Advanced Lithium-Ion Energy Storage Devices
Patent Information
- Application Number
- JP2023523248
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-10-19
- Filing Date
- 2021-10-19
- Publication Date
- 2024-10-25
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing lithium-ion capacitors (LiCs) have lower energy density compared to lithium-ion batteries (LiBs) and face challenges in combining the advantages of both in a single form, with manufacturing processes being time-consuming and costly.
A lithium ion capacitor device with a binder-free hybrid composite cathode and anode, utilizing high aspect ratio carbon elements and an ultrathin lithium film for prelithiation, eliminating the need for polymer binders and optimizing electrode thickness and capacitance ratios.
The device achieves higher energy and power densities, improved cycle life, and reduced manufacturing time and cost, bridging the gap between LiB and LiC performance.
Abstract
Description
[Technical Field]
[0001] Related Reference Cross-Reference This application is related to U.S. Provisional Patent Application No. 63 / 093441, entitled "Advanced Lithium-Ion Energy Storage Device," filed October 19, 2020; U.S. Provisional Patent Application No. 63 / 021492, entitled "Wide Temperature Electrolyte," filed May 8, 2020; U.S. Patent No. 10,600,582, entitled "Composite Electrode," issued March 24, 2020; U.S. Patent No. 9,001,495, entitled "High power and high energy electrodes using carbon nanotubes," issued April 7, 2015; and U.S. Patent No. 9,218,917, entitled "Energy storage media for ultracapacitors," issued December 22, 2015, the entire disclosures of which are incorporated herein by reference for all purposes.
[0002] The invention disclosed herein relates to energy storage devices, and in particular to lithium-containing electrodes made substantially without binder materials. [Background technology]
[0003] Lithium (Li)-ion batteries (LiBs) and electric double-layer capacitors (EDLCs) are two widely used electrochemical energy storage devices. Typical LiBs are fabricated using a lithium (Li)-intercalated anode and a Li-metal oxide cathode (thus relying on a reduction process or Faradaic mechanism of energy storage), whereas EDLCs are fabricated using high-surface-area activated carbon (AC) for both the anode and cathode (thus relying on double-layer capacitance or a non-Faradaic form of energy storage). As a result of their different energy storage mechanisms, these devices differ in their energy and power performance. LiBs exhibit high specific energy, e.g., 100–250 Wh / kg, but also have low specific power, e.g., <0.5 kW / kg, and poor cycle life, e.g., <5,000 cycles. EDLCs exhibit high specific power, e.g., 10 kW / kg, and long cycle life, e.g., >100,000 cycles, but EDLCs exhibit much lower specific energy, e.g., <6 Wh / kg.
[0004] An energy storage device that can combine the advantages of LiBs and EDLCs in a single form is highly desirable. As a new generation of supercapacitors, Li-ion capacitors (LiCs) are advanced energy storage devices that contain an EDLC cathode and a prelithiated anode, where ions shuttle between the EDLC cathode and the prelithiated anode during the charge and discharge process. Due to the use of a prelithiated low-surface anode material, LiCs can be charged to a voltage as high as 4.0 V, which is much higher than EDLCs and comparable to LiBs. Although LiCs can achieve a much higher power density than LiBs, their energy density is approximately 10–20 Wh / kg, which is still much lower than LiBs. Therefore, the energy density of LiC energy storage devices needs to be further improved.
[0005] What is needed are methods and apparatus to enhance the viability of LiC technology, preferably methods and apparatus that also reduce the cost and time required for manufacturing. Summary of the Invention
[0006] In one embodiment, a lithium ion capacitor device is provided that includes a positive electrode comprising a carbon network substantially free of binder material, a negative electrode comprising a carbon network substantially free of binder material separated from the positive electrode by a separator, and a film of lithium disposed on the negative electrode to provide prelithiation of the capacitor, wherein at least one of the positive and negative electrodes includes a network of high aspect ratio carbon elements defining voids within the network, and a plurality of electrode active material particles disposed in the voids within the network and entangled in the network.
[0007] In some embodiments, the high aspect ratio carbon elements include elements each having two major dimensions and one minor dimension, wherein the ratio of the length of each of the major dimensions is at least 10 times the length of the minor dimension. The high aspect ratio carbon elements may include elements each having two major dimensions and one minor dimension, wherein the ratio of the length of each of the major dimensions is at least 100 times the length of the minor dimension. The high aspect ratio carbon elements may include elements each having two major dimensions and one minor dimension, wherein the ratio of the length of each of the major dimensions is at least 1,000 times the length of the minor dimension. The high aspect ratio carbon elements may include elements each having one major dimension and two minor dimensions, wherein the ratio of the length of each of the major dimensions is at least 10,0000 times the length of the minor dimension. The high aspect ratio carbon elements may include elements each having one major dimension and two minor dimensions, wherein the ratio of the length of each of the major dimensions is at least 10 times the length of the minor dimension. The high aspect ratio carbon elements may include elements each having one major dimension and two minor dimensions, wherein the ratio of the length of each of the major dimensions is at least 100 times the length of each of the minor dimensions. The high aspect ratio carbon elements may include elements each having one major dimension and two minor dimensions, wherein the ratio of the length of each of the major dimensions is at least 1,000 times the length of each of the minor dimensions. The high aspect ratio carbon elements may include elements each having one major dimension and two minor dimensions, wherein the ratio of the length of each of the major dimensions is at least 10,000 times the length of each of the minor dimensions. The high aspect ratio carbon elements may include carbon nanotubes or carbon nanotube bundles. The high aspect ratio carbon elements may include graphene flakes. The electrode active layer may contain less than 10 wt. % of a polymer binder disposed in the voids. The electrode active layer may contain less than 1 wt. % of a polymer binder disposed in the voids. The electrode active layer may contain less than 1 wt% of a polymer binder disposed in the voids. The electrode active layer may be substantially free of polymeric materials other than the surface treatment. The electrode active layer may be substantially free of polymeric materials. The network may be at least 90 wt% carbon. The network may be at least 95 wt% carbon. The network may be at least 99 wt% carbon. The network may be at least 99.9 wt% carbon.The network may include an electrically interconnected network of carbon elements exhibiting connectivity above the percolation threshold. The network may define one or more highly conductive pathways. The pathways may have lengths greater than 100 μm. The pathways may have lengths greater than 1,000 μm. The pathways may have lengths greater than 10,000 μm. The network may include one or more structures formed from carbon elements, the structures having a total length at least 10 times the length of the longest dimension of the carbon elements. The network may include one or more structures formed from carbon elements, the structures having a total length at least 100 times the length of the longest dimension of the carbon elements. The network may include one or more structures formed from carbon elements, the structures having a total length at least 1,000 times the length of the longest dimension of the carbon elements. The positive electrode may include an electrode active material including at least one from the list consisting of activated carbon, carbon black, graphite, hard carbon, soft carbon, nanomorphic carbon, high aspect ratio carbon, and mixtures thereof. The positive electrode has a specific surface area of 1000 to 3000 m. 2 The positive electrode may include an electrode active material including activated carbon (AC) having a particle size D50≦10 μm. The negative electrode may include an electrode active material including activated carbon (AC) having a particle size D50≦10 μm. The positive electrode may include an electrode active material including activated carbon (AC), carbon black (BC), and high aspect ratio carbon, wherein the mass ratio of the active material to the high aspect ratio carbon is within a range of 80:20 to 99:1. The total thickness of the positive electrode and the lithium film may be within a range of 40 μm to 450 μm. The total thickness of the negative electrode may be within a range of 20 μm to 350 μm. The thickness ratio of the total thickness of the positive electrode active layer to the total thickness of the negative electrode active layer may be within a range of 1:2 to 3:1. The capacity ratio of the positive electrode active layer to the negative electrode active layer is within a range of 1:12 to 1:2. The lithium film may include an ultrathin lithium film containing pores. The mass per unit area of the lithium source on the side of the negative active layer is 0.1 mg / cm2 to 3 mg / cm2. 2The thickness of the lithium source on the side of the negative active electrode layer can be in the range of 2 to 50 μm. The surface area of the lithium film can be about 25% to about 100% of the surface area of the side of the negative electrode. The lithium film can include pores, the area size percentage range of which is about 0.01% to about 75% of the total area of the film.
[0008] In another embodiment, a method of making a lithium ion capacitor is provided. The method includes providing an energy storage cell by selecting a positive electrode including a carbon network substantially free of binder material, selecting a negative electrode including a carbon network substantially free of binder material separated from the positive electrode by a separator, disposing a film of lithium on the negative electrode to provide prelithiation of the capacitor, and sealing the energy storage cell and electrolyte in a housing to provide the capacitor. The lithium ion capacitor may include the device described above. [Brief explanation of the drawings]
[0009] The features and advantages of the present invention will become apparent from the following description taken in conjunction with the accompanying drawings.
[0010] A series of photomicrographs, a flow chart and performance graphs are provided. DETAILED DESCRIPTION OF THE INVENTION
[0011] Disclosed herein are methods and apparatus for the fabrication of hybrid binder-free electrodes useful in energy storage devices. Advantageously, by being substantially free of binder materials traditionally used in the construction of electrodes, the electrodes disclosed herein can provide superior electrical performance and require fewer steps in the manufacturing process.
[0012] The energy storage devices disclosed herein combine the advantages of LiB and LiC while avoiding their inherent drawbacks, bridging the gap between the high energy density offered by LiB and the high power density exhibited by LiC. In particular, the fundamental difference between this Li-ion energy storage device and LiC is that hybrid Li-ion technology integrates two separate energy storage devices into one by synergistically combining LiB and LiC cathode materials together to form a hybrid composite cathode. Non-faradaic capacitor materials can initially be electrostatically charged until the electrode potential reaches the reduction reaction potential of the faradaic battery material, where the battery material is charged while maintaining a constant battery reduction reaction potential. Once fully charged, the capacitor material is charged again until the limiting potential of the capacitor material is reached.
[0013] Generally, the disclosed technology relates to a hybrid lithium-ion energy storage device including a binder-free hybrid composite cathode electrode, a binder-free anode electrode, a separator, an organic solvent electrolyte solution containing a lithium salt as an electrolyte, and an ultrathin lithium film (μ-Li) source. The ultrathin lithium film may include a plurality of pores. The ultrathin lithium film pre-dopes the anode electrode with sufficient lithium ions. The pre-doping may occur by disposing the ultrathin lithium film substantially on the surface of the anode electrode. Additionally, the hybrid composite cathode may be fabricated using a polymer binder-free manufacturing process, and the resulting capacity ratio of the hybrid composite cathode to the anode electrode may be 0.1 to 1.2. The mass of the ultrathin lithium film disposed on the anode electrode may be predetermined by a calculation formula to achieve high energy, power, and long cycle life performance in a full-cell format design.
[0014] A schematic diagram of an energy storage device is shown in Figure 1. In the example of Figure 1, the energy storage device (ESD) 10 is a three-layer cell. Opposing current collectors 2 host cathode material 3. Collectively, the current collectors 2 and cathode material 3 provide each of the two cathodes 4 shown. An anode 8 is shown disposed between the cathodes 3. In this example, the anode 8 comprises opposing layers of anode material 5 disposed on separate current collectors 6. A lithium source 7 is disposed on each layer of anode material. In this example, the current collector 2 for the cathode is made from aluminum, and the current collector 6 for the anode is made from copper.
[0015] 2A and 2B, an example of a cathode material 3 comprising activated carbon is shown. These figures show SEM images of cathode material 3 from the prior art (FIG. 2A) and in accordance with the teachings herein (FIG. 2B). As can be seen, the image of the cathode 4 disclosed herein contains substantially more carbon, which, as can be easily inferred, allows for greater energy storage than the device of FIG. 2A.
[0016] For discussion purposes, two examples of cathode materials are presented herein. The first example includes an electrode with pure activated carbon (AC) (LiC with 0% lithium iron phosphate (LFP)), and the second example includes a hybrid binder-free electrode (with a 20:80 LFP to AC ratio). In the binder-free electrode, the provided carbon structure provides excellent bonding with the active material and serves to bind the cathode together without the need for traditional polymers or similar non-conductive or low-conductivity binders. As a result of the absence of a (non-conductive) binder, the carbon structure results in higher conductivity and higher cell performance. In this disclosure, a commercially available dry-process AC binder-based electrode is used as a baseline for comparison.
[0017] Generally, binder materials are non-conductive or low-conductivity materials added to electrode materials to promote the mechanical integrity of the electrode layer and good adhesion to the current collector. The use of binder materials replaces other materials capable of energy storage and conduction, reducing the power output of the energy storage cell used. One example of a binder is PVDF. Polyvinylidene fluoride (PVDF) is a highly non-reactive thermoplastic fluoropolymer produced by polymerization of vinylidene difluoride. PVDF is typically used in cathodes. A common anode binder material is styrene-butadiene copolymer.
[0018] Similarly, Figures 3A, 3B, and 3C show anode material 5. Figure 3A shows an SEM of hard carbon powder. Figure 3B shows a prior art anode 8 made from hard carbon powder and a binder material. Figure 3C shows an embodiment of anode 8 in accordance with the teachings herein.
[0019] For illustrative purposes, the anode 8 presented herein was composed of hard carbon (HC) as the active material. A slurry mixture for the anode was prepared, which included HC with a particle size (D50) of 2 μm and carbon nanotubes (CNT and CMC) with carboxymethyl cellulose serving as a binder material. In this example, the mass ratio of the three components was 98.33:0.67:1. After the slurry was prepared, it was coated onto a 10 μm-thick copper (Cu) foil substrate. The electrode was then dried in an oven at 160°C for 3 hours with flowing air. The active material layer on each side was approximately 75 μm thick and had a tap density of 1.0 g / cm. 3 Anode electrode sheets were fabricated using a hard carbon anode. The porosity of the hard carbon anode was approximately 50 percent. Electrodes were then cut from the electrode sheets to the desired dimensions (4.6 cm x 4.6 cm (active area) for the anode and 4.5 cm x 4.5 cm for the cathode), then vacuum dried overnight at 120 degrees Celsius and transferred to a dry room environment where the final cell was assembled. The electrodes were assembled into the configuration shown in Figure 1.
[0020] In the assembly of ESD 10, a lithium source 7 was incorporated into all anodes 8. In each embodiment, the lithium source 7 comprised an ultrathin lithium film with holes therein. The holes were cut from a 20 μm Li metal sheet (99.9% purity). The lithium source 7 provided lithium sources of various sizes for prelithiation to fabricate various LFP / AC hybrid composite cathode-based LiB / LiC cells. Based on the first lithium intercalation specific capacity of the HC anode, which was approximately 372 mAh / g, the amount of u-Li preloaded with holes on the surface of the HC anode to fully prelithiate the HC was determined to be approximately 10% (u-Li preload mass / anode active layer mass). In the cell design for LiC (0% LFP), the cathode-to-anode capacity ratio was approximately 0.14 (1:7), so it was determined that the anode should be prelithiated (at approximately 10% lithium loading). This LiC cell design enables LiC to have long cycles and high energy and power densities. However, when LFP is mixed into the hybrid composite binder-free cathode, the LFP provides an additional lithium source from the hybrid cathode when charging to the maximum operating voltage. To avoid the growth of lithium dendrites in the anode during cell charging, the actual mass loading of the lithium source 7 (i.e., the ultrathin lithium film with pores) placed on the surface of the anode should take into account the portion of the lithium source provided by the LFP in the hybrid cathode and therefore should be less than 10% of the anode active layer weight. We can conclude that the decrease in the lithium source 7 in the anode is likely correlated with the increase in LFP in the cathode.
[0021] During cell assembly, the lithium source 7 was filled in a dry room environment. The ultrathin lithium membrane was placed under pressure. An example of an assembled ESD 10 follows the scheme shown in Figure 1. The anode was a double-sided HC anode preloaded with a porous lithium source and sandwiched between two single-sided LFP / AC composite cathodes. The electrolyte used was 1 M LiPF6 in a 1:1 weight ratio mixture of ethylene carbonate (EC) and dimethyl carbonate (DMC). All pouch cell assembly was performed in a dry room environment (dew point -40 °C). Figure 4 shows the charge / discharge profiles collected during initial testing.
[0022] Figure 4 shows the initial test results of LiC using binder-free AC and HC electrodes under different current charge and discharge conditions. Test conditions for these examples included a cathode porosity of 83.1% and an anode porosity of 64.1%. The cell voltage ranged from 3.8 to 2.2 V, the capacitance was 11.2 F, the ESR was 0.127 Ω, and the RC constant was 1.4 s. The specific energy and energy density, based on the weight and volume of the cathode and anode active layers, were measured to be 36.6 Wh / kg and 20.1 Wh / L, respectively. The maximum specific power and power density, based on the weight and volume of the cathode and anode active layers, were measured to be 69.7 kW / kg and 35.3 kW / L, respectively.
[0023] As a result, with this cell design, it is estimated that the specific energy and energy density of a full-sized multi-layer 1000F LiC pouch cell can be 9 Wh / kg and 16 Wh / L, which are substantially higher than the competitive 1000F LiC energy density (13.7 Wh / L). Furthermore, with this cell design, it is estimated that the ESR of a full-sized multi-layer 1000F LIC pouch cell can be 1.4 mohm, which is lower than the ESR of a competitive 1000F LIC cell (1.6 mohm). Table 1 below provides a more detailed comparison with the prior art. [Table 1]
[0024] As can be seen from the comparison in Table 1, the ESR of the binder-free electrode-based LiC was 30.6% lower than that of the binder-based (i.e., prior art) control sample. Similarly, the RC constant of the LiC with the binder-free electrode was only 1.4 seconds, while the binder-based LiC had an RC constant of 5.1 seconds. The maximum specific power and power density of the binder-free electrode-based LiC were 131.6 percent and 64.6 percent higher, respectively, than that of the binder-based (i.e., prior art) control sample. Figure 5A shows the comparative ESR, and Figure 5B is an exploded view of the curve shown in Figure 5A. Aspects of the second embodiment tested are presented in Figures 6A, 6B, 7A, and 7B.
[0025] In the second embodiment, comparative performance was investigated using soft carbon and AC and LFP binder-free electrodes. The SC:CNT:CMC ratio was the same as in the HC slurry, but this time 20 percent LFP was added to the carbon framework along with activated carbon (AC) to achieve a hybrid composite electrode. Figures 6A and 6B are micrographs of the soft carbon-based electrode. Figures 7A and 7B are micrographs of the AC and LFP binder-free electrode. The storage cell was assembled using the same procedure as in the first embodiment outlined above. The physical aspects of the storage cell are listed in Table 2. [Table 2]
[0026] In Table 2, the control cells (i.e., prior art soft carbon) are identified as A53 and A21. The storage cells made without binder are identified as B43 and B44. The electrolytes used in the storage cells were as follows: A53: 1.0 M LiPF6 + 1% VC in EC / DMC; A21: 1.0 M LiPF6 + 0.1 M LiDFOB in EC / EMC / MB (20:20:60 by volume); B43: 1.0 M LiFSI + 1% VC in EC / EMC / DEC / PC (20:46.7:23.3:10 by volume); and B44: 1.0 M LiFSI + 1% VC in EC / EB / DEC / PC (20:46.7:23.3:10 by volume). The initial charge-discharge profiles of the storage cells were 0.25 and 12.5 mA / cm2 (10 and 500 mA). Figure 8 shows the charge / discharge performance of the four cells, including the initial constant current charge / discharge along with the ESR results.
[0027] Figure 9 shows the results of the low-temperature test. Because A53 did not operate below -45°C, it was not included in the charge-discharge test. In the test, A21 showed the highest capacity retention at -45°C (approximately 40%). B44 showed the second-highest capacity retention at -45°C (approximately 30%). Based on the cell design, the specific energy of the LIC was approximately 22.4 Wh / kg, and 30% retention was 6.7 Wh / kg, which is still half the original design's 13 Wh / kg. The LFP additive appeared to reduce capacity retention for the low-temperature test. Figure 10 provides a comparative performance of the soft and hard carbon anodes. It can be seen that B44 exhibited the best impedance compared to the other two electrolytes. In terms of EIS, the hard carbon anode performed slightly better than the soft carbon anode with LIC, as indicated by the smaller semicircle in the graph.
[0028] The third embodiment was directed to the optimization of electrolyte formulations for both high and low temperatures. In this embodiment, Y4 was the electrolyte control sample and was 1.0 M LiTFSI, EC / EMC / MB (20:20:60 by volume) + 1 percent VC. Y5 and Y5.1 were BCN solvent-based electrolytes containing LiTFSI salts with additives including VC, FEC, LiDFOB, LiBOB, LiDFOP, and LiNO. The electrolyte formulation for Y5 was 1.0 M LiTFSI in BCN / EC / VC (80 / 10 / 10 by volume), and the electrolyte formulation for Y5.1 was 1.0 M LiTFSI in BCN / EC / VC (80 / 10 / 10 by volume) + 1% OS3, a commercially available additive.
[0029] Figure 11 is a graph showing ESR performance as a function of temperature for three different electrolytes. At temperatures as low as minus 40 degrees Celsius, the binder-free LIC had an ESR increase of 3.4 Ω, while the conventional binder-based LIC had an ESR increase of 5.1 Ω. Using the Y5 electrolyte, the cell also passed long-term cycle life testing, and the results are shown in Figure 12. Figure 12 shows room-temperature, high-C-rate cycle life testing of the LIC using the Y5 electrolyte. The voltage range is 3.8 to 2.2 V, and the current is approximately 500 mA.
[0030] In the fourth experiment, the performance of both high-temperature (85°C) and low-temperature (-55°C) electrolyte formulations was evaluated. Y7 was designated a BCN solvent-based electrolyte containing LiTFSI salt with cosolvents including GBL (gamma-butyrolactone), VC, and FEC, and additives including LiDFOB, LiBOB, LiDFOP, LiNO3, etc. The Y7 electrolyte formulation was 1.0 M LiTFSI in BCN / GBL / VC / OS3 (74.5 / 12.5 / 10 / 3 by volume). Figures 13-15 show the high-temperature cycling and direct charging results of LICs using the Y7 electrolyte. Y7 has the same low-temperature performance at -55°C as Y5 and Y5.1. Figure 13 shows the cycle life performance plot of a cell with the Y7 electrolyte charged and discharged from 3.8 V to 2.2 V under a constant current of 500 mA, showing the capacitance / ESR retention as a function of cycle number, in an 85°C cycling environment. Figure 14 shows the discharge curves for various cycle numbers when LIC cycling at 85°C based on Y7 electrolyte, and Figure 15 shows a comparison of the discharge curves after holding a constant voltage of 3.8V (float test) at 85°C for around 330 hours.
[0031] A method for fabricating a storage cell in accordance with the teachings herein is illustrated in FIG.
[0032] In some embodiments, the positive electrode used is an electrode comprising a sheet metal current collector coated on both sides with a conductive material and electrode layers formed on both sides of the current collector, each consisting of a positive electrode active material and CNTs.The negative electrode used in this LIC laminate cell is an electrode comprising a sheet metal current collector coated on both sides with a conductive material and electrode layers formed on both sides of the current collector, each consisting of a negative electrode active material and an additive.
[0033] The current collector used for the positive electrode can be made of aluminum, stainless steel, or other materials. In some of the examples presented, aluminum is used. The current collector used for the negative electrode can be made of stainless steel, copper, nickel, etc., and in some of the examples presented, copper is used. Generally, the thickness of the positive and negative electrode current collectors is within the range of approximately 5 to 50 μm. In the examples presented, the range is 8 to 25 μm. This range ensures high strength of the resulting positive and negative electrodes and facilitates application of the conductive paint slurry. This improves the coating accuracy, volumetric energy density, and weight energy density of the conductive material. Carbon conductive paint slurry was spray-coated on both sides of the positive and negative electrode current collectors and dried to obtain current collectors with conductive layers for both the positive and negative electrodes. The thickness of the carbon conductive coating on one side of the current collector is 1 to 20 μm. In the examples presented, the thickness was within the range of 3 to 12 μm.
[0034] The positive and negative electrodes can be made using the electrode active materials described above. Specifically, the positive and negative electrode active material powders, CNTs, and some solvent are dispersed and mixed in a blender / mixer to form a wet slurry mixture. The percentage of additives added to the powder / slurry mixture is preferably 2 to 12 percent. For positive electrode fabrication, the slurry may be prepared without a binder. The slurry mixture is then coated onto a substrate, which will serve as the positive electrode active material layer. The thickness of the positive electrode active layer is 30 to 250 μm, or in some embodiments, 50 to 200 μm. The binder-free electrode is then calendered using a hot mill roller at a high temperature to form the final positive electrode for LIC cells with the desired porosity and press density. The positive electrode active material, additives, and deionized water / IPA as a solvent are first mixed in a mixer for a sufficient time to form a uniform wet slurry. Next, the slurry is coated onto both sides of a precoated carbon conductive current collector using an electrode coater equipped with a drying oven to dry the coated electrode. The gap of the coating machine can be adjusted according to the initial thickness requirements for the electrode. The dried electrode is then pressed through a hot press calendar to the desired active layer thickness, forming the final positive electrode for the LIC cell. The thickness of the positive electrode active layer, based on the wet slurry fabrication method on one side of the current collector, is 3 to 250 μm, and in some embodiments, 5 to 200 μm.
[0035] The negative electrode active material, CNT / CMC additive, and deionized water as a solvent are first mixed in a mixer for a sufficient time to form a uniform wet slurry. The slurry is then coated onto both sides of a pre-coated carbon conductive current collector using an electrode coater equipped with a drying oven to allow the coated electrode to dry. The gap of the coater can be adjusted according to the initial thickness requirements for electrode fabrication. The dried electrode is then pressed down through a hot press calendar to the desired active layer thickness to form the final negative electrode for an LIC cell. The thickness of the negative electrode active layer based on the wet slurry fabrication method on one side of the current collector is 3 to 200 μm, with 5 to 160 μm being used in some embodiments.
[0036] In some embodiments of the LiC cells presented herein, the total thickness of the positive electrode, including the thickness of the double-sided conductive material pre-coated current collector and the thickness of the double-sided active layer, can be 40 μm to 450 μm. In some embodiments of the LiC cells presented herein, the total thickness of the negative electrode, including the thickness of the double-sided conductive material pre-coated current collector and the thickness of the double-sided active material layer, can be 20 μm to 350 μm. In some embodiments of the LiC cells presented herein, the thickness ratio of the total thickness of the positive electrode active layer to the total thickness of the negative electrode active layer can be 1:2 to 3:1.
[0037] Generally, the positive electrode used is an electrode comprising a sheet metal current collector coated on both sides with a conductive material and an electrode layer formed on both sides of the current collector, the electrode layer being composed of a positive electrode active material and CNTs. The negative electrode used in the LIC laminate cell of the present invention is an electrode comprising a sheet metal current collector coated on both sides with a conductive material and an electrode layer formed on both sides of the current collector, the electrode layer being composed of a negative electrode active material and an additive.
[0038] Generally, the Li source preloaded on the surface of the negative electrode is an ultra-thin Li film with holes. The ultra-thin Li film with holes is applied to the surface of all pre-fabricated negative electrodes by a manufacturing method of laminating negative electrodes with upper and lower ultra-thin Li films with holes, which is described in detail in U.S. Patent Application No. 15 / 489,813, the entire contents of which are incorporated herein by reference. The manufacturing can be carried out in a dry room with a dew point below -45°C. The pressure of the laminating roll is 40 kg / cm. 2 ~400kg / cm 2 In some embodiments of the LiC cells presented herein, the mass per unit area of the pore-filled ultrathin Li film on one surface of the negative electrode can be 0.1 mg / cm 2 ~3mg / cm 2 The thickness of the ultrathin Li film having holes preloaded on one side of the negative electrode is preferably 2 to 50 μm. The length of the ultrathin Li film having holes as Li sources filled on the surface of the negative electrode may be 30 mm to 250 mm, and the width of the ultrathin Li film having holes as Li sources filled on the surface of the negative electrode may be 30 mm to 150 mm. The area of the ultrathin Li film having holes as Li sources filled on the surface of the negative electrode may be about 25% to about 100% of the area of the negative electrode. The area size percentage range of the holes in the ultrathin Li film having holes as Li sources filled on the surface of the negative electrode may be about 0.01% to about 75%. The mass ratio percentage of the ultrathin Li film having holes preloaded on both sides of the negative electrode to the negative electrode active layer on both sides is preferably 7% to 14%. After all of the ultrathin Li films having holes are pressed onto the negative electrode, a uniform thin layer Li source position distribution may be present on the surface of the negative electrode.
[0039] In some embodiments of the LiC cells presented herein, electrodes, including positive and negative electrodes with a lithium source preloaded on their surfaces, are cut to a specified size along with some additional current collector tabs before being stacked into a cell core unit. The size of the electrodes determines the final size of the LiC cell, since the outer container must match the size of the electrodes. In some embodiments, the length and width of the negative electrode are 0.5 mm to 5 mm larger than those of the positive electrode of the LiC cell. In some embodiments of the LiC cells presented herein, the length of the cut positive and negative electrodes may be 30 mm to 250 mm, and the width of the cut positive and negative electrodes may be 30 mm to 150 mm.
[0040] Having introduced aspects of the lithium ion capacitor, additional features and embodiments will now be introduced.
[0041] In LiC, activated carbon may be used as the positive electrode (PE), while the negative electrode (NE) material may include various materials such as soft carbon, hard carbon, graphite, etc.
[0042] The cell components and design can be modified to improve the electrochemical performance of LiC. This may include the active materials and CNTs selected for the PE and NE active materials, the thickness / mass ratio of the PE to NE active layer (without the current collectors containing aluminum (Al) and copper (Cu)), the capacity ratio of the PE to NE active layer, the sizing and number of layers of the PE and NE, the type of material for the separator, the electrolyte composition, and the prelithiation method for the NE. For PE, the active material can be binderless activated carbon (AC). For NE, the active material can be hard carbon (HC), soft carbon (SC), graphite (G), and other carbon-based materials, and a network of CNTs with a CMC can be relied upon to create a robust carbon structure for the active material. The separator material can be polypropylene (PP), polyethylene (PE), cellulose, or other similar materials.
[0043] In some embodiments of the LiC cell presented herein, a cell core unit is formed by stacking a positive electrode and a negative electrode through a separator in an outer container, such as a laminated outer container. The negative electrode is pre-doped by pressing a lithium source containing an ultra-thin Li film with holes onto the surface of the negative electrode. "Pre-doping" broadly describes the phenomenon in which lithium ions penetrate into the negative electrode active layer. The ultra-thin Li film with holes is the lithium ion source for pre-doping the negative electrode. The lithium source filling process ensures that the negative electrode contains uniform lithium on its surface, so that the negative electrode can be smoothly and uniformly pre-doped with lithium ions once the electrolyte is filled.
[0044] In some embodiments of the LiC cell presented herein, the Cu and Al substrates are welded to nickel (Ni)-coated copper (Cu) and aluminum (Al) current collector tabs, respectively. After the lamination and welding process, the electrode unit is placed in a container, such as an aluminum laminated case suitable for the size of the electrode unit, and a three-sided heat-sealing process is applied. A desired amount of electrolyte is then filled into the LIC laminated cell to immerse the cell, initiating the pre-doping process by intercalating lithium into the negative electrode. After the cell has been immersed for a sufficient time, a vacuum sealing process is applied to the cell to remove excess gas trapped within the LIC laminated cell. As a result, such a configuration can be realized in the LIC laminated cell.
[0045] The organic electrolyte can be a Li-ion battery electrolyte containing a Li salt. Prelithiation of the NE can be performed to ensure that the LIC can achieve the desired electrochemical performance. Some prelithiation methods, including the electrochemical (EC) method and the external short-circuit (ESC) method, involve predoping a graphite electrode or an HC electrode with lithium using a piece of Li metal as a sacrificial third electrode. In the EC prelithiation method, the NE and Li metal are separated by a separator in a lithium salt-based organic electrolyte, and the predoping process can be carried out by an electronic charger that controls the charging current or voltage.
[0046] The positive electrode active material is preferably capable of reversibly absorbing and desorbing lithium ions and anions in an electrolyte such as tetrafluoroborate. One example of such an active material is activated carbon powder. The specific surface area of activated carbon is 1,500 m 2 / g~2,800m 2 / g, preferably 1,600m 2 / g~2,400m 2 / g. The 50% cumulative volume diameter (D50) (average particle diameter) of the activated carbon is preferably 2 μm to 10 μm. To further improve the energy density and power density of the LIC laminate cell, it is particularly preferably 3 μm or more and 8 μm or less. Some other examples of such materials are carbon black and activated carbon / carbon black / CNT composite materials (AC / CB / CNT).
[0047] It is desirable for the negative electrode active material to be capable of reversible intercalation and deintercalation of lithium ions. Examples of such active materials include graphite-based composite particles, difficult-to-graphitize carbon (hard carbon, (HC)), and easily graphitized carbon (soft carbon, (SC)). In some embodiments, HC and SC particles are preferred as negative electrode active materials because they can achieve higher power performance and cycle stability than graphite materials. However, graphite materials can achieve higher energy performance relative to LICs because graphite has a higher specific capacity than HC and SC. To improve the output performance of LIC cells, it is preferable to use HC and SC negative electrode active materials with particle sizes whose 50% cumulative volume diameter (D50) is in the range of 1.0 to 10 μm, and in some embodiments, preferably in the range of 2 to 6 μm.
[0048] It is difficult to produce HC and SC particles having a 50% cumulative volume diameter (D50) of less than 10 μm. If the 50% cumulative volume diameter (D50) of the HC and SC particles exceeds 10 μm, it becomes difficult to realize an LIC cell having a sufficiently low internal resistance. In some embodiments, the negative electrode active material has a particle diameter of 0.1 to 200 μm. 2 / g, and has a specific surface area of 0.6 to 60 m 2 The reason for setting the range is that the specific surface area of the negative electrode active material is 0.1 m / g. 2 / g, the resistance of the LIC cell can be increased, and the specific surface area of the negative electrode active material is 200m 2 This is because if it is greater than 1 / g, the irreversible capacity of the LIC laminate cell during charging can be increased.
[0049] In the ESC prelithiation method, the NE and sacrificial Li metal third electrodes are short-circuited through an external electrical wire connection. However, with conventional prelithiation methods, it takes time for the lithium to dissipate and the cell to fully lithiate the NE in the LIC laminate cell. This time adds to the cost of this method. Additionally, with conventional prelithiation methods, both the PE and NE current collectors must be porous to provide a path for lithium ions to migrate from the Li metal electrode through the LIC laminate cell, which also increases the manufacturing cost of the electrodes.
[0050] The prelithiation technique disclosed herein addresses some of these issues. By filling the surface of NEs with an ultrathin, porous lithium film (abbreviated as u-Li), the cell fabrication process can be facilitated and prelithiation can be accelerated. Because Li metal can be directly coated onto the carbon electrode, the current collector does not need to be porous to allow Li ions to intercalate into the NEs. After the cell is impregnated with electrolyte, the Li source on the surface of the NEs electrochemically reacts with the carbon electrode active layer and intercalates into the NEs.
[0051] Some advantages of the techniques disclosed herein are now presented.
[0052] An advantage of the disclosed technology is a lithium ion capacitor (LIC) that has excellent characteristics in life, including cycle life and DC life, while maintaining high energy density and power density.
[0053] The advantage of the disclosed technology is an LIC that has a binder-free positive electrode, a negative electrode with a lithium source preloaded on its surface called an ultrathin porous lithium film (u-Li), a separator, and an organic solvent electrolyte solution with a lithium salt as the electrolyte.
[0054] An advantage of the disclosed technology is a LIC cell in which the positive electrode active material is preferably activated carbon, carbon black, CNT, and activated carbon / carbon black / CNT mixture (AC / CB / CNT), and the negative electrode active material is preferably hard carbon, soft carbon, graphite, CNT, and any possible mixture of the above materials.
[0055] The advantage of the disclosed technology is that the positive electrode active material activated carbon (AC) is 1000 to 3000 m 2 The LIC cells have a surface area in the range of 1 / g.
[0056] An advantage of the disclosed technology is a LIC cell in which the positive electrode active material activated carbon (AC) has a particle size D50≦10 μm and the negative electrode active material has a particle size D50≦10 μm.
[0057] An advantage of the disclosed technology is an LIC cell in which no polymer binder is used in the cathode material, which increases the conductivity of the electrode and improves power performance.
[0058] An advantage of the disclosed technology is an LIC cell in which the positive electrode formulation can be tailored with a range of mass ratios between AC / CB and CNT / carbon framework, and no or substantially no polymer binder is used.
[0059] An advantage of the disclosed technology is a LIC cell, wherein the additives for manufacturing the negative electrode used in the LIC cell are preferably CNTs and carboxymethyl cellulose (CMC).
[0060] An advantage of the disclosed technology is a LIC cell in which the negative electrode formulation can be tailored with a range of mass ratios between the negative electrode active material and CNT / CMC.
[0061] An advantage of the disclosed technology is an LIC cell in which the total thickness of the positive electrode, including the thickness of the double-sided conductive material pre-coated aluminum (Al) foil and the thickness of the double-sided active material layer, is 40 μm to 450 μm.
[0062] An advantage of the disclosed technology is an LIC cell in which the total thickness of the negative electrode, including the thickness of the double-sided conductive material pre-coated copper (Cu) foil and the thickness of the double-sided active material layer, is 20 μm to 350 μm.
[0063] An advantage of the disclosed technology is an LIC cell in which the thickness ratio between the total thickness of the positive electrode active layer and the total thickness of the negative electrode active layer is preferably 1:2 to 3:1.
[0064] An advantage of the disclosed technology is an LIC cell in which the capacity ratio between the positive electrode active layer and the negative electrode active layer is preferably 1:12 to 1:2.
[0065] The advantage of the disclosed technology is an LIC cell in which the separator material is a cellulose, polypropylene (PP) and polyethylene (PE) based material.
[0066] The advantage of the disclosed technology is that the mass per unit area of the Li source, which includes an ultrathin lithium film with filled pores on one surface of the negative electrode, is 0.1 mg / cm 2 ~3mg / cm 2 Preferably, the LIC cell is
[0067] An advantage of the disclosed technology is a LIC cell in which the thickness of the Li-source ultrathin Li film (u-Li) with filled pores on one surface of the negative electrode is preferably 2-50 μm.
[0068] The advantage of the disclosed technology is a LIC cell in which the area of the ultrathin Li film (u-Li) having holes as a Li source preloaded on one surface of the negative electrode is about 25% to about 100% of the area of the negative electrode.
[0069] An advantage of the disclosed technology is a LIC cell having pores as Li sources preloaded on the surface of the negative electrode, where the pore area size percentage range of the ultrathin Li film is 0.01% to about 75%.
[0070] The advantage of the disclosed technology is that, in an LIC cell, the mass ratio percentage of a Li source including an ultrathin Li film with holes preloaded on one surface of a negative electrode to the active layer of one negative electrode is preferably 7% to 14%.
[0071] An advantage of the disclosed technology is that the LIC cell is a laminated cell or a prismatic cell.
[0072] The advantage of the disclosed technology is an ultrathin (≦1 mm thick) LIC with two ultrathin (≦50 μm thick) single-sided positive electrodes, one ultrathin (≦50 μm thick) double-sided negative electrode with a porous ultrathin lithium film (u-Li) preloaded on its surface, a separator, and an organic solvent electrolyte solution with a lithium salt as the electrolyte.
[0073] Advantages of the disclosed technology include an unexpected solution to the problem of creating lithium ion capacitor (LIC) cells with high energy and power densities, along with excellent cycleability and DC life. In a preferred embodiment of the LIC cell system of the present invention, the negative electrode is pre-doped with lithium ions by applying a lithium source comprising an ultrathin porous Li film onto the surface of the negative electrode.
[0074] When pre-doped in this manner, there are many factors that affect the electrochemical performance and capacity of LIC cells, including: (1) the materials used in the positive and negative electrodes, including the active materials and additives; (2) the method for manufacturing the positive and negative electrodes; (3) the thickness of the positive and negative electrodes; (4) the thickness ratio of the total thickness of the positive electrode active layer to the total thickness of the negative electrode active layer; (5) the capacity ratio of the positive electrode active layer to the negative electrode active layer; (6) the material of the separator for the LIC cell; (7) the mass per unit area of the Li source including the ultrathin Li film with holes preloaded on the surface of the negative electrode; (8) the thickness of the Li source including the ultrathin Li film with holes preloaded on the surface of the negative electrode; (9) the area design of the ultrathin Li film with holes preloaded on the surface of the negative electrode and the area design of the holes in the ultrathin Li film with holes; and (10) the mass ratio percentage of the Li source including the ultrathin Li film with holes preloaded on one surface of the negative electrode relative to the negative electrode active layer on one side.
[0075] An advantage of the disclosed technology is a LIC cell that includes a polymer binder-free positive electrode, a polymer binder-free negative electrode preloaded on its surface with a lithium source that includes an ultrathin lithium film with holes, a separator, and an organic solvent electrolyte solution with a lithium salt as the electrolyte.
[0076] In some embodiments, the positive electrode active material is activated carbon, carbon black, CNT, or an activated carbon / carbon black / CNT mixture (AC / CB / CNT). In the LIC cells of the present invention, the negative electrode active material is preferably graphite, hard carbon, and soft carbon, or any possible mixture of the above materials.
[0077] In some embodiments, the positive electrode active material activated carbon (AC) is 1000 to 3000 m 2 / g.
[0078] In some embodiments, the positive electrode active material activated carbon (AC) has a particle size D50≦10 μm, and the negative electrode active material has a particle size D50≦10 μm.
[0079] In some embodiments, the positive electrode formulation can be adjusted in a range of mass ratios between AC / CB and CNT, where the mass ratio between AC and CB is 80:20 to 99:1.
[0080] In some embodiments, the total thickness of the positive electrode, including the thickness of the double-sided conductive material-precoated aluminum foil and the thickness of the double-sided active material layer, is 40 μm to 450 μm. In the LIC cell of the present invention, the total thickness of the negative electrode, including the thickness of the double-sided conductive material-precoated copper foil and the thickness of the double-sided active material layer, is 20 μm to 350 μm. In the LIC cell of the present invention, the thickness ratio of the total thickness of the positive electrode active layer to the total thickness of the negative electrode active layer is preferably 1:2 to 3:1.
[0081] In some embodiments, the volume ratio of the positive electrode active layer to the negative electrode active layer is preferably 1:12 to 1:2.
[0082] In some embodiments, in LIC cells, the separator material is preferably cellulose, polypropylene (PP) and polyethylene (PE) based materials.
[0083] In some embodiments, the mass per unit area of the Li source comprising an ultrathin Li film with filled pores on one surface of the negative electrode is 0.1 mg / cm 2 ~3mg / cm 2 Preferably, the LIC cell is
[0084] In some embodiments, the thickness of the Li source comprising an ultrathin Li film with preloaded holes on one surface of the negative electrode is preferably 2 to 50 μm.
[0085] In some embodiments, the area of the ultrathin Li film having holes as a Li source preloaded on the surface of the negative electrode is preferably about 25% to about 100% of the area of the negative electrode.
[0086] In some embodiments, the area size percentage range of the pores in the ultrathin Li film having pores as Li sources preloaded on the surface of the negative electrode is preferably about 0.01% to about 75%.
[0087] In some embodiments, the mass ratio percentage of the Li source including the ultrathin Li film with holes preloaded on both sides of the negative electrode to the active layers of both negative electrodes is preferably 7% to 14%.
[0088] In some embodiments, an ultrathin (≦1 mm thick) LIC cell is provided with two ultrathin (≦50 μm thick) single-sided positive electrodes, one ultrathin (≦50 μm thick) double-sided negative electrode with a porous ultrathin lithium film (u-Li) preloaded on its surface, a separator, and an organic solvent electrolyte solution with a lithium salt as the electrolyte.
[0089] In some embodiments, LIC cells are provided that have high energy density, high power density, and long life performance.
[0090] With regard to the above description, it should be understood that the optimum dimensional relationships of the parts of the present invention, including variations in size, material, shape, form, function, and method of operation, assembly, and use, will be readily apparent and self-evident to those skilled in the art, and that all equivalent relationships to those shown in the drawings and described herein are intended to be encompassed by the present invention. The foregoing is therefore considered merely illustrative of the principles of the present invention. Moreover, since numerous modifications and changes will readily occur to those skilled in the art, it is not desired to limit the invention to the exact construction and operation shown and described, and therefore, all suitable modifications and equivalents are intended to be embraced within the scope of the present invention.
[0091] As used herein, certain acronyms should be associated with the following terminology: dimethyl carbonate (DMC); lithium difluoro(oxalato)borate (LiDFOB); lithium bis(fluorosulfonyl)imide (LiFSI); propylene carbonate (PC); ethylene carbonate (EC); ethyl methyl carbonate (EMC); ethylene glycol monobutyl ether (EB); diethyl carbonate (DEC); vinylene carbonate (VC); boron nitride carbon (BCN); lithium difluoro(oxalato)borate (LiDFOB); lithium bis(oxalato)borate (LiBOB); lithium difluorobis(oxalato)phosphate (LiDFOP); lithium bis(trifluoromethanesulfonyl)imide (LiTFSI).
[0092] Various other components may be included or referenced to provide aspects of the teachings herein. For example, additional materials, combinations of materials, and / or omissions of materials may be used to provide additional embodiments that are within the scope of the teachings herein. Various modifications of the teachings herein may be implemented. Generally, modifications may be designed according to the needs of a user, designer, manufacturer, or other similar stakeholder. Modifications may be intended to meet particular criteria of performance deemed important by that party.
[0093] No accompanying claim or claim element should be construed as invoking 35 U.S.C. § 112(f) unless the words "means for" or "step for" are expressly used in a particular claim.
[0094] When introducing elements of the present invention or embodiments thereof, the articles "a," "an," and "the" are intended to mean that there are one or more elements. Similarly, the adjective "another," when used to introduce an element, is intended to mean that there are one or more elements. The terms "including" and "having" are intended to be inclusive so that there may be additional elements other than the listed elements. As used herein, the term "exemplary" is not intended to connote the best example. Rather, "exemplary" refers to an example embodiment that is one of many possible embodiments.
[0095] While the invention has been described with reference to exemplary embodiments, those skilled in the art will recognize that various changes can be made and equivalent elements can be substituted without departing from the scope of the invention. In addition, those skilled in the art will recognize many modifications that can be made to adapt a particular instrument, situation, or material to the teachings of the invention without departing from the essential scope of the invention. Therefore, it is not intended that the invention be limited to the particular embodiment disclosed as the best mode contemplated for carrying out this invention, but rather, the invention is intended to include all embodiments falling within the scope of the appended claims.
Claims
1. A lithium ion capacitor device, a positive electrode comprising a carbon network substantially free of binder material; a negative electrode comprising a network of carbon substantially free of binder material separated from the positive electrode by a separator; a film of lithium disposed on the negative electrode to provide prelithiation of the capacitor; At least one of the positive electrode and the negative electrode is a network of high aspect ratio carbon elements defining voids within the network; a plurality of electrode active material particles disposed in the voids within the network and entangled in the network.
2. 2. The apparatus of claim 1, wherein the high aspect ratio carbon elements include elements each having two major dimensions and one minor dimension, the ratio of the length of each of the major dimensions being at least 10 times the length of the minor dimension.
3. 10. The apparatus of any one of the preceding claims, wherein the high aspect ratio carbon elements include elements each having two major dimensions and one minor dimension, the ratio of the length of each of the major dimensions being at least 100 times the length of the minor dimension.
4. 10. The apparatus of any one of the preceding claims, wherein the high aspect ratio carbon elements include elements each having two major dimensions and one minor dimension, the ratio of the length of each of the major dimensions being at least 1,000 times the length of the minor dimension.
5. 10. The apparatus of any one of the preceding claims, wherein the high aspect ratio carbon elements include elements each having two major dimensions and one minor dimension, the ratio of the length of each of the major dimensions being at least 10,0000 times the length of the minor dimension.
6. 10. The apparatus of any one of the preceding claims, wherein the high aspect ratio carbon elements include elements each having one major dimension and two minor dimensions, the ratio of the length of each of the major dimensions being at least 10 times the length of each of the minor dimensions.
7. 10. The apparatus of any one of the preceding claims, wherein the high aspect ratio carbon elements include elements each having one major dimension and two minor dimensions, the ratio of the length of each of the major dimensions being at least 100 times the length of each of the minor dimensions.
8. 10. The apparatus of any one of the preceding claims, wherein the high aspect ratio carbon elements include elements each having one major dimension and two minor dimensions, the ratio of the length of each of the major dimensions being at least 1,000 times the length of each of the minor dimensions.
9. 10. The apparatus of any one of the preceding claims, wherein the high aspect ratio carbon elements include elements each having one major dimension and two minor dimensions, the ratio of the length of each of the major dimensions being at least 10,000 times the length of each of the minor dimensions.
10. 2. An apparatus according to any one of the preceding claims, wherein the high aspect ratio carbon elements comprise carbon nanotubes or carbon nanotube bundles.
11. 2. The apparatus of any one of the preceding claims, wherein the high aspect ratio carbon elements comprise graphene flakes.
12. 2. A device according to any one of the preceding claims, wherein the electrode active layer contains less than 10% by weight of a polymer binder disposed within the voids.
13. 2. A device according to any one of the preceding claims, wherein the electrode active layer contains less than 1 wt% of a polymer binder disposed within the voids.
14. 2. A device according to any one of the preceding claims, wherein the electrode active layer contains less than 1 wt% of a polymer binder disposed within the voids.
15. 10. A device according to any one of the preceding claims, wherein the electrode active layer is substantially free of polymeric material other than a surface treatment.
16. 10. A device according to any one of the preceding claims, wherein the electrode active layer is substantially free of polymeric material.
17. 10. A device according to any one of the preceding claims, wherein the network is at least 90% by weight carbon.
18. 10. A device according to any one of the preceding claims, wherein the network is at least 95% by weight carbon.
19. 10. A device according to any one of the preceding claims, wherein the network is at least 99% by weight carbon.
20. 10. A device according to any one of the preceding claims, wherein the network is at least 99.9% by weight carbon.