ZINC SECONDARY BATTERY
By applying insulating tape to cover welded sections on uncoated areas of electrode plates in zinc secondary batteries, the risk of short circuits caused by electrode tongue peeling is minimized, improving battery durability and extending charge/discharge life.
Patent Information
- Application Number
- DE112022006545
- Authority / Receiving Office
- DE · DE
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-03-28
- Filing Date
- 2022-10-25
- Publication Date
- 2024-11-28
AI Technical Summary
Zinc secondary batteries face issues with short circuits due to zinc dendrites penetrating through separators, leading to reduced charge/discharge life, particularly in tab-up type batteries where insufficient welding of electrode tongues can cause peeling and subsequent short circuits.
Incorporating an insulating tape on uncoated areas of electrode plates to cover welded sections, ensuring that electrode tongues are less likely to peel off and reducing the risk of short circuits by providing insulation at the junctions.
The use of insulating tape on uncoated areas of electrode plates significantly reduces the likelihood of short circuits, enhancing the durability and longevity of zinc secondary batteries by preventing electrode tongue peeling and penetration through hydroxide ion-conducting separators.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The present disclosure relates to a zinc secondary battery. BACKGROUND
[0002] It is known that in zinc secondary batteries, such as nickel-zinc secondary batteries and air-zinc secondary batteries, metallic zinc precipitates in dendrite form from a negative electrode during charging, penetrates into the cavities of a separator, such as a nonwoven fabric, and reaches a positive electrode, resulting in a short circuit. This short circuit due to such zinc dendrites leads to a shortened repeated charge / discharge life.
[0003] To address the problems described above, a battery comprising a layered double hydroxide (LDH) separator has been proposed, which blocks the penetration of zinc dendrites while selectively permeating hydroxide ions. For example, Patent Literature 1 (WO2013 / 118561) discloses a nickel-zinc secondary battery including an LDH separator provided between a positive electrode and a negative electrode. Patent Literature 2 (WO2016 / 076047) discloses a separator structure comprising an LDH separator attached to or bonded to an outer resin frame, wherein the LDH separator has a high density so that it exhibits gas impermeability and / or water impermeability. Furthermore, the literature also discloses that the LDH separator may be bonded to a porous substrate.Furthermore, Patent Literature 3 (WO2016 / 067884) discloses various methods for forming a dense LDH membrane on a surface of a porous substrate to obtain a composite material. This method includes steps of uniformly adhering a raw material capable of providing the porous substrate with a starting point for LDH crystal growth, and hydrothermally treating the porous substrate in an aqueous raw material solution to form a dense LDH membrane on a surface of the porous substrate. An LDH separator further densified by roll pressing an LDH / porous substrate composite material prepared by hydrothermal treatment has also been proposed.For example, Patent Literature 4 (WO2019 / 124270) discloses an LDH separator comprising a porous polymer substrate and an LDH filled into the porous substrate and having a linear transmittance at a wavelength of 1000 nm of 1% or more.
[0004] Furthermore, LDH-type compounds are known as hydroxides and / or oxides with a layered crystal structure that cannot be referred to as LDH but are analogous thereto, which have hydroxide ion-conducting properties similar to those of a compound to the extent that they can be collectively referred to as hydroxide ion-conducting layered compounds together with LDH. For example, Patent Literature 5 (WO2020 / 255856) discloses a hydroxide ion-conducting separator comprising a porous substrate and a layered double hydroxide (LDH)-type compound that clogs pores in the porous substrate, wherein the LDH-type compound is a hydroxide and / or oxide with a layered crystal structure containing Mg and one or more elements including at least Ti and selected from the group consisting of Ti, Y, and Al.It is described that this hydroxide ion conductive separator has excellent alkali resistance compared to a conventional LDH separator and can also effectively inhibit short circuit due to zinc dendrites.
[0005] Incidentally, Patent Literature 6 (WO2019 / 069760) and Patent Literature 7 (WO2019 / 077953) have proposed a zinc secondary battery having a configuration in which the entire negative electrode active material layer is covered or wrapped with a liquid-holding member and an LDH separator, and a positive electrode active material layer is covered or wrapped with a liquid-holding member. A nonwoven fabric is used as the liquid-holding member. It is described that according to such a configuration, complicated sealing and bonding between the LDH separator and a battery container is unnecessary, and thus a zinc secondary battery (especially a stacked cell battery thereof) capable of preventing the propagation of zinc dendrites can be manufactured extremely easily and with high productivity.Patent Literature 8 (WO2021 / 193436) has disclosed a zinc secondary battery in which a laminate alternately including a positive electrode plate and a negative electrode plate, a positive electrode current collector tab connected to a positive electrode current collector in the positive electrode plate, and a negative electrode current collector tab connected to a negative electrode current collector in the negative electrode plate are vertically arranged, and the positive electrode current collector tab and the negative electrode current collector tab protrude upward from the laminate. CITATION LISTPATENT LITERATURE Patent literature 1: WO2013 / 118561 Patent literature 2: WO2016 / 076047 Patent literature 3: WO2016 / 067884 Patent literature 4: WO2019 / 124270 Patent literature 5: WO2020 / 255856 Patent literature 6: WO2019 / 069760 Patent literature 7: WO2019 / 077953 Patent literature 8: WO2021 / 193436 SUMMARY OF THE INVENTION
[0006] In manufacturing a zinc secondary battery of a type in which a current collector tab extends upward from an electrode laminate (hereinafter referred to as the upward tab type) as disclosed in Patent Literature 8, a tab (current collector tab) is connected to an electrode current collector by welding, and the tab is connected to an electrode terminal. Fig. 9A and Fig. 9B shows an example of a zinc secondary battery 110 of such a tongue-up type. The zinc secondary battery 110 includes an electrode laminate 111 comprising a positive electrode plate 112 including a positive electrode active material layer 112a and a positive electrode current collector 112b, and a negative electrode plate 114 including a negative electrode active material layer 114a and a negative electrode current collector 114b. Above the positive electrode plate 112 (or the negative electrode plate 114) is an uncoated area U in which the positive electrode current collector 112b (or the negative electrode current collector 114b) is exposed without being covered with the positive electrode active material layer 112a (or the negative electrode active material layer 114a), as shown in FIG. Fig. 10, and a positive electrode tab 113 (or a negative electrode tab 115) is connected by welding to this uncoated area U. The positive electrode plate 112 (or the negative electrode plate 114) is covered or wrapped with a hydroxide ion conductive separator 116 and / or a liquid holding member 117, as shown in Fig. 11. Then, as in Fig. 9A and Fig. 9B illustrates, the positive electrode tabs 113 extending from a plurality of positive electrode plates 112 are connected together with a positive electrode terminal 126 in a positive electrode tab connecting portion 130, and the negative electrode tabs 115 extending from a plurality of negative electrode plates 114 are connected together with a negative electrode terminal 128 in a negative electrode tab connecting portion 132.
[0007] However, if the tabs 113 or 115 and the current collectors 112b or 114b are insufficiently welded, the tabs 113 or 115 may be peeled off (or partially peeled off) from the current collector 112b or 114b due to a load caused when the plurality of tabs 113 or 115 are collected. For example, such peeling may be caused by a load due to expansion / shrinkage of the positive electrode plate 112 and / or the negative electrode plate 114 at the time of charging / discharging. In such a case, a sharp end of the tab 113 or 115 may break through the hydroxide ion conductive separator 116 and / or the nearby liquid holding member 117, which may cause a short circuit S.
[0008] The inventors have now found that a tab-up type zinc secondary battery is less likely to experience a short circuit by placing an insulating tape on an uncoated portion of an electrode plate to cover a portion where a tab is welded.
[0009] Accordingly, an object of the present invention is to provide a tab-up type zinc secondary battery which is less likely to cause a short circuit.
[0010] The present invention provides the following aspects: [Aspect 1]
[0011] Zinc secondary battery comprising: a positive electrode plate comprising a positive electrode active material layer and a positive electrode current collector; a positive electrode tab extending from one end of the positive electrode plate; a negative electrode plate comprising a negative electrode active material layer comprising at least one of the following elements: zinc, zinc oxide, a zinc alloy, and a zinc compound, and a negative electrode current collector; a negative electrode tab extending from one end of the negative electrode plate at a position not overlapping with the positive electrode tab; a hydroxide ion conductive separator that separates the positive electrode plate and the negative electrode plate to make hydroxide ions conductive; and an electrolyte solution, wherein the positive electrode plate, the positive electrode tab, the negative electrode plate, the negative electrode tab and the hydroxide ion conductive separator are each arranged vertically and the positive electrode tab and the negative electrode tab extend upwards, wherein the positive electrode plate has an uncoated region free of the positive electrode active material layer along an upper end of the positive electrode plate, and the positive electrode tongue is welded to the positive electrode current collector in the uncoated region, and an insulating tape is arranged on the uncoated region to cover the welded portion with the insulating tape, and / or wherein the negative electrode plate has an uncoated region free from the negative electrode active material layer along an upper end of the negative electrode plate, and the negative electrode tongue is welded to the negative electrode current collector in the uncoated region, and an insulating tape is arranged on the uncoated region to cover the welded portion with the insulating tape. [Aspect 2]
[0012] The zinc secondary battery according to aspect 1, wherein 60% or more of an area of the uncoated region on both surfaces of the positive electrode plate is covered with the insulating tape and / or 60% or more of an area of the uncoated region on both surfaces of the negative electrode plate is covered with the insulating tape. [Aspect 3]
[0013] Zinc secondary battery according to aspect 1 or 2, wherein a lower end of the insulating tape is arranged on the positive electrode plate between an upper end of the positive electrode active material layer and a lower end of the positive electrode tongue, and / or wherein a lower end of the insulating tape is arranged on the negative electrode plate between an upper end of the negative electrode active material layer and a lower end of the negative electrode tongue. [Aspect 4]
[0014] Zinc secondary battery according to one of aspects 1 to 3, wherein the insulating tape is arranged on both surfaces of the uncoated portion of the positive electrode plate so that an upper end of the insulating tape is arranged over an upper end of the positive electrode current collector, whereby upper end portions of the insulating tape projecting over the upper end of the positive electrode current collector are fixed to each other, and / or wherein the insulating tape is disposed on both surfaces of the uncoated portion of the negative electrode plate such that an upper end of the insulating tape is disposed over an upper end of the negative electrode current collector, whereby upper end portions of the insulating tape projecting over the upper end of the negative electrode current collector are fixed to each other. [Aspect 5]
[0015] Zinc secondary battery according to aspect 4, wherein the insulating tape is arranged on both surfaces of the uncoated portion of the positive electrode plate such that left and right ends of the insulating tape are arranged outside the left and right ends of the positive electrode current collector, and left and right end portions of the insulating tape projecting beyond the left and right ends of the positive electrode current collector are fixed to each other, and / or wherein the insulating tape is arranged on both surfaces of the uncoated portion of the negative electrode plate such that left and right ends of the insulating tape are arranged outside the left and right ends of the negative electrode current collector, and left and right end portions of the insulating tape projecting beyond the left and right ends of the negative electrode current collector are fixed to each other. [Aspect 6]
[0016] The zinc secondary battery according to any one of aspects 1 to 5, wherein the positive electrode plate and / or the negative electrode plate is covered or wrapped with the hydroxide ion conductive separator. [Aspect 7]
[0017] The zinc secondary battery according to any one of aspects 1 to 6, wherein not only the hydroxide ion conductive separator but also a liquid holding member is disposed between the positive electrode plate and the negative electrode plate. [Aspect 8]
[0018] The zinc secondary battery according to aspect 7, wherein the positive electrode plate and / or the negative electrode plate is covered or wrapped with the liquid holding member. [Aspect 9]
[0019] The zinc secondary battery according to any one of aspects 1 to 8, wherein the hydroxide ion conductive separator is an LDH separator containing a layered double hydroxide (LDH) and / or an LDH-like compound. [Aspect 10]
[0020] The zinc secondary battery according to aspect 9, wherein the LDH separator further comprises a porous substrate and is bonded to the porous substrate, wherein the LDH and / or the LDH-like compound is filled in pores in the porous substrate. [Aspect 11]
[0021] The zinc secondary battery according to any one of aspects 1 to 10, wherein the positive electrode active material layer contains nickel hydroxide and / or nickel oxyhydroxide, whereby the zinc secondary battery is configured as a nickel-zinc secondary battery. [Aspect 12]
[0022] The zinc secondary battery according to any one of aspects 1 to 10, wherein the positive electrode active material layer is an air electrode layer, whereby the zinc secondary battery is configured as an air-zinc secondary battery. [Aspect 13]
[0023] A zinc secondary battery according to any one of aspects 1 to 12, comprising a plurality of unit cells each comprising a pair of the positive electrode plate and the negative electrode plate together with the hydroxide ion conductive separator, whereby the plurality of unit cells form a multilayer cell as a whole. BRIEF DESCRIPTION OF THE DRAWINGS Fig. 1 is a schematic cross-sectional view illustrating an example of a zinc secondary battery of the present invention. Fig. 2 is a view schematically showing a cross section AA' of the Fig. 1 shown zinc secondary battery. Fig. 3 is a perspective view schematically showing an electrode laminate of the Fig. 1 shown zinc secondary battery. Fig. 4A is a cross-sectional view schematically showing the electrode laminate of the Fig. 1 shown zinc secondary battery. Fig. 4B is a cross-sectional view schematically showing a state in the Fig. 4A, in which a tab is removed. Fig. 5 is a perspective view illustrating an example of a positive electrode plate or a negative electrode plate to which an insulating tape is applied in the manner shown in Fig. 1 shown zinc secondary battery. Fig. 6 is a perspective view showing an aspect of the Fig. 5 shown positive electrode plate or the negative electrode plate covered with a hydroxide ion conductive separator or a liquid holding member. Fig. 7 is a diagram showing an example of an attachment position of the insulating tape in the Fig. 1 shown zinc secondary battery. Fig. 8 is a diagram showing another example of the attachment position of the insulating tape in the Fig. 1 shown zinc secondary battery. Fig. 9A is a cross-sectional view schematically illustrating an electrode laminate of a conventional zinc secondary battery. Fig. 9B is a cross-sectional view schematically showing a state in the Fig. 9A, in which a tab is removed. Fig. 10 is a perspective view showing a positive electrode plate or a negative electrode plate in the Fig. 9A and Fig. 9B shown conventional zinc secondary battery. Fig. 11 is a perspective view showing an aspect of the Fig. 10 shown positive electrode plate or the negative electrode plate covered with a hydroxide ion conductive separator or a liquid holding member. DESCRIPTION OF EMBODIMENTSZinc secondary battery
[0024] A zinc secondary battery of the present invention is not particularly limited as long as it is a secondary battery that uses zinc as a negative electrode and uses an alkaline electrolyte solution (representatively, an aqueous alkali metal hydroxide solution). Accordingly, it may be a nickel-zinc secondary battery, a silver oxide-zinc secondary battery, a manganese oxide-zinc secondary battery, an air-zinc secondary battery, or any of other various alkaline zinc secondary batteries. For example, it is preferable that an active material layer of the positive electrode contains nickel hydroxide and / or nickel oxyhydroxide, thereby configuring the zinc secondary battery as a nickel-zinc secondary battery. Alternatively, an active material layer of the positive electrode may be an air electrode layer, thereby configuring the zinc secondary battery as an air-zinc secondary battery.
[0025] Fig. 1 to Fig. 6 illustrate a zinc secondary battery 10 according to one aspect of the present invention and components thereof. The zinc secondary battery 10 includes an electrode laminate 11 and an electrolyte solution (not shown) housed in a battery case 20. The electrode laminate 11 includes a positive electrode plate 12, a positive electrode tab 13, a negative electrode plate 14, a negative electrode tab 15, and a hydroxide ion conductive separator 16. The positive electrode plate 12 includes a positive electrode active material layer 12a and a positive electrode current collector 12b, and the positive electrode tab 13 extends from one end of the positive electrode plate 12.The negative electrode plate 14 includes a negative electrode active material layer 14a and a negative electrode current collector 14b, and the negative electrode tab 15 extends from one end of the negative electrode plate 14 at a position that does not overlap with the positive electrode tab 13. The negative electrode active material layer 14a includes at least one of the following elements: zinc, zinc oxide, a zinc alloy, and a zinc compound. The hydroxide ion conductive separator 16 separates the positive electrode plate 12 and the negative electrode plate 14 so that hydroxide ions can be conducted. The positive electrode plate 12, the positive electrode tab 13, the negative electrode plate 14, the negative electrode tab 15, and the hydroxide ion conductive separator 16 are each arranged vertically, and the positive electrode tab 13 and the negative electrode tab 15 extend upward.The positive electrode plate 12 has an uncoated region U along an upper end of the positive electrode plate 12 that is free of the active material layer of the positive electrode 12a, and in this uncoated region U, the positive electrode tab 13 is welded to the current collector of the positive electrode 12b, and an insulating tape 18 is arranged on the uncoated region U to cover a welded portion W with the insulating tape 18. Additionally / alternatively, the negative electrode plate 14 has an uncoated region U along an upper end of the negative electrode plate 14 that is free of the active material layer of the negative electrode 14a, and in this uncoated region U, the negative electrode tab 15 is welded to the current collector of the negative electrode 14b, and the insulating tape 18 is arranged on the uncoated region U to cover a welded portion W with the insulating tape 18.In this way, in the tab-up type zinc secondary battery 10, the insulating tape 18 is disposed on the uncoated area U of the electrode plate 12 or 14 to cover the portion where the tab 13 or 15 is welded, and thus there is less possibility of a short circuit occurring.
[0026] In particular, as mentioned above with reference to Fig. 9A to Fig. As described in FIG. 11, in a conventional tab-up type zinc secondary battery 110, a tab 113 or 115 is connected to a current collector 112b or 114b by welding, and this tab 113 or 115 is connected to an electrode terminal 126 or 128. However, if the tab 113 or 115 and the current collector 112b or 114b are insufficiently welded, the tab 113 or 115 may be peeled off (or partially peeled off) from the current collector 112b or 114b due to a load caused when a plurality of tabs 113 or 115 are collected. For example, such peeling may occur due to a load caused by expansion / shrinkage of the positive electrode plate 112 and / or the negative electrode plate 114 at the time of charge / discharge.In such a case, a sharp end of the tongue 113 or 115 may break through a hydroxide ion conductive separator 116 and / or a nearby liquid holding member 117, which may cause a short circuit S. On the contrary, in the zinc secondary battery 10 of the present invention, the insulating tape 18 is arranged on the uncoated area U of the electrode plate 12 or 14 to cover the portion where the tongue 13 or 15 is welded, and thus there is less possibility of a short circuit occurring.This is because, due to the insulating tape 18 covering the welded portion of the tongue 13 or 15, i) the welded portion W of the tongue 13 or 15 is less likely to be peeled off, and ii) even if the tongue 13 or 15 is peeled off in the welded portion W and contacts another component at its tip, the tongue 13 or 15 contacts another component (such as the hydroxide ion conductive separator 16 or the liquid holding member 17) with its tip protected by the insulating tape 18, as shown in FIG. Fig. 4B as a peeling D. In particular, there is less likelihood that the tip of the tongue 13 or 15 penetrates into the hydroxide ion conductive separator 16 or the liquid holding member 17, and when the tip penetrates these to contact the electrode plate 12 or 14, the insulating tape 18 additionally functions as an insulating material, and thus there is less likelihood of a short circuit occurring.
[0027] The insulating tape 18 is preferably applied to both the positive electrode plate 12 and the negative electrode plate 14 as in the illustrated example, but may be applied to only one of the positive electrode plate 12 and the negative electrode plate 14. In this case, too, there is less likelihood of a short circuit occurring due to peeling off one of the positive electrode tabs 13 and the negative electrode tab 15. The insulating tape 18 is not particularly limited, and a commercially available insulating tape can be used. The insulating tape 18 typically includes a substrate made of an insulating resin and an adhesive layer or a pressure-sensitive adhesive layer provided on the substrate. An example of the insulating resin includes polypropylene. The thickness of the insulating tape 18 is preferably 30 to 70 μm, and more preferably 40 to 60 μm.When the insulating tape has such a thickness, a level difference between the positive electrode active material layer 12a and the positive electrode current collector 12b or a level difference between the negative electrode active material layer 14a and the negative electrode current collector 14b can be advantageously filled, and thus, the upper end of the positive electrode active material layer 12a or the negative electrode active material layer 14a is less likely to be damaged. Accordingly, an insulating tape 18 having a thickness not greater than the level difference between the positive electrode active material layer 12a and the positive electrode current collector 12b or the level difference between the negative electrode active material layer 14a and the negative electrode current collector 14b is preferably used.
[0028] The positive electrode plate 12 includes the positive electrode active material layer 12a. A positive electrode active material contained in the positive electrode active material layer 12a is not particularly limited and can be appropriately selected from known positive electrode materials in accordance with the type of zinc secondary battery. For example, in a nickel-zinc secondary battery, a positive electrode containing nickel hydroxide and / or nickel oxyhydroxide may be used. In this case, the positive electrode active material layer 12a may contain an additive that is at least one of the following elements: a silver compound, a manganese compound, and a titanium compound, and thus a positive electrode reaction for absorbing hydrogen gas generated by a self-discharge reaction can be accelerated.In addition, the active material layer of the positive electrode 12a may further contain cobalt. Cobalt is preferably contained in the positive electrode plate 12 in the form of cobalt oxyhydroxide. In the active material layer of the positive electrode 12a, cobalt acts as a conductive aid to contribute to improving the charge / discharge capacity. Alternatively, in an air-zinc secondary battery, an air electrode may be used as the positive electrode.
[0029] The positive electrode plate 12 further includes the positive electrode current collector 12b. A preferable example of the positive electrode current collector 12b includes a porous nickel substrate, such as a foam nickel plate. In this case, for example, if a paste containing an active electrode material, such as nickel hydroxide, is uniformly applied to a porous nickel substrate and the resultant is dried, a positive electrode plate including a positive electrode current collector can be advantageously manufactured. At this point, it is also preferable that the dried positive electrode plate (namely, the positive electrode current collector) be subjected to pressing to prevent the active electrode material from dissolving and to improve the electrode density.When the positive electrode current collector 12b is a porous nickel substrate such as a foam nickel plate, the uncoated portion of the positive electrode current collector 12b can be processed into a tongue by pressing.
[0030] The positive electrode tab 13 is provided so as to extend from the end of the positive electrode plate 12. The positive electrode tab 13 is not particularly limited, and a commercially available sheet metal piece can be used. It is preferable that a plurality of positive electrode tabs 13 are connected to a positive electrode terminal 26 or a member electrically connected thereto to form a positive electrode tab connection portion 30. In this way, current collection can be performed with a simple configuration and with high space efficiency, and connection to the positive electrode terminal 26 can be facilitated.The connection between the positive electrode tongue 13 and the positive electrode current collector 12b and a member such as the positive electrode terminal 26 can be performed by any of known joining methods such as ultrasonic welding (ultrasonic bonding), laser welding, TIG welding, and resistance welding.
[0031] As in Fig. As illustrated in Fig. 7, the positive electrode plate 12 has the uncoated region U along the upper end of the positive electrode plate 12, which is free from the positive electrode active material layer 12a, and in the uncoated region U, the positive electrode tab 13 is welded to the positive electrode current collector 12b. The insulating tape 18 is arranged on the uncoated region U to cover the welded portion W with the insulating tape 18. Due to this configuration, there is less likelihood of a short circuit occurring due to the peeling off of the positive electrode tab 13, as described above. The insulating tape 18 is preferably arranged on both surfaces of the positive electrode plate 12.In this case, separate insulating tapes 18 may be disposed on one surface and the other surface of the positive electrode plate 12, respectively, or one insulating tape 18 may be reversed to be disposed on both surfaces of the positive electrode plate 12. In the latter case, one insulating tape 18 may be wound at least once around both surfaces of the positive electrode plate 12, and in this case, the insulating tape 18 and the positive electrode tab 13 are even less likely to be peeled off. It is preferable that 60% or more, more preferably 70% or more, further preferably 80% or more, and ideally 100% of the area (including the area of a pore, if the pore exists) of the uncoated region U on both surfaces of the positive electrode plate 12 is covered with the insulating tape.In this way, a connecting area between the positive electrode current collector 12b and the insulating tape 18 is increased, and therefore the insulating tape 18 is less likely to be peeled off.
[0032] The lower end of the insulating tape 18 on the positive electrode plate 12 is preferably disposed between an upper end P3 of the positive electrode active material layer and a lower end P2 of the positive electrode tab 13. In this case, the lower end of the insulating tape 18 is disposed lower than the lower end P2 of the positive electrode tab 13, and therefore, the tip of the positive electrode tab 13 is protected by the insulating tape 18, and therefore, the positive electrode tab 13 is even less likely to be peeled off, and even if the positive electrode tab 13 is peeled off, there is less possibility of a short circuit occurring. In addition, the lower end of the insulating tape 18 is disposed above the upper end P3 of the positive electrode active material layer 12a, and therefore, capacity loss can be prevented.In particular, when the active material layer of the positive electrode 12a is covered with the insulating tape 18, a region that does not contribute to a reaction is inevitably formed, which reduces the battery capacity, but when the configuration described above is used, the active material layer of the positive electrode 12a is not covered with the insulating tape 18, and therefore this problem can be avoided.
[0033] It is preferable that the insulating tape 18 is arranged on both surfaces of the uncoated area U of the positive electrode plate 12 such that the upper end of the insulating tape 18 is arranged above an upper end P1 of the positive electrode current collector 12b, and therefore, upper end portions of the insulating tape 18 projecting above the upper end P1 of the positive electrode current collector 12b are fixed to each other. In this way, the end of the positive electrode current collector 12b can be protected, and therefore, a short circuit derived from the end of the positive electrode current collector 12b can be prevented. More preferably, as shown in Fig. 8, the insulating tape 18 is arranged on both surfaces of the uncoated area U of the positive electrode plate 12 so that the left and right ends of the insulating tape 18 are located outside the left and right ends of the positive electrode current collector 12b, and therefore, left and right end portions of the insulating tape 18 projecting beyond the left and right ends of the positive electrode current collector 12b are fixed to each other. In this way, even if the adhesion between the positive electrode current collector 12b and the insulating tape 18 is low, the projecting portions on the three sides of the insulating tape 18 projecting beyond the upper end and the left and right ends of the positive electrode current collector 12b are bonded to each other with high adhesion of the insulating tape 18, and therefore, the insulating tape 18 can be effectively prevented from being peeled off.It is noted that a fixed portion between the positive electrode tab 13 and the insulating tape 18 has a high adhesion area ratio (since the positive electrode tab 13 is typically made of a non-porous material) and therefore can originally ensure high adhesion.
[0034] The negative electrode plate 14 includes the negative electrode active material layer 14a. A negative electrode active material contained in the negative electrode active material layer 14a includes at least one of the following elements: zinc, zinc oxide, a zinc alloy, and a zinc compound. The zinc can be contained in any form of a zinc metal, a zinc compound, and a zinc alloy as long as it has electrochemical activity suitable for the negative electrode. Preferred examples of the negative electrode material include zinc oxide, a zinc metal, and calcium zincate, and a mixture of a zinc metal and zinc oxide is more preferred. The negative electrode active material may be in the form of a gel or may be mixed with the electrolyte solution to obtain a negative electrode mixture.For example, a gelled negative electrode can be easily obtained by adding an electrolyte solution and a thickener to a negative electrode active material. Examples of the thickener include polyvinyl alcohol, polyacrylate, CMC, and alginic acid, with polyacrylic acid being preferred due to its excellent chemical resistance to strong alkali.
[0035] As the zinc alloy, a zinc alloy that contains neither mercury nor lead can be used, known as a mercury-free zinc alloy. For example, a zinc alloy containing 0.01 to 0.1 mass% indium, 0.005 to 0.02 mass% bismuth, and 0.0035 to 0.015 mass% aluminum is preferred because it has the effect of inhibiting hydrogen gas generation. In particular, indium and bismuth are advantageous in improving discharge performance. When a zinc alloy is used in the negative electrode, a self-dissolution rate in an alkaline electrolyte solution is reduced to inhibit hydrogen gas generation, and thus safety can be improved.
[0036] The form of the negative electrode material is not particularly limited and is preferably powdered, thus increasing the surface area to accommodate a large current discharge. A preferred average particle size of the negative electrode material when using a zinc alloy is in a range of 3 to 100 μm along the minor axis. When the average particle size is within this range, the surface area is large enough to suitably accommodate a large current discharge. In addition, the material can be easily mixed homogeneously with an electrolyte solution and a gelling agent, and the handling during battery assembly is advantageous.
[0037] The negative electrode plate 14 further includes a negative electrode current collector 14b. The negative electrode active material layer 14a may be disposed on both surfaces of the negative electrode current collector 14b, or the negative electrode active material layer 14a may be disposed on only one surface of the negative electrode current collector 14b. The negative electrode current collector 14b preferably uses a metal plate having a plurality of (or a large number of) openings from the perspective of attaching the negative electrode active material to the current collector. Preferred examples of such a negative electrode current collector 14b include an expanded metal, a stamped metal, a metal mesh, and a combination thereof; more preferred examples include a copper expanded metal, a copper stamped metal, and a combination thereof; and a particularly preferred example includes a copper expanded metal.In this case, for example, a negative electrode plate comprising a negative electrode current collector / negative electrode can be advantageously manufactured by applying a mixture containing a zinc oxide powder and / or a zinc powder and optionally a binder (for example, a polytetrafluoroethylene particle) to a copper expanded metal. At this point, it is also preferable that the dried negative electrode plate (namely, the negative electrode current collector / negative electrode) be subjected to pressing to prevent the active electrode material from dissolving and to improve the electrode density. An expanded metal refers to a mesh-shaped metal plate obtained by forming and stretching staggered cuts in a metal plate with an expanded metal machine, and forming the cuts into a diamond shape or a hexagonal shape.A stamped metal is also called a perforated metal and refers to a metal plate that has holes punched into it. A metal mesh is a metal product with a wire mesh structure and is different from expanded metal and stamped metal.
[0038] The negative electrode tab 15 is provided so as to extend from one end of the negative electrode plate 14 at a position that does not overlap with the positive electrode tab 13 (see Fig. 3). The negative electrode tab 15 is not particularly limited, and a commercially available sheet metal piece can be used. It is preferable that a plurality of negative electrode tabs 15 are connected to a negative electrode terminal 28 or a member electrically connected thereto to form a negative electrode tab connection portion 32. In this way, current collection can be performed with a simple configuration and with high space efficiency, and connection to the negative electrode terminal 28 can be facilitated. The connection between the negative electrode tab 15 and the negative electrode current collector 14b and a member such as the negative electrode terminal 28 can be performed by any of known joining methods such as ultrasonic welding (ultrasonic bonding), laser welding, TIG welding, and resistance welding.
[0039] As in Fig. As illustrated in Fig. 7, the negative electrode plate 14 has the uncoated region U free from the negative electrode active material layer 14a along the upper end of the negative electrode plate 14, and in the uncoated region U, the negative electrode tab 15 is welded to the negative electrode current collector 14b. The insulating tape 18 is arranged on the uncoated region U to cover the welded portion W with the insulating tape 18. Due to this configuration, as described above, the occurrence of a short circuit caused due to the peeling off of the negative electrode tab 15 can be made difficult. The insulating tape 18 is preferably arranged on both surfaces of the negative electrode plate 14.In this case, separate insulating tapes 18 may be disposed on one surface and the other surface of the negative electrode plate 14, respectively, or one insulating tape 18 may be reversed to be disposed on both surfaces of the negative electrode plate 14. In the latter case, one insulating tape 18 may be wound at least once around both surfaces of the negative electrode plate 14, and in this case, the insulating tape 18 and the negative electrode tab 15 are even less likely to be peeled off. It is preferable that 60% or more, more preferably 70% or more, further preferably 80% or more, and ideally 100% of the area (including the area of a pore, if the pore exists) of the uncoated region U on both surfaces of the negative electrode plate 14 is covered with the insulating tape.In this way, a connecting area between the negative electrode current collector 14b and the insulating tape 18 is increased, and therefore the insulating tape 18 is less likely to be peeled off.
[0040] The lower end of the insulating tape 18 on the negative electrode plate 14 is preferably disposed between an upper end P3 of the negative electrode active material layer 14a and a lower end P2 of the negative electrode tab 15. In this case, the lower end of the insulating tape 18 is disposed lower than the lower end P2 of the negative electrode tab 15, and therefore, the tip of the negative electrode tab 15 is protected by the insulating tape 18, and therefore, the negative electrode tab 15 is even less likely to be peeled off, and even if the negative electrode tab 15 is peeled off, there is less possibility of a short circuit occurring. In addition, the lower end of the insulating tape 18 is disposed above the upper end P3 of the negative electrode active material layer, and therefore, capacity loss can be prevented.In particular, when the active material layer of the negative electrode 14a is covered with the insulating tape 18, a region that does not contribute to a reaction is inevitably formed, which reduces the battery capacity, but when the configuration described above is used, the active material layer of the negative electrode 14a is not covered with the insulating tape 18, and therefore this problem can be avoided.
[0041] It is preferable that the insulating tape 18 is arranged on both surfaces of the uncoated area U of the negative electrode plate 14 such that the upper end of the insulating tape 18 is arranged above an upper end P1 of the negative electrode current collector 14b, and therefore, upper end portions of the insulating tape 18 projecting above the upper end P1 of the negative electrode current collector 14b are fixed to each other. In this way, the end of the negative electrode current collector 14b can be protected, and therefore, a short circuit derived from the end of the negative electrode current collector 14b can be prevented. More preferably, as shown in Fig. 8, the insulating tape 18 is disposed on both surfaces of the uncoated area U of the negative electrode plate 14 so that the left and right ends of the insulating tape 18 are located outside the left and right ends of the negative electrode current collector 14b, and therefore, the left and right end portions of the insulating tape 18 that protrude beyond the left and right ends of the negative electrode current collector 14b are fixed to each other. In this way, even if the adhesion between the negative electrode current collector 14b and the insulating tape 18 is low, the protruding portions on the three sides of the insulating tape 18 that protrude beyond the upper end and the left and right ends of the negative electrode current collector 14b are bonded to each other with high adhesion of the insulating tape 18, and therefore, the insulating tape 18 can be effectively prevented from being peeled off.For example, when the negative electrode current collector 14b is a porous material such as expanded metal, stamped metal, or metal mesh, an adhesion area ratio to the insulating tape 18 is low, and therefore, the adhesion between the negative electrode current collector 14b and the insulating tape 18 is poor. Even in such a case, peeling off of the insulating tape 18 can be effectively prevented due to the high adhesion in the protruding portions over the above-mentioned three sides. Note that a fixed portion between the negative electrode tab 15 and the insulating tape 18 has a high adhesion area ratio (since the negative electrode tab 15 is typically made of a non-porous material) and can therefore originally ensure high adhesion.
[0042] The hydroxide ion conductive separator 16 is provided to separate the positive electrode plate 12 and the negative electrode plate 14 so that hydroxide ions can be conducted. For example, as shown in the Fig. 4A, Fig. 4B and Fig. As illustrated in Figure 6, the positive electrode plate 12 and / or the negative electrode plate 14 (preferably the negative electrode plate 14) may be covered or wrapped with the hydroxide ion conductive separator 16. Thus, complicated sealing and bonding between the hydroxide ion conductive separator 16 and the battery container is unnecessary, and thus a nickel-zinc secondary battery (particularly a stacked cell battery thereof) capable of preventing the propagation of zinc dendrites can be manufactured extremely easily and with high productivity. A simple configuration in which the hydroxide ion conductive separator 16 is disposed on one side of the positive electrode plate 12 or the negative electrode plate 14 can be used.
[0043] The hydroxide ion-conductive separator 16 is not particularly limited as long as it is a separator capable of separating the positive electrode plate 12 and the negative electrode plate 14 so that hydroxide ions can be conducted, and is representative of a separator containing a hydroxide ion-conductive solid electrolyte and selectively transmitting hydroxide ions by exclusively utilizing hydroxide ion conductivity. A preferred hydroxide ion-conductive solid electrolyte is a layered double hydroxide (LDH) and / or an LDH-type compound. Accordingly, the hydroxide ion-conductive separator 16 is preferably an LDH separator. The "LDH separator" herein is a separator containing an LDH and / or an LDH-type compound and is defined as a separator that selectively transmits hydroxide ions by exclusively utilizing hydroxide ion conductivity of the LDH and / or the LDH-type compound.The "LDH-like compound" herein is a hydroxide and / or oxide having a layered crystal structure analogous to LDH, but is a compound that cannot be called LDH, and can be considered an equivalent of LDH. However, according to a broad definition, it can be recognized that "LDH" includes not only LDH but also LDH-like compounds. The LDH separator is preferably bonded to a porous substrate. Accordingly, it is preferred that the LDH separator further comprises a porous substrate and is bonded to the porous substrate, with the LDH and / or LDH-like compound being filled in pores in the porous substrate.In other words, in a preferred LDH separator, the LDH and / or the LDH-like compound plugs pores in the porous substrate so that hydroxide ion conductivity and gas impermeability can be exhibited (thereby enabling the LDH separator to function as an LDH separator exhibiting hydroxide ion conductivity). The porous substrate is preferably made of a polymer material, and the LDH is more preferably incorporated over the entire area in the thickness direction of the porous substrate made of a polymer material. For example, known LDH separators disclosed in Patent Literatures 1 to 7 can be used. The thickness of the LDH separator is preferably 5 to 100 μm, more preferably 5 to 80 μm, further preferably 5 to 60 μm, and particularly preferably 5 to 40 μm.
[0044] It is preferable that not only the hydroxide ion conductive separator 16 but also the liquid holding member 17 is arranged between the positive electrode plate 12 and the negative electrode plate 14. Then, as shown in the Fig. 4A, Fig. 4B and Fig. 6, the positive electrode plate 12 and / or the negative electrode plate 14 is preferably covered or wrapped with the liquid-retaining member 17. A simple configuration in which the liquid-retaining member 17 is disposed on one side of the positive electrode plate 12 or the negative electrode plate 14 can be used. In either configuration, since the liquid-retaining member 17 is thus disposed, the electrolytic solution can be uniformly present between the positive electrode plate 12 and / or the negative electrode plate 14 and the hydroxide ion-conductive separator 16, and thus hydroxide ions can be efficiently transferred between the positive electrode plate 12 and / or the negative electrode plate 14 and the hydroxide ion-conductive separator 16.The liquid holding member 17 is not particularly limited as long as it is a member capable of holding the electrolyte solution, and is preferably a sheet-shaped member. Preferred examples of the liquid holding member 17 include a nonwoven fabric, a water-absorbent resin, a liquid-retaining resin, a porous sheet, and various spacers. A nonwoven fabric is particularly preferred because a negative electrode structure with good performance can be manufactured at a low cost. The liquid holding member 17 or the nonwoven fabric has a thickness of preferably 10 to 200 μm, more preferably 20 to 200 μm, further preferably 20 to 150 μm, particularly preferably 20 to 100 μm, and most preferably 20 to 60 μm.When the thickness falls within this range, with the entire size of the positive electrode structure and / or the negative electrode structure efficiently suppressed to be compact, a sufficient amount of the electrolyte solution can be held in the liquid holding member 17.
[0045] When the positive electrode plate 12 and / or the negative electrode plate 14 are covered or wrapped with the liquid-retaining member 17 and / or the separator 16, the outer edges thereof (except for the sides from which the positive electrode tab 13 and the negative electrode tab 15 extend) are preferably closed. In this case, closed sides of the outer edges of the liquid-retaining member 17 and / or the separator 16 are preferably realized by bending the liquid-retaining member 17 and / or the separator 16 or sealing the edges of the liquid-retaining member 17 and / or the edges of the separator 16. Preferred examples of the sealing method include an adhesive, thermal welding, ultrasonic welding, an adhesive tape, a sealing tape, and a combination thereof.In particular, an LDH separator comprising a porous substrate made of a polymer material has flexibility and is thus advantageously easily bent. Therefore, it is preferable that the LDH separator formed into a rectangular shape be bent to maintain a state where one side of the outer edges is closed. For thermal welding and ultrasonic welding, a commercially available heat sealer or the like can be used. When sealing the edges of an LDH separator, it is preferable to perform thermal welding and ultrasonic welding with an outer peripheral portion of the liquid holding member 17 sandwiched between outer peripheral portions of the LDH separator, because sealing can thus be performed more effectively.On the other hand, commercially available products can be used as an adhesive, an adhesive tape, and a sealing tape. To prevent deterioration otherwise caused in an alkaline electrolytic solution, one containing an alkali-resistant resin is preferred. From this point of view, preferred examples of the adhesive include an epoxy resin-based adhesive, a natural resin-based adhesive, a modified olefin resin-based adhesive, and a modified silicone resin-based adhesive. Among them, an epoxy resin-based adhesive is more preferable due to its excellent alkali resistance. An example of the epoxy resin-based adhesive includes an epoxy adhesive Hysol® (manufactured by Henkel).
[0046] The outer edge on a side corresponding to the upper edge of the separator 16 is preferably open. Such an open-top type configuration makes it possible to deal with a problem that occurs when a nickel-zinc battery or the like is overcharged. In particular, when a nickel-zinc battery or the like is overcharged, oxygen (O2) may be generated in the positive electrode plate 12, but the LDH separator has such a high density that it essentially only allows hydroxide ions to pass through and thus does not allow O2 to pass through. In this regard, when the above-described open-top type configuration is used, O2 can be transferred above the positive electrode plate 12 to be guided to the negative electrode plate 14 through the open-top portion in the battery case 20, and thus Zn of a negative electrode active material can be oxidized with the O2 to be recycled to ZnO.Due to such an oxygen reaction cycle, overcharge resistance can be improved by using an open-top type electrode laminate 11 in a sealed zinc secondary battery. Even if the outer edge on a side corresponding to the upper edge of the separator 16 or the liquid holding member 17 is closed, the same effect as that obtained by the open-type configuration can be expected by providing a vent hole in a part of the closed outer edge. For example, a vent hole may be formed after sealing the outer edge on a side corresponding to the upper edge of the LDH separator, or a part of the outer edge may be left unsealed during sealing to form a vent hole therein.
[0047] The electrolyte solution preferably contains an aqueous alkali metal hydroxide solution. Although the electrolyte solution in Fig. 1 to Fig. 4B is not illustrated, this is because the electrolytic solution spreads all over the positive electrode plate 12 and the negative electrode plate 14. Examples of an alkali metal hydroxide include potassium hydroxide, sodium hydroxide, lithium hydroxide, and ammonium hydroxide, and potassium hydroxide is more preferable. To inhibit the self-dissolution of zinc and / or zinc oxide, a zinc compound such as zinc oxide or zinc hydroxide may be added to the electrolytic solution. As described above, the electrolytic solution may be mixed with the positive electrode active material and / or the negative electrode active material to form a positive electrode mixture and / or a negative electrode mixture. In addition, the electrolytic solution may be gelled to prevent leakage of the electrolytic solution.As the gelling agent, a polymer that absorbs a solvent of the electrolyte solution to swell is preferably used, and a polymer such as polyethylene oxide, polyvinyl alcohol or polyacrylamide or starch is used.
[0048] The electrode laminate 11 is a laminate comprising a plurality of electrode layers. The electrode laminate 11 is preferably formed as shown in the Fig. 3, Fig. 4A and Fig.4B, formed into a positive / negative electrode laminate including a plurality of positive electrode plates 12, a plurality of negative electrode plates 14, and a plurality of separators 16 in which a unit of the positive electrode plate 12 / the separator 16 / the negative electrode plate 14 is repeatedly stacked. In other words, it is preferable that the zinc secondary battery 10 includes a plurality of unit cells 10a, each comprising a pair of the positive electrode plate 12 and the negative electrode plate 14 together with the hydroxide ion conductive separator 16, and thus the plurality of unit cells 10a constitute a multilayer cell as a whole. This is a configuration of a so-called battery pack or stacked cell battery, and this configuration is advantageous for obtaining high voltage and large current.
[0049] The battery case 20 is preferably made of a resin. The resin constituting the battery case 20 is preferably a resin having resistance to an alkali metal hydroxide such as potassium hydroxide, more preferably a polyolefin resin, an ABS resin, or a modified polyphenylene ether, and further preferably an ABS resin or a modified polyphenylene ether. The battery case 20 has a top cover 20a. The battery case 20 (for example, the top cover 20a) may have a pressure relief valve for discharging a gas. Furthermore, a case group in which two or more battery cases 20 are arranged may be housed in an outer frame to obtain a configuration of a battery module. LDH-like compounds
[0050] According to a preferred aspect of the present invention, the LDH separator may be a separator containing an LDH-like compound. The definition of the LDH-like compound is as described above. Preferred LDH-like compounds are as follows: (a) a hydroxide and / or oxide having a layered crystal structure containing Mg and one or more elements selected from the group consisting of Ti, Y and Al, and containing at least Ti; or (b) a hydroxide and / or oxide having a layered crystal structure containing (i) Ti, Y, optionally Al and / or Mg and (ii) at least one additive element M selected from the group consisting of In, Bi, Ca, Sr and Ba, or (c) a hydroxide and / or oxide having a layered crystal structure containing Mg, Ti, Y, optionally Al and / or In, wherein in (c) the LDH-like compound is in the form of a mixture with In(OH)3.
[0051] According to preferred aspect (a) of the present invention, the LDH-type compound may be a hydroxide and / or oxide having a layered crystal structure containing Mg and one or more elements selected from the group consisting of Ti, Y, and Al, and containing at least Ti. Thus, a typical LDH-type compound is a complex hydroxide and / or complex oxide of Mg, Ti, optionally Y, and optionally Al. The above elements may be replaced by other elements or ions to an extent that the basic properties of the LDH-type compound are not impaired, but the LDH-type compound preferably does not contain Ni. For example, the LDH-type compound may be a compound further containing Zn and / or K.
[0052] LDH-like compounds can be identified by X-ray diffraction. In particular, when X-ray diffraction is performed on the surface of the LDH separator, a peak attributed to the LDH-like compound is typically detected in the range of 5° ≤ 20 ≤ 10°, and more typically in the range of 7° ≤ 20 ≤ 10°. As described above, LDH is a substance with an alternating laminated structure in which exchangeable anions and H2O exist as an intermediate layer between the stacked hydroxide base layers. In this regard, when LDH is analyzed by the X-ray diffraction method, a peak attributed to the crystal structure of LDH (i.e., the peak attributed to (003) of LDH) is initially detected at a position of 20 = 11 to 12°.On the other hand, when the LDH-type compound is analyzed by X-ray diffraction, a peak is typically detected in the above-mentioned region, which is shifted to the lower angle side than the above peak position of LDH. Furthermore, the interlayer spacing of the layered crystal structure can be determined by the Bragg equation using 20, which corresponds to the peak assigned to the LDH-type compound in X-ray diffraction. The interlayer spacing of the layered crystal structure of the LDH-type compound thus determined is typically 0.883 to 1.8 nm, and more typically 0.883 to 1.3 nm.
[0053] The LDH separator according to the above-mentioned aspect (a) has an atomic ratio of Mg / (Mg+Ti+Y+Al) in the LDH-type compound, as determined by energy dispersive X-ray spectroscopy (EDS), which is preferably 0.03 to 0.25, and more preferably 0.05 to 0.2. Furthermore, the atomic ratio of Ti / (Mg+Ti+Y+Al) in the LDH-type compound is preferably 0.40 to 0.97, and more preferably 0.47 to 0.94. Further, the atomic ratio of Y / (Mg+Ti+Y+Al) in the LDH-type compound is preferably 0 to 0.45, and more preferably 0 to 0.37. Furthermore, the atomic ratio of Al / (Mg+Ti+Y+Al) in the LDH-type compound is preferably 0 to 0.05, and more preferably 0 to 0.03. Within the above ranges, the alkali resistance is excellent, and the effect of inhibiting short circuit due to zinc dendrites (ie, dendrite resistance) can be more effectively realized.Incidentally, LDH, which is conventionally known for LDH separators, has the basic composition which can be represented by the following formula: M. 2+ 1-x M 3+ x (OH)2A n- x / n·mH2O, where M 2+ is a divalent cation, M 3+ is a trivalent cation, A n-is an n-valent anion, n is an integer of 1 or more, x is 0.1 to 0.4, and m is 0 or more. The atomic ratios in the LDH-type compound generally differ from those in the above formula for LDH. Therefore, the LDH-type compound in the present aspect can generally be considered to have a composition ratio (atomic ratio) different from that of conventional LDH. EDS analysis is preferably performed with an EDS analyzer (e.g., X-act, manufactured by Oxford Instruments Plc.) by 1) acquiring an image at an accelerating voltage of 20 kV and a magnification of 5,000x, 2) performing three-point analysis at intervals of about 5 µm in the point analysis mode, 3) repeating steps 1) and 2) above once more, and 4) calculating the average value of a total of 6 points.
[0054] According to a further preferred aspect (b) of the present invention, the LDH-type compound may be a hydroxide and / or oxide having a layered crystal structure containing (i) Ti, Y, and optionally Al and / or Mg, and (ii) additive element M. Therefore, a typical LDH-type compound is a complex hydroxide and / or complex oxide of Ti, Y, additive element M, optionally Al, and optionally Mg. The additive element M is In, Bi, Ca, Sr, Ba, or combinations thereof. The above elements may be replaced by other elements or ions to an extent that the basic properties of the LDH-type compound are not impaired, but the LDH-type compound preferably does not contain Ni.
[0055] The LDH separator according to the above-mentioned aspect (b) has an atomic ratio of Ti / (Mg+Al+Ti+Y+M) in the LDH-type compound, as determined by energy-dispersive X-ray spectroscopy (EDS), that is preferably 0.50 to 0.85, and more preferably 0.56 to 0.81. The atomic ratio of Y / (Mg+Al+Ti+Y+M) in the LDH-type compound is preferably 0.03 to 0.20, and more preferably 0.07 to 0.15. The atomic ratio of M / (Mg+Al+Ti+Y+M) in the LDH-type compound is preferably 0.03 to 0.35, and more preferably 0.03 to 0.32. The atomic ratio of Mg / (Mg+Al+Ti+Y+M) in the LDH-type compound is preferably 0 to 0.10, and more preferably 0 to 0.02. Then, the atomic ratio of Al / (Mg+Al+Ti+Y+M) in the LDH-type compound is preferably 0 to 0.05, and more preferably 0 to 0.04. Within the above ranges, the alkali resistance is excellent, and the effect of inhibiting a short circuit due to zinc dendrites (ie,Dendrite resistance) can be realized more effectively. Incidentally, LDH, which is conventionally known for LDH separators, has the basic composition, which can be represented by the following formula: M. 2+ 1-x M 3+ x (OH)2A n- x / n· mH2O, where M 2+ is a divalent cation, M 3+ is a trivalent cation, A n-is an n-valent anion, n is an integer of 1 or more, x is 0.1 to 0.4, and m is 0 or more. The atomic ratios in the LDH-type compound generally differ from those in the above formula for LDH. Therefore, the LDH-type compound in the present aspect can generally be considered to have a composition ratio (atomic ratio) different from that of conventional LDH. EDS analysis is preferably performed with an EDS analyzer (e.g., X-act, manufactured by Oxford Instruments Plc.) by 1) acquiring an image at an accelerating voltage of 20 kV and a magnification of 5,000x, 2) performing three-point analysis at intervals of about 5 µm in the point analysis mode, 3) repeating steps 1) and 2) above once more, and 4) calculating the average value of a total of 6 points.
[0056] According to another preferred aspect (c) of the present invention, the LDH-type compound may be a hydroxide and / or oxide having a layered crystal structure containing Mg, Ti, Y, and optionally Al and / or In, wherein the LDH-type compound is in the form of a mixture with In(OH)3. The LDH-type compound in this aspect is a hydroxide and / or oxide having a layered crystal structure containing Mg, Ti, Y, and optionally Al and / or In. Therefore, a typical LDH-type compound is a complex hydroxide and / or complex oxide of Mg, Ti, Y, optionally Al, and optionally In. The In that may be contained in the LDH-type compound may be not only In that is intentionally added to the LDH-type compound, but also that that is inevitably mixed into the LDH-type compound due to the formation of In(OH)3 or the like.The above elements can be replaced with other elements or ions to the extent that the basic properties of the LDH-type compound are not impaired, but the LDH-type compound preferably does not contain Ni. Incidentally, LDH, which is conventionally known for LDH separators, has the basic composition represented by the following formula: M. 2+ 1-x M 3+ x (OH)2A n- x / n mH2O, where M 2+ is a divalent cation, M 3+ is a trivalent cation, A n-is an n-valent anion, n is an integer of 1 or more, x is 0.1 to 0.4, and m is 0 or more. The atomic ratios in the LDH-type compound generally differ from those in the above formula for LDH. Therefore, it can generally be considered that the LDH-type compound in the present aspect has a composition ratio (atomic ratio) different from that of conventional LDH.
[0057] The mixture according to aspect (c) above contains not only the LDH-type compound but also In(OH)3 (which typically consists of the LDH-type compound and In(OH)3). The contained In(OH)3 can effectively improve the alkali resistance and dendrite resistance in LDH separators. The content ratio of In(OH)3 in the mixture is preferably the amount that can improve the alkali resistance and dendrite resistance with little deterioration of the hydroxide ion conductivity of the LDH separator, and is not particularly limited. In(OH)3 may have a cubic crystal structure and a configuration in which the In(OH)3 crystals are surrounded by LDH-type compounds. In(OH)3 can be identified by X-ray diffraction. QUOTES CONTAINED IN THE DESCRIPTION
[0000] This list of documents submitted by the applicant was generated automatically and is included solely for the convenience of the reader. This list is not part of the German patent or utility model application. The DPMA assumes no liability for any errors or omissions. Cited patent literature
[0000] WO2013 / 118561 [0003, 0005] WO2016 / 076047 [0003, 0005] WO2016 / 067884 [0003, 0005] WO2019 / 124270 [0003, 0005] WO2020 / 255856 [0004, 0005] WO2019 / 069760
[0005] WO2019 / 077953
[0005] WO2021 / 193436
[0005]
Claims
[1] Zinc secondary battery, comprising: a positive electrode plate comprising a positive electrode active material layer and a positive electrode current collector; a positive electrode tab extending from one end of the positive electrode plate; a negative electrode plate comprising a negative electrode active material layer comprising at least one of the following elements: zinc, zinc oxide, a zinc alloy, and a zinc compound, and a negative electrode current collector; a negative electrode tab extending from one end of the negative electrode plate at a position not overlapping with the positive electrode tab; a hydroxide ion conductive separator that separates the positive electrode plate and the negative electrode plate to make hydroxide ions conductive; and an electrolyte solution, wherein the positive electrode plate, the positive electrode tab, the negative electrode plate, the negative electrode tab and the hydroxide ion conductive separator are each arranged vertically and the positive electrode tab and the negative electrode tab extend upwards, wherein the positive electrode plate has an uncoated region free of the positive electrode active material layer along an upper end of the positive electrode plate, and the positive electrode tongue is welded to the positive electrode current collector in the uncoated region, and an insulating tape is arranged on the uncoated region to cover the welded portion with the insulating tape, and / or wherein the negative electrode plate has an uncoated region free from the negative electrode active material layer along an upper end of the negative electrode plate, and the negative electrode tongue is welded to the negative electrode current collector in the uncoated region, and an insulating tape is arranged on the uncoated region to cover the welded portion with the insulating tape. [2] The zinc secondary battery according to claim 1, wherein 60% or more of an area of the uncoated portion on both surfaces of the positive electrode plate is covered with the insulating tape and / or 60% or more of an area of the uncoated portion on both surfaces of the negative electrode plate is covered with the insulating tape. [3] Zinc secondary battery according to claim 1 or 2, wherein a lower end of the insulating tape is arranged on the positive electrode plate between an upper end of the positive electrode active material layer and a lower end of the positive electrode tongue, and / or wherein a lower end of the insulating tape is arranged on the negative electrode plate between an upper end of the negative electrode active material layer and a lower end of the negative electrode tongue. [4] Zinc secondary battery according to claim 1 or 2, wherein the insulating tape is arranged on both surfaces of the uncoated portion of the positive electrode plate so that an upper end of the insulating tape is arranged over an upper end of the positive electrode current collector, whereby upper end portions of the insulating tape projecting over the upper end of the positive electrode current collector are fixed to each other, and / or wherein the insulating tape is disposed on both surfaces of the uncoated portion of the negative electrode plate such that an upper end of the insulating tape is disposed over an upper end of the negative electrode current collector, whereby upper end portions of the insulating tape projecting over the upper end of the negative electrode current collector are fixed to each other. [5] Zinc secondary battery according to claim 4, wherein the insulating tape is arranged on both surfaces of the uncoated portion of the positive electrode plate such that left and right ends of the insulating tape are arranged outside the left and right ends of the positive electrode current collector, and left and right end portions of the insulating tape projecting beyond the left and right ends of the positive electrode current collector are fixed to each other, and / or wherein the insulating tape is arranged on both surfaces of the uncoated portion of the negative electrode plate such that left and right ends of the insulating tape are arranged outside the left and right ends of the negative electrode current collector, and left and right end portions of the insulating tape projecting beyond the left and right ends of the negative electrode current collector are fixed to each other. [6] The zinc secondary battery according to claim 1 or 2, wherein the positive electrode plate and / or the negative electrode plate is covered or wrapped with the hydroxide ion conductive separator. [7] The zinc secondary battery according to claim 1 or 2, wherein not only the hydroxide ion conductive separator but also a liquid holding member is disposed between the positive electrode plate and the negative electrode plate. [8] The zinc secondary battery according to claim 7, wherein the positive electrode plate and / or the negative electrode plate is covered or wrapped with the liquid holding member. [9] The zinc secondary battery according to claim 1 or 2, wherein the hydroxide ion conductive separator is an LDH separator containing a layered double hydroxide (LDH) and / or an LDH-like compound. [10] Zinc secondary battery according to claim 9, wherein the LDH separator further comprises a porous substrate and is connected to the porous substrate, wherein the LDH and / or the LDH-like compound is filled in pores in the porous substrate. [11] The zinc secondary battery according to claim 1 or 2, wherein the positive electrode active material layer contains nickel hydroxide and / or nickel oxyhydroxide, whereby the zinc secondary battery is configured as a nickel-zinc secondary battery. [12] The zinc secondary battery according to claim 1 or 2, wherein the positive electrode active material layer is an air electrode layer, whereby the zinc secondary battery is configured as an air-zinc secondary battery. [13] A zinc secondary battery according to claim 1 or 2, comprising a plurality of unit cells each comprising a pair of the positive electrode plate and the negative electrode plate together with the hydroxide ion conductive separator, whereby the plurality of unit cells form a multi-layer cell as a whole.
Citation Information
Patent Citations
Zinc secondary cell
WO2013118561A1
Method for forming layered double hydroxide dense membrane
WO2016067884A1
Separator structure body for use in zinc secondary battery
WO2016076047A1
Negative electrode structure for zinc secondary battery
WO2019069760A1
Zinc secondary battery
WO2019077953A1