Method for protecting workpiece and method for machining workpiece
By forming a convex pattern on the workpiece surface and attaching a protection sheet that avoids contact with the circuit, the method effectively protects sensitive semiconductor circuits from contamination and damage during processing.
Patent Information
- Application Number
- JP2023045464
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
AI Technical Summary
Existing methods for protecting semiconductor circuits using adhesive tapes during wafer processing cannot prevent contact between the adhesive and the circuit surface, which can damage sensitive circuits like image sensors and MEMS.
A convex pattern is formed on the surface of the workpiece to surround the circuit, with a surface protection sheet attached to the convex pattern, ensuring the sheet remains non-contact with the circuit surface, and the sheet is peeled off after processing.
The circuit surface is reliably protected from contact with other members, preventing contamination and damage during processing, particularly in sensitive circuits.
Smart Images

Figure 2024134988000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for protecting and machining a workpiece, and more particularly to a method for protecting a workpiece in which it is highly necessary to prevent a circuit formed on the surface of the workpiece from coming into contact with other members. [Background technology]
[0002] As semiconductor devices become more and more integrated and miniaturized, there is a continuing demand for thinner semiconductor chips. In order to make chips smaller and thinner, it is common to thin the wafer by grinding the backside of the wafer.
[0003] During back grinding of the wafer, a surface protection sheet called backgrind tape is affixed to the wafer surface to protect the circuits and chips arranged on the wafer surface and to hold the wafer.
[0004] Patent Document 1 discloses an adhesive tape for processing semiconductor wafers that has good conformability to the surface of semiconductor wafers having steps and protrusions and can be peeled off without damaging the semiconductor wafer or leaving any adhesive residue.
[0005] When the circuit surface is protected using the above-mentioned adhesive tape for semiconductor wafer processing, the adhesive comes into contact with the circuit surface. In general semiconductor elements, even if the adhesive comes into contact with the circuit surface, there is no problem as long as the adhesive tape can be peeled off without leaving any adhesive residue. However, circuits such as image sensors and MEMS (Micro Electro Mechanical Systems) require extremely high clarity, and even if an organic substance such as an adhesive comes into contact with a part of the circuit surface, there is a risk of impairing the function. In particular, as a result of the rapid miniaturization of circuits in recent years, there is an increasing need to prevent circuits such as image sensors from coming into contact with other components. [Prior art documents] [Patent documents]
[0006]
Patent Document 1
Summary of the Invention
Problems to be Solved by the Invention
[0007] However, in the protection method using an adhesive tape for semiconductor wafer processing as in Patent Document 1, it is inevitable that the adhesive comes into contact with the circuit surface. For this reason, there has been a demand for a work protection method that can reliably protect the work with a surface protection sheet while preventing contact between the circuit surface and other members including the protection sheet.
Means for Solving the Problems
[0008] In response to such problems, the inventor of the present invention conceived of forming a convex pattern on the surface of a work on which a circuit is formed so as to surround the circuit formation portion, and attaching a protection sheet thereon, thereby reliably protecting the circuit surface without contact between the circuit surface and other members including the protection sheet, and completed the present invention.
[0009] Aspects of the present invention are as follows. (1) A work protection method having a step of attaching a surface protection sheet to the surface of a work, The surface of the work has an inner peripheral portion on which a plurality of circuits are formed and an outer peripheral portion having no circuit surrounding the inner peripheral portion, Convex patterns are formed between the circuits and on the outer peripheral portion, A work protection method in which a surface protection sheet is attached to the surface provided with the convex pattern. (2) The work protection method according to (1), wherein the height Hc of the circuit formed in the inner peripheral portion and the height Hp of the convex pattern satisfy the relationship Hc < Hp. (3) The work protection method according to (1), wherein the convex pattern is made of resin. (4) The work protection method according to (1), wherein the surface protection sheet is a resin film. (5) Protecting a work by the method according to any one of (1) to (4) above, Grind the back side of the workpiece while protecting it. The surface protection sheet is peeled off, and the convex pattern is removed together with the surface protection sheet. (6) A step of forming a groove on the surface of the workpiece before the step of forming a convex pattern on the surface of the workpiece, A method for processing a workpiece according to (5), wherein in the step of grinding the back surface of the workpiece, the workpiece is diced into a plurality of workpiece pieces starting from the grooves. (7) A process for forming a modified region inside the workpiece before the process for grinding the back surface of the workpiece, A method for processing a workpiece according to (5), wherein in the step of grinding the back surface of the workpiece, the workpiece is diced into a plurality of workpiece pieces starting from modified regions. Effect of the Invention
[0010] According to the present invention, the circuit surface of the workpiece can be reliably protected without the circuit surface coming into contact with other members, including the surface protection sheet. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a plan view of the circuit surface. [Diagram 2] FIG. 2 is a plan view showing an example of a convex pattern formed on the surface of a circuit. [Diagram 3] FIG. 3 is a plan view showing another example of a convex pattern formed on the circuit surface. [Figure 4] FIG. 4 is a schematic cross-sectional view taken along line AA in FIG. [Diagram 5] FIG. 5 is a schematic cross-sectional view showing a state in which a surface protection sheet is attached onto the convex pattern. [Figure 6] FIG. 6 is a schematic cross-sectional view showing a state in which the back surface of a workpiece is being machined (ground) while the workpiece is being protected by the workpiece protection method of the present invention. [Figure 7] FIG. 7 is a schematic cross-sectional view showing a state in which the surface protection sheet is being peeled off after the rear surface of the workpiece has been processed. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The present invention will now be described in detail with reference to the accompanying drawings based on specific embodiments. First, the main terms used in this specification will be explained.
[0013] The work refers to a plate-like body to which a surface protection sheet is attached and then cut into individual pieces. Examples of the work include a circular wafer (including a case having an orientation flat), a rectangular panel level package, and a strip (rectangular substrate) sealed with molded resin. Among them, a wafer having a circuit is preferable from the viewpoint of easily obtaining the effect of the present invention. The wafer may be, for example, a semiconductor wafer such as a silicon wafer, a gallium arsenide wafer, a silicon carbide wafer, a gallium nitride wafer, or an indium phosphide wafer, or an insulating wafer such as a glass wafer, a lithium tantalate wafer, or a lithium niobate wafer, or may be a reconstructed wafer made of a resin and a semiconductor used for producing a fan-out package or the like. From the viewpoint of easily obtaining the effect of the present invention, the wafer is preferably a semiconductor wafer or an insulating wafer, and more preferably a semiconductor wafer.
[0014] Singulation of a work refers to dividing the work into individual circuits to obtain individual work pieces. For example, if the work is a wafer, the individual work pieces are chips, and if the work is a panel level package or a strip (rectangular substrate) sealed with molded resin, the individual work pieces are semiconductor packages.
[0015] The "front surface" of a workpiece refers to the surface on which a circuit is formed, and the "back surface" of a workpiece refers to the surface on which no circuit etc. is formed. The circuit is not particularly limited, but the method of the present invention is particularly preferably used for image sensor circuits and MEMS, in which contact between the circuit and other members is strongly discouraged.
[0016] DBG is a method in which a groove of a specified depth is formed on the front side of a wafer, and then the wafer is ground from the back side to separate the wafer by grinding. The grooves formed on the front side of the wafer are formed by methods such as blade dicing, laser dicing, and plasma dicing.
[0017] LDBG is a modified version of DBG, in which a modified region is created inside the wafer using a laser, and the wafer is divided into individual pieces by the stress generated during back grinding of the wafer.
[0018] The term "group of individual workpieces" refers to a plurality of individual workpieces held on the surface protection sheet of the present invention after the workpiece is singulated. These individual workpieces, as a whole, form a shape similar to that of the workpiece. The term "group of chips" refers to a plurality of chips held on the surface protection sheet of the present invention after the wafer as the workpiece is singulated. These chips, as a whole, form a shape similar to that of the wafer.
[0019] "(Meth)acrylate" is used as the term to refer to both "acrylate" and "methacrylate," and similar terms.
[0020] The "energy rays" refer to ultraviolet rays, electron beams, etc., and are preferably ultraviolet rays.
[0021] Unless otherwise specified, the "weight average molecular weight" is a polystyrene equivalent value measured by gel permeation chromatography (GPC). Measurements by such a method are performed, for example, using a high-speed GPC device "HLC-8120GPC" manufactured by Tosoh Corporation with a high-speed column "TSK guard column H XL -H", "TSK Gel GMH XL ", "TSK Gel G2000 H XL (All of the above are manufactured by Tosoh Corporation) connected in the above order, the column temperature was 40° C., the liquid flow rate was 1.0 mL / min, and the detector was a differential refractometer.
[0022] The release sheet is a sheet that supports the pressure-sensitive adhesive layer in a releasable manner. The term "sheet" is not limited to a specific thickness, and is used to include a film.
[0023] The mass ratios in the explanations of the compositions such as the pressure sensitive adhesive and the convex pattern forming composition are based on the active ingredients (solid content), and do not include the solvent unless otherwise specified.
[0024] As an embodiment of the present invention, as one of the processing of a workpiece having a circuit or the like formed on one surface (front surface) and no circuit or the like formed on the other surface (back surface), grinding the back surface of the workpiece is exemplified. By grinding the back surface, the thickness of the workpiece can be reduced, and by using the above DBG and LDBG, the thickness of the workpiece obtained by dividing the workpiece can be reduced.
[0025] At this time, a surface protection sheet is attached to the surface of the workpiece in order to protect the surface of the workpiece before grinding the backside of the workpiece. By attaching the surface protection sheet to the surface of the workpiece, contamination of circuits, etc. due to intrusion of abrasives, cooling water, etc. into the workpiece surface during backside grinding, and damage to circuits, etc. due to the force applied during backside grinding can be prevented.
[0026] The workpiece protected by the method according to this embodiment has, on its surface, an inner periphery on which a plurality of circuits are formed, and an outer periphery surrounding the inner periphery and having no circuits.
[0027] In the following description, reference will be made to the drawings, in which the relative size of the circuits to the workpiece (wafer) and the circuit spacing are greatly exaggerated.
[0028] Figure 1 shows a plan view from the surface side of the workpiece. On the surface of the workpiece 1, multiple circuits are formed, surrounded by the planned cutting lines 3 shown by dashed lines. In the drawing, the part of the circuit that is particularly susceptible to contact with other components is shown by the reference numeral 2. Hereinafter, this area will be referred to as the "specific area 2." This workpiece will ultimately be cut into each circuit along the planned cutting lines 3 shown by dashed lines, and divided into multiple element pieces (chips).
[0029] The workpiece protection method according to this embodiment includes the following steps 1 and 2. Step 1: Forming a convex pattern between specific areas on the workpiece surface and on the outer periphery Step 2: A process of attaching a surface protection sheet to the surface with the convex pattern.
[0030] In the following, a method for protecting a workpiece will be described assuming that the workpiece is a wafer.
[0031] (Process 1) In step 1, a convex pattern is formed between specific regions on the inner periphery of the wafer surface and on the outer periphery. The "between specific regions" refers specifically to the vicinity of the lines 3 along which the wafer is to be cut, and the convex pattern is provided so as to cover the lines 3 along which the wafer is to be cut. The outer periphery is the edge of the wafer, and refers to the area where no circuits are formed. Generally, the area extending about 10 mm from the edge of the wafer becomes the outer periphery, which does not have any circuits.
[0032] (Convex pattern 4) The convex pattern 4 is a pattern formed on the surface of the wafer 1 so as to protrude in the thickness direction of the wafer 1. Such convex pattern 4 is formed between specific regions 2 of the circuit on the inner periphery of the surface of the wafer and on the outer periphery, so that even when the surface protection sheet 10 is attached to the surface of the wafer 1, the surface protection sheet 10 and the specific regions 2 remain out of contact with each other.
[0033] In this embodiment, it is preferable to set the height Hp of the convex pattern 4 according to the height Hc of the circuit 2 on the surface of the wafer. Note that the height Hc of the circuit 2 refers to the height of the highest part of the circuit with respect to the flat part between the circuits on the wafer surface. The height Hp of the convex pattern 4 refers to the height of the highest part of the convex pattern with respect to the flat part between the circuits on the wafer surface. It is preferable that the height Hp of the convex pattern 4 and the height Hc of the circuit 2 on the surface of the wafer satisfy the relationship Hc < Hp. By setting the height Hp of the convex pattern 4 to be higher than the height Hc of the circuit 2 on the surface of the wafer, it is possible to prevent the surface protection sheet 10 attached on the convex pattern 4 from contacting the circuit 2.
[0034] In this embodiment, the height Hp of the convex pattern is preferably 1 to 2000 μm.
[0035] The material constituting the convex pattern 4 may be any material that can stably hold the surface protection sheet 10 attached thereon. In this embodiment, from the viewpoint of easy formation of the convex pattern, the material constituting the convex pattern is preferably a resin. As the resin, an adhesive resin that adheres to the wafer surface is preferable. Examples of the adhesive resin include acrylic resin, silicone resin, urethane resin, epoxy resin, phenol resin, urea resin, alkyd resin, vinyl acetate resin, vinyl chloride resin, amide resin, imide resin, chloroprene rubber, nitrile rubber, styrene-butadiene rubber, nylon, polycarbonate, polypropylene, and the like.
[0036] Further, the adhesive resin is preferably curable. Before curing, it is easy to form a predetermined shape, and after curing, it is easy to make the material hard enough to suppress the intrusion of abrasive, cooling water, etc. into the circuits of the wafer during back grinding.
[0037] Examples of the curable resin include thermosetting resins and energy ray curable resins. From the viewpoint of removing the convex pattern from the wafer surface after back grinding, an energy ray curable resin is preferable.
[0038] The shear storage modulus of the convex pattern at 23° C. is preferably 50 MPa or more. When the shear storage modulus at 23° C. is within the above range, the convex pattern becomes relatively hard, and even during back grinding, the height difference between the outer periphery and the inner periphery of the wafer is suppressed. When the convex pattern is formed from a curable resin, the shear storage modulus is a value measured for the resin after curing.
[0039] The convex pattern 4 is formed between specific regions on the inner periphery of the wafer surface and on the outer periphery, as shown in Figures 2, 3, and 4. The convex pattern 4 may be formed so as to cover the entire surface except the specific region 2, as shown in Figure 2. Alternatively, the convex pattern 4 may be formed so as to cover a part of the surface except the specific region 2, as shown in Figure 3. It is preferable that the convex pattern 4 is formed continuously and without interruption. If the convex pattern 4 is formed continuously, it can be peeled off continuously when removing the convex pattern. On the other hand, if the convex pattern is discontinuous, a part of the convex pattern may remain on the wafer surface when it is removed.
[0040] The means for forming the convex pattern 4 may be determined according to the material for forming the convex pattern 4. For example, when forming the convex pattern using a curable resin, a means for applying a liquid resin before curing can be used. Specifically, a coating device such as a die coater, curtain coater, spray coater, slit coater, or knife coater; a printing device such as a screen printer or inkjet printer; or a dropping device such as a dispenser can be used.
[0041] (Process 2) As shown in FIG. 5, after the convex pattern 4 is formed, a surface protection sheet 10 is attached to the top of the convex pattern 4. (Surface protection sheet 10) The surface protection sheet 10 may be configured to protect the circuits and the like on the wafer surface. If the surface protection sheet 10 has good adhesion to the material of the convex pattern, the surface protection sheet 10 may be a resin film. The resin film is a thin-layered resin molding that does not have an adhesive layer, and may be a single layer or a laminate. Such a resin film generally does not have adhesive properties, but if the resin film has high affinity with the material of the convex pattern, the resin film can be attached to the convex pattern by applying an appropriate pressure and heating as necessary.
[0042] The surface protection sheet 10 may also be a so-called adhesive sheet having a substrate and an adhesive layer. The adhesive layer is attached to the tops of the convex patterns 4, thereby reliably protecting the specific region 2. The surface protection sheet 10 may also have an intermediate layer between the substrate and the adhesive layer. Furthermore, another layer may be formed between the intermediate layer and the adhesive layer.
[0043] When the surface protective sheet is a resin film, it may be composed of a single layer film made of one resin film, or may be composed of a multilayer film in which a plurality of resin films are laminated.
[0044] In this embodiment, examples of the material for the resin film include polyesters such as polyethylene terephthalate, polyethylene naphthalate, polybutylene terephthalate, wholly aromatic polyesters, polyamides, polycarbonates, polyacetals, modified polyphenylene oxides, polyphenylene sulfides, polysulfones, polyether ketones, biaxially oriented polypropylenes, etc. Among these, polyesters are preferred, and polyethylene terephthalate is more preferred.
[0045] The thickness of the resin film affects the rigidity of the surface protection sheet, and may be set according to the material of the resin film. In this embodiment, the thickness of the resin film is preferably 25 μm or more and 200 μm or less, more preferably 35 μm or more and 150 μm or less, and even more preferably 40 μm or more and 150 μm or less.
[0046] The surface protection sheet 10 may be a so-called adhesive sheet having a substrate and an adhesive layer. The above-mentioned resin film is used as the substrate of such an adhesive sheet. The composition of the adhesive layer is not limited as long as it has enough adhesiveness to be attached to the top of the convex pattern. In this embodiment, the adhesive layer is preferably composed of, for example, an acrylic adhesive, a urethane adhesive, a rubber adhesive, a silicone adhesive, or the like. In addition, the adhesive layer is preferably formed of an energy ray-curable acrylic adhesive. One surface of the substrate may be subjected to an adhesion treatment such as a corona treatment in order to improve adhesion with the adhesive layer.
[0047] The thickness of the adhesive layer is not particularly limited as long as it is thick enough to be adhered to the top of the convex pattern. In this embodiment, the thickness of the adhesive layer is preferably 1 μm or more and 100 μm or less, more preferably 5 μm or more and 50 μm or less. The thickness of the adhesive layer means the thickness of the entire adhesive layer. For example, the thickness of an adhesive layer composed of multiple layers means the total thickness of all layers constituting the adhesive layer.
[0048] (How to protect the work) In this embodiment, as shown in FIG. 5, a surface protection sheet 10 is attached to the top of the convex pattern 4 to protect the workpiece. The surface protection sheet 10 may be cut to the same shape as the workpiece in advance, or the surface protection sheet 10 may be cut to match the outer peripheral shape of the workpiece after the surface protection sheet 10 is attached. When the workpiece is a semiconductor wafer having a circuit, each specific area 2 is surrounded by the convex pattern 4 and is covered thereon with the surface protection sheet 10. In addition, since the convex pattern 4 is provided higher than the circuit, the surface protection sheet 10 does not come into contact with the specific area. Therefore, according to this embodiment, the specific area of the circuit can be protected cleanly. In this state, even if the workpiece is transported, stored, or processed, the specific area will not be damaged.
[0049] (Workpiece processing method) According to this embodiment, the workpiece can be processed while being protected. In the following, an example will be described in which the workpiece is a semiconductor wafer having a circuit on its surface, and the processing is grinding of the back surface of the wafer.
[0050] In the workpiece processing method of the present invention, the wafer with the surface protection sheet attached is placed on a chuck table (not shown) with the surface protection sheet 10 side. The chuck table has, for example, a porous holding surface, and the surface protection sheet is adsorbed and fixed to the chuck table by suction from the holding surface.
[0051] As shown in Fig. 6, after the wafer is fixed to the chuck table, the back surface of the wafer is ground, for example, by a grinding wheel 5 or the like. During back grinding of the wafer, water is sprayed onto the grinding surface while grinding in order to remove heat and grinding debris generated during grinding. However, according to the method for protecting a workpiece of the present invention, the specific area of the workpiece is protected by the convex pattern and the surface protection sheet, so that the intrusion of cleaning water during grinding does not occur and the specific area of the wafer is not contaminated. The thickness of the wafer after back grinding is, for example, about 25 μm to 600 μm.
[0052] After grinding, the suction is released and the wafer and surface protection sheet are released from the chuck table.
[0053] (Peeling process) When peeling off the surface protection sheet 10, as shown in Fig. 7, a pick-up tape 12 is attached to the back side of the workpiece 1 after the backside grinding, and the position and direction are adjusted so that the workpiece can be picked up. At this time, a ring frame 14 arranged on the outer periphery of the workpiece 1 is also attached to the pick-up tape 12, and the outer periphery of the pick-up tape 12 is fixed to the ring frame 14. The workpiece 1 and the ring frame may be attached to the pick-up tape 12 at the same time, or may be attached at different times. Next, the surface protection sheet 10 is peeled off from the workpiece 1 held on the pick-up tape 12.
[0054] In this embodiment, the surface protection sheet 10 is peeled off from the work 1 after the back surface grinding. At this time, the convex pattern 4 is peeled off together with the surface protection sheet 10. If a resin film having a high affinity with the material of the convex pattern 4 is used as the surface protection sheet 10, the surface protection sheet 10 and the convex pattern 4 can be peeled off in an integrated state. For example, if the convex pattern 4 and the resin film are formed from the same or similar resin, the resin film and the convex pattern can be peeled off in an integrated state. Also, even if an adhesive sheet is used as the surface protection sheet 10, the convex pattern 4 adheres to the adhesive sheet, so the surface protection sheet 10 and the convex pattern 4 can be peeled off in an integrated state.
[0055] (DBG or LDBG) When the workpiece processing method according to this embodiment is applied to DBG or LDBG, a step of forming a groove on the surface of the wafer (step 3A: DBG) or a step of forming a modified region inside the wafer (step 3B: LDBG) is included in addition to the above steps 1 and 2. The groove and modified region are formed so as to follow the cutting lines 3 along which the wafer is divided into individual pieces in the above-mentioned back grinding.
[0056] When grooves are formed on the surface of the wafer by dicing or the like, steps 1 and 2 are performed after step 3A. That is, in step 1, a convex pattern is formed so as to cover the grooves formed in step 3A described later. If the viscosity of the resin forming the convex pattern is too low, the resin will penetrate between the grooves and bond the chips together after division, making it impossible to pick up the chips. For this reason, when the workpiece processing method according to this embodiment is applied to DBG, it is preferable to set the viscosity of the resin material forming the convex pattern to be high.
[0057] The grooves formed in step 3A are shallower than the thickness of the wafer. The grooves can be formed by dicing using a conventionally known dicing device. The wafer is divided into a plurality of chips along the grooves by the stress applied during back grinding.
[0058] On the other hand, when forming a modified region on the wafer, steps 1 and 2 may be performed before or after step 3 B. In this embodiment, when forming a modified region on the wafer, steps 1 and 2 are preferably performed before step 3 B.
[0059] In addition, the modified region is a brittle portion of the wafer, and is the starting point for the wafer to be destroyed and diced into chips when the wafer becomes thinner due to grinding in the grinding process or when stress is applied during backside grinding.
[0060] The modified region is formed inside the wafer by irradiating the laser focused on the inside of the wafer. The laser may be irradiated from the front side or the back side of the wafer. In the embodiment in which the modified region is formed, when the step 3B is performed after the step 1 and the laser is irradiated from the front side of the wafer, the laser is irradiated to the wafer through the surface protection sheet.
[0061] In DBG, back grinding is performed to thin the wafer at least to the bottom of the groove. This back grinding turns the groove into a cut that penetrates the wafer, and the wafer is divided by the cut and singulated into individual chips, resulting in a group of chips aligned on the surface protection sheet, and a group of singulated workpieces is obtained on the surface protection sheet.
[0062] In LDBG, the grinding surface (wafer back surface) may reach the modified region by grinding, but it does not have to reach the modified region strictly. In other words, it is sufficient to grind to a position close to the modified region so that the wafer is broken and singulated into chips starting from the modified region. As a result, the workpiece is singulated into individual chips, resulting in a group of chips aligned on the surface protection sheet, and a group of workpiece singulations is obtained on the surface protection sheet. In addition, the actual singulation of the chips may be performed by applying a pick-up tape and then stretching the pick-up tape.
[0063] After the back surface grinding is completed, dry polishing may be performed prior to picking up the chips.
[0064] The shape of the individualized chips (workpiece individualized products) may be square or elongated, such as rectangular. The thickness of the individualized chips is not particularly limited, but is preferably about 5 to 100 μm, and more preferably 10 to 45 μm. LDBG makes it easy to make the thickness of the individualized chips 50 μm or less, and more preferably 10 to 45 μm. The size of the individualized chips is not particularly limited, but is preferably 600 mm or less. 2 Less than 400mm, more preferably 2 Less than 120mm, more preferably 2 is less than.
[0065] Although the embodiment of the present invention has been described above, the present invention is not limited to the above embodiment, and may be modified in various aspects within the scope of the present invention. EXAMPLES
[0066] The present invention will be described in more detail below using examples, but the present invention is not limited to these examples.
[0067] The evaluation methods in the present examples are as follows.
[0068] (Staining) When the surface protection sheet comes into contact with a specific area of the circuit, organic matter from the surface protection sheet adheres to the specific area, contaminating the specific area. To check for the presence or absence of this contamination, the following evaluation was performed.
[0069] (1. Creating an adhesive sheet) To 100 parts by mass of an energy ray curable acrylic copolymer (weight average molecular weight: 800,000) obtained by adding 2-isocyanatoethyl methacrylate (MOI) to an acrylic copolymer obtained by copolymerizing 80 parts by mass of butyl acrylate (BA) and 20 parts by mass of 2-hydroxyethyl acrylate (HEA) so that the addition rate is 80 equivalents relative to the hydroxyl group (100 equivalents) derived from HEA, 1.5 parts by mass of trimethylolpropane adduct tolylene diisocyanate (manufactured by Tosoh, Coronate L) as a crosslinking agent and 2.2 parts by mass of 2,2-dimethoxy-2-phenylacetophenone (manufactured by IGM Resin, Omnirad651) as a photopolymerization initiator were added, and toluene was further added to adjust the solid content concentration to 30%, and the mixture was stirred for 30 minutes to prepare a pressure-sensitive adhesive composition.
[0070] Next, the prepared solution of the adhesive composition was applied to a PET film (thickness 110 μm) and dried to form an adhesive layer with a thickness of 20 μm, thereby producing an adhesive sheet.
[0071] (2. Creating a sample wafer) An ultraviolet-curable resin was obtained by mixing 25 parts by mass of bifunctional polyol-modified urethane acrylate (molecular weight 7300), 75 parts by mass of isobornyl acrylate, 20 parts by mass of dipentaerythritol hexaacrylate, and 0.5 parts by mass of a photopolymerization initiator (Omnirad1173, manufactured by IGM Resin).
[0072] The following ultraviolet-curing resin was applied to the mirror surface of a 12-inch silicon mirror wafer (720 μm thick) in a grid pattern with a width of 200 μm, a thickness of 20 μm, and 10 mm intervals, leaving a 10 mm x 10 mm non-coated area. The outer periphery of the wafer was also coated with a similar ultraviolet-curing resin with a width of 3 mm and a thickness of 20 μm, so that no gaps were created between the wafer and the outer edge. UV irradiation (illuminance 150 mW / cm 2 , irradiation amount 300mJ / cm 2) and the resin was cured. As a result, a sample wafer was created with many 10mm x 10mm wafer mirror surface exposed areas surrounded by 20μm high convex patterns on the inner periphery of the silicon wafer. The wafer mirror surface exposed areas are regarded as the specific areas (areas of the circuit that should avoid contact with other components) and the following tests are carried out.
[0073] (3. Measurement of Water Contact Angle) The water contact angle of the mirror-exposed surface of the sample wafer was measured in accordance with JIS R 3257: 1999. Specifically, in the examples and comparative examples, purified water was dropped onto the mirror-exposed surface of the wafer after the surface protection sheet was peeled off, and the static contact angle was measured under the following conditions using a fully automatic contact angle measuring instrument (manufactured by Kyowa Interface Science Co., Ltd., product name "DM-701").
[0074] Immediately after the sample wafer was produced, the water contact angle of the exposed mirror surface of the wafer was 2°. When the exposed mirror surface of the wafer comes into contact with an organic member, the exposed mirror surface of the wafer becomes contaminated and the water contact angle increases. ·Measurement temperature: 23℃ -Droplet volume of purified water: 2μl ·Measurement time: 1 second after dropping Image analysis method: θ / 2 method
[0075] [Example 1] A 50 μm thick PET film was attached onto the above-mentioned convex pattern. In this state, the back surface of the wafer was ground to a thickness of 200 μm. After grinding was completed, the adhesive sheet was peeled off and the water contact angle of the mirror exposed surface of the sample wafer was measured. The results are shown in Table 1.
[0076] [Example 2] The adhesive layer of the adhesive sheet prepared in 1 was attached onto the above-mentioned convex pattern. In this state, the back surface of the wafer was ground to a thickness of 200 μm. After grinding was completed, the adhesive sheet was peeled off and the water contact angle of the mirror-exposed surface of the sample wafer was measured. The results are shown in Table 1.
[0077] [Comparative Example 1] The above adhesive sheet was directly attached to the surface of a sample wafer without a convex pattern, and in this state, the back surface of the wafer was ground to a thickness of 200 μm. After grinding was completed, the adhesive sheet was peeled off, and the water contact angle of the sample wafer surface was measured. The results are shown in Table 1.
[0078] [Table 1]
[0079] According to the method for protecting a workpiece of the present invention, the object to be protected (for example, a circuit) can be reliably protected without coming into contact with other members including a surface protection sheet during protection of the workpiece. [Explanation of symbols]
[0080] 1. Work 2...A specific area of a circuit that should avoid contact with other components 3…Line to be cut 4…Convex pattern 10...Surface protection sheet 12...Pickup tape 14…Ring frame
Claims
1. A method for protecting a workpiece, comprising a step of attaching a surface protection sheet to a surface of the workpiece, The surface of the workpiece has an inner periphery on which a plurality of circuits are formed and an outer periphery surrounding the inner periphery and having no circuits; forming a convex pattern between the circuits and on the outer periphery; A method of protecting a workpiece by attaching a surface protection sheet to a surface with a convex pattern.
2. 2. The method for protecting a workpiece according to claim 1, wherein a height Hc of the circuit formed on the inner peripheral portion and a height Hp of the convex pattern satisfy the relationship Hc<Hp.
3. The method for protecting a workpiece according to claim 1 , wherein the convex pattern is made of resin.
4. The method for protecting a workpiece according to claim 1 , wherein the surface protection sheet is a resin film.
5. Protecting a workpiece by the method according to any one of claims 1 to 4, Grind the back side of the workpiece while protecting it. The surface protection sheet is peeled off, and the convex pattern is removed together with the surface protection sheet.
6. A step of forming a groove on the surface of the workpiece before the step of forming a convex pattern on the surface of the workpiece, The method for machining a workpiece according to claim 5 , wherein in the step of grinding the rear surface of the workpiece, the workpiece is diced into a plurality of workpiece pieces starting from the grooves.
7. A process for forming a modified region inside the workpiece before the process for grinding the back surface of the workpiece, The method for machining a workpiece according to claim 5 , wherein in the step of grinding the rear surface of the workpiece, the workpiece is diced into a plurality of workpiece individual pieces starting from modified regions.
Citation Information
Patent Citations
Dicing method and micromachine device
JP2004050305A
Surface protection sheet and method for grinding semiconductor wafer
JP2005123382A
Adhesive tape for semiconductor wafer surface protection and method for processing semiconductor wafer
JP2016072546A
Processing method of semiconductor protective tape and wafer
JP2017125093A
Adhesive tape for semiconductor wafer processing, manufacturing method of adhesive tape for semiconductor wafer processing, and processing method of semiconductor wafer
JP2017171896A