Workpiece processing method
The method forms a processing groove and uses a protective member to prevent contamination and lateral cracks during workpiece division, ensuring effective chip separation.
Patent Information
- Application Number
- JP2023053836
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing methods for cutting workpieces with steps on dividing lines can cause lateral cracks and debris contamination of device chips.
A method involving forming a processing groove from the back side, using a protective member, and irradiating a laser beam from the surface side along the dividing line to divide the workpiece, with a wavelength transparent to the workpiece, and expanding the protective member to suppress contamination.
Suppresses contamination of device chips without reducing divisibility, preventing lateral cracks and debris from contaminating the chips.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for machining a workpiece. [Background technology]
[0002] A processing method is known in which a workpiece having a surface on which devices are formed in areas partitioned by a plurality of intersecting division lines is cut from the back side along the planned division lines with a cutting blade to divide the workpiece into a plurality of device chips (see, for example, Patent Document 1).
[0003] However, in the processing method disclosed in Patent Document 1, when a workpiece having a step formed on the intended dividing line is cut from the back side, the step may cause a lateral crack that reaches the device. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2020-178064 A Summary of the Invention [Problem to be solved by the invention]
[0005] To achieve this, a method has been proposed in which the workpiece is cut from the back side along the intended dividing line to form a cutting groove that does not reach the front side, and then a laser beam is irradiated from the front side along the intended dividing line, dividing the workpiece using the modified layer formed inside as the starting point.
[0006] However, when an attempt was made to use a laser beam to form a modified layer that reached the bottom of the cut groove in order to improve separation, a new problem arose in that debris was scattered from the bottom of the cut groove, contaminating the device chip.
[0007] An object of the present invention is to provide a method for processing a workpiece that can suppress contamination of device chips without reducing separability. [Means for solving the problem]
[0008] In order to solve the above-mentioned problems and achieve the object, the method for processing a workpiece of the present invention is a method for processing a workpiece having a surface on which devices are formed in areas partitioned by a plurality of intersecting planned division lines, and is characterized in that it comprises a processing groove forming step of forming a processing groove along the planned division lines from the back side of the workpiece, a adhesion step after the processing groove forming step of attaching a protective material to the back side of the workpiece and closely adhering the protective material to the processing groove, and a dividing step after the adhesion step of irradiating the workpiece with a laser beam along the planned division lines from the front side of the workpiece to divide the workpiece along the planned division lines.
[0009] In the method for processing the workpiece, the dividing step may include a dividing starting point forming step of irradiating a laser beam having a wavelength that is transparent to the workpiece from the surface side of the workpiece along the intended dividing line to form a dividing starting point inside the workpiece, and an expanding step of expanding the protective member to divide the workpiece after the dividing starting point forming step.
[0010] In the method for machining a workpiece, the division start point in the division start point forming step may be formed so as to reach a bottom of the machined groove.
[0011] In the method for processing a workpiece, the adhering step may include mounting the protective member on the back surface of the workpiece in a vacuum chamber. Effect of the Invention
[0012] The present invention has an effect of suppressing contamination of device chips without reducing separability. [Brief description of the drawings]
[0013] [Figure 1] FIG. 1 is a perspective view that typically shows a workpiece to be processed by the workpiece processing method according to the first embodiment. [Diagram 2] FIG. 2 is a flowchart showing a flow of the method for processing a workpiece according to the first embodiment. [Diagram 3] FIG. 3 is a cross-sectional view that typically shows a groove forming step in the method for machining the workpiece shown in FIG. [Figure 4] FIG. 4 is a cross-sectional view that typically shows a state in which a workpiece and an annular frame are supported on a support table of a vacuum chamber in the contact step of the method for processing the workpiece shown in FIG. [Diagram 5] FIG. 5 is a cross-sectional view that typically shows a state in which a protection member is in close contact with the workpiece and the annular frame shown in FIG. [Figure 6] FIG. 6 is a cross-sectional view that typically shows the workpiece after the contact step of the method for processing the workpiece shown in FIG. [Figure 7] FIG. 7 is a cross-sectional view that typically shows a dividing start point forming step in the method of processing the workpiece shown in FIG. [Figure 8] FIG. 8 is a cross-sectional view that typically shows a main part of the workpiece after the dividing start point forming step of the method for processing the workpiece shown in FIG. [Figure 9] FIG. 9 is a cross-sectional view showing a schematic diagram of an expansion step of the method for machining the workpiece shown in FIG. [Figure 10] FIG. 10 is a cross-sectional view that typically illustrates a groove forming step in the method for machining a workpiece according to the first modified example of the first embodiment. [Figure 11] FIG. 11 is a cross-sectional view that illustrates a dividing step of a method for processing a workpiece according to Modification 2 of the first embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] The form (embodiment) for carrying out the present invention will be described in detail with reference to the drawings. The present invention is not limited to the contents described in the following embodiment. Furthermore, the components described below include those that a person skilled in the art can easily imagine and those that are substantially the same. Furthermore, the configurations described below can be appropriately combined. Furthermore, various omissions, substitutions, or modifications of the configurations can be made without departing from the gist of the present invention.
[0015] [Embodiment 1] A method for processing a workpiece according to a first embodiment of the present invention will be described with reference to the drawings. Fig. 1 is a perspective view showing a schematic view of a workpiece to be processed by the method for processing a workpiece according to the first embodiment. Fig. 2 is a flow chart showing the flow of the method for processing a workpiece according to the first embodiment.
[0016] (workpiece) The method for processing a workpiece according to the first embodiment is a method for processing a workpiece 1 shown in Fig. 1. The workpiece 1 shown in Fig. 1, which is to be processed by the method for processing a workpiece according to the first embodiment, is a wafer such as a disk-shaped semiconductor wafer or an optical device wafer, with a substrate 2 made of silicon, sapphire, gallium, or the like. As shown in Fig. 1, the workpiece 1 has a plurality of planned division lines 4 that intersect with a surface 3 of the substrate 2. The workpiece 1 has the surface 3 on which devices 5 are formed in each region partitioned by the planned division lines 4.
[0017] The device 5 is, for example, an integrated circuit such as an IC (Integrated Circuit) or an LSI (Large Scale Integration), an image sensor such as a CCD (Charge Coupled Device) or a CMOS (Complementary Metal Oxide Semiconductor), an optical element such as an LED (Light-Emitting Diode), a MEMS (Micro Electro Mechanical Systems) or a semiconductor memory (semiconductor memory device).
[0018] In the workpiece 1, the devices 5 protrude from the surface 3 of the substrate 2, forming a step between the surface 3 of the substrate 2 and the devices 5. In the embodiment 1, the workpiece 1 has a metal film 7 formed on a back surface 6 behind the surface 3 of the substrate 2. In the embodiment 1, the workpiece 1 is divided into individual device chips 10 along the planned division lines 4. The device chips 10 include a part of the substrate 2 and the devices 5 formed on the surface 3 of the substrate 2.
[0019] (Processing method of workpiece) The method for processing a workpiece according to the first embodiment is also a method for dividing the workpiece 1 into individual device chips 10 along the planned dividing lines 4. As shown in FIG. 2, the method for processing a workpiece includes a groove forming step 101, a bonding step 102, and a dividing step 103.
[0020] (Groove formation step) Fig. 3 is a cross-sectional view that shows a schematic diagram of a groove forming step in the method for processing the workpiece shown in Fig. 2. The groove forming step 101 is a step of forming a groove 11 (shown in Fig. 3) along the intended division line 4 from the rear surface 6 side of the workpiece 1.
[0021] In the first embodiment, in the machining groove forming step 101, the protective tape 20 is applied to the surface 3 of the workpiece 1, and the cutting device 30 sucks and holds the surface 3 of the workpiece 1 on the holding surface of a chuck table (not shown) via the protective tape 20. In the first embodiment, the protective tape 20 is an adhesive tape that includes a base layer made of a non-adhesive and flexible resin and a glue layer made of an adhesive and flexible resin laminated on the base layer, and the glue layer is attached to the surface 3 of the workpiece 1, but in the present invention, it may be a sheet that does not include a glue layer and is composed only of a base layer made of a thermoplastic resin and is thermocompressed to the surface 3 of the workpiece 1.
[0022] In the first embodiment, in the processing groove forming step 101, the cutting device 30 holds the front surface 3 side of the workpiece 1 on the holding surface by suction, then images the workpiece 1 with the imaging unit to detect the division lines 4, and performs alignment to align the division lines 4 of the workpiece 1 with the cutting blade 31. In the first embodiment, in the processing groove forming step 101, the cutting device 30 cuts the cutting blade 31 into the division lines 4 from the back surface 6 side while relatively moving the workpiece 1 and the cutting blade 31 in the horizontal direction along the division lines 4, as shown in FIG. 3. In the first embodiment, in the processing groove forming step 101, the cutting device 30 cuts the cutting blade 31 into the division lines 4 from the back surface 6 side to the center of the thickness of the substrate 2 of the workpiece 1, and forms processing grooves 11 in the workpiece 1 along all the division lines 4 that open to the back surface 6 side and do not divide the workpiece 1.
[0023] (Adhesion step) Fig. 4 is a cross-sectional view showing a state where a workpiece and an annular frame are supported on a support table of a vacuum chamber in a contact step of the method for processing the workpiece shown in Fig. 2. Fig. 5 is a cross-sectional view showing a state where a protective member is contacted with the workpiece and the annular frame shown in Fig. 4. Fig. 6 is a cross-sectional view showing a state where a workpiece is after the contact step of the method for processing the workpiece shown in Fig. 2.
[0024] The adhesion step 102 is a step of adhering the protective member 21 to the back surface 6 of the workpiece 1 after the processing groove forming step 101, and adhering the protective member 21 to the processing groove 11. In the first embodiment, the protective member 21 is a sheet composed only of a base material layer made of a thermoplastic resin without a glue layer and heat-pressed to the back surface 6 of the workpiece 1, but in the present invention, it may be an adhesive tape that includes a base material layer made of a resin having non-adhesive properties and flexibility, and a glue layer laminated on the base material layer and made of a resin having adhesive properties and flexibility, and the glue layer is attached to the back surface 6 of the workpiece 1.
[0025] In the first embodiment, in the adhesion step 102, the protective tape 20 is peeled off from the workpiece 1, and the front surface 3 side of the workpiece 1 is placed on the holding surface of the support table 44 in the lower housing 43 of the vacuum chamber 41 separated from the upper housing 42 of the vacuum chamber 41 of the vacuum mounter 40. Also, in the first embodiment, in the adhesion step 102, an annular frame 8 having an inner diameter larger than the outer diameter of the workpiece 1 is placed on the holding surface of the support table 44. In the first embodiment, in the adhesion step 102, as shown in FIG. 4, a protective member 21 is placed on the back surface 6 of the workpiece 1 on the holding surface of the support table 44 and on the annular frame 8.
[0026] In the first embodiment, in the adhesion step 102, the vacuum mounter 40 adheres the upper housing 42 to the lower housing 43 to isolate the insides of these housings 42, 43 from the outside. Then, these housings 42, 43 are separated by the protective member 21. The on-off valves 421, 431 are closed to seal the insides of the housings 42, 43, and the on-off valves 422, 432 are opened to reduce the pressure inside the housings 42, 43 by the suction sources 423, 433 while the heater 45 in the support table 44 heats and softens the protective member 21 via the workpiece 1 and the annular frame 8.
[0027] In the first embodiment, in the adhesion step 102, the vacuum mounter 40 closes the on-off valves 422 and 432 as shown in Fig. 5, and then opens the on-off valve 421 to open the inside of the upper housing 42 to the atmosphere. Then, the protective member 21 is heated by the heater 45 and softened, and is thermocompression-bonded to the workpiece 1 and the annular frame 8 due to the pressure difference between the housings 42 and 43, and is in close contact with the inner surface of the processed groove 11 as shown in Fig. 6, and is bonded to the workpiece 1 and the annular frame 8.
[0028] In the first embodiment, in the adhesion step 102, the protective member 21 adhered to the workpiece 1 and the annular frame 8 is cut between the inner edge and the outer edge of the annular frame 8, and the workpiece 1 is supported in the inner opening of the annular frame 8 by the protective member 21, as shown in Fig. 6. Thus, in the first embodiment, the adhesion step 102 mounts (attaches) the protective member 21 to the back surface 6 of the workpiece 1 in the vacuum chamber 41.
[0029] (split step) The dividing step 103 is a step following the adhering step 102, in which a laser beam 52 (shown in FIG. 7) is irradiated from the front surface 3 side of the workpiece 1 along the intended dividing lines 4 to divide the workpiece 1 along the intended dividing lines 4. In the first embodiment, the dividing step 103 includes a dividing start point forming step 1031 and an expanding step 1032, as shown in FIG.
[0030] (Splitting point formation step) Fig. 7 is a cross-sectional view showing a schematic diagram of a splitting start point forming step in the method for processing a workpiece shown in Fig. 2. Fig. 8 is a cross-sectional view showing a schematic diagram of a main part of a workpiece after the splitting start point forming step in the method for processing a workpiece shown in Fig. 2. The splitting start point forming step 1031 is a step of irradiating a laser beam 52 having a wavelength that is transparent to the workpiece 1 along the intended splitting line 4 from the side of the front surface 3 of the workpiece 1, and forming a modified layer 12 serving as a splitting start point inside the workpiece 1.
[0031] The modified layer 12 refers to a region in which the density, refractive index, mechanical strength, and other physical properties are different from those of the surrounding area, and examples of such regions include a melting treatment region, a crack region, a dielectric breakdown region, a refractive index change region, and a region in which these regions are mixed, etc. The mechanical strength of the modified layer 12 is lower than the mechanical strength of the other parts of the workpiece 1 than the modified layer 12.
[0032] In the first embodiment, in the division starting point forming step 1031, the laser processing device 50 suction-holds the back surface 6 of the workpiece 1 on the holding surface of a chuck table (not shown) via the protective member 21. In the first embodiment, in the division starting point forming step 1031, after the laser processing device 50 suction-holds the back surface 6 of the workpiece 1 on the holding surface, the imaging unit captures an image of the workpiece 1 to detect the planned division line 4, and performs alignment to align the planned division line 4 of the workpiece 1 with the laser beam application unit 51.
[0033] In embodiment 1, in the division starting point formation step 1031, as shown in FIG. 7, the laser processing apparatus 50 positions the focal point 53 of a laser beam 52 having a wavelength that is transparent to the substrate 2 of the workpiece 1 inside the substrate 2 at the planned division line 4 of the workpiece 1, and irradiates the laser beam 52 from the laser beam application unit 51 to the planned division line 4 from the surface 3 side while moving the workpiece 1 and the laser beam application unit 51 relatively in the horizontal direction along the planned division line 4.
[0034] Then, since the wavelength of the laser beam 52 is a wavelength that is transparent to the substrate 2 of the workpiece 1, a modified layer 12 is formed inside the substrate 2 of the workpiece 1 along the intended division line 4. In addition, in the first embodiment, in the division start point forming step 1031, the laser processing device 50 irradiates the laser beam 52 by extending the condensing point 53 in the thickness direction so that the modified layer 12 reaches the bottom surface 13 that is the bottom of the processed groove 11, and the length 121 of the modified layer 12 in the thickness direction of the substrate 2 exceeds 1 / 2 the thickness 111 of the bottom of the processed groove 11 and is equal to or less than the thickness 111 of the bottom of the processed groove 11, as shown in FIG. 8. Thus, in the first embodiment, the modified layer 12 that is the division start point in the division start point forming step 1031 is formed so as to reach the bottom surface 13 of the processed groove 11 and extend from the bottom surface 13 to a position on the back surface 6 side of the substrate 2 relative to the front surface 3. In the first embodiment, in the division start point forming step 1031, a hole 122 communicating with the modified layer 12 is formed in the bottom surface 13 of the processed groove 11 as shown in FIG.
[0035] (Extended Step) Fig. 9 is a cross-sectional view showing a schematic diagram of an expanding step of the method for processing the workpiece shown in Fig. 2. The expanding step 1032 is a step of expanding the protective member 21 to divide the workpiece 1 after the division start point forming step 1031.
[0036] In the first embodiment, in the expansion step 1032, the expansion device 60 holds the annular frame 8 between the frame mounting plate 62 and the frame pressing plate 63 of the clamping mechanism 61, as shown in Fig. 9, and abuts the expansion roller 65 at the upper end of the cylindrical expansion drum 64 between the annular frame 8 of the protective member 21 and the workpiece 1. In the first embodiment, in the expansion step 1032, the expansion device 60 moves the expansion drum 64 upward relative to the clamping mechanism 61. Then, the gap between the annular frame 8 of the protective member 21 and the workpiece 1 is pressed, and the protective member 21 is expanded in the surface direction.
[0037] In the expanding step 1032, as a result of the expansion of the protective member 21, a tensile force acts radially on the protective member 21. When a tensile force acts radially on the protective member 21 attached to the rear surface 6 side of the workpiece 1 in this manner, the workpiece 1 is divided into individual device chips 10 along the planned division lines 4, starting from the modified layer 12, since the modified layer 12 has been formed along the planned division lines 4. Thus, the individually divided device chips 10 are picked up from the protective member 21.
[0038] In the method for processing a workpiece according to the first embodiment described above, a groove 11 that does not divide the workpiece 1 is formed from the back surface 6 side of the workpiece 1 in a groove forming step 101, and then a laser beam 52 is irradiated from the front surface 3 side in a dividing step 103 to divide the workpiece 1 into individual device chips 10. For this reason, the method for processing a workpiece according to the first embodiment can suppress the occurrence of lateral cracks that reach the device 5 due to a step between the front surface 3 of the substrate 2 of the workpiece 1 and the device 5.
[0039] Moreover, in the method for processing a workpiece according to the first embodiment, in the adhering step 102, the protective member 21 is brought into close contact with the inner surface of the processed groove 11, and the protective member 21 is bonded to the back surface 6 of the workpiece 1. For this reason, in the method for processing a workpiece according to the first embodiment, it is possible to prevent debris generated by irradiation with the laser beam 52 in the dividing step 103 from being attached to the protective member 21, and to prevent the debris from contaminating the individually divided device chips 10.
[0040] As a result, the method for processing the workpiece according to embodiment 1 has the effect of suppressing contamination of the device chip 10 without reducing separability, even in the case of a workpiece 1 in which a step is formed between the surface 3 of the substrate 2 and the device 5.
[0041] [Variation 1] A method for processing a workpiece according to Modification 1 of the first embodiment will be described with reference to the drawings. Fig. 10 is a cross-sectional view that shows a schematic diagram of a processing groove forming step of the method for processing a workpiece according to Modification 1 of the first embodiment. In Fig. 10, the same parts as those in the first embodiment are given the same reference numerals and the description thereof will be omitted. The method for processing a workpiece according to Modification 1 is the same as that in the first embodiment, except that the processing groove forming step 101 is different from that in the first embodiment.
[0042] In the first modification, in the processed groove forming step 101, a protective tape 20 is applied to the surface 3 side of the workpiece 1, and the laser processing device 70 suction-holds the surface 3 side of the workpiece 1 on the holding surface of a chuck table (not shown) via the protective tape 20. In the first modification, in the processed groove forming step 101, after the laser processing device 70 suction-holds the surface 3 side of the workpiece 1 on the holding surface, an image of the workpiece 1 is captured by an imaging unit to detect the planned division lines 4, and an alignment is performed to align the planned division lines 4 of the workpiece 1 with the laser beam application unit 71.
[0043] In the first modification, in the processed groove forming step 101, the laser processing device 70 positions a focal point 73 of a laser beam 72 having a wavelength absorbed by the metal film 7 and substrate 2 of the workpiece 1 on the surface of the metal film 7 of the workpiece 1, as shown in Fig. 10, and irradiates the laser beam 72 from the laser beam application unit 71 to the division lines 4 from the back surface 6 while moving the workpiece 1 and the laser beam application unit 71 relatively in the horizontal direction along the division lines 4. In the first modification, in the processed groove forming step 101, the laser processing device 70 performs ablation processing on the metal film 7 and the substrate 2 to form processed grooves 11 in the workpiece 1 along all of the division lines 4, the processed grooves opening on the back surface 6 side.
[0044] In the method for processing a workpiece according to the first modification, a groove 11 that does not divide the workpiece 1 is formed from the back surface 6 side of the workpiece 1 in a groove forming step 101, and then the workpiece 1 is divided into individual device chips 10 in a dividing step 103, and a protective member 21 is bonded to the back surface 6 of the workpiece 1 by bonding the protective member 21 to the inner surface of the groove 11 in a bonding step 102. As a result, the method for processing a workpiece according to the first modification has the effect of suppressing contamination of the device chips 10 without reducing the divisibility, even in the case of a workpiece 1 in which a step is formed between the front surface 3 of the substrate 2 and the device 5, as in the first embodiment.
[0045] [Modification 2] A method for processing a workpiece according to Modification 2 of the first embodiment will be described with reference to the drawings. Fig. 11 is a cross-sectional view that shows a schematic diagram of a dividing step of the method for processing a workpiece according to Modification 2 of the first embodiment. In Fig. 11, the same parts as those in the first embodiment are denoted by the same reference numerals, and the description thereof will be omitted. The method for processing a workpiece according to Modification 2 is the same as that in the first embodiment, except that the dividing step 103 is different from that in the first embodiment.
[0046] In the second modification, in the dividing step 103, the laser processing device 80 suction-holds the back surface 6 of the workpiece 1 on the holding surface of a chuck table (not shown) via the protective member 21. In the second modification, in the dividing step 103, after the laser processing device 80 suction-holds the back surface 6 of the workpiece 1 on the holding surface, the imaging unit captures an image of the workpiece 1 to detect the planned dividing line 4, and performs alignment to align the planned dividing line 4 of the workpiece 1 with the laser beam application unit 81.
[0047] In the second modification, in the dividing step 103, the laser processing device 80 positions a focusing point 83 of a laser beam 82 having a wavelength absorbent for the substrate 2 of the workpiece 1 on the surface 3 of the division line 4 of the workpiece 1, as shown in Fig. 11, and irradiates the laser beam 82 from the laser beam application unit 81 to the division line 4 from the surface 3 side while relatively moving the workpiece 1 and the laser beam application unit 81 in the horizontal direction along the division line 4. In the second modification, in the processed groove forming step 101, the laser processing device 80 performs ablation processing on the bottoms of the processed grooves 11 formed on the division line 4 of the substrate 2 to cut the bottoms of all the processed grooves 11, and divides the workpiece 1 along the division line 4 into individual device chips 10.
[0048] In the method for processing a workpiece according to the second modification, a groove 11 that does not divide the workpiece 1 is formed from the back surface 6 side of the workpiece 1 in a groove forming step 101, and then the workpiece 1 is divided into individual device chips 10 in a dividing step 103, and a protective member 21 is bonded to the back surface 6 of the workpiece 1 by bonding the protective member 21 to the inner surface of the groove 11 in a bonding step 102. As a result, the method for processing a workpiece according to the second modification has the effect of suppressing contamination of the device chips 10 without reducing the divisibility, even in the case of a workpiece 1 in which a step is formed between the front surface 3 of the substrate 2 and the device 5, as in the first embodiment.
[0049] In the second modification, in the groove forming step 101, the groove 11 may be formed by irradiating the laser beam 72, similarly to the first modification.
[0050] It should be noted that the present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the gist of the present invention. [Explanation of symbols]
[0051] 1 Workpiece 3 surface 4. Planned division line 5 Devices 6 Back side 11 Machining groove 12 Modified layer (starting point of division) 13 Bottom (Bottom) 21 Protective materials 41 Vacuum Chamber 52 Laser beam 82 Laser Beam 101 Groove forming step 102 Close Contact Step 103 division steps 1031 Division origin formation step 1032 Extended Step
Claims
1. A method for processing a workpiece having a surface on which devices are formed in areas partitioned by a plurality of intersecting planned division lines, comprising the steps of: a groove forming step of forming a groove along the intended dividing line from the rear surface side of the workpiece; a contact step of adhering a protective member to the back surface of the workpiece after the processing groove forming step and contacting the protective member with the processing groove; a dividing step of dividing the workpiece along the dividing lines by irradiating the workpiece with a laser beam from a front surface side of the workpiece after the adhering step; A method for processing a workpiece comprising the steps of:
2. The division step comprises: a division starting point forming step of irradiating a laser beam having a wavelength that is transparent to the workpiece along the division line from a surface side of the workpiece to form a division starting point inside the workpiece; an expanding step of expanding the protective member to divide the workpiece after the dividing start point forming step; The method for processing a workpiece according to claim 1 , comprising:
3. 3. The method for machining a workpiece according to claim 2, wherein the division start point in the division start point forming step is formed so as to reach a bottom of the machined groove.
4. 4. The method for processing a workpiece according to claim 1, wherein the contact step comprises mounting the protective member on the back surface of the workpiece in a vacuum chamber.
Citation Information
Patent Citations
Chip manufacturing method
JP2020178064A