Banknote with antiviral protective varnish, method for producing a banknote with antiviral protective varnish and use of a banknote with antiviral protective varnish as an antiviral object
Patent Information
- Application Number
- DE502021005209
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-10-27
- Filing Date
- 2021-10-25
- Publication Date
- 2024-10-02
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Banknotes are susceptible to viral contamination due to their smooth surfaces, which allow viruses to persist and transmit effectively, and existing antimicrobial coatings do not adequately address this issue.
A banknote with an antiviral protective varnish that features an antiviral roughness on its outer surface, created through a combination of micropores, fillers, and light-unstable polymer particles, which enhances the virucidal effect by promoting quicker evaporation of viruses and facilitating the diffusion of active antiviral substances.
The antiviral roughness significantly reduces the persistence of viruses on the banknote surface, making it safer by design, and the combination of surface roughness and active ingredients effectively kills viruses, thereby preventing colonization and transmission.
Description
[0001] The invention relates to a banknote comprising a carrier substrate, at least two security elements, and a protective varnish. At least one of the two security elements is embodied as a print. The print is formed between the carrier substrate and the protective varnish. Furthermore, the outer surface of the banknote is formed by the protective varnish. The carrier substrate is at least partially surrounded by the protective varnish. Furthermore, the protective varnish or the protective varnish layer is designed to protect the print and the carrier substrate. The invention also relates to a corresponding method and a use.
[0002] A banknote is a document that serves as a means of payment in a particular country or currency area, is issued by an authorized institution and is usually denominated in a round face value of a currency unit.
[0003] Banknotes are a popular means of payment and typically change hands regularly. A payer typically picks up a banknote with their bare hand and passes it to a payee. The payee also typically accepts the banknote with their bare hand.
[0004] In this case, the banknote—like any other everyday object, such as a door handle or the keypad of a credit card terminal used to enter a credit card PIN—may contain germs. These germs can take the form of algae, bacteria, parasites, fungi, prions, protists, viruses, or viroids. Viruses have emerged as a particularly relevant germ.
[0005] EP 2 634 309 A1 describes a security paper comprising a flat substrate at least partially provided with a dirt-repellent and antimicrobial coating. The coating comprises 1,2-benzisothiazol-3-(2H)-one as at least one first antimicrobial agent and silver as the second antimicrobial agent.
[0006] AU 2012314478 A1 describes a method for treating the surface of a banknote having at least one printed object consisting of at least one motif on at least one of its opposite surfaces, said surface and the associated printed piece being covered with a transparent protective layer, wherein a coating containing a varnish and an organic chemical compound containing fluorine atoms is applied by printing.
[0007] WO 2004 / 072378 A1 describes a security paper for producing security documents such as banknotes, passports, identification documents, or the like, comprising a flat substrate at least partially provided with a dirt-repellent protective layer to extend its service life and usability. According to the invention, the protective layer comprises at least two lacquer layers. A first lower lacquer layer consists of a physically drying lacquer layer that is applied to the substrate, establishes contact with the underlying substrate, and closes its pores. Furthermore, a second upper lacquer layer is provided, which protects the substrate from physical and chemical influences.
[0008] EP 2897649 A1 describes self-cleaning banknotes using coatings, inks and additives that are photoactive and catalyze reactions that effectively break down organic contaminants or dirt to enable self-cleaning of the banknotes by exposure to ambient light as well as cleaning of banknotes.
[0009] EP 2660067 A1 describes a banknote with protective layers consisting of frosted areas and non-frosted areas or areas with different degrees of gloss, so that security elements are covered by the non-frosted areas.
[0010] The aim is to provide a banknote which has antiviral effects, as well as to create a process for producing such a banknote and to specify the use of such a banknote.
[0011] This object is achieved according to the invention by a banknote, a method, and a use having the features according to the respective independent claims. Advantageous embodiments of the invention are the subject of the dependent claims.
[0012] A banknote according to the invention comprises a carrier substrate, at least two security elements, and a protective varnish. At least one of the two security elements is embodied as a print. The print is formed between the carrier substrate and the protective varnish. The outer surface of the banknote is formed by the protective varnish. Furthermore, the carrier substrate is at least partially surrounded by the protective varnish, and the protective varnish is designed to protect the print and the carrier substrate. As an important idea, it is provided that the protective varnish is embodied as an antiviral protective varnish and has an antiviral roughness on the outer surface.
[0013] The invention is based on the finding that roughness imparts a stronger antiviral effect to the protective coating. It was surprisingly discovered that viruses, especially enveloped viruses, especially coronaviruses, persist for a shorter time on a rougher surface than on a smooth one. The persistence (lifespan) of the virus therefore depends on the degree of roughness of the surface. This is a passive effect in which viral colonization is prevented by the surface structure. This can also be described, for example, with the slogan "safe by design," analogous to the well-known lotus effect or hydrophobicity. One possible reason for the virucidal effect of roughness is that viruses dry out faster on a rough surface than on a smooth surface and then no longer persist, or at least are less or no longer infectious.
[0014] A virus is usually transmitted as an aerosol, through breathing / coughing or contact. Research shows that a virus can usually only survive in a watery environment. The antiviral protective coating increases the surface area and accelerates the evaporation of liquids, especially water.
[0015] Furthermore, micropores or capillaries can also be manufactured as absorbers. The absorber can be special fillers with a hydrophilic, microporous surface, for example, in an ink-receiving layer of a banknote. An aqueous component of the protective varnish then penetrates the ink-receiving layer (physical drying). Or the aerosol droplets spread more widely on the enlarged surface, reducing the layer thickness and shortening the evaporation time. A combination of the two mechanisms is also possible.
[0016] In addition, a porous surface can help active antiviral components in the lacquer and / or in or on the carrier substrate to reach the virus more quickly due to faster diffusion of organic antiviral substances or, in the case of silver, singlet oxygen to kill the virus more quickly.
[0017] In particular, the antiviral roughness is irregularly formed.
[0018] In particular, the banknote is designed as a freshly printed banknote or unused banknote that has not yet been in cash circulation.
[0019] In particular, the antiviral protective coating's roughness creates a multitude of raised and / or recessed areas, thus creating a texture. This texture can effectively counteract viruses.
[0020] In particular, in addition to its antiviral function, the protective varnish also provides protection against mechanical influences on the banknote.
[0021] Preferably, the protective coating with the antiviral roughness has an elongated surface of at least 80%, preferably at least 100%, in particular at least 120%, and more particularly at least 150%. The antiviral roughness with the elongated surface increases the virucidal effect of the protective coating.
[0022] Preferably, the protective coating with the antiviral roughness has a maximum stretched surface area of 500%. Excessively roughened surfaces can lead to increased susceptibility to dirt. A maximum stretched surface area of 500% can effectively limit the contamination of the banknote.
[0023] The stretched surface area (Sdr) describes the relationship between an ideally flat surface and a real measuring surface and is therefore a measure of the roughness of the surface. For rough surfaces, the real surface area is significantly larger than the ideally flat or smooth surface. The stretched surface area is also known as the actual surface area or actual surface area ratio or developed interface ratio and is described, for example, in the DIN EN ISO 25178 series of standards, which concerns areal roughness measurement. The stretched surface area is the percentage of additional area that is added to the developed area (surface of the measured shape) due to the texture, compared to the area of the measured shape in the direct plan view.
[0024] An ideally flat surface has an actual surface area, or stretched surface area, of 0%. A stretched surface area of 80% is therefore 1.8 times larger than an ideally flat surface. A stretched surface area of 120% is therefore 2.2 times larger than an ideally flat surface.
[0025] Furthermore, it is preferably provided that the antiviral roughness is formed by open pores, and the respective pore openings are formed with a semi-major axis or a diameter of at least 1 µm and at most 20 µm in the plane of the outer surface of the banknote. The open pores allow the desired drying of the viruses to occur even more quickly.
[0026] Furthermore, it is preferably provided that the antiviral protective varnish is formed with a matting agent, wherein a ratio of matting agent to an antiviral active ingredient of the protective varnish is greater than 10:1, in particular by weight. This means that there is one part antiviral active ingredient to at least ten parts matting agent. The matting agent is in particular formed as a filler, silicate, silicic acid, quartz sand, micronized wax comprising zinc and / or PTFE (polytetrafluoroethylene), and / or organic filler. In this case, the matting agent not only reduces the gloss but also leads to greater porosity and / or greater roughness. In an advantageous embodiment, the proportion of matting agent is above 10 percent by weight. In a particularly advantageous embodiment, the ratio of matting agent to antiviral active ingredient is between 10:1 and 20:1, in particular by weight.
[0027] Furthermore, it is preferably provided that the antiviral protective coating is produced with hydrophilic, pre-swollen microparticles. In particular, the protective coating is mixed with hydrophilic, swellable microparticles pre-swollen in water. In the swollen state, the microparticles have a diameter of 2 µm to 30 µm in particular. Due to the temperature development during UV drying, for example from infrared radiation from mercury lamps, the bound water evaporates, resulting in small holes or microcracks in the protective coating at these points, depending on the particle size of the swollen polymer particles and the bound water content. Instead of water, a mixture of water and alcohol can be used to accelerate the drying of the polymers, or a mixture of water and glycerin to slow down the physical drying. This is advantageous because the specific surface area is further increased.Furthermore, this also reduces the barrier effect against migrating active ingredients present beneath or within the protective coating layer.
[0028] Furthermore, it is preferably provided that the antiviral protective lacquer is produced with light-unstable polymer particles. The light-unstable polymer particles can, for example, be a shell-core particle. The core can be designed, for example, as a UV light absorber such as nanoscale titanium dioxide. The shell can, for example, be designed as a light-unstable polymer. The protective lacquer, in particular a UV lacquer, is cured or crosslinked with a very high dose of UV radiation from 250 nm to 400 nm. If polymer particles unstable to UV radiation are used, they decompose and thus become porous. In this case, too, this leads to an advantageous increase in the stretched surface or actual surface of the protective lacquer. The antiviral effect is increased.
[0029] In a further embodiment, titanium dioxide particles of the anatase modification are added to the coating, preferably at a nanoscale, to maintain the transparency of the coating. During UV curing, local degradation of the polymers near the titanium dioxide particles occurs, i.e., crosslinked monomers and prepolymers in the immediate vicinity of the titanium dioxide particles, which in turn leads to structuring on the surface of the protective coating and further increases the virucidal effect of the protective coating.
[0030] In a further preferred embodiment, particles with a high specific gravity in g / cm 3 are used, which is at least twice as high as that of the binder of the protective lacquer. The binder of the protective lacquer has in particular a specific gravity of 0.85 g / cm 3 to 1.0 g / cm 3. These particles sink to the bottom after application, i.e. in the direction of the side of the protective lacquer facing the carrier substrate, and thus form craters on the surface of the protective lacquer. A particular prerequisite is that the size of the particles is smaller than the thickness of the applied protective lacquer layer or of the protective lacquer. The curing of the lacquer film takes place during or after crater formation. An advantageous material is barium sulfate (4.5 g / cm 3 ), as it is also transparent.
[0031] In a further embodiment, particles with a diameter larger than the layer thickness of the protective coating are used. The particles have a diameter of 2 µm to 50 µm in particular. The layer thickness of the protective coating is in particular between 1 µm and 4 µm. These particles sink to the bottom after application, i.e., towards the side of the protective coating facing the carrier substrate, and thus form craters on the surface of the protective coating. A prerequisite is, in particular, that the size of the particles is smaller than the thickness of the applied protective coating layer or the protective coating. An advantageous material is barium sulfate, as it is also transparent.
[0032] Furthermore, it is preferably provided that the antiviral protective coating is produced by emulsifying an alcohol-water mixture. In particular, water, alcohol, and / or a water-alcohol mixture are emulsified as small droplets using a dissolver. The size of the droplets is preferably dependent on the shear rate and / or the interfacial tension of the protective coating. In this case, the protective coating is particularly designed as a UV-drying coating (UV = ultraviolet). During UV drying, small craters form due to evaporation and the dispersion of the droplets. Advantageously, leveling agents are preferably omitted from the coating in order to keep the droplets stable after the shear forces have been applied.
[0033] Furthermore, it is preferably provided that the antiviral protective varnish is produced by dispersing a gas. By dispersing gases such as air, the polymeric varnish layer or the protective varnish becomes locally thinner and, due to trapped µm-sized air bubbles or burst air bubbles on the surface, a crater in the µm range is formed and / or defects in the varnish layer in the µm range occur. A heavy gas such as sulfur hexafluoride is preferably used instead of air, as this can be processed more easily in the printing press, in particular the varnish storage tank or the chambered doctor blade in a flexographic printing press. This prevents air bubbles from floating to the surface.
[0034] Another possibility is to add polyethylene glycol, in particular polyethylene glycol 400 or higher molecular weight microparticles, in particular 1µm to 30µm particle size, to the UV-drying protective varnish in concentrations of 5% to 15%, since the water content of the virus aerosols is absorbed by the polyethylene glycol particles.
[0035] Furthermore, it is preferably provided that the antiviral protective coating is created by microperforation. The microperforation is created in particular by material removal and / or material displacement. The microperforation is created in particular with a needle corona. For example, banknotes coated with the protective coating and UV-cured, preferably still in sheet form, as well as before the individual banknotes are cut, can be processed using the needle corona to reliably create the roughness.
[0036] Furthermore, it is preferably provided that the antiviral protective coating is formed with transparent polyurethane particles or polymethyl methacrylate (PMMA) particles. For this purpose, polyurethane beads in the range of 5 µm to 30 µm in size are mixed into the protective coating to create greater roughness and porosity.
[0037] Furthermore, it is preferably provided that the antiviral protective coating is formed with a photosensitizer that releases singlet oxygen upon irradiation and / or is formed with nano-titanium dioxide in the anatase modification, which releases singlet oxygen upon irradiation. The irradiation occurs in particular in the UV and / or short-wave VIS range. During irradiation, the singlet oxygen is generated, in particular by photocatalysis. The singlet oxygen has virucidal properties.
[0038] Additionally or alternatively, the ink-receiving layer of a polymer or hybrid substrate may also contain particles or elements that increase roughness. A standard varnish can then be used for the final coating, i.e., after printing. The particles will still protrude even after the final coating, since the protective varnish is applied in a thinner layer, for example, from 0.5 µm to 3 µm.
[0039] Alternatively, the ink-receiving layer can be applied in a structured manner between the carrier substrate and the protective coating to create the roughness or the desired structure with an enlarged surface. This can also be applied in combination with one or more non-structured ink-receiving layers. The desired structures are created, for example, by screen printing, e.g., a 64-inch screen with 10% area coverage, or by autotypical gravure printing with varying cell depths, or by inkjet printing. The roughness of the protective coating results from a partially varying layer thickness of the ink-receiving layer and / or additional particles contained in the ink-receiving layer, which are preferably thicker than the thickness of the applied protective coating.
[0040] In a further advantageous embodiment, the antiviral roughness is carried out by means of the intaglio printing process as so-called blind embossing, i.e. printing without inking the printing plate in these areas, or as intaglio printing with transparent white. In this case, the intaglio printing plate is provided with a uniform or irregular engraving with deeper areas, preferably in a range of 2 µm to 30 µm, in particular 5 µm to 25 µm, in particular outside the visually visible intaglio printing motifs, preferably greater than or equal to 1 mm, in particular greater than or equal to 3 mm, at a distance from these visually visible motifs. By means of registered inking of the printing plate using a stencil roller or plate, it can be achieved that in the case of blind embossing the inking of the printing plate only occurs for the visually visible intaglio printing motifs.In the case of visually invisible printing areas, these areas can be inked with the transparent, visually invisible ink using an additional stencil cylinder or stencil plate. The spacing of at least 1 mm, preferably 3 mm, between the visually visible inkjet motifs and the visually invisible microstructure of the substrate enables a clean transition between the visually visible motif and the visually invisible microstructure of the substrate, which is difficult due to the wiping process after inking the printing plate to remove excess ink from the printing plate.The area of the carrier substrate which has the microstructuring produced by means of the intaglio printing process leads, due to the high contact pressure during steel intaglio printing, to a raised, visually invisible structure on the printing side and to a depression on the opposite side and thus also to the desired enlargement of the stretched surface.
[0041] Since the embossing using the inkjet printing process on polymer substrates is usually not as pronounced as on cotton substrates, microstructuring on polymer substrates is preferably carried out using a visually invisible transparent inkjet printing process.
[0042] However, if a photocatalytic paper is used as the carrier substrate, the coating can also contain a matting agent to create open porosity. The matting agent can also be applied in a structured manner.
[0043] Furthermore, it is preferably provided that the antiviral protective coating is formed with nanosilver, silver salt, and / or silver phosphate glass. Silver salt and / or silver phosphate glass exhibits an antiviral and antibacterial effect. In combination with a rough surface or the antiviral roughness of the protective coating, viruses are combated even more effectively.
[0044] Furthermore, it is preferably provided that the antiviral protective coating is formed with antiviral metal ions. Metal ions, such as singly positively charged copper ions (Cu(I) ions), exhibit antiviral properties. Together with the antiviral roughness of the protective coating, viruses are combated even more effectively.
[0045] Furthermore, it is preferred that the antiviral protective coating be formulated with 3-iodo-2-propynyl butylcarbamate. The advantage here is that these compounds can also effectively kill fungi, for example. This makes the banknote even more secure to provide.
[0046] Furthermore, it is preferred that the antiviral protective coating be produced as a UV-curing textured coating or sand coating using screen printing. This allows the surface of the protective coating to be made even rougher, thus enhancing the antiviral effect.
[0047] Furthermore, it is preferred that the antiviral protective coating be made hydrophobic, particularly by using water-repellent wax crystals. This can protect the protective coating from microbial attack (lotus effect). The advantage of this is that the surface is made hydrophobic, reducing the adhesion between deposits and the surface.
[0048] Furthermore, it is preferably provided that, after a printing process in which at least one of the two security elements is applied, and before the application of the protective varnish, the banknote has a smooth front side and a rough back side, wherein the smooth front side is formed with the antiviral roughness after the application of the antiviral protective varnish. The rough back side is formed, in particular, by an impression roller or a counter-pressure element during the printing of the banknote, in particular by gravure printing.
[0049] Furthermore, it is preferably provided that the carrier substrate of the banknote is designed as a cotton substrate and the stretched surface of the smooth front side of the banknote with the cotton substrate is at least 100%, preferably at least 120%, more preferably at least 150%.
[0050] Furthermore, it is preferably provided that the carrier substrate of the banknote is designed as a polymer substrate or hybrid substrate.
[0051] In particular, the carrier substrate of the banknote is designed as a polymer substrate and the stretched surface is in particular at least 50%, preferably at least 80%, in particular at least 100%, or the carrier substrate of the banknote is in particular designed as a hybrid substrate and the stretched surface is in particular at least 80%, preferably at least 100%, in particular at least 120%.
[0052] Preferably, the carrier substrate can also contain an antiviral agent. This antiviral agent can then diffuse through the protective coating.
[0053] The protective varnish is preferably transparent.
[0054] The invention also relates to a method. In the method according to the invention, a banknote is produced according to one of the aforementioned embodiments.
[0055] In the method according to the invention, a banknote is produced or manufactured with a carrier substrate, at least two security elements, and a protective varnish. At least one of the two security elements is designed as a print. Furthermore, the print is formed between the carrier substrate and the protective varnish. The outer surface of the banknote is formed by the protective varnish, and the carrier substrate is at least partially surrounded by the protective varnish. Furthermore, the protective varnish protects the print and the carrier substrate. The protective varnish is designed as an antiviral protective varnish, and an antiviral roughness is formed on the outer surface.
[0056] Preferably, the antiviral protective varnish is produced with hydrophilic pre-swollen microparticles.
[0057] Furthermore, the antiviral protective varnish is preferably produced with light-unstable polymer particles.
[0058] Furthermore, the antiviral protective varnish is preferably produced by emulsifying an alcohol-water mixture and / or by dispersing a gas.
[0059] Furthermore, the antiviral protective varnish is preferably produced by microperforation.
[0060] The invention also relates to the use of a banknote according to the invention, which has a protective varnish and an antiviral roughness on the outer surface of the protective varnish, as an antiviral article.
[0061] The preferred embodiments and their advantages presented with reference to the banknote according to the invention apply accordingly to the method according to the invention and the use according to the invention. The preferred embodiments and their advantages presented with reference to the method according to the invention and the use according to the invention apply accordingly to the banknote according to the invention.
[0062] Further features of the invention emerge from the claims, the figures and the description of the figures.
[0063] Embodiments of the invention are explained in more detail below with reference to a schematic drawing.
[0064] Showing: Fig. 1 shows a schematic top view of an embodiment of a banknote according to the invention with a carrier substrate and an antiviral protective varnish having an antiviral roughness on the outer surface; Fig. 2 shows a schematic sectional view of an embodiment of the banknote with the antiviral protective varnish on both main sides of the carrier substrate; Fig. 3 shows a schematic detailed sectional view of an embodiment of the antiviral protective varnish with an antiviral roughness created by a filler; Fig. 4 shows a schematic detailed sectional view of an embodiment of the antiviral protective varnish with an antiviral roughness created by open pores; Fig. 5 shows a schematic profile view of an embodiment of the antiviral protective varnish with an antiviral roughness created by fillers; and Fig.6An Abbott curve of an embodiment of the antiviral protective coating with an antiviral roughness created by open pores.
[0065] In the figures, identical or functionally identical elements are provided with the same reference symbols.
[0066] Fig. 1 shows a banknote 1 with a carrier substrate 2, a first security element 3, a second security element 4 and a protective varnish 5.
[0067] The carrier substrate 2 can be a paper substrate, in particular a cotton paper substrate, for example, supplemented with other natural or synthetic fibers. However, the carrier substrate 2 can also be a polymer substrate or a film composite substrate.
[0068] The paper fibers in cotton paper are mainly formed as cotton noils, optionally with additions of other natural fibers or synthetic fibers, which are fixed by means of mass sizing and / or surface sizing.
[0069] The carrier substrate 2 can also be designed as precoated cotton paper. This is designed analogously to cotton paper, but with an additional surface coating, which is applied in the paper machine or separately and is based on acrylates, polystyrene-acrylates, and / or polyurethanes.
[0070] Furthermore, the carrier substrate 2 can be designed as a polymer substrate. In this case, a film core based, for example, on biaxially stretched PET films (PET - polyethylene terephthalate) with an ink-receiving layer on both outer sides that is opaque in some areas and optionally transparent in other areas.
[0071] Furthermore, the carrier substrate 2 can also be designed as a hybrid substrate. This is designed analogously to the paper substrate, with a thin transparent film laminated on both sides and the outer sides of the film additionally provided with a transparent ink-receiving layer.
[0072] The carrier substrate 2 may also consist of a transparent polymer core and outer paper layers bonded to the polymer core. Bonding is achieved, for example, by polymer melting.
[0073] The first security element 3 is designed, for example, as a print 6, for example as an image or inscription.
[0074] The second security element 4 is designed, for example, as a further print, printing element, security thread, security patch, watermark or hologram.
[0075] It is also possible for the banknote 1 to have yet another print on the protective varnish 5. This further print can be designed, for example, as a continuous numbering pattern. Additionally or alternatively, the carrier substrate 2 may also have an area recessed from the protective varnish 5, in which a continuous numbering pattern is applied directly to the carrier substrate 2.
[0076] The protective coating 5 can be either a water-based or a solvent-based coating. In particular, the protective coating 5 is designed as a UV-curing coating (UV - ultraviolet radiation).
[0077] The protective lacquer 5 is formed at least in regions, in particular over the entire surface, indirectly or directly on the carrier substrate 2.
[0078] The protective varnish 5 has in particular a layer thickness of 0.5 µm to 3 µm.
[0079] Furthermore, the protective coating 5 has an appearance or feel that is matt-glossy or smooth-rough.
[0080] In addition to the antiviral roughness, the protective coating 5 can be formed with further antiviral chemical agents.
[0081] The other antiviral chemical agents are preferably integrated into the protective coating 5.
[0082] In particular, the other antiviral chemical active ingredients exhibit a homogeneous distribution in the protective coating 5.
[0083] The additional antiviral agents can be nanosilver, silver salts, and / or silver phosphate glass, for example. Virucidal metal ions such as copper, cobalt, and / or zinc can also be added as a supplement or alternative.
[0084] In particular, the use of a catalytic antiviral agent is envisaged, i.e., a substance that continuously generates the active ingredient catalytically without being consumed. The resulting longer effectiveness of the antiviral property allows Banknote 1 to remain in circulation for a longer period before it is withdrawn from circulation, for example, by a central bank and replaced with a new banknote.
[0085] In particular, it is also intended to form the protective lacquer 5 with an increased refractive index of at least 1.4. This allows micro-optical elements, such as microlenses, to be clearly visible despite the coating with the protective lacquer 5.
[0086] Furthermore, the protective varnish 5 is applied in particular as a UV-curing structural varnish or sand varnish using the screen printing process.
[0087] According to the exemplary embodiment, the protective lacquer 5 is formed on all sides of the carrier substrate 2. In the exemplary embodiment, the carrier substrate is thus completely surrounded by the protective lacquer 5 and is thus also seamlessly protected.
[0088] In an embodiment not shown, the protective varnish 5 can also be applied only at areas particularly worthy of protection, i.e., areas where the mechanical stress and / or viral load is highest. Areas with the highest viral load are, for example, areas where the banknote is typically gripped with the fingers.
[0089] The protective varnish 5 has an outer surface 7. According to the exemplary embodiment, the outer surface 7 of the protective varnish also describes the outside of the banknote 1.
[0090] Furthermore, the protective varnish 5 has an antiviral roughness 8 on the outer surface 7.
[0091] The protective lacquer 5 with the antiviral roughness 8 is formed with an actual surface or an extended surface of at least 80%, preferably at least 100%, in particular at least 120%, further in particular at least 150%.
[0092] The stretched surface area may also depend on the type of carrier substrate 2. Thus, for a polymer substrate, the stretched surface area may be at least 50%, preferably at least 80%, in particular at least 100%. The polymer substrate is in particular formed entirely from polymer.
[0093] In a hybrid substrate having a paper core with at least partial polymer coating, the stretched surface can be at least 80%, preferably at least 100%, in particular at least 120%.
[0094] With a cotton substrate, a distinction can also be made between a smooth front side and a rough back side. The difference in roughness between the front and back sides can be explained, for example, by the intaglio printing process used. In the intaglio printing process, a high contact pressure is exerted on the side to be printed in order to transfer the ink to the carrier substrate 2. In order to transfer this contact pressure to the carrier substrate, counterpressure is required on the side opposite the side to be printed, which is exerted, for example, by an impression roller. Due to this counterpressure, the back side, i.e. the counterpressure side of the carrier substrate 2, is rougher than the front side after the intaglio printing process.In particular, it is further provided to form the smooth front side of the carrier substrate 2 with the protective lacquer 5 having the antiviral roughness 8, thereby providing a stretched surface of at least 100%, preferably at least 120%, more preferably at least 150%. In this case, a protective lacquer formulation that significantly increases roughness is preferably used for the front side, and a protective lacquer formulation that increases roughness less, e.g., a standard protective lacquer with an antiviral active ingredient, is preferably used for the inherently rougher back side.
[0095] Due to the antiviral roughness 8, viruses present on the protective coating 5 dry out more quickly and are therefore less contagious than if the drying out is not promoted by the roughness 8.
[0096] Fig. 2 shows a schematic cross-sectional view of banknote 1. The protective varnish 5 is shown on both sides of the carrier substrate 2.
[0097] Between the carrier substrate 2 and the protective lacquer layers 5, the printing 6 or an imprint is arranged on one side of the carrier substrate 2 and on an opposite side of the carrier substrate 2, a further printing 9 or a further imprint is arranged as the second security element 4.
[0098] According to the embodiment, the print 6 is designed as an intaglio print and the print 9 is designed as an offset print.
[0099] The protective lacquer 5 is preferably directly adjacent to the carrier substrate 2, except for the locations at which the first security element 3 and the second security element 4 are formed.
[0100] Fig. 3 shows an exemplary embodiment in a schematic sectional view. The protective coating 5 comprises a filler 10. On the outer surface 7, elevations 11 are formed by protruding fillers 10, and craters or depressions 12 are formed by sinking fillers 10. This results in the antiviral roughness 8 on the outer surface 7.
[0101] The filler 10 can be formed, for example, as a matting agent, hydrophilic pre-swollen microparticles, light-unstable polymer particles, alcohol-water mixture, polyethylene glycol 400, gas and / or polyurethane elements.
[0102] Fig. 4 shows a further exemplary embodiment in a schematic sectional view. The protective lacquer 5 or the protective lacquer layer has open pores 13 and closed pores 14. The open pores 13 can also be described as craters. The open pores 13 and / or the closed pores 14 are caused by gas-filled bubbles and / or by small defective coatings on the banknote 1 caused by escaping gas. The antivirally effective roughness and defects within the protective lacquer are visible, which lead to the porosity, i.e., the open pores 13 and / or the closed pores 14.
[0103] The closed pores offer the advantage that, upon subsequent wear of the protective lacquer 5 or the protective lacquer layer or the binding agent of the protective lacquer layer, they move to the outer surface 7 and thus contribute to the roughness. Furthermore, the barrier against diffusible active substances is lower at this point.
[0104] Banknotes 1 make it possible to shorten the effectiveness of viruses, as the antiviral roughness 8 causes them to dry out faster than with known, smooth banknotes without antiviral roughness.
[0105] Fig. 5 shows a compressed sectional profile of banknote 1. Fillers 10 or particles are added to the protective lacquer 5, which create or enhance the antiviral roughness 8. The fillers 10 are, in particular, spherical and compressed in the transverse direction of the figure only for simplified representation. Furthermore, no separation is shown between the protective lacquer 5 and the carrier substrate 2. Also not shown is the fact that the fillers 10 are coated with the protective lacquer 5 in the exemplary embodiment. The units of the axes of the diagram in which the profile is shown are µm.
[0106] Fig. 6shows an Abbott curve 15 for a banknote 1 with a polymer substrate as the carrier substrate 2. The Abbott curve 15 has a histogram 16, which describes the distribution of the elevations of the protective varnish 5. Furthermore, the Abbott curve 15 shows a cumulative sum histogram 17, in which the number of individual bins is summed.
Claims
1. Banknote (1) having a carrier substrate (2), at least two security elements (3, 4) and a protective varnish (5), where at least one of the two security elements (3, 4) takes the form of a print (6), and where the print (6) is formed between the carrier substrate (2) and the protective varnish (5), where the protective varnish (5) forms the outer surface (7) of the banknote (1) and the carrier substrate (2) is at least partly surrounded by the protective varnish (5), where the protective varnish (5) is designed to protect the print (6) and the carrier substrate (2), and where the protective varnish (5) takes the form of an antiviral protective varnish, characterized in that the protective varnish (5) has, on the outer surface (7), a roughness (8) that has an antiviral effect.
2. Banknote (1) according to Claim 1, wherein the protective varnish (5) having the antiviral roughness (8) has an extended surface area of at least 80%.
3. Banknote (1) according to Claim 1 or 2, wherein the antiviral roughness (8) is formed by open pores (13) and the respective opening of the pores (13) with a semimajor axis of at least 1 µm and at most 20 µm is formed in the plane of the outer surface (7) of the banknote (1).
4. Banknote (1) according to any of the preceding claims, wherein the antiviral protective varnish (5) is formed with a flatting agent, where a ratio of flatting agent to an active antiviral ingredient of the protective varnish is greater than 10:1.
5. Banknote (1) according to any of the preceding claims, wherein the antiviral protective varnish (5) is formed with polyurethane particles (10) or polymethylmethacrylate particles (10).
6. Banknote (1) according to any of the preceding claims, wherein the antiviral protective varnish (5) is formed with a photosensitizer which releases singlet oxygen on irradiation and / or is formed with nano-titanium dioxide in the anatase modification, which releases singlet oxygen on irradiation.
7. Banknote (1) according to any of the preceding claims, wherein the banknote (1), after a printing operation in which at least one of the two security elements (3, 4) is applied and prior to the application of the protective varnish (5), has a smooth front side and a rough reverse side, where the smooth front side is formed with the antiviral roughness after the antiviral protective varnish (5) has been applied.
8. Banknote (1) according to Claim 7, wherein the carrier substrate (2) of the banknote (1) takes the form of a cotton substrate and the extended surface area of the smooth front side of the banknote with the cotton substrate is at least 100%.
9. Banknote (1) according to Claim 1 or any of Claims 3 to 6, wherein the carrier substrate (2) of the banknote (1) takes the form of a polymer substrate and the extended surface area is at least 50%, or the carrier substrate (2) of the banknote (1) takes the form of a hybrid substrate and the extended surface area is at least 80%.
10. Method of producing a banknote (1) having a carrier substrate (2), at least two security elements (3, 4) and a protective varnish (5), where at least one of the two security elements (3, 4) takes the form of a print (6), and where the print (6) is formed between the carrier substrate (2) and the protective varnish (5), where the protective varnish (5) forms the outer surface (7) of the banknote (1) and the carrier substrate (2) is at least partly surrounded by the protective varnish (5), where the protective varnish (5) is designed to protect the print (6) and the carrier substrate (2), and where the protective varnish (5) takes the form of an antiviral protective varnish and, on the outer surface (7), a roughness (8) that has an antiviral effect is formed.
11. Method according to Claim 10, wherein the antiviral protective varnish (5) is produced with hydrophilic preswollen microparticles (10).
12. Method according to Claim 10 or 11, wherein the antiviral protective varnish (5) is produced with light-unstable polymer particles (10).
13. Method according to any of Claims 10 to 12, wherein the antiviral protective varnish (5) is produced by emulsifying incorporation of an alcohol-water mixture (10) and / or by dispersing operation of a gas (10).
14. Method according to any of Claims 10 to 13, wherein the antiviral protective varnish (5) is produced by microperforation.
15. Use of a banknote (1) according to any of Claims 1 to 9, having a protective varnish (5) and, on the outer surface (7) of the protective varnish (5), an antiviral roughness (8), as antiviral article.