Reflective coating for reflectors of an optical encoder and optical encoders manufactured in this way

DE602021021425T2Active Publication Date: 2024-11-06CODECHAMP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602021021425
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-06-30
Filing Date
2021-06-18
Publication Date
2024-11-06
Estimated Expiration
2041-06-18

AI Technical Summary

Technical Problem

Existing optical encoders face challenges in maintaining a high and durable reflection coefficient over time while ensuring easy manufacturing and controlled costs, with existing reflective surfaces prone to modification and light loss.

Method used

A reflective coating comprising a flat glass strip with a gold or gold alloy layer having a reflection coefficient greater than 96% and a protective layer, adhered using chromium or silver alloys, is applied to the optical encoder's reflective surfaces, ensuring minimal size impact and easy handling.

Benefits of technology

The solution provides a durable and high reflection coefficient that maintains initial reflection values over time, reducing light loss and ensuring accurate angular position measurements without altering the sensor's bulk, while being cost-effective and easy to implement.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a reflective coating of the reflection means of an optical encoder as well as the optical encoder thus produced.

[0002] An optical encoder, in particular a so-called high-resolution optical encoder, is a device for determining the angular position of a moving object relative to another. For this purpose, according to a type of optical encoder described in EP-B-964 226, an optical beam is emitted towards reflective means ensuring the deflection of the light beam towards beam reception means. A rotating disk whose angular position is to be determined is placed between the beam emission and reception means and the light beam reflection means. The disk comprises tracks defined by opaque zones and translucent zones, characteristic of each disk. It also comprises diffraction means formed by a reticle. Openings form the reflective means for diffracting the light beam between the emission and reception means.These openings comprise at least two surfaces arranged angularly relative to the plane in which the means for emitting and receiving the light beam are located. The light beam passes successively over the two surfaces between emission and reception, the optical path of the beam also passing at least once through the rotating disc and at least once through the reticle ensuring diffraction.

[0003] Here, the reflective surfaces are arranged angularly, for example at 45°. If such an encoder allows, in a reduced space requirement, to measure the angular position of a rotating object, it is essential to ensure optimal reflection of the light beam between the surfaces. In other words, there must not be a change over time in the reflection coefficient between the surfaces, for the wavelength concerned, knowing that the reflection coefficient must be as high as possible, in order to avoid any light loss during the path of the optical beam. However, here, the reflective surfaces are obtained, according to one embodiment, by machining openings of given shapes in a block of material and by polishing the surfaces. Alternatively, prisms are positioned in the openings and define the reflective surfaces arranged angularly.US-A-2013 / 221212 discloses a reflection surface integrated into the sensor body. The surface is formed by a layer of corrosion-resistant noble metal such as gold and fixed on a layer of another metal, so that the whole does not protrude from the sensor surface. EP-A-2006712 describes a reflection surface of an optical encoder based on chromium and titanium silicide as an adhesion material to gold to produce a coating with asperities allowing the phase change of the reflection on the coating.

[0004] It is therefore not easy with state-of-the-art reflective surfaces to obtain minimal, long-lasting reflection loss while maintaining easy manufacturing at a controlled cost.

[0005] The invention aims to address this need by proposing a coating of the reflective surfaces of an optical sensor ensuring a high and durable reflection coefficient over time, easy implementation, without modifying the initial size of the sensor, at a controlled cost.

[0006] To this end, the invention relates to a reflective coating of the means for reflecting a light beam emitted by a light source of an optical encoder, the reflection of the light beam being directed towards a photoreceptor, characterized in that the coating comprises at least one flat glass lamella, one face of which forms a connecting means on a part of the reflection means of said optical encoder, said lamella being provided, on the face opposite the face forming a connecting means, with at least one layer of at least one material having a reflection coefficient greater than 96% for the wavelengths of the light beam to be reflected, said material having a reflection coefficient greater than 96% being gold or a gold-based alloy and in that it comprises a layer of material for protecting the gold layer.

[0007] This produces a reflective coating that incorporates the bonding means on the reflection means of the optical encoder. The use of a glass slide, in addition to not significantly modifying the size of the reflection means, facilitates the handling and installation of the coating. Since the reflective material is present from the start on the glass slide, once the latter is fixed to the reflection means, the latter is directly operational, the protective layer making it possible to maintain the initial reflection value over time. In addition, a glass slide makes it possible to obtain a perfectly flat surface on which it is possible to deposit a uniform layer of reflective material of a controlled thickness.

[0008] According to advantageous but not mandatory aspects of the invention, such a reflective coating may comprise one or more of the following characteristics: the glass face opposite the face forming a bonding means receives a layer of a material having physicochemical characteristics such that it adheres, on the one hand, to said glass face and, on the other hand, that it adheres to another material or to a mixture or alloy of materials having a reflection coefficient greater than 96% for the wavelengths of the light beam to be reflected. The material ensuring the bond between the face and the reflective material is chromium or a chromium alloy. The material having a reflection coefficient greater than 96% is silver or a silver-based alloy. The glass slide and the layers of materials are fixed on a support formed by a polymer sheet.

[0009] The glass strip and material layers are pre-cut on the sheet to the desired dimensions corresponding to those of the reflective coating.

[0010] The invention also relates to an optical encoder equipped with at least one reflection means conforming to one of the preceding characteristics.

[0011] The invention will be better understood and other advantages thereof will appear more clearly on reading the description which follows, given solely by way of non-limiting example and made with reference to the appended drawings in which: [ Fig. 1 ] illustrates a perspective view of the part of an optical encoder comprising reflection means according to an embodiment of the invention, [ Fig. 2 ] is a diagram, on another scale, illustrating the operating principle of an optical encoder according to an embodiment of the invention, [ Fig. 3 ] is a simplified and enlarged perspective view of a coating of a means of reflection of the figure 1 And [ Fig. 4 ] is a perspective view, on another scale and simplified, of the method of supplying a set of coverings as shown in the figure 3 .

[0012] There figure 1 is a representation of a part of an optical encoder, referenced 1, which corresponds to the part of the optical encoder receiving the reflection means, referenced 2. Part 1 is configured in a circular volume open at the top when looking at the figure 1 This upper opening allows the other constituent elements of an optical encoder to be received, as schematically illustrated in figure 2 . The bottom 3 of the part 1 is flat and, in the example, equipped with three rectangular through cutouts 4. Alternatively, the number of cutouts is other than three. The walls 5 of these cutouts 4 corresponding to the short sides of the rectangular cutouts 4 are inclined at 45° relative to the main plane P of the bottom 3. The inclination of the walls 5 is oriented so that the opening of the angle defined by the walls 5 is located on the internal face 6 of the bottom 3, therefore the face oriented in the direction of the other constituent elements of the optical encoder when the latter are in place above the part 1.

[0013] As is evident from the figure 1 , in this type of optical encoder, the main longitudinal axes A of the cutouts 4 are oriented angularly with respect to each other. These cutouts 4 are distributed on the bottom 3, between the center C of the bottom 3 and the peripheral wall 7 limiting the bottom 3. Thus, the cutouts 4 and the inclined walls 5 define the reflection means 2. In a variant not illustrated, the number, arrangement, shape and dimensions of the cutouts 4 are different.

[0014] There figure 2 schematically represents the operation of such an optical encoder and, in particular, the role of the reflection means 2. A light-emitting diode 8 emits, advantageously in the infrared, a light beam F which passes through a glass reticle 9 before striking one of the walls 5 which deflects it and returns it to the other wall 5 of a cutout 4, in a direction parallel to the plane P of the bottom 3, due to the 45° inclination. The beam F passes back through the glass reticle 9 and through a glass disc 10 before striking photoreceptors 11. The disc 10 is rotatable, with opaque areas and translucent areas. The glass reticle 9 ensures the diffraction of the beam F. A detailed operation of this type of optical encoder is, for example, provided by EP-B-964 226.

[0015] There figure 2 illustrates the role of the walls 5 which ensure the reflection in defined directions of the optical beam F. Such a generally U-shaped path of the beam F makes it possible to position in the optical encoder the emitter 8 and the receiver 11 of the light beam F on the same plane, which allows a gain in the total size of the encoder, in particular in thickness.

[0016] It is noted that the reflection of the beam F between the walls 5 must be done constantly, without any optical loss and by precisely respecting the parallelism of the optical paths of the beam F between the transmitter 8 and one wall 5 and between the other wall 5 and the receiver 11, to guarantee the accuracy of the measurement. The characteristics of the reflection must be constant over time, without alteration or modification, regardless of the number of measurements carried out, the environmental conditions such as, for example, thermal differences, vibrations, shocks and this over the entire lifetime of an optical encoder knowing that this lifetime is at least 20 years.

[0017] Each wall 5 is thus provided with a reflective coating 12. This coating 12 is particularly visible at the figure 3 . According to the invention, the coating 12 comprises a flat glass lamella 13. Such a lamella 13 has a thickness of between 0.15 mm and 0.25 mm, advantageously close to 0.2 mm. Insofar as the inclined planes are machined with an optimal angle to achieve the path of the light beam, the coating must have a minimal impact on the initial reflection, therefore a minimal thickness in order to limit the optical imperfections of reflection, while being sufficiently strong and rigid. Therefore, a thickness of the glass lamella close to 0.2 mm is retained. A lower face 14, looking at the figure 3 , of the strip 13 is adapted to be fixed on a wall 5. The fixing is done by gluing, advantageously with an adhesive polymerizable under ultraviolet. Such an adhesive must be fluid to be used in a thin layer so as not to affect the total thickness of the coating. This adhesive must withstand shocks, vibrations, large thermal amplitudes, for example from -40°C to +150°C, be durable over time taking into account the lifespan of an encoder which is at least 20 years and be sufficiently flexible to accommodate the different thermal expansions between the glass of the strip and the metal of the inclined wall. Furthermore, the polymerization of the adhesive must be almost immediate, typically of the order of 15 s once the strip is in position and the user wishes to carry out the gluing. Such an adhesive is, for example, a transparent acrylic-based adhesive marketed by the company PANACOL.Alternatively, another glue is used, for example one that is heat-curable at ambient temperatures, generally between 20°C and 25°C.

[0018] Face 15, opposite face 14, is schematically represented in figure 3 by hatching, for greater readability. The face 15 receives a layer of a material 16 having physicochemical characteristics such that it adheres, on the one hand, perfectly to the glass and, on the other hand, that it adheres to another material or to a mixture or alloy of materials having a reflection coefficient greater than 96% for the wavelengths concerned, namely in this case wavelengths between 800 nm and 900 nm. Here, the material 16 is chromium. Alternatively, it is a material or an alloy of materials allowing adhesion to glass and also exhibiting adhesion to gold.

[0019] It is understood that material 16, in this case chromium, is chosen not only as having optimal adhesion to the glass but also as a function of material 17 chosen for its high reflection coefficient. Here, material 17 is 99.99% pure gold whose reflection coefficient at 850 nm is 97.8%.

[0020] The chromium 16 layer is fixed on the face 15 by techniques known per se, for example by deposition under evaporation. Such a technique makes it possible to produce a chromium 16 layer of between 0.05 micron and 0.1 micron.

[0021] The gold layer 17 is also deposited using this technique and it also has a thickness of between 0.05 microns and 0.1 microns. In other words, the cumulative thicknesses of the lamella 13, the chromium 16 and gold 17 layers are of the order of 0.2 mm, which does not significantly modify the thickness of the walls 5 and therefore the path of the beam F.

[0022] Gold is chosen to produce the layer of reflective material 17 because, in addition to a high reflection coefficient, namely greater than 96% for wavelengths between 800 nm and 900 nm, therefore in the infrared, this metal is inert, almost insensitive to corrosion, totally non-magnetic, ductile, malleable and easily polished. It is used to obtain a reflective, regular, homogeneous flat surface, while preserving the initial flatness, close to mirror polish, of glass. Because gold is a malleable and soft metal at room temperature, a layer 17 of gold is all the more sensitive to marking and shocks the thinner it is. A patination phenomenon is also observed over time. Advantageously, the gold layer 17 is coated with a layer of protective material 18. Indeed, it is necessary to avoid any marking of the surface of the layer 17 and any oxidation or patination effect of the gold layer 17.In the absence of a protective layer 18, a degradation of the reflection is observed over time, due to the tarnishing of the layer by patina and / or oxidation phenomena. Since maintaining the reflection coefficient over time is an important point for the reliability of the encoder, the presence of a protective layer 18 making it possible to maintain a constant reflection coefficient over a period of at least 20 years is necessary. It is therefore advantageous to deposit a layer 18 of a protective material on it. The latter must be completely transparent and optically neutral so as not to affect the path of the beam, either by deflecting it and / or by absorbing part of it. Alumina meets these requirements. For this, a layer of alumina with a thickness of around 0.015 mm is deposited on the layer 17. Such a thickness of the protective layer 18 ensures optimal protection without affecting the nominal thickness of the coating.Alternatively, it is another material or a composite material, for example silica, which can be used to protect, for example, other deposits of a material other than gold, for example silver-based deposits.

[0023] The dimensions of the coating 12, therefore of the glass lamella 13 coated with the chromium layer 16, the gold layer 17 and the protective layer 18 are generally between 2.5 mm and 3 mm wide and 2.5 mm to 3 mm long with a thickness of less than 0.3 mm.

[0024] It is therefore understood that the handling, transport and storage of such coatings 12 are not easy. Consequently, as is apparent from the figure 4 , the coatings 12 are produced prior to the implementation of the invention by pre-cutting in a sheet 19 which defines a means of storage and transport of the coatings 12. This sheet 19 is obtained from a sheet of polymers on which, by techniques known per se such as deposition by evaporation, the different layers 13, 16 to 18 constituting the coating 12 are deposited. By sawing, each coating 12 is then pre-cut to the desired dimensions. Here, the pre-cut coatings 12 are arranged in parallel rows. Each coating 12 being adjacent to another coating 12, the separation between two coatings 12 being materialized by a cutting line, in order to be able to take a coating 12 individually without risk of damaging a neighboring coating 12, as illustrated in figure 4. Alternatively, the arrangement of the coatings 12 on the sheet 19 is different. Such sheets 19 are produced beforehand, by techniques known per se from specialized suppliers.

[0025] It is then easy to take the pre-cut coverings 12 from the sheet 19 and position them on the walls 5. The fixing, as indicated previously, is carried out by gluing, advantageously with polymerization of the glue under UV. Alternatively, another type of glue is used, for example, a glue polymerizable at room temperature, in the presence or absence of an activator.

[0026] The coating 12 is positioned on the wall 5, during the bonding fixing step, so that it covers the entire surface of the wall 5. Thus, when the beam F strikes the reflective layer 17, even if the beam F is not perfectly in the center of the reflective layer 17, this does not affect the optical path of the beam F towards the other wall 5.

[0027] In other embodiments of the invention, the reflective coating having a reflection coefficient of at least 96% at the wavelengths considered is obtained by machining, polishing the material constituting the walls 5. In such a case, said walls 5 are, for example, made of another metal or metal alloy or material having similar optical properties. The material having a reflection coefficient greater than 96% is gold or a gold alloy with an expansion similar to that of glass. ;

Claims

1. A reflective coating (12) of means of reflection (2) of a light beam (F) emitted by a light source (8) of an optical encoder, the reflection of the light beam (F) being directed towards a photo receptor (11) characterized in that the coating (12) comprises at least one flat glass blade (13), incorporating the coating, the face (14) of which forms a means of a connection on one part (5) of the means of reflection (2) of said optical encoder, said blade being coated, on the face (15) opposite the face (14) forming a means of connection, of at least one layer of gold or gold alloy (17) having a coefficient of reflection greater than 96% for the wavelengths of the light beam (F) comprised between 800 nm and 900 nm, the blade (13) having a nominal thickness comprised between 0.15 mm and 0.25 mm, and in that the coating comprises a layer of protective material (18) of the gold layer (17), the protective material being transparent, optically neutral and not affecting the nominal thickness of the gold (17) coated blade (13).

2. The coating according to claim 1, characterized in that the face (15) opposite the face (14) forming a means of connection receives a layer of a material (16) having physical and chemical characteristics such that the coating adheres both to the glass face (15) and to another material (17) or to a mixture or to a mixture or alloy of materials having a coefficient of reflection greater than 96% for the wavelengths of the light beam (F) to reflect.

3. The coating according to claim 2 characterized in that the material (16) providing the connection between the face (15) and the reflecting material (17) is chromium or an alloy of chromium.

4. The coating according to claim 2 characterized in that the glass blade (13) and the layers of materials (16 to 18) are attached onto a support formed by a sheet of polymers (19).