Method and system for fabricating MMIC and RF devices on engineered substrates
Patent Information
- Application Number
- JP2023522756
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-10-14
- Filing Date
- 2021-10-13
- Publication Date
- 2024-10-23
AI Technical Summary
High frequency RF and MMIC devices face challenges due to lattice mismatch and thermal expansion coefficient differences between GaN and carrier substrates, leading to defects, dislocations, and increased manufacturing costs, limiting substrate wafer size and overall cost efficiency.
The use of engineered substrates with matched thermal expansion coefficients, such as polycrystalline ceramics like aluminum nitride, encapsulated with adhesion and barrier layers, allows for the growth of high-quality GaN epitaxial layers on larger wafers, reducing defects and enabling lower-cost manufacturing through processes like LPCVD and wafer bonding.
This approach enables the fabrication of MMIC devices on larger substrates with reduced defects and thermal resistance, lowering manufacturing costs and improving performance by minimizing losses and heat generation during high-frequency operations.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical Field]
[0001] Cross-reference of related applications
[0002]
[0001] This application claims priority to U.S. Provisional Patent Application No. 63 / 091,777, filed on 14 October 2020, the disclosure of which is incorporated herein by reference for all purposes. [Background technology]
[0003]
[0002] High-frequency, high-performance radio frequency (RF) integrated devices, such as high-frequency transistors or high-electron-mobility transistors (HEMTs), can be manufactured using compound semiconductors. For example, to manufacture RF devices, an epitaxial layer, such as gallium nitride (GaN), may be formed by a heteroepitaxial (epi) growth process that involves depositing GaN on a semiconductor carrier substrate having a different lattice structure (or lattice constant) than the deposited GaN, such as silicon, silicon carbide (SiC), sapphire, or other substrates. Lattice mismatch between GaN and the carrier substrate can cause defects, dislocations, and strains that can adversely affect the yield and performance of the device. Furthermore, the GaN layer and the carrier substrate may have different coefficients of thermal expansion (CTE). Heat treatment (such as GaN epitaxial growth) can cause cracking, delamination, and bending of the GaN, and in some cases, damage to the carrier substrate. Different CTEs can limit substrate wafer size, limit scalability, and hinder the reduction of the overall manufacturing cost of RF devices and solutions.
[0004]
[0003] Monolithic microwave integrated circuit (MMIC) devices are integrated circuit devices that operate at microwave frequencies, for example, 300 MHz to 300 GHz. MMIC devices are suitable for applications such as microwave mixing, power amplification, and high-frequency switching. Despite advances in the manufacture of RF and MMIC devices, there is a technical need for improved methods and systems related to the manufacture of RF and MMIC devices. [Overview of the project]
[0005]
[0004] The present invention generally relates to a method and system for manufacturing RF and MMIC devices using a fabricated substrate. More specifically, the present invention relates to a method and system for manufacturing an MMIC device structure using a fabricated substrate. As just one example, the present invention has been applied to a method and system for manufacturing an MMIC device using a device layer coupled to an alternative fabricated substrate characterized by low loss during high-frequency operation of the MMIC device. The method and technique can be applied to a variety of semiconductor processing operations.
[0006]
[0005] According to embodiments of the present invention, a monolithic microwave integrated circuit (MMIC) system is provided. The MMIC system includes a growth substrate, a device layer bonded to the growth substrate, and a plurality of MMIC device elements bonded to the device layer. The MMIC system also includes a plurality of metallization structures bonded to the plurality of MMIC device elements, a carrier substrate bonded to the plurality of metallization structures, and a cooling structure bonded to the carrier substrate.
[0007]
[0006] According to another embodiment of the present invention, a method for manufacturing an MMIC system is provided. The method includes providing a processed substrate including a growth substrate and a device layer bonded to the growth substrate, manufacturing a plurality of MMIC device elements using the device layer, and providing a carrier substrate including a plurality of metallic structures. The method also includes bonding the plurality of metallic structures to the plurality of MMIC device elements, removing a portion of the growth substrate, and removing a portion of the carrier substrate. The method further includes forming a ground / power plane bonded to the growth substrate, forming a plurality of vias from the ground / power plane to one or more of the plurality of MMIC device elements, and bonding a cooling structure to the carrier substrate.
[0008]
[0007] According to a specific embodiment of the present invention, a monolithic microwave integrated circuit (MMIC) system is provided. The MMIC system includes a substitute fabricated substrate, a device layer coupled to the substitute fabricated substrate, a plurality of MMIC device elements coupled to the device layer, and a carrier substrate coupled to a plurality of metallization structures. The MMIC system also includes a ground / power plane coupled to the substitute fabricated substrate, a plurality of vias connecting the ground / power plane to the plurality of MMIC device elements, and a cooling structure coupled to the ground / power plane.
[0009]
[0008] According to another specific embodiment of the present invention, a method for manufacturing an MMIC system is provided. The method includes providing a processed substrate including a growth substrate and a device layer bonded to the growth substrate; manufacturing a plurality of MMIC device elements using the device layer; providing a carrier substrate; bonding the carrier substrate to the plurality of MMIC device elements; and removing the growth substrate. The method also includes bonding an alternative processed substrate to the device layer; removing a portion of the alternative processed substrate; forming a ground / power plane bonded to the alternative processed substrate; forming a plurality of vias from the ground / power plane to one or more of the plurality of MMIC device elements; and bonding a cooling structure to the ground / power plane.
[0010]
[0009] According to a particular embodiment of the present invention, a monolithic microwave integrated circuit (MMIC) system is provided. The MMIC system includes an alternative fabricated substrate, a device layer coupled to the alternative fabricated substrate, a plurality of MMIC device elements coupled to the device layer, a ground / power plane coupled to the alternative fabricated substrate, a plurality of vias connecting the ground / power plane to the plurality of MMIC device elements, and a cooling structure coupled to the ground / power plane.
[0011]
[0010] According to another specific embodiment of the present invention, a method for manufacturing an MMIC system is provided. The method includes providing a processed substrate including a growth substrate and a device layer bonded to the growth substrate, bonding a handle substrate to the device layer, and removing the growth substrate. The method also includes bonding an alternative processed substrate to the device layer, removing the handle substrate, manufacturing a plurality of MMIC device elements using the device layer, and removing a portion of the alternative processed substrate. The method further includes forming a ground / power plane bonded to the remaining portion of the alternative processed substrate, forming a plurality of vias from the ground / power plane to one or more of the plurality of MMIC device elements, and bonding a cooling structure to the ground / power plane.
[0012]
[0011] The present invention achieves more advantages than the prior art. For example, embodiments of the present invention provide a system and method for manufacturing MMIC devices that can be manufactured at a lower cost by manufacturing on a larger substrate and by simpler and faster manufacturing steps. These embodiments of the present invention, as well as other embodiments, along with many of their advantages and features, will be described in more detail below with the text and accompanying figures. [Brief explanation of the drawing]
[0013] [Figure 1] This is a simplified schematic diagram showing a processed substrate according to one embodiment of the present invention. [Figure 2]This is a simplified schematic diagram showing an alternative engineering structure according to one embodiment of the present invention. [Figure 3A] This is a cross-sectional view of an MMIC device element formed on a processed substrate according to one embodiment of the present invention. [Figure 3B] This is a cross-sectional view of a carrier substrate with metal interconnects according to one embodiment of the present invention. [Figure 3C] Figure 3A is a cross-sectional view showing the arrangement of a processed substrate having an MMIC device element, relating to a carrier substrate having a metal interconnect shown in Figure 3C according to one embodiment of the present invention. [Figure 3D] This is a cross-sectional view showing the bonding of a processed substrate equipped with an MMIC device element to a carrier substrate equipped with a metal interconnect according to one embodiment of the present invention. [Figure 3E] This is a cross-sectional view showing the removal of a portion of the processed substrate and a portion of the carrier substrate according to one embodiment of the present invention. [Figure 3F] This is a cross-sectional view showing the formation of vias in a processed substrate according to one embodiment of the present invention. [Figure 3G] This is a cross-sectional view showing the attachment of a cooling structure to a carrier substrate according to one embodiment of the present invention. [Figure 3H] This is a simplified flowchart illustrating the manufacturing method of an MMIC system according to one embodiment of the present invention. [Figure 4A] This is a cross-sectional view showing an alternative embodiment utilizing a double-sided cooling structure according to one embodiment of the present invention. [Figure 4B] This is a cross-sectional view showing a second alternative embodiment utilizing a double-sided ground / power plane and cooling structure according to one embodiment of the present invention. [Figure 5A] This is a cross-sectional view of an MMIC device element formed on the device layer of a processed substrate according to one embodiment of the present invention. [Figure 5B] This is a cross-sectional view showing the bonding of a carrier substrate to an MMIC device element according to one embodiment of the present invention. [Figure 5C] This is a cross-sectional view showing the removal of a portion of a processed substrate according to one embodiment of the present invention. [Figure 5D]A cross-sectional view showing the bonding of an alternative processing substrate to a device layer according to an embodiment of the present invention. [Figure 5E] A cross-sectional view showing the removal of a part of an alternative processing substrate according to an embodiment of the present invention. [Figure 5F] A cross-sectional view showing the formation of vias in the remaining part of an alternative processing substrate according to an embodiment of the present invention. [Figure 5G] A cross-sectional view showing the removal of a part of a carrier substrate according to an embodiment of the present invention. [Figure 5H] A cross-sectional view showing the attachment of a cooling structure to an alternative processing substrate according to an embodiment of the present invention. [Figure 5I] A simplified flowchart showing a manufacturing method of a MMIC system according to an embodiment of the present invention. [Figure 6] A cross-sectional view showing an alternative embodiment using a double-sided ground / power plane according to an embodiment of the present invention. [[ID=二十]] [Figure 7A] A cross-sectional view of a processed substrate provided with a device layer according to an embodiment of the present invention. [Figure 7B] A cross-sectional view showing the bonding of a handle substrate to a device layer according to an embodiment of the present invention. [Figure 7C] A cross-sectional view showing the removal of a growth substrate according to an embodiment of the present invention. [Figure 7D] A cross-sectional view showing the bonding of an alternative processing substrate to a device layer according to an embodiment of the present invention. [Figure 7E] A cross-sectional view showing the removal of a handle substrate according to an embodiment of the present invention. [Figure 7F] A cross-sectional view showing the formation of MMIC device elements in a device layer according to an embodiment of the present invention. [Figure 7G] A cross-sectional view showing the removal of a part of an alternative processing substrate according to an embodiment of the present invention. [Figure 7H] A cross-sectional view showing the formation of vias in the remaining part of an alternative processing substrate according to an embodiment of the present invention. [Figure 7I] A cross-sectional view showing the attachment of a cooling structure to an alternative processing substrate according to an embodiment of the present invention. [Figure 7J] This is a simplified flowchart illustrating the manufacturing method of an MMIC system according to one embodiment of the present invention. [Figure 8A] This is a cross-sectional view showing an alternative embodiment utilizing a thin carrier substrate according to one embodiment of the present invention. [Figure 8B] This is a cross-sectional view showing a second alternative embodiment utilizing a bifacial ground / power plane according to one embodiment of the present invention. [Modes for carrying out the invention]
[0014]
[0046] Discrete RF devices and MMIC devices have different design constraints and benefit from different semiconductor structures. Both discrete RF devices and MMIC devices preferably have low thermal resistance, low drain-source parasitic capacitance, high mobility, and high carrier density, which allows for the formation of a two-dimensional electron gas in the device structure, including HEMT structures. Furthermore, due to the buffer layer and trapping on the device surface, both discrete RF devices and MMIC devices preferably have low current decay and need to be suitable for the formation of through-substrate vias suitable for high-power operation. In addition to these design constraints and advantages characterizing discrete RF devices, MMIC devices preferably have a semi-insulating substrate (e.g., around 50 μm to 100 μm) with low substrate loss that can be used as a waveguide, and suitable for high-power waveguides.
[0015]
[0047] Figure 1 is a simplified schematic diagram showing a fabricated substrate 100 according to one embodiment of the present invention. The fabricated substrate 100 shown in Figure 1 is suitable for a variety of electronic and optical applications. The fabricated substrate 100 includes a core 110 which may have a CTE substantially matching that of the epitaxial material grown on the fabricated substrate 100. An epitaxial material 130, which may include GaN or a GaN-based material, is not required as an element of the fabricated substrate 100 and is therefore shown as an option, but will typically be grown on the fabricated substrate 100. In some embodiments, the fabricated substrate 100 may include one or more layers or elements deposited on or otherwise bonded to the fabricated substrate, and is therefore called a fabricated substrate structure.
[0016]
[0048] For applications involving the growth of gallium nitride (GaN)-based materials (epitaxial layers including a GaN-based layer), the core 110 is a polycrystalline ceramic material, such as polycrystalline aluminum nitride (AlN), which may contain a binder such as yttrium oxide. Other materials that can be used as the core 110 include polycrystalline gallium nitride (GaN), polycrystalline aluminum gallium nitride (AlGaN), polycrystalline silicon carbide (SiC), polycrystalline zinc oxide (ZnO), and polycrystalline gallium trioxide (Ga2O3). The thickness of the core 110 can be approximately 100 to 1500 μm, for example, 750 μm.
[0017]
[0049] The core 110 can be encapsulated in a first adhesive layer 112, which may be called a shell or encapsulation shell. In one embodiment, the first adhesive layer 112 comprises a tetraethyl orthosilicate (TEOS) oxide layer with a thickness of about 1,000 Å. In other embodiments, the thickness of the first adhesive layer 112 varies, for example, in the range of 100 Å to 2,000 Å. The TEOS oxide includes an oxide material deposited using TEOS as a precursor and can be used in the adhesive layer in some embodiments, but other materials (e.g., ceramics, especially polycrystalline ceramics) that provide adhesion between the later deposited layer and the underlying layer or material can be used by other embodiments of the present invention. For example, SiO2 or other silicon oxides (Si x O y The first adhesive layer 112 can adhere well to ceramic materials and provide a surface suitable for subsequent deposition, such as the deposition of conductive materials. In some embodiments, the first adhesive layer 112 can be formed using an LPCVD process or other suitable deposition process, which may be compatible with semiconductor processes, particularly polycrystalline or composite substrates and layers. In some embodiments, the first adhesive layer 112 can be formed on one side of the core 110. The first adhesive layer 112 provides a surface to which subsequent layers adhere to form an element of the processed substrate.
[0018]
[0050] In addition to using LPCVD processes, spin-on-glass / dielectric, and furnace-based processes for forming encapsulated adhesive layers, other semiconductor processes according to embodiments of the present invention, including CVD processes or similar deposition processes, can be utilized. For example, a deposition process can be used to coat a portion of the core. That is, the core can be flipped over, and additional portions of the core can be coated by repeating the deposition process. Therefore, while LPCVD technology is used in some embodiments to provide a fully encapsulated structure, other film formation techniques may be used depending on the specific application.
[0019]
[0051] A conductive layer 114 is formed on the first adhesive layer 112. In one embodiment, the conductive layer 114 is a shell of polysilicon (i.e., polycrystalline silicon) formed around the first adhesive layer 112. However, polysilicon may exhibit poor adhesion to ceramic materials. In embodiments where the conductive layer 114 is polysilicon, the thickness of the polysilicon layer can be on the order of 500 to 5,000 Å, for example, 2,500 Å. In some embodiments, the polysilicon layer can be formed as a shell that completely surrounds the first adhesive layer 112 (e.g., a TEOS oxide layer), thereby forming a completely encapsulated adhesive layer, and can be formed using an LPCVD process. In other embodiments, the conductive material can be formed on a part of the adhesive layer, such as on the upper half of the substrate. In some embodiments, the conductive material can be formed as a completely encapsulated layer and subsequently removed on one side of the substrate.
[0020]
[0052] In one embodiment, the conductive layer 114 can be a polysilicon layer doped to provide a highly conductive material. For example, the conductive layer 114 may be doped with boron to provide a p-type polysilicon layer. In some embodiments, doping with boron is at a level of 1×10 19 cm -3 to 1×10 20 cm -3 and provides high conductivity. Other dopants (e.g., phosphorus, arsenic, bismuth, etc.) with different dopant concentrations (e.g., in the range of 1×10 16 cm -3 to 5×10 18 cm -3 can be utilized to provide either an n-type or p-type semiconductor material suitable for use in the conductive layer. Those skilled in the art will recognize many variations, modifications, and alternative forms.
[0021]
[0053] The presence of the conductive layer 114 is useful during electrostatic chucking of the workpiece substrate to a semiconductor processing tool, such as a tool having an electrostatic chuck (ESC or electronic chuck). The conductive layer 114 allows for rapid de-chucking after processing with the semiconductor processing tool. In embodiments of the present invention, the conductive layer allows for electrical contact with the chuck or capacitive coupling to the electronic chuck during future processing, including bonding. Thus, embodiments of the present invention provide a substrate structure that can be processed in the same manner as conventional silicon wafers. Those skilled in the art will recognize many variations, modifications, and alternative forms. Furthermore, having a substrate structure with high thermal conductivity in combination with ESD chucking can provide better deposition conditions for subsequent processing layer and epitaxial layer formation, as well as for subsequent device manufacturing steps. For example, it can provide a desirable thermal profile that can result in lower stress, more uniform deposition thickness, and better stoichiometric control through subsequent layer formation.
[0022]
[0054] A second adhesive layer 116 (for example, a TEOS oxide layer with a thickness of about 1,000 Å) is formed on the conductive layer 114. In some embodiments, the second adhesive layer 116 completely surrounds and encloses the conductive layer 114, forming a fully sealed structure, and can be formed using an LPCVD process, a CVD process, or any other suitable deposition process including spin-on dielectric deposition.
[0023]
[0055] A barrier layer 118, such as a silicon nitride layer, is formed on the second adhesive layer 116. In one embodiment, the barrier layer 118 is a silicon nitride layer with a thickness of approximately 4,000 Å to 5,000 Å. In some embodiments, the barrier layer 118 completely surrounds the second adhesive layer, forming a fully encapsulated structure, and is formed using an LPCVD process. In addition to silicon nitride layers, amorphous materials including SiCN, SiON, AlN, SiC, etc., can be used as barrier layers. In some implementation configurations, the barrier layer 118 includes a number of sub-layers constructed to form the barrier layer 118. Therefore, the term barrier layer does not refer to a single layer or single material, but rather encompasses one or more materials layered in a composite manner. Those skilled in the art will recognize many variations, modifications, and alternative configurations.
[0024]
[0056] In some embodiments, a barrier layer 118, such as a silicon nitride layer, prevents elements present in the core, such as yttrium (element), yttrium oxide (i.e., yttria), oxygen, metallic impurities, and other trace elements, from diffusing and / or releasing gases into the semiconductor processing chamber environment where the processed substrate may be present, for example, during high-temperature (e.g., 1,000°C) epitaxial growth processes. Using the encapsulation layers described herein, ceramic materials containing polycrystalline AlN designed for non-cleanroom environments can be utilized in semiconductor process flows and cleanroom environments.
[0025]
[0057] In some embodiments, the ceramic material used to form the core may be fired at temperatures in the range of 1,800°C. This process is expected to remove a considerable amount of impurities present in the ceramic material. These impurities may include yttrium, calcium, and other elements and compounds resulting from the use of yttria as a sintering agent. Subsequently, during the epitaxial growth process, which may be carried out at much lower temperatures in the range of 800°C to 1,100°C, it would be expected that the subsequent diffusion of these impurities would not be significant. However, contrary to conventional expectations, significant diffusion of elements through the layers of the processed substrate may occur even during the epitaxial growth process at temperatures much lower than the firing temperature of the ceramic material. Therefore, embodiments of the present invention build up a barrier layer on the processed substrate to prevent this undesirable diffusion.
[0026]
[0058] Accordingly, some embodiments of the present invention integrate a silicon nitride layer as a barrier layer 118 to prevent the diffusion of background elements from a polycrystalline ceramic material (e.g., AlN) into a workpiece layer and epitaxial layer, such as an arbitrary GaN layer 130. The barrier layer 118, which encapsulates the underlying layers and material, provides the desired barrier layer functionality. Integration of the barrier layer 118 into the workpiece substrate prevents the diffusion of calcium, yttrium, and aluminum into the workpiece layer during the annealing process, which would typically occur if the barrier layer were not present. Thus, the use of the barrier layer 118 prevents these elements from diffusing through the barrier layer, thereby preventing the release of elements into the environment surrounding the workpiece substrate. Similarly, other impurities contained within the bulk ceramic material will be contained by the barrier layer.
[0027]
[0059] The bonding layer 120 (e.g., a silicon oxide layer) may be deposited on a portion of the barrier layer 118, for example, on the upper surface of the barrier layer 118, and subsequently used during bonding of a substantial single-crystal layer 122 (e.g., a single-crystal silicon layer such as a delamination silicon (111) layer). In some embodiments, the bonding layer 120 may have a thickness of approximately 1.5 μm. In some embodiments, the thickness of the bonding layer 120 is 20 nm or more for bonding-induced void relaxation. In some embodiments, the thickness of the bonding layer 120 is in the range of 0.75 to 1.5 μm.
[0028]
[0060] The bonding layer 120 can be formed by depositing a thick oxide layer (e.g., 2-5 μm thick) and then thinning the oxide to a thickness of approximately 1.5 μm or less using a chemical mechanical polishing (CMP) process. The thick initial oxide remains present to smooth any surface features that may remain on the support structure after the fabrication of the polycrystalline core, and to form the encapsulation layer shown in Figure 1. The CMP process provides a substantially flat surface free of voids, which can then be used during the wafer transfer process to bond the single-crystal silicon layer 122 to the bonding layer 120.
[0029]
[0061] The substantially single-crystal layer 122 (e.g., exfoliated Si(111)) is suitable for use as a growth layer during the epitaxial growth process for forming an epitaxial material. In some embodiments, the epitaxial material may include a GaN layer with a thickness of 2 μm to 10 μm, which can be used as one of several layers utilized in optoelectronics, RF, and power devices. In one embodiment, the substantially single-crystal layer 122 includes a single-crystal silicon layer attached to the junction layer using a layer transfer process.
[0030]
[0062] The layer transfer process may be carried out using a silicon wafer. The silicon wafer may be implanted with several elements to form a damaged interface within the Si, which can help form a single crystal layer 122 for adhesion to the bonding layer 120. For example, pressure may be applied to the silicon wafers bonded to each other and to the bonding layer 120, thereby atomically bonding the silicon wafer to the bonding layer 120.
[0031]
[0063] After the bonding process, the delamination process may activate the damaged interface inside the silicon wafer, causing the elements injected into the single crystal layer 122 to expand, and thus the upper part of the silicon wafer may be separated from the ceramic wafer 110 by the processed layer. The remaining single crystal layer 122 bonded to the bonding layer 120 may be relatively thin, such as about 5 microns or less, and therefore may not contribute significantly to the CTE of the processed substrate 100. Thus, the CTE of the processed substrate 100 is mainly determined by the CTE of the ceramic core 110.
[0032]
[0064] Materials other than silicon can be used to create single-crystal thin-film junction layers. These single-crystal materials may include SiC, GaN, AlGaN, AlN, ZnO, and sapphire.
[0033]
[0065] The GaN epitaxial layer 130 (which may also be referred to as the epitaxial layer) can be formed by epitaxially growing a number of layers or sublayers to form an epitaxial structure on the processed substrate 110. As will be more fully described herein, the GaN epitaxial layer 130 is an example of a device layer epitaxially grown on a substrate. As will be apparent to those skilled in the art, the manufacture of MMICs and RF devices and epitaxial structures suitable for MMICs and RF devices do not necessarily consist of a single epitaxial layer, but may include a number of layers with different compositions, thicknesses, doping densities, etc. Therefore, as used herein, the terms “layer” and “device layer” should be understood to include structures comprising multiple layers or sublayers of the same or different materials. In some embodiments, the buffer layer may be formed on the junction layer 120, and the GaN epitaxial layer 130 (epitaxial layer) may be formed on the buffer layer. The CTEs of the ceramic wafer 110 and the GaN epitaxial layer 130 may be substantially matched over a wide temperature range (e.g., about 25°C to about 1200°C), such as within about 0.1%, 0.5%, 1%, 2%, 5%, or 10% of each other. This CTE matching allows for the formation of a high-quality epitaxial layer on a larger ceramic wafer 110 without cracking or warping. For example, the GaN epitaxial layer 130 may be formed on a 6-inch, 8-inch, 12-inch, or larger processed substrate 100. Using larger wafers can potentially increase the number of devices per wafer, making GaN devices less expensive.
[0034]
[0066] This CTE matching can enable the formation of a significantly thick GaN epitaxial layer 130 (e.g., tens or hundreds of microns) on the fabricated substrate 110. The bonded epitaxial layer can reduce the overall dislocation density of the lattice structure between the GaN epitaxial layer 130 and the single crystal layer 122. Furthermore, using more epitaxial layers allows for the fabrication of more complex circuits for a wider range of GaN device arrays.
[0035]
[0067] Additional information relating to processed substrates is provided in U.S. Patent No. 10,297,445 issued on 21 May 2019 and U.S. Patent No. 10,134,589 issued on 20 November 2018, and that disclosure is incorporated herein by reference for all purposes.
[0036]
[0068] Figure 2 is a simplified schematic diagram showing an alternative processed substrate according to one embodiment of the present invention. The alternative processed substrate 200 shown in Figure 2 shares some common elements with the processed substrate 100 shown in Figure 1, and the explanation provided in relation to Figure 1 is applicable to Figure 2 as appropriate. Referring to Figure 2, the alternative processed substrate 200 includes a core 110, for example, polycrystalline AlN, which may have a coefficient of thermal expansion (CTE) substantially matching that of the epitaxial material grown on the alternative processed substrate 200. In addition to polycrystalline AlN, other materials used to form the core 110 can be used as discussed in relation to Figure 1. The thickness of the core 110 can be about 100 to 1500 μm, for example, 750 μm.
[0037]
[0069] The core 110 may be encapsulated in an adhesive layer 212, which may be called a shell or encapsulation shell. The adhesive layer 212 may include a tetraethyl orthosilicate (TEOS) oxide layer with a thickness of about 1,000 Å, as discussed in relation to Figure 1. While TEOS oxide can be used for the adhesive layer in some embodiments, other materials that provide adhesion between the later deposited layer and the underlying layer or material (e.g., ceramics, particularly polycrystalline ceramics) are used in other embodiments of the present invention. In the illustrated embodiment, the adhesive layer 212 completely surrounds the core 110, forming a fully encapsulated core, and may be formed using an LPCVD process or other suitable deposition process.
[0038]
[0070] The barrier layer 214, for example, a silicon nitride layer, is formed on top of the adhesive layer 212. In one embodiment, the barrier layer 214 is a silicon nitride layer with a thickness of approximately 4,000 Å to 5,000 Å, as discussed in relation to Figure 1. In the embodiment shown in Figure 2, the barrier layer 214 forms a structure that completely surrounds and encapsulates the adhesive layer 212 and can be formed using an LPCVD process. In addition to silicon nitride layers, amorphous materials including SiCN, SiON, AlN, SiC, etc., can be used as barrier layers. In some implementation configurations, the barrier layer 214 includes a number of sublayers constructed to form the barrier layer 214. Therefore, the term barrier layer does not refer to a single layer or single material, but rather encompasses one or more materials layered in a complex manner. Those skilled in the art will recognize many variations, modifications, and alternative configurations.
[0039]
[0071] As discussed in relation to Figure 1, for example, during high-temperature (e.g., 1,000°C) epitaxial growth processes, the barrier layer 214 prevents elements present in the core 110, such as yttrium (element), yttrium oxide (i.e., yttria), oxygen, metallic impurities, and other trace elements, from diffusing into the semiconductor processing chamber environment where alternative processing substrates 200 may be present and / or releasing gases. Thus, using a barrier layer 214 as described herein, ceramic materials containing polycrystalline AlN designed for non-cleanroom environments can be used in semiconductor process flows and cleanroom environments.
[0040]
[0072] Figure 3A is a cross-sectional view of an MMIC device element formed on a processed substrate according to one embodiment of the present invention. In Figure 3A, the processed substrate 310 includes a growth substrate 305 and a device layer 307, which in the illustrated embodiment is represented by a GaN layer. The growth substrate 305 and the device layer 307 can be mounted using a processed substrate 100 having a device layer 307 corresponding to a GaN epitaxial layer 130, as shown in Figure 1. The device layer 307 is used to manufacture MMIC device elements 320a, 320b, and 320c. Each of the MMIC device elements 320 represents a different MMIC device; for example, MMIC device element 320a may be a capacitor, MMIC device element 320b may be a transistor, and MMIC device element 320b may be a waveguide. Each of the different MMIC device elements 320 includes a metallic structure 322. In Figure 3A, the device layer 307 is a GaN layer, which can have a thickness of approximately 1 to 10 μm and is used to reduce losses and capacitance.
[0041]
[0073] Therefore, the MMIC device element 320 represents a device fabricated in the device layer 307. It will be apparent to those skilled in the art that the term “fabricated in the device layer” does not mean that all device elements are fabricated using the original semiconductor material that constitutes the device layer, and that other materials may be deposited on the device layer during the fabrication process, including ion implantation, diffusion doping, patterning and etching, and deposition of insulators and metals for contacts. Therefore, the MMIC device element 320 shown in Figure 3A is intended to represent a set of different device elements that can be used individually or in combination to form electronic components. Consequently, the discussion provided herein uses language indicating that devices are fabricated in the device layer, but it is understood that the device layer provides a starting point for device fabrication. This may include the removal of portions of the device layer and the addition of other appropriate materials to a particular device element. Those skilled in the art will recognize many variations, alterations, and alternative forms.
[0042]
[0074] Figure 3B is a cross-sectional view of a carrier substrate with metal interconnects according to one embodiment of the present invention. In Figure 3B, the carrier substrate 330 has a plurality of metal interconnects 332 corresponding to the metal structures 322a, 322b, and 322c shown in Figure 3A. In the processing stage shown in Figure 3B, the carrier substrate 330 is inverted to orient the metal interconnects 332 for subsequent bonding operations.
[0043]
[0075] Figure 3C is a cross-sectional view showing the arrangement of a processed substrate having the MMIC device element shown in Figure 3A, relating to a carrier substrate having the metal interconnects shown in Figure 3C according to one embodiment of the present invention. As shown in Figure 3C, the processed substrate 310 having the MMIC device element 320 is arranged adjacent to a carrier substrate 330 having metal interconnects 332 that face each other. An alignment process is used to align the metal interconnects 332a, 332b, and 332c with the metal structures 322a, 322b, and 322c.
[0044]
[0076] Figure 3D is a cross-sectional view showing the bonding of a fabricated substrate equipped with an MMIC device element to a carrier substrate having metal interconnects according to one embodiment of the present invention. As shown in Figure 3D, after the bonding process is completed, the metal interconnects 332a, 332b, and 332c are bonded to the corresponding metal structures 322a, 322b, and 322c. The intermetallic bonding shown in Figure 3D provides a mechanically strong bond with high conductivity.
[0045]
[0077] Figure 3E is a cross-sectional view showing the removal of a portion of the processed substrate, namely a portion of the growth substrate 305 and a portion of the carrier substrate 330, according to one embodiment of the present invention. In order to reduce thermal resistance, the growth substrate 305 and the carrier substrate 330 are thinned to a thickness of approximately 50 μm, for example.
[0046]
[0078] The substrate thinning process shown in Figure 3E can be carried out in several ways. For example, a mechanical grinding process can be used to remove most of the carrier substrate 330. Next, chemical etching, which may be selective etching, can be used to remove the material and expose the desired layer. For example, chemical etching may utilize potassium hydroxide (KOH) or tetramethylammonium hydroxide (TMAH) during the etching process. Finally, physical etching, such as a reactive ion etching (RIE) process, can be used to smooth and prepare the surface for subsequent metallization and other processes.
[0047]
[0079] Figure 3F is a cross-sectional view illustrating the formation of vias in a processed substrate according to one embodiment of the present invention. In Figure 3F, vias 340 and 342 are formed through the remainder of the processed substrate 310 so as to be in electrical contact with MMIC device elements 320b and 320c, respectively. A ground / power plane 344 is formed and electrically connected to vias 340 and 342. Depending on the specific application, the ground / power plane 344 is useful for providing a connection to ground or for supplying power from a power source. Vias 340 and 342 can be manufactured using appropriate semiconductor processing techniques, including etching, laser ablation, etc. In some embodiments, once the MMIC device elements 320b and 320c are connected, the methods can be combined to terminate the via formation process.
[0048]
[0080] Although only two vias, via 340 and via 342, are shown in Figure 3F, there are no vias formed on the MMIC device element 320a, and these are not required by the present invention. In other embodiments, vias can be formed on all MMIC device elements, or vias can be formed on a smaller subset of MMIC device elements. For example, if the MMIC device element 320a is a capacitor, vias may be omitted.
[0049]
[0081] Although via formation is illustrated after the bond between the processed substrate 310 and the carrier substrate 330, it should be noted that this is not required in the present invention and other embodiments. That is, via formation can be performed after device manufacturing, as illustrated in Figure 3A. Those skilled in the art will recognize many variations, modifications, and alternative forms.
[0050]
[0082] Figure 3G is a cross-sectional view showing the attachment of a cooling structure to a carrier substrate according to one embodiment of the present invention. The cooling structure 350 can be used to provide one-sided cooling in a manner that isolates the ground / power plane 344 from the cooling structure 350. During device operation, heat generated by the MMIC device element 320 can be conducted to the cooling structure 350 through the metal structure 322 and the carrier substrate 330.
[0051]
[0083] Figure 3H is a simplified flowchart illustrating a method for manufacturing an MMIC system according to one embodiment of the present invention. Method 370 includes providing a processed substrate comprising a growth substrate and a device layer bonded to the growth substrate (371), and manufacturing a plurality of MMIC device elements using the device layer (372). The coefficient of thermal expansion (CTE) of the growth substrate substantially matches that of the device layer. The growth substrate may include a polycrystalline ceramic core, such as aluminum nitride. The thickness of the device layer can be 1 to 10 μm, and the device layer may include GaN and GaN-based materials.
[0052]
[0084] The method also includes providing a carrier substrate containing multiple metal structures (374), bonding the multiple metal structures to multiple MMIC device elements (376), removing a portion of the growth substrate, and removing a portion of the carrier substrate (378).
[0053]
[0085] The method further includes forming a ground / power plane coupled to a growth substrate (380), forming a plurality of vias from the ground / power plane to one or more of a plurality of MMIC device elements (382), and bonding a cooling structure to a carrier substrate (384). In some embodiments, the method further includes bonding a second cooling structure to the ground / power plane. In some mounting configurations, before bonding the cooling structure to the carrier substrate, the method includes forming a second ground / power plane coupled to the carrier substrate, and forming a second plurality of vias from the second ground / power plane to one or more of a plurality of metal structures. The method may include bonding a second cooling structure to the ground / power plane.
[0054]
[0086] It should be understood that the specific steps shown in Figure 3H provide a specific method for manufacturing an MMIC system according to one embodiment of the present invention. Other sequences of steps may also be performed by alternative embodiments. For example, alternative embodiments of the present invention may perform the steps outlined above in a different order. Furthermore, the individual steps shown in Figure 3H may include multiple substeps that can be performed in various orders as appropriate. In addition, additional steps may be added and some steps removed depending on the specific application. Those skilled in the art will recognize many variations, modifications, and alternative forms.
[0055]
[0087] Figure 4A is a cross-sectional view showing an alternative embodiment utilizing a double-sided cooling structure according to one embodiment of the present invention. In the alternative embodiment shown in Figure 4A, the second cooling structure 360 is attached to the ground / power plane 344, providing double-sided cooling and a higher level of thermal performance.
[0056]
[0088] Figure 4B is a cross-sectional view showing a second alternative embodiment utilizing a bifacial ground / power plane and cooling structure according to one embodiment of the present invention. In the second alternative embodiment shown in Figure 4B, additional vias 362 and 364 are formed that pass through the remainder of the carrier substrate 330 and are electrically connected to the ground / power plane 366 before the cooling structure 368 is mounted. Subsequently, the cooling structure 368 is mounted to the ground / power plane 366. In this implementation, the bifacial electrical planes, i.e., the ground / power plane 344 and the ground / power plane 366, effectively provide a three-layer circuit structure, enabling reduced routing complexity, reduced device area, and the like. Furthermore, bifacial cooling is appropriately provided to specific MMIC devices included in the device. Those skilled in the art will recognize many variations, modifications, and alternative forms.
[0057]
[0089] Figure 5A is a cross-sectional view of an MMIC device element formed on a device layer of a processed substrate according to one embodiment of the present invention. In a similar manner to the MMIC device element shown in Figure 3A, the processed substrate 510 includes a growth substrate 505 and a device layer 507, which in the illustrated embodiment is represented by a GaN layer. The growth substrate 505 and the device layer 507 can be mounted using a processed substrate 100 having a device layer 507 corresponding to a GaN epitaxial layer 130, as shown in Figure 1. Although the device layer 507 is shown as a single layer, this is not essential in the present invention, and it should be understood that the device layer 507 can include multiple layers with different compositions, different doping densities, different thicknesses, etc. Thus, various epitaxial structures suitable for use in the manufacture of MMIC device elements can be represented by the device layer 507. As mentioned above, the CTE match between the core 110 of the processed substrate 100 and the epitaxial material constituting the device layer 507 enables high-quality growth not provided by the prior art.
[0058]
[0090] The device layer 507 is used in the fabrication of MMIC device elements 520a, 520b, and 520c. Each of the MMIC device elements 520 represents a different MMIC device; for example, MMIC device element 520a can be a capacitor, MMIC device element 520b can be a transistor, and MMIC device element 520b can be a waveguide. Each of the different MMIC device elements 520 includes a metallic structure 522. In Figure 5A, the device layer 507 is a GaN layer with a thickness of approximately 1 to 10 μm and is used to reduce losses and capacitance, improve the characteristics of the two-dimensional electron gas (2DEG) formed in some MMIC device structures, and reduce electron trapping.
[0059]
[0091] Therefore, the MMIC device element 520 represents a device fabricated in the device layer 507. It will be apparent to those skilled in the art that the term “fabricated in the device layer” does not mean that all device elements are fabricated using the original semiconductor material that constitutes the device layer, and that other materials may be deposited on the device layer during the fabrication process, including ion implantation, diffusion doping, patterning and etching, and deposition of insulators and metals for contacts. Therefore, the MMIC device element 520 shown in Figure 5A is intended to represent a set of different device elements that can be used individually or in combination to form electronic components. Consequently, the discussion provided herein uses language indicating that devices are fabricated in the device layer, but it will be understood that the device layer provides a starting point for device fabrication. This may include the removal of portions of the device layer and the addition of other appropriate materials to specific device elements. Those skilled in the art will recognize many variations, alterations, and alternative forms.
[0060]
[0092] Figure 5B is a cross-sectional view showing the bonding of a carrier substrate to an MMIC device element according to one embodiment of the present invention. As shown in Figure 5B, a bonding process is used to bond the carrier substrate 530 to the metal structures 522a, 522b, and 522c. In some embodiments, the carrier substrate 530 is mounted as an alternative processed substrate 200 shown in Figure 2. Using a carrier substrate 530 similar to the alternative processed substrate 200 provides a core for the carrier substrate, such as polycrystalline AlN, and has a CTE that substantially matches the epitaxial material present in other elements in the MMIC device structure, which can be beneficial during semiconductor processing operations. The use of adhesives and barrier layers, as discussed in relation to Figure 2, enables the barrier layer, which prevents background elements present in the polycrystalline ceramic core from diffusing into the environment surrounding the processed substrate.
[0061]
[0093] In some embodiments, the carrier substrate 530 is bonded to the metal structures 522a, 522b, and 522c by wafer bonding techniques including intermetallic bonding by providing matching metal patterns on the carrier substrate, or by interoxide bonding by coating both wafers with, for example, SiO2. In some embodiments, the bonding surface of the carrier substrate 530 can be coated with an adhesion promoter to enhance the bonding strength. As an example, a metal layer (not shown) can be deposited on the carrier substrate 530 to perform intermetallic bonding and used during bonding to the metal structures 522a, 522b, and 522c.
[0062]
[0094] Figure 5C is a cross-sectional view showing the removal of a portion of a processed substrate according to one embodiment of the present invention. Various techniques can be used to remove the growth substrate 505 while leaving the device layer 507 bonded to the carrier substrate 530. For example, a chemical mechanical polishing (CMP) process may be used to remove the growth substrate 505, terminating at or within the device layer 507. In other embodiments, a CMP process is used to remove a portion of the growth substrate 505, and then a chemical and / or physical etching process is used to remove the remainder of the growth substrate 505. Alternatively, a portion or all of the growth substrate 505 can be removed using chemical etching, which may be selective etching. Chemical etching may be selective to terminate at the layer of interest, for example, the device layer 507. Finally, a physical etching process, such as reactive ion etching (RIE), can be used to remove a portion or all of the growth substrate 505 and / or smooth and prepare the device layer 507 for subsequent bonding and processing steps.
[0063]
[0095] The removal of the processed substrate can be carried out in several ways. For example, a mechanical grinding process can be used to remove most of the processed substrate. Next, chemical etching, which may be selective etching, can be used to remove the material and expose the desired layer. Finally, physical etching, such as reactive ion etching (RIE) process, can be used to remove the interface layer.
[0064]
[0096] Removing the growth substrate 505 allows for the removal of structures that could otherwise result in losses during the operation of the MMIC device. As an example, the processed substrate 100 shown in Figure 1 includes a conductive layer 114, which can be a polysilicon layer doped to provide a highly conductive material. During high-frequency operation, the electric and / or magnetic fields generated by the MMIC device may interact with such conductive layers, potentially resulting in losses, heat generation, and other undesirable effects. Therefore, by removing the growth substrate 505 and the layers / structures within the growth substrate 505 that could adversely affect the performance of the MMIC device, embodiments of the present invention provide methods and systems with lower losses than comparable conventional devices and structures.
[0065]
[0097] As an example, the device layer 507 may include a buffer layer and other layers utilized during initial epitaxial growth, for example, during the epitaxial growth of GaN material. These layers, including the buffer layer, may impair the performance of the MMIC device in a similar manner to conductive layers, for example, by causing losses. Therefore, as illustrated in Figure 5C, these layers can be removed along with the growth substrate 505. Those skilled in the art will recognize many variations, alterations, and alternative configurations.
[0066]
[0098] Figure 5D is a cross-sectional view showing the bonding of an alternative fabricated substrate to a device layer according to one embodiment of the present invention. In some embodiments, the alternative fabricated substrate 540 is implemented as the alternative fabricated substrate 200 shown in Figure 2. The use of an alternative fabricated substrate 540 similar to the alternative fabricated substrate 200 provides a core for an alternative fabricated substrate, such as polycrystalline AlN, which may have a CTE substantially matching the epitaxial material present in other elements in the MMIC device structure, which may be beneficial during semiconductor processing operations. Furthermore, as discussed in relation to the removal of the growth substrate 505, the alternative fabricated substrate 540 can be manufactured using a material suitable for low-loss, high-frequency operation. As an example, the alternative fabricated substrate 540 may be substantially silicon-free, which may adversely affect the performance of the MMIC device.
[0067]
[0099] In some embodiments, the alternative processed substrate 540 is bonded to the device layer 507 using wafer bonding techniques including intermetallic bonding by providing a matching metal pattern on a carrier substrate, or by interoxide bonding by coating both wafers with, for example, SiO2. In some embodiments, the bonding surface of the alternative processed substrate 540 can be coated with an adhesion promoter to enhance bonding strength.
[0068]
[0100] Figure 5E is a cross-sectional view showing the removal of a portion of the alternative processed substrate according to one embodiment of the present invention. As discussed in relation to Figure 3E, in order to reduce thermal resistance, the alternative processed substrate 540 is thinned to a thickness of, for example, about 50 μm.
[0069]
[0101] The substrate thinning process shown in Figure 5E can be carried out in several ways. For example, a mechanical grinding process can be used to remove a portion of the alternative processed substrate 540. Then, the illustrated portion of the alternative processed substrate 540 can be removed using chemical etching, which can be selective etching. For example, the chemical etching may utilize potassium hydroxide (KOH) or tetramethylammonium hydroxide (TMAH) during the etching process. Finally, in addition to, or in combination with, the chemical grinding process and / or chemical etching, a physical etching process, such as reactive ion etching (RIE), can be used to remove the illustrated portion of the alternative processed substrate 540. The physical etching process can then be used to smooth and prepare the surface for subsequent metallization or other processes.
[0070]
[0102] Figure 5F is a cross-sectional view showing via formation in the remaining portion of a replacement substrate according to one embodiment of the present invention. In Figure 5F, vias 542 and 544 are formed through the remaining portion of the replacement substrate 540 to make electrical contact with MMIC device elements 520b and 520c, respectively. A ground / power plane 546 is formed and electrically connected to vias 542 and 544. Vias 542 and 544 are manufactured using appropriate semiconductor processing techniques, including etching, laser ablation, etc. In some embodiments, once MMIC device elements 520b and 520c are connected, the via formation process can be terminated by combining methods.
[0071]
[0103] Only two vias, via 542 and via 544, are shown in Figure 5F, and there are no vias formed on the MMIC device element 520a, which are not required by the present invention. In other embodiments, vias can be formed on all MMIC device elements, or vias can be formed on a smaller subset of MMIC device elements. For example, if the MMIC device element 520a is a capacitor, vias may not be provided.
[0072]
[0104] As shown in Figure 5E, via formation is shown after the alternative processed substrate 540 has been thinned, but it should be noted that this is not required by the present invention, and in other embodiments, via formation can be performed before substrate thinning. Those skilled in the art will recognize many variations, modifications, and alternative forms.
[0073]
[0105] Figure 5G is a cross-sectional view showing the removal of a portion of the carrier substrate according to one embodiment of the present invention. As discussed in relation to Figure 5E and the alternative processed substrate 540, the carrier substrate 530 can be thinned to, for example, about 50 μm in thickness. The thinning process discussed in relation to Figures 3E and 5E can be used as appropriate.
[0074]
[0106] Figure 5H is a cross-sectional view showing the attachment of a cooling structure to an alternative fabricated substrate according to one embodiment of the present invention. The cooling structure 550 can be used to provide one-sided cooling in a manner that isolates the ground / power plane 546 from the cooling structure 550. During device operation, heat generated by the MMIC device element 520 may be conducted to the cooling structure 550 through the device layer 507, the rest of the alternative fabricated substrate 540, and the ground / power plane 546.
[0075]
[0107] Figure 5I is a simplified flowchart illustrating a method for manufacturing an MMIC system according to one embodiment of the present invention. Method 560 includes providing a processed substrate including a growth substrate and a device layer bonded to the growth substrate (570), and manufacturing a plurality of MMIC device elements using the device layer (572). The method also includes providing a carrier substrate (574) and bonding the carrier substrate to a plurality of MMIC device elements (576). The coefficient of thermal expansion (CTE) of the alternative processed substrate substantially matches that of the device layer. The alternative processed substrate may include a polycrystalline ceramic core, such as aluminum nitride. The thickness of the device layer may be greater than 1 μm, for example, 1 μm to 10 μm.
[0076]
[0108] The method further includes removing the growth substrate (578), bonding a replacement processed substrate to the device layer, and removing a portion of the replacement processed substrate (580). The method further includes forming a ground / power plane coupled to the replacement processed substrate, and forming a plurality of vias from the ground / power plane to one or more of the plurality of MMIC device elements (582). The method also includes bonding a cooling structure to the ground / power plane (584). In some embodiments, the method may also include removing at least a portion of the carrier substrate. Furthermore, in some packaging configurations, the method includes forming a second ground / power plane coupled to the remaining portion of the carrier substrate, and forming a second plurality of vias from the second ground / power plane to one or more of the plurality of MMIC device elements.
[0077]
[0109] It should be understood that the specific steps shown in Figure 5I provide a specific method for manufacturing an MMIC system according to one embodiment of the present invention. Other sequences of steps may also be performed by alternative embodiments. For example, alternative embodiments of the present invention may perform the steps outlined above in a different order. Furthermore, the individual steps shown in Figure 5I may include multiple substeps that can be performed in various orders as appropriate. In addition, additional steps may be added and some steps may be omitted depending on the particular application. Those skilled in the art will recognize many variations, modifications, and alternative forms.
[0078]
[0110] Figure 6 is a cross-sectional view showing an alternative embodiment utilizing a double-sided ground / power plane according to one embodiment of the present invention. In Figure 6, vias 640 and 642 are formed through the remainder of the carrier substrate 530 and electrically contact the MMIC device elements 520b and 520c, respectively. A ground / power plane 644 is formed and electrically connected to vias 640 and 642. Vias 640 and 642 can be manufactured using appropriate semiconductor processing techniques, including etching, laser ablation, etc. In some embodiments, once the MMIC device elements 520b and 520c are connected, the via formation process can be terminated by combining methods. The ground / power plane 650 and cooling structure 652 are utilized as discussed in relation to Figure 5H.
[0079]
[0111] Although only two vias, via 640 and via 642, are shown in Figure 6, there are no vias formed on the MMIC device element 520a, and these are not required by the present invention. In other embodiments, vias can be formed on all MMIC device elements, or vias can be formed on a smaller subset of MMIC device elements. For example, if the MMIC device element 520a is a capacitor, vias may be omitted.
[0080]
[0112] Figure 7A is a cross-sectional view of a processed substrate with a device layer according to one embodiment of the present invention. In Figure 7A, the processed substrate 710 includes a growth substrate 705 and a device layer 707, which in the illustrated embodiment is represented by a GaN layer. The growth substrate 705 and the device layer 707 can be mounted using a processed substrate 100 having a device layer 707 corresponding to a GaN epitaxial layer 130, as shown in Figure 1. The device layer 707 is used to manufacture an MMIC device element, as will be described in more detail below.
[0081]
[0113] Figure 7B is a cross-sectional view showing the bonding of a handle substrate to a device layer according to one embodiment of the present invention. In some embodiments, the handle substrate 750 is mounted as a silicon substrate, a sapphire substrate, and the like. The handle substrate 750 is characterized by its mechanical rigidity and the ability to be removed in later stages of manufacturing. In contrast to some of the other substrates discussed and utilized in the embodiments described herein, the handle substrate 750 is removed before the final processing step. Therefore, useful properties discussed with respect to other substrates, such as compatibility with CTE matching and low loss, and high-frequency operation, are not required for the handle substrate 750.
[0082]
[0114] In some embodiments, the handle substrate 750 is bonded to the device layer 707 using wafer bonding techniques including intermetallic bonding by providing a matching metal pattern on the handle substrate, or by interoxide bonding by coating both wafers with, for example, SiO2. In some embodiments, the bonding surface of the handle substrate 750 can be coated with an adhesion promoter to enhance the bonding strength.
[0083]
[0115] Figure 7C is a cross-sectional view showing the removal of the growth substrate according to one embodiment of the present invention. As shown in Figure 7C, the growth substrate 705 is removed to expose the device layer 707.
[0084]
[0116] Various techniques can be used to remove the growth substrate 705 while leaving the device layer 507 bonded to the handle substrate 750. For example, a chemical mechanical polishing (CMP) process may be used to remove the growth substrate 705, terminating at or within the device layer 707. In other embodiments, a CMP process may be used to remove a portion of the growth substrate 705, and then a chemical and / or physical etching process may be used to remove the remainder of the growth substrate 705. Alternatively, a portion or all of the growth substrate 705 can be removed using chemical etching, which may be selective etching. The chemical etching may be selective to terminate at the desired layer, e.g., the device layer 707. Finally, a physical etching process, such as reactive ion etching (RIE), may be used to remove a portion or all of the growth substrate 705 and / or smooth and prepare the device layer 707 for subsequent bonding and processing steps.
[0085]
[0117] Removing the growth substrate 705 allows for the removal of structures that may result in losses during the operation of the MMIC device subsequently fabricated in the device layer 707. As an example, the fabricated substrate 100 illustrated in Figure 1 includes a conductive layer 114, which may be a polysilicon layer doped to provide a highly conductive material. During high-frequency operation, electric and / or magnetic fields generated by the MMIC device may interact with such conductive layers, potentially resulting in losses, heat generation, and other undesirable effects. Therefore, by removing the growth substrate 705 and the layers / structures within the growth substrate 705 that may adversely affect the performance of the MMIC device, embodiments of the present invention provide methods and systems with lower losses than comparable conventional devices and structures.
[0086]
[0118] As an example, the device layer 707 may include a buffer layer and other layers utilized during initial epitaxial growth, such as the epitaxial growth of a GaN material. These layers, including the buffer layer, can impair the performance of the MMIC device in a similar manner to conductive layers, for example, by causing losses. Therefore, as shown in Figure 7C, these layers can be removed along with the growth substrate 705. Those skilled in the art will recognize many variations, alterations, and alternative configurations.
[0087]
[0119] Figure 7D is a cross-sectional view showing the bonding of an alternative fabricated substrate to a device layer according to one embodiment of the present invention. In some embodiments, the alternative fabricated substrate 760 is mounted as the alternative fabricated substrate 200 shown in Figure 2. The use of an alternative fabricated substrate 760 similar to the alternative fabricated substrate 200 provides a core for an alternative fabricated substrate, such as polycrystalline AlN, which may have a CTE substantially matching the epitaxial material present in other elements within the MMIC device structure, which may be beneficial during semiconductor processing operations. Furthermore, as discussed in relation to the removal of the growth substrate 705, the alternative fabricated substrate 760 may be manufactured using a material suitable for low-loss, high-frequency operation. As an example, the alternative fabricated substrate 760 may be substantially silicon-free, which may adversely affect the performance of the MMIC device.
[0088]
[0120] As an example, comparing an alternative processed substrate 760 bonded to the device layer 707 with a silicon substrate having an epitaxially grown GaN layer on a silicon substrate, an MMIC device fabricated with the device layer 707 bonded to the alternative processed substrate 760 would be characterized by low losses due to the properties of the alternative processed substrate 760. In contrast, if the alternative processed substrate 760 is replaced with a silicon substrate, an MMIC device fabricated with the device layer 707 would be characterized by higher losses resulting from the interaction between the electric and magnetic fields and the silicon substrate, which may include interface losses.
[0089]
[0121] In some embodiments, the alternative processed substrate 760 is bonded to the device layer 707 using wafer bonding techniques including intermetallic bonding by providing a matching metal pattern on the alternative processed substrate, or by interoxide bonding by coating both wafers with, for example, SiO2. In some embodiments, the bonding surface of the alternative processed substrate 760 can be coated with an adhesion promoter to enhance the bonding strength.
[0090]
[0122] Figure 7E is a cross-sectional view showing the removal of the handle substrate according to one embodiment of the present invention. Subsequently, the handle substrate 750 is removed as shown in Figure 7E to expose the device layer 707 used in the MMIC device manufacturing process.
[0091]
[0123] Various techniques can be used to remove the handle substrate 750 while leaving the device layer 707 bonded to the alternative processing substrate 760. For example, a chemical mechanical polishing (CMP) process may be used to remove the handle substrate 750, terminating at or within the device layer 707. In other embodiments, a CMP process may be used to remove a portion of the handle substrate 750, and then a chemical and / or physical etching process may be used to remove the remainder of the handle substrate 750. Alternatively, a portion or all of the handle substrate 750 may be removed using chemical etching, which may be selective etching. The chemical etching may be selective to terminate at the desired layer, e.g., the device layer 707. Finally, a physical etching process, e.g., reactive ion etching (RIE), may be used to remove a portion or all of the handle substrate 750 and / or smooth and prepare the device layer 707 for subsequent epitaxial growth and / or processing steps.
[0092]
[0124] The handle substrate 750 can be removed in several ways. For example, a mechanical grinding process can be used to remove most of the handle substrate. Next, chemical etching, which may be selective etching, can be used to remove the material and expose the desired layer. Finally, physical etching, such as reactive ion etching (RIE) process, can be used to remove any existing interface layers.
[0093]
[0125] Removing the handle substrate 750 allows for the removal of structures that could otherwise result in losses during the operation of the MMIC device. For example, the handle substrate 750 may include a conductive layer that can interact with the electric and / or magnetic fields generated by the MMIC device during high-frequency operation, potentially resulting in losses, heat generation, and other undesirable effects. Therefore, by removing the handle substrate 750 and the layers / structures within it that could adversely affect the performance of the MMIC device, embodiments of the present invention provide methods and systems with lower losses than comparable conventional devices and structures.
[0094]
[0126] Referring to the alternative processed substrate 760 and device layer 707 shown in Figure 7E, a substrate structure is provided that can be used in an MMIC manufacturing line, as will be described in more detail below. The alternative processed substrate 760 may be provided in a large size suitable for an MMIC manufacturing line, e.g., 200 mm or 300 mm. Furthermore, since the alternative processed substrate 760 can include a barrier layer that can prevent outward diffusion from the ceramic material, including polycrystalline AlN, the substrate structure can be used in semiconductor process flows and cleanroom environments. Moreover, since the alternative processed substrate 760 can be CTE-matched to the epitaxial layer that is subsequently grown, the alternative processed substrate provides the benefits available using the growth substrate 705, but does not include any structures or materials that could adversely affect the performance of the MMIC device.
[0095]
[0127] Figure 7F is a cross-sectional view showing the formation of an MMIC device element in a device layer according to one embodiment of the present invention. In Figure 7F, the substrate structure 770 includes an alternative processing substrate 760 and a device layer 707, which is a GaN layer in the illustrated embodiment. The device layer 707 is used to manufacture MMIC device elements 720a, 720b, and 720c. Each of the MMIC device elements 720 represents a different MMIC device. For example, MMIC device element 720a can be a capacitor, MMIC device element 720b can be a transistor, and MMIC device element 720b can be a waveguide. Each of the different MMIC device elements 720 includes a metal structure 722. In Figure 7F, the device layer 707 is a GaN layer, which can have a thickness of about 1 to 10 μm and is used to reduce losses and capacitance.
[0096]
[0128] As shown in Figure 7F, in contrast to the process flow associated with Figure 3A, device manufacturing is performed after the device layer 707 has been bonded to the alternative fabricated substrate 760. As a result, the alternative fabricated substrate 760 may be selected to provide low loss during high-frequency operation of the MMIC device, as described above. Furthermore, the properties of the alternative fabricated substrate 760 may be selected to provide compliance with the foundry process. In addition, the use of the alternative fabricated substrate 760 enables the use of substrates in the MMIC device manufacturing process that would not be available by other means. For example, if the alternative fabricated substrate 200 shown in Figure 2 is used as the alternative fabricated substrate 760, the device layer 707 can have a diameter such as 200 mm or 300 mm. Using a 200 mm GaN layer as the device layer 707 bonded to the alternative fabricated substrate 760, a foundry process suitable for a 200 mm wafer can be used. In contrast, if the device layer 707 is grown on a silicon carbide substrate, size limitations prevent the use of these large-diameter device layers.
[0097]
[0129] Figure 7G is a cross-sectional view showing the removal of a portion of the alternative processed substrate according to one embodiment of the present invention. As discussed in relation to Figure 3E, in order to reduce thermal resistance, the alternative processed substrate 760 can be thinned to, for example, about 50 μm in thickness.
[0098]
[0130] The substrate thinning process shown in Figure 7G can be carried out in several ways. For example, a portion of the alternative processed substrate 760 can be removed using a mechanical grinding process. Alternatively, or in combination with the mechanical grinding process, the illustrated portion of the alternative processed substrate 760 can be removed using chemical etching, which may be selective etching. For example, chemical etching may utilize potassium hydroxide (KOH) or tetramethylammonium hydroxide (TMAH) during the etching process. Finally, in addition to, or in combination with, the mechanical grinding process and / or chemical etching, the illustrated portion of the alternative processed substrate 760 can be removed using physical etching, such as reactive ion etching (RIE) process. The physical etching process can smooth and prepare the surface for subsequent metallization or other processes.
[0099]
[0131] In contrast to techniques that remove portions of other types of substrates, the thinned alternative substrate 760, as shown in Figure 7G, provides mechanical stability to the device layer 707 and the MMIC device elements. This mechanical stability is due to the low level of residual stress associated with the device layer 707 bonded to the alternative substrate 760. For example, if the device layer 707 were grown on a silicon substrate, the residual stress present in the device layer 707 would result in warping and / or bending of the silicon substrate after the thinning process shown in Figure 7G. In contrast, since the device layer 707 was CTE-matched to the growth substrate 705, the residual stress present in the device layer 707 is low, enabling the high level of mechanical stability after the thinning process shown in Figure 7G.
[0100]
[0132] Figure 7H is a cross-sectional view showing via formation in the remaining portion of a replacement substrate according to one embodiment of the present invention. In Figure 7H, vias 762 and 764 are formed through the remaining portion of the replacement substrate 760 to make electrical contact with MMIC device elements 720b and 720c, respectively. A ground / power plane 766 is formed and electrically connected to vias 762 and 764. Vias 762 and 764 may be manufactured using appropriate semiconductor processing techniques, including etching, laser ablation, etc. In some embodiments, once the MMIC device elements 720b and 720c are connected, the via formation process can be terminated by a combination of methods.
[0101]
[0133] Although only two vias, vias 762 and 764, are shown in Figure 7H, there are no vias formed on the MMIC device element 720a, and these are not required by the present invention. In other embodiments, vias can be formed on all MMIC device elements, or vias can be formed on a smaller subset of MMIC device elements. For example, if the MMIC device element 720a is a capacitor, vias may not be provided.
[0102]
[0134] Figure 7I is a cross-sectional view showing the attachment of a cooling structure to a replacement substrate according to one embodiment of the present invention. The cooling structure 775 is attached to the ground / power plane 766, and during device operation, heat generated by the MMIC device element 720 can be conducted to the cooling structure 775 via the device layer 707, the rest of the replacement substrate 760, and the ground / power plane 766.
[0103]
[0135] Figure 7J is a simplified flowchart illustrating a method for manufacturing an MMIC system according to one embodiment of the present invention. Method 780 includes providing a processed substrate including a growth substrate and a device layer bonded to the growth substrate (781), and bonding a handle substrate to the device layer (782). The method also includes removing the growth substrate and bonding a replacement processed substrate to the device layer (784). The method further includes removing the handle substrate (786) and manufacturing a plurality of MMIC device elements using the device layer (788).
[0104]
[0136] Furthermore, the method includes removing a portion of the replacement substrate and forming a ground / power plane coupled to the remaining portion of the replacement substrate (790). The method also includes forming multiple vias from the ground / power plane to one or more of the multiple MMIC device elements (792) and bonding a cooling structure to the ground / power plane (794). Since the structure manufactured using the method described in relation to Figure 7J has elements in common with the structure manufactured using the methods described in relation to Figures 3H and 5I, the steps used in conjunction with Figures 3H and 5I can be appropriately applied to Figure 7J.
[0105]
[0137] It should be understood that the specific steps shown in Figure 7J provide a specific method for manufacturing an MMIC system according to an embodiment of the present invention. Other sequences of steps may also be performed by alternative embodiments. For example, alternative embodiments of the present invention may perform the steps outlined above in a different order. Furthermore, each of the individual steps shown in Figure 7J may include multiple substeps that can be performed in various orders as appropriate. In addition, additional steps may be added or removed depending on the specific application. Those skilled in the art will recognize many variations, modifications, and alternative forms.
[0106]
[0138] Figure 8A is a cross-sectional view showing an alternative embodiment utilizing a thinned carrier substrate according to one embodiment of the present invention. Figure 8A provides a structure corresponding to that shown in Figure 5H, which can be used in conjunction with the formation of vias passing through the thinned carrier substrate to provide electrical contact to MMIC device elements.
[0107]
[0139] Figure 8B is a cross-sectional view showing a second alternative embodiment utilizing a bifacial ground / power plane according to one embodiment of the present invention. The bifacial ground / power plane is implemented in Figure 8B in a similar manner to that discussed in Figure 6. Vias 820 and 822 are formed through a thinned carrier substrate 810 to electrically contact the MMIC device elements. A ground / power plane 824 is formed and electrically connected to vias 820 and 822. Vias 820 and 822 may be manufactured using appropriate semiconductor processing techniques, including etching, laser ablation, etc. In some embodiments, once the MMIC device elements are connected, the methods can be combined to terminate the via formation process. The second ground / power plane 805 is coupled to a cooling structure 550.
[0108]
[0140] Although only two vias, via 820 and via 822, are shown in Figure 8B, there are no vias formed on at least one of the MMIC device elements, and this is not required by the present invention. In other embodiments, vias can be formed on all MMIC device elements, or vias can be formed on a smaller subset of MMIC device elements.
[0109]
[0141] While several embodiments have been discussed in relation to layers, the term "layer" should be understood to include a number of sub-layers constructed to form the layer in question. Thus, the term "layer" is not intended to refer to a single layer consisting of a single material, but rather to encompass one or more materials layered in a complex manner to form the desired structure. Those skilled in the art will recognize numerous variations, alterations, and alternative forms.
[0110]
[0142] The examples and embodiments described herein are for illustrative purposes only, and it will be understood that various modifications or changes in light thereof are suggested to those skilled in the art and are included in the spirit and scope of this application and in the appended claims.
Claims
1. 1. A monolithic microwave integrated circuit (MMIC) system comprising: A growth substrate; a device layer bonded to the growth substrate; a plurality of MMIC device elements coupled to the device layer; a plurality of metallization structures coupled to the plurality of MMIC device elements; a carrier substrate coupled to the plurality of metallization structures; a cooling structure coupled to the carrier substrate; Equipped with The carrier substrate is disposed between the plurality of metallization structures and the cooling structure, forming a monolithic microwave integrated circuit (MMIC) system.
2. The MMIC system of claim 1 , wherein a coefficient of thermal expansion (CTE) of said growth substrate is substantially matched to a CTE of said device layers.
3. The MMIC system of claim 1 , wherein said growth substrate comprises a polycrystalline ceramic core.
4. The MMIC system of claim 3 , wherein said polycrystalline ceramic core comprises aluminum nitride.
5. The MMIC system of claim 1 , wherein the device layer has a thickness of greater than 1 μm.
6. The MMIC system of claim 5, wherein said thickness is between 1 and 10 μm.
7. The MMIC system of claim 1 further comprising a plurality of vias connecting ground / power planes to said plurality of MMIC device elements.
8. The MMIC system of claim 7 further comprising a second cooling structure coupled to said ground / power plane.
9. a second ground / power plane coupled to the carrier substrate; a second plurality of vias leading from the second ground / power plane to one or more of the plurality of metal structures; The MMIC system of claim 1 further comprising:
10. The MMIC system of claim 9 further comprising a second cooling structure coupled to said second ground / power plane.
11. The MMIC system of claim 1 , wherein said device layer comprises Gallium Nitride (GaN).
12. 1. A method for manufacturing a monolithic microwave integrated circuit (MMIC) system, the method comprising: providing an engineered substrate comprising a growth substrate and a device layer bonded to the growth substrate; fabricating a plurality of MMIC device elements using the device layer; Providing a carrier substrate including a plurality of metal structures; bonding the plurality of metal structures to the plurality of MMIC elements; removing a portion of the growth substrate; removing a portion of the carrier substrate; forming a ground / power plane coupled to the growth substrate; forming a plurality of vias from said ground / power plane to one or more of said plurality of MMIC device elements; bonding a cooling structure to the carrier substrate; A method for manufacturing a MMIC system, comprising:
13. The method of claim 12 , further comprising bonding a second cooling structure to the ground / power plane.
14. Prior to bonding the cooling structure to the carrier substrate, forming a second ground / power plane coupled to the carrier substrate; forming a second plurality of vias from the second ground / power plane to one or more of the plurality of metal structures; The method of claim 12 further comprising:
15. The method of claim 14 , further comprising bonding a second cooling structure to the ground / power plane.
16. The method of claim 12 , wherein a coefficient of thermal expansion (CTE) of the growth substrate is substantially matched to a CTE of the device layer.
17. The method of claim 12 , wherein the growth substrate comprises a polycrystalline ceramic core.
18. The method of claim 17 , wherein the polycrystalline ceramic core comprises aluminum nitride.
19. The method of claim 12, wherein the device layer has a thickness of 1 to 10 μm.
20. 20. The method of claim 19, wherein the device layer comprises gallium nitride (GaN).
21. 1. A monolithic microwave integrated circuit (MMIC) system comprising: An alternative processed substrate; a device layer bonded to the alternative processing substrate; a plurality of monolithic microwave integrated circuit (MMIC) device elements coupled to the device layer; a carrier substrate coupled to the plurality of MMIC device elements; a ground / power plane coupled to the alternative engineering substrate; a plurality of vias connecting the ground / power plane to the plurality of MMIC device elements; a cooling structure coupled to the ground / power plane; A monolithic microwave integrated circuit (MMIC) system comprising:
22. 22. The MMIC system of claim 21, wherein a coefficient of thermal expansion (CTE) of said alternative processing substrate is substantially matched to a CTE of said device layer.
23. The MMIC system of claim 21 wherein said alternative processing substrate comprises a polycrystalline ceramic core.
24. 24. The MMIC system of claim 23, wherein said polycrystalline ceramic core comprises aluminum nitride.
25. 22. The MMIC system of claim 21, wherein the device layer has a thickness of greater than 1 μm.
26. 22. The MMIC system of claim 21 further comprising a second plurality of vias connecting a second ground / power plane coupled to said plurality of MMIC device elements.
27. 1. A method for manufacturing a monolithic microwave integrated circuit (MMIC) system, the method comprising: providing an engineered substrate comprising a growth substrate and a device layer bonded to the growth substrate; fabricating a plurality of MMIC device elements using the device layer; Providing a carrier substrate; bonding the carrier substrate to the plurality of MMIC device elements; removing the growth substrate; bonding a replacement engineered substrate to the device layer; removing a portion of the replacement engineered substrate; forming a ground / power plane coupled to the alternative engineered substrate; forming a plurality of vias from said ground / power plane to one or more of said plurality of MMIC device elements; bonding a cooling structure to the ground / power plane; A method for manufacturing a monolithic microwave integrated circuit (MMIC) system, comprising:
28. The method of claim 27 , further comprising removing at least a portion of the carrier substrate.
29. forming a second ground / power plane coupled to a remainder of the carrier substrate; forming a second plurality of vias from the second ground / power plane to one or more of the plurality of MMIC device elements; 30. The method of claim 28, further comprising:
30. 30. The method of claim 27, wherein the coefficient of thermal expansion (CTE) of the alternative processing substrate is substantially matched to a CTE of the device layer.
31. The method of claim 27 , wherein the alternative engineered substrate comprises a polycrystalline ceramic core.
32. The method of claim 31 , wherein the polycrystalline ceramic core comprises aluminum nitride.
33. 28. The method of claim 27, wherein the device layer has a thickness greater than 1 μm.
34. 1. A monolithic microwave integrated circuit (MMIC) system comprising: An alternative processed substrate; a device layer bonded to the alternative processing substrate; a plurality of MMIC device elements coupled to the device layer; a ground / power plane coupled to the alternative engineering substrate; a plurality of vias connecting the ground / power plane to the plurality of MMIC device elements; a cooling structure coupled to the ground / power plane; A monolithic microwave integrated circuit (MMIC) system comprising:
35. 35. The MMIC system of claim 34, wherein a coefficient of thermal expansion (CTE) of said alternative processing substrate is substantially matched to a CTE of said device layer.
36. 35. The MMIC system of claim 34, wherein said alternative processing substrate comprises a polycrystalline ceramic core.
37. 37. The MMIC system of claim 36, wherein said polycrystalline ceramic core comprises aluminum nitride.
38. The MMIC system of claim 34, wherein the device layer has a thickness of 1 μm to 10 μm.
39. 35. The MMIC system of claim 34 further comprising a carrier substrate coupled to said plurality of MMIC device elements.