Construction of an environmental barrier layer
An anti-wetting surface layer of noble metal or alloy, combined with ceramic and conductive layers, addresses the issue of CMAS infiltration and corrosion in SiC/SiC CMCs, ensuring the durability and protection of turbomachine parts by limiting CMAS spread and infiltration.
Patent Information
- Application Number
- FR2023003160
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-04
AI Technical Summary
SiC/SiC ceramic matrix composites (CMCs) used in high-temperature turbine parts are susceptible to corrosion and oxidation in oxidizing environments, particularly due to the presence of CMAS, leading to spalling and destruction of the environmental barrier coating (EBC) due to thermal expansion coefficient differences and CMAS infiltration.
Application of an anti-wetting surface layer comprising a noble metal or alloy with at least one noble metal, optionally combined with ceramic and electrically conductive layers, to prevent CMAS infiltration and spreading on the surface of turbomachine parts, thereby enhancing the protective capacity of the EBC.
The anti-wetting surface layer effectively limits CMAS infiltration and spreading, maintaining the integrity of the EBC and reducing thermomechanical stress, thus protecting the turbomachine parts from corrosion and oxidation.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Title of the invention: Construction of an environmental barrier layer technical field
[0001] The present invention relates to the general field of protective coatings used for parts in high-temperature environments such as parts used in hot sections of aeronautical or land-based turbomachinery. Previous technique
[0002] Carbide-based ceramic matrix composites (CMCs) (generally referred to as "SiC / SiC") are now used for manufacturing parts for high- and low-pressure turboshaft engines, with the aim of reducing, or even eliminating, the cooling flow rate traditionally used in the design of nickel-based (Ni) alloy metal parts. This benefit is linked to the intrinsic refractivity of SiC ceramics, allowing for higher turbine operating temperatures while reducing the engine's specific fuel consumption (Cs) (as a consequence of the reduced cooling air intake).
[0003] However, in an oxidizing and / or corrosive environment in which a turbine operates, SiC / SiC CMCs are subject to a non-passivating corrosion and / or recession phenomenon resulting from oxidation leading to the formation of SiO2 and the volatilization of this oxide in the presence of water. Thus, for high-temperature applications in oxidizing environments in the presence of water, the application of a protective coating to the SiC / SiC CMCs is necessary.
[0004] The protective coating applied is generally called an "environmental barrier" (EBC) and consists of a bonding layer (bond coat), usually silicon-based, and a layer providing corrosion protection. This latter protective layer (generally called a top coat) is made of rare-earth disilicate or monosilicate. The coating must meet a number of requirements: - a coefficient of expansion compatible with that of the CMC substrate, - low permeability to oxidizing and / or corrosive species, - thermomechanical stability at the operating temperatures of the part and - very good resistance to CMAS.
[0005] The low permeability to oxidizing and / or corrosive species relates both to molecular diffusion directly linked to the physical parameter of hermeticity and to the diffusion of ionic species O2 and HO, intrinsic characteristics of rare earth disilicates and monosilicates.
[0006] Among the ceramicizable parts offering the greatest benefit in terms of Cs savings, turbine blades and distributors can be cited. However, the design of such parts in CMC presents several technical challenges: - they are subjected to strong thermomechanical stresses associated with a particularly harsh chemical environment; - they often have complex geometric shapes; - their production rate, particularly with regard to production for civil aviation, is very high.
[0007] The particularly harsh chemical environment is generally due to the presence of dioxygen (O2), water (H2O), and calcium magnesium aluminosilicates (CMAS). CMAS are notably present in the form of sand, which can be drawn into the engine when the aircraft flies over certain desert regions of the globe, such as the Sahara, China, and India.
[0008] The complex geometric shapes are due in particular to the fact that the parts are made up of several sub-assemblies associated with their own functions, to the presence of leading edges, trailing edges or hollow cavities.
[0009] The EBCs applied to these parts, in addition to their own functional performance, must satisfy all of these requirements. Among other things, with regard to parts with a leading edge and / or trailing edge whose aerodynamic performance is directly related to the thickness of these parts, and in particular the trailing edge, the EBC deposition process must be compatible with the creation of very thin layers (typically less than 150 µm) while preserving their protective capacity of the CMC.
[0010] The EBCs currently developed are composed of: - a silicon bonding layer; and - a protective layer of rare earth disilicate.
[0011] The main function of the bonding layer is to protect against oxidation and / or corrosion and to promote the adhesion of the protective layer.
[0012] During an EBC stabilization treatment, a passivating silica layer (also called "thermally grown oxide" or TGO) forms, providing protection against oxidation of the CMC SiC / SiC. This silica layer can also undergo continuous growth during operation, depending on the EBC's airtightness level.
[0013] Rare earth disilicate has the formula RE2Si2O7, where RE denotes rare earth. Generally, the rare earth is yttrium (Y), ytterbium (Yb), or yttrium-ytterbium (YYb). The rare earth disilicate layer acts as a barrier against the diffusion of oxidizing species and protects the CMC against high-temperature corrosion.
[0014] To meet dimensional requirements, the silicon bonding layer is generally produced by chemical vapor deposition (CVD), and the rare-earth disilicate layer by liquid deposition, particularly by electrophoresis. These two processes have the advantage of being non-directional; they are thus suitable for complex shapes. They allow for the deposition of thicknesses of around ten micrometers.
[0015] The electrophoretic deposition process consists of immersing a part in a ceramic powder suspension. A counter electrode is positioned opposite the part to be coated. An electric field is applied between the counter electrode and the part. Under the influence of this electric field, the ceramic particles contained in the suspension migrate and are deposited onto the part to be coated.
[0016] However, CMAS have a melting point lower than the operating temperature of the turbomachine. As a result, silicate liquids form on the turbomachine. These silicate liquids generate thermomechanical stresses, ultimately leading to spalling due in particular to differences in the coefficient of thermal expansion between the CMAS and the EBC, and thermochemical stresses, e.g., dissolution of the EBC and precipitation of new phases. These various phenomena lead to the destruction of the coating. It is therefore necessary to prevent these CMAS from infiltrating the surface of the turbomachine.
[0017] Furthermore, these sands, by virtue of their chemical formula, exhibit total wettability on the EBC coating. By total wettability, it is understood that the CMAS spreads over the ceramic matrix composite turbomachine parts and creates an attack on the external surface of these parts.
[0018] It is therefore imperative to better protect these turbomachine parts from these CMAS. Summary
[0019] This disclosure improves the situation.
[0020] A turbomachine part is proposed comprising a ceramic matrix composite substrate coated with an environmental barrier stack having an anti-wetting surface layer comprising a noble metal or an alloy comprising at least one noble metal.
[0021] During CMAS melting tests, it was observed that the noble metals from which the crucibles used in these tests were formed exhibit particularly interesting wetting properties, as they are anti-wetting with respect to molten CMAS. This observation is exploited in the present turbomachine component to obtain improved protection against CMAS. Indeed, the surface layer in question prevents CMAS from infiltrating the re The coating on the turbomachine component could allow infiltration that could lead to the destruction of the environmental barrier layer. This surface layer also prevents or reduces the spread of a droplet of liquid CMAS on the surface of the turbomachine component, thus limiting the component's exposure to CMAS. It can also limit the droplet's adhesion to the turbomachine component.
[0022] By anti-wetting agent, it is understood that there is no total wetting of the CMAS on the outer layer, that is to say, there is no complete spreading of the CMAS to form a film, with a zero wetting angle. The wetting angle of the CMAS fused to this outer layer can not only be non-zero, but it can even be between 90 degrees and 180 degrees.
[0023] The anti-wetting surface layer can be a layer of noble metal or a layer of an alloy comprising at least one noble metal.
[0024] The anti-wetting surface layer may include inclusions of noble metal or an alloy comprising at least one noble metal in a ceramic matrix.
[0025] If the environmental barrier layer cracks, the infiltration of CMAS into this crack will be greatly limited. Indeed, the opening of the crack will cause, at the operating temperature, the flow of the noble metal or molten alloy into the crack, protecting the crack walls and thus limiting infiltration by the CMAS.
[0026] The noble metal may be gold.
[0027] Gold has a melting point low enough to penetrate the ceramic layer at the operating temperatures of the turbomachine part.
[0028] The environmental barrier stack may include under the anti-wetting surface layer one or more ceramic layers alternating with one or more electrically conductive layers of noble metal, an alloy comprising at least one noble metal or graphite.
[0029] The ceramic layer(s) may be made of a rare earth monosilicate or a rare earth disilicate, preferably the rare earth is yttrium, ytterbium or yttrium-ytterbium.
[0030] The ceramic matrix composite substrate may comprise silicon carbide fibers and a silicon carbide matrix.
[0031] This document relates to a method for obtaining a turbomachine part comprising a ceramic matrix composite substrate coated with an environmental barrier stack,
[0032] characterized in that it comprises, during the formation of the environmental barrier stack: - the formation of a surface anti-wetting layer comprising a noble metal or an alloy comprising at least one noble metal.
[0033] The process may further include the formation under the anti-wetting surface layer of one or more ceramic layers alternating with one or more electrically conductive layer(s) of noble metal, of an alloy comprising at least one noble metal or of graphite.
[0034] The rare earth disilicate may be RE2Si2O7, RE being a rare earth, preferably RE is yttrium, Y, ytterbium, Yb, or YYb.
[0035] The formation of the electrically conductive layer(s) can be carried out by dry means such as physical vapor deposition and chemical vapor deposition, by inkjet printing or by electrophoresis. Brief description of the drawings
[0036] Other features, details and advantages will become apparent from reading the detailed description below and from analyzing the accompanying drawings, in which: Fig. 1
[0037] [Fig.1] shows an illustration defining a wetting angle. Fig. 2
[0038] [Fig.2] schematically shows in figure 2A a CMAS deposit on a turbomachine part and in figure 2B the spreading occurring of the CMAS at a later time, according to the prior art. Fig. 3
[0039] [Fig.3] shows part of a turbomachine component in Figure 3A and 3B, according to one embodiment of the invention. Fig. 4
[0040] [Fig.4] shows part of a turbomachine component, according to a second embodiment of the invention. Fig. 5
[0041] [Fig.5] schematically shows the mechanical behavior of an external anti-wetting layer when a crack appears on the surface of the turbomachine part, according to the invention. Fig. 6
[0042] [Fig.6] shows a turbomachine part according to the prior art. Fig. 7
[0043] [Fig.7] shows an experimental result of a turbomachine part treated according to the invention. Fig. 8
[0044] [Fig.8] shows an experimental result. [Fig.9]
[0045] [Fig.9] shows a method for obtaining a turbomachine part, according to the invention. Description of the implementation methods
[0046] Reference is now made to [Fig.2].
[0047] Figure 2A schematically illustrates a CMAS 4 deposition on a turbomachine part comprising a ceramic matrix composite substrate 6 coated with an environmental barrier stack. This environmental barrier stack 8 comprises a ceramic layer 10 on a silicon layer 12. In such a case, when CMAS 4 is deposited on the turbomachine part, it spreads over the ceramic layer 10 and chemically attacks it.
[0048] The turbomachine part according to the invention avoids CMAS attack and comprises a ceramic matrix composite substrate 6 coated with an environmental barrier stack 8 having an anti-wetting surface layer comprising a noble metal or an alloy comprising at least one noble metal.
[0049] The noble metal of the anti-wetting surface layer 14 can be selected from: gold, silver, ruthenium, rhodium, palladium, osmium, iridium and platinum. Preferably, the noble metal is gold or platinum.
[0050] The stack 8 may further comprise a ceramic layer 10 or several ceramic layers 10 alternating with one or more electrically conductive layers 16.
[0051] The ceramic layer(s) 10 may be made of a rare-earth monosilicate or a rare-earth disilicate. Rare-earth monosilicates have the formula RE'RE2 SiO5 (where RE1 and RE2 each represent a rare earth, and RE1 and RE2 may or may not be the same rare earth). Rare-earth disilicates have the formula RE1RE2Si2O7. Each of the RE1 and RE2 elements can be independently selected from the group consisting of: yttrium (Y), lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), and lutetium (Lu). Among these rare earth elements, Y and Yb are preferred.Thus, the following are some of the preferred silicates: yttrium monosilicate (Y₂SiO₅ or YMS), ytterbium monosilicate (Yb₂SiO₅ or YbMS), yttrium-ytterbium monosilicate (YYbSiO₅ or YYbMS), yttrium disilicate (Y₂Si₂O₇ or YDS), ytterbium disilicate (Yb₂Si₂O₇ or YbDS), and yttrium-ytterbium disilicate (YYbSi₂O₇ or YYbDS). Titanium disilicide is another possible silicate. (TiSi2) and zirconium disilicide (ZrSi2).
[0052] The electrically conductive layer(s) 16 may be made of a noble metal, an alloy comprising at least one noble metal, or graphite. The noble metal may be selected from: gold, silver, ruthenium, rhodium, palladium, osmium, iridium, and platinum. Preferably, the noble metal is gold or platinum.
[0053] Reference is now made to [Fig.3].
[0054] Fig. 3 schematically illustrates a first embodiment of the invention and more specifically the physico-chemical behavior of CMAS when these CMAS are found on the surface of a turbomachine part according to the invention.
[0055] In this embodiment, a portion of a turbomachine component is schematically represented in Figures 3A and 3B. This turbomachine component comprises a ceramic matrix composite substrate 6 coated with an environmental barrier stack 8. The environmental barrier stack 8 comprises a ceramic layer 10 on a silicon layer 12. The environmental barrier stack 8 further comprises an anti-wetting surface layer 14 made of a noble metal or an alloy containing at least one noble metal. That is to say, the noble metal or the alloy containing at least one noble metal constitutes the material of the anti-wetting surface layer 14. By anti-wetting surface layer, we mean the outermost layer of the component and, more precisely, the layer in contact with the external environment.This surface layer has anti-wetting properties, meaning that thanks to this surface layer, the CMAS coating does not spread completely across the surface of the part. The wetting angle is not zero, and is even between 90 and 180°: there is no total wetting.
[0056] Thanks to the anti-wetting surface layer 14, when CMAS are deposited on the turbomachine part (as illustrated by Figure 3A), they do not spread completely on the anti-wetting surface layer 14 of the turbomachine part (as illustrated in Figure 3B).
[0057] Reference is now made to [Fig.4].
[0058] This [Fig. 4] schematically illustrates a second embodiment of the invention. In this embodiment, a ceramic matrix composite substrate 6 of a turbomachine part is coated with an environmental barrier stack 8. This environmental barrier stack 8 comprises a silicon layer 12 on the ceramic matrix composite substrate 6.
[0059] This environmental barrier stack 8 further comprises a wetting-resistant surface layer 14 made of a noble metal or an alloy comprising at least one noble metal. That is to say, the noble metal or the alloy comprising at least one noble metal constitutes the material of the wetting-resistant surface layer 14.
[0060] The turbomachine component further comprises, beneath the anti-wetting surface layer 14, two ceramic layers 10 alternating with an electrically conductive layer 16, made of an alloy comprising at least one noble metal or of graphite. The turbomachine component thus comprises, between the silicon layer 12 and the anti-wetting surface layer 14, a stack of three layers: in order, a ceramic layer 10, an electrically conductive layer 16, and a ceramic layer 10.
[0061] In another case, the environmental barrier stack 8 may include under the anti-wetting surface layer 14 several ceramic layers 10 alternating with several electrically conductive layers 16.
[0062] A ceramic layer 10 is in contact with the silicon layer 12 and another ceramic layer 10 is in contact with the anti-wetting surface layer 14.
[0063] If n is the number of ceramic layers 10, then the number of electrically conductive layers is n-1, with n greater than 2.
[0064] This configuration provides additional protection against CMAS, particularly when the electrically conductive layer(s) are made of a noble metal or an alloy containing at least one noble metal. Indeed, in the event of cracking or removal of the anti-wetting surface layer 14 and the ceramic layer(s) 10, the electrically conductive layer(s) will act as an anti-wetting agent, limiting the propagation of CMAS within the stack 8, or limiting its spreading. It has been noted that graphite, like noble metals such as platinum or gold, is anti-wetting with respect to CMAS. Although graphite exhibits anti-wetting properties, it is poorly suited as a surface layer. In fact, it could not replace the anti-wetting surface layer 14 because it presents a risk of oxidation.
[0065] Reference is now made to [Fig.5].
[0066] Figure 5 schematically illustrates, in A) another embodiment for the anti-wetting surface layer and in B) the particular mechanical behavior of such an anti-wetting surface layer 14.
[0067] As illustrated in Figure 5A, the anti-wetting surface layer comprises inclusions 20 of noble metal or an alloy containing at least one noble metal in a ceramic matrix. The size of the inclusions 20 allows them to be homogeneously embedded in the ceramic matrix. In Figure 5B, it can be seen that in the event of a crack, at the operating temperature of the turbomachine, the molten noble metal or alloy of the anti-wetting surface layer 14 seeps into the crack formed on the surface of said turbomachine component and coats the crack walls. This thus limits the infiltration of CMAS into the crack.
[0068] In this particular embodiment, the noble metal is preferably gold because it is liquid at the operating temperature of the turbomachine part.
[0069] The ceramic matrix can be made of the same material as the ceramic layer(s) described above.
[0070] Alternatively, such a layer comprising inclusions of noble metal or of a noble metal alloy in a ceramic matrix may be provided under the anti-wetting surface layer of Figures 3A, 3B and 4.
[0071] Thus, the environmental barrier stacking could include, from the deepest to the most superficial: - a layer of silicon 12; - a ceramic layer 10; - optionally, one or more electrically conductive layers 16 alternating with one or more ceramic layers 10, - a layer containing inclusions of noble metal or a noble metal alloy in a ceramic matrix; and - a surface anti-wetting layer as described for figures 3A, 3B and 4.
[0072] Reference is now made to figures 6, 7 in order to discuss experimental results obtained.
[0073] Figure 6 shows a part without an anti-wetting surface coating, and Figure 7 shows a part with an anti-wetting surface coating. More specifically, the part illustrated in Figure 6A has a ceramic matrix composite substrate 6 with silicon carbide fibers and matrix, and a solid CMAS 4 powder deposited on the upper surface of the part. In Figure 6B, the part undergoes a heat treatment at 1300°C for five hours, and the CMAS melts. In Figure 6C, it can be seen that after this heat treatment, the CMAS spread over a large part of the substrate, even extending onto the rear surface of the part. This is complete wetting by the CMAS. The part shown in Figure 6C is the rear surface of the part, while Figures 6A and 6B are the front surfaces. This demonstrates the extent of CMAS penetration into the part.
[0074] In contrast, the part illustrated in Figure 7A comprises a ceramic matrix composite substrate 6 with silicon carbide fibers and matrix, and an anti-wetting surface layer 14 made of platinum on the upper surface of which a solid CMAS 4 powder is deposited. In Figure 7B, the part of Figure 7A undergoes heat treatment at 1300°C for five hours and contact with CMAS. Figure 7C shows the rear face of the part, and it can be seen that after this heat treatment, the spreading of the CMAS 4 on the part is more limited: the CMAS has not attacked the rear face of the part.
[0075] Reference is made to [Fig. 8], which represents a second experimental result. A first sphere 25, composed of 20% yttrium monosilicate and 80% CMAS, a second sphere 26, composed of 20% yttrium disilicate and 80% CMAS, and a third sphere 27, composed of 60% ytterbium disilicate and 40% CMAS, were placed on cups. These cups were made of an alloy consisting of 95% platinum and 5% gold, thus corresponding to the material of an anti-wetting surface layer. Each cup, containing a sphere of material, underwent a heat treatment at 1300°C for 165 hours. As can be seen in [Fig. 8], after this heat treatment, none of the spheres of material completely spread out on the cups, demonstrating the non-wetting behavior of the platinum / gold mixture with respect to CMAS.
[0076] Reference is now made to [Fig.9] representing a method for obtaining a turbomachine part according to the invention and in particular as described above.
[0077] According to the process of the invention, a turbomachine component comprising a ceramic matrix composite substrate is treated to impart anti-wetting properties and to prevent or limit CMAS attack. This ceramic matrix composite may comprise silicon carbide fibers in a silicon carbide matrix.
[0078] This process includes the formation on the substrate of an environmental barrier stack comprising a silicon layer and an anti-wetting surface layer. Thus, the formation of the stack includes the formation 30 of the silicon layer and the formation 70 of the anti-wetting surface layer.
[0079] The formation 70 of the anti-wetting surface layer can be carried out by dry means such as physical vapor deposition and chemical vapor deposition, by inkjet printing, by electrophoresis or by dip-coating.
[0080] The formation 70 of the anti-wetting surface layer may also include sintering thereof.
[0081] The process may also include the formation 40, 60 of one or more ceramic layers, the first of which is on the silicon layer.
[0082] The formation of the ceramic layer(s) can be carried out by electrophoretic deposition. Electrophoretic deposition can be performed using a voltage between 50 V and 150 V, for a duration of, in particular, between 30 s and 5 min. In general, the applied voltage is higher for the deposition of ceramic layers (from the second layer onwards) onto the electrically conductive layers than for the deposition of the ceramic layer (first) onto the silicon layer. For example, the deposition of the first ceramic layer onto the silicon layer can be carried out at a voltage of 80 V for 1 min and 30 s; and at 120 V for 2 min for subsequent ceramic layers.
[0083] Sintering can be carried out at the end of the formation of each ceramic layer. For example, S120 sintering can be carried out at a temperature between 1200 °C and 1350 °C, in particular for a duration of between 5 h and 20 h. For example, at a temperature of 1350 °C for 10 h.
[0084] In the case where there is formation of a plurality of ceramic layers, the process also includes the formation 50 of one or more electrically conductive layers alternating with the ceramic layers.
[0085] The formation 50 of the electrically conductive layer(s) can be carried out by dry means such as physical vapor deposition, chemical vapor deposition or inkjet printing.
Claims
Claims
1. Turbomachine part comprising a ceramic matrix composite substrate (6) coated with an environmental barrier stack (8) comprising an anti-wetting surface layer comprising a noble metal or an alloy comprising at least one noble metal.
2. A turbomachine part according to claim 1, wherein the anti-wetting surface layer is a layer of noble metal or an alloy layer comprising at least one noble metal.
3. A turbomachine part according to claim 1, in which the anti-wetting surface layer comprises inclusions 20 of noble metal or of an alloy comprising at least one noble metal in a ceramic matrix.
4. A turbomachine part according to claim 3, wherein the noble metal is gold.
5. Turbomachine part according to one of the preceding claims, in which the environmental barrier stack comprises under the anti-wetting surface layer one or more ceramic layers alternating with one or more electrically conductive layers of noble metal, of an alloy comprising at least one noble metal or of graphite.
6. A turbomachine part according to claim 5, wherein the ceramic layer(s) (10) are made of a rare earth monosilicate or a rare earth disilicate, preferably the rare earth is yttrium, ytterbium or yttrium-ytterbium.
7. A turbomachine part according to one of the preceding claims, wherein the ceramic matrix composite substrate (6) comprises silicon carbide fibers and a silicon carbide matrix.
8. Method for obtaining a turbomachine part comprising a ceramic matrix composite substrate (6) coated with an environmental barrier stack (8), characterized in that it comprises during the formation of the environmental barrier stack: - the formation of an anti-wetting surface layer (14) comprising a noble metal or an alloy comprising at least one noble metal.
9. Method according to claim 8, further comprising, forming under the anti-wetting surface layer (14), one or more ceramic layers alternating with one or more electrically conductive layers of noble metal, of an alloy comprising at least one noble metal or of graphite.
10. Method according to one of claims 8 or 9, in which the formation of the electrically conductive layer(s) is carried out by a dry method such as physical vapor deposition and chemical vapor deposition, by inkjet printing or by electrophoresis.
Citation Information
Patent Citations
Method of forming a coating resistant to deposits and coating formed thereby
EP1335040A2
Protection of thermal barrier coating with an impermeable barrier coating
US5871820A