Optical control device and manufacturing method of the same
The integration of EO polymer and inorganic waveguides with different heights and a manufacturing method using sacrificial substrates addresses the compactness and efficiency issues of optical phased arrays, achieving a low-power, high-speed optical control device suitable for distance measurement and communication.
Patent Information
- Application Number
- JP2023046717
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-23
- Publication Date
- 2024-10-04
AI Technical Summary
Existing optical phased arrays face challenges in compactness and high-speed operation due to the need for numerous signal lines and long wiring, which increases stray capacitance and power consumption, especially when using Si3N4 waveguides formed by low-temperature PE-CVD, leading to light absorption issues.
The optical control device integrates a semiconductor integrated circuit with embedded drive circuits and a phase control unit that includes EO polymer waveguides and inorganic waveguides with different heights, allowing for compact design and reduced stray capacitance by overlapping electrodes, and uses a manufacturing method involving sacrificial substrates to form high-quality waveguides at elevated temperatures.
This configuration results in a compact optical control device with reduced stray capacitance, enabling low power consumption and high-speed phase control, suitable for applications like distance measurement and communication.
Smart Images

Figure 2024135834000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an optical control device and a manufacturing method thereof, and more particularly to an optical control device including a waveguide on a semiconductor integrated circuit and a manufacturing method thereof. [Background technology]
[0002] Conventionally, an optical phased array using a multi-optical waveguide and a phase controller has been proposed (see, for example, Patent Document 1). FIG. 12 is a schematic diagram showing an example of a conventional optical phase array. The optical phased array 101 shown in FIG. 12 includes an optical input section 103, an optical separation section 104, a phase control section 105, a multi-optical waveguide section 106, and an optical output end 107. The optical phased array 101 is configured as an optical phased array chip having these components on a substrate 110. Note that in FIG. 12, only an optical waveguide core is illustrated as the waveguide 108, and the cladding layer around the core is omitted.
[0003] The phase control section 105 controls the phase of each waveguide 108. The phase control section 105 includes an upper electrode 135, which is a control electrode that applies different voltages to each of the waveguides 108 in order to control the phase of the light propagating through each of the waveguides 108, and a lower electrode 133 as an electrode common to each channel. The waveguide core region of each channel sandwiched between the lower electrode 133 and the upper electrode 135 via a cladding layer functions as a phase controller.
[0004] The multi-optical waveguide unit 106 has, as an example, eight-channel waveguides 108. Voltages and signals for phase control of each channel are input to the optical phased array 101 from a driving circuit 31, which is a device outside the chip, via a signal line. In Fig. 12, the driving circuits 31 for phase control are illustrated diagrammatically according to the type of applied voltage. V1 to V8 diagrammatically indicate eight driving circuits 31 that individually drive the eight-channel waveguides 108, respectively.
[0005] An optical phased array can deflect the light beam from the optical output end by using diffraction and interference by controlling the phase of light between the waveguides using a phase controller installed in each waveguide. The divergence angle of the light beam at a location away from the optical output end follows the following formula (1). Ψ = sin -1 [1.22λ / ((N-1) d)] (1) Here, λ is the wavelength of light, N is the number of waveguides, and d is the waveguide pitch.
[0006] According to formula (1), in order to create a narrow optical beam with a small divergence angle (proportional to the spot diameter), it is necessary to increase the number of waveguides if the waveguide pitch is constant. When the number of waveguides increases, the number of signal lines for driving the phase controller corresponding to the number of waveguides increases, and these many signal lines must be taken out of the optical phased array chip. As an example of the number of required signal lines, an optical phased array using a 1024-line waveguide array has been reported (see Non-Patent Document 1). To route such a large number of wires to an external signal circuit, it is necessary to use space-consuming wires such as flexible cables. In addition, the wiring becomes long, which increases the load due to floating electrostatic capacitance and hinders high-speed operation.
[0007] Also, a manufacturing process of a Si3N4 waveguide as an optical waveguide is described in Non-Patent Document 2. The technology described in Non-Patent Document 2 is premised on forming a Si3N4 waveguide on a semiconductor integrated circuit (CMOS (Complementary Metal-Oxide-Semiconductor) circuit), and uses low-temperature (400°C) plasma-enhanced chemical vapor deposition (PE-CVD) deposition. In addition, an optical phased array has been reported that uses a polymer having an EO effect (EO polymer) in the optical waveguide of the phase control section (see Non-Patent Document 3). [Prior art documents] [Patent documents]
[0008] [Patent Document 1] JP 2022-133031 A [Non-patent literature]
[0009] [Non-Patent Document 1] Guangzhen Luo et. al., “1024-channel Passive Optical Phased Array with High Angular Resolution”, Asia Communications and Photonics Conference 2021, T3D.5 (2021). [Non-Patent Document 2] AZ Subramanian et. al., “Low-Loss Single mode PECVD Silicon Nitride Photonic Wire Waveguides for 532-900 nm Wavelength Window Fabricated Within a CMOS Pilot Line”, IEEE Photonics Journal, Vol. 5, No. 6, 2202809, (2013). [Non-Patent Document 3] Yuji Miyamoto et al., "Design and Fabrication of Organic / Inorganic Layered Optical Phased Array," Abstracts of the 2022 Annual Conference of the Institute of Image Information and Television Engineers, 13C-5 (2022). Summary of the Invention [Problem to be solved by the invention]
[0010] In order to make the optical phased array and its control board compact, it is conceivable to fabricate a semiconductor integrated circuit (drive circuit LSI) having a drive circuit as an optical phased array drive control chip and form an optical phased array directly on the optical phased array drive control chip. However, for example, when forming a Si3N4 waveguide on a semiconductor integrated circuit (CMOS circuit), if the technology described in Non-Patent Document 2 is applied, the formed Si3N4 has the following problems. The Si3N4 formed by low-temperature PE-CVD has many defects due to N-H bonds and absorbs light with a wavelength of around 1550 nm, making it unusable for optical phased arrays for distance measurement, communication, and other applications. The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a small-sized optical control device that includes a waveguide on a semiconductor integrated circuit and facilitates wiring, and a method for manufacturing the same. [Means for solving the problem]
[0011] In order to solve the above problems, an optical control device according to the present invention includes a phase control section drive circuit section made of a semiconductor integrated circuit having a plurality of drive circuits embedded therein for driving an optical phased array and a plurality of first electrodes each electrically connected to the plurality of drive circuits, and an optical phased array mounted on the phase control section drive circuit section, wherein the optical phased array includes a light separation section having a plurality of input side inorganic waveguides and separating incident light into a plurality of channels, a phase control section having a plurality of EO polymer waveguides for guiding the light separated into the plurality of channels, and a plurality of output side inorganic waveguides respectively on extensions of the plurality of input side inorganic waveguides and for guiding phase-controlled light. and a common second electrode formed on the phase control section so as to overlap, in a planar view, with each of the plurality of first electrodes at different heights, wherein the height of the EO polymer waveguide and the heights of the input side inorganic waveguide and the output side inorganic waveguide are different, and the EO polymer waveguide has an overlapping region with the input side inorganic waveguide and the output side inorganic waveguide in a planar view, and in the phase control section drive circuit section, the plurality of first electrodes are formed along the EO polymer waveguide at different heights in a region between the input side inorganic waveguide and the output side inorganic waveguide.
[0012] According to this configuration, in the optical phased array of the optical control device, the input light travels through the input inorganic waveguide, enters the EO polymer waveguide by optically coupling the input inorganic waveguide and the EO polymer waveguide at a region where they overlap in a planar view with different heights, and enters the output inorganic waveguide by optically coupling the EO polymer waveguide and the output inorganic waveguide at a region where they overlap in a planar view with different heights, and is emitted to the outside. In the optical control device, the drive circuit embedded in the phase control unit drive circuit unit can apply individual voltages to the EO polymer waveguides of the phase control unit via the multiple first electrodes, thereby controlling the phase of the light propagating through the EO polymer waveguide. In the optical control device, the drive circuit and the first electrode, which is the control electrode, are provided in the phase control unit drive circuit unit made of a semiconductor integrated circuit, so that the optical phased array and the phase control unit drive circuit unit, which is the control board thereof, are made compact. As a result, the optical control device can reduce the distance between the drive circuit and the first electrode. Therefore, the optical control device minimizes stray capacitance caused by the wiring from the drive circuit to the first electrode, enabling low power consumption and high-speed phase control.
[0013] Moreover, a manufacturing method of an optical control device according to a first aspect of the present invention is a manufacturing method of an optical control device in which a phase control section drive circuit section made of a semiconductor integrated circuit and an optical phased array are integrally formed, the manufacturing method including the steps of: forming a drive circuit substrate in which a plurality of drive circuits are embedded and which has a plurality of first electrodes each electrically connected to the plurality of drive circuits; forming a film made of an inorganic material on a sacrificial substrate at a temperature exceeding the heat resistance temperature of the semiconductor integrated circuit; patterning the film made of the inorganic material to form a waveguide substrate including a plurality of pairs each including an input side inorganic waveguide and an output side inorganic waveguide arranged on an extension line of the input side inorganic waveguide; The method includes the steps of: bonding the drive circuit board and the waveguide substrate so that the first electrode overlaps in a region between the input side inorganic waveguide and the output side inorganic waveguide in a planar view; laminating an EO polymer film on the surface exposed by removing the sacrificial substrate so that the EO polymer film overlaps with the input side inorganic waveguide and the output side inorganic waveguide in a planar view; dividing the EO polymer film to form a plurality of EO polymer waveguides along the pair of the input side inorganic waveguide and the output side inorganic waveguide; and forming a common second electrode on the plurality of EO polymer waveguides so as to overlap with the plurality of first electrodes in a planar view.
[0014] According to this procedure, the method for manufacturing an optical control device includes a step of separately forming a drive circuit board and a waveguide board, and a step of bonding the drive circuit board and the waveguide board, so that an appropriate value can be applied to the process temperature that gives characteristics to the drive circuit board, and an appropriate value can be applied to the process temperature that gives characteristics to the waveguide board. The method for manufacturing an optical control device forms a film made of an inorganic material on a sacrificial substrate at a temperature exceeding the heat resistance temperature of the semiconductor integrated circuit, so that defects in the input side inorganic waveguide and the output side inorganic waveguide formed on the waveguide substrate can be reduced. Therefore, the method for manufacturing an optical control device can manufacture a small optical control device with easy wiring by providing a high-quality input side inorganic waveguide and an output side inorganic waveguide on a semiconductor integrated circuit.
[0015] Furthermore, a manufacturing method for an optical control device according to a second aspect of the present invention is a manufacturing method for an optical control device in which a phase control section drive circuit section made of a semiconductor integrated circuit and an optical phased array are integrally formed, the manufacturing method including the steps of: forming a drive circuit board in which a plurality of drive circuits are embedded and which has a plurality of contact electrodes each electrically connected to the plurality of drive circuits; forming a film made of an inorganic material on a sacrificial substrate at a temperature exceeding the heat resistance temperature of the semiconductor integrated circuit; patterning the film made of the inorganic material to form a plurality of pairs each including an input side inorganic waveguide and an output side inorganic waveguide arranged on an extension line of the input side inorganic waveguide; the step of forming a waveguide substrate by forming first electrodes in the regions between the first electrodes and the second electrodes; the step of bonding the drive circuit substrate and the waveguide substrate so that the plurality of contact electrodes and the plurality of first electrodes face each other; the step of laminating an EO polymer film on the surface exposed by removing the sacrificial substrate so as to overlap the input side inorganic waveguide and the output side inorganic waveguide in a planar view; the step of dividing the EO polymer film to form a plurality of EO polymer waveguides aligned with the input side inorganic waveguide and the output side inorganic waveguide; and the step of forming a common second electrode on the plurality of EO polymer waveguides so as to overlap the plurality of first electrodes in a planar view.
[0016] According to this procedure, the method for manufacturing an optical control device includes a step of separately forming a drive circuit board and a waveguide board, and a step of bonding the drive circuit board and the waveguide board, so that the process temperature for giving characteristics to the drive circuit board and the waveguide board can be set to a value appropriate for each board. The method for manufacturing an optical control device forms an input side inorganic waveguide and an output side inorganic waveguide by patterning before bonding the drive circuit board and the waveguide board, so that the restriction on alignment during substrate bonding can be reduced. The method for manufacturing an optical control device forms a film made of an inorganic material on a sacrificial substrate at a temperature exceeding the heat resistance temperature of a semiconductor integrated circuit, so that defects of the input side inorganic waveguide and the output side inorganic waveguide formed on the waveguide substrate can be reduced. Therefore, the method for manufacturing an optical control device can manufacture a small optical control device with easy wiring by providing a high-quality input side inorganic waveguide and an output side inorganic waveguide on a semiconductor integrated circuit. Effect of the Invention
[0017] According to the present invention, it is possible to provide a small-sized optical control device having a waveguide on a semiconductor integrated circuit and facilitating wiring. Also, according to the present invention, it is possible to manufacture a small-sized optical control device having a waveguide on a semiconductor integrated circuit and facilitating wiring. [Brief description of the drawings]
[0018] [Figure 1] FIG. 2 is a schematic exploded view showing the light control device according to the first embodiment. [Diagram 2] 1(a) and 1(b) are schematic cross-sectional views of the light control device according to the first embodiment. [Diagram 3] 4 is a flowchart showing a flow of a manufacturing process for the light control device according to the first embodiment. [Figure 4] 5(a) to 5(f) are cross-sectional views showing the process of forming a drive circuit board. [Diagram 5] 1(a) to 1(h) are cross-sectional views showing steps for forming a waveguide substrate. [Figure 6]1(a) to 1(f) are cross-sectional views showing the first half of the process from bonding the substrates to completion. [Figure 7] 4(a) to 4(f) are cross-sectional views showing the latter half of the process from bonding the substrates to completion. [Figure 8] 13(a) and 13(b) are schematic cross-sectional views of a light control device according to a modified example. [Figure 9] 10 is a flowchart showing a flow of a manufacturing process for the light control device according to the second embodiment. [Figure 10] 5(a) to 5(f) are cross-sectional views showing the process of forming a drive circuit board. [Figure 11] 1(a) to 1(d) are cross-sectional views showing the steps from completing a waveguide substrate to bonding substrates. [Figure 12] FIG. 1 is a schematic diagram showing an example of an optical face array using a conventional multi-optical waveguide and a phase controller. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] (First embodiment) [Outline of optical control device] First, an overview of the optical control device 1 according to the first embodiment will be described with reference to Fig. 1, Fig. 2(a) and Fig. 2(b). In the drawings to be referred to, the width direction of the optical control device 1 is the x-axis, the height direction of the optical control device 1 is the y-axis, and the depth direction of the optical control device 1 is the z-axis. Also, as an example, the waveguide array is shown with four waveguides, but in reality, the waveguide array is composed of a larger number of waveguides, such as 16, 32, 64, .... For convenience, the waveguides are called channel 1, channel 2, ... from the left in Fig. 2(b). Fig. 2(a) is a schematic diagram showing a main part of a yz cross section when cut in the z direction along the waveguide of the channel 1 of the optical control device 1. Fig. 2(a) shows a part of the size necessary for phase control, including the phase control section 5. Note that the same applies to other schematic diagrams showing yz cross sections, including drawings for explaining the manufacturing process. Fig. 2(b) is a schematic diagram showing an xy cross section when cut in the x direction across the waveguides of each channel of the optical control device 1. Fig. 2(b) corresponds to a cross-sectional view taken along line IIb-IIb in Fig. 2(a), but the Si3N4 waveguide 8a and the driving circuit 31 are arranged for reference so that they can be easily understood intuitively. Note that these members are shown in the same sense in other schematic diagrams showing xy cross sections, including drawings for explaining the manufacturing process.
[0020] As shown in Fig. 1, the optical control device 1 includes a phase-controller drive circuit section 30 and an optical phased array 2 mounted on the phase-controller drive circuit section 30. For convenience of explanation, the phase-controller drive circuit section 30 and the optical phased array 2 are shown separately in Fig. 1, but in reality, the optical phased array 2 is stacked directly on the phase-controller drive circuit section 30, and the two are integrally formed. The phase control unit driving circuit unit 30 is composed of a semiconductor integrated circuit, has multiple driving circuits 31 embedded therein that drive the optical phased array 2, and has multiple lower electrodes (first electrodes) 33 that are each electrically connected to the multiple driving circuits 31.
[0021] The optical phased array 2 includes an optical separator 4, a phase controller 5, a multi-optical waveguide section 6, and a common upper electrode (second electrode) . The light separating section 4 separates the incident light into a plurality of channels. The phase shift section 5 has a plurality of EO polymer waveguides 9. The plurality of EO polymer waveguides 9 guide the light separated into the plurality of channels, respectively. The optical separation section 4 has a plurality of Si3N4 waveguides (input side inorganic waveguides) 8a, and the multi-optical waveguide section 6 has a plurality of Si3N4 waveguides (output side inorganic waveguides) 8b. The plurality of Si3N4 waveguides 8b guide the phase-controlled light, and are provided on the extensions of the plurality of Si3N4 waveguides 8a. The upper electrode 35 is formed on the phase shifting section 5 so as to overlap the plurality of lower electrodes 33 in a plan view with the height directions being different from each other.
[0022] In the light control device 1, the height of the EO polymer waveguide 9 and the height of the Si3N4 waveguides 8a and 8b are made different, and the EO polymer waveguide 9 and the Si3N4 waveguides 8a and 8b have a region where they overlap in a plan view. In the phase control section driver circuit section 30, a plurality of lower electrodes 33 are formed along the EO polymer waveguide 9 at different heights in the region between the Si3N4 waveguide 8a and the Si3N4 waveguide 8b.
[0023] [Configuration of each part of the optical control device] The light input unit 3 is an element for inputting light from the outside into the light control device 1. A light source for inputting light into the light input unit 3 is preferably a laser that has excellent coherence and can adjust the polarization, but an LED (light emitting diode) or an SLD (super luminescent diode) may also be used. In this embodiment, the light input unit 3 is fabricated simultaneously with the Si3N4 waveguides 8a and 8b, and is therefore fabricated from Si3N4 like these waveguides.
[0024] The light splitter 4 is an element that splits the light input from the light input unit 3 into equal intensities according to the number of EO polymer waveguides 9 constituting the phase control unit 5. In this embodiment, one-input, four-branch multimode interference (1x4MMI) is used to split the light into four waveguides. As a splitting method, in addition to using 1x4MMI, 1xnMMI (n: an integer of 2 or more, for example, 1x2) or Y-branching may be used and arranged in a cascade shape. In this embodiment, the light splitter 4 is fabricated simultaneously with the Si3N4 waveguides 8a and 8b, and is therefore fabricated from Si3N4 like these waveguides.
[0025] An upper electrode 35 common to all channels is disposed via an upper clad 20c above the EO polymer waveguide 9 of the phase control section 5. A lower electrode 33 divided for each channel is disposed below the EO polymer waveguide 9 via an intermediate clad 20a and a lower clad 20b.
[0026] As the EO polymer constituting the EO polymer waveguide 9, for example, a polymer material in which an organic dye exhibiting a nonlinear response is dispersed and blended in a polymethyl methacrylate (PMMA) system can be used. Other EO dyes such as Disperse Red can be used. In the input side optical coupling section 11 and the output side optical coupling section 12, the Si3N4 waveguides 8a and 8b are shown as having a parallel width in the drawings, but it is preferable that the width in a plan view is formed in a tapered shape tapering toward the end face. Note that, if the wavelength range used is limited to a communication band of 1.3 to 1.6 μm, the Si3N4 waveguide (input / output side inorganic waveguide) 8a and the Si3N4 waveguide (output side inorganic waveguide) 8b may be replaced with Si waveguides.
[0027] The upper electrode 35 is a flat electrode. The upper electrode 35 is disposed above the EO polymer waveguide 9 with a gap therebetween via the upper clad 20c. The upper electrode 35 is a common electrode for, for example, a plurality of (for example, four) EO polymer waveguides 9, and is grounded here (see FIG. 2(b)). The lower electrode 33 is divided along the EO polymer waveguide 9. The lower electrodes 33 are arranged below the EO polymer waveguide 9 at opposing positions with different heights, with the lower clad 20b interposed between them. The lower electrodes 33 are electrodes provided for applying individual voltages V1 to V4 (see FIG. 2(b)) to, for example, each of the multiple (e.g., four) EO polymer waveguides 9. The lower electrode 33 has a length necessary for phase control in the longitudinal direction, with the longitudinal direction being the z direction. Materials that can be selected for use in the upper electrode 35 and the lower electrode 33 include metal electrodes such as Ti, Cr, Au, Cu, and Al, and transparent electrodes such as ZnO, ITO (Indium Tin Oxide), and IZO (Indium Zinc Oxide).
[0028] The clad 20 includes an intermediate clad 20a, a lower clad 20b, and an upper clad 20c, which are laminated in, for example, three different steps during the manufacture of the light control device 1. The lower clad 20b is disposed below the Si3N4 waveguides 8a and 8b. The upper clad 20c is disposed above the Si3N4 waveguides 8a and 8b. The intermediate clad 20a is disposed between the lower clad 20b and the upper clad 20c. When the intermediate clad 20a, the lower clad 20b, and the upper clad 20c are not to be distinguished from each other, they are simply referred to as the clad 20.
[0029] The material of the cladding 20 is preferably one whose refractive index is smaller than that of the EO polymer and whose difference in refractive index with the EO polymer is as large as possible. For example, SiO2 (refractive index 1.48) can be used as such a material. The substrate 10 may be any substrate having sufficient mechanical strength to support each layer, but it is preferable to select a substrate having a small difference in linear expansion coefficient between each layer, such as a silicon substrate.
[0030] [Operation of the optical control device] Next, the operation of the optical control device will be described with reference to Fig. 1, Fig. 2(a) and Fig. 2(b). Coherent light incident on the optical input section 3 from an optical fiber or the like is distributed to a desired number of waveguides by the optical splitter section 4. The distributed light travels in the z direction through the Si3N4 waveguide 8a, and enters the EO polymer waveguide 9 of the phase control section from the Si3N4 waveguide 8a at the input side optical coupling section 11. The light that has traveled through the EO polymer waveguide 9 is optically coupled to the Si3N4 waveguide 8b of the multi-optical waveguide section 6 at the output side optical coupling section 12, travels through the Si3N4 waveguide 8b, and is emitted into space from the optical output end 7. The respective lights that have passed through the waveguides of the respective channels and are emitted from the optical output end 7 interfere and diffract while propagating through space, and are observed as a single optical beam at a location far away from the optical output end 7.
[0031] In the optical control device 1, when a potential (0 V or ground potential) common to each channel is applied to the upper electrode 35 and a voltage for controlling the refractive index of the EO polymer film for each channel is applied to each lower electrode 33, the phase of light can be modulated for each channel in the phase control section 5. The amount of phase shift Δφ in the EO polymer film relative to the voltage is given by the following formula (2).
[0032] Δφ=πn0 3 r V L / (λ d) … (2) Here, n0 is the refractive index when no electric field is applied, r is the electro-optic constant due to the electric tensor, V is the voltage, L is the optical path length in the light propagation direction (z direction) when voltage is applied, λ is the wavelength of light, and d is the thickness of the medium (EO polymer film). By controlling the phase between the waveguides according to the formula (2), the light beam emitted from the light output end 7 can be deflected. In Fig. 1, the beam direction when the light control device 1 does not perform phase control, for example, is shown typically by a hollow arrow, and the beam direction when the light control device 1 performs phase control is shown typically by a dashed arrow. That is, the light control device 1 of this embodiment can deflect the light beam so as to be inclined from the z direction to the x direction in the zx plane.
[0033] The optical control device 1 according to the present embodiment includes a plurality of lower electrodes 33 provided for applying individual voltages to the EO polymer waveguides 9 of the phase control section 5, and an upper electrode 35 common to each channel. Here, as Comparative Example 1, it is assumed that an optical control device is provided with an optical phased array 101 shown in FIG. 12 mounted on an optical phased array drive control chip. In Comparative Example 1, the drive of each phase controller is controlled by each control electrode (upper electrode 135) in the phase control section 105. In this case, for example, wiring must be provided from each control electrode (upper electrode 135) to the optical phased array drive control chip. That is, wiring is required to penetrate the substrate of the optical phased array and connect to the drive circuit. In addition, an extra space is required for the wiring to wrap around downwards, which requires a larger substrate area than before, resulting in a problem of size increase. In addition, the stray capacitance increases due to the longer wiring, and when a high optical deflection operation speed is required, power consumption increases. In contrast, in the optical control device 1 according to this embodiment, the drive circuit 31 and the control electrode (lower electrode 33) are provided in the phase control section drive circuit section 30 made of a semiconductor integrated circuit, so that the optical phased array 2 and the phase control section drive circuit section 30, which is its control board, are made compact. This allows the optical control device 1 to have an extremely short distance between the drive circuit 31 and the control electrode (lower electrode 33). Therefore, the optical control device 1 minimizes stray capacitance due to the wiring from the drive circuit 31 to the control electrode (lower electrode 33), enabling low power consumption and high-speed phase control.
[0034] [Method of manufacturing optically controlled device 1] Next, an outline of a method for manufacturing an optical control device according to the first embodiment will be described with reference to Fig. 3. As shown in Fig. 3, the method for manufacturing an optical control device 1 includes a step of forming a drive circuit board (step S10), a step of forming an oxide film on the surface of a sacrifice substrate (step S20), a step of forming a film made of an inorganic material on the oxide film formed on the surface of the sacrifice substrate (step S30), a step of forming a waveguide substrate (step S40), a step of bonding the drive circuit board and the waveguide substrate (step S50), a step of stacking an EO polymer film (step S60), a step of forming an EO polymer waveguide (step S70), and a step of forming an upper electrode (step S80). The step S10 includes a step of forming a lower electrode on a Si substrate (step S11), a step of embedding the lower electrode with an oxide film (step S12), and a step of planarizing the surface of the oxide film (step S13). In this embodiment, a bare Si substrate is used as a sacrificial substrate, and in step S20, an oxide film is formed on the bare Si substrate. In this embodiment, Si3N4 is used as an inorganic material, and in step S30, a Si3N4 film is formed on the oxide film. Step S40 includes a step of forming a Si3N4 waveguide (step S41) and a step of forming a cladding and planarization (step S42). Step S60 includes a step of removing the upper Si substrate (step S61) and a step of stacking an oriented EO polymer (step S62). Step S80 includes a step of forming an upper cladding (step S81) and a step of forming an upper electrode (step S82).
[0035] (Process for forming a drive circuit board) In the process of forming the drive circuit board (step S10), in step S11, as shown in Figures 4(a) and 4(b), a normal semiconductor integrated circuit manufacturing process is used to form lower electrodes 33 corresponding to the number of waveguides on the surface of the substrate 41. The lower electrodes 33 may be made of a general metal material such as metals such as Cu, Al, Ta, Cr, W, Ag, Au, Pt, or alloys thereof.
[0036] An integrated circuit having, for example, a CMOS driving circuit 31 embedded therein corresponding to the number of waveguides can be prepared as the substrate 41. Such an integrated circuit has, for example, semiconductor elements such as an N-channel MOS transistor or a P-channel MOS transistor as the driving circuit 31 on an SOI (Silicon on Insulator) substrate. In the process of step S11, a lower electrode 33 is formed on the surface of the substrate 41 so as to be electrically connected to the wiring of the driving circuit 31 embedded in the substrate 41. Before forming the lower electrode 33, a Si bare substrate or an SOI substrate may be prepared and an integrated circuit including the driver circuit 31 may be formed by a general semiconductor process.
[0037] Next, in the process of step S12, as shown in Fig. 4(c) and Fig. 4(d), an oxide film 43 is formed so as to cover the surface of the lower electrode 33. The oxide film 43 is formed for insulation and protection. In this embodiment, the oxide film 43 is, for example, a SiO2 film. For the formation of the oxide film, for example, a vacuum deposition method, a sputtering method, a chemical vapor deposition method (CVD method), or any other known method that forms a film at or below the heat resistance temperature of a semiconductor integrated circuit can be used.
[0038] Next, in the process of step S13, as shown in Fig. 4(e) and Fig. 4(f), the oxide film 43 on the lower electrode 33 is planarized. As a method for planarization, a chemical mechanical polishing (CMP) method or the like can be used. For convenience, this finally completed substrate is referred to as drive circuit substrate 45. By the process of step S10, a plurality of drive circuits 31 are embedded, and drive circuit substrate 45 having a plurality of lower electrodes 33 each electrically connected to the plurality of drive circuits 31 is formed. Upper surface 47 of drive circuit substrate 45 is entirely covered with oxide film 43.
[0039] (Process of forming an oxide film on a bare Si substrate) Next, in the process of forming an oxide film on a bare Si substrate (step S20), as shown in FIG. 5(a) and FIG. 5(b), an oxide film 51 is formed on a sacrificial substrate 49. The sacrificial substrate 49 is a Si substrate (bare Si substrate). The oxide film 51 can be formed by, for example, thermal oxidation, vacuum deposition, sputtering, or CVD. If the sacrificial substrate 49 is a Si substrate as in this embodiment, the oxide film can be formed by thermal oxidation to form an oxide film with a uniform thickness within the surface. In addition, since it is a film formation, the film thickness can be strictly controlled. The oxide film 51 formed in the process of step S20 becomes the intermediate cladding 20a (see FIG. 2(a)).
[0040] (Process of forming a Si3N4 film on an oxide film) Next, in the process of forming a Si3N4 film on the oxide film (step S30), as shown in Figures 5(c) and 5(d), a Si3N4 film 53 is formed on the oxide film 51 at a temperature exceeding the heat resistance temperature of the semiconductor integrated circuit. For example, a sputtering method or a CVD method can be used to form the Si3N4 film. In particular, in order to obtain a good quality film, the LP-CVD (Low-Pressure Chemical Vapor Deposition) method, which can form a film at 800°C or higher, is desirable (see, for example, Reference 1 below). (References) Reference 1: Xingchen Ji et. al., “Methods to achieve ultra-high quality factor silicon nitride resonators”, APL Photon. 6, 071101 (2021).
[0041] In the process of step S30, since the sacrificial substrate 49 is a Si substrate, the deposition on the oxide film 51 is the same as deposition on a simple Si substrate, and therefore a method of depositing the film at a temperature equal to or higher than the heat resistance temperature of the semiconductor integrated circuit may be used. In addition, if an annealing process is performed at 1000°C or higher after deposition, the number of N-H bonds can be further reduced (for example, see Reference 1).
[0042] (Process for forming a waveguide substrate) Next, in the process of forming a waveguide substrate (step S40), as shown in Fig. 5(e) to Fig. 5(h), the Si3N4 film 53 is patterned to form a waveguide substrate 57 having a plurality of pairs of a Si3N4 waveguide 8a and a Si3N4 waveguide 8b arranged on an extension line of the Si3N4 waveguide 8a. In detail, in the process of forming a Si3N4 waveguide (step S41), as shown in Fig. 5(e) and Fig. 5(f), the Si3N4 film 53 is formed into a waveguide-like pattern by photolithography and dry etching. At this time, the light separation unit 4 (see Fig. 1) is also formed at the same time.
[0043] Next, in the cladding formation and planarization process (step S42), as shown in FIG. 5(g) and FIG. 5(h), the Si3N4 waveguides 8a, 8b are buried with an oxide film 55 by using, for example, any one of a vacuum deposition method, a sputtering method, and a CVD method. The oxide film is, for example, SiO2. After the Si3N4 waveguides 8a, 8b are buried with the oxide film 55, the oxide film 55 on the Si3N4 waveguides 8a, 8b is planarized. The planarization method may be a CMP method or the like. Note that FIG. 5(g) and FIG. 5(h) show a state where the planarization is completed.
[0044] In the process of step S42, it is preferable to form the SiO2 film by CVD at a high temperature (800°C). The reason is that when the SiO2 film in contact with the Si3N4 waveguide is formed by CVD at a high temperature (800°C), the SiO2 film becomes dense, the defects at the Si3N4-SiO2 interface are reduced, and the propagation loss of light in the waveguide can be reduced. In addition, the oxide film 55 formed in the process of step S42 becomes a part of the lower cladding 20b (see FIG. 2(a)). For convenience, the substrate completed after the process of step S42 is called a waveguide substrate 57. The upper surface 59 of the waveguide substrate 57 is entirely covered with the oxide film 55.
[0045] (Step of bonding the drive circuit board and the waveguide board) Next, in the step of bonding the drive circuit board and the waveguide board (step S50), as shown in FIG. 6(a) and FIG. 6(b), the waveguide board 57 is laminated on the drive circuit board 45. At this time, the upper surface 47 (see FIG. 4(f)) of the drive circuit board 45 and the upper surface 59 (see FIG. 5(h)) of the waveguide board 57 are laminated facing each other. Then, as shown in FIG. 6(b), the drive circuit board 45 and the waveguide board 57 are aligned so that the lower electrode 33 overlaps the region between the Si3N4 waveguide 8a and the Si3N4 waveguide 8b in the z direction in a plan view, and then bonded to each other. In addition, before bonding, the drive circuit board 45 and the waveguide board 57 are aligned with high precision so that the lower electrode 33 does not shift in the x direction relative to the Si3N4 waveguide 8a as shown in FIG. 6(a). As the alignment device, a known alignment device used for substrate bonding can be used. In order to align and bond substrates with high accuracy, it is preferable to use an alignment device with high accuracy, for example, on the order of sub-μm. The alignment accuracy of substrate bonding has improved with the recent progress of lamination technology, and it has been reported that the accuracy is within ±100 nm.
[0046] The entire opposing surfaces of the substrates are covered with an oxide film (SiO2 film). Known techniques can be used for bonding. For example, there is diffusion bonding, in which the surfaces of each substrate are cleaned with O2 plasma or Ar plasma, then moisture is absorbed and the substrate is heated and pressurized at 300°C, or room temperature bonding, in which a Si film is formed on both sides in atomic layers and then pressure is applied at room temperature. When SiO2 substrates are bonded together in this way, a bonding strength comparable to that of bulk substrates can be obtained.
[0047] (EO polymer film lamination process) In the process of stacking EO polymer films (step S60), first, in the process of removing the upper Si substrate (step S61), the Si substrate (sacrificial substrate 49) on the upper side of the two bonded substrates is removed. Figures 6(c) and 6(d) show the state after the Si substrate (sacrificial substrate 49) has been removed. The surface 61 exposed by removing the Si substrate is the surface of the oxide film 51.
[0048] The Si substrate can be removed by dry etching. In dry etching using xenon difluoride gas (XeF2), Si is isotropically etched, but SiO2 film and Si3N4 film are hardly etched, so they can be used as etch stoppers. In this way, the oxide film 51 formed in step S20 on the waveguide substrate 57 can be left with the same thickness.
[0049] In the process of step S61, the Si substrate (sacrificial substrate 49) can be mechanically polished before dry etching. Since the Si substrate is relatively thick, it is preferable to thin the thickness of the Si substrate to about 20 μm by mechanical polishing. In this way, the time required for the process of removing the Si substrate can be shortened, and the consumption of expensive xenon difluoride gas can be suppressed, thereby reducing costs.
[0050] By the process of step S61, a substrate having Si3N4 waveguides 8a, 8b and a light separating unit 4 embedded in an oxide film 55 (lower clad 20b) and an oxide film 51 (middle clad 20a) is completed on the driving circuit 31 and the lower electrode 33. The following processes are steps for forming a phase control unit using an EO polymer waveguide on this substrate.
[0051] Next, in the process of laminating the oriented EO polymer (step S62), an EO polymer film 63 is attached to the exposed surface of the substrate, where the oxide film 51 (intermediate cladding 20a) is exposed, so as to overlap the Si3N4 waveguides 8a and 8b in a plan view. Figures 6(e) and 6(f) show a state where the attachment of the EO polymer film 63 is completed. In the process of step S62, an oriented EO polymer film may be prepared as the EO polymer film 63. Alternatively, an EO polymer film may be formed on a separate support substrate (not shown) and then oriented (poling) may be performed.
[0052] (Process for forming EO polymer waveguide) Next, in the process of forming an EO polymer waveguide (step S70), the EO polymer film 63 is patterned into a waveguide shape by photolithography and etching. Figures 7(a) and 7(b) show a state in which the EO polymer waveguide 9 is divided into a plurality of EO polymer waveguides 9.
[0053] (Step of forming second electrode) Next, in the process of forming a second electrode (step S80), in the process of forming an upper clad (step S81), the EO polymer waveguide 9 is embedded in an oxide film 65 (upper clad 20c: see FIG. 2(a)) as shown in FIG. 7(c) and FIG. 7(d). Next, in the process of forming an upper electrode (step S82), a common upper electrode 35 is formed on the multiple EO polymer waveguides 9 via the oxide film 65 so as to overlap the multiple lower electrodes 33 in a plan view as shown in FIG. 7(e) and FIG. 7(f). The same material as the lower electrode 33 can be used for the upper electrode 35.
[0054] Thereafter, although not shown, a process of polishing the end face of the optical input portion 3 and the end face of the optical output portion 7 to prevent reflection and a process of exposing the electrode pads can be performed. Here, the electrode pads are members for electrically connecting to an external device. The external device applies a voltage, a signal, etc. for operating the drive circuit 31 to the drive circuit 31 via the electrode pads.
[0055] As described above, the manufacturing method according to this embodiment includes a step (step S50) of bonding the drive circuit board 45 and the waveguide board 57, which are separately manufactured. As a result, the manufacturing method according to this embodiment has the following effects. It is assumed that the optical control device 1 shown in FIG. 2(a) is manufactured by a conventional optical phased array manufacturing method, and this is set as Comparative Example 2. In Comparative Example 2, the optical control device 1 is manufactured by stacking the necessary members in order from the substrate 10 side. That is, in Comparative Example 2, for example, the Si3N4 waveguides 8a, 8b are formed on the lower clad 20b, an oxide film (SiO2) is formed as a clad material, and the EO polymer waveguide 9 is formed after the surface is planarized (CMP, etc.). Of these steps, the oxide film (SiO2) polishing in the CMP planarization step provides a desired gap as the thickness of the intermediate clad 20a between the Si3N4-EO polymer. Non-Patent Document 3 describes that the gap between the Si3N4-EO polymers must be precisely defined because there is an optimum value depending on the shape of the Si3N4 core in the overlapping portion. However, since CMP polishing depends on the pattern shape of the base, the polishing speed is different between the center and the periphery of the chip. Or, when multiple chips are arranged on a wafer, the polishing speed is different between the center and the periphery of the wafer. Therefore, among the steps of Comparative Example 2, it is difficult to uniformly control the gap (thickness of the intermediate cladding 20a) in CMP polishing. In Comparative Example 2, the thickness of the intermediate cladding 20a to be left as a gap is measured each time, and polishing is repeated, making film thickness control difficult and the process complicated. Furthermore, even if a gap is not required, it is difficult to uniformly expose the Si3N4 waveguides 8a, 8b (to make the thickness of the Si3N4 waveguides 8a, 8b uniform) and to flatten the surface of the Si3N4 waveguides 8a, 8b and the surface of the SiO2 arranged between the waveguides without creating a step.
[0056] In contrast, in the manufacturing method according to the present embodiment, an intermediate cladding 20a (gap) with a strictly controlled thickness can be obtained by forming an oxide film 51 on the sacrificial substrate 49 by thermal oxidation in step S20. Therefore, the manufacturing method according to the present embodiment can provide a Si3N4-EO polymer gap that has good in-plane uniformity and is formed with a highly accurate thickness.
[0057] According to the manufacturing method of this embodiment, in the step (step S61) of removing the upper Si substrate (sacrificial substrate 49), dry etching is performed using xenon difluoride gas (XeF2), so that the oxide film 51 formed in step S20 can be left with its original thickness. Therefore, in the input side optical coupling section 11 and the output side optical coupling section 12 (see FIG. 2(a)), a proper gap can be precisely provided as the intermediate cladding 20a (see FIG. 2(a)) between the Si3N4 waveguides 8a, 8b and the EO polymer waveguide 9.
[0058] Furthermore, according to the manufacturing method of this embodiment, an appropriate value (relatively low temperature) can be applied to the process temperature that imparts characteristics to the drive circuit board 45 (see FIG. 4(f)), and an appropriate value (relatively high temperature) can be applied to the process temperature that imparts characteristics to the waveguide substrate 57 (see FIG. 5(h)). Therefore, for example, the Si3N4 waveguides 8a, 8b formed in the waveguide substrate 57 (see FIG. 5(h)) have reduced defects due to N-H bonds, and the optical control device 1 manufactured by this manufacturing method can also be used for distance measurement, communication, and other applications.
[0059] (Modification) An optical control device 1B shown in Fig. 8(a) has a grating 67 provided in a Si3N4 waveguide 8B on the output side after passing through an EO polymer waveguide 9. An optical control device 1C shown in Fig. 8(b) has a grating 69 provided in a Si3N4 waveguide 8C on the output side after passing through an EO polymer waveguide 9. The optical control devices 1B and 1C can emit a light beam in the y direction.
[0060] As a method for manufacturing the optical control device 1B, if the pattern shape in photolithography is changed to reflect the shape of the grating 67 in the step (step S41) of forming the Si3N4 waveguide shown in Fig. 5(f), the optical control device 1B can be manufactured by the above-mentioned manufacturing method. In Fig. 8(a) and Fig. 8(b), reference characters are used to explain the manufacturing method. That is, the oxide film 51 corresponds to the intermediate cladding 20a (see Fig. 2(a)), the oxide film 55 corresponds to the lower cladding 20b, and the oxide film 65 corresponds to the upper cladding 20c.
[0061] The optical control device 1C may be manufactured as follows. For example, in step S61, the Si substrate (sacrificial substrate 49) is removed to expose the surface 61 of the oxide film 51 (see FIG. 6(d)), and a part of the oxide film 51 is etched together with a part of the Si3N4 waveguide 8b directly below it. At this time, the Si3N4 waveguide 8b directly below the oxide film 51 is half-etched to form the Si3N4 waveguide 8C having a recess of a predetermined depth. Then, an EO polymer film 63 is laminated (step S62). Thereafter, in the step of forming the upper clad (step S82) shown in FIG. 7(c) and FIG. 7(d), the recess of the Si3N4 waveguide 8C together with the EO polymer waveguide 9 may be filled with the oxide film 65 (upper clad 20c).
[0062] The shape of the grating is not limited to that shown in Fig. 8(a) and Fig. 8(b). In the present embodiment, the multiple Si3N4 waveguides 8b are periodically arranged with equal intervals, but the multiple Si3N4 waveguides 8b may be non-periodically arranged.
[0063] In the manufacturing method according to the present embodiment, in the process of step S30 shown in Fig. 3, Fig. 5(c) and Fig. 5(d), a Si3N4 film is formed on the oxide film 51 formed on the surface of the sacrificial substrate 49 made of a Si substrate, but the present invention is not limited to this. For example, when manufacturing an optical control device that does not require a gap between the Si3N4 waveguides 8a, 8b and the EO polymer waveguide 9 due to the oxide film 51 (intermediate clad 20a), the process of step S20 shown in Fig. 3, Fig. 5(a) and Fig. 5(b) may be omitted. In this case, in the process of step S30 following step S10, the Si3N4 film 53 is simply formed on the Si substrate (sacrificial substrate 49) at a temperature exceeding the heat resistance temperature of the semiconductor integrated circuit, and the subsequent processes can be performed in the same manner.
[0064] Second embodiment [Method of manufacturing optically controlled device 2] Next, an outline of a manufacturing method according to a second embodiment will be described with reference to Fig. 9. Note that the same steps as those in the manufacturing process shown in Fig. 3 are denoted by the same reference numerals and will not be described. 9, the manufacturing method according to the second embodiment of the optical control device 1 includes a step of forming a drive circuit board (step S10B), a step of forming an oxide film on the surface of a sacrificial substrate (step S20), a step of forming a film made of an inorganic material on the oxide film formed on the surface of the sacrificial substrate (step S30), a step of forming a waveguide substrate (step S40B), a step of bonding the drive circuit board and the waveguide substrate (step S50B), a step of stacking an EO polymer film (step S60), a step of forming an EO polymer waveguide (step S70), and a step of forming an upper electrode (step S80). The step S10B includes a step of forming a contact electrode on a Si substrate (step S11B), a step of embedding an oxide film in the contact electrode (step S12B), and a step of exposing the surface of the contact electrode by CMP (step S13B). In this embodiment, a bare Si substrate is also used as a sacrificial substrate, and an oxide film is formed on the bare Si substrate in step S20. In this embodiment, Si3N4 is also used as an inorganic material, and an Si3N4 film is formed on the oxide film in step S30. However, the process of forming a waveguide substrate (step S40B) includes a process of forming a Si3N4 waveguide (step S41), a process of forming a clad (oxide film) on the Si3N4 waveguide and flattening the surface of the clad (step S42), and a process of forming lower electrodes and burying the lower electrodes in the clad (oxide film) (step S43). Step S50B is a process in which the accuracy of alignment during bonding can be relaxed compared to step S50, as described later.
[0065] (Process for forming a drive circuit board) In the step of forming the drive circuit board (step S10B), in the step S11B, as shown in FIG. 10(a) and FIG. 10(b), a contact electrode 71 corresponding to the number of waveguides is formed on the surface of the substrate 41 using a normal semiconductor integrated circuit manufacturing process. The contact electrode 71 is an electrode on the surface connected to the drive circuit 31. In step S11B, the contact electrode 71 is formed smaller than the lower electrode 33. It is desirable that the length of the contact electrode 71 in the x direction is equal to or shorter than the length of the lower electrode 33 in the x direction, and it is desirable that the length of the contact electrode 71 in the z direction is shorter than the length of the lower electrode 33 in the z direction. The contact electrode 71 can be made of a general metal material, as with the lower electrode 33. The contact electrode 71 can be formed by stacking a plurality of types of metal films. In that case, it is preferable that the metal film on the outermost surface is made of Au or Cu.
[0066] Next, in the process of step S12B, as shown in FIG. 10(c) and FIG. 10(d), an oxide film 43 is formed so as to cover the surface of the contact electrode 71. Next, in the process of step S13B, as shown in FIG. 10(e) and FIG. 10(f), the oxide film 43 on the contact electrode 71 is first flattened. As a method of flattening, a CMP method or the like can be used. However, in step S13B, in the CMP polishing, the polishing agent (slurry) is changed, the oxide film 43 on the contact electrode 71 is removed, the upper surface 77 of the contact electrode 71 is exposed, and the step between the upper surface 77 of the contact electrode 71 and the upper surface 79 of the oxide film 43 adjacent to the contact electrode 71 is made as small as possible. Note that the step between the upper surface 77 of the contact electrode 71 and the upper surface 79 of the oxide film 43 is preferably 5 to 10 nm or less. For convenience, this finally completed substrate is called a drive circuit substrate 73.
[0067] By the process of step S10B, a plurality of drive circuits 31 are embedded, and a drive circuit board 73 is formed having a plurality of contact electrodes 71 each electrically connected to the plurality of drive circuits 31. Most of the upper surface of drive circuit board 73 is covered with oxide film 43, but drive circuit board 73 differs from drive circuit board 45 (see FIG. 4(f)) in that upper surfaces 77 of contact electrodes 71 are exposed. It should be noted that steps S20 and S30 are the same as the manufacturing process shown in FIG. 3, and therefore a description thereof will be omitted.
[0068] (Process for forming a waveguide substrate) In the step of forming a waveguide substrate (step S40B), a step of forming a Si3N4 waveguide (step S41) shown in FIG. 5(e) and FIG. 5(f) and a cladding and flattening step (step S42) shown in FIG. 5(g) and FIG. 5(h) are performed, which is similar to step S40 shown in FIG. 3. When steps S41 and S42 are completed, a waveguide substrate 57 (see FIG. 5(h)) is completed. The waveguide substrate 57 includes a plurality of pairs of a Si3N4 waveguide 8a and a Si3N4 waveguide 8b. The upper surface 59 of the waveguide substrate 57 is entirely covered with an oxide film 55. Next, in the step of embedding a lower electrode (step S43), first, a lower electrode 33 is formed in the region between the Si3N4 waveguide 8a and the Si3N4 waveguide 8b in the z direction as shown in FIG. 11(a) and FIG. 11(b).
[0069] In detail, in step S43, as shown in FIG. 5(h), a metal film made of an electrode material is formed on the entire upper surface 59 of the waveguide substrate 57 on which the Si3N4 waveguide 8a and the Si3N4 waveguide 8b are already formed. Then, patterning is performed by photolithography so that the desired arrangement and shape are obtained as the lower electrode. At this time, since photolithography is used, the position of the lower electrode 33 relative to the region between the Si3N4 waveguide 8a and the Si3N4 waveguide 8b can be patterned with alignment accuracy of sub-μm order. The lower electrode 33 can be formed by stacking a plurality of types of metal films. In this case, it is preferable that the outermost metal film is formed of the same material as the outermost metal film of the contact electrode 71. When the metal film on the outermost surface of the contact electrode 71 is formed of Au, the metal film on the outermost surface of the lower electrode 33 is also formed of Au, and when the metal film on the outermost surface of the contact electrode 71 is formed of Cu, the metal film on the outermost surface of the lower electrode 33 is also formed of Cu.
[0070] In step S43, after the lower electrode 33 is formed, a process of burying the lower electrode 33 with an oxide film is performed, and then a process of exposing the lower electrode 33 by the CMP method is performed. These processes are similar to the processes in step S12B (see FIG. 10(c) and FIG. 10(d)) and step S13B (see FIG. 10(e) and FIG. 10(f)), and therefore detailed explanations are omitted. Note that FIG. 11(a) and FIG. 11(b) show a state in which the oxide film on the lower electrode 33 is removed by CMP polishing to expose the upper surface 85 of the lower electrode 33, and the step between the upper surface 85 of the lower electrode 33 and the upper surface 83 of the oxide film 55 adjacent to the lower electrode 33 is minimized. For convenience, this finally completed substrate is called a waveguide substrate 81. The waveguide substrate 81 has most of its upper surface covered with an oxide film 55, but differs from the waveguide substrate 57 (see FIG. 5(h)) in that the lower electrode 33 is embedded and its upper surface 85 is exposed.
[0071] (Step of bonding the drive circuit board and the waveguide board) In the process of bonding the drive circuit board and the waveguide substrate (step S50B), as shown in Figures 11(c) and 11(d), the waveguide substrate 81 is laminated on the drive circuit board 73. At this time, the drive circuit board 73 and the waveguide substrate 81 are bonded such that the contact electrodes 71 of the drive circuit board 73 and the lower electrodes 33 of the waveguide substrate 81 face each other.
[0072] Before bonding the two substrates, as shown in FIG. 10(f), the upper surface 77 of the contact electrode 71 and the upper surface 79 of the oxide film 43 of the drive circuit substrate 73 were flattened. Also, as shown in FIG. 11(b), the upper surface 85 of the lower electrode 33 and the upper surface 83 of the oxide film 55 of the waveguide substrate 81 were flattened. Therefore, when the two substrates are bonded, the contact electrode 71 of the drive circuit substrate 73 and the lower electrode 33 of the waveguide substrate 81 are bonded, and the oxide film 43 of the drive circuit substrate 73 and the oxide film 55 of the waveguide substrate 81 are bonded. That is, the electrodes are bonded to each other and the oxide films are bonded to each other. In particular, if the upper surface 77 of the contact electrode 71 and the upper surface 85 of the lower electrode 33 are formed of gold (Au), atomic-level diffusion occurs on the Au-Au surface, resulting in a strong bond, so it is preferable to form each electrode in this manner. Alternatively, the upper surface 77 of the contact electrode 71 and the upper surface 85 of the lower electrode 33 may each be formed of Cu, and then firmly joined by Cu-Cu bonding. After step S50B, steps S60, S70, and S80 are similar to the manufacturing process shown in FIG. 3, and therefore a description thereof will be omitted.
[0073] According to the manufacturing method of the second embodiment, the lower electrode 33 of the waveguide substrate 81 is already aligned with the Si3N4 waveguides 8a, 8b before the step of bonding the two substrates. Also, the contact electrode 71 of the drive circuit substrate 73 is formed smaller than the lower electrode 33 of the waveguide substrate 81, and it does not matter if the larger lower electrode 33 is electrically connected to the smaller contact electrode 71 during bonding. Therefore, according to the manufacturing method of the second embodiment, the alignment during bonding of the two substrates (step S50B) can be significantly relaxed compared to the alignment in step S50 shown in FIG.
[0074] (Modification) In the manufacturing method according to the second embodiment, as in the manufacturing method according to the first embodiment, the optical control device 1B shown in FIG. 8(a) and the optical control device 1C shown in FIG. 8(b) can be manufactured in the same manner. Note that the shape of the grating is not limited to that shown in FIG. 8(a) and FIG. 8(b). In addition, in the manufacturing method according to the second embodiment, an optical control device in which a plurality of Si3N4 waveguides 8b are non-periodically arranged can be manufactured.
[0075] In addition, when a light control device that does not require a gap between the Si3N4 waveguides 8a, 8b and the EO polymer waveguide 9 is manufactured by the manufacturing method according to the second embodiment, the process of step S20 shown in Figures 5(a) and 5(b) may be omitted. In this case, in the process of step S30 shown in Figures 5(c) and 5(d), a Si3N4 film 53 is formed on a Si substrate (sacrificial substrate 49) at a temperature exceeding the heat resistance temperature of the semiconductor integrated circuit.
[0076] Also, in the manufacturing method according to the second embodiment, in the process of step S30 shown in FIG. 9, FIG. 5(c) and FIG. 5(d), a Si3N4 film is formed on the oxide film 51 formed on the surface of the sacrificial substrate 49 made of a Si substrate, but the present invention is not limited to this. For example, when manufacturing an optical control device that does not require a gap between the Si3N4 waveguides 8a, 8b and the EO polymer waveguide 9 due to the oxide film 51 (intermediate clad 20a), the process of step S20 shown in FIG. 9, FIG. 5(a) and FIG. 5(b) may be omitted. In this case, in the process of step S30 following step S10B, the Si3N4 film 53 is simply formed on the Si substrate (sacrificial substrate 49) at a temperature exceeding the heat resistance temperature of the semiconductor integrated circuit, and the subsequent processes can be performed in the same manner. [Explanation of symbols]
[0077] 1,1B,1C Optical control device 2. Optical Phased Array 3 Optical input section 4 Light separation section 5 Phase control section 6 Multi-optical waveguide section 7 Optical output terminal 8a Si3N4 waveguide (input inorganic waveguide) 8b,8B,8C Si3N4 waveguide (output side inorganic waveguide) 9 EO Polymer Waveguide 10 Substrate 11 Input side optical coupling section 12 Output side optical coupling section 20 Clad 20a mid-clad 20b Lower Cladding 20c upper cladding 30 Phase control circuit drive circuit section 31 Drive circuit 33 Lower electrode (1st electrode) 35 Upper electrode (second electrode) 41 Substrate 43 Oxide Film 45 Drive circuit board 47 Top 49 Sacrificial Substrate 51 Oxide Film 53 Si3N4 film 55 Oxide Film 57 Waveguide Substrate 59 Top 61 Surface 63 EO polymer film 65 Oxide Film 67,69 Grating 71 Contact electrode 73 Drive circuit board 77,79 Top surface 81 Waveguide Substrate 83,85 Top surface
Claims
1. a phase control section drive circuit section formed of a semiconductor integrated circuit having a plurality of drive circuits for driving the optical phased array embedded therein and a plurality of first electrodes each electrically connected to the plurality of drive circuits; An optical phased array mounted on the phase control unit drive circuit unit, The optical phased array includes: a light splitting unit having a plurality of input-side inorganic waveguides and splitting incident light into a plurality of channels; a phase control section having a plurality of EO polymer waveguides for guiding light separated into a plurality of channels; a multi-optical waveguide section having a plurality of output-side inorganic waveguides on extensions of a plurality of input-side inorganic waveguides, and guiding phase-controlled light; a common second electrode formed on the phase control section so as to overlap the plurality of first electrodes in a plan view with different heights, a height of the EO polymer waveguide, and heights of the input side inorganic waveguide and the output side inorganic waveguide are made different, and the EO polymer waveguide has an overlapping region with the input side inorganic waveguide and the output side inorganic waveguide in a plan view; An optical control device characterized in that in the phase control unit driving circuit unit, the multiple first electrodes are formed along the EO polymer waveguide with different heights in the region between the input side inorganic waveguide and the output side inorganic waveguide.
2. The cores of the input side inorganic waveguide and the output side inorganic waveguide are made of Si 3 N 4 2. The optical control device according to claim 1, wherein the optical control device is formed of:
3. A method for manufacturing an optical control device in which a phase control section drive circuit section made of a semiconductor integrated circuit and an optical phased array are integrally formed, comprising: forming a drive circuit substrate having a plurality of drive circuits embedded therein and a plurality of first electrodes respectively connected to the plurality of drive circuits; forming a film made of an inorganic material on a sacrificial substrate at a temperature exceeding a heat-resistant temperature of the semiconductor integrated circuit; A process of forming a waveguide substrate including a plurality of pairs of an input side inorganic waveguide and an output side inorganic waveguide arranged on an extension line of the input side inorganic waveguide by patterning the film made of the inorganic material; a step of bonding the drive circuit board and the waveguide substrate such that the first electrode overlaps a region between the input side inorganic waveguide and the output side inorganic waveguide in a plan view; a step of laminating an EO polymer film on the surface exposed by removing the sacrificial substrate so as to overlap the input side inorganic waveguide and the output side inorganic waveguide in a plan view; dividing the EO polymer film to form a plurality of EO polymer waveguides along the pair of the input inorganic waveguide and the output inorganic waveguide; and forming a common second electrode on the plurality of EO polymer waveguides so as to overlap the plurality of first electrodes in a planar view.
4. A method for manufacturing an optical control device in which a phase control section drive circuit section made of a semiconductor integrated circuit and an optical phased array are integrally formed, comprising: forming a drive circuit substrate having a plurality of drive circuits embedded therein and a plurality of contact electrodes respectively connected to the plurality of drive circuits; forming a film made of an inorganic material on a sacrificial substrate at a temperature exceeding a heat-resistant temperature of the semiconductor integrated circuit; A step of patterning the film made of the inorganic material to form a plurality of pairs of an input side inorganic waveguide and an output side inorganic waveguide arranged on an extension line of the input side inorganic waveguide; forming a waveguide substrate by forming first electrodes in regions between the input-side inorganic waveguide and the output-side inorganic waveguide; bonding the drive circuit board and the waveguide substrate so that the contact electrodes and the first electrodes face each other; a step of laminating an EO polymer film on the surface exposed by removing the sacrificial substrate so as to overlap the input side inorganic waveguide and the output side inorganic waveguide in a plan view; dividing the EO polymer film to form a plurality of EO polymer waveguides aligned with the input inorganic waveguide and the output inorganic waveguide; and forming a common second electrode on the plurality of EO polymer waveguides so as to overlap the plurality of first electrodes in a planar view.
5. The cores of the input side inorganic waveguide and the output side inorganic waveguide are made of Si 3 N 4 5. The method for manufacturing an optical control device according to claim 3, wherein the optical control device is formed of
6. A step of forming an oxide film on a surface of the sacrificial substrate before a step of forming a film made of an inorganic material on the sacrificial substrate, 5. The method for manufacturing an optical control device according to claim 3, further comprising forming a film made of the inorganic material on the oxide film formed on the surface of the sacrificial substrate at a temperature exceeding the heat resistance temperature of the semiconductor integrated circuit.
7. The oxide film is SiO 2 It consists of: the sacrificial substrate is a Si substrate, The sacrificial substrate made of the Si substrate was removed by dry etching using xenon difluoride gas to expose the SiO 2 7. The method for manufacturing an optical control device according to claim 6, further comprising laminating the EO polymer film on a surface of an oxide film consisting of:
Citation Information
Patent Citations
Hybrid array waveguide type light deflector
JP2022133031A