Method for recycling spent lithium iron phosphate batteries
The method recycles both cathode and anode materials from lithium iron phosphate batteries, regenerating a high-capacity lithium iron phosphate/C cathode material with a carbon cross-linked structure, addressing the inefficiencies and environmental concerns of existing recycling methods by achieving superior cycle stability and discharge capacity.
Patent Information
- Application Number
- GB2023013110
- Authority / Receiving Office
- GB · GB
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-06-24
- Filing Date
- 2022-09-28
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2042-09-28
AI Technical Summary
Current methods for recycling lithium iron phosphate batteries only recover the cathode material using a wet process with low efficiency and high costs, resulting in suboptimal performance and limited applications for the recycled product, while neglecting the anode material and introducing environmental pollution.
A method that simultaneously recycles both cathode and anode materials from lithium iron phosphate batteries through preprocessing, using a mixed acid solution for graphite treatment, and a calcination process to regenerate a high-capacity lithium iron phosphate/C cathode material with a carbon cross-linked structure, enhancing lithium ion transmission and structural stability.
The method achieves high cycle stability and discharge capacity comparable to new lithium iron phosphate cathode materials, with improved raw material utilization and cost performance, suitable for large-scale recycling with excellent electrochemical performance.
Abstract
Description
Generally speaking, the residual energy density of the waste lithium iron phosphate power battery can still reach 60 Wh / kg to 90 Wh / kg, and the recycling life of the waste lithium iron phosphate power battery can also reach 400 cycles to 1,000 cycles. The raw material cost of the waste lithium iron phosphate is generally less than 10,000 RMB / ton. Moreover, the lithium iron phosphate battery contains more harmful substances, which is easy to cause environmental pollution. Therefore, the cost performance and environmental protection of the industry of effectively recycling the lithium 20 iron phosphate waste battery are very high. However, in the prior art, only the cathode material in the lithium iron phosphate battery is recycled, and the cathode material mainly recycled and further regenerated by a wet method. This method introduces many kinds of production reagents and high-demand process steps, and the recycling efficiency is not high, which leads to the increase of the cost of the final recycled product. At the same time, the performance of the recycled product is not ideal, 25 the performance between batches cannot be matched, which makes the available fields of the recycled product are few. SUMMARY Based on the shortcomings of the prior art, the object of the present disclosure is to provide a method for recycling a lithium iron phosphate waste battery. By using the method, a cathode material 30 and an anode material in the waste lithium iron phosphate battery can be simultaneously recycled, 07 02 24 and a high-capacity regenerated lithium iron phosphate / C cathode material can be prepared with the recycled cathode and anode materials. To achieve the above object, the technical solutions used by the present disclosure are as follows: A method for recycling a lithium iron phosphate waste battery comprises the following steps of: 5 (1) preprocessing a cathode material: subjecting a cathode plate of the lithium iron phosphate waste battery to washing, impurity removing by heating, and sieving to obtain a lithium iron phosphate powder A; (2) preprocessing an anode material: after washing and drying an anode graphite plate of the lithium iron phosphate waste battery, adding the obtained graphite powder into a mixed acid solution, 10 stirring and reacting for 5 hours to 10 hours to obtain a mixed solution B; wherein, the mixed acid solution is a mixed solution of hydrochloric acid and nitric acid, and a ratio of a mass of the graphite powder to a volume of the mixed acid solution is (100 to 300) g: 1 L; and then, adding an oxidant into the mixed solution B, and heating until the reaction is complete, then adding a reductant for a reduction reaction, and obtaining a modified graphite powder C after heating and heat preservation; (3) preparing a precursor; dispersing the lithium iron phosphate powder A and the modified graphite powder C in deionized water, introducing a soluble ferric salt, PEG, a soluble phosphate and gelatin, uniformly mixing, then adding a lithium salt, and drying to obtain a precursor gel D; wherein a mass ratio of the lithium iron phosphate powder A to the modified graphite powder C and the gelatin 20 is 1: (0.1 to 0.5): (0.01 to 0.5); and (4) preparing a regenerated lithium iron phosphate / C cathode material: calcining the precursor gel D at 600°C to 800°C in an inert atmosphere for 5 hours to 10 hours, washing and drying to obtain the regenerated lithium iron phosphate / C cathode material. In the method for recycling the lithium iron phosphate waste battery according to the present 25 disclosure, it takes the waste lithium iron phosphate contained in the cathode plate as a main body, uses a lithium source, a ferric source and a phosphorus source to supplement lithium to the cathode material for repairing, and meanwhile, rebuilds a new lithium iron phosphate coating layer containing a carbon layer cross-linked structure on a surface of the cathode material to realize regeneration of the lithium iron phosphate. The built coating layer can effectively accelerate the rapid transmission 30 of lithium ions, and meanwhile, can alleviate structural damage of the regenerated lithium iron phosphate in the process of charging and discharging to a certain extent, so that the regenerated material has charge and discharge capacity and stability comparable to that of a newly-made lithium Q7 02 24 iron phosphate cathode material. Secondly, the graphite material in the anode plate is used as a matrix, and the graphite material has more tiny defects because the graphite material undergoes multiple lithium ion interpenetration during the process of charging the battery. After the chemical oxidationreduction method is used to further process and treat the graphite material, the microscopic carbon 5 layer generates obvious expansion and differentiation phenomena, and the obtained modified graphite material has an excellent porous cross-linked structure. The gelatin is used as a cross-linking agent to fully combine the modified graphite material and the raw materials lithium iron phosphate of each coating layer (the gelatin can also form a cross-linked carbon network structure after carbonization), and a specific surfactant PEG (polyethylene glycol) is matched, so that the precursor material is in a 10 relatively dispersed gel state before calcination, and may not precipitate to the bottom, the finally prepared regenerated material has high dispersibility and uniform shape, and the contained lithium iron phosphate active material cannot agglomerate or cannot be supplemented with lithium, and the electrochemical performance is far better than that of a doped lithium iron phosphate material prepared by adopting other carbon sources. Bu using the method, the cathode material and the anode 15 material in the waste lithium iron phosphate battery can be simultaneously used, so that the raw material utilization rate is high, the cost performance is high, and the obtained regenerated material has excellent performance, which is very suitable for recycling large quantities of waste lithium iron phosphate batteries. In addition, the content of the carbon material in the recycled material is relatively low, so the prepared regenerated lithium iron phosphate / C cathode material has high unit capacity and high application prospect. Preferably, in the step (1), the cathode plate is washed with an organic solvent. Preferably, the organic solvent is at least one selected from the group consisting of ethanol, methanol and NMP. Preferably, in the step (1), a condition of the impurity removing by heating is: heating the washed 25 cathode plate to 100°C to 200°C in an inert atmosphere and keep the temperature for 1 hour to 2 hours. In the process of recycling, the lithium iron phosphate cathode material in the waste battery not only contains impurities from inside the battery, such as electrolyte, electrode plate binder, but also introduces other types of substances, such as separating agent, detergent, etc. Therefore, it is necessary to wash with an organic solvent and calcine at low temperature to remove the impurities. 30 Preferably, in the step (2), a concentration of the hydrochloric acid in the mixed solution is 6 mol / L to 8 mol / L, and a concentration of the nitric acid is 1 mol / L to 2 mol / L. Unlike conventional graphite or the reduced graphene prepared by simple HUMMER method, an interlayer spacing of anode graphite layers in the lithium iron phosphate battery after tens of 07 02 24 thousands of lithium deintercalations is usually large. The solvent oxidation by the mixed solution of the hydrochloric acid and the nitric acid with a high concentration can further increase the interlayer spacing between the graphite layers, so that the lithium iron phosphate can be effectively inserted between the layers to form a composite material with a three-dimensional structure subsequently, and 5 organic polymer impurities contained in the graphite can also be effectively removed. Meanwhile, the inventor found that when an oxidation degree of the solvent is too large, the graphite layer will be seriously gelatinized, which will reduce a modification degree of the subsequent oxidation-reduction method. Moreover, it is not conducive to the full dispersion of the lithium iron phosphate in the subsequent process of preparing the precursor by mixing with the gelatin, and the final product 10 performance is not ideal. Preferably, in the step (2), the oxidant is at least one selected from the group consisting of sodium hypochlorite and potassium hypochlorite, and the reductant is hydrogen peroxide. Preferably, in the step (2), a condition of the heating and heat preservation is: heating the reactant to 450°C to 600°C in an inert atmosphere and keep the temperature for 1 hour to 3 hours. Preferably, in the step (3), the soluble ferric salt comprises at least one selected from the group consisting of ferric sulfate, ferric nitrate and ferric chloride. Preferably, in the step (3), the soluble phosphate is ammonium dihydrogen phosphate. Preferably, in the step (3), the lithium salt is at least one selected from the group consisting of lithium carbonate, lithium oxalate, lithium acetate and lithium bromide. 20 Preferably, a molar ratio of Fe3+ in the soluble ferric salt, PO43' in the soluble phosphate and Li+ in the lithium salt is (0.8 to 1): (0.8 to 1): (1 to 1.2). More preferably, a molar ratio of Fe3+ in the soluble ferric salt, PO43' in the soluble phosphate and Li+ in the lithium salt is 1: 1: 1.2. More preferably, a molar ratio of Li+ in the lithium salt to the lithium iron phosphate powder A 25 is (0.05 to 0.1): 1. In the process of the present disclosure, on the basis of the original lithium iron phosphate powder A, it is necessary to regenerate a new lithium iron phosphate coating composite layer on a surface layer of the lithium iron phosphate powder A, and meanwhile, it is also necessary to properly supplement lithium for some of the original lithium iron phosphate powder A which lacks lithium. It 30 is confirmed by the inventor through experiment that a lithium supplement effect of the lithium iron phosphate in the final product is the best when the raw materials are mixed with the above ratio, and the new and old lithium iron phosphate active ingredients have the best performance. 07 02 24 Another object of the present disclosure is to provide a regenerated lithium iron phosphate / C cathode material prepared by the method for recycling the lithium iron phosphate waste battery. According to the recycling method of the present disclosure, the cathode material and the carbon anode material in the waste battery are reprocessed at the same time, and the prepared regenerated 5 lithium iron phosphate / C cathode material has excellent cycle stability and high charge and discharge capacity through a proper coating process. The lithium ion half battery prepared by using the cathode material has a specific discharge capacity of 140 mAh / g after 200 cycles at a multiplying factor of 0.5 C, and has a high coulomb efficiency, which can be completely comparable to a newly-made lithium iron phosphate cathode material. 10 The present disclosure has the below beneficial effects. The present disclosure provides the method for recycling the lithium iron phosphate waste battery, which takes the lithium iron phosphate contained in the cathode plate of the waste lithium iron phosphate battery as a main body, uses a lithium source, a ferric source and a phosphorus source to supplement lithium to the cathode material for repairing, and meanwhile, rebuilds a new lithium iron phosphate coating layer containing a carbon layer cross-linked structure on a surface of the cathode material to realize regeneration of the lithium iron phosphate. The built coating layer comprises the graphite material in the waste lithium iron phosphate anode plate, and gelatin and PEG are matched to be used as precursors to prepare the modified graphite material, so that the modified graphite material has an excellent porous crosslinking structure, which enables the finally prepared regenerated material to have high dispersibility and uniform shape. The contained lithium iron phosphate active material cannot agglomerate or cannot be supplemented with lithium, and the electrochemical performance is far better than that of a doped lithium iron phosphate material prepared by adopting other carbon sources. In the method, the cathode material and the anode material in the waste lithium iron phosphate battery are used simultaneously, so that the raw material utilization rate is high, the cost performance is high, and the 25 obtained regenerated material has excellent performance, which is very suitable for recycling large quantities of waste lithium iron phosphate batteries. In addition, the content of the carbon material in the recycled material is relatively low, so the prepared regenerated lithium iron phosphate / C cathode material has high unit capacity and high application prospect. The present disclosure also provides the regenerated lithium iron phosphate / C cathode material prepared by the recycling method. 30 DETAILED DESCRIPTION In order to better explain the objects, technical solutions and advantages of the present disclosure, the present disclosure will be further explained with reference to specific embodiments and 07 02 24 comparative examples, with the aim of understanding the content of the present disclosure in detail, but not limiting the present disclosure. All other embodiments obtained by those having ordinary skills in the art without paying creative work belong to the protection scope of the present disclosure. Unless otherwise specified, the experimental reagents, raw materials and instruments designed in the 5 embodiments and comparative examples of the present disclosure are all commonly used common reagents, raw materials and instruments, especially the used lithium iron phosphate waste battery. The cathode material and the anode graphite material in the battery are all conventionally purchased raw materials, and the self-made recycled raw materials are also be used. Example 1 10 A method for recycling a lithium iron phosphate waste battery according to an example of the present disclosure comprised the following steps of: (1) preprocessing a cathode material: washing a cathode plate of the lithium iron phosphate waste battery by using a mixed solution of ethanol and NMP (volume ratio of 1: 1), heating to 150°C in an argon atmosphere in a sealed manner, preserving heat for 2 hours, removing impurities, and sieving to obtain a lithium iron phosphate powder A; (2) preprocessing an anode material: after washing an anode graphite plate of the lithium iron phosphate waste battery with ethanol and drying, adding the obtained graphite powder into a mixed acid solution, stirring and reacting for 8 hours to obtain a mixed solution B; wherein, the mixed acid solution was a mixed solution of hydrochloric acid (6 mol / L) and nitric acid (2 mol / L), and a ratio of 20 a mass of the graphite powder to a volume of the mixed acid solution was 200 g: 1 L; and then, adding an oxidant sodium hypochlorite into the mixed solution B, and heating until the reaction is complete, then adding a reductant hydrogen peroxide for a reduction reaction (a mass ratio of the graphite powder to the oxidant to the hydrogen peroxide was 1:0.5: 1), and obtaining a modified graphite powder C after heating and heat preservation for 2 hours at 500°C under an argon atmosphere; 25 (3) preparing a precursor: dispersing the lithium iron phosphate powder A and the modified graphite powder C in deionized water, introducing a soluble ferric salt ferric chloride, PEG, a soluble phosphate ammonium dihydrogen phosphate and gelatin, uniformly mixing, then adding a lithium salt lithium carbonate, and drying to obtain a precursor gel D; wherein a mass ratio of the lithium iron phosphate powder A to the modified graphite powder C and the gelatin was 1: 0.2: 0.04; a molar ratio 30 of Li+ in the lithium salt to the lithium iron phosphate powder A was 0.1: 1; and a molar ratio of Fe3+ in the soluble ferric salt, PO43' in the soluble phosphate and Li+ in the lithium salt was 1: 1.1: 1.2; and 07 02 24 (4) preparing a regenerated lithium iron phosphate / C cathode material: calcining the precursor gel D at 700°C in an argon atmosphere for 8 hours, washing and drying to obtain the regenerated lithium iron phosphate / C cathode material. Example 2 5 A method for recycling a lithium iron phosphate waste battery according to an example of the present disclosure comprised the following steps of: (1) preprocessing a cathode material: washing a cathode plate of the lithium iron phosphate waste battery by using a mixed solution of ethanol and NMP (volume ratio of 1: 1), heating to 200°C in an argon atmosphere in a sealed manner, preserving heat for 1.5 hours, removing impurities, and 10 sieving to obtain a lithium iron phosphate powder A; (2) preprocessing an anode material: after washing an anode graphite plate of the lithium iron phosphate waste battery with ethanol and drying, adding the obtained graphite powder into a mixed acid solution, stirring and reacting for 8 hours to obtain a mixed solution B; wherein, the mixed acid solution was a mixed solution of hydrochloric acid (6 mol / L) and nitric acid (2 mol / L), and a ratio of a mass of the graphite powder to a volume of the mixed acid solution was 200 g: 1 L; and then, adding an oxidant potassium hypochlorite into the mixed solution B, and heating until the reaction is complete, then adding a reductant hydrogen peroxide for a reduction reaction (a mass ratio of the graphite powder to the oxidant to the hydrogen peroxide was 1:0.5: 1), and obtaining a modified graphite powder C after heating and heat preservation for 2 hours at 500°C under an argon atmosphere; 20 (3) preparing a precursor: dispersing the lithium iron phosphate powder A and the modified graphite powder C in deionized water, introducing a soluble ferric salt ferric nitrate, PEG, a soluble phosphate ammonium dihydrogen phosphate and gelatin, uniformly mixing, then adding a lithium salt lithium acetate, and drying to obtain a precursor gel D; wherein a mass ratio of the lithium iron phosphate powder A to the modified graphite powder C and the gelatin was 1: 0.2: 0.04; a molar ratio 25 of Li+ in the lithium salt to the lithium iron phosphate powder A was 0.1: 1; and a molar ratio of Fe3+ in the soluble ferric salt, PO43" in the soluble phosphate and Li+ in the lithium salt was 1: 1.1: 1.2; and (4) preparing a regenerated lithium iron phosphate / C cathode material: calcining the precursor gel D at 650°C in an argon atmosphere for 10 hours, washing and drying to obtain the regenerated 30 lithium iron phosphate / C cathode material. Example 3 A method for recycling a lithium iron phosphate waste battery according to an example of the 07 02 24 present disclosure comprised the following steps of: (1) preprocessing a cathode material: washing a cathode plate of the lithium iron phosphate waste battery by using a mixed solution of ethanol and NMP (volume ratio of 1: 1), heating to 150°C in an argon atmosphere in a sealed manner, preserving heat for 2 hours, removing impurities, and 5 sieving to obtain a lithium iron phosphate powder A; (2) preprocessing an anode material: after washing an anode graphite plate of the lithium iron phosphate waste battery with ethanol and drying, adding the obtained graphite powder into a mixed acid solution, stirring and reacting for 8 hours to obtain a mixed solution B; wherein, the mixed acid solution was a mixed solution of hydrochloric acid (8 mol / L) and nitric acid (1 mol / L), and a ratio of 10 a mass of the graphite powder to a volume of the mixed acid solution was 300 g: 1 L; and then, adding an oxidant sodium hypochlorite into the mixed solution B, and heating until the reaction is complete, then adding a reductant hydrogen peroxide for a reduction reaction (a mass ratio of the graphite powder to the oxidant to the hydrogen peroxide was 1:0.5: 1), and obtaining a modified graphite powder C after heating and heat preservation for 2 hours at 500°C under an argon atmosphere; (3) preparing a precursor: dispersing the lithium iron phosphate powder A and the modified graphite powder C in deionized water, introducing a soluble ferric salt ferric nitrate, PEG, a soluble phosphate ammonium dihydrogen phosphate and gelatin, uniformly mixing, then adding a lithium salt lithium carbonate, and drying to obtain a precursor gel D; wherein a mass ratio of the lithium iron phosphate powder A to the modified graphite powder C and the gelatin was 1: 0.2: 0.04; a molar ratio 20 of Li+ in the lithium salt to the lithium iron phosphate powder A was 0.1: 1; and a molar ratio of Fe3+ in the soluble ferric salt, PO43'in the soluble phosphate and Li+in the lithium salt was 1: 1.1: 1.2; and (4) preparing a regenerated lithium iron phosphate / C cathode material: calcining the precursor gel D at 750°C in an argon atmosphere for 6 hours, washing and drying to obtain the regenerated lithium iron phosphate / C cathode material. 25 Example 4 The only difference between this example and Example 1 was that a mass ratio of the lithium iron phosphate powder A to the modified graphite powder C and the gelatin in the step (3) was 1: 0.5: 0.05. Example 5 30 The only difference between this example and Example 1 was that a mass ratio of the lithium iron phosphate powder A to the modified graphite powder C and the gelatin in the step (3) was 1:0.1: 0.01. 07 02 24 Comparative Example 1 The only difference between this comparative example and Example 1 was that the soluble ferric salt, the soluble phosphate and the lithium salt were not introduced in the step (3). Comparative Example 2 5 The only difference between this comparative example and Example 1 was that the modified graphite powder C in the step (3) was replaced by commercially available graphite. Comparative Example 3 The only difference between this comparative example and Example 1 was that the modified graphite powder C in the step (3) was replaced by self-prepared graphene by using HUMMER method. 10 The specific steps of HUMMER method were as follows: adding 5 g of graphite powder, 1 g of sodium nitrate and 6 g of potassium permanganate into an appropriate amount (about 200 mL) of a mixed solution of high-concentration concentrated sulfuric acid solution and phosphoric acid solution at 0°C in an ice bath, stirring and mixing, adding 6 g of potassium permanganate again, heating to a normal temperature, reacting for 12 hours, adding an appropriate amount of hydrogen peroxide for completely reaction, drying the resulted product to be viscous, dispersing a part of the viscous product in water, adding an appropriate amount of hydrazine hydrate under an ultrasonic condition, reacting for 24 hours completely, washing the obtained product with ethanol and water, and drying to obtain the self-prepared graphene. Comparative Example 4 20 The only difference between this comparative example and Example 1 was that in the step (2), the graphite powder was added into the mixed acid solution and stirred for reaction for 15 hours to obtain the mixed solution B; and a ratio of a mass of the graphite powder to a volume of the mixed acid solution was 50 g: 1 L. Comparative Example 5 25 The only difference between this comparative example and Example 1 was that the gelatin in the step (3) was replaced by glucose. Comparative Example 6 The only difference between this comparative example and Example 1 was that the gelatin in the step (3) was replaced by sucrose. 30 Comparative Example 7 The only difference between this comparative example and Example 1 was that the PEG in the step (3) was replaced by CT AB (cetyltrimethylammonium bromide). Comparative Example 8 The only difference between this comparative example and Example 1 was that a mass ratio of 5 the lithium iron phosphate powder A to the modified graphite powder C and the gelatin in the step (3) was 1: 0.2: 0.005. Comparative Example 9 The only difference between this comparative example and Example 1 was that a mass ratio of the lithium iron phosphate powder A to the modified graphite powder C and the gelatin in the step (3) 10 was 1: 0.1: 0.1. Effect Example 1 In order to verify the performances of the regenerated lithium iron phosphate / C cathode materials prepared by the method for recycling the lithium iron phosphate waste battery according to the present disclosure, the products of each example and comparative example were prepared into lithium ion half batteries for performance test, wherein the lithium-ion half batteries were assembled by using metal lithium plates as anode electrodes and commercial electrolyte. The test was carried out at a working voltage of 2.5 V to 4.3 V. Each group of assembled batteries was subjected to long cycle tests for 200 cycles at a multiplying factor of 0.5 C, and the results were shown in Table 1. 07 02 24 Table 1 Tested performance Initial specific discharge capacity at (mAh / g) Specific discharge capacity after 200 cycles (mAh / g) Example 1 152.5 142.7 Example 2 150.1 139 Example 3 155.6 140.5 Example 4 143 136.1 Example 5 158.4 137 Comparative Example 1 121.5 98.6 Comparative Example 2 154.7 126 07 02 24 Comparative Example 3 153.9 131 Comparative Example 4 145.3 118.4 Comparative Example 5 148 115.9 Comparative Example 6 150.5 106 Comparative Example 7 146.7 121.8 Comparative Example 8 156 125.5 Comparative Example 9 141.2 113.7 As can be seen from Table 1, the initial capacity of all the regenerated lithium iron phosphate / C cathode material prepared by the method for recycling the lithium iron phosphate waste battery according to the present disclosure is high, and the specific discharge capacity is still maintained more than 135 mAh / g after 200 cycles at a low multiplying factor of 0.5 C. After calculation, the capacity 5 retention rates of Examples 1 to 5 are 93.57%, 92.6%, 90.29%, 95.17% and 86.48% respectively. In contrast, the long-cycle specific discharge capacities or capacity retention rates of the products of the comparative examples are difficult to reach the level of the examples, and the products of Comparative Example 1 prepared without building a new lithium iron phosphate layer and lithium supplementation of the original lithium iron phosphate layer have either low initial specific discharge 10 capacity or capacity retention rate. However, in Comparative Examples 2 and 3, the commercial graphite or graphene which are common in the prior art are used as the graphite layers in the process, since the interlayer spacing between the commercial graphite and graphene is small, it is difficult to achieve an ideal lithium iron phosphate loading effect, and the cycle stability is not as good as that of the product of Example 1. The degree of acidification and oxidation of the graphite powder in the 15 product of Comparative Example 4 are too high, so an interlayer structure of the graphite powder is destroyed to a certain extent. The original lithium iron phosphate particles from the waste battery are difficult to uniformly load on the surface of the graphite layer, and the newly generated lithium iron phosphate cannot be uniformly dispersed, so the cycle stability of the product is not high. An amorphous carbon source and a surfactant used in the process methods of Comparative Examples 5 to 7 are not the preferred types of the present disclosure. Compared with the gelatin, the soluble carbon source is difficult to form a good gel dispersion system in the precursor preparation process, and the product appears obvious unevenness in the subsequent sintering process. Even if the gelatin 5 is used as the amorphous carbon source matching the graphite layer, selecting other kinds of surfactants will also lead to the difficulty in reaching the ideal degree of uniformity of each component, so the specific discharge capacity and cycle stability of the product are not high. The ratio of the graphite powder to the amorphous carbon in Comparative Examples 8 and 9 is inappropriate, and the specific discharge capacities or cycle stabilities of the products are not as good as those of Examples 10 1,4 and 5. Effect Example 2 The same method as that in Effect Example 1 was used. When testing the electrochemical performance, each product was first cycled for 20 cycles at a multiplying factor rate of 0.5 C, then cycled for 200 cycles at a multiplying factor of IC, and finally lowered to a multiplying factor of 0.5 C again. The test results were shown in Table 2. 07 02 24 Table 2 Tested performance Initial specific discharge capacity at 0.5 C (mAh / g) Specific discharge capacity at 1 C (mAh / g) Specific discharge capacity after returning back to 0.5 C (mAh / g) Example 1 150.6 132.5 139.5 Example 2 151.3 126.1 137 Example 3 157.2 128 135.8 Example 4 139.5 118.5 129.5 Example 5 152.6 119.6 126 Comparative Example 1 125.4 76.8 92.2 Comparative Example 2 150 115 124 Comparative Example 3 152.7 120.7 125.7 Comparative Example 4 148.1 108.5 120.5 Comparative Example 5 145.2 105.2 116.7 Comparative Example 6 151 96.5 109 Comparative Example 7 148.9 115.9 122.6 Comparative Example 8 152.5 104.6 119.2 Comparative Example 9 145.7 98.5 108 It can be seen from Table 2 that the regenerated lithium iron phosphate / C cathode material OZ 02 24 prepared by the method for recycling the lithium iron phosphate waste battery according to the present disclosure also has an ideal rate performance, and can still maintain a specific discharge capacity more than 115 mAh / g at a multiplying factor of 1 C. At the same time, the capacity of the product returning back to multiplying factor cycle after high multiplying factor cycle is equivalent to that of low multiplying factor cycle in Table 1, indicating that the product has high structural stability and will not be destroyed by high multiplying factor cycle. Finally, it should be noted that the embodiments above are merely used to illustrate the technical solutions of the present disclosure, but are not intended to limit the protection scope of the present 10 disclosure. Although the present disclosure has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solutions of the present disclosure can be modified or equivalently replaced without departing from the essence and scope of the technical solutions of the present disclosure.
Claims
1. A method for recycling a lithium iron phosphate waste battery, comprising the following steps of:(1) preprocessing a cathode material: subjecting a cathode plate of the lithium iron phosphate 5 waste battery to washing, impurity removing by heating, and sieving to obtain a lithium iron phosphate powder A;(2) preprocessing an anode material: after washing and drying an anode graphite plate of the lithium iron phosphate waste battery, adding the obtained graphite powder into a mixed acid solution, stirring and reacting for 5 hours to 10 hours to obtain a mixed solution B; wherein, the mixed acid 10 solution is a mixed solution of hydrochloric acid and nitric acid, and a ratio of a mass of the graphite powder to a volume of the mixed acid solution is (100 to 300) g: 1 L; andthen, adding an oxidant into the mixed solution B, and heating until the reaction is complete, then adding a reductant for a reduction reaction, and obtaining a modified graphite powder C after heating and heat preservation;(3) preparing a precursor: dispersing the lithium iron phosphate powder A and the modified graphite powder C in deionized water, introducing a soluble ferric salt, PEG, a soluble phosphate and gelatin, uniformly mixing, then adding a lithium salt, and drying to obtain a precursor gel D; wherein a mass ratio of the lithium iron phosphate powder A to the modified graphite powder C and the gelatin is 1: (0.1 to 0.5): (0.01 to 0.5); and20 (4) preparing a regenerated lithium iron phosphate / C cathode material: calcining the precursorgel D at 600°C to 800°C in an inert atmosphere for 5 hours to 10 hours, washing and drying to obtain the regenerated lithium iron phosphate / C cathode material.
2. The method for recycling the lithium iron phosphate waste battery according to claim 1, wherein in the step (1), the cathode plate is washed with an organic solvent; and25 preferably, the organic solvent is at least one selected from the group consisting of ethanol, methanol and NMP.
3. The method for recycling the lithium iron phosphate waste battery according to claim 1, wherein in the step (1), the impurity removing by heating is heating the washed cathode plate to 100°C to 200°C in an inert atmosphere and keep the temperature for 1 hour to 2 hours.30 4. The method for recycling the lithium iron phosphate waste battery according to claim 1,wherein in the step (2), a concentration of the hydrochloric acid in the mixed solution is 6 mol / L to 8mol / L, and a concentration of the nitric acid is 1 mol / L to 2 mol / L.
5. The method for recycling the lithium iron phosphate waste battery according to claim 1, wherein in the step (2), the oxidant is at least one selected from the group consisting of sodium hypochlorite and potassium hypochlorite, and the reductant is hydrogen peroxide.5 6. The method for recycling the lithium iron phosphate waste battery according to claim 1,wherein in the step (2), the heating and heat preservation is heating the reactant to 450°C to 600°C in an inert atmosphere and keep the temperature for 1 hour to 3 hours.
7. The method for recycling the lithium iron phosphate waste battery according to claim 1, wherein in the step (3), the soluble ferric salt comprises at least one selected from the group consisting 10 of ferric sulfate, ferric nitrate and ferric chloride: the soluble phosphate is ammonium dihydrogen phosphate; and the lithium salt is at least one selected from the group consisting of lithium carbonate, lithium oxalate, lithium acetate and lithium bromide.
8. The method for recycling the lithium iron phosphate waste battery according to claim 7, wherein a molar ratio of Fe3+ in the soluble ferric salt, PO43' in the soluble phosphate and Li+ in the lithium salt is (0.8 to 1): (0.8 to 1): (1 to 1.2).
9. The method for recycling the lithium iron phosphate waste battery according to claim 8, wherein a molar ratio of Li+ in the lithium salt to the lithium iron phosphate powder A is (0.05 to 0.1): 1.
Citation Information
Patent Citations
Lithium iron phosphate composite positive electrode material, preparation method thereof, lithium-ion battery and capacitor
CN110277541A
In-situ regeneration method of waste lithium iron phosphate battery positive electrode material
CN110581323A
Lithium supplementing and repairing method for waste lithium iron phosphate, and application thereof
CN113072052A
Composite positive electrode material obtained by utilizing waste lithium iron phosphate battery, method and application thereof
CN113161524A