Transistor and method for manufacturing transistor
By using polysilicon as a catalyst for tungsten deposition, the transistor design addresses the challenge of forming plugs in high aspect ratio openings, reducing gate resistance and simplifying manufacturing, thereby enhancing transistor performance and efficiency.
Patent Information
- Application Number
- JP2023045684
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
AI Technical Summary
In transistors, reducing gate resistance is essential, especially as they become smaller, but forming plugs in dielectric layers with high aspect ratios is challenging due to incomplete metal filling, necessitating thinner layers and increased manufacturing steps.
A transistor design where polysilicon acts as a catalyst for tungsten deposition, allowing plugs to be formed even in high aspect ratio openings, reducing the need for multiple layers and simplifying the manufacturing process.
This approach enables effective plug formation in high aspect ratio openings, reducing gate resistance and simplifying the manufacturing process while maintaining the integrity of the dielectric layer.
Smart Images

Figure 2024135144000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to transistors and methods for making transistors. [Background technology]
[0002] Patent Document 1 discloses a high electron mobility transistor (HEMT). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2017-069565 A [Non-patent literature]
[0004] [Non-Patent Document 1] "Innovative Manufacturing Technologies in the Semiconductor and Display Industries (Part 1)", Technology Alliance Group, Inc., 155 pages [Non-Patent Document 2] Hitoshi Itoh et al., "Mechanism for Initial Stage of SelectiveTungsten Growth Employing a WF6 and SiH4 Mixture", JapaneseJournal of Applied Physics,Vol.30, No.7, pp. 1525-1529 (1991) Summary of the Invention [Problem to be solved by the invention]
[0005] In a transistor, at least one of a gate electrode, a source electrode, and a drain electrode may be provided with a wiring provided on the electrode and a plug connecting the wiring and the electrode. For example, when a transistor is used in a high frequency band, it is required to reduce the gate resistance. On the other hand, there is a demand for miniaturization of transistors, and the cross-sectional area of the gate electrode is gradually becoming smaller. The smaller the cross-sectional area of the gate electrode, the higher the gate resistance. The gate resistance can be reduced by forming a wiring along the gate electrode in a wiring layer above the gate electrode and connecting the gate electrode to the wiring through a plug that penetrates a dielectric layer interposed between the wiring layer and the gate electrode.
[0006] However, the formation of a plug penetrating a dielectric layer has the following problems. When forming a plug, an opening is formed in the dielectric layer, and a metal material (e.g., tungsten) is embedded in the opening by using a film formation method such as thermal CVD. When the width of the plug is reduced by miniaturizing the electrode, the width of the opening is also reduced. If the aspect ratio of the opening (a value obtained by dividing the depth by the width) is large, the metal material does not sufficiently enter the opening, making it difficult to form the plug. Therefore, the dielectric layer must be formed thin to make the opening shallow, and in that case, it may be necessary to form the plug and wiring in a multi-layered manner. This increases the number of steps required to form the plug and wiring.
[0007] An object of the present disclosure is to provide a transistor that allows an aspect ratio of an opening into which a plug is embedded to be increased, and a method for manufacturing the transistor. [Means for solving the problem]
[0008] In order to solve the above-mentioned problems, a transistor according to one embodiment of the present disclosure includes a semiconductor laminate, a source electrode and a drain electrode provided on the semiconductor laminate, and a gate electrode provided between the source electrode and the drain electrode on the semiconductor laminate, a first polysilicon film provided on a first electrode which is one of the gate electrode, the source electrode and the drain electrode, a dielectric layer provided on the semiconductor laminate, covering the gate electrode, the source electrode, the drain electrode and the first polysilicon film and having a first opening formed on the first polysilicon film, a first plug containing tungsten, embedded in the first opening and in contact with the first polysilicon film, and a first wiring provided on the dielectric layer and in contact with the first plug. Effect of the Invention
[0009] According to the present disclosure, it is possible to provide a transistor that allows an aspect ratio of an opening into which a plug is embedded to be increased, and a method for manufacturing the transistor. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a cross-sectional view showing a configuration of a transistor according to an embodiment of the present disclosure. [Diagram 2] 2(a), (b) and (c) are cross-sectional views showing steps in a method for manufacturing a transistor. [Diagram 3] 3(a) and 3(b) are cross-sectional views showing steps in a method for manufacturing a transistor. [Figure 4] 4(a) and 4(b) are cross-sectional views showing steps in a method for manufacturing a transistor. [Diagram 5] 5(a), (b), and (c) are cross-sectional views showing steps in a method for manufacturing a transistor according to a reference example. [Figure 6] 6(a), 6(b) and 6(c) are cross-sectional views showing steps in a method for manufacturing a transistor according to a reference example. [Figure 7]7(a) and 7(b) are cross-sectional views showing steps in a method for manufacturing a transistor according to a reference example. [Figure 8] FIG. 8 is a plan view showing a wiring shape as a modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] [Description of the embodiments of the present disclosure] First, the contents of the embodiments of the present disclosure will be listed and described. [1] A transistor according to one aspect of the present disclosure includes a semiconductor laminate, a source electrode and a drain electrode provided on the semiconductor laminate, a gate electrode provided between the source electrode and the drain electrode on the semiconductor laminate, a first polysilicon film provided on a first electrode which is one of the gate electrode, the source electrode, and the drain electrode, a dielectric layer provided on the semiconductor laminate, covering the gate electrode, the source electrode, the drain electrode, and the first polysilicon film, and having a first opening formed on the first polysilicon film, a first plug including tungsten, embedded in the first opening, and in contact with the first polysilicon film, and a first wiring provided on the dielectric layer and in contact with the first plug.
[0012] This transistor includes a first polysilicon film on a first electrode, which is one of a gate electrode, a source electrode, and a drain electrode. When forming a first plug containing tungsten, polysilicon acts as a catalyst and has an effect of decomposing a tungsten material (e.g., WF6). Therefore, the material of the first plug containing tungsten selectively grows on the first polysilicon film exposed in the opening. Therefore, even if the aspect ratio of the opening is large, the material of the first plug can sufficiently enter the first opening, and the first plug can be suitably formed. Therefore, according to this transistor, the aspect ratio of the opening in which the first plug is embedded can be increased. As a result, the number of stages of the plug and the wiring can be reduced, and an increase in the number of steps for forming the plug and the wiring can be suppressed.
[0013] [2] In the transistor of [1] above, at least a portion of the first electrode that contacts the first polysilicon film may contain nickel in its composition. When the first polysilicon film is formed, the nickel in the first electrode acts to promote decomposition of the material of the first polysilicon film (e.g., SiH4). Therefore, the first polysilicon film can be easily formed.
[0014] [3] In the transistor of [2] above, at least a portion of the first electrode that is in contact with the first polysilicon film may be made of nickel only. In this case, decomposition of the material of the first polysilicon film is more effectively promoted. Therefore, the first polysilicon film can be formed more easily.
[0015] [4] In the transistor according to any one of [1] to [3] above, the first plug may be made of tungsten alone. In this case, the polysilicon acts as a catalyst to more suitably form the first plug in the first opening.
[0016] [5] In the transistor of any one of [1] to [4] above, the ratio (D / A) of the depth D to the opening width A of the first opening may be equal to or greater than 2. According to the transistor of any one of [1] to [4] above, the first plug can be embedded even in the first opening having such a large aspect ratio.
[0017] [6] Any one of the transistors [1] to [5] above may further include a second polysilicon film provided on the second electrode, which is the other of the gate electrode, the source electrode, and the drain electrode, and a third polysilicon film provided on the third electrode, which is the remaining of the gate electrode, the source electrode, and the drain electrode. The dielectric layer may further cover the second polysilicon film and the third polysilicon film, and may further include a second opening and a third opening formed on the second polysilicon film and the third polysilicon film, respectively. The transistor may further include a second plug containing tungsten, embedded in the second opening and in contact with the second polysilicon film, a third plug containing tungsten, embedded in the third opening and in contact with the third polysilicon film, and a second wiring and a third wiring provided on the dielectric layer and in contact with the second plug and the third plug, respectively. In this case, wiring and plugs can be provided for all electrodes, the gate electrode, the source electrode, and the drain electrode. For example, when a transistor is used in a high frequency band, it is required to reduce noise superimposed on a gate signal. Generally, the source electrode is connected to a reference potential line (GND line), so by sandwiching the wiring among the first wiring, the second wiring, and the third wiring that corresponds to the gate electrode between the wiring among the first wiring, the second wiring, and the third wiring that corresponds to the source electrode, it is possible to reduce noise superimposed on the gate signal.
[0018] [7] In the transistor of [6] above, at least a portion of the second electrode in contact with the second polysilicon film and at least a portion of the third electrode in contact with the third polysilicon film may contain nickel in their composition. When the second polysilicon film and the third polysilicon film are formed, the nickel in the second electrode and the third electrode acts to promote decomposition of the material (e.g., SiH4) of the second polysilicon film and the third polysilicon film, respectively. Therefore, the second polysilicon film and the third polysilicon film can be easily formed.
[0019] [8] In the transistor of [6] or [7] above, the gate electrode, the source electrode, and the drain electrode may contain nickel in their composition, and the semiconductor laminate may have a semiconductor layer containing a group III nitride semiconductor and in contact with the gate electrode, a first high-concentration n-type semiconductor region containing a group III nitride semiconductor and in contact with the source electrode, and a second high-concentration n-type semiconductor region containing a group III nitride semiconductor and in contact with the drain electrode. The electrode containing nickel in its composition forms a Schottky contact with a group III nitride semiconductor, such as GaN or AlGaN, which has a low dopant concentration or is undoped, but has a sufficiently low contact resistance with a high-concentration n-type group III nitride semiconductor, such as high-concentration n-type GaN. Therefore, according to the transistor of [8] above, even if the gate electrode, the source electrode, and the drain electrode contain nickel in their composition, a suitable contact form between these electrodes and the semiconductor laminate can be obtained. In addition, the nickel in the gate electrode, the source electrode, and the drain electrode acts to promote the decomposition of the materials (e.g., SiH4) of the first polysilicon film, the second polysilicon film, and the third polysilicon film.
[0020] [9] In the transistor of [8] above, the semiconductor laminate may have a channel layer provided between the first high-concentration n-type semiconductor region and the second high-concentration n-type semiconductor region, and an electron supply layer having a band gap larger than that of the channel layer. In this case, a high electron mobility transistor (HEMT) can be obtained.
[0021]
[10] A method for manufacturing a transistor according to one embodiment of the present disclosure includes an electrode formation step of forming a source electrode, a drain electrode, and a gate electrode located between the source electrode and the drain electrode on a semiconductor laminate; a polysilicon film formation step of forming a first polysilicon film on a first electrode that is one of the gate electrode, the source electrode, and the drain electrode; a dielectric layer formation step of forming a dielectric layer on the semiconductor laminate to cover the gate electrode, the source electrode, the drain electrode, and the first polysilicon film; an opening formation step of forming a first opening on the first polysilicon film in the dielectric layer; a plug formation step of forming a first plug in contact with the first polysilicon film by filling the first opening with a material containing tungsten; and a wiring formation step of forming a first wiring in contact with the first plug on the dielectric layer.
[0022] In this manufacturing method, in the electrode formation step, a first polysilicon film is formed on a first electrode, which is one of the gate electrode, source electrode, and drain electrode. When forming a first plug containing tungsten in the plug formation step, polysilicon acts as a catalyst and has the effect of decomposing a tungsten material (e.g., WF6). Therefore, the material of the first plug containing tungsten selectively grows on the first polysilicon film exposed in the opening. Therefore, even if the aspect ratio of the opening is large, the material of the first plug can sufficiently enter the first opening, and the first plug can be suitably formed. Therefore, according to this manufacturing method, the aspect ratio of the opening in which the first plug is embedded can be increased. As a result, the number of stages of the plug and the wiring can be reduced, and an increase in the number of steps for forming the plug and the wiring can be suppressed.
[0023]
[11] In the manufacturing method of
[10] above, in the electrode formation step, a first electrode containing nickel in its composition at least in a portion in contact with the first polysilicon film may be formed. When the first polysilicon film is formed, the nickel in the first electrode acts to promote decomposition of the material of the first polysilicon film (e.g., SiH4). Therefore, the first polysilicon film can be easily formed.
[0024]
[12] In the manufacturing method of
[11] above, in the electrode forming step, the first electrode may be formed such that at least a portion in contact with the first polysilicon film is made of only nickel. In this case, decomposition of the material of the first polysilicon film is more effectively promoted. Therefore, the first polysilicon film can be formed more easily.
[0025]
[13] In the manufacturing method of
[11] or
[12] above, in the polysilicon film forming step, SiH4 may be used as a film forming source, and the first polysilicon film may be formed at room temperature. When SiH4 is used as the film forming source, nickel in the first electrode acts more effectively, and the decomposition of the material (SiH4) of the first polysilicon film is further promoted. Therefore, the first polysilicon film can be easily formed at room temperature.
[0026]
[14] In any one of the manufacturing methods
[10] to
[13] above, in the plug forming step, the first plug may be formed only from tungsten. In this case, polysilicon serves as a catalyst to more suitably form the first plug in the first opening.
[0027]
[15] In any one of the manufacturing methods
[10] to
[14] above, in the opening formation step, the ratio (D / A) of the depth D to the opening width A of the first opening may be equal to or greater than 2. According to any one of the manufacturing methods
[10] to
[14] above, the first plug can be embedded even in the first opening having such a large aspect ratio.
[0028]
[16] In any one of the manufacturing methods
[10] to
[15] above, in the polysilicon film forming step, a second polysilicon film is further formed on the second electrode, which is the other of the gate electrode, the source electrode, and the drain electrode, and a third polysilicon film is further formed on the third electrode, which is the remaining of the gate electrode, the source electrode, and the drain electrode, in the dielectric layer forming step, a dielectric layer is further formed to cover the second polysilicon film and the third polysilicon film, in the opening forming step, a second opening is further formed on the second polysilicon film and a third opening is further formed on the third polysilicon film in the dielectric layer, in the plug forming step, a material containing tungsten is further embedded in the second opening and the third opening to further form a second plug in contact with the second polysilicon film and a third plug in contact with the third polysilicon film, and in the wiring forming step, a second wiring in contact with the second plug and a third wiring in contact with the third plug may be further formed on the dielectric layer. In this case, wiring and plugs can be provided for all of the electrodes, the gate electrode, the source electrode, and the drain electrode. For example, by sandwiching the wiring among the first wiring, the second wiring, and the third wiring that corresponds to the gate electrode between the wiring among the first wiring, the second wiring, and the third wiring that corresponds to the source electrode, it is possible to reduce noise superimposed on the gate signal.
[0029]
[17] In the manufacturing method of
[16] above, in the electrode formation step, a second electrode containing nickel in its composition at least in a portion in contact with the second polysilicon film, and a third electrode containing nickel in its composition at least in a portion in contact with the third polysilicon film may be formed. When the second polysilicon film and the third polysilicon film are formed, the nickel in the second electrode and the third electrode act to promote decomposition of the material (e.g., SiH4) of the second polysilicon film and the third polysilicon film, respectively. Therefore, the second polysilicon film and the third polysilicon film can be easily formed.
[0030]
[18] In the manufacturing method of the above
[16] or
[17] , the semiconductor laminate may have a semiconductor layer containing a group III nitride semiconductor, a first high-concentration n-type semiconductor region containing a group III nitride semiconductor, and a second high-concentration n-type semiconductor region containing a group III nitride semiconductor, and in the electrode forming step, a gate electrode, a source electrode, and a drain electrode each containing nickel in their composition may be formed, the gate electrode may be in Schottky contact with the semiconductor layer, the source electrode may be in contact with the first high-concentration n-type semiconductor region, and the drain electrode may be in contact with the second high-concentration n-type semiconductor region. The electrode containing nickel in its composition may form a Schottky contact with a group III nitride semiconductor, such as GaN or AlGaN, which has a low dopant concentration or is undoped, but has a sufficiently low contact resistance with a high-concentration n-type group III nitride semiconductor, such as high-concentration n-type GaN. Therefore, according to the manufacturing method of the above
[18] , even if the gate electrode, source electrode, and drain electrode contain nickel in their composition, a suitable contact form between these electrodes and the semiconductor laminate may be obtained. In addition, nickel in the gate electrode, source electrode, and drain electrode acts to promote decomposition of the materials (eg, SiH4) of the first polysilicon film, the second polysilicon film, and the third polysilicon film, respectively.
[0031]
[19] In the manufacturing method of
[18] above, the semiconductor laminate may have a channel layer provided between the first high-concentration n-type semiconductor region and the second high-concentration n-type semiconductor region, and an electron supply layer having a band gap larger than that of the channel layer. In this case, a high electron mobility transistor (HEMT) can be obtained.
[0032] [Details of the embodiment of the present disclosure] Specific examples of the transistor and the method for manufacturing the transistor according to the present embodiment will be described with reference to the drawings as necessary. Note that the present invention is not limited to these examples, but is indicated by the claims, and is intended to include all modifications within the meaning and scope equivalent to the claims. In the following description, the same elements in the description of the drawings are given the same reference numerals, and duplicated descriptions will be omitted.
[0033] FIG. 1 is a cross-sectional view showing a configuration of a transistor 10 according to an embodiment of the present disclosure. For convenience of explanation, an XYZ orthogonal coordinate system is also shown in FIG. 1. The transistor 10 of this embodiment is a high electron mobility transistor (HEMT) mainly including a group III nitride semiconductor such as GaN and AlGaN. The transistor 10 is used in a power amplifier (for example, a power amplifier for a mobile base station) because of its characteristics such as low noise, high gain at high frequencies, and high breakdown voltage. The transistor 10 is used in a high frequency band, for example, from 10 GHz to 80 GHz. The transistor 10 includes a substrate 20, a semiconductor laminate 30, a gate electrode 41, a source electrode 42, a drain electrode 43, polysilicon films 51, 52, and 53, dielectric layers 61 and 62, plugs 71, 72, and 73, and wirings 81, 82, 83, and 84.
[0034] The substrate 20 is a plate-like member having a main surface 21 and a back surface 22. The substrate 20 is a substrate for crystal growth. The substrate 20 may be a semiconductor substrate. The substrate 20 is, for example, a SiC substrate or a GaN substrate. The substrate 20 may be made of a material other than a semiconductor, for example, sapphire. The thickness direction of the substrate 20 is along the Z direction, and the main surface 21 and the back surface 22 extend along the X direction and the Y direction.
[0035] The semiconductor laminate 30 has a channel layer 31, an electron supply layer (barrier layer) 32, a first high concentration n-type semiconductor region 33, and a second high concentration n-type semiconductor region 34. The channel layer 31 is a semiconductor layer epitaxially grown on the primary surface 21 of the substrate 20. The channel layer 31 mainly contains a Group III nitride semiconductor such as gallium nitride (GaN), and in one example, is made only of a Group III nitride semiconductor. The thickness of the channel layer 31 is, for example, not less than 1000 nm and not more than 3000 nm.
[0036] The electron supply layer 32 is a semiconductor layer epitaxially grown on the channel layer 31, and has a larger band gap than the channel layer 31. The stacking direction of the channel layer 31 and the electron supply layer (barrier layer) 32 is along the Z direction. The electron supply layer 32 mainly contains a group III nitride semiconductor, and in one example, is made of only a group III nitride semiconductor except for n-type impurities. Examples of such group III nitride semiconductors include AlGaN and InAlN. The thickness of the electron supply layer 32 is, for example, 10 nm or more and 30 nm or less. A two-dimensional electron gas (2DEG) is generated at the interface between the channel layer 31 and the electron supply layer 32 due to the piezoelectric effect. As a result, a channel region 31a is formed in the vicinity of the surface of the channel layer 31 on the electron supply layer 32 side. The electron supply layer 32 is a low-concentration n-type or undoped. The n-type impurity concentration of the electron supply layer 32 is, for example, 0 cm -3 Over 10 16 cm -3 The following is the result.
[0037] The first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34 are regions epitaxially grown in recesses 30a, 30b formed by etching the electron supply layer 32 or the electron supply layer 32 plus a part of the channel layer 31. The first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34 mainly contain a high-concentration n-type Group III nitride semiconductor, and in one example, are made only of a high-concentration n-type Group III nitride semiconductor. The first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34 are made only of a high-concentration n-type GaN, for example. The n-type impurity is, for example, silicon (Si). The n-type impurity concentrations of the first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34 are, for example, 10 19 cm -3 Over 10 21 cm -3 The following is the result.
[0038] The second high-concentration n-type semiconductor region 34 is arranged in a direction (for example, the X direction) intersecting the stacking direction of the channel layer 31 and the electron supply layer 32 with respect to the first high-concentration n-type semiconductor region 33. A part of the channel layer 31 and the electron supply layer 32 are provided between the first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34. The thickness of the first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34 is equal to or greater than the thickness of the electron supply layer 32 and is smaller than the combined thickness of the electron supply layer 32 and the channel layer 31. Therefore, the side surfaces of the first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34 are in contact with the channel region 31a. The thickness of the first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34 is, for example, 20 nm or more and 100 nm or less.
[0039] The dielectric layer 61 is provided on the semiconductor laminate 30 and covers the surface of the semiconductor laminate 30. The dielectric layer 61 mainly includes an inorganic dielectric. The dielectric layer 61 mainly includes a silicon compound, such as silicon nitride (SiN), silicon oxide (SiO2), or silicon oxynitride (SiON). In one embodiment, the dielectric layer 61 is made of only SiN, SiO2, or SiON. The dielectric layer 61 has a gate opening 61a for the gate electrode 41, a source opening 61b for the source electrode 42, and a drain opening 61c for the drain electrode 43. The gate opening 61a is provided on the electron supply layer 32. A first high concentration n-type semiconductor region 33 is embedded in the source opening 61b. A second high concentration n-type semiconductor region 34 is embedded in the drain opening 61c.
[0040] The gate electrode 41, the source electrode 42, and the drain electrode 43 are provided on the semiconductor laminate portion 30. The gate electrode 41 is located between the source electrode 42 and the drain electrode 43 in the X direction. The gate electrode 41, the source electrode 42, and the drain electrode 43 extend along a direction (e.g., Y direction) intersecting the arrangement direction (e.g., X direction). The gate electrode 41 is embedded in the gate opening 61a and has a T-shaped cross section. The gate electrode 41 contacts the electron supply layer 32 through the gate opening 61a. The gate electrode 41 forms a Schottky contact with the electron supply layer 32.
[0041] At least a portion of the gate electrode 41 in contact with the electron supply layer 32 contains a material that forms a Schottky contact with the electron supply layer 32. The material that forms a Schottky contact with the group III nitride semiconductor of the electron supply layer 32 is, for example, nickel (Ni). Also, a portion of the gate electrode 41 that constitutes the surface opposite to the electron supply layer 32, in other words, at least a portion of the gate electrode 41 that contacts the polysilicon film 51 contains Ni. In one embodiment, at least the portion of the gate electrode 41 that contacts the polysilicon film 51 consists of only Ni. Alternatively, in another embodiment, the entire gate electrode 41 contains Ni in its composition or consists of only Ni.
[0042] The source electrode 42 is provided on the first high-concentration n-type semiconductor region 33 exposed from the source opening 61b, and is in contact with the first high-concentration n-type semiconductor region 33. At least a portion of the source electrode 42 in contact with the first high-concentration n-type semiconductor region 33 contains a material that forms a low contact resistance with the first high-concentration n-type semiconductor region 33. The material that forms a low contact resistance with the high-concentration n-type III nitride semiconductor of the first high-concentration n-type semiconductor region 33 is, for example, Ni. In addition, a portion of the source electrode 42 that forms a surface opposite to the first high-concentration n-type semiconductor region 33, in other words, at least a portion of the source electrode 42 that contacts the polysilicon film 52 contains Ni. In one embodiment, at least a portion of the source electrode 42 that contacts the polysilicon film 52 is made of only Ni. Alternatively, in another embodiment, the entire source electrode 42 contains Ni in its composition or is made of only Ni. The source electrode 42 may be provided on a recess formed by etching a part of the first high-concentration n-type semiconductor region 33.
[0043] The drain electrode 43 is provided on the second high-concentration n-type semiconductor region 34 exposed from the drain opening 61c, and is in contact with the second high-concentration n-type semiconductor region 34. At least a portion of the drain electrode 43 in contact with the second high-concentration n-type semiconductor region 34 contains a material that forms a low contact resistance with the second high-concentration n-type semiconductor region 34. The material that forms a low contact resistance with the high-concentration n-type III nitride semiconductor of the second high-concentration n-type semiconductor region 34 is, for example, Ni. In addition, a portion of the drain electrode 43 that forms a surface opposite to the second high-concentration n-type semiconductor region 34, in other words, at least a portion of the drain electrode 43 that contacts the polysilicon film 53 contains Ni. In one embodiment, at least a portion of the drain electrode 43 that contacts the polysilicon film 53 is made of only Ni. Alternatively, in another embodiment, the entire drain electrode 43 contains Ni in its composition or is made of only Ni. The drain electrode 43 may be provided on a recess formed by etching a part of the second high-concentration n-type semiconductor region 34.
[0044] In this embodiment, one of the gate electrode 41, the source electrode 42, and the drain electrode 43 corresponds to a first electrode in this disclosure. The remaining two of the gate electrode 41, the source electrode 42, and the drain electrode 43 correspond to a second electrode and a third electrode in this disclosure.
[0045] The polysilicon film 51 is provided on the gate electrode 41. The polysilicon film 52 is provided on the source electrode 42. The polysilicon film 53 is provided on the drain electrode 43. In this manner, the polysilicon films 51, 52, and 53 are selectively formed on the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. Moreover, the polysilicon films 51, 52, and 53 overlap the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively, in a plan view, without protruding from or being missing from the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. The polysilicon films 51, 52, and 53 extend in the Y direction along the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively.
[0046] The polysilicon films 51, 52, and 53 are electrically isolated from each other. The polysilicon films 51, 52, and 53 are made of only polysilicon (polycrystalline silicon). In one example, the polysilicon films 51, 52, and 53 are in contact with the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. The thickness of the polysilicon films 51, 52, and 53 is, for example, 5 nm or more and 10 nm or less.
[0047] In this embodiment, the polysilicon film provided on the first electrode among the polysilicon films 51, 52, and 53 corresponds to the first polysilicon film in this disclosure. The polysilicon film provided on the second electrode among the polysilicon films 51, 52, and 53 corresponds to the second polysilicon film in this disclosure. The polysilicon film provided on the third electrode among the polysilicon films 51, 52, and 53 corresponds to the third polysilicon film in this disclosure.
[0048] The dielectric layer 62 is provided on the semiconductor laminate 30 and on the dielectric layer 61. The dielectric layer 62 covers the gate electrode 41, the source electrode 42, the drain electrode 43, and the polysilicon films 51, 52, and 53. The dielectric layer 62 mainly contains an inorganic dielectric. The dielectric layer 62 mainly contains a silicon compound, for example, silicon nitride (SiN), silicon oxide (SiO2), or silicon oxynitride (SiON). In one embodiment, the dielectric layer 62 is made of only SiN, SiO2, or SiON. The dielectric layer 62 may be made of the same material as the dielectric layer 61.
[0049] The dielectric layer 62 has an opening (contact hole) 62a formed on the polysilicon film 51, an opening (contact hole) 62b formed on the polysilicon film 52, and an opening (contact hole) 62c formed on the polysilicon film 53. In a plan view, the openings 62a, 62b, and 62c extend in the Y direction along the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. The openings 62a, 62b, and 62c penetrate the dielectric layer 62 in the thickness direction (Z direction) of the dielectric layer 62. In other words, one end of each of the openings 62a, 62b, and 62c in the thickness direction (Z direction) of the dielectric layer 62 reaches the polysilicon films 51, 52, and 53, respectively. The other end of each of the openings 62a, 62b, and 62c in the thickness direction (Z direction) of the dielectric layer 62 reaches the surface of the dielectric layer 62 on the opposite side to the dielectric layer 61. The width of the openings 62a, 62b and 62c in the X direction gradually narrows from the surface of the dielectric layer 62 toward the polysilicon films 51, 52 and 53.
[0050] The depth D of the openings 62a, 62b, and 62c is, for example, 1000 nm or more and 4000 nm or less. The opening width A of the openings 62a, 62b, and 62c is, for example, 500 nm or more and 2000 nm or less. The opening width A here means the average value of the width in the X direction of the openings 62a, 62b, and 62c at one end (i.e., one end located on the surface of the dielectric layer 62) opposite the polysilicon films 51, 52, and 53 among both ends of the openings 62a, 62b, and 62c in the thickness direction (Z direction) of the dielectric layer 62, over the Y direction. The aspect ratio (D / A) of the openings 62a, 62b, and 62c is, for example, 2 or more and 8 or less.
[0051] In this embodiment, the openings 62a, 62b, and 62c formed on the first polysilicon film correspond to the first opening in this disclosure. The openings 62a, 62b, and 62c formed on the second polysilicon film correspond to the second polysilicon film in this disclosure. The openings 62a, 62b, and 62c formed on the third polysilicon film correspond to the third opening in this disclosure.
[0052] The plugs 71, 72, and 73 are embedded in the openings 62a, 62b, and 62c, respectively, and contact the polysilicon films 51, 52, and 53, respectively. In a plan view, the plugs 71, 72, and 73 extend in the Y direction along the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. The plugs 71, 72, and 73 are made of metal and contain tungsten (W). In one example, the plugs 71, 72, and 73 are made only of W. In the thickness direction (Z direction) of the dielectric layer 62, one end of each of the plugs 71, 72, and 73 contacts the polysilicon films 53, 54, and 55, respectively, and the other end of each of the plugs 71, 72, and 73 is exposed from the dielectric layer 62.
[0053] In this embodiment, the plug embedded in the first opening among the plugs 71, 72, and 73 corresponds to the first plug in this disclosure. The plug embedded in the second opening among the plugs 71, 72, and 73 corresponds to the second plug in this disclosure. The plug embedded in the third opening among the plugs 71, 72, and 73 corresponds to the third plug in this disclosure.
[0054] The wirings 81, 82, and 83 are metal films and are provided on the dielectric layer 62. The wirings 81, 82, and 83 contact the other ends of the wirings 71, 72, and 73, respectively. As a result, the wirings 81, 82, and 83 are electrically connected to the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. The wirings 81, 82, and 83 contain, for example, aluminum (Al), and in one example, are made of only Al. In a plan view, the wirings 81, 82, and 83 extend in the Y direction along the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. The thickness of the wirings 81, 82, and 83 is, for example, 1000 nm or more and 5000 nm or less.
[0055] The wiring 84 is a metal film, and is provided on the rear surface 22 of the substrate 20. The wiring 84 fills an opening 91 that extends from the rear surface 22 of the substrate 20 to the source electrode 42, and is in contact with the source electrode 42 to be electrically connected to the source electrode 42. The wiring 84 is made of a metal such as gold (Au).
[0056] A method for manufacturing the transistor 10 of this embodiment having the above configuration will be described below. Figures 2, 3, and 4 are cross-sectional views illustrating the steps in the method for manufacturing the transistor 10.
[0057] First, as shown in part (a) of FIG. 2, the channel layer 31 and the electron supply layer 32 are epitaxially grown in sequence on the main surface 21 of the substrate 20. Next, the dielectric layer 61 is formed on the electron supply layer 32 by, for example, chemical vapor deposition (CVD). A first resist pattern having openings corresponding to the source electrode 42 and the drain electrode 43 is formed on the dielectric layer 61 by photolithography. Using this first resist pattern as a mask, a source opening 61b and a drain opening 61c are formed in the dielectric layer 61 by reactive ion etching. Furthermore, by continuing the reactive ion etching, recesses 30a and 30b are formed that penetrate the electron supply layer 32 and reach the channel layer 31. The semiconductor materials of the first high concentration n-type semiconductor region 33 and the second high concentration n-type semiconductor region 34 are selectively regrown in the recesses 30a and 30b to form the first high concentration n-type semiconductor region 33 and the second high concentration n-type semiconductor region 34. As a result, a semiconductor laminate 30 having a channel layer 31, an electron supply layer 32, a first high concentration n-type semiconductor region 33, and a second high concentration n-type semiconductor region 34 is formed. After that, the first resist pattern is removed using an organic solvent. Through the above steps, the semiconductor laminate 30 is formed. Using a lift-off method, a source electrode 42 is formed on the first high concentration n-type semiconductor region 33, and a drain electrode 43 is formed on the second high concentration n-type semiconductor region 34 (electrode formation step). Using a photolithography method, a second resist pattern having an opening corresponding to the gate electrode 41 is formed on the dielectric layer 61. Using this second resist pattern as a mask, a gate opening 61a of the dielectric layer 61 is formed by reactive ion etching. After that, the second resist pattern is removed using an organic solvent. Using a lift-off method, a gate electrode 41 is formed by, for example, a vacuum deposition method from above the electron supply layer 32 in the gate opening 61a to above the surrounding dielectric layer 61 (electrode formation step).
[0058] Next, as shown in FIG. 2(b), polysilicon is selectively deposited on the gate electrode 41, the source electrode 42, and the drain electrode 43 to form polysilicon films 51, 52, and 53 (polysilicon film formation process). In this process, a polysilicon material, for example, monosilane (SiH4), is introduced into a chamber for plasma CVD. At this time, on the surface of a metal containing Ni (or consisting only of Ni), the polysilicon material (for example, SiH4) decomposes at room temperature (see Non-Patent Document 1). As described above, at least the portion of the gate electrode 41 that contacts the polysilicon film 51, at least the portion of the source electrode 42 that contacts the polysilicon film 52, and at least the portion of the drain electrode 43 that contacts the polysilicon film 53 contain Ni, so that polysilicon is selectively deposited on the gate electrode 41, the source electrode 42, and the drain electrode 43 at room temperature.
[0059] 2(c), a dielectric layer 62 covering the gate electrode 41, the source electrode 42, the drain electrode 43, and the polysilicon films 51, 52, and 53 is formed on the semiconductor laminate 30 (dielectric layer formation process). In this process, the dielectric layer 62 is formed by, for example, a plasma CVD method. The uneven shape on the semiconductor laminate 30 caused by the gate electrode 41, the source electrode 42, the drain electrode 43, and the polysilicon films 51, 52, and 53 is transferred to the surface of the dielectric layer 62. Thereafter, the surface of the dielectric layer 62 is planarized by a chemical mechanical polishing (CMP) method.
[0060] 3(a), in the dielectric layer 62, an opening 62a reaching the polysilicon film 51 is formed on the polysilicon film 51, an opening 62b reaching the polysilicon film 52 is formed on the polysilicon film 52, and an opening 62c reaching the polysilicon film 53 is formed on the polysilicon film 53 (opening formation process). In this process, the openings 62a, 62b, and 62c are formed by anisotropic etching such as dry etching. When the dielectric layer 62 contains a silicon compound, the etching gas is, for example, a fluorine-based gas. As described above, the aspect ratio (D / A) of the openings 62a, 62b, and 62c is, for example, 2 or more and 8 or less.
[0061] 3(b), a material containing W is embedded in the openings 62a, 62b, and 62c to form a plug 71 in contact with the polysilicon film 51, a plug 72 in contact with the polysilicon film 52, and a plug 73 in contact with the polysilicon film 53 (plug formation step). At this time, the polysilicon contained in the polysilicon films 51, 52, and 53 serves as a catalyst to decompose the W material (e.g., WF6) according to the following reaction formula (1) (see Non-Patent Document 2). WF6+3Si→W+3SiF2 (1) Therefore, the material of the W-containing plugs 71, 72, and 73 selectively grows on the polysilicon films 51, 52, and 53 exposed in the openings 62a, 62b, and 62c, respectively. Therefore, the material of the plugs 71, 72, and 73 hardly grows on the dielectric layer 62 except in the openings 62a, 62b, and 62c.
[0062] 4(a), wirings 81, 82, and 83, which are in contact with the plugs 71, 72, and 73, respectively, are formed on the dielectric layer 62 (wiring formation process). In this process, the metal material (e.g., Al) of the wirings 81, 82, and 83 is uniformly formed on the dielectric layer 62 by, for example, a sputtering method, and then a resist mask is formed on the metal film by photolithography, and unnecessary portions of the metal film are removed by dry etching. The etching gas is, for example, chlorine gas.
[0063] 4(b), the rear surface 22 of the substrate 20 is polished to reduce the thickness of the substrate 20, and then an opening 91 extending from the rear surface 22 of the substrate 20 to the source electrode 42 is formed in the substrate 20 and the semiconductor laminate portion 30. In this step, the opening 91 is formed by anisotropic etching such as dry etching. Then, the wiring 84 is formed over the entire surface of the rear surface 22, and the opening 91 is filled with the metal material of the wiring 84. Through the above steps, the transistor 10 of this embodiment is fabricated.
[0064] The effects obtained by the transistor 10 of this embodiment having the above configuration and the manufacturing method thereof will be described below based on a comparison with a reference example. Figures 5, 6, and 7 are cross-sectional views showing each step in the manufacturing method of the transistor according to the reference example.
[0065] 5(a), a channel layer 31 and an electron supply layer 32 are sequentially grown on the main surface 21 of a substrate 20. Next, a dielectric layer 61 is formed on the electron supply layer 32. After a source opening 61b and a drain opening 61c are formed in the dielectric layer 61, recesses 30a and 30b are formed. The above steps are the same as those in the manufacturing method of the transistor 10.
[0066] Thereafter, the source electrode 45 and the drain electrode 46 are formed by a vacuum deposition method and a lift-off method using the resist mask used for forming the recesses 30a and 30b as it is. Specifically, titanium (Ti) layers 451 and 461 for ohmic contact are formed inside the recesses 30a and 30b, respectively. Next, aluminum (Al) layers 452 and 462 are formed on the Ti layers 451 and 461, respectively. Then, molybdenum (Mo) layers 453 and 463 are formed on the Al layers 452 and 462, respectively. Gold (Au) layers 454 and 464 are formed on the Mo layers 453 and 463, respectively. The Ti layer 451, the Al layer 452, the Mo layer 453, and the Au layer 454 constitute the source electrode 45. The Ti layer 461, the Al layer 462, the Mo layer 463, and the Au layer 464 constitute the drain electrode 46.
[0067] Next, a gate opening 61a is formed in the dielectric layer 61. A Ni layer 441, which will become a part of the gate electrode 41, is formed by vacuum deposition on the electron supply layer 32 in the gate opening 61a. The Ni layer 441 forms a Schottky contact with the electron supply layer 32. Next, an Au layer 442, which will become the remaining part of the gate electrode 41, is formed by vacuum deposition on the Ni layer 441. The Au layer 442 reduces the resistance between the Ni layer 441 and the plug 71. Unnecessary Ni and Au around the gate electrode 41 are removed by lift-off.
[0068] Next, as shown in FIG. 5B, a dielectric layer 62 covering the gate electrode 44, the source electrode 45, and the drain electrode 46 is formed on the dielectric layer 61. Then, as shown in FIG. 5C, the surface of the dielectric layer 62 is planarized by using a CMP method. As shown in FIG. 6A, in the dielectric layer 62, openings 62a, 62b, and 62c reaching the Au layers 442, 454, and 464, respectively, are formed on the Au layers 442, 454, and 464, respectively. In the reference example, the aspect ratio (D / A) of the openings 62a, 62b, and 62c is about 1. As shown in FIG. 6B, a W film 74 is uniformly formed on the dielectric layer 62 by thermal CVD using WF6 gas as a raw material gas. At this time, W is generated by the following reaction formula (2) between the raw material gas WF6 and the reducing gas H2. WF6+3H2→W+6HF (2) The W film 74 is also embedded in the openings 62a, 62b, and 62c, and is in contact with the Au layers 442, 454, and 464. Thereafter, in order to remove the portion of the W film 74 deposited on the region on the dielectric layer 62 excluding the openings 62a, 62b, and 62c, the W film 74 is etched back by isotropic etching using, for example, a fluorine-based gas, as shown in Fig. 6(c). As a result, a plug 71 in contact with the Au layer 442, a plug 72 in contact with the Au layer 454, and a plug 73 in contact with the Au layer 464 remain.
[0069] 7(a), wirings 81, 82, and 83 in contact with plugs 71, 72, and 73, respectively, are formed on dielectric layer 62. As shown in part (b) of FIG. 7, rear surface 22 of substrate 20 is polished to reduce the thickness of substrate 20, and then opening 91 is formed from rear surface 22 of substrate 20 to source electrode 42. Then, wiring 84 is formed over the entire surface of rear surface 22, and opening 91 is filled with the metal material of wiring 84.
[0070] The manufacturing method of the transistor according to the reference example has the following problems. When the width of the plugs 71, 72, and 73 is reduced by miniaturizing the gate electrode 44, the source electrode 45, and the drain electrode 46 (particularly the gate electrode 44), the width of the openings 62a, 62b, and 62c is also reduced. If the aspect ratio of the openings 62a, 62b, and 62c is large, WF6 gas does not sufficiently enter the openings 62a, 62b, and 62c when forming the W film 74, and gaps are formed between the plugs 71, 72, and 73 and the Au layers 442, 454, and 464. Therefore, the dielectric layer 62 must be formed thin to make the openings 62a, 62b, and 62c shallow (i.e., to reduce the aspect ratio), and in that case, it may be necessary to form the plugs 71, 72, and 73 and the wirings 81, 82, and 83 in a multi-stage stack. This results in an increase in the number of steps required to form the plugs 71, 72, and 73 and the wirings 81, 82, and 83.
[0071] Furthermore, when the W film 74 is formed on the dielectric layer 62 by thermal CVD using WF6 gas as a raw material gas, HF vapor is generated as a by-product. The HF vapor corrodes the silicon compound of the dielectric layer 62, which impairs the flatness of the surface of the dielectric layer 62. In addition, the fluorine-based gas used to etch back the W film 74 also corrodes the silicon compound of the dielectric layer 62, so that the etch back needs to be stopped when the dielectric layer 62 is exposed, making it difficult to control the etching time.
[0072] In response to the above problem, in the manufacturing method of this embodiment, in the electrode formation step, polysilicon films 51, 52, and 53 are formed on the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. In addition, the transistor 10 of this embodiment includes polysilicon films 51, 52, and 53 on the gate electrode 41, the source electrode 42, and the drain electrode 43, respectively. As described above, when forming the plugs 71, 72, and 73 containing W, polysilicon serves as a catalyst to decompose the material of W (e.g., WF6). Therefore, the material of the plugs 71, 72, and 73 containing W selectively grows on the polysilicon films 51, 52, and 53 exposed in the openings 62a, 62b, and 62c. Therefore, even if the aspect ratios of the openings 62a, 62b, and 62c are large, the material of the plugs 71, 72, and 73 can sufficiently enter the openings 62a, 62b, and 62c, and the plugs 71, 72, and 73 can be suitably formed. Therefore, according to the transistor 10 and the manufacturing method thereof of the present embodiment, it is possible to increase the aspect ratio of the openings 62a, 62b, and 62c into which the plugs 71, 72, and 73 are embedded. As a result, the number of stages of the plugs 71, 72, and 73 and the wirings 81, 82, and 83 can be reduced, and an increase in the number of steps for forming the plugs 71, 72, and 73 and the wirings 81, 82, and 83 can be suppressed.
[0073] In addition, in W film formation using polysilicon as a catalyst, HF vapor is not generated as shown in the above-mentioned reaction formula (1). Therefore, it is possible to prevent the flatness of the surface of the dielectric layer 62 from being impaired. Furthermore, by using polysilicon as a catalyst, the material of the plugs 71, 72, and 73 is selectively deposited in the openings 62a, 62b, and 62c, and is hardly deposited on the dielectric layer 62 except for the openings 62a, 62b, and 62c. This makes it possible to eliminate the need to etch back the W film.
[0074] As in this embodiment, at least the portions of the gate electrode 41, source electrode 42, and drain electrode 43 in contact with the polysilicon films 51, 52, and 53 may contain Ni in their composition. Similarly, in the electrode formation step, the gate electrode 41, source electrode 42, and drain electrode 43 may be formed so that at least the portions in contact with the polysilicon films 51, 52, and 53 contain Ni in their composition. When forming the polysilicon films 51, 52, and 53, Ni in the gate electrode 41, source electrode 42, and drain electrode 43 acts to promote decomposition of the material (e.g., SiH4) of the polysilicon films 51, 52, and 53. Therefore, the polysilicon films 51, 52, and 53 can be easily formed.
[0075] As in this embodiment, at least the portions of the gate electrode 41, source electrode 42, and drain electrode 43 that are in contact with the polysilicon films 51, 52, and 53, respectively, may be made of only Ni. Similarly, in the electrode formation step, the gate electrode 41, source electrode 42, and drain electrode 43 may be formed such that at least the portions in contact with the polysilicon films 51, 52, and 53, respectively, are made of only Ni. In this case, decomposition of the material of the polysilicon films 51, 52, and 53 is more effectively promoted. Thus, the polysilicon films 51, 52, and 53 can be formed more easily.
[0076] As in this embodiment, in the polysilicon film formation process, SiH4 may be used as a film-forming raw material, and polysilicon films 51, 52, and 53 may be formed at room temperature. When SiH4 is used as a film-forming raw material, Ni in gate electrode 41, source electrode 42, and drain electrode 43 acts more effectively, and decomposition of the material (SiH4) of polysilicon films 51, 52, and 53 is further promoted. Therefore, polysilicon films 51, 52, and 53 can be easily formed at room temperature.
[0077] As in this embodiment, the plugs 71, 72, and 73 may be made of only W. Similarly, in the plug formation step, the plugs 71, 72, and 73 may be formed of only W. In this case, polysilicon serves as a catalyst, and the plugs 71, 72, and 73 can be more suitably formed inside the openings 62a, 62b, and 62c, respectively.
[0078] As in this embodiment, the ratio (D / A) of the depth D to the opening width A of openings 62a, 62b, and 62c may be equal to or greater than 2. Similarly, in the opening formation step, the ratio (D / A) of the depth D to the opening width A of openings 62a, 62b, and 62c may be equal to or greater than 2. According to transistor 10 and its manufacturing method of this embodiment, plugs 71, 72, and 73 can be embedded even in openings 62a, 62b, and 62c having such a large aspect ratio.
[0079] As in this embodiment, the gate electrode 41, the source electrode 42, and the drain electrode 43 may contain Ni in their composition, and the semiconductor laminate 30 may have an electron supply layer 32 containing a group III nitride semiconductor and in contact with the gate electrode 41, a first high-concentration n-type semiconductor region 33 containing a group III nitride semiconductor and in contact with the source electrode 42, and a second high-concentration n-type semiconductor region 34 containing a group III nitride semiconductor and in contact with the drain electrode 43. An electrode containing Ni in its composition forms a Schottky contact with, for example, a group III nitride semiconductor having a low dopant concentration or being undoped, but has a sufficiently low contact resistance with a high-concentration n-type group III nitride semiconductor such as high-concentration n-type GaN. Therefore, according to the transistor 10 of this embodiment, even if the gate electrode 41, the source electrode 42, and the drain electrode 43 contain Ni in their composition, a suitable contact form between these electrodes and the semiconductor laminate 30 can be obtained.
[0080] As in this embodiment, the semiconductor laminate 30 may have a channel layer 31 provided between the first high-concentration n-type semiconductor region 33 and the second high-concentration n-type semiconductor region 34, and an electron supply layer 32 having a band gap larger than that of the channel layer 31. In this case, a HEMT can be obtained. [Variations]
[0081] Fig. 8 is a plan view showing the wiring shape as a modified example of the above embodiment. In Fig. 8, two transistors 10A are arranged side by side in the X direction. Each transistor 10A is different from the transistor 10 of the above embodiment in that it includes a wiring 82A instead of the wiring 82, and includes a gate wiring 85 and a drain wiring 86, but is the same as the transistor 10 of the above embodiment in other respects. The drain electrodes 43 (see Fig. 1) and wiring 83 of the transistors 10A are common to each other.
[0082] The gate wiring 85 and the drain wiring 86 are a metal (e.g., Al) film provided on the dielectric layer 62. The gate wiring 85 and the drain wiring 86 extend in the X direction across the two transistors 10. The gate wiring 85 and the drain wiring 86 are provided at positions sandwiching the two transistors 10 in a plan view. One end in the Y direction of the wiring 81 corresponding to the gate electrode 41 is connected to the gate wiring 85. One end in the Y direction of the wiring 83 corresponding to the drain electrode 43 is connected to the gate wiring 85. The gate wiring 85 and the drain wiring 86 may be formed simultaneously with the wirings 81, 82A, and 83 in a wiring formation step.
[0083] The wiring 82A differs from the wiring 82 of the above embodiment in planar shape, but is the same as the wiring 82 in other respects. The wiring 82A includes a wiring portion 821 extending along the source electrode 42, and a wiring portion 822 provided between the wiring 81 and the wiring 83 and extending in the Y direction. The wiring portion 821 and the wiring portion 822 are integrally connected near the other end of the wiring 81, so that the wiring 82A has a planar shape such as a U-shape. In other words, the wiring 82A surrounds the wiring 81 on three sides.
[0084] Generally, the wiring 84 provided on the rear surface 22 of the substrate 20 is set to a reference potential (GND potential), and therefore the potential of the source electrode 42 is also set to the reference potential. Therefore, the potentials of the wirings 82 and 82A are also set to the reference potential. For example, when the transistor 10 is used in a high frequency band, it is required to reduce noise superimposed on the gate signal. As in this modification, by sandwiching the wiring 81 corresponding to the gate electrode 41 between the wiring 82A corresponding to the source electrode 42, the wiring 82A exerts a shielding effect, and it is possible to reduce noise superimposed on the gate signal.
[0085] The transistor and the method of manufacturing the transistor according to the present disclosure are not limited to the above-mentioned embodiment, and various other modifications are possible. For example, in the above-mentioned embodiment, the gate electrode 41, the source electrode 42, and the drain electrode 43 are all provided with polysilicon films, plugs, and wiring, but one or two of the gate electrode 41, the source electrode 42, and the drain electrode 43 may be provided with polysilicon films, plugs, and wiring.
[0086] Furthermore, in the above embodiment, the gate electrode 41, the source electrode 42 and the drain electrode 43 contain Ni, but they do not have to contain Ni as long as a polysilicon film can be formed thereon. [Explanation of symbols]
[0087] 10,10A...Transistor 20...Substrate 21…Main surface 22…Back side 30...Semiconductor laminate 30a, 30b...recess 31…Channel layer 31a…Channel region 32...electron supply layer 33...First high concentration n-type semiconductor region 34...Second high concentration n-type semiconductor region 41, 44...Gate electrode 42, 45…Source electrode 43, 46...Drain electrode 51, 52, 53, 54...Polysilicon film 61...Dielectric layer 61a…gate opening 61b…Source opening 61c…Drain opening 62...Dielectric layer 62a, 62b, 62c…opening 71, 72, 73…Plugs 74...W membrane 81, 82, 82A, 83, 84...Wiring 85…Gate wiring 86…Drain wiring 91...Aperture 441...Ni layer 442…Au layer 451,461…Ti layer 452,462…Aluminum layer 453,463…Mo layer 454,464…Au layer 821,822…Wiring part A…Opening width D…Depth
Claims
1. A semiconductor laminate portion; a source electrode and a drain electrode provided on the semiconductor laminate, and a gate electrode provided between the source electrode and the drain electrode on the semiconductor laminate; a first polysilicon film provided on a first electrode which is one of the gate electrode, the source electrode, and the drain electrode; a dielectric layer provided on the semiconductor laminate portion, covering the gate electrode, the source electrode, the drain electrode and the first polysilicon film, and having a first opening formed on the first polysilicon film; a first plug including tungsten, embedded in the first opening and in contact with the first polysilicon film; a first wiring provided on the dielectric layer and in contact with the first plug; A transistor comprising:
2. 2. The transistor according to claim 1, wherein at least a portion of said first electrode in contact with said first polysilicon film contains nickel in its composition.
3. 3. The transistor according to claim 2, wherein at least a portion of said first electrode that is in contact with said first polysilicon film is made of only nickel.
4. The transistor of claim 1 , wherein the first plug is made of tungsten alone.
5. 4. The transistor according to claim 1, wherein a ratio (D / A) of a depth D to an opening width A of the first opening is 2 or greater.
6. a second polysilicon film provided on a second electrode which is the other of the gate electrode, the source electrode, and the drain electrode; a third polysilicon film provided on a third electrode which is the remaining one of the gate electrode, the source electrode, and the drain electrode; Further comprising: the dielectric layer further covers the second polysilicon film and the third polysilicon film, and further has a second opening and a third opening formed on the second polysilicon film and the third polysilicon film, respectively; The transistor is a second plug including tungsten, embedded in the second opening and in contact with the second polysilicon film; a third plug including tungsten, embedded in the third opening and in contact with the third polysilicon film; a second wiring and a third wiring provided on the dielectric layer and in contact with the second plug and the third plug, respectively; The transistor of claim 1 , further comprising:
7. 7. The transistor according to claim 6, wherein at least a portion of said second electrode in contact with said second polysilicon film and at least a portion of said third electrode in contact with said third polysilicon film contain nickel in their composition.
8. the gate electrode, the source electrode, and the drain electrode each contain nickel in their composition; 7. The transistor according to claim 6, wherein the semiconductor laminate comprises: a semiconductor layer including a Group III nitride semiconductor and in contact with the gate electrode; a first high-concentration n-type semiconductor region including a Group III nitride semiconductor and in contact with the source electrode; and a second high-concentration n-type semiconductor region including a Group III nitride semiconductor and in contact with the drain electrode.
9. The semiconductor laminate portion is a channel layer provided between the first high concentration n-type semiconductor region and the second high concentration n-type semiconductor region; an electron supply layer having a band gap larger than that of the channel layer; The transistor of claim 8 having
10. an electrode forming step of forming a source electrode, a drain electrode, and a gate electrode located between the source electrode and the drain electrode on the semiconductor laminate; a polysilicon film forming step of forming a first polysilicon film on a first electrode which is one of the gate electrode, the source electrode, and the drain electrode; a dielectric layer forming step of forming a dielectric layer on the semiconductor laminate portion to cover the gate electrode, the source electrode, the drain electrode and the first polysilicon film; forming a first opening on the first polysilicon film in the dielectric layer; a plug forming step of forming a first plug in contact with the first polysilicon film by filling the first opening with a material containing tungsten; a wiring forming step of forming a first wiring on the dielectric layer in contact with the first plug; A method for manufacturing a transistor, comprising:
11. 11. The method for manufacturing a transistor according to claim 10, wherein in the electrode forming step, the first electrode is formed so that at least a portion in contact with the first polysilicon film contains nickel in its composition.
12. 12. The method for manufacturing a transistor according to claim 11, wherein in the electrode formation step, the first electrode is formed so that at least a portion thereof in contact with the first polysilicon film is made of only nickel.
13. In the polysilicon film formation process, the film formation raw material is SiH 4 12. The method of claim 11, wherein the first polysilicon film is formed at room temperature using a method according to claim 11.
14. 14. The method for manufacturing a transistor according to claim 10, wherein in the plug forming step, the first plug is formed from tungsten alone.
15. 14. The method of claim 10, wherein in the opening formation step, a ratio (D / A) of a depth D to an opening width A of the first opening is set to 2 or more.
16. In the polysilicon film forming step, a second polysilicon film is further formed on a second electrode which is the other one of the gate electrode, the source electrode, and the drain electrode, and a third polysilicon film is further formed on a third electrode which is the remaining one of the gate electrode, the source electrode, and the drain electrode; In the dielectric layer forming step, the dielectric layer is formed to further cover the second polysilicon film and the third polysilicon film, In the opening forming step, a second opening is further formed on the second polysilicon film in the dielectric layer, and a third opening is further formed on the third polysilicon film; In the plug forming step, a material containing tungsten is further embedded in the second opening and the third opening to further form a second plug in contact with the second polysilicon film and a third plug in contact with the third polysilicon film; 14. The method for manufacturing a transistor according to claim 10, wherein in the wiring forming step, a second wiring in contact with the second plug and a third wiring in contact with the third plug are further formed on the dielectric layer.
17. 17. The method for manufacturing a transistor according to claim 16, wherein in the electrode formation step, the second electrode includes nickel in a composition at least in a portion in contact with the second polysilicon film, and the third electrode includes nickel in a composition at least in a portion in contact with the third polysilicon film.
18. the semiconductor laminate portion has a semiconductor layer including a Group III nitride semiconductor, a first high-concentration n-type semiconductor region including a Group III nitride semiconductor, and a second high-concentration n-type semiconductor region including a Group III nitride semiconductor, 17. The method for manufacturing a transistor according to claim 16, wherein in the electrode formation step, the gate electrode, the source electrode, and the drain electrode each containing nickel in a composition are formed, the gate electrode is in Schottky contact with the semiconductor layer, the source electrode is in contact with the first high concentration n-type semiconductor region, and the drain electrode is in contact with the second high concentration n-type semiconductor region.
19. The semiconductor laminate portion is a channel layer provided between the first high concentration n-type semiconductor region and the second high concentration n-type semiconductor region; an electron supply layer having a band gap larger than that of the channel layer; The method of claim 18 , comprising:
Citation Information
Patent Citations
GaN-based HEMT device with low input capacitance
CN112086508A
Low-resistance contact structure and method for manufacturing the same
JP2010503224A
Semiconductor device and manufacturing method of the same
JP2013080891A
GaN Transistor with a polysilicon layer for creating additional components
JP2016529710A
Nitride semiconductor device and method for manufacturing the same
JP2017073499A