Method for manufacturing a part made of ceramic matrix composite material
A protective Si-B-C barrier formed by boron diffusion addresses the issue of silicon carbide degradation in CMCs, enhancing structural integrity and mechanical performance by shielding the pre-densification matrix from molten silicon attack.
Patent Information
- Application Number
- FR2022010905
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-10-21
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2042-10-21
AI Technical Summary
Ceramic matrix composite materials (CMCs) used in turbomachines face variability in rupture behavior due to uncontrolled attack on the silicon carbide pre-densification matrix by molten silicon during infiltration, leading to degradation of the fibrous reinforcement and reduced structural integrity.
A protective Si-B-C barrier is formed by diffusing boron from a second layer into the silicon carbide layer during a heat treatment, creating a homogeneous protective layer within the pre-densified fibrous structure to shield the underlying silicon carbide from molten silicon attack.
The Si-B-C barrier enhances the composite's breaking behavior, improving overall performance by protecting the silicon carbide and maintaining mechanical integrity, while minimizing volume fraction impact on other material stages.
Smart Images

Figure 00000011_0000 
Figure 00000012_0000 
Figure 00000012_0001
Abstract
Description
Title of the invention: Method for manufacturing a part made of ceramic matrix composite material Technical field
[0001] The invention relates to the manufacture of a part made of ceramic matrix composite material ("Ceramic Matrix Composite"; "CMC") during which the ceramic matrix is formed by infiltration of a molten silicon-based composition ("Melt-Infiltration"; "MI"). The invention proposes the presence of a Si-BC protective barrier making it possible to protect the underlying pre-densification silicon carbide from attack by the molten silicon. The part made of composite material thus obtained can find an application as a hot part of a turbomachine, in particular an aeronautical turbomachine, such as a turbine part. Prior art
[0002] Ceramic matrix composite materials withstand temperatures ranging from 600°C to 1400°C. Due to their better resistance to high temperatures, CMCs require less cooling. This cooling traditionally comes from a sample in the compressor which impacts the efficiency of the turbomachine, CMC materials therefore make it possible to improve engine efficiency which reduces fuel consumption. Furthermore, their use contributes to optimizing the performance of turbomachines, in particular by reducing the overall mass of the turbomachine which further contributes to a reduction in fuel consumption and therefore to a significant reduction in pollutant emissions.
[0003] CMC parts can be densified by melt infiltration. In this technique, a molten silicon composition can be introduced into the porosity of a fibrous structure pre-densified by a silicon carbide deposit and loaded with silicon carbide particles. This method makes it possible to obtain a fully dense Si-SiC matrix of high modulus and a composite with a high linearity limit. The resulting composites have good mechanical properties but the inventors have observed a certain variability in the elongation at break which reduces the damage tolerance of the material. It is desirable to propose a solution to address this drawback. Statement of the invention
[0004] The invention relates to a method for manufacturing a part made of ceramic matrix composite material, comprising: - the formation of a precursor deposit of pre-densification matrix in a porosity of a fibrous structure, comprising the deposition of a first layer of silicon carbide and the deposition of a second layer of boron-doped silicon covering the first layer, - a solid-phase boron diffusion heat treatment by subjecting the precursor deposit thus formed to a treatment temperature of between 1350°C and 1400°C in order to form a protective barrier in a Si-BC ternary system at the interface between the first layer and the second layer and thus obtain a pre-densified fibrous structure, and - infiltration of the pre-densified fibrous structure thus obtained by a molten infiltration composition comprising silicon in order to form a ceramic matrix in a residual porosity of the pre-densified fibrous structure.
[0005] The inventors found that the variability of the fracture behavior was linked to an uncontrolled attack of the silicon carbide of the pre-densification matrix by the molten silicon in the solution of the prior art. This phenomenon can go as far as the degradation of the fiber reinforcement and the interphase resulting in a reduction of the structural character of the composite. The invention proposes a functionalization of the pre-densification matrix so as to integrate therein a Si-BC protective barrier which makes it possible to reduce the attack of the silicon carbide of the pre-densification matrix. This barrier is formed by the diffusion of the boron of the second layer into the silicon carbide of the first layer during the heat treatment.The protective barrier, an integral part of the pre-densification matrix, is distributed homogeneously in the pre-densified fibrous structure to provide protection throughout its volume and throughout infiltration. This results in composite materials with much better breaking behavior.
[0006] In an exemplary embodiment, a thickness of the second layer, before the heat treatment, is between 0.5 μm and 1 μm.
[0007] Such a characteristic makes it possible to obtain improved overall performance by providing the desired protection of the silicon carbide while having a volume fraction occupied by the second layer limited so as not to substantially modify the other steps of the range, in particular by only slightly affecting the volume fraction of the first layer which makes a large contribution to mechanical performance of the material, as well as the residual porosity of the pre-densified structure in order to avoid complicating a possible subsequent introduction of powdery composition before infiltration.
[0008] In an exemplary embodiment, boron is present in an atomic proportion of between 0.05% and 1% in the second layer before the heat treatment.
[0009] Such a feature helps to further improve the protection of the underlying silicon carbide.
[0010] In an exemplary embodiment, the method further comprises, before the treatment thermal, an introduction of a silicon carbide powder into a residual porosity of the fibrous structure provided with at least the first layer of silicon carbide.
[0011] Such a characteristic advantageously makes it possible to take advantage of the solid-phase boron diffusion heat treatment which makes it possible to form the barrier described above to also carry out deoxidation of the powder in order to improve wetting by the molten silicon.
[0012] In particular, the silicon carbide powder can be introduced into the residual porosity of the fibrous structure provided with the precursor deposit.
[0013] In this case, the silicon carbide powder is introduced after the deposition of the first layer of silicon carbide and the second layer of boron-doped silicon, but it does not depart from the scope of the invention when the silicon carbide powder is introduced between the first and second layers. In the latter case, an additional protective barrier in a Si-BC ternary system is also formed at the interface between the silicon carbide powder and the second layer, in addition to the protective barrier at the interface between the first layer and the second layer described above.
[0014] In an exemplary embodiment, the treatment temperature is between 1370°C and 1390°C.
[0015] In one exemplary embodiment, the infiltration composition comprises boron.
[0016] Such a characteristic advantageously makes it possible to further protect the underlying silicon carbide.
[0017] In an exemplary embodiment, the fibrous structure is provided with a boron nitride interphase on which the first layer is deposited during the formation of the precursor deposit.
[0018] The presence of a boron nitride interphase advantageously makes it possible to deflect cracks which may appear in the matrix of the composite part during operation so as to preserve the fibrous reinforcement, and to provide resistance to oxidation.
[0019] In an exemplary embodiment, the fibrous structure comprises a fibrous reinforcement formed by three-dimensional weaving or from a plurality of two-dimensional fibrous layers.
[0020] In an exemplary embodiment, the part is a turbomachine part.
[0021] The part may be a turbine part, for example an aircraft engine turbine part. The part may for example be a turbomachine blade, a turbine ring sector or a distributor. Brief description of the drawings
[0022] [Fig.l] [Fig.l] is a flowchart showing a succession of steps of an example of a method according to the invention.
[0023] [Fig.2] [Fig.2] schematically and partially represents an example of a fibrous structure provided with a precursor deposit of pre-densification matrix which can be implemented within the framework of the invention.
[0024] [Fig.3] [Fig.3] schematically and partially represents the fibrous structure of [Fig.2] after the boron diffusion heat treatment. Description of the embodiments
[0025] An example of a method for manufacturing a part made of CMC material according to the invention will now be described in connection with the flowchart of [Fig. 1] and the architectures illustrated in Figures 2 and 3.
[0026] A first step S10 of the method may consist of forming the fibrous structure by implementing one or more textile operations such as three-dimensional weaving. The fibrous structure may be formed of ceramic threads, for example silicon carbide threads. The fibrous structure may constitute the fibrous reinforcement 10 of the composite material part to be obtained. Examples of usable silicon carbide threads may be threads marketed under the reference “Nicalon”, “Hi-Nicalon”, “Hi-Nicalon-S” or Tyranno SA3 from the company UBE Industries. The ceramic threads of the fibrous structure may have an oxygen content of less than or equal to 1% in atomic percentage. The “Hi-Nicalon-S” threads, for example, have such a characteristic. By “three-dimensional weaving” or “3D weaving”, it is necessary to understand a weaving method by which at least some of the warp threads bind weft threads over several weft layers.A role reversal between warp and weft is possible in this text and should be considered as also covered by the claims. The fiber structure may for example have an interlock weave. By "interlock weave or fabric" is meant a 3D weave in which each layer of warp threads links several layers of weft threads with all the threads of the same warp column having the same movement in the plane of the weave. It is also possible to start from fiber textures such as two-dimensional fabrics or unidirectional sheets, and to obtain the fiber structure by draping such fiber textures on a form. These textures can optionally be linked together for example by sewing or implantation of threads to form the fiber structure.
[0027] In a step S20, a chemical vapor infiltration weakening interphase 20 can be formed on the threads of the fibrous structure. The fibrous structure can be positioned in a shaping tool allowing it to be shaped into the part to be obtained during the deposition of the interphase. The thickness e20 of the interphase may for example be between 10 nm and 1000 nm, and for example between 200 nm and 500 nm. After formation of the interphase, the fibrous structure remains porous, the initial accessible porosity being filled only for a minor part by the interphase. The interphase may be single-layer or multi-layer. The interphase may comprise at least one layer of pyrolytic carbon (PyC), boron nitride (BN), silicon-doped boron nitride (BN(Si), with silicon in a mass proportion of between 5% and 40%, the remainder being boron nitride) or boron-doped carbon (BC, with boron in an atomic proportion of between 5% and 20%, the remainder being carbon).The interphase here has a function of weakening the composite material which promotes the deflection of any cracks reaching the interphase after having propagated in the matrix, preventing or delaying the breakage of fibers by such cracks. Alternatively, it will be noted that it is possible to form the interphase on the threads before the formation of the fiber structure, that is to say before implementation of step S10.
[0028] A step S30 of forming a silicon carbide deposit is then carried out. This step S30 can be separated into two phases. During the first phase, the fibrous structure is still in the shaping tool and a silicon carbide consolidation layer 301 is deposited on the interphase 20 and the fibrous reinforcement 10. The consolidation layer 301 can be deposited in contact with the interphase 20. This layer has a sufficient thickness to sufficiently bond the fibers so that the structure retains its shape without assistance from the holding tool. This layer provides protection to the interphase against oxidation and can be formed by chemical vapor infiltration in a manner known per se, for example from a gas phase comprising methyltrichlorosilane (MTS) and hydrogen (H2). The thickness e30i of the consolidation layer 301 may be greater than or equal to 0.1 pm, for example between 0.1 pm and 5 pm.During the second phase, the consolidated and shaped fibrous structure of the part to be obtained can be removed from the tooling and the formation of the precursor deposit 35 of the pre-densification matrix can be initiated by depositing a first layer 302 thereof made of silicon carbide. The first layer 302 can be deposited in contact with the consolidation layer 301. The thickness e302 of the first layer 302 can be greater than the thickness e30i of the consolidation layer 301. This first layer of silicon carbide makes a large contribution to the mechanical performance of the composite material and provides protection against the molten silicon used during the subsequent infiltration. The thickness e302 of the first layer 302 can be greater than or equal to 1 μm, for example between 1 μm and 20 μm.As with the consolidation layer, the first layer of the precursor deposit can be formed by chemical vapor infiltration in a manner known per se. In a manner . Generally, the precursor deposit can be formed by chemical vapor infiltration. According to a variant not shown, the layer 301 could be omitted and the first layer 302 of the precursor deposit could be formed directly on the interphase 20.
[0029] The formation of the precursor deposit can be continued by forming the second layer 40 of boron-doped silicon on the first layer 302 (step S40). This layer 40 is intended to provide boron allowing the formation of the Si-BC protective barrier after the diffusion heat treatment in order to protect the underlying silicon carbide from attack by the molten silicon. In the example of [Fig.2], the precursor deposit 35 comprises a single second layer 40 of boron-doped silicon. The second layer 40 can be deposited in contact with the first layer 302. In the example illustrated, the precursor deposit 35 comprises only the first 302 and the second 40 layers. The thickness e40 of the second layer 40 can be between 0.5 μm and 1 μm. Boron may be present in an atomic proportion of between 0.05% and 1% in the second layer 40 before the boron diffusion heat treatment, the remainder being silicon.The second layer 40 may correspond to a binary eutectic composition of silicon and boron. The residual porosity of the fibrous structure provided with the precursor deposit 35 may be between 20% and 40%, for example between 30% and 35%. The second layer 40 may be formed by chemical vapor infiltration. A mixture of a first gaseous precursor comprising silicon, for example chosen from SiCl4, SiHCl3, SiH2Cl2, SiH3Cl, SiH4, CH3SiCl3 or CH3SiH3, and a second gaseous precursor comprising boron, for example chosen from BC13, BF3 or B2H6, may be used. The relative ratios of the precursors are adjusted according to their reactivity. The second layer 40 may be formed by imposing a temperature between 700°C and 1200°C. The second layer 40 can be formed in a medium at a pressure less than or equal to 200 mbar, for example between 1 mbar and 200 mbar to promote good infiltration of the deposit.In an exemplary embodiment, a combination of SiHCl3 and BC13 can be used in ratios between 1 / 1 and 100 / 1 at a temperature of 1000°C and at a pressure of 100 mbar.
[0030] The method continues by introducing a powdery composition into a residual porosity of the structure provided with the precursor deposit 35 (step S50). This powdery composition can be introduced into the fibrous structure by slurry-casting in a manner known per se. The powdery composition can comprise a silicon carbide powder and / or a carbon powder and / or a boron carbide powder. According to one example, the powdery composition comprises the silicon carbide powder, and optionally the carbon powder and / or the boron carbide powder.
[0031] The diffusion heat treatment of the boron comprising the application of a temperature between 1350°C and 1400°C, for example between 1370°C and 1390°C, for example between 1375°C and 1385°C, in particular at around 1380°C. Generally, this temperature can be applied for a period of at least 30 minutes. Whatever the embodiment considered, the heat treatment can be carried out under vacuum or under a pressure less than or equal to 100 mbar of a neutral gas. During the heat treatment, the boron of the second layer 40 diffuses towards the first layer 302 to form a barrier 38 in the Si-BC ternary system at the interface between the first layer 302 and the second layer 40. After the diffusion heat treatment, a second layer 402 depleted in boron is obtained which has an atomic proportion of boron lower than the atomic proportion of boron in the second layer 40 before this heat treatment.The reduction in the atomic proportion of boron in the second layer 40 following the heat treatment may be greater than or equal to 80%, or even 90%. According to one example, substantially all of the boron in the second layer 40 may be consumed following the heat treatment. The protective barrier 38 may have a thickness e38 greater than or equal to 1 nm, for example between 1 nm and 30 nm. In the example considered, the heat treatment also allows deoxidation of the previously introduced silicon carbide powder.
[0032] After the diffusion heat treatment, the pre-densification matrix 37 is obtained, which successively comprises the first layer 302, the protective barrier 38 and the second layer 402 depleted in boron or substantially devoid of boron. In the example illustrated, the second layer 402 defines an external surface Sext of the pre-densification matrix, that is to say it forms the layer furthest from the fibrous reinforcement 10 during infiltration. Thus, during infiltration, no other layer is interposed between the layer 402 and the infiltration composition. The residual porosity volume rate of the pre-densified fibrous structure loaded with the powdery composition may be less than or equal to 25%, for example between 15% and 25%.An embodiment has been described in which the powdery composition is introduced after formation of the second layer 40 of boron-doped silicon, but it does not depart from the scope of the invention when the powdery composition is introduced after formation of the first layer 302 but before formation of the second layer 40 with subsequent performance of the diffusion heat treatment. In this case, the second layer 40 covers the silicon carbide powder as well as the first layer 302. The silicon carbide powder is interposed between the first 302 and the second layer 40. Generally speaking, the powdery composition, which may at least comprise the silicon carbide powder, may be introduced after deposition of the second layer before or after the heat treatment. diffusion, or be introduced between the deposition of the first layer and the second layer.
[0033] After introduction of the powdery composition, step S70 is carried out during which the residual porosity is infiltrated with a molten infiltration composition comprising at least silicon so as to form a ceramic matrix in the porosity of the fibrous structure. The formation of this ceramic matrix can make it possible to finalize the densification of the part. This infiltration step corresponds to a molten infiltration step. The infiltration composition can consist of pure molten silicon or, alternatively, be in the form of a molten alloy of silicon and one or more other constituents. The infiltration composition can comprise predominantly silicon by mass, i.e. have a silicon content by mass greater than or equal to 50%. The infiltration composition can, for example, have a silicon content by mass greater than or equal to 75%.The constituent(s) present within the silicon alloy may be chosen from B, Al, Mo, Ti, Ge and mixtures thereof. When the powder composition comprises carbon particles, a chemical reaction may occur between the infiltration composition and these carbon particles during infiltration resulting in the formation of silicon carbide.
[0034] After step S70, a part made of CMC material is obtained. Such a part made of CMC material may be a static or rotating part of a turbomachine. Examples of turbomachine parts have been mentioned above. Such a part may further be coated with an environmental or thermal barrier coating before use.
[0035] The expression “between ... and ...” must be understood as including the limits.
Claims
Claims
1. Method for manufacturing a part made of ceramic matrix composite material, comprising: - the formation of a precursor deposit (35) of pre-densification matrix (37) in a porosity of a fibrous structure, comprising the deposition of a first layer (302) of silicon carbide and the deposition of a second layer (40) of boron-doped silicon covering the first layer, - a heat treatment (S60) for diffusion of boron in solid phase by subjecting the precursor deposit thus formed to a treatment temperature of between 1350°C and 1400°C in order to form a protective barrier (38) in a Si-BC ternary system at the interface between the first layer and the second layer and thus obtain a pre-densified fibrous structure,and - infiltration (S70) of the pre-densified fibrous structure thus obtained by a molten infiltration composition comprising silicon in order to form a ceramic matrix in a residual porosity of the pre-densified fibrous structure.,
2. The method of claim 1, wherein a thickness (e40) of the second layer (40), before the heat treatment (S60), is between 0.5 pm and 1 pm.
3. A method according to claim 1 or 2, wherein boron is present in an atomic proportion of between 0.05% and 1% in the second layer (40) before the heat treatment.
4. Method according to any one of claims 1 to 3, wherein the method further comprises, before the heat treatment (S60), an introduction (S50) of a silicon carbide powder into a residual porosity of the fibrous structure provided with at least the first layer (302) of silicon carbide.
5. Method according to claim 4, in which the silicon carbide powder is introduced into the residual porosity of the fibrous structure provided with the precursor deposit (35).
6. A method according to any one of claims 1 to 5, wherein the treatment temperature is between 1370°C and 1390°C.
7. A method according to any one of claims 1 to 6, wherein the infiltration composition comprises boron.
8. A method according to any one of claims 1 to 7, wherein the fibrous structure is provided with an interphase (20) of boron nitride on which the first layer (302) is deposited during the formation of the precursor deposit (35).
9. A method according to any one of claims 1 to 8, wherein the fibrous structure comprises a fibrous reinforcement (10) formed by three-dimensional weaving or from a plurality of two-dimensional fibrous plies.
10. A method according to any one of claims 1 to 9, wherein the part is a turbomachine part.