Structure protective sheet and manufacturing method of reinforced structure

JP2023018895A5Inactive Publication Date: 2024-11-21KEIWA INCORPORATED
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2021123258
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2021-07-28
Publication Date
2024-11-21
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional concrete repair sheets face issues with adhesive strength variations between layers, elongation differences leading to peeling, and low water vapor permeability causing moisture retention, resulting in prolonged construction times and reduced durability.

Method used

A structure protection sheet comprising a polymer cement hardened layer and a resin layer, designed to maintain moisture permeability within specific limits even under sunlight exposure, allowing mass production and easy application, enhancing adhesion and durability.

Benefits of technology

The sheet significantly reduces construction time, ensures long-term protection, and maintains performance by controlling moisture permeability, preventing deterioration factors like water and chloride ions, while being applicable by unskilled workers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

To provide a structure protective sheet that can significantly reduce a construction period when setting a protective layer on the surface of a structure such as concrete, and can also protect the structure for a long period of time with excellent strength.SOLUTION: A structure protective sheet of the present invention comprises: a polymer cement hardening layer provided on the structure side; and a resin layer provided on the polymer cement hardened layer. The rate of change in moisture permeability is 35% or less before and after being irradiated with light that is emitted from a xenon lamp with radiation intensity of 180 W / m2 for 72 hours.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a structure protection sheet and a method for manufacturing a reinforced structure. More specifically, the present invention relates to a structure protection sheet that can significantly reduce the construction period when providing a protective layer on the surface of a structure such as concrete and can protect the structure over a long period of time, and a method for manufacturing a reinforced structure using the structure protection sheet.

Background Art

[0002] Civil structures such as road bridges, tunnels, river management facilities such as floodgates, sewer pipelines, and coastal walls are repaired and reinforced as they age. Repair work is carried out by applying a coating material multiple times after repairing damaged and vulnerable parts. On the other hand, reinforcement work is carried out by applying a reinforcing coating material multiple times to the entire part to be reinforced.

[0003] Such multi-layer coating applied in these repair and reinforcement works, for example, primer, intermediate coat, and top coat are applied in sequence on concrete. Usually, however, the intermediate coat and each coating process cannot be carried out continuously to dry the coating. For example, when applying a total of 5 layers of coating, such as primer, first intermediate coat, second intermediate coat, first top coat, and second top coat, it takes at least 5 days for the construction period. Moreover, since it is outdoor painting, it is affected by the weather, and in rainy weather, sufficient drying may not be possible, or the painting work itself may not be possible. Therefore, it is difficult to shorten the construction period, which results in increased labor costs, and the quality of the construction and the paint film (film thickness, surface roughness, water content, etc.) are likely to be unstable due to the external environment (humidity, temperature, etc.) during the painting process.

[0004] In addition, painting is performed by trowel painting or spray painting, etc. Stable repair and reinforcement by uniform painting greatly depends on the skill of the craftsman. Therefore, the quality of the paint film also varies depending on the skill of the craftsman. Furthermore, with the aging of construction workers and the decrease in population, there is a demand for a simpler repair method that can be performed even by non-skilled workers, as the number of workers engaged in concrete repair and reinforcement work has been decreasing recently.

[0005] As a technology to solve these problems, for example, Patent Document 1 proposes a sheet and method that is simple, low-cost, shortens the construction period, and reliably prevents concrete deterioration. This technology is a concrete repair method in which a concrete repair sheet, comprising an intermediate layer having a resin film and a surface layer made of fabric material laminated on both sides via an adhesive resin, is attached to the concrete surface to be repaired with an adhesive, and then a paint is applied to the surface layer of the attached concrete repair sheet that is opposite to the concrete surface.

[0006] Improvements have also been made to the coating materials. For example, Patent Document 2 proposes a method for protecting concrete structures using a coating material that prevents alkali-aggregate reaction, has excellent crack-following properties for concrete structures, does not cause blistering of the coating film even when the temperature rises after the coating film is formed, and prevents spalling of the concrete. This technology involves forming a base coat on the surface of the concrete structure and then forming a coating film on the surface of that base coat. The base coat is formed from a composition containing a cationic (meth)acrylic polymer emulsion and an inorganic hydraulic substance. The coating film formed on the surface of the base coat is a coating film formed from a composition containing an alkyl (meth)acrylate emulsion and an inorganic hydraulic substance, with an elongation rate of 50-2000% at 20°C and a salt-blocking property of 10 -2 ~10 -4 mg / cm 2 The film thickness is 100-5000 μm, the water vapor permeability is 5 g / m·day or more, and the film thickness is 0.day. [Prior art documents] [Patent Documents]

[0007] [Patent Document 1] Japanese Patent Publication No. 2010-144360 [Patent Document 2] Japanese Patent Publication No. 2000-16886 [Overview of the project] [Problems that the invention aims to solve]

[0008] Conventional concrete repair sheets, such as those described in Patent Document 1, have several issues that need to be addressed, including differences in adhesive strength between the base material and other layers (e.g., adhesive layer and reinforcing member), differences in elongation of the base material, adhesive layer, and reinforcing member, and problems with the adhesive strength between the adhesive layer and concrete. Specifically, although the base material and reinforcing member are bonded together by an adhesive layer, when stress is applied to the concrete repair sheet during or after its installation, differences in elongation of the base material, adhesive layer, and reinforcing member can cause delamination at the layer interface based on differences in adhesive strength between the base material and adhesive layer and between the adhesive layer and reinforcing member.

[0009] Furthermore, although the adhesive layer on the concrete repair sheet softens upon heating and adheres to the concrete, if sufficient adhesive strength is not achieved, the concrete repair sheet may peel off from the concrete surface and fail to function as a repair sheet. In addition, concrete that has been installed with a concrete repair sheet may swell over time. This phenomenon is thought to be because the water vapor inside the concrete has nowhere to escape due to the presence of the repair sheet, which has low water vapor permeability.

[0010] Furthermore, as explained in the background technology section above, the method of forming a coating film on-site takes one day for each layer applied, and if a coating film of six layers, for example, is to be formed from the undercoat to the topcoat, it takes six days. Moreover, the film thickness varies, and the quality and characteristics such as surface roughness and water content are difficult to stabilize.

[0011] Furthermore, since concrete repair sheets typically target large concrete members such as road bridges, tunnels, river management facilities like sluice gates, sewer pipes, and harbor walls, the concrete repair sheets themselves are required to have sufficient strength (tensile strength, bending strength, hardness, surface strength, punch-out strength, toughness, etc.; the same applies hereinafter in this specification). However, conventional concrete repair sheets do not have sufficient strength, which presents a challenge.

[0012] The present invention was made to solve the above problems, and its purpose is to provide a structural protection sheet that can significantly reduce the construction period when applying a protective layer to the surface of a structure such as concrete, and can protect the structure over a long period of time, and a method for manufacturing a reinforced structure using the structural protection sheet. [Means for solving the problem]

[0013] The inventors have researched a concrete protection sheet that can stably protect concrete for a long period of time without using a construction method that forms a layer on the surface of concrete by coating means. As a result, they have completed a structural protection sheet having a polymer cement hardened layer and a resin layer that further provides the concrete protection sheet with performance according to the characteristics of concrete, specifically, a followability that can follow cracks and expansion that occur in concrete, waterproofing that prevents deterioration factors such as water and chloride ions from penetrating into the concrete, salt barrier properties, carbonation prevention properties, and water vapor permeability that allows moisture in the concrete to be released as water vapor. However, the structural protection sheet previously completed by the inventors had the potential to deteriorate due to the alteration of the polymer cement hardened layer when exposed to sunlight, potentially reducing the performance imparted according to the properties of the concrete. Therefore, after further intensive research, the inventors achieved a result in which the rate of change in moisture permeability of the structural protection sheet before and after exposure to sunlight falls within a specific range, thus completing the present invention. Furthermore, this technical concept can be applied as a structural protection sheet to structures other than concrete.

[0014] (1) The structural protection sheet according to the present invention comprises a polymer cement hardened layer provided on the structure side and a resin layer provided on the polymer cement hardened layer, and has a radiation intensity of 180 W / m 2 This material is characterized by having a change rate of 35% or less in moisture permeability before and after 72 hours of irradiation with light from a xenon lamp.

[0015] According to the present invention, even when the polymer cement hardened layer is exposed to sunlight, it is possible to suitably prevent the degradation of the imparted performance. In addition, since the structure protection sheet can be mass-produced by the coating process and the drying process on the production line of the factory, it is possible to achieve cost reduction, a significant reduction in the working period at the site, and long-term protection of the structure.

[0016] In the structure protection sheet according to the present invention, it is preferable that the polymer cement hardened layer is subjected to a water absorption treatment.

[0017] According to the present invention, it is possible to suitably prevent the degradation of the performance imparted to the polymer cement hardened layer when exposed to sunlight.

[0018] In the structure protection sheet according to the present invention, the water absorption treatment includes a method of adding a water-absorbing polymer to the polymer cement hardened layer, a method of adding an inorganic water-absorbing substance to the polymer cement hardened layer, a method of performing an aging treatment when producing the polymer cement hardened layer in a high-humidity environment, a method of performing a heat treatment when forming the resin layer in a high-humidity environment, a method of providing a water-containing sheet that absorbs moisture into the polymer cement hardened layer, and a method of performing wet curing after the structure protection sheet is constructed. It is preferably any method selected from the group consisting of these methods.

[0019] According to the present invention, it is possible to suitably realize the water absorption treatment of the polymer cement hardened layer.

[0020] In the structure protection sheet according to the present invention, the polymer cement hardened layer is a layer containing a cement component and a resin, and the resin may be contained in an amount of 10% by weight or more and 40% by weight or less. More preferably, the resin is 20% by weight or more and 30% by weight or less.

[0021] According to the present invention, by controlling the ratio of the cement component and the resin component, it becomes easier to form a polymer cement cured layer. Moreover, since the polymer cement cured layer is likely to become a layer with excellent compatibility and followability, the adhesion of the layer itself tends to be improved. Further, the cement component contained in the polymer cement cured layer on the structure side acts to enhance the adhesion to the structure such as concrete.

[0022] (2) The present invention is a method for manufacturing a structure using the structure protection sheet according to the above-mentioned present invention, characterized in that the structure protection sheet is bonded after applying an adhesive on the structure.

[0023] According to the present invention, since a structure protection sheet composed only of a layer not including a base material or a reinforcing member is used, it can be easily bonded to the surface of the structure. As a result, even an unskilled worker can stably provide a structure protection sheet with excellent strength on the surface of the structure, significantly reducing the construction period and protecting the structure over a long period.

[0024] In the method for manufacturing a reinforced structure according to the present invention, a primer layer may be provided between the structure and the adhesive.

[0025] According to the present invention, the primer layer provided between the structure and the adhesive acts to enhance the mutual adhesion, so that the structure protection sheet can stably protect the structure for a long time.

Effects of the Invention

[0026] According to the present invention, even when the structural protection sheet is applied to the surface of a structure such as concrete and exposed to sunlight, the rate of change in moisture permeability remains within a predetermined range, so the deterioration of the imparted performance can be effectively prevented, and the surface of the structure can be protected for a long period of time. The present invention also provides a method for manufacturing a reinforced structure using the structural protection sheet. In particular, it is possible to provide a structural protection sheet that imparts performance according to the characteristics of the structure, such as following cracks and expansion that occur in the structure, preventing deterioration factors such as water and chloride ions from penetrating the structure, providing permeability that allows moisture and deterioration factors in the structure to be discharged, and improving strength. Furthermore, it has the advantage of improving the stability and uniformity of quality compared to layers that have been formed by hand application until now. [Brief explanation of the drawing]

[0027] [Figure 1] This is a cross-sectional diagram showing an example of a structural protection sheet according to the present invention. [Figure 2] This is an explanatory diagram of the installation method for structural protective sheets. [Figure 3] This is an explanatory diagram showing an example of applying a structural protection sheet to a cast-in-place construction method. [Figure 4] This graph shows the results of the change in moisture permeability for the examples and comparative examples. [Modes for carrying out the invention]

[0028] The structural protection sheet and reinforced concrete structure using the same according to the present invention will be described below with reference to the drawings. It should be noted that the present invention is capable of various modifications as long as it retains its technical features, and is not limited to the forms described below and shown in the drawings.

[0029] [Structural protection sheet] As shown in Figure 1 or Figure 2(C), the structural protection sheet 1 according to the present invention comprises a polymer cement hardened layer 3 provided on the structure 21 side and a resin layer 2 provided on the polymer cement hardened layer 3. Both the polymer cement hardened layer 3 and the resin layer 2 may be formed as single layers or as laminates. Depending on the required performance, another layer may be provided between the polymer cement hardened layer 3 and the resin layer 2.

[0030] The structural protective sheet 1 according to the present invention has a radiation intensity of 180 W / m². 2 The change in moisture permeability before and after 72 hours of irradiation from a xenon lamp is 35% or less. The above change in moisture permeability is calculated using {(N2-N1) / N2}×100, where N1 is the moisture permeability before irradiation with the xenon lamp and N2 is the moisture permeability after irradiation with the xenon lamp. If the above rate of change in moisture permeability exceeds 35%, there is a problem in that the performance imparted by the structural protection sheet 1 according to the present invention deteriorates when it is exposed to sunlight after being attached to the surface of a structure. The preferred lower limit of the above rate of change in moisture permeability is 0%, and the preferred upper limit is 20%. The above moisture permeability values ​​were measured according to JIS Z0208:1976.

[0031] The reason why defining such a rate of change in moisture permeability can prevent deterioration of the performance of the structural protection sheet 1 according to the present invention is as follows. The polymer cement hardened layer 3 is a layer containing cement components and resin components, as described later. In the structural protective sheet 1 manufactured according to the present invention, the polymer cement hardened layer 3 continues to harden due to the moisture it contains, transforming into a stronger layer. When such a structural protection sheet 1 according to the present invention is attached to the surface of a structure 21, conventional structural protection sheets have the problem that the moisture content in the polymer cement hardened layer 3 decreases due to irradiation with sunlight (and also due to being placed in a high-temperature environment), and if the hardening reaction of the polymer cement hardened layer 3 changes over time, it will not harden sufficiently. Therefore, the structural protection sheet 1 according to the present invention limits the upper limit of the rate of change in moisture permeability by irradiating it with a xenon lamp, which is simulating sunlight, under predetermined conditions.

[0032] To satisfy this rate of change in moisture permeability, for example, it is preferable that the structural protective sheet 1 according to the present invention is subjected to a water absorption treatment on the polymer cement hardened layer 3. The above water absorption treatment is a process that allows moisture to be carried within the polymer cement hardened layer 3. By applying this water absorption treatment, the moisture retention rate within the polymer cement hardened layer 3 can be maintained, making it possible to satisfy the above-mentioned rate of change in moisture permeability.

[0033] As for the above water absorption treatment, any method selected from the group consisting of, for example, a method of adding a water-absorbing polymer to the polymer cement hardened layer 3, a method of adding an inorganic water-absorbing substance to the polymer cement hardened layer 3, a method of performing an aging treatment when producing the polymer cement hardened layer 3 in a high-humidity environment, a method of performing a heat treatment when forming the resin layer 2 in a high-humidity environment, a method of providing a water-absorbing sheet on the polymer cement hardened layer 3, or a method of performing wet curing after installing the structural protection sheet 1 is preferable.

[0034] In the method of adding a water-absorbing polymer to the polymer cement hardened layer 3 described above, examples of the water-absorbing polymer include Aqualic CA (manufactured by Nippon Shokubai Co., Ltd.). The content of the above-mentioned water-absorbing polymer is preferably, for example, 0.15 to 0.30 parts by mass per 100 parts by mass of the resin component in the polymer cement hardened layer 3. If it is less than 0.15 parts by mass, the rate of change in moisture permeability of the structural protective sheet 1 according to the present invention may increase, and if it exceeds 0.30 parts by mass, it may thicken and become impossible to coat.

[0035] In the method for producing the polymer cement hardened layer 3 described above, the aging treatment is carried out in a high-humidity environment, and the high-humidity environment is preferably an environment with a humidity of 50% RH or less. Furthermore, the aging treatment mentioned above specifically involves leaving the polymer cement hardened layer 3 in the high-humidity environment for 24 to 72 hours.

[0036] In the method of performing the heat treatment for forming the resin layer 2 in a high-humidity environment, the high-humidity environment refers to the environment described above, and the temperature of the heat treatment is appropriately determined according to the resin material constituting the resin layer 2 used, but is preferably 60 to 80°C.

[0037] In the method of providing a water-absorbing sheet in the polymer cement hardened layer 3 described above, the water-absorbing sheet can be, for example, a nonwoven fabric or the like that has been impregnated with water. Furthermore, the water-containing sheet may be embedded inside the polymer cement hardened layer 3, or it may be provided on the surface of the polymer cement hardened layer 3 on the resin layer 2 side, or on the opposite side of the polymer cement hardened layer 3 on the resin layer 2 side.

[0038] As for the method of wet curing after installing the above-mentioned structural protection sheet 1, the same method as conventionally used to accelerate the hardening of cement can be used, and specifically, it is preferable to wrap the hardened cement with a water-retaining sheet.

[0039] The structural protection sheet 1 according to the present invention preferably has a thickness distribution of ±100 μm or less. Because the thickness distribution of this structural protection sheet 1 is within the above range, even inexperienced workers can stably provide a layer with small thickness variations on the surface of the structure 21. Furthermore, controlling the thickness distribution within the above range makes it easier to uniformly reinforce the structure. The polymer cement hardened layer 3 provided on the structure 21 side has excellent adhesion to the structure 21 and, because it has a known primer layer 5, the process of applying and drying an adhesive is unnecessary. In addition, the resin layer 2 provided on the polymer cement hardened layer 3 can be given properties such as waterproofing, salt resistance, and neutralization prevention. Furthermore, since the structural protection sheet 1 can be mass-produced through coating and drying processes on the factory production line, it is possible to reduce costs, significantly shorten on-site work time, and achieve long-term protection of structures. As a result, the time required to adhere it to the surface of the structure 21 can be greatly reduced, and the structure 21 can be protected for a long period of time.

[0040] The following provides a detailed explanation of specific examples of each component.

[0041] (structure) The structure 21 is the mating member to which the structural protective sheet 1 according to the present invention is applied. Structure 21 can be a structure made of concrete. The above-mentioned concrete is generally obtained by pouring and curing a cement composition containing at least cement-based inorganic substances, aggregates, admixtures, and water. Such concrete is widely used as civil engineering structures such as road bridges, tunnels, river management facilities such as sluice gates, sewer pipes, and port quays. In the present invention, by applying the structural protection sheet 1 to a concrete structure 21, it is possible to follow cracks and expansions that occur in the concrete, prevent deterioration factors such as water and chloride ions from penetrating into the concrete, and allow moisture in the concrete to be released as water vapor, which are exceptional advantages.

[0042] (Polymer cement hardened layer) The polymer cement hardened layer 3 is a layer placed on the structure side, as shown in Figure 2(C). This polymer cement hardened layer 3 may be a single layer or a laminated layer, but whether it is a single layer or a laminated layer is arbitrarily determined considering the overall thickness, the function to be imparted (conformability, adhesion to the structure, etc.), the factory's production line, production costs, etc. For example, if the production line is short and a single layer cannot reach the required thickness, it can be formed by applying two or more layers in overlapping layers. Note that, for example, when applying two layers in overlapping layers, the second layer is formed after the first layer has dried. Furthermore, the polymer cement hardened layer 3 may have a structure in which layers with different properties are laminated together. For example, by making the layer with a higher proportion of resin components on the side of the resin layer 2, the layer with a higher resin component adheres to the resin layer 2, and the layer with a higher cement component adheres to the concrete structure 21, resulting in extremely excellent adhesion to both.

[0043] The polymer cement hardened layer 3 is obtained by applying a paint made from a resin (resin component) containing cement components. When the method of adding a water-absorbing polymer or inorganic water-absorbing substance to the polymer cement hardened layer 3 as the water absorption treatment is adopted, the water-absorbing polymer or inorganic water-absorbing substance is added to the paint. Examples of cement components include various types of cement, limestone containing calcium oxide, and clays containing silicon dioxide. Cement is preferred among these, and examples include Portland cement, alumina cement, high-early-strength cement, and fly ash cement. The choice of cement is made according to the properties that the polymer cement hardened layer 3 should possess, for example, by considering the degree of conformability to the concrete structure 21. Portland cement as specified in JIS R5210 is particularly preferred.

[0044] Examples of the above-mentioned resin components include acrylic resin, acrylic urethane resin, acrylic silicone resin, fluororesin, flexible epoxy resin, polybutadiene rubber, and acrylic resins exhibiting rubber properties (for example, synthetic rubber mainly composed of acrylic acid ester). From the viewpoint of improving adhesion between the polymer cement hardened layer 3 and the resin layer 2, it is preferable that these resin components are the same as the resin components constituting the resin layer 2 described later. Furthermore, the resin component may be a thermoplastic resin, a thermosetting resin, or a photocurable resin. The term "cured" in polymer cement cured layer 3 does not mean that the resin component is limited to a resin that cures and polymerizes, such as a thermosetting resin or a photocurable resin, but rather that any material that cures when it becomes the final layer may be used.

[0045] The content of the above resin component is adjusted as appropriate depending on the materials used, but preferably it is 10% by mass or more and 40% by mass or less relative to the total amount of cement component and resin component. If it is less than 10% by mass, the adhesion to the resin layer 2 tends to decrease and it may become difficult to maintain the polymer cement hardened layer 3 as a layer, and if it exceeds 40% by mass, the adhesion to the concrete structure 21 may be insufficient. From the above viewpoint, a more preferable range for the content of the above resin component is 15% by mass or more and 35% by mass or less, but even more preferably it is 20% by mass or more and 30% by mass or less.

[0046] The coating for forming the polymer cement hardened layer 3 is a coating liquid obtained by mixing cement components and resin components with a solvent. The resin component is preferably an emulsion. For example, an acrylic emulsion is a polymer fine particle obtained by emulsion polymerization of monomers such as acrylic acid esters using an emulsifier. As an example, an acrylic acid polymer emulsion obtained by polymerizing a monomer or monomer mixture containing one or more acrylic acid esters and methacrylic acid esters in water containing a surfactant can be preferably cited. The content of acrylic acid esters and other components constituting the above-mentioned acrylic emulsion is not particularly limited, but is selected from within the range of 20 to 100% by mass. Furthermore, a surfactant is added as needed, and the amount is not particularly limited, but an amount sufficient to form an emulsion is added.

[0047] The polymer cement hardened layer 3 is formed by applying the coating liquid onto a release sheet and then drying off the solvent (preferably water). For example, a mixed composition of cement components and an acrylic emulsion is used as the coating liquid to form the polymer cement hardened layer 3. Note that the resin layer 2 may be formed on the release sheet after the polymer cement hardened layer 3 is formed, or the polymer cement hardened layer 3 may be formed after the resin layer 2 is formed on the release sheet. Specifically, for example, a resin layer is coated onto process paper used as a release sheet, a coating liquid for polymer cement is applied after drying, and a Young's modulus adjustment layer is bonded to the wet surface before drying, and then dried. Subsequently, by applying a coating liquid for polymer cement to the surface to which the Young's modulus adjustment layer has been bonded and drying it, a structural protective sheet having a Young's modulus adjustment layer in the polymer cement hardened layer according to the present invention can be obtained. Furthermore, it is also possible to obtain a structural protective sheet in which a Young's modulus adjustment layer exists within the polymer cement hardened layer according to the present invention by coating a resin layer onto process paper as a release sheet, applying a coating liquid for polymer cement after drying, bonding a Young's modulus adjustment layer while the Young's modulus adjustment layer is still wet before drying, then applying another coating liquid for polymer cement to the surface to which the Young's modulus adjustment layer is bonded without going through the drying step, and then drying the entire sheet.

[0048] The thickness of the polymer cement hardened layer 3 is not particularly limited and can be arbitrarily set depending on the form of use of the structure 21 (road bridges, tunnels, river facilities such as sluice gates, sewer pipes, port quays and other civil engineering structures), the age of the structure, its shape, etc. For example, the thickness of the polymer cement hardened layer 3 can be in the range of 0.5 mm to 1.5 mm. If the thickness is 1 mm, it is preferable that the thickness variation be within ±100 μm. Such precision in thickness is impossible to achieve with on-site coating and can only be achieved by stable coating on a factory production line. Furthermore, even if the thickness is greater than 1 mm, the thickness variation can be kept within ±100 μm. Also, if the thickness is less than 1 mm, the thickness variation can be further reduced.

[0049] This polymer cement hardened layer 3 allows water vapor to pass through more easily than the resin layer 2 described later, due to the presence of cement components. The water vapor transmission rate in this case is, for example, 20-60 g / m³. 2The hardening time is approximately 0 days. Furthermore, the cement component can be made to have good compatibility with the cement component that makes up concrete, for example, and to have excellent adhesion to the concrete surface. Also, as shown in Figure 2, even when the undercoat layer 22 and adhesive 23 are applied sequentially to the surface of the structure 21, the polymer cement hardened layer 3 containing the cement component adheres well to the adhesive 23. In addition, since this polymer cement hardened layer 3 is stretchable, it can follow changes in the concrete even if cracks or expansion occur in the structure 21.

[0050] (Resin layer) As shown in Figure 2(C), the resin layer 2 is positioned on the opposite side of the structure 21 and is the layer that appears on the surface. This resin layer 2 may be a single layer, as shown in Figure 1(A), or it may be a laminate consisting of at least two layers, as shown in Figure 1(B). Whether to make it a single layer or a multilayer is determined by considering the overall thickness, the functions to be provided (waterproofing, salt resistance, carbonation prevention, water vapor permeability, etc.), the length of the factory's production line, production costs, etc. For example, if the production line is short and a single layer cannot reach the required thickness, it can be formed by applying two or more layers in overlapping layers. When applying overlapping layers, the second layer is applied after the first layer has dried. The second layer is then dried.

[0051] The resin layer 2 is obtained by applying a coating that is flexible, can follow cracks and fissures that occur in the concrete, and forms a resin layer with excellent waterproofing, salt-blocking, carbonation-preventing, and water vapor permeability properties. Examples of resins that make up the resin layer 2 include acrylic resins exhibiting rubber properties (for example, synthetic rubber mainly composed of acrylic acid ester), acrylic urethane resin, acrylic silicone resin, fluororesin, flexible epoxy resin, and polybutadiene rubber. It is preferable that this resin material is the same as the resin component that makes up the polymer cement layer 2 described above. It is particularly preferable that the resin contains an elastic film-forming component such as rubber.

[0052] Of these, the acrylic resin exhibiting rubber properties is preferably an aqueous emulsion of an acrylic rubber copolymer, due to its excellent safety and coating properties. The proportion of the acrylic rubber copolymer in the emulsion is, for example, 30 to 70% by mass. The acrylic rubber copolymer emulsion is obtained, for example, by emulsion polymerization of monomers in the presence of a surfactant. Any anionic, nonionic, or cationic surfactant can be used.

[0053] The coating for forming the resin layer 2 is prepared by mixing a resin composition with a solvent to create a coating solution, applying the coating solution to a release sheet, and then drying and removing the solvent to form the resin layer 2. The solvent may be water or an aqueous solvent, or an organic solvent such as xylene mineral spirits. In the examples described later, an aqueous solvent is used, and the resin layer 2 is made from an acrylic rubber composition. The order of the layers formed on the release sheet is not limited; for example, the order may be resin layer 2 followed by polymer cement hardened layer 3 as described above, or polymer cement hardened layer 3 followed by resin layer 2. However, as shown in the examples described later, it is preferable to form the resin layer 2 on the release sheet and then form the polymer cement hardened layer 3.

[0054] The thickness of the resin layer 2 is arbitrarily set depending on the usage of the structure 21 (road bridges, tunnels, river management facilities such as sluice gates, sewer pipes, port quays and other civil engineering structures), the age of the structure, its shape, etc. As an example, it is preferable to set the thickness to any thickness within the range of 50 to 150 μm, with a thickness variation of ±50 μm or less. Such precision in thickness is impossible to achieve with on-site coating, but can be reliably achieved on a factory production line.

[0055] This resin layer 2 has high water resistance, salt resistance, and carbonation prevention properties, but it is preferable that it allows water vapor to pass through. The water vapor transmission rate in this case is, for example, 10 to 50 g / m². 2It is desirable to set the time to approximately .day. By doing so, the structural protection sheet 1 can be given high waterproofness, salt resistance, neutralization prevention, and a predetermined water vapor permeability. Furthermore, by being composed of the same type of resin component as the polymer cement hardened layer 3, it can be made to have good compatibility with the polymer cement hardened layer 3 and excellent adhesion. The water vapor permeability was measured in accordance with JIS Z0208 "Test method for moisture permeability of moisture-proof packaging materials".

[0056] Furthermore, the resin layer 2 may contain a pigment from the viewpoint of providing a wide variety of color options for the structural protection sheet 1 according to the present invention. Furthermore, the resin layer 2 may contain inorganic materials. Including inorganic materials can impart scratch resistance to the resin layer 2. The inorganic material is not particularly limited, and examples include conventionally known materials such as silica, alumina, and metal oxide particles such as titania. Furthermore, the resin layer 2 may contain a known antifouling agent. Since the structural protection sheet according to the present invention is usually used for repairing concrete structures installed outdoors, the resin layer 2 is often contaminated, but by including an antifouling agent, contamination of the structural protection sheet according to the present invention can be effectively prevented. The antifouling agent is not particularly limited and can be a conventionally known material. Furthermore, the resin layer 2 may contain additives that can impart various functions. Examples of such additives include cellulose nanofibers.

[0057] (Other configurations) The manufactured structural protection sheet 1 may have a release sheet on one side of the polymer cement hardened layer 3 and the resin layer 2. The release sheet can protect the surface of the structural protection sheet 1 when it is brought to the construction site, and at the construction site, the structural protection sheet 1 with the release sheet attached can be bonded to the target structure 21 (or via the undercoat layer 22 or adhesive 23), and then the release sheet can be easily peeled off, greatly improving workability at the construction site. Preferably, the release sheet is a process paper used in the production process of the structural protection sheet 1.

[0058] The process paper used as a release sheet is not particularly limited in terms of material, etc., as long as it is a conventionally known type used in the manufacturing process. For example, like known process papers, laminated paper having an olefin resin layer such as polypropylene or polyethylene, or a layer containing silicone, is preferred. Its thickness is also not particularly limited, but it can be any thickness, for example, about 50 to 500 μm, as long as it does not hinder handling during manufacturing and installation.

[0059] As described above, the structural protection sheet 1 controls the rate of change in moisture permeability to a predetermined value or less, so even when exposed to sunlight, it can effectively prevent the deterioration of its performance and protect structures 21 such as concrete over a long period of time. In particular, the structural protection sheet 1 can be given performance according to the characteristics of the structure 21, allowing it to follow cracks and expansions that occur in the structure 21, preventing deterioration factors such as water and chloride ions from penetrating the structure 21, and providing permeability that allows moisture and deterioration factors in the structure to be discharged. Furthermore, since such structural protection sheets 1 can be manufactured in a factory, high-quality products with stable properties can be mass-produced. As a result, it can be installed without relying on the skills of craftsmen, achieving shorter construction periods and reduced labor costs.

[0060] [Manufacturing method for reinforced structures using structural protection sheets] The method for manufacturing a reinforced structure using the structural protection sheet according to the present invention, as shown in Figure 2, is a construction method using the structural protection sheet 1 according to the present invention, characterized in that an adhesive 23 is applied to the structure 21 and then the structural protection sheet 1 is bonded to it. This construction method allows the structural protection sheet 1 to be easily bonded to the surface of the structure 21. As a result, even without skilled workers, the structural protection sheet 1, which is composed of layers with little variation in thickness, can be installed on the structure 21, significantly reducing the construction period and protecting the structure 21 for a long period of time.

[0061] Figure 2 is an explanatory diagram of the construction method (manufacturing method of reinforced structure) of the structural protection sheet 1. The construction involves forming a primer layer 22 on the surface of the structure 21, as shown in Figure 2(A). The primer layer 22 can be formed by applying a coating liquid, a mixture of a resin such as epoxy resin and a solvent, to the structure 21, and then allowing the solvent in the coating liquid to evaporate and dry. The solvent used in this process can also be water, as described above. The thickness of the primer layer 22 is not particularly limited, but can be, for example, within the range of 100 to 150 μm. The primer layer 22, provided between the structure 21 and the adhesive 23, enhances mutual adhesion, allowing the structural protection sheet 1 to stably protect the structure 21 for a long period. If cracks or defects occur in the structure 21, it is preferable to repair them before applying the primer layer 22. While the repair is not particularly limited, cement mortar or epoxy resin are commonly used.

[0062] After forming the undercoat layer 22, the adhesive 23 is applied as shown in Figure 2(B). Without drying the applied adhesive 23, the structural protection sheet 1 is bonded to it as shown in Figure 2(C). Examples of adhesives 23 include urethane adhesives, epoxy adhesives, and adhesives using acrylic resins exhibiting rubber properties (for example, synthetic rubber mainly composed of acrylic acid ester). Among these, an adhesive 23 made of the same type of resin component as the resin component constituting the polymer cement hardened layer 3 of the structural protection sheet 1 is more preferable because it provides higher adhesive strength to the polymer cement hardened layer 3. The thickness of the adhesive 23 is not particularly limited. The adhesive 23 is usually applied to the concrete by means of brushing or spraying, and then hardens by natural drying over time.

[0063] Figure 3 is an explanatory diagram showing an example of applying a structural protection sheet 1 to a cast-in-place concrete construction method. A cast-in-place concrete construction method is a method in which formwork 24 is formed at the work site, a concrete composition 21' is poured into the formwork 24, and left to harden to obtain a concrete structure 21. In this cast-in-place construction method, after the hardened concrete structure 21 is formed, a structural protection sheet 1 can be attached to its surface to make the structure 21 less susceptible to deterioration. For attachment, a primer layer 22 is applied to the surface of the concrete structure 21 and dried, then an adhesive 23 is applied on top of that, and then the structural protection sheet 1 is attached. After that, the adhesive 23 is usually left to dry and harden naturally, and the structural protection sheet 1 is adhered.

[0064] On the other hand, for structures 21 that have already developed cracks or other damage, the structural protection sheet 1 is applied after repairing the damaged portion using the same construction method as described above. In this way, the lifespan of the concrete structure 21 can be extended. [Examples]

[0065] The present invention will be further described in detail by examples and comparative examples.

[0066] (Example 1) A 130 μm thick release sheet made of PP laminated paper was used. A resin layer was formed on this release sheet using the following method. First, an emulsion composition was prepared containing 60 parts by mass of acrylic silicone resin, 25 parts by mass of titanium dioxide, 10 parts by mass of ferric oxide, and 5 parts by mass of carbon black. This emulsion composition was applied to the release sheet, and then heat-treated to cure it and form a resin layer. The thickness of the resin layer was set to 0.1 mm. Next, a polymer cement hardened layer was formed on top of the resin layer. Specifically, "Aronbu Coat A450X Setter" (manufactured by Toagosei Co., Ltd.) was used as the cement type, and "Acryset EMN-325E" (manufactured by Nippon Shokubai Co., Ltd.) was used as the resin component. The polymer cement hardened layer obtained by applying and drying the polymer cement layer-forming composition, which is a mixture of these, is a composite layer containing 0.08 parts by mass of water-absorbing polymer per 100 parts by mass of resin component, and containing 50% by mass of cement type in the resin component. The above polymer cement hardening layer forming composition was applied to the resin layer to a thickness of 1.0 mm before drying. After drying at 80°C for 50 minutes, it was aged at 50% RH and 80°C for 3 days to form a polymer cement hardening layer 3 with a thickness of 1.29 mm. In this way, a structural protection sheet with a total thickness of 1.39 mm was manufactured. This structural protection sheet was continuously produced in a factory controlled at approximately 25°C and wound into rolls including the release sheet.

[0067] (Examples 2-12) A structural protection sheet was prepared in the same manner as in Example 1, except that the cement type and resin components were changed to those listed in Table 1, and the amount of water-absorbing polymer, drying time, and humidity during aging were changed as listed in Table 1.

[0068] (Comparative Examples 1-6) A structural protective sheet according to Comparative Examples 1 to 6 was prepared in the same manner as in Examples 1 to 6, except that a water-absorbent polymer was not added.

[0069] [Table 1] In Table 1, the cement type "Aronbull" represents "Aronbull Coat A-450X Setter" (manufactured by Toagosei Co., Ltd.), "Nippon Stucco" represents "Spring Coat Trowel" (manufactured by Nippon Stucco Co., Ltd.), the resin component "EMN" represents "Acryset EMN-325E" (manufactured by Nippon Shokubai Co., Ltd.), "Aronbull" represents "Aronbull Coat A-450 Base" (manufactured by Toagosei Co., Ltd.), and "Trowel" represents "Spring Coat Trowel" (manufactured by Nippon Stucco Co., Ltd.).

[0070] [Measurement of moisture permeability] The moisture permeability of the structural protection sheets obtained in the examples and comparative examples was measured using the cup method (in accordance with JIS Z0208:1976). Next, the structural protective sheets according to the obtained examples and comparative examples were subjected to a radiant intensity of 180 W / m² using a xenon lamp. 2 The samples were irradiated with light for 72 hours, and the moisture permeability before and after irradiation was measured using the cup method in accordance with JIS Z0208:1976, and the rate of change in moisture permeability was calculated. Examples 1-6 (Group 1) were divided into three groups: Examples 7-12 (Group 2) with 0.08 parts by mass of superabsorbent polymer added, Examples 7-12 (Group 2) with 0.13 parts by mass added, and Comparative Examples 1-6 (Group 3) with no additive. The average moisture permeability before and after irradiation with a xenon lamp was calculated for each group. The results are shown in Figure 4. As shown in Figure 4, the average percentage change in moisture permeability for Groups 1 and 2, which included the addition of a water-absorbing polymer, was 32.1% and 15.0%, respectively, while the average percentage change in moisture permeability for Group 3, which was a comparative example without the addition of a water-absorbing polymer, was 59.1%. The percentage change in moisture permeability for the structural protection sheets in all of the examples was 35% or less. [Explanation of Symbols]

[0071] 1. Structural protection sheet 2 resin layers 3. Polymer cement hardened layer 5. Primer layer 21. Structures (Concrete) 21' Concrete composition (structural composition) 22. Undercoat layer 23 Adhesives 24 formwork

Claims

1. A structure protection sheet comprising a hardened polymer cement layer provided on a structure side, and a resin layer provided on the hardened polymer cement layer, Radiation intensity 180W / m 2 The rate of change in moisture permeability before and after irradiation with light from a xenon lamp for 72 hours is 35% or less, The structure protection sheet, wherein the cured polymer cement layer is subjected to a water absorption treatment.

2. 2. The structure protection sheet according to claim 1, wherein the water absorption treatment is any method selected from the group consisting of a method of adding a water-absorbing polymer to the polymer cement cured layer, a method of adding an inorganic water-absorbing material to the polymer cement cured layer, a method of performing an aging treatment in a high humidity environment when preparing the polymer cement cured layer, a method of performing a heat treatment in a high humidity environment when forming the resin layer, a method of providing the polymer cement cured layer with a moisture-containing sheet that has absorbed moisture, and a method of performing wet curing after applying the structure protection sheet.

3. 3. The structure protection sheet according to claim 1, wherein the cured polymer cement layer is a layer containing a cement component and a resin, and the resin is contained in an amount of 10% by weight or more and 40% by weight or less.

4. A method for manufacturing a reinforced structure using the structure protection sheet according to claim 1, 2 or 3, comprising applying an adhesive onto a structure and then laminating the structure protection sheet.

5. The method for producing a reinforced structure according to claim 4, further comprising providing a primer layer between the structure and the adhesive.