Chemical modification of solids as backbones for controlled deposition of metal or bimetallic nanoparticles for tuning surface and antibacterial properties

By employing diazonium salts with controlled reduction methods, the surface modification of diverse substrates allows for uniform metal nanoparticle deposition, addressing the limitations of existing methods and enhancing antibacterial properties on non-conductive surfaces.

GB2592233BInactive Publication Date: 2024-10-02FAKHRADIN MIRKHALAF +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
GB2020002384
Authority / Receiving Office
GB · GB
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-02-20
Publication Date
2024-10-02
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing surface modification methods using diazonium compounds are limited by their requirement for conductive substrates and often result in uncontrollable multi-layered coatings and contamination, making it difficult to modify non-conducting surfaces and maintain uniformity.

Method used

The use of diazonium salts, such as benzoic and decylbenzene diazonium tetrafluoroborate, with controlled reduction methods, including ultrasound and microwave-assisted reductions, to achieve covalent attachment on various substrates, including non-conductive surfaces, allowing for the formation of monolayers and subsequent metal nanoparticle deposition with tailored size and shape.

Benefits of technology

This approach enables strong, uniform bonding of metal nanoparticles to diverse surfaces, preventing environmental release and effectively reducing bacterial adhesion and biofilm formation, while avoiding the use of hazardous chemicals and ensuring robustness against sterilization processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000002_0000
    Figure 00000002_0000
  • Figure 00000003_0000
    Figure 00000003_0000
  • Figure 00000004_0000
    Figure 00000004_0000
Patent Text Reader

Abstract

A method of tuning surfaces and their antibacterial properties including hydrophobicity and bacterial adhesion comprising the creation of a backbone structure for the in situ formation of metal nanoparticles on metallic and non-metallic surfaces. Preferably the surface is first functionalised through chemical or electrochemical reduction of a diazonium salt with carboxyphenyl or decylphenyl functionalities, followed by the controlled reduction of metal salts into metal nanoparticles. The functionalisation is preferably on a silica or alumina substrate and the nanoparticles are preferably silver and / or copper. The surfaces may form antibacterial and antibiofilm coatings on wound dressings and medical devices.
Need to check novelty before this filing date? Find Prior Art

Description

1 .Background of the Invention 1.1. Surface modification of solid supports with diazonium compounds [0001 ] Modification of the surfaces of such materials, for example by grafting of functional groups, has applications in a wide variety of fields. For instance, organic layers on electrode surfaces can be used to modify the electrocatalytic behaviour of the electrode and / or to improve the uniformity of subsequent metal deposition. Such modified electrode surfaces can be used in fuel cells, batteries, solar cells, metal corrosion, electrocatalysis, sensors, drug delivery and in other electrochemical applications.

[0002] Many other materials benefit from surface modification in order to alter their properties or to immobilise specific chemical functionalities which permit coupling to other moieties. For example, organic groups can be grafted onto metal surfaces to impart the ability to bind to other chemical or biological entities; carbon fibres can be modified by binding to epoxy resins to form carbon composite materials having improved mechanical properties; carbon nanotubes can be functionalised to modify their properties (e.g. to prevent bundling); and silicon wafer surfaces can be functionalised to modify their performance. Current methods for surface modification include the grafting of organic groups to carbon or metal surfaces via the chemical or electrochemical reduction of the corresponding diazonium derivatives. Due to their spontaneous surface reactivity in the presence of reducing agents, diazonium derivatives have also been reported for use in electroless grafting of organic residues to metal nanoparticles (Mirkhalaf et al. J. Am. Chern. Soc. 128: 7400-7401,2006) and Indium Tin Oxide (ITO) surfaces (Mirkhalaf et al., Langmuir, 27: 1853-1858,2011).

[0004] Electrochemical reduction of diazonium derivatives is the most widely used method for coating metal and carbon-containing surfaces, especially electrode materials. In such methods, a diazonium salt of the desired organic group is electrochemically reduced to form a highly reactive organic radical with the spontaneous elimination of dinitrogen. The resulting radical can then form a covalent bond with a conducting or semi-conducting surface.

[0005] For example, US 2002 / 0144912 discloses a method in which organic diazonium salts are electrochemically reduced in a protic solvent in acidic medium leading to binding of the organic group to the surface of the carbon-containing material. In the electrochemical process, the carbon-containing substrate forms the negative electrode and is maintained at a potential value such that it can donate an electron to the diazonium salt. Cathodic reduction of the diazonium salt is effected either by repetitive cyclic voltammetry in a potential range in which the diazonium salts are reduced, or by electrolysis at a potential which is more negative than the reduction potential of the diazonium salt. The resulting organic radical binds to a carbon of the carbon-containing electrode. A disadvantage of this particular method is that the substrate to be coated must be conducting (or semi-conducting). Such electrochemical methods are thus not suitable for modifying the surfaces of nonconducting substrates, e.g. non-conducting fabrics, polymeric and inorganic materials.

[0006] There are also further disadvantages associated with electrochemical methods, which involve the reduction of diazonium species. The radicals formed on electrochemical reduction of diazonium salts are highly reactive and have a tendency to react with one another to form dimers or other polymeric species before bonding to the substrate surface. This can lead to the formation of multi-layered coatings (which may, in some cases, be undesirable) and, more generally, to difficulties in controlling the extent of surface coverage. Furthermore, the conventional use of both chemical and electrochemical reducing agents leads to the formation of contaminants during the grafting process which need to be removed. These contaminants can also result in undesirable side-reactions taking place

[0007] Any diazonium salt whose organic residue, R, in radical form is stable enough to covalently bind to a substrate surface may be used in the method of the invention. Suitable diazonium salts are those of the formula RN2+X'where R is an organic residue and X- is an organic or inorganic counteranion (e.g. selected from halides, sulphates, phosphates, perchlorates, tetrafluoroborates, carboxylates and hexafluorophosphates, etc.). Ultrasound-assisted reduction of such salts may be represented as follows: RN2+^ RN2-R-+ N2

[0008] Diazonium salts can easily be prepared using well known syntheses. These may, for example, be prepared in a one-step process from a wide range of anilines (diazotisation of the aniline derivative readily leads to the formation of an aryl diazonium compound). Alternatively, the diazonium salts may be prepared by reaction of the corresponding amine with sodium or potassium nitrite in a mineral acid. If required, the desired diazonium compound can be generated in situ (S. Branton and D. Belanger, J. Phys. Chem. 2005, 109, 24401).

[0009] The diazonium salt concentration may be varied according to the desired extent of surface modification and the nature of the substrate surface. Suitable concentrations may readily be determined by those skilled in the art.

[0010] Typically, the molar concentration of the diazonium salt will be between about 1 mM and 20 mM, preferably around 10 mM.

[0011] Substrate surfaces which may be modified according to the invention include carbon-containing surfaces such as those comprising carbon materials (carbon black, glassy carbon, carbon powder, the surfaces of carbon nanotubes , diamond, synthetic diamond nanopowders, doped diamond substances and graphite), metal oxides (e.g. aluminium oxide, iron oxide, titanium dioxide) and silicon dioxide (silica) 11 05 20 11 05 20 particles. Such materials may take any form, such as fibres, powders, felts, fabric, beads, composites, particulates, etc. Metal surfaces and metal nanoparticles (including those which comprise alloys) may also be modified according to the methods herein described and may include, in particular Pt, Ag, Au, Pd, Zn, Ti, Fe, Cu, Co, Ni or stainless steel. Semi-conducting and non-conducting surfaces may also be suitably modified. Semi-conducting surfaces include those comprising silicon or indium doped tin oxide (ITO) surfaces (Mirkhalaf etal., Langmuir, 27: 1853-1858, 20110). The term "substrate surface" as used herein is to be construed broadly and is considered to encompass the surfaces of particles (e.g. nanoparticles) and beads, etc. 1.2. Metal Nanoparticles as Antibacterial Agents

[0012] The most commonly used metal nanoparticles for the application as antibacterial materials is silver (Ag NPs) which are being used widely in various products including wound management. The antimicrobial activity of these materials is associated with a potential environmental risk once these NPs are discharged into the environment. Therefore, there is an excessive concern about leaching these NPs from products into the environment thus causing toxic effects when they are exposed to live species. It is known that the toxic effect of these NPs is highly dependent to their size and shapes (J. Fabrega etal, Environ. Sci. Technol., 2009, 43, 7285). Wound dressings containing silver nanocrystals (e.g. ACTICOAT® from Smith & Nephew) are created via a physical vapour deposition process to form nanocrystalline structures with large accessible surface area. However, the bonding between these crystalline silvers and the dressing support are weak and they can be easily released to the environment. Due to the increasing use and bulk production of these products, they will cause serious risks to the environment. Herein, an alternative route for the bulk production AgNPs on medical device is disclosed. This procedure, allows strong bonding of these NPs and other species on fabrics, metals and non-metallic supports and thus the release of toxic materials to the environment is avoided. The procedure involves simple metal deposition of metal ions after their electrostatic adsorption onto negatively charged template molecules covalently attached on solid supports. This template deposition allows to control size and shape of deposited metal NPs by selecting suitable molecular templates and deposition conditions.

[0013] Biofilms are found everywhere, the majority of bacteria spend significant fractions of their lives adhering to the surfaces. Their adherence is a major health issue. Bacteria concentrated in biofilms are up to 1,000 times more resistant to antibiotics than those suspended in liquids. The fixation of antibacterial groups on surfaces can prevent formation of biofilms. 2. Details of Invention 2.1. Surface Modification of Fabrics, Metals and oxides (silica or alumina particles)

[0014] In order to functionalise fabrics, metals and particles with covalent attachment, the reduction of the corresponding diazonium salts are used. Diazonium salt of benzoic was either synthesised and separated or made in situ followed by the attachment to the supports. 2.1.1. Procedure 1 Synthesis of 4-carboxybenzene diazonium tetraflouroborate salt (BAD) and 4-decylbenzene diazonium tetraflouroborate (DBD):

[0015] 12 gr p-aminobenzoic acid is dispersed in 50 ml water to form a suspension. In order to improve dissolving, a few drops of 4 M NaOH is added with stirring. Then 200 ml HCI (1:1) is added with strong stirring in an ice bath. Then 9.8 gr NaNo2 is added slowly in several portions with strong stirring in the ice bath. After one hour stirring, 100 ml HBF4 is added with continued stirring in the ice bath for further one hour. The solution was left to the yellow precipitate to be settled down an then filtered on a sintered glass funnel and dried under the vacuum (yield=4.7 gr). For DBD, same procedure but 4-amino decylbenzene was used as the starting material.

[0016] The product is soluble in alkaline water and its reaction with alkaline beta-Naphtol solution gives a deep red precipitate confirming the presence of diazonium groups. ATR-FTIR and Raman spectra of the product show diazonium group. 11 05 20 Figure 1. Raman reflectance spectra of the product (excitation laser= 785 nm). Peak at 2309 cm-1 represents diazonium groups and peaks at 1710 cm-1 show carboxylic acid functionality. Peaks correspond to the ring can also be assigned.

[0017] The product was used for the attachment on various solid supports including: carbon powder and fibre, silica, alumina and dressing fabrics. The reduction of the diazonium salt on various supports was achieved by using either strong or weak reducing agents. 2.1.2. Procedure 2: Example 1: Reduction with strong reducing agent;

[0018] 0.5 gr BAD is dissolved in either iso-propanol or water containing a few drops of surfactant (Triton-Xi 00) to improve solubility. Solid samples to be functionalised were immersed in this solutions and the reduction of BAD is taken place by adding droplets of sodium borohydride (0.05 gr NaBH4 in 50 ml water) in a sonicating bath. The complete reduction of diazonium leads to evolving nitrogen gas and the covalent attachment of carboxyphenyl functionalities. The modified fabrics are washed with water in the sonication bath to remove physically adsorbed materials and have a final light yellow colour. Modified powders are vacuum filtered and washed with water several times. Example 2: Reduction with a user friendly procedure: 11 05^0

[0019] This procedure does not require strong reducing agents and is user and environmental friendly. The formation of reactive radicals from polymers and alcohols and their reductive effects for the reduction of metal ions leading to the formation of metal NPs have previously been reported (C. E. Hoppe, Langmuir, 2006, 22, 7027; J. Kou, Chern Comm., 2013, 49, 692).

[0020] Herein, we report the reduction BAD by poly vinyl pyrrolidone (PVP-40) and / or glycerol together with microwave radiations instead of using hazardous strong chemical reducing agents.

[0021] 0.5 gr BAD is dissolved in 50 ml water containing few drops of surfactant (Triton-Xi 00) with stirring, then 1 gr PVP-40 (Aldrich) is added and after complete dissolving, solid samples immersed in the solution. The container is then covered with a lid and left in a microwave, high power for 5 min. Then, the samples are washed with water. The modified samples are then used for the templated attachment of NPs and the quaternary ammonium salt. 2.1.3. Procedure 3: modification with a mixture of two diazonium compounds

[0022] The formation of mixed monolayers with different chain lengths and functionalities can be used to tune size and shape of deposited metal NPs on these monolayers as templates. In this procedure, two monolayers of carboxyphenyl and decylphenyl are used. One monolayer contains carboxylic acid functionality and the other contains long alkyl chain thus providing narrow channels for the formation of metal NPs with tuned sizes and shapes after the deposition. 23] 0.2 gr decylaniline (Aldrich) and 0.2 gr p-aminobenzoic acid are dissolved in 30 ml propionic acid. The solution is placed in an ice bath with strong stirring and 0.2 gr sodium nitrite (NaNO2) was added in several portions with strong stirring for 30 min. Then, 10 ml tetrafolouroboric acid (HBF4) was added and further stirred on the ice bath for 30 min. The solid crystals can be filtered over the vacuum. The crystals are dissolved in iso-propanol and in the presence of the solid support, the diazonium is reduced by using a reducing agent. Alternatively, the solution without separation of the solid as outlined above.

[0024] The modified samples do not show diazo signal (-N=N) at 2309 Cm-1 on both ATR-IR and Raman spectra representing complete reduction of the diazonium groups after the attachment. 2.1.4. Formation of mixture of two monolayers via electrochemical reduction Scheme 1. Synthesis of 4-dcylbenzene diazonium tetraflouroborate (DBD) and 4-carboxybenzene diazonium tetrafolouroborate (BAD)

[0025] 0.3 gr of each diazonium were dissolved in 20 ml of NaNO3 0.1 M, two drops of Triton X-100 to improve dissolving in water. For the mixture of the diazonium salts, 50:50 by weight of the two diazonium salts were used. Three cycles were performed at a scan rate of 50 mV / s. In order to ensure complete electrode grafting, the WE was further kept at the reduction potential for 60 seconds before taking the electrode out. The electrode was then rinsed thoroughly and dried in air. Scheme 2. Schematic representation of the modification types Scheme 3. Diazonium reduction and possible bond formations on solid surfaces and possible cross-linking due to the formation of radicals 11^05 20 2.1.5. Electrochemical Grafting

[0026] Figure 3 shows the grafting scans of BAD on a stainless steel (SS) slide between +0.7 to -0.7 Volt starting from the positive potential. For the first scan, a strong reduction current around -0.45 V was observed. It is known that the reduction of the diazonium salts leads to the formation of aryl radicals which are very active and bind immediately onto metal surfaces to form M-C covalent bonds [chehimi, m. (Ed), 2012, Aryl diazonium salts: New Coupling Agents in Polymer and Surface Science. Wiley-VCH]. For the second scan, however, the reduction current is extensively reduced representing that most of the surface attachment points are populated by the molecular film as also observed previously [F. Mirkhalaf, K. Tammeveski and D.J. Schiffrin, Phys. Chern. Chern. Phys., 2004, 6, 1321-1327], For the third cycle, the current is further shrinks due to the extensive coverage of the surface by the molecular film. In order to ensure a full monolayer is obtained, the electrode was kept at -0.6 V for 60 seconds. 2.1.6. Electrochemical deposition of metal NPs on modified supports For the electrodeposition of the metal nanoparticles (e.g. Ag), the modified supports with the above functionalities are immersed in a 0.01 M solution of AgNo3 for 30 min, then removed and rinse gently with water. The electrodeposition is then carried out in a 0.1 M supporting electrolyte by applying a pulse voltages of -0.8 V at 0.5 sec and sample time of 0.05 sec. The pulse deposition is carried out in a 3-electrode cell comprising a Pt counter electrode, Ag / AgCI reference electrode and the modified support as working electrode. 2.1.7. Non-electrochemical deposition of metal NPs on modified supports

[0028] The modified supports functionalised with caboxyphenyl or mixture of carboxyphenly+decylphenyl groups are dipped in an alkaline solution (20 ml NaOH 0.2 M) followed by washing to induce carboxylate anion formation. The samples are then dipped in metal salts (e.g. 20 ml AgNO3 0.01 M) with sonication for 5 min for the formation of ion pairs between carboxylate anions with metal cations. The samples are then removed and washed several times with sonication. The samples are then reduced in pure water (20 ml) containing either strong reducing agent (NaBH4) with sonication or weak (0.1 gr PVP-40+ few drops glycerol) with microwave as above. The samples are then washed several times with sonication.

[0029] Bimetallic nanoparticles of silver-copper can also be formed by mixture of two salts of the corresponding metals in the immersing solution.

[0030] It is generally accepted that the formation of molecular films on surfaces after the reduction of diazonium salts could to the generation of multilayers in addition to the monolayer films (J. pinson in M. Chehimi (Ed), Aryl Diazonium Salts, Wiley-VCH, 2012). Therefore, it is proposed multilayer films according to Scheme 3 and 4 are formed in the present case according to the support material and experimental condition. Therefore, multilayers of individual metal clusters leading to controlled size and shape with high surface area active NPs are also expected (Scheme 4).

[0031] Therefore, the present innovation allows formation of high surface area and active NPs films on various supports that are strongly boded to the surface and do not release to the environment under harsh physical or biological conditions. Scheme 4. Schematic representation of formation of silver nanoparticles as a result of controlled reduction. Figure 2. Viscose dressing modified with carboxyphenyl functionalities and deposited with silver NPs. 05 20 2.2. Experimental Characterisations

[0032] Figure 4 depicts the grafting scans of DBD on a Ti slide with the same experimental condition. The reduction peak for this compound shows a maximum at around -0.35 V for the first scan. For the second scan, the current is shifted to more negative voltage and diminished due to the population of the surface in the first scan. Oxygen reduction could start at -0.6 V that might interfere with extending the scan to more negative potentials in this case. Again a full monolayer was ensured by keeping the WE at -0.5 V for 60 s. if©033] Figure 5 represents cyclic voltammograms for the grafting of a mixture of BAD and DCBD (50% each). For the first scan, two reduction peak are observed corresponding to the reduction of two different diazonium compounds. The first peak appears around -0.3 V corresponds to the reduction of DBD as also observed for the compound alone (Figure 4). The second peak appears at more negative potential corresponds to the reduction of BAD as observed in Fig 3. The difference between the reduction potentials is probably due to two different groups with different activation properties to the aromatic ring due to their electron donating and electron withdrawing properties for the decyl and -COOH functionalities respectively. This could affect the rate of the electrochemical reduction and thus the reduction potentials. Again, the consecutive scans represent decreasing in peak currents due to the population of the surface as mentioned before. The three scans are followed by keeping the WE at -0.65 V to ensure complete coverage of the surface. Figure 3. Attachment cycles of BAD on Stainless steel (SS) slides for first three cycles Figure 4. Attachment scans of DBD on Titanium slides (Ti) for first three cycles Figure 5. Attachment cycles of mixture of BAD + DBD (50:50 by weight) on Ti slides for first three cycles

[0034] Figure 6 demonstrates FTIR RA spectrum of a SS-DC-BA slide compared with an unmodified SS coupon. The modified slide shows strong bands at 1100 cm-1 for aromatic ring breathing, CH, OH stretching at 2870 and 2920 cm-1, C=O at 1717 cm-1 and COOH bands as discussed above. Figure 6. FT-IR reflection-absorption spectrum of Stainless Steel slides before and after electrochemical attachment of mixed monolayers composed of DCBD + BAD (50:50).

[0035] In order to ensure the robustness of the attached organic molecules onto metal surfaces and due to the essential sterilization of medical implants and devices before their use, the modified SS-BA with and without Ag NPs were check by FT-IR before and after autoclaving (data not shown). The FT-IR scans showed that the autoclaving process for 30 min used for sterilization of the slide does not make significant change to the spectra representing a robust molecular film which withstands with the sterilization process. Water contact angle measurements were carried out in order to determine the hydrophobicity of modified metal slides. This is of particular importance due to the effect of hydrophobicity and functionality of metal surfaces to the bacterial adhesion and thus biofilm formation [R. Oliveira, J. Azeredo, P. Teixeira and A. P. Fonseca, HYDROPHOBICITY AND ADHESION, (2001), BioLine®, 11-22], A linear relationship between hydrophobicity and adherence of bacterial cells have been observed. In fact, the interaction between two hydrophobic entities was shown to be favored because they can enter into closer contact through the facilitated “squeezing of water” in between [Oliveira 2001],

[0037] Figure 7 shows water contact angle measure on bare and surface modified Ti slides. Low value of contact angle for bare clean Ti slide represent a hydrophilic surface. However, functionalization of the surface with BA, increases the value of contact angle indicating some degree of hydrophobic surface due to the introduction of the caboxyphenyl functionality. The hydrophobicity of the surface is extensively increased with the attachment of decylphenyl functionality (Ti-DB) due to hydrophobic nature of decybenzene molecule. The addition of carboxyphenyl functionality to the latter, leads to slight decrease in contact angle due to polar carboxyphenyl groups (Ti-BA-DB). The deposition of Ag NPs leads to slight increase in contact angle and thus hydrophobicity for all samples probably due to blocking of polar carboxylic acid groups and pits resulting from imperfect monolayers. Figure 7. Water contact angle measurement results for bare and various surfaces modified Ti slides. Figure 8. A): Ag NPs deposited on functionalised silica particles ; B): Ag NP deposited on functionalised filter paper; C); EDS spectrum for silica modified particles to show the presence of Ag signals. The particle size for both cases are between 10-20 nm. Figure 9. A) SEM images of Ag-Cu bimetallic NPs deposited on functionalised viscose dressing fabrics; B) the corresponding EDS spectrum showing Ag and weak Cu signals proving the presence of Ag-Cu bimetallic NPs; C) functionalised alumina particles (0.05 micron) loaded with Ag-Cu nanoparticles. Figure 10. SEM image of Ag nanoparticles synthesized with template deposition onto a titanium slide modified with carboxylic acids 2.3 Antibacterial and Antibiofilm Results 2.3.1. Modified Metal Slides CKP38] The modified slides were used for antibacterial and antibiofilm studies on S. Aureus. Figure 11 shows bacterial adhesion and growth in contact with various samples. LO Bacterial adhesion and growth is highly increased when Ti is modified with carboxyphenyl functionality (i.e. Ti-BA). This phenomenon is less significant for the ___ decylphenyl functionality (i.e. Ti-DB) probably due to its hydrophobic nature. 1        However, the adhesion and growth of the bacteria are extensively increased when a T”     mixture of both of the two functionalities were used for the modification of Ti (i.e. Ti- BA-DB). The non-uniform nature of the film due to two different sizes, polarities, and hydrophobicity extensively supports strong and irreversible adhesion of the bacteria to the surface leading to biofilm formation. These results show that the bacterial adhesion is not linearly dependent to the hydrophobicity of the surface.

[0039] Figure 10 shows that the deposition of Ag NPs on the molecular film functionalities, extensively reduces the bacterial adhesion and growth due to the strong antibacterial action of Ag NPs. The value of growth and adhesion of the bacteria for the sample Ti-BA-DB-Ag 25 and 26 times are reduced respectively compared to the surface without Ag NPs (i.e. Ti-BA-DB). This reduction for the case of Ti-BA-Ag for both adhesion and growth of the bacteria is 42 times less than that for Ti-BA. The degrees of growth and adhesion reduction for Ti-DB-Ag compared to those of Ti-DB are 22 and 21 times respectively. Although it is difficult to make an absolute interpretation, but from these results it is safe to conclude that the degree of the bacterial reduction could be due to several parameters including surface morphology, hydrophobicity and polarity of surface molecules AND population and sizes of Ag NPs formed. The latter could be due to the effects of former parameters on the adsorption, seed formation and growth of Ag NPs on the film.

[0040] The results show that, by the careful manipulation of the surface, it is possible to tune the bacterial adhesion to the surface thus control bacterial biofilm formation on these SMART surfaces. Figure 11. Growth (top) and adhesion (bottom) of S. Aurous onto Ti slides attached with various monolayers with and without Ag nanoparticles compared with bare Ti. 2.3.2. Nanoparticles Deposited on carbon Fibre [0041 ] Deposition of silver and silver / copper on carbon fibres modified with BAD as above compared with those without the template functionality and metal. The measurement of bacterial growth for two bacteria (E. Coli and S. Aurous) were carried out with the following procedure: a. Measure 70 mg of fibres, bake to sterile and put them in universals; b. Add 10 ml LB medium and 6 pl of each bacteria to each universal, c. Incubate at 37°C and 225 RPM. d. Measure the OD 550 after 6 hours.

[0042] The results are outlined in Figure 12. As seen, the growth of the two bacteria (E. coli and S. Aureus) for fibres modified with BA followed by deposition of Ag-Cu bimetallic NPs is minimum confirming the highest antibacterial properties compared to C-BA. Figure 12. Bacterial growth in the presence of carbon fibres with various modifications and metal depositions: 1. C-BA; 2. C-BA-Cu; 3. C-BA-Ag; 4. C-BA-AgCu; 5. C-Ag; 6. C-Cu As seen from the graph in Fig 12, C fibre-BA has not much effect on bacterial growth, deposition of Cu has not a significant effect. However, the deposition of Ag inhibits significantly the growth of E.Coli with minor effect on S. Aureus. In addition, the deposition of Ag-Cu bimetallic nanoparticles inhibits significantly the growth of both bacteria. 2.3.2. Modified Dressings and other supports

[0044] Viscose fabrics functionalised with carboxyphenyl groups based on procedures outlined in section 1 above. Standard viscose fabric dressings were used for modification with BAD followed by metal deposition (Scheme 4). The three bacterial strains were harvested from Tryptone Soya Agar (TSA) plate and suspended in 20 ml of TSA to give an OD59o=0.13, which corresponds to a bacterial concentration of 108 cfuml'1 ad diluted to a final concentration of 105 cfuml’1. The modified dressings were cut into 1.5 cm2 pieces and added to 4 ml of each bacterial suspension and they were incubated at 370C and 50 rpm for 24 hours. Figure 13. Standard viscose dressings (D) modified with modifiers with and without metal deposition: 1: D ; 2: D-BA; 3: D-BA-Cu; 4: D-BA-Ag; 5: D-BA-AgCu.

[0045] As seen from Fig. 13, the best results are obtained with a dressing fabric functionalised with a mixture of the two modifiers (i.e. decyl phenyl and carboxypheny) followed by silver deposition with maximum inhibition to the growth of all of the three bacteria compared to dressings modified with modifiers alone. This probably corresponds to the controlled deposition of silver nanoparticles with tailored size and shape with maximum antibacterial effect. The latter effect can be related to the formation of long channels due to the presence of long chain decyl benzene groups that drives the formation of silver nanoparticles in an ordered shape and size as shown in Scheme 4. Bimetallic Ag-Cu nanoparticles also show good antibacterial activity. Dressings containing copper deposited particles do not show strong antibacterial effect.

[0046] It is also shown that the increase of the surface area of metal NPs attached to the dressings increase antibacterial properties of the coating. A comparison of Silica or alumina NPs when they are modified with the above procedure with those dressings modified without the use of these base materials, confirms that the antibacterial effects of the latter dressings with high surface area silica or alumina are enhanced on the bacteria models selected (i.e. S. Aureus, E. Coli) as shown in Figure 14. Figure 14. Antibacterial effect of templated metal deposition on functionalised dressings modified with; 1:CBD, 2:CBD-Ag,3:CBD-AgCuZn, 4:CBD-AgZn, 5: Silica-CBD-AgCu, 6: Alumina-CBD-AgCu. Summary: This invention relates to the creation of molecular backbones for the facile nucleation and formation of metal and bimetallic nanoparticles on conductive and non-conductive surfaces for tailoring surface properties including hydrophobicity / weteability and bacterial adhesion and growth onto surfaces. The immediate application as antibacterial and antibiofilm coatings on wound dressings and medical devices is disclosed herein. 11 05 20

Claims

1. An antibacterial surface comprising a covalently attached molecular backbone structure for the controlled inclusion of deposited metal nanoparticles wherein the backbone comprises carboxyphenyl and decylphenyl functionalities.

2. The surface of claim 1 wherein the metal nanoparticles are selected from the group comprising silver, copper, zinc or their bimetallic nanoparticles.

3. The surface of claim 2 wherein the metal nanoparticle is Ag-Cu.

4. The surface of any one of the previous claims wherein the surface comprises Silica, Alumina,metals and / or textiles.

5. The surface of any one of the previous claims wherein the surface comprises narrow long channels formed by decyl benzene and carboxyphenyl monoIyer assemblies.

6. The surface of any one of the previous claims comprising a backbone structure comprising phenyl and decylphenyl functionalities, and one or more metal nanoparticle.A wound dressing or medical device comprising an antibacterial surface comprising the as claimed in any one of the previous claims.A method fortuning surfaces and their antibacterial properties comprising depositing onsaid surface of a molecular backbone structure for metal nanoparticles comprising a molecular film to support controlled nucleation of antibacterial metal nanoparticles on metallic and non-metallic surfaces, wherein the backbone is selected from the group comprising carboxyphenyl and decylphenyl functionalities.

9. The method as claimed in claim 8 comprising the chemical or electrochemical reduction of aryl diazonium salts facilitating the controlled deposition of nanoparticles.

10. The method of claim 9 comprising the use of strong and / or weak reducing agents for the reduction of p-benzoic acid and P-decy I benzene diazonium ions leading to covalent binding of carboxypheyl and / or decylphenyl functionalities on solid surfaces.

11. The method of claim 10 wherein the reducing agents used for chemical reduction include mild or strong materials.

12. The method ofdaim 11 wherein the reducing agents used for chemical reduction includeascorbic acid or sodium borohydride.

13. The method of any one of claims 8 to 12 wherein the metal nanoparticles comprise silver, copper, zinc or their bimetallic nanoparticles.

14. The method as claimed in claim 13 wherein the metal nanoparticles are formed through one-step reduction process.

15. The method as claimed in claim 14 wherein the metal or bimetal nanoparticles are formed by electric pulse reduction protocol for conductive surfaces.

16. The method as claimed in claim 15 comprising the useof Poly Vinyl Pyrrolidon (PVP-40) and microwave.^^I7. The method as claimed in claim 8 wherein the surface comprises any one or more of ^^netals, carbon, viscose, cotton, silica, alumina and / or metal oxide particles.^^I8. The method as claimed in claim 8 for the deposition of antibacterial films on wound dressing and medical devices.

Citation Information

Patent Citations

  • Titanium alloy containing antibacterial coating as well as preparation method and application thereof

    CN104357814A

  • Gold nano-particle based antibacterial product and preparation method and application thereof

    CN105597159A

  • Antibacterial composite and method for preparing the same

    US20180049431A1

  • Antibacterial spectacle part and antibacterial treament method

    US20180228160A1

  • System and method for medical or genome data management using blockchain network

    KR102164156B1