Characterization test specimen made of composite material

FR3115604B1Active Publication Date: 2024-11-08SAFRAN AIRCRAFT ENGINES SAS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2020011041
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-28
Publication Date
2024-11-08
Estimated Expiration
2040-10-28

Smart Images

  • Figure 00000010_0000
    Figure 00000010_0000
  • Figure 00000010_0001
    Figure 00000010_0001
  • Figure 00000010_0002
    Figure 00000010_0002
Patent Text Reader

Abstract

Characterization Specimen in Composite Material The invention relates to a characterization specimen (20) made of a composite material comprising a fibrous preform having a weave between a first plurality of yarns and a second plurality of yarns densified by a matrix, the specimen comprising a loading zone (23) located between two clamping zones 24 in the direction of the stress and characterized in that the yarns of the first plurality of yarns of the fibrous preform extending in the direction of the stress have a greater degree of weave in the loading zone than in the clamping zones. Figure for the abstract: Fig. 4
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Composite material characterization test piece Technical field

[0001] The invention relates to the field of composite materials, and more specifically to the preparation of characterization specimens for such composite materials. Prior art

[0002] The preparation of characterization specimens makes it possible to validate the behavior of a material before its use for a technological application.

[0003] However, such a test piece must be perfectly representative of the material that it characterizes, in particular in its loading zone.

[0004] The representativeness of a characterization test piece is difficult to obtain for a composite material, in particular due to the heterogeneity at the microscopic scale of these materials due to their fibrous preform, reinforced by a matrix. These heterogeneities, which have implications on the mechanical properties of the material, make their mechanical behavior difficult to reproduce at the scale of a test piece.

[0005] In particular, it is often observed that the measurements carried out on characterization specimens can be very dispersed, or that the results obtained depend on the dimensions of the specimen. In addition, it is also observed that, when subjected to mechanical stress, such specimens can break at a location other than in the loading zone, in this case the central zone of the specimen. In this case, they are useless for characterizing composite materials because it is the central zone of the specimen which is representative of the material. However, for cost reasons, it is preferable to carry out tests on characterization specimens rather than on complex parts.It is therefore desirable to have test pieces which faithfully reproduce the behaviour of larger composite materials and to take the necessary steps to reduce the stress concentrations which may exist and thus pollute the mechanical characteristics which are supposed to be intrinsic to the material and not to the shape of the test piece. Description of the invention.

[0006] To address this problem, the inventors propose a characterization test piece made of a composite material comprising a fiber preform having a weave between a first plurality of threads and a second plurality of threads densified by a matrix, the test piece comprising a loading zone located between two clamping zones in the direction of the stress and characterized in that the threads of the first plurality of threads of the fiber preform extending in the direction of the ground licitation have a greater fogging in the loading zone than in the clamping zones.

[0007] Such a test piece makes it possible to ensure rupture of the characterization test piece in the stress zone, which makes it possible to reproduce and characterize the behavior of the composite material on the scale of the test piece.

[0008] In one embodiment of a characterization test piece according to the invention, the spacing between the threads of the second plurality of threads of the fiber preform which extend in a direction perpendicular to the stress direction is greater in the clamping zones than in the loading zone.

[0009] In this embodiment, the increased spacing in the clamping zones between the rows of yarns of the second plurality of yarns of the fiber preform makes it possible to increase the fogging in the loading zone compared to the fogging of the clamping zones, and thus, makes it possible to ensure that the rupture of a characterization test piece when the latter is subjected to a stress in the stress direction, takes place in the loading zone.

[0010] In a different embodiment, or in addition to the above embodiment, the tension of the yarns of the first plurality of yarns of the fiber preform in the loading zone is greater than or equal to the tension of the yarns of the fiber preform in the direction of stress in the clamping zones.

[0011] Increasing the tension of the yarns of the first plurality of yarns of the preform of a characterization specimen in the loading zone relative to their tension in the clamping zones makes it possible to increase the fogging in the loading zone, thus making it possible to address the technical problem.

[0012] In an embodiment different from or in addition to at least one of the embodiments described above, the diameter of the yarns of the second plurality of yarns of the fiber preform is larger in the loading zone than in the clamping zones.

[0013] This increase in the diameter of the threads of the second plurality of threads of the fiber preform makes it possible to increase the fogging in the loading zone and thus allows the rupture of a characterization specimen when the latter is subjected to stress to take place in the loading zone.

[0014] This solution also allows simplified weaving of the characterization test piece, since the weaving of the test piece is only modified to increase the spacing between the threads of the second plurality of threads when weaving the loading zone.

[0015] The embodiments presented above each make it possible to increase the embouchure in the loading zone, by modifying a particular weaving parameter.

[0016] The described modes do not present any incompatibility between them, and in certain embodiments of the invention, it is possible to combine the effects of two or three of the embodiments described above in order to produce a characterization test piece according to the invention.

[0017] Changing several of the weaving parameters rather than just one allows the desired difference in weaving to be achieved by varying each of the parameters less significantly than when only one parameter is changed. However, it is observed that, even when all three parameters are changed during the weaving of a test piece, the change only requires adjustment of the weaving conditions at changes between a clamping zone and a characterization zone, which allows relatively easy weaving of the test piece preform to be maintained.

[0018] According to a particular characteristic of the invention, the width of the fiber preform of the characterization test piece is the same in the clamping zones and in the loading zone. In other words, in one embodiment, the first and second plurality of wires of the preform form a rectangular preform.

[0019] The inventors have found that this rectangular test piece geometry makes it possible to avoid stress concentration zones that can occur when the geometry of the characterization test piece is more complex. In particular, the inventors have observed that the so-called "dog bone" shape of the characterization test pieces of the prior art had such stress concentration zones, and that such test pieces sometimes broke between the clamping zones and the loading zone.

[0020] By avoiding stress concentration zones, the creation of fragile points in the test piece is reduced and the rupture of the test piece in the loading zone of the test piece is further promoted, and thus a test piece is obtained whose stress behavior is representative of that of a composite part.

[0021] According to another particular characteristic of the invention, no yarn of the first plurality of yarns is extracted from the fiber preform of the characterization test piece between the clamping zones and the loading zone.

[0022] This makes it possible to improve the continuity of the forces transmitted from the clamping zones when the test piece is stressed and thus avoid the appearance of stress zones when the test piece is stressed.

[0023] In one embodiment, the fiber preform does not include any other yarns added during a step subsequent to its weaving. In one embodiment, no yarn is added to the test piece after the weaving of the fiber preform it includes.

[0024] In one embodiment, each of the first plurality of wires is present in both the clamping zones and the loading zone. In other terms, no yarn of the fiber preform is removed, added or cut in the direction of stress of the test piece. The continuity of the yarns of the first plurality of yarns of the fiber preform makes it possible to avoid the appearance of particular stress zones, which could cause local variations in mechanical properties, and give the test piece a mechanical behavior different from the material it characterizes.

[0025] In one embodiment, the fibrous preform may be woven in two or three dimensions.

[0026] In one embodiment of a test piece, additional material may be added to the test piece, on the outer faces of the clamping areas, thereby forming a layer over and under the clamping areas of the test piece.

[0027] This embodiment makes it possible to prevent a clamping member that may be useful for carrying out a mechanical test from weakening the test piece in the clamping zones. However, such an additional layer is not necessary, because the clamping zone is stronger than the loading zone, and as long as the clamping member does not damage the clamping zone, the test piece will indeed break in the loading zone.

[0028] According to another of its aspects, the invention relates to a method for characterizing a composite material, comprising a step during which a characterization test piece as described above is subjected to loading in the direction of the threads of the first plurality of threads of the fiber preform of said test piece.

[0029] In the application, it is understood that the direction of the threads of the first plurality of threads of the fiber preform is the direction of stress of the characterization test piece. The term "direction of the threads of the first plurality of threads of the fiber preform" is understood to correspond to the direction of these threads averaged over the entire test piece, because weaving requires that the threads of the first plurality of threads are not perfectly straight.

[0030] In one embodiment, the direction of the yarns of the first plurality of yarns of the fiber preform may be the largest dimension of the characterization specimen. Brief Description of the Drawings

[0031] [fig. 1] [fig.l] is a schematic representation of the weaving of a characterization test piece in one embodiment of the invention,

[0032] [fig.2] [fig.2] is a schematic representation of the weaving of a test piece of characterization in one embodiment of the invention,

[0033] [fig.3] [fig.3] is a schematic representation of a test piece of character dog bone-shaped structure according to a geometry of the prior art,

[0034] [fig.4] [fig.4] is a schematic representation of a test piece of character rization according to an embodiment of the invention. Description of the embodiments

[0035] Certain embodiments of the invention will now be described in more detail, in particular by means of figures, but are only particular embodiments of the invention and they should not be considered as limiting the scope of the invention. The figures are not shown to scale, and only represent examples allowing a better understanding of the invention. In particular, the size of the wires as well as the absolute values ​​of the embuvages that can be read in the figures are not representative of reality.

[0036] In a characterization test piece of the invention, it is the loading zone which is representative of the material that the test piece characterizes. For this reason, it is necessary that the loading zone is made up of a fiber preform and a matrix identical to that of the characterized material, but also that the fiber preform has in the loading zone characteristics identical to those of the composite material that it is desired to characterize, and in particular in terms of density, fiber volume ratio, amount of porosity and fogging.

[0037] Ensuring that the rupture of the test piece occurs in the loading zone, during mechanical stress, makes it possible to ensure that the behavior of the test piece is representative of the material of the characterization zone, and therefore of the material that the test piece characterizes.

[0038] The differences between the clamping zones and the characterization zone have no influence on the mechanical behavior of the characterization zone, but make it possible to ensure that the mechanical resistance properties are greater in the clamping zones, and consequently, that the rupture of the test piece takes place in the loading zone.

[0039] For the purposes of the invention, "the weaving" is understood to be the angle formed by the yarns of the first plurality of yarns 1 with the horizontal direction at the locations where the yarns of the first plurality of yarns 1 cross the yarns of the second plurality of yarns 2. The weaving is a parameter which is determined by the weaving conditions as well as the dimensions and the nature of the yarns used to weave the fiber preform.

[0040] The inventors have found that the reduction in fogging in the clamping zones compared to the loading zone ensures that the latter has less mechanical resistance than the clamping zones and therefore ensures that the rupture of the test piece takes place in the loading zone.

[0041] [Fig. 1] schematically represents the weaving of the fiber preform of a test piece 20 in one embodiment of the invention. The test piece comprises a first plurality of threads 1 and a second plurality of threads 2, the weaving of which is shown schematically here. The test piece 20 comprises two clamping zones 24 and a loading zone 23.

[0042] In the embodiment shown, the direction of stress of the test piece corresponds to the horizontal direction, aligned with the direction of the first plurality of threads 1, while the second plurality of threads 2 corresponds to the weft threads. The invention is not limited to this single embodiment.

[0043] The embouchure in the clamping zone 8 and the embouchure in the loading zone 9 are shown schematically in [fig.l].

[0044] As shown in [fig.l], increasing the spacing between the wires of the second plurality of wires 2, in the clamping zone relative to the spacing in the loading zone makes it possible to increase the fogging in the loading zone 9 relative to the fogging in the clamping zone 8.

[0045] [Fig. 2] schematically represents the weaving of the fiber preform of a test piece 20 in one embodiment of the invention. Identical numerical symbols refer to the same as those described in [Fig. 1].

[0046] In the embodiment of [fig.2], the wires of the second plurality of wires are thinner when they are the wires 4 of a clamping zone 24 and thicker when they are the wires 3 of the loading zone 23. The difference in thickness between the wires 3, 4 of the second plurality of wires causes an increase in the fogging 9 in the loading zone compared to the fogging 8 in the clamping zone.

[0047] [Fig. 3] is a representation of a test piece 10 obtained according to a method of the prior art, seen from above and comprising a so-called “dog bone” geometry.

[0048] Such a geometry is characterized by a reduction in the width L of the test piece, and this reduction in width can cause the appearance of stress concentrations, in particular in the zones 11 between the clamping zones 14 and the loading zone 13 in the middle of the test piece.

[0049] Thus, a geometry without such a reduction in width makes it possible to reduce the appearance of such stress concentration zones 11 between the clamping zones 14 of the loading zone 13, and thus further promote the rupture of the test piece in the loading zone 13.

[0050] Similarly, extracting threads from the preform, for example to give it a particular shape, can cause stress concentration zones where threads are extracted, and thus cause weak points outside the loading zone of the test piece. Thus, it is preferred that the test piece has a rectangular geometry that can be obtained simply from a fiber preform in which no threads are extracted between the clamping zones and the loading zone.

[0051] [Fig. 4] represents a test piece geometry 20 according to an embodiment of the invention. In this embodiment, the test piece has a rectangular geometry, in which the width L of the test piece does not vary between the clamping zones 24, and loading zone 23.

[0052] In order to ensure that the loading zones have mechanical characteristics identical to those of the material that one wishes to characterize, it is possible to define the weaving characteristics of the fiber preform of the characterization test piece using simulation tools such as, for example, finite element simulation calculations.

[0053] Of course, the embodiments described above can be combined with each other in order to further increase the probability that the characterization test piece is indeed broken in its loading zone.

Claims

Claims

1. Characterization test piece (20) made of a composite material comprising a fibrous preform having a weave between a first plurality of threads (1) and a second plurality of threads (2) densified by a matrix, the test piece comprising a loading zone (23) located between two clamping zones (24) in the direction of stress and characterized in that the threads of the first plurality of threads of the fibrous preform extending in the direction of stress have a greater weaving in the loading zone than in the clamping zones.

2. Characterization specimen according to claim 1, wherein the spacing between the threads of the second plurality of threads of the fiber preform (2) which extend in a direction perpendicular to the stress direction is greater in the clamping zones (24) than in the loading zone (23).

3. Characterization test piece according to claim 1 or 2, wherein the tension of the yarns of the first plurality of yarns (1) of the fiber preform in the loading zone (23) is greater than or equal to the tension of the yarns of the first plurality of yarns (1) of the fiber preform in the clamping zones (24).

4. Characterization test piece according to any one of claims 1 to 3, wherein the diameter of the threads of the second plurality of threads (2) of the fiber preform is larger in the loading zone (23) than in the clamping zones (24).

5. Characterization specimen according to any one of claims 1 to 4, wherein the width of the fiber preform of the characterization specimen is the same in the clamping zones (24) and in the loading zone (23).

6. Characterization specimen according to any one of claims 1 to 5, wherein no yarn of the first plurality of yarns (1) is extracted from the fiber preform of the characterization specimen between the clamping zones (24) and the loading zone (23).

7. Characterization test piece according to any one of claims 1 to 6, wherein the fibrous preform is a three-dimensional woven preform.

8. Method for characterizing a composite material, comprising a step during which a characterization test piece according to one of any of claims 1 to 6 is subjected to loading in the direction of the yarns of the first plurality of yarns (1) of the fibrous preform of said test piece.