Manufacturing method for electrostatic chuck

The method of laser processing and mirror polishing in electrostatic chuck manufacturing addresses uneven protrusion issues, enhancing stability and temperature control by ensuring uniform protrusion heights and positions, thus improving wafer holding and reducing gas leakage.

JP2024135977AActive Publication Date: 2024-10-04NITERRA CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023046914
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-23
Publication Date
2024-10-04
Estimated Expiration
2043-03-23

AI Technical Summary

Technical Problem

Existing electrostatic chucks face issues with uneven protrusion heights and positions due to thermal expansion differences between the chuck and wafer, leading to unstable wafer holding and improper temperature control, especially after reprocessing.

Method used

A method involving laser processing to adjust the machining amount for each convex portion and concave bottom surface, ensuring uniform heights and positions of protrusions, followed by mirror polishing to enhance surface smoothness.

Benefits of technology

Stabilizes wafer holding and improves temperature control by making protrusion heights uniform, preventing reduced adsorption force and inert gas leakage, while maintaining withstand voltage characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024135977000001_ABST
    Figure 2024135977000001_ABST
Patent Text Reader

Abstract

To provide a manufacturing method for an electrostatic chuck having a plurality of protrusions, which provides another technique for making the positions of the plurality of protrusions in the height direction approximately uniform.SOLUTION: A manufacturing method for an electrostatic chuck including a plate-shaped portion having a first surface with a plurality of convex portions and a concave bottom surface between the plurality of convex portions, and a second surface which is the reverse side of the first surface, and capable of holding an object on the first surface of the plate-shaped portion, includes an electrostatic chuck preparation step of preparing an electrostatic chuck, a processing amount data preparation step of preparing processing amount data indicating the processing amount of at least one of the plurality of convex portions and the concave bottom surface of the first surface of the prepared electrostatic chuck, and a laser processing step of laser processing at least one of the plurality of convex portions and the concave bottom surface of the prepared electrostatic chuck on the basis of the processing amount data.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing an electrostatic chuck. [Background technology]

[0002] For example, an electrostatic chuck is used as a holding device for holding an object such as a wafer during semiconductor manufacturing. The electrostatic chuck includes a plate-shaped portion on which the object is placed and a chuck electrode that is disposed inside the plate-shaped portion and generates an electrostatic attractive force, and uses the electrostatic attractive force generated by applying a voltage to the chuck electrode to attract and hold the wafer or the like onto the surface of the plate-shaped portion (hereinafter also referred to as the "attraction surface").

[0003] Conventionally, in an electrostatic chuck, the temperature distribution of the attracting surface of the plate-shaped portion is controlled by heating with a heater electrode disposed on the plate-shaped portion, or by cooling by supplying a coolant to a coolant flow path formed in a base member joined to the plate-shaped portion, thereby controlling the temperature distribution of a wafer held by the electrostatic chuck. By controlling the temperature of the wafer in this manner, the accuracy of each process (film formation, etching, etc.) on the wafer can be improved.

[0004] In some electrostatic chucks, a continuous wall-shaped convex portion (hereinafter referred to as "wall-shaped convex portion") is formed near the outer edge of the attracting surface of the plate-shaped portion, and a plurality of independent columnar convex portions (hereinafter referred to as "columnar convex portions") are formed in an area on the inside of the wall-shaped convex portion on the attracting surface of the plate-shaped portion. In such electrostatic chucks, the area on the inside of the wall-shaped convex portion on the attracting surface of the plate-shaped portion where no columnar convex portion is formed is a concave bottom surface. The wall-shaped convex portion and each columnar convex portion (when not distinguishing between them, they are also simply called "convex portions") are formed, for example, by arranging a mask that shields the parts corresponding to each convex portion on the planar surface of the plate-shaped portion, and performing shot blasting to project particles such as ceramics.

[0005] The wafer is supported by a plurality of convex portions on the suction surface of the plate-shaped portion. In this state, a space exists between the surface of the wafer and the concave portions on the suction surface of the plate-shaped portion. In order to improve the heat transfer characteristics between the wafer and the plate-shaped portion and to improve the controllability of the temperature distribution of the wafer, an inert gas such as helium gas may be supplied into the space.

[0006] When such an electrostatic chuck is used repeatedly, contaminants such as residual cleaning liquid from the wafer adhere to the attracting surface of the plate-shaped part, or fine irregularities are formed on the attracting surface of the plate-shaped part. Hereinafter, the layer on the attracting surface of the plate-shaped part to which the contaminants adhere or on which fine irregularities are formed is referred to as an altered layer. When an altered layer of a certain thickness is formed on the attracting surface of the plate-shaped part, the adsorption force for adsorbing the wafer decreases, or the adhesion between the wall-shaped convex part and the wafer decreases, which may cause leakage of inert gas. Therefore, in such a case, a process is performed to regenerate the electrostatic chuck by removing the altered layer.

[0007] As a process for regenerating an electrostatic chuck, a technique has been proposed in which a mask is placed to shield the areas corresponding to the multiple convex portions, the deteriorated layer in the concave portions is removed by shot blasting, and then the top surfaces of the multiple convex portions are mirror-polished to remove the deteriorated layer on the top surfaces (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0008] [Patent Document 1] Patent No. 7096133 Summary of the Invention [Problem to be solved by the invention]

[0009] The technology described in Patent Document 1 is said to be able to prevent the thickness of the plate-shaped portion (the distance from the chuck electrode to the adsorption surface) from becoming excessively thin, thereby preventing a decrease in voltage resistance characteristics, and to prevent a decrease in uniformity in the heights of multiple convex portions.

[0010] Incidentally, when the electrostatic chuck is new, the positions and heights of the multiple protrusions of the plate-shaped part are approximately uniform. However, the plate-shaped part of the electrostatic chuck and the wafer often have different thermal expansion coefficients, and the plate-shaped part and the wafer may rub against each other due to the difference in thermal expansion between the plate-shaped part and the wafer caused by temperature changes during use of the electrostatic chuck, causing the multiple protrusions to be scraped. As a result, the amount of scraping at each protrusion may not be the same, and the positions of the multiple protrusions in the height direction may become uneven. Even if the plate-shaped part of the electrostatic chuck and the wafer have the same thermal expansion coefficient, the surface pressure applied to each protrusion when the wafer is held by the electrostatic chuck is different, so the amount of scraping at each protrusion may differ, causing the positions of the multiple protrusions in the height direction to become uneven.

[0011] In this way, when the height positions of the multiple protrusions in the electrostatic chuck to be regenerated are non-uniform, in the technology described in the above Patent Document 1, the height positions of the multiple protrusions of the electrostatic chuck after the regeneration process remain non-uniform, just as they were before the regeneration. In this case, when the regenerated electrostatic chuck is used, there is a risk that the wafer cannot be stably held. In addition, when the heights of the multiple protrusions are non-uniform, there is a risk that the wafer temperature cannot be appropriately controlled due to the above-mentioned bias of the inert gas.

[0012] Note that this problem is not limited to the method for regenerating an electrostatic chuck, but is a problem common to all manufacturing methods for electrostatic chucks having a plurality of protrusions.

[0013] The present invention has been made to solve the above-mentioned problems, and has an object to provide another technique for making the height-wise positions of the multiple protrusions approximately uniform in a manufacturing method for an electrostatic chuck having multiple protrusions. [Means for solving the problem]

[0014] The present invention has been made to solve the above-mentioned problems, and can be realized in the following forms.

[0015] (1) According to one aspect of the present invention, there is provided a method for manufacturing an electrostatic chuck that includes a plate-shaped portion having a first surface with a plurality of protrusions and a concave bottom surface between the plurality of protrusions, a second surface that is a back surface of the first surface, and a chuck electrode that is disposed inside the plate-shaped portion and generates an electrostatic attraction force, and that can hold an object on the first surface of the plate-shaped portion. The method for manufacturing an electrostatic chuck includes an electrostatic chuck preparation step of preparing the electrostatic chuck, a processing amount data preparation step of preparing processing amount data indicating a processing amount of at least one of the plurality of protrusions and the concave bottom surface of the first surface of the prepared electrostatic chuck, and a laser processing step of laser processing at least one of the plurality of protrusions and the concave bottom surface of the prepared electrostatic chuck based on the processing amount data.

[0016] According to the manufacturing method of the electrostatic chuck of this embodiment, since the laser processing step is included, the processing amount can be changed for each of the convex portions and the concave bottom surface. Therefore, even if the positions of the multiple convex portions in the height direction are not uniform, the positions of the top surfaces of the multiple convex portions in the height direction can be made constant by changing the processing amount for each convex portion. This can improve the stability of supporting the wafer by the electrostatic chuck. In addition, when the positions of the concave bottom surface in the height direction differ for each location of the concave bottom surface, the heights of the multiple convex portions can be made approximately uniform by changing the processing amount for each location on the concave bottom surface. In this way, the temperature control of the wafer can be appropriately performed. Furthermore, since the processing amount can be changed for each location by the laser processing, the heights of the multiple convex portions can be made approximately uniform while suppressing the processing amount. In other words, the reduction in the thickness of the plate-shaped portion can be suppressed, and the reduction in the withstand voltage characteristics can be suppressed.

[0017] (2) In the method for manufacturing an electrostatic chuck according to the above aspect, the laser processing step may include laser processing the plurality of protrusions and the concave bottom surface of the prepared electrostatic chuck. In this way, even if the positions of the top surfaces of the plurality of protrusions in the height direction are nonuniform and the positions of the concave bottom surface in the height direction vary from place to place, the heights of the plurality of protrusions can be made approximately uniform.

[0018] (3) In the method for manufacturing an electrostatic chuck according to the above aspect, the processing amount data may be determined so that the lowest position in the height direction of the top faces of the plurality of protrusions measured with reference to a predetermined reference plane of the plate-shaped portion of the prepared electrostatic chuck becomes the new position of the top faces of the plurality of protrusions after the laser processing, and the heights of the plurality of protrusions are approximately constant. In this way, the processing amount can be reduced, and therefore a decrease in the thickness of the plate-shaped portion can be further suppressed.

[0019] (4) In the method for manufacturing an electrostatic chuck according to the above aspect, the processing amount data preparation step may include a measurement step of measuring the height positions of the top faces of the plurality of protrusions and the height position of the concave bottom face with respect to the predetermined reference plane of the plate-like portion of the prepared electrostatic chuck, and a processing amount data creation step of creating the processing amount data using the measurement results of the height positions of the top faces of the plurality of protrusions and the height position of the concave bottom face in the measurement step. Even in this manner, it is possible to suppress a decrease in the thickness of the plate-like portion and to make the heights of the plurality of protrusions approximately uniform.

[0020] (5) In the method for manufacturing an electrostatic chuck according to the above aspect, the electrostatic chuck preparation step may include preparing an electrostatic chuck having top surfaces of the plurality of protrusions at different positions in the height direction. Even in this case, since the laser processing step is included, the amount of processing of each protrusion can be made different, thereby suppressing a decrease in the thickness of the plate-shaped portion and making the heights of the plurality of protrusions approximately uniform.

[0021] (6) The method for manufacturing an electrostatic chuck according to the above aspect may further include a mirror polishing step of mirror-polishing the top surfaces of the plurality of convex portions of the plate-shaped portion after the laser processing step. In this way, it is possible to suppress a decrease in the surface roughness of the top surfaces of the convex portions after the laser processing step. As a result, it is possible to reduce the probability that a wafer will come into point contact with the plurality of convex portions of the electrostatic chuck compared to a case in which the mirror polishing step is not performed, and it is possible to suppress the generation of particles (contamination).

[0022] The present invention can be realized in various forms, for example, in the form of a manufacturing method for a semiconductor manufacturing device including an electrostatic chuck. [Brief description of the drawings]

[0023] [Figure 1] 1 is a perspective view showing an outline of an external configuration of an electrostatic chuck according to an embodiment; [Diagram 2] FIG. 2 is an explanatory diagram illustrating a schematic XZ cross-sectional configuration of the electrostatic chuck. [Diagram 3] 4 is an explanatory diagram showing a planar configuration of a first surface side of a plate-shaped portion. FIG. [Figure 4] 1A to 1C are process diagrams showing a flow of a manufacturing method for an electrostatic chuck. [Diagram 5] 4A to 4C are explanatory views of some of the steps of a method for manufacturing an electrostatic chuck. [Figure 6] 4A to 4C are explanatory views of some of the steps of a method for manufacturing an electrostatic chuck. [Figure 7] 1A to 1C are explanatory diagrams conceptually illustrating an example of a method for manufacturing an electrostatic chuck. [Figure 8] 1A to 1C are explanatory diagrams conceptually showing a manufacturing method of an electrostatic chuck of a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0024] <Embodiment> FIG. 1 is a perspective view that shows a schematic external configuration of an electrostatic chuck 10 according to an embodiment. FIG. 2 is an explanatory diagram that shows a schematic XZ cross-sectional configuration of the electrostatic chuck 10. In FIG. 1 and FIG. 2, mutually orthogonal X, Y and Z axes are shown to specify the directions. In FIG. 2, the positive Y direction is the direction toward the back side of the paper. In this specification, for convenience, the positive Z direction is referred to as the upward direction and the negative Z direction is referred to as the downward direction, but the electrostatic chuck 10 may actually be installed in a direction different from these directions.

[0025] The electrostatic chuck 10 is a device that attracts and holds an object (e.g., a wafer W) by electrostatic attraction, and is used, for example, to fix the wafer W in a vacuum chamber of a semiconductor manufacturing device. The electrostatic chuck 10 includes a plate-shaped portion 100, a cooling portion 200, and a joining portion 400 that joins the plate-shaped portion 100 and the cooling portion 200, which are arranged side by side in the vertical direction (Z-axis direction).

[0026] The plate-shaped portion 100 is a plate-shaped member having a first surface S1 and a second surface S2 which is the back surface of the first surface S1. In detail, the plate-shaped portion 100 includes a first plate-shaped portion 110 which is a plate-shaped member having a first surface S1 which is substantially circular and flat, and a second plate-shaped portion 120 which is a plate-shaped member having a second surface S2 which is substantially circular and flat and has a larger diameter than the first plate-shaped portion 110, and is a plate-shaped member whose diameter increases stepwise downward (toward the negative direction of the Z axis) (FIG. 1). In this embodiment, the first surface S1 of the plate-shaped portion 100 functions as a mounting surface on which the wafer W is mounted. A third surface S3 which is the upper surface (the surface in the positive direction of the Z axis) of the second plate-shaped portion 120 is engaged with, for example, a jig (not shown) for fixing the electrostatic chuck 10.

[0027] The plate-shaped portion 100 is a dense body mainly composed of ceramics (e.g., alumina, aluminum nitride, etc.) known as fine ceramics or new ceramics. In this specification, when a specific component is "the main component" or "the main material forming the specific component," it means that the content of the specific component is 50 volume % or more. In other embodiments, the plate-shaped portion 100 may be formed mainly of a material other than ceramics, such as a resin such as polyimide, or transparent glass.

[0028] The diameter of the first surface S1 of the first plate-shaped portion 110 is, for example, about 50 mm to 500 mm (usually about 200 mm to 350 mm). In this specification, when a numerical range is described using "to" it is intended to include the lower limit and the upper limit unless otherwise specified. For example, the description "10 to 20" is intended to include both the lower limit "10" and the upper limit "20". In other words, "10 to 20" has the same meaning as "10 or more and 20 or less".

[0029] A chuck electrode 130 (FIG. 2) made of a conductive material (e.g., tungsten, molybdenum, etc.) is disposed inside the plate-shaped portion 100. The shape of the chuck electrode 130 as viewed in the Z-axis direction is, for example, substantially circular. When a voltage is applied to the chuck electrode 130 from a power source (not shown), an electrostatic force is generated, and the wafer W is attracted and fixed to the first surface S1 of the plate-shaped portion 100 by this electrostatic force.

[0030] Furthermore, inside the plate-shaped part 100, a heater 140 (FIG. 2) that is spiral-shaped as viewed in the Z-axis direction is disposed below the chuck electrode 130 (negative side of the Z-axis). In this embodiment, the heater 140 is a metallized layer formed of tungsten, molybdenum, or the like. The shape of the heater 140 is not limited to this embodiment, and may be, for example, a disk shape. In other embodiments, the plate-shaped part 100 may not include the heater 140.

[0031] FIG. 3 is an explanatory diagram showing a planar configuration of the first surface S1 side of the plate-shaped portion 100. As shown in FIG. 2 and FIG. 3, a continuous wall-shaped convex portion (hereinafter also referred to as "wall-shaped convex portion") 112 is formed on the first surface S1 side of the plate-shaped portion 100. The wall-shaped convex portion 112 is also called a seal band. As shown in FIG. 3, the shape of the wall-shaped convex portion 112 when viewed in the Z-axis direction is annular. Also, as shown in FIG. 2, the shape of the cross section of the wall-shaped convex portion 112 (a cross section parallel to the Z-axis and passing through the center of the above-mentioned circle) is substantially rectangular. The height of the wall-shaped convex portion 112 is, for example, about 10 μm to 20 μm, and is substantially uniform. Also, the width of the wall-shaped convex portion 112 (the size in the direction perpendicular to the extension direction of the wall-shaped convex portion 112 when viewed in the Z-axis direction) is, for example, about 0.5 mm to 5.0 mm. 2 and 3, reference numerals are given to only some of the plurality of protrusions 113 and the plurality of top surfaces 113t, and the remaining reference numerals are omitted. In this specification, the word "approximately" means that manufacturing errors, measurement errors, etc. are allowed.

[0032] In addition, a plurality of independent, substantially cylindrical convex portions (hereinafter, referred to as "columnar convex portions") 114 are formed in an area inside the wall-shaped convex portions 112 of the plate-shaped portion 100. Here, in the area inside the wall-shaped convex portions 112 of the plate-shaped portion 100, a portion between the plurality of columnar convex portions 114 is referred to as a concave bottom surface 116. As shown in the figure, the plurality of columnar convex portions 114 are arranged at substantially equal intervals when viewed in the Z-axis direction. Also, as shown in FIG. 2, the shape of a cross section (cross section parallel to the Z-axis) of each columnar convex portion 114 is substantially rectangular. The height of the columnar convex portion 114 is substantially the same as the height of the convex portion 112, and is, for example, about 10 μm to 20 μm. Also, the width of the columnar convex portion 114 (the maximum diameter of the columnar convex portion 114 when viewed in the Z-axis direction) is, for example, about 0.5 mm to 1.5 mm. The first surface S1 includes a top surface 112t (a surface in the positive Z-axis direction) of the wall-shaped protrusion 112, a top surface 114t (a surface in the positive Z-axis direction) of the columnar protrusion 114, and a concave bottom surface 116. Note that the gas flow path 500 is not shown in FIG.

[0033] The wafer W is supported by the wall-shaped protrusions 112 and the plurality of columnar protrusions 114 of the plate-shaped part 100. At this time, the top surface 112t of the wall-shaped protrusions 112 of the plate-shaped part 100 and the top surface 114t of the plurality of columnar protrusions 114 are in contact with the wafer W. In a state in which the wafer W is supported by the wall-shaped protrusions 112 and the plurality of columnar protrusions 114, a space exists between the surface (lower surface) of the wafer W and the concave bottom surface 116 of the first surface S1 of the plate-shaped part 100. As described later, an inert gas (e.g., helium gas) is supplied to this space. When the wall-shaped protrusions 112 and the columnar protrusions 114 are not distinguished from each other, they are also simply called "protrusions 113", and when the top surface 112t of the wall-shaped protrusions 112 and the top surface 114t of the columnar protrusions 114 are not distinguished from each other, they are also simply called "top surface 113t of the protrusions".

[0034] 2, the electrostatic chuck 10 has a gas flow passage 500 which is a through-hole penetrating the electrostatic chuck 10 in the stacking direction (Z-axis direction). The gas flow passage 500 is a hole for supplying an inert gas (e.g., helium gas) for cooling the wafer W to the above-mentioned space (the space between the front surface (lower surface) of the wafer W and the concave bottom surface 116 of the first surface S1 of the plate-shaped portion 100). Note that the gas flow passage 500 is preferably in a form having a plurality of outlets in the concave bottom surface 116 in order to uniformly supply the inert gas to the above-mentioned space.

[0035] In the electrostatic chuck 10 of the present embodiment, when the wafer W is attracted to the first surface S1 side, an inert gas is supplied to the space between the first plate-shaped portion 110 and the wafer W via the gas flow passage 500. By flowing the inert gas between the electrostatic chuck 10 and the wafer W, the wafer W can be cooled or heated in combination with a heater, thereby controlling the temperature of the wafer W during processing.

[0036] The electrostatic chuck 10 in this embodiment has a plurality of protrusions 113, and an inert gas is filled in the space between the first plate-shaped portion 110 and the wafer W, so that the distribution of the inert gas between the electrostatic chuck 10 and the wafer W becomes uniform, and the wafer W can be held while maintaining a uniform temperature distribution of the wafer W. In addition, since the plate-shaped portion 100 has a plurality of columnar protrusions 114, the remaining time of the chucking force after the voltage to the chuck electrode 130 is removed can be shortened.

[0037] The cooling part 200 is a plate-like member having a substantially circular flat shape with a larger diameter than the plate-like part 100. The cooling part 200 may contain at least one metal selected from the group consisting of aluminum, magnesium, molybdenum, titanium, tungsten, and nickel. Among the above-mentioned metals, molybdenum, titanium, and tungsten have relatively small coefficients of thermal expansion, and therefore, when the cooling part 200 is constructed using at least one of these metals, it is desirable to suppress the difference in coefficient of thermal expansion between the cooling part 200 and the plate-like part 100. In this specification, the term "coefficient of thermal expansion" refers to the "coefficient of linear expansion." Furthermore, since magnesium has a relatively small Young's modulus, when the cooling part 200 is constructed using magnesium, it is desirable to reduce the thermal stress generated in the cooling part 200. Furthermore, aluminum has a relatively high thermal conductivity, is easy to process, and is low in cost. Therefore, when the cooling part 200 is constructed using aluminum, it is desirable to increase the cooling efficiency of the plate-like part 100 and the wafer W by the cooling part 200 and suppress the manufacturing cost of the electrostatic chuck 10. From the viewpoint of suppressing manufacturing costs while increasing the cooling efficiency of the cooling part 200, it is desirable that the cooling part 200 has a high metal content, and it is desirable that the cooling part 200 is mainly composed of metal. For example, it is desirable that the cooling part 200 contains 90 mass % or more of aluminum, which is highly versatile (for example, it is made of an aluminum alloy such as A6061 or A5052). However, the cooling part 200 may contain components other than metal, such as ceramic. The diameter of the cooling part 200 is, for example, about 220 mm to 550 mm (usually 220 mm to 350 mm), and the thickness of the cooling part 200 is, for example, about 20 mm to 40 mm.

[0038] A coolant flow passage 210 (FIG. 2) is formed inside the cooling part 200. When the wafer W held on the plate-shaped part 100 of the electrostatic chuck 10 is processed using plasma, heat is input from the plasma to the wafer W, and the temperature of the wafer W rises. When a coolant (e.g., a fluorine-based inert liquid or water) flows through the coolant flow passage 210 formed in the cooling part 200, the cooling part 200 is cooled. The plate-shaped part 100 is cooled by heat transfer between the cooling part 200 and the plate-shaped part 100 via the bonding part 400, and the wafer W held on the first surface S1 of the plate-shaped part 100 is cooled. This realizes temperature control of the wafer W. In other embodiments, the cooling part may not have a coolant flow passage formed therein, and may be cooled from the outside.

[0039] The joining part 400 is a substantially circular flat plate-like member having the same diameter as the second surface S2 of the plate-like part 100, and joins the plate-like part 100 and the cooling part 200. The joining part 400 is formed from an adhesive, and for example, an adhesive mainly composed of an organic material such as acrylic or polyimide, or silicone, etc. can be used.

[0040] The electrostatic chuck 10 can be manufactured, for example, by regenerating a used electrostatic chuck 10 . Fig. 4 is a process diagram showing the flow of a manufacturing method of the electrostatic chuck 10. Figs. 5 and 6 are explanatory views of some of the processes of the manufacturing method of the electrostatic chuck 10. Figs. 5 and 6 show an enlarged portion of the cross section of the electrostatic chuck 10 similar to that of Fig. 2.

[0041] When the electrostatic chuck 10 is used repeatedly, contaminants such as residues of a cleaning liquid from the wafer W adhere to the first surface S1 and the third surface S3 of the plate-shaped portion 100, and minute irregularities are formed. Hereinafter, the layer on the plate-shaped portion 100 to which the contaminants adhere or to which minute irregularities are formed is referred to as an altered layer TL (FIG. 5(A)). When an altered layer TL of a certain thickness is formed on the first surface S1 of the plate-shaped portion 100, the chucking force for chucking the wafer W decreases, or the adhesion between the wall-shaped convex portion 112 and the wafer W decreases, which may cause leakage of the inert gas.

[0042] Furthermore, when the electrostatic chuck 10 is used repeatedly, the wafer W and the plate-shaped part 100 rub against each other due to the difference in thermal expansion between them, and the top surfaces 112t and 114t of the multiple protrusions 113 (the wall-shaped protrusions 112 and the multiple columnar protrusions 114) may be scraped off. The amount by which the top surfaces 112t and 114t are scraped off may differ for each protrusion. For example, the difference in thermal expansion between the wafer W and the plate-shaped part 100 is greater toward the periphery, so the outer periphery is more likely to be scraped off. Furthermore, when the wafer W is attracted to the electrostatic chuck 10, the surface pressure applied to the multiple protrusions 113 is different. The outermost periphery has a low surface pressure and is less likely to be scraped off. Furthermore, the protrusions may be scraped off when the wafer W is dechucked or when the electrostatic chuck is cleaned. Furthermore, the plate-shaped part 100 may be warped due to the difference in thermal expansion between the plate-shaped part 100 and the cooling part 200. Therefore, after repeated use, the electrostatic chuck 10 may have variation in height of the plurality of protrusions 113. In such a case, the chucking force for chucking the wafer W may decrease, or the adhesion between the wall-like protrusions 112 and the wafer W may decrease, which may cause leakage of the inert gas. In such a case, the electrostatic chuck 10 can be regenerated by, for example, the following method (FIG. 4).

[0043] In the electrostatic chuck preparation step P102, an electrostatic chuck 10 is prepared. For example, an electrostatic chuck 10 that is repeatedly used and has a variation in the positions in the height direction of the multiple protrusions 113 and the heights of the multiple protrusions 113 is prepared.

[0044] In the processing amount data preparation step P104, processing amount data indicating the processing amount of at least one of the multiple convex portions 113 and the concave bottom surface 116 of the electrostatic chuck 10 is prepared. This embodiment includes a measurement step P112 in which the height position of the top surfaces 113t of the multiple convex portions 113 and the height position of the concave bottom surface are measured based on a predetermined reference plane of the plate-shaped portion 100 of the electrostatic chuck 10 prepared in the electrostatic chuck preparation step P102, and a processing amount data creation step P114 in which processing amount data is created using the measurement results of the height positions of the top surfaces 112t, 114t of the multiple convex portions 113 and the height position of the concave bottom surface 116 in the measurement step P112.

[0045] In the measurement process P112, for example, a white light interferometer, a laser microscope, or the like is used to measure the height direction (Z-axis direction) position of the top surfaces 113t of the multiple convex portions 113 and the height direction (Z-axis direction) position of the concave bottom surface 116. For example, a contact-type height measurement using a touch probe (device name: Quick Vision, manufactured by Mitutoyo Corporation) can be used to touch the top surfaces 113t of the multiple convex portions 113 and the concave bottom surface 116 around each convex portion 113, and the height can be measured as the difference.

[0046] In this embodiment, the processing amount data is determined so that the lowest position among the height direction positions of the top faces 113t of the multiple convex parts 113 measured in the measurement process P112 becomes the new position of the top faces 113t of the multiple convex parts 113 after laser processing, and the height of the multiple convex parts 113 becomes a substantially constant height. The processing amount data creation process is executed by a computer. In detail, the measurement results of the height direction positions of the top faces 113t of the multiple convex parts 113 and the height direction position of the concave bottom face 116 by a white light interferometer, a laser microscope, etc. are inputted into a computer, and the computer calculates the processing amount using the inputted measurement results, and creates the processing amount data. The method of calculating the processing amount data will be described later.

[0047] In the laser processing step P106, at least one of the multiple convex portions 113 and the concave bottom surface 116 of the electrostatic chuck 10 prepared in the electrostatic chuck preparation step P102 is laser processed based on the processing amount data prepared in the processing amount data preparation step P104. Fig. 5(A) shows how the first surface S1 of the plate-shaped portion 100 is laser processed. As the laser, for example, a non-thermal laser such as an ultrashort pulse laser is used. As shown in the figure, during the laser processing, the third surface S3 of the second plate-shaped portion 120 of the plate-shaped portion 100 is covered with a protective cover PC.

[0048] As described above, the processing amount data prepared in the processing amount data preparation process P104 is determined so that the positions in the height direction and the height of the multiple protrusions 113 are approximately constant, and therefore, by the laser processing in the laser processing process P106, the positions in the height direction and the height of the multiple protrusions 113 become approximately uniform. Also, by the laser processing process P106, the deteriorated layer TL formed on the first surface S1 and the side surface of the first plate-shaped portion 110 of the plate-shaped portion 100 is removed.

[0049] In the surface polishing and machining process P108, surface polishing and machining are performed on the third surface S3, which is the upper surface (the surface on the positive side in the Z-axis direction) of the second plate-shaped portion 120 of the plate-shaped portion 100. Fig. 5(B) shows the surface polishing using a grinder GR and the machining using a machining device MD being performed on the third surface S3 of the second plate-shaped portion 120. The affected layer TL formed on the third surface S3 of the plate-shaped portion 100 is removed by this surface polishing and machining.

[0050] In the mirror polishing process P110, the top surfaces 113t of the multiple convex portions 113 of the plate-shaped portion 100 are ground by mirror polishing. Fig. 6 shows how the top surface 113t of the plate-shaped portion 100 is mirror-polished using a polishing pad PP while a polishing liquid PS is being supplied. This mirror polishing grinds the top surfaces of the wall-shaped convex portion 112 and each of the columnar convex portions 114, and the top surfaces of the wall-shaped convex portion 112 and each of the columnar convex portions 114 become smooth mirror surfaces. During the mirror polishing, the third surface S3 of the plate-shaped portion 100 is covered with a protective cover PC.

[0051] By regenerating the electrostatic chuck through the above process, the altered layer TL that was present on the first surface S1 of the plate-shaped portion 100 is removed, and an electrostatic chuck 10 is produced in which the height-wise positions and heights of the wall-shaped protrusions 112 and the multiple columnar protrusions 114 are approximately uniform.

[0052] 7 is an explanatory diagram conceptually illustrating an example of a method for manufacturing an electrostatic chuck. In FIG. 7, a cross-sectional view of a plate-shaped portion 100 cut in the XZ plane as in FIG. 2 is shown. FIG. 7(A) shows an example of an electrostatic chuck 10 prepared in the electrostatic chuck preparation step P102 described above. The plate-shaped portion 100 shown in FIG. 7(A) has a plurality of protrusions 113 with different heights. In FIG. 7, in order to distinguish three columnar protrusions 114 among the plurality of protrusions 113, they are indicated by adding alphabets at the end as columnar protrusions 114a, 114b, and 114c.

[0053] FIG. 7(B) shows an example of the processing amount data. As shown in FIG. 7(B), the second surface S2 of the plate-shaped part 100 is set as the reference position P0 (also called the reference surface P0), and the height direction position of the top surface 113t of the plurality of convex parts 113 is measured (measurement process P112), and the processing amount data of the plurality of convex parts 113 is determined so that the lowest height direction position P1 is the position of the new top surface 113t (processing amount data creation process P114). In this example, the processing amount data of the concave bottom surface 116 is determined with the height of the new plurality of convex parts 113 set as h. That is, the height direction position P2 of the concave bottom surface 116 is the position obtained by subtracting the height h of the plurality of convex parts 113 from the position P1 of the top surface 113t of the plurality of convex parts 113. In FIG. 7(B), the processing location CP indicated by the processing amount data is cross-hatched. As shown in the figure, the machining amount of the multiple convex portions 113 differs from one another, and the machining amount of the concave bottom surface 116 also differs from place to place.

[0054] Fig. 7(C) is a conceptual diagram of the plate-shaped portion 100 after the laser processing step P106 is completed. As shown in the figure, the processed portion CP shown in Fig. 7(B) is removed by laser processing, and the electrostatic chuck 10 is reconstructed such that the positions in the height direction of the multiple protrusions 113 of the plate-shaped portion 100 are P1, the heights of the multiple protrusions 113 are h, and the positions and heights of the multiple protrusions 113 in the height direction are substantially uniform.

[0055] As described above, the manufacturing method for an electrostatic chuck according to this embodiment includes the laser processing step P106, and the amount of processing can be changed for each convex portion 113 and for each location on the concave bottom surface 116. Therefore, even if the positions of the multiple convex portions 113 in the height direction are not uniform as shown in Fig. 7(A), the positions of the top surfaces of the multiple convex portions 113 in the height direction can be made constant by varying the amount of processing for each convex portion 113. This can improve the stability of supporting the wafer by the electrostatic chuck.

[0056] Furthermore, even if the position in the height direction of concave bottom surface 116 differs for each location on concave bottom surface 116, the heights of multiple protrusions 113 can be made approximately uniform by varying the amount of processing for each location on concave bottom surface 116. Therefore, when the wafer is supported by the electrostatic chuck, the temperature of the wafer can be appropriately controlled.

[0057] In the example shown in Fig. 7, the processing amount data is determined so that the lowest position P1 among the height direction positions of the top faces of the multiple protrusions 113 measured based on the second surface S2 of the plate-shaped portion 100 of the prepared electrostatic chuck is the new position of the top faces of the multiple protrusions 113 after laser processing. Therefore, it is not necessary to process the columnar protrusions 114a and the columnar protrusions 114c whose top faces 114t are located at position P1, and the amount of processing by the laser can be reduced compared to the case where the new positions of the top faces of the multiple protrusions 113 after laser processing are determined to be lower than position P1. As a result, it is possible to suppress a decrease in the withstand voltage characteristic of the electrostatic chuck 10 due to an excessive thinning of the thickness of the plate-shaped portion 100 (specifically, the distance from the first surface S1 to the chuck electrode 130).

[0058] FIG. 8 is an explanatory diagram conceptually showing a manufacturing method of an electrostatic chuck of a comparative example. In the manufacturing method of an electrostatic chuck of a comparative example, the wall-shaped convex portion and each columnar convex portion are completely removed by plane polishing using a grinder or the like, and then, new wall-shaped convex portions and each columnar convex portion are formed by performing shot blasting using a mask. FIG. 8 shows an example of regenerating an electrostatic chuck that is the same as the electrostatic chuck shown in FIG. 7(A). The plate-shaped portion 100 shown in FIG. 8(A) has a variation in height of a plurality of convex portions 113. In FIG. 8(B), the processed portion CP that is cut by plane polishing using a grinder is shown with cross-hatching. In the manufacturing method of an electrostatic chuck of a comparative example, the wall-shaped convex portion 112 and each columnar convex portion 114 are completely removed by plane polishing using a grinder, as shown in FIG. 8(B). Then, the position in the height direction of the upper surface (the surface in the positive direction of the Z axis) of the plate-shaped portion 100 becomes position P3. As shown in the figure, position P3 coincides with the lowest point of the height direction of the concave bottom surface 116, and is lower than position P1. In the comparative example, position P3 is the height direction position of the top surface 113t of the new plurality of convex portions 113. In FIG. 8(C), cross-hatching is added to the processed portion CP to be ground by shot blasting using a mask. In the comparative example, when forming the convex portion 113 having the same height h as the example shown in FIG. 7, the position P4 in the height direction of the concave bottom surface 116 is lower than the position of the chuck electrode 130. Therefore, in the manufacturing method of the electrostatic chuck of the comparative example, the electrostatic chuck cannot be regenerated or the height of the convex portion 113 needs to be lowered. If the height of the convex portion 113 is lowered and regenerated, the amount of inert gas supplied between the wafer W and the concave bottom surface 116 may be insufficient, and the temperature control of the wafer W may not be performed appropriately. Furthermore, when regenerated by the method of the comparative example, the thickness of the plate-shaped portion 100 (the distance from the chuck electrode 130 to the first surface S1) becomes excessively thin, which may deteriorate the withstand voltage characteristics of the electrostatic chuck 10. In contrast, in the example shown in Fig. 7, the amount of processing of the plate-shaped portion 100 can be reduced compared to the manufacturing method of the electrostatic chuck of the comparative example, and therefore it is possible to suppress the thickness of the plate-shaped portion 100 (specifically, the distance from the first surface S1 to the chuck electrode 130) becoming excessively thin and thus the deterioration of the withstand voltage characteristics of the electrostatic chuck 10.Moreover, according to the manufacturing method of the electrostatic chuck of the embodiment, the number of times of regeneration can be increased compared to the manufacturing method of the comparative example.

[0059] Moreover, the manufacturing method for an electrostatic chuck according to the present embodiment includes a mirror polishing step P110. Since the top surfaces of the convex portions 113 after the degraded layers TL are removed by the laser processing step P106 have poor surface roughness, the top surfaces of the convex portions 113 are mirror polished in the mirror polishing step P110, thereby preventing a decrease in the surface roughness of the top surfaces of the convex portions 113. As a result, the probability that the wafer comes into point contact with the multiple convex portions 113 of the electrostatic chuck 10 can be reduced compared to the case where the mirror polishing step P110 is not performed, and the generation of particles (contamination) and a decrease in heat transfer characteristics due to leakage of inert gas from the wall-like convex portions 112 on the periphery can be prevented.

[0060] <Modifications of this embodiment> The present invention is not limited to the above-described embodiment, and can be embodied in various forms without departing from the spirit and scope of the invention. For example, the following modifications are also possible.

[0061] In the above embodiment, an example has been described in which the processing amount data preparation step P104 includes the measurement step P112 and the processing amount data creation step P114, but the processing amount data preparation step P104 may prepare processing amount data that has been created in advance. For example, processing amount data that has been created corresponding to the electrostatic chuck 10 to be remanufactured by a person (such as a company) different from the person who implements the manufacturing method of the electrostatic chuck may be prepared.

[0062] In the example shown in FIG. 7, both the plurality of convex portions 113 and the concave bottom surface 116 of the prepared electrostatic chuck 10 are laser-processed in the laser processing step, but either the convex portions 113 or the concave bottom surface 116 may be laser-processed. For example, when the positions of the top surfaces of the plurality of convex portions 113 of the electrostatic chuck to be recycled in the height direction are not uniform but the position of the concave bottom surface 116 in the height direction is uniform, only the plurality of convex portions 113 may be laser-processed. Also, when the positions of the top surfaces of the plurality of convex portions 113 of the electrostatic chuck to be recycled in the height direction are substantially uniform but the position of the concave bottom surface 116 in the height direction is not uniform, only the concave bottom surface 116 may be laser-processed. In this manner, an electrostatic chuck in which the positions and heights of the plurality of convex portions 113 in the height direction are substantially uniform can be provided.

[0063] 7, the positions in the height direction and the heights of the multiple protrusions of the regenerated electrostatic chuck are approximately uniform, but the heights of the multiple protrusions do not have to be uniform. For example, the heights of the multiple protrusions may be different from one another from the viewpoint of temperature control of the first surface S1 by a heater or a coolant.

[0064] In the example shown in Fig. 7, the processing amount data is created so that the lowest position among the measured height direction positions of the top faces of the multiple convex parts becomes the new position of the top faces of the multiple convex parts after laser processing, but the method of creating the processing amount data is not limited to this. For example, the processing amount data may be created so that a position lower than the lowest position among the measured height direction positions of the top faces of the multiple convex parts becomes the new position of the top faces of the multiple convex parts after laser processing. However, as in the example shown in Fig. 7, if the processing amount data is created so that the lowest position among the measured height direction positions of the top faces of the multiple convex parts becomes the new position of the top faces of the multiple convex parts after laser processing, it is preferable because the processing amount can be minimized and the height direction positions of the multiple convex parts 113 can be approximately uniform.

[0065] In the example shown in Fig. 7, an electrostatic chuck having a plurality of convex portions whose top surfaces are different in height direction is prepared in the electrostatic chuck preparation step, but in other examples, an electrostatic chuck having a plurality of convex portions whose top surfaces are uniform in height direction may be prepared in the electrostatic chuck preparation step. In such a case, by preparing processing amount data in which the processing amount for each convex portion is equal, it is possible to remove the affected layer and provide an electrostatic chuck in which the positions of the plurality of convex portions in the height direction are approximately uniform. Furthermore, an electrostatic chuck in which the positions of the top surfaces of the plurality of convex portions in the height direction and the heights of the plurality of convex portions are uniform may be prepared.

[0066] 7, the reference position P0 is set to the second surface S2 of the plate-shaped portion 100, but the reference position can be set arbitrarily. For example, a virtual plane including the chuck electrode 130 may be set to the reference position (reference surface). The mounting surface of the mounting table on which the plate-shaped portion 100 is placed, the surface of the cooling portion 200, or the mounting surface of the mounting table on which the cooling portion 200 is placed may also be set to the reference position (reference surface).

[0067] In the above embodiment, the method for manufacturing an electrostatic chuck includes the mirror polishing step P110. However, in other embodiments, the mirror polishing step P110 may not be included.

[0068] In the above embodiment, the holding device is provided with a stack of plate-like members having a substantially circular planar shape, but the planar shape is not limited to the above embodiment. For example, the holding device may have a rectangular planar shape, a polygonal planar shape, or the like.

[0069] In the above embodiment, an example has been shown in which electrostatic chuck 10 is manufactured by regenerating a used electrostatic chuck, but the above-described method for manufacturing an electrostatic chuck may also be applied to an electrostatic chuck before use. That is, although an example has been shown in which a used electrostatic chuck is prepared in the electrostatic chuck preparation step P102, an electrostatic chuck in which the positions in the height direction and the height of the multiple protrusions of plate-shaped portion 100 are non-uniform may also be prepared in the electrostatic chuck preparation step P102 even before use.

[0070] The present invention is not limited to the above-mentioned embodiments and modifications, and can be realized in various configurations without departing from the spirit of the present invention. For example, the technical features in the embodiments corresponding to the technical features in each aspect described in the Summary of the Invention column can be appropriately replaced or combined in order to solve some or all of the above-mentioned problems or to achieve some or all of the above-mentioned effects. Furthermore, if a technical feature is not described as essential in this specification, it can be appropriately deleted.

[0071] The present disclosure can also be realized in the following application examples. [Application example 1] A plate-shaped portion having a first surface including a plurality of convex portions and a concave bottom surface between the plurality of convex portions, and a second surface that is a reverse surface of the first surface; a chuck electrode disposed inside the plate-shaped portion and configured to generate an electrostatic attraction force; A method for manufacturing an electrostatic chuck capable of holding an object on the first surface of the plate-shaped portion, comprising: an electrostatic chuck preparation step of preparing the electrostatic chuck; a processing amount data preparation step of preparing processing amount data indicating a processing amount of at least one of the plurality of convex portions and the concave bottom surface of the first surface of the prepared electrostatic chuck; a laser processing step of laser processing at least one of the plurality of convex portions and the concave bottom surface of the prepared electrostatic chuck based on the processing amount data; Characterized in that it has A method for manufacturing an electrostatic chuck. [Application example 2] A method for manufacturing an electrostatic chuck according to Application Example 1, comprising: The laser processing step includes: The plurality of convex portions and the concave bottom surface of the prepared electrostatic chuck are laser processed. A method for manufacturing an electrostatic chuck. [Application example 3] A method for manufacturing an electrostatic chuck according to the first or second aspect of the present invention, The processing amount data is a lowest position among height direction positions of the top surfaces of the plurality of convex portions measured with reference to a predetermined reference plane of the plate-shaped portion of the prepared electrostatic chuck becomes a new top surface position of the plurality of convex portions after the laser processing, and the heights of the plurality of convex portions are determined to be a substantially constant height. A method for manufacturing an electrostatic chuck. [Application example 4] A method for manufacturing an electrostatic chuck according to any one of Application Examples 1 to 3, comprising: The processing amount data preparation step includes: a measuring step of measuring positions in a height direction of top surfaces of the plurality of convex portions and a position in a height direction of the concave bottom surface, based on the predetermined reference surface of the plate-shaped portion of the prepared electrostatic chuck; a processing amount data creation step of creating the processing amount data using measurement results of the height direction positions of the top surfaces of the plurality of convex portions and the height direction positions of the concave bottom surface in the measurement step; The present invention is characterized in that it comprises A method for manufacturing an electrostatic chuck. [Application example 5] A method for manufacturing an electrostatic chuck according to any one of Application Examples 1 to 4, comprising: In the electrostatic chuck preparation step, the electrostatic chuck is prepared, the electrostatic chuck having portions where the positions of the top surfaces of the plurality of convex portions in a height direction are different from each other. A method for manufacturing an electrostatic chuck. [Application Example 6] A method for manufacturing an electrostatic chuck according to any one of Aspects 1 to 5, comprising: The method further comprises a mirror polishing step of mirror-polishing the top surfaces of the plurality of convex portions of the plate-shaped portion after the laser processing step. A method for manufacturing an electrostatic chuck. [Explanation of symbols]

[0072] 10...Electrostatic chuck 100…Plate-shaped part 110...First plate-shaped portion 112…Wall-shaped protrusion 112t, 113t, 114t...Top surface 113…Convex part 114, 114a, 114c...columnar protrusions 116…Concave bottom surface 120…Second plate-shaped portion 130...Chuck electrode 140…Heater 200...Cooling section 210... Coolant flow path 400…Joint part 500…Gas flow path W…wafer P102...Electrostatic chuck preparation process P104...Processing volume data preparation process P112…Measurement process P114...Processing volume data creation process P106...Laser processing process P108...Machining process P110…Mirror polishing process P0…Reference position P1, P2, P3, P4...Position S1...Side 1 S2...Side 2 S3...Side 3 PC…Protective cover MD: Machining equipment TL: Altered layer PP...Polishing pad CP: Processing area GR…Grinder PS…polishing liquid

Claims

1. A plate-shaped portion having a first surface including a plurality of convex portions and a concave bottom surface between the plurality of convex portions, and a second surface that is a back surface of the first surface; a chuck electrode disposed inside the plate-shaped portion and configured to generate an electrostatic attraction force; A method for manufacturing an electrostatic chuck capable of holding an object on the first surface of the plate-shaped portion, comprising: an electrostatic chuck preparation step of preparing the electrostatic chuck; a processing amount data preparation step of preparing processing amount data indicating a processing amount of at least one of the plurality of convex portions and the concave bottom surface of the first surface of the prepared electrostatic chuck; a laser processing step of laser processing at least one of the plurality of convex portions and the concave bottom surface of the prepared electrostatic chuck based on the processing amount data; Characterized in that it has A method for manufacturing an electrostatic chuck.

2. 2. A method for manufacturing an electrostatic chuck according to claim 1, comprising the steps of: The laser processing step includes: The plurality of convex portions and the concave bottom surface of the prepared electrostatic chuck are laser processed. A method for manufacturing an electrostatic chuck.

3. 2. A method for manufacturing an electrostatic chuck according to claim 1, comprising the steps of: The processing amount data is a lowest position among height direction positions of the top surfaces of the plurality of convex portions measured with reference to a predetermined reference plane of the plate-shaped portion of the prepared electrostatic chuck becomes a new top surface position of the plurality of convex portions after the laser processing, and the heights of the plurality of convex portions are determined to be a substantially constant height. A method for manufacturing an electrostatic chuck.

4. 4. A method for manufacturing an electrostatic chuck according to claim 3, comprising the steps of: The processing amount data preparation step includes: a measuring step of measuring positions in a height direction of top surfaces of the plurality of convex portions and a position in a height direction of the concave bottom surface, based on the predetermined reference surface of the plate-shaped portion of the prepared electrostatic chuck; a processing amount data creation step of creating the processing amount data using measurement results of the height direction positions of the top surfaces of the plurality of convex portions and the height direction positions of the concave bottom surface in the measurement step; The present invention is characterized in that it comprises A method for manufacturing an electrostatic chuck.

5. A method for manufacturing an electrostatic chuck according to any one of claims 1 to 4, comprising the steps of: In the electrostatic chuck preparation step, the electrostatic chuck is prepared, the electrostatic chuck having portions where the positions of the top surfaces of the plurality of convex portions in a height direction are different from each other. A method for manufacturing an electrostatic chuck.

6. A method for manufacturing an electrostatic chuck according to any one of claims 1 to 4, comprising the steps of: The method further comprises a mirror polishing step of mirror-polishing the top surfaces of the plurality of convex portions of the plate-shaped portion after the laser processing step. A method for manufacturing an electrostatic chuck.

Citation Information

Patent Citations

  • How to determine a target mesa configuration for an electrostatic chuck

    JP2009520452A

  • Manufacturing method of electrostatic chuck

    JP2020006501A

  • Electrostatic chuck regenerating method and electrostatic chuck

    JP2020061489A

  • Electrode embedded member, manufacturing method thereof, and substrate holding member

    JP2022131548A

  • Substrate holding member and manufacturing method for the same

    JP2023031456A