamber has been cooled and ventilated and the vacuum suction has been switched off, the filled substrate (the filled wafer) 12 can be removed. In the following, a further exemplary, basic flow diagram 100-7 of the manufacturing method 100 for producing an electrically conductive channel structure 12-2 in a substrate 12 by introducing a metallic filler material 12 according to a further exemplary embodiment will now be described with reference to Fig. 21. The process 100-7 of Fig. 21 differs from the process 100-6 of Fig. 20 in that the substrate (e.g., a perforated glass wafer) 12 has channel structures 12-1 in the form of both blind holes and vias. According to the process flow 100-7, both the channel structures 12-1 formed as vias and blind holes in the substrate 12 can be filled with the molten metal. In the following, a further exemplary, basic flow diagram 100-8 of the manufacturing method 100 for producing an electrically conductive channel structure 12-2 in a substrate 12 by introducing a metallic filler material 12 according to a further exemplary embodiment will now be described with reference to Fig. 22. In the process sequence 100-8 shown in Fig. 22, aluminum pressure melt filling is performed with a flow stop by the counter substrate 34 (without using a surface seal 16). In step 120, a substrate 12 (a perforated glass wafer) provided with channel structures 12-1 is arranged on a counter substrate (second tool) 34 coated with a rough anti-adhesion layer 36. In step 140, the pressure filling of the channel structures 12-1 takes place with a flow stop effect on the surface of the counter substrate 34. In step 160, the substrate (glass substrate) 12 equipped with aluminum TGVs can be removed. Although some aspects of the present disclosure have been described as features in the context of an apparatus, it is to be understood that such a description may also be considered a description of corresponding method features. Although some aspects have been described as features in the context of a method, it is to be understood that such a description may also be considered a description of corresponding features of an apparatus or the functionality of an apparatus. Some or all of the method steps may be performed by (or using) a hardware apparatus, such as a microprocessor, a programmable computer, or electronic circuitry. In some embodiments, some or more of the method steps may be performed by such an apparatus.Depending on particular implementation requirements, embodiments of the invention may be implemented in hardware or in software, or at least partially in hardware or at least partially in software. In the foregoing Detailed Description, various features have been grouped together in examples in order to streamline the disclosure. This manner of disclosure should not be interpreted as intending that the claimed examples include more features than are expressly recited in each claim. Rather, as the following claims reflect, the subject matter may lie in fewer than all of the features of a single disclosed example. Accordingly, the following claims are hereby incorporated into the Detailed Description, with each claim being capable of standing as its own separate example.While each claim may stand as its own separate example, it should be noted that although dependent claims in the claims refer to a specific combination with one or more other claims, other examples also include a combination of dependent claims with the subject matter of any other dependent claim or a combination of any feature with other dependent or independent claims. Such combinations are intended to be encompassed unless it is stated that a specific combination is not intended. Furthermore, it is intended to encompass a combination of features of a claim with any other independent claim, even if that claim is not directly dependent on the independent claim.

Claims

Method (100; 100-#) for producing an electrically conductive channel structure in a substrate, comprising the following steps: Providing (120) a stack arrangement (10) in a clamping device (30), wherein the stack arrangement (10) comprises a substrate (12) provided with a channel structure (12-1), a metal foil (14) comprising an aluminum material on the substrate (12), and a compressible sealing element (16) which is designed to surround the metal foil (14) at least laterally under pressure, Exerting (140) a surface-acting mechanical process pressure (FP) and a process temperature (PT) with the clamping device (30) onto the stack arrangement (10) in order to melt the metal foil (14) comprising the aluminum material at the process temperature and to insert it into the channel structure as a metallic filler material (14-1) by means of the surface-acting mechanical process pressure (12-1), andcooling (160) the stack arrangement (10),to solidify the introduced metallic filler material (14-1) and to obtain the electrically conductive channel structure (12-2) filled with the metallic filler material (14-1). Method (100) according to claim 1, wherein the channel structure is formed as at least one through-hole structure, as at least one blind hole structure or as at least one 3D structure in the substrate. Method (100) according to claim 1 or 2, wherein the metal foil comprises the aluminum material as a main component (≥ 80%) for a resulting melting point of at least 420°C or between 420°C and 850°C. Method (100) according to one of the preceding claims, wherein the process temperature is set to a value of at least 10 K above the melting temperature of the metal foil comprising the aluminum material. Method (100) according to one of the preceding claims, wherein the channel structure has a wall coating comprising a nitride material with a thickness in a range of 5 to 100 nm. Method (100) according to one of the preceding claims, wherein the compressible sealing element is designed as a reusable high-temperature seal. Method (100) according to one of the preceding claims, wherein the compressible sealing element is designed as a compressible surface sealing element, and wherein the surface sealing element covers the metal foil and has a lateral overhang in order to enclose the metal foil up to the substrate when the mechanical process pressure is exerted. Method (100) according to claim 7, wherein the surface sealing element comprises a graphite foil having a thickness in a range of 0.3 to 1 mm or of about 0.5 mm. Method (100) according to one of claims 1 to 6, wherein the compressible sealing element is designed as a compressible ring sealing element, and wherein the ring sealing element surrounds the edge region of the metal foil and laterally encloses the metal foil under the application of pressure. Method (100) according to claim 9, wherein the annular sealing element comprises a structured graphite foil having a thickness in a range of 0.3 to 1 mm or of about 0.5 mm. The method (100) of any preceding claim, wherein the clamping device (30) comprises a first and a second tool, and wherein the stacking arrangement is disposed between the first and second tools. Method (100) according to one of the preceding claims, wherein the step of exerting mechanical pressure between the first and second tools is carried out with a contact pressure in a range of 10 N / cm2 to 600 N / cm2. Method (100) according to claim 11, wherein the first and / or second tool is configured to heat the stack assembly to the process temperature. Method (100) according to claim 11 or 13, wherein the first tool is designed as a press stamp and the second tool as a counter substrate, wherein a main surface area of the second tool facing the substrate has a surface roughness with a mean roughness value Ra or an average roughness depth RZ between 0.5 to 10 µm or of approximately 3 µm. The method (100) of claim 14, wherein the main surface area of the second tool facing the substrate comprises a coating to provide the surface roughness of the main surface area of the second tool facing the substrate. Method (100) according to claim 14 or 15, wherein the coating comprises a boron nitride material. Method (100) according to one of claims 14 to 16, wherein the surface roughness of the main surface area of the second tool adjacent to the substrate is selected to act as a flow stop for the molten metal and to allow lateral escape of a gas present in the channel structure. Method (100) according to one of the preceding claims, wherein the substrate comprises a glass, quartz, sapphire, ceramic or semiconductor material. Method (100) according to one of the preceding claims, further comprising the step of:removing excess metallic filler material on one side of a main surface area or on both sides of both opposite main surface areas of the substrate. Method (100) according to claim 19, wherein the removal of the excess material is carried out by means of a CMP process (CMP = chemical mechanical polishing). The method (100) of any preceding claim, further comprising the steps of:removing the stack assembly from the clamping device (30), andremoving the sealing element from the substrate. Method (100) according to one of the preceding claims, further comprising the following step: performing a single-sided or double-sided metallization by means of a thin-film deposition process in order to obtain, via a lithographic structuring process and a subsequent etching step, a metallization structure electrically connected to the conductive channel structure on one or both main surface regions of the substrate formed with the conductive channel structure.

Citation Information

Patent Citations

  • Hybrid integrated component and method for its manufacture

    DE102012208033A1

  • Semiconductor package and methods for its manufacture

    DE102020128994A1

  • BAVV resonators with antisymmetric thickness electrodes

    DE112020002022T5

  • Low-Temperature Wafer Level Processing for MEMS Devices

    US20130115730A1

  • Method for forming through substrate vias

    US20160093530A1