Detection device, production control system, detection method and control program
The detection device addresses bonding issues in film rolls by analyzing film joint images to ensure proper bonding, preventing defects and ensuring continuous production.
Patent Information
- Application Number
- JP2023054674
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-11
AI Technical Summary
In film roll manufacturing, poor bonding conditions during the joining process lead to edge deformation, misalignment, cracking, or breakage of films during stretching, affecting the optical properties and production continuity.
A detection device that photographs the film joint using an imaging unit, calculates the degree of bonding by analyzing frame images, and determines the deviation between actual and ideal lines to assess bonding quality, with output units displaying results and controlling manufacturing conditions to prevent defects.
Prevents film defects and production stoppages by accurately detecting bonding conditions, ensuring proper film grip and alignment, thereby maintaining film quality and production efficiency.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a detection device, a production management system, a detection method, and a control program for detecting a film transport state in a film roll production line. [Background technology]
[0002] Liquid crystal display devices are increasingly being used in large-screen televisions and large monitors, and as a result, there is a demand for wider films to be used on the display surfaces of liquid crystal display devices. For example, wide films of 2000 mm or more are in demand. In addition, in order to anticipate substrate loss (film loss) and to reduce transportation costs, there is a demand for the production of long film rolls with winding lengths of 1000 m or more, and even 3000 m or more.
[0003] In a film roll production line, for example, a solution casting method is used in which a raw resin is dissolved in a solvent, various additives are added to the dope, and the dope is extruded from a die onto an endlessly rotating metal support, and after casting in a casting process, the solvent is removed to a certain extent on the support, and the film is peeled off from the endless support to form a film, which is then dried to remove the solvent and wound around a winding shaft to produce a film roll. In addition, after the casting process, a stretching process is performed in which both ends of the heated resin film are held with multiple clips and stretched as a method for adjusting the optical properties of the film.
[0004] In some cases, it may be more appropriate to set different conveying speeds in the casting process and the stretching process rather than setting them to the same speed. Patent Document 1 discloses a film production method called offline stretching, in which a film production line for producing a film by a casting process or the like is separated from a stretching line for performing a stretching process. In this offline stretching, in order to improve productivity, multiple film rolls are continuously stretched while being joined in a joining process. In this joining process, after a film is sent out from one film roll, the leading end of the following film sent out from the next film roll is joined to the trailing end of the preceding film by a process such as heat fusion. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2012-088592 A Summary of the Invention [Problem to be solved by the invention]
[0006] In the film roll production line, a preceding film and a following film are joined in the joining process as described above, and the joined film is subjected to a subsequent stretching process and the like to produce a film roll. In these processes, if the joining process is not performed well, the following problems will occur in the stretching process. For example, if the joining is performed under excessive conditions to increase the joining strength, the end deformation in the area around the joint will be large, and the end of the film cannot be properly gripped in the stretching process. Even if the end of the film can be gripped, the grip position will shift in the conveying direction, and the optical properties of the stretched film will be poor. On the other hand, if the joining is performed under conditions where the joining strength is insufficient to suppress the deformation of the end, even if the end of the film can be gripped, the film will crack or break when stretched in the width direction. In this way, in the production of film rolls, it is required to ensure the performance of the film after stretching by suppressing the end deformation while ensuring the joining strength.
[0007] The present invention has been made in consideration of the above-mentioned circumstances, and aims to prevent the occurrence of events that lead to production stoppages such as defective film products or breakage of the film by detecting the degree of bonding of the film bonding portion during film production. [Means for solving the problem]
[0008] The above object of the present invention can be achieved by the following means.
[0009] (1) A detection device used in a production line for a film roll, which is manufactured by a delivery process in which a film is paid out, a stretching process in which both side ends of the film being transported and heated are gripped with a plurality of pairs of gripping parts while the pair of gripping parts is gradually widened in the width direction to stretch the film, a winding process in which the stretched film is wound around a core, and a joining process in which a preceding film and a following film are joined at a joint where the leading and trailing ends of the two films are overlapped prior to the stretching process, an imaging unit that captures an image of the film being transported; A processing unit that calculates a degree of bonding of the film by the bonding portion by analyzing a frame image of the film including the bonding portion obtained by the imaging unit, The processing unit calculates an approximation line connecting multiple end points of the detected film and an ideal line calculated from multiple end points excluding the end points of the film that overlap the joint, and calculates the degree of joint based on the approximation line and the ideal line.
[0010] (2) The detection device according to (1) above, wherein the degree of bonding is an evaluation of the deviation between the ideal line and the approximation line.
[0011] (3) The detection device described in (2) above, wherein the deviation between the ideal line and the approximation line is the difference in angle between the ideal line and the approximation line, or the size of the area between the ideal line and the approximation line over a specified length before and after the joint in the conveying direction.
[0012] (4) An output unit that outputs the degree of bonding, The detection device according to (1) above, wherein the output unit causes the display unit to display the approximation line and the ideal line superimposed on the display image of the frame image.
[0013] (5) the processing unit detects unevenness of the film by analyzing the frame images; The detection device according to (4) above, wherein the output section displays the detected irregularities on a display image of the frame image by superimposing the detected irregularities on the display image.
[0014] (6) further comprising a storage unit for storing data on the manufacturing history of the film roll; The detection device described in (4) above, wherein the output unit superimposes the approximation line and / or the ideal line calculated during a past film roll production stored in the production history on a display image of the frame image of the film roll currently being produced.
[0015] (7) A detection device according to any one of (1) to (6) above, comprising a light source for irradiating light onto a monitoring area of the film.
[0016] (8) The detection device according to (4) above, wherein the output unit outputs an alarm when the degree of bonding exceeds a threshold value.
[0017] (9) A film roll manufacturing device for manufacturing a film roll by the steps of: a delivery step for paying out a film; a stretching step for stretching the film by gradually increasing the widthwise distance between a plurality of pairs of gripping parts while gripping both side ends of the film being transported and heated; a winding step for winding the stretched film around a core; and a joining step for joining a leading film and a trailing film at a joint where the leading and trailing ends of the films are overlapped prior to the stretching step; A manufacturing control system including a detection device, The detection device includes: an imaging unit that captures an image of the film being transported; A processing unit that calculates a degree of bonding of the film by the bonding portion by analyzing a frame image of the film including the bonding portion obtained by the imaging unit, the processing unit calculates an approximation line connecting the detected side ends of the film and an ideal line connecting the side ends of the film excluding the end point of the film related to the joint, and calculates the degree of joint based on the approximation line and the ideal line. Manufacturing management system.
[0018] (10) The manufacturing management system according to (9) above, further comprising an output unit that outputs alert information when the bonding degree exceeds a threshold value.
[0019] (11) The film roll production apparatus includes a control device, The manufacturing management system according to (9) or (10) above, wherein the control device changes the clip conditions of the gripping part in the stretching process or stops the production of the film roll in progress when the degree of joining exceeds a threshold value.
[0020] (12) The film roll production apparatus includes a control device, The manufacturing management system according to (9) or (10), wherein the control device changes the transport conditions of the preceding film or the winding conditions in the winding process when the degree of bonding exceeds a threshold value.
[0021] (13) The film roll production apparatus includes a control device, When the degree of joining exceeds a threshold value, the manufacturing conditions related to the subsequent unwinding of the film in the sending step and / or the joining in the joining step are changed as the manufacturing conditions, and the changed manufacturing conditions are stored. The manufacturing management system according to (9) or (10) above, wherein when a next film roll is manufactured or when a next joining process is performed in a next joining step, a film roll is manufactured under the stored changed manufacturing conditions.
[0022] (14) A method for detecting a state of bonding at a bonding portion used in a production line for a film roll manufactured by a delivery process for unstretching an unstretched film, a stretching process for stretching the film by gradually increasing the widthwise distance between a plurality of pairs of gripping portions while gripping both side ends of the film being transported and heated, a winding process for winding the stretched film around a core, and a bonding process for bonding a leading film and a trailing film at a bonding portion where the leading and trailing ends of the films are overlapped, the method comprising: (a) a step of photographing a transported film; (b) calculating a degree of bonding of the film by the bonding portion by analyzing a frame image of the film including the bonding portion obtained by photographing. In the step (b), an approximation line connecting the detected side edges of the film and an ideal line connecting the side edges of the film excluding the end point of the film related to the joint are calculated, and the degree of joint is calculated based on the approximation line and the ideal line.
[0023] (15) A control program for controlling a detection device for detecting a state of bonding at a bonding portion used in a production line for a film roll manufactured by a delivery process for unwinding a film, a stretching process for stretching the film by gradually increasing the widthwise distance between a plurality of pairs of gripping portions while gripping both side ends of the film being transported and heated, a winding process for winding the stretched film around a core, and a bonding process for bonding a leading film and a trailing film at a bonding portion where the leading and trailing ends of the films are overlapped prior to the stretching process, the control program comprising: (a) a step of photographing a transported film; (b) calculating a degree of bonding of the film by the bonding portion by analyzing a frame image of the film including the bonding portion obtained by photographing. A control program for causing a computer to execute a process in which, in step (b), an approximation line connecting the detected side edges of the film and an ideal line connecting the side edges of the film excluding the end point of the film related to the joint are calculated, and the degree of joint is calculated based on the approximation line and the ideal line. Effect of the Invention
[0024] The detection device 90 used in the film roll production line of the present invention includes an imaging section that captures the film being conveyed, and a processing section that calculates the degree of splicing of the film by the splice by analyzing frame images of the film including the splice captured by the imaging section, and the processing section calculates an approximation line connecting multiple end points of the detected film and an ideal line calculated from multiple end points of the film excluding the end points of the film that overlap the splice, and calculates the degree of splicing based on the approximation line and the ideal line. In this way, by detecting the degree of splicing of the film when it is manufactured, it is possible to prevent the occurrence of events that lead to production stoppage, such as breakage. [Brief description of the drawings]
[0025] [Figure 1] FIG. 2 is a schematic diagram showing a film roll production line. [Diagram 2] FIG. 2 is a schematic diagram showing a configuration of a bonding processing unit. [Diagram 3] FIG. 2 is a perspective view showing a schematic configuration of a stretching step and a trimming step. [Figure 4] FIG. 2 is a block diagram of a manufacturing control system. [Diagram 5] 4 is a diagram showing an example of the arrangement of an imaging unit and a light source of the detection device. FIG. [Figure 6] 10 is a flowchart showing a process of detecting a joining condition by a detection device. [Figure 7A] 11 is an example of a target frame image. [Figure 7B] 7B is an example of a display image generated based on the target frame image of FIG. 7A. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] Hereinafter, an embodiment of the present invention will be described with reference to the attached drawings. However, the scope of the present invention is not limited to the disclosed embodiment. In the description of the drawings, the same elements are given the same reference numerals, and duplicated descriptions are omitted. In addition, the dimensional ratios of the drawings are exaggerated for the convenience of explanation, and may differ from the actual ratios.
[0027] First, a manufacturing line for a film roll 85 will be described with reference to Figs. 1 to 3. Fig. 1 is a schematic diagram showing a manufacturing line for a film roll. Fig. 2 is a schematic diagram showing a joining processing unit 02. Fig. 3 is a schematic diagram showing the configuration of a stretching process and a trimming process. In each figure, the vertical direction is the Z direction, the main transport direction of the film F8 is the X direction, and the direction perpendicular to the transport direction, the width direction of the film F8, is the Y direction. The X direction or the transport direction is also called MD (Machine Direction). The Y direction or the width direction is also called TD (Transverse Direction) or the left-right direction.
[0028] (Overview of the film roll production line) 1 uses an offline stretching method to manufacture a film roll 85. Although details will be described later, the film roll manufacturing apparatus 100 performs the following steps (1) to (5). (1) A process of unwinding a film from a roll 80 (also called a film roll) (2) A stretching process in which the unwound film is heated and stretched while being continuously transported. (3) Trimming process in which both ends (edges) of the stretched film are cut and removed. (4) Cooling process in which cooling is performed while transporting (5) The winding process involves winding the cooled film around a shaft to produce a film roll. The (2) stretching step includes an MD stretching step in which the film is heated and then stretched in the conveying direction, and a TD stretching step in which both ends are held by multiple grippers and the film is stretched in the width direction. The stretching step may be not only a TD stretching step in which the film is stretched in a direction parallel to the width direction, i.e., the film is expanded at an angle of 0° with the width direction, but also an oblique stretching step in which both ends of the heated film are held by multiple grippers and the film is stretched in an oblique direction at an angle of 40 to 50° with the width direction of the film (referred to as "oblique stretching") in order to adjust the optical properties of the film. In this case, the cooling step may include a heat relaxation step in which the stretched film is continuously transported and heat-treated for stress relaxation. When the film on the original roll runs out (more specifically, just before the film on the original roll runs out), the preceding film is stopped and cut. After that, the rear end is placed in a specified position (joining position), and then a joining process is performed in which film is immediately unwound from a new original roll and the leading end of the following film unwound from the new original roll is overlapped and joined to the rear end of the preceding film.
[0029] In this embodiment, the "stretching process in which both side edges of a heated film being transported are gripped with a plurality of pairs of gripping parts and the widthwise distance between the pairs of gripping parts is gradually increased to thereby stretch the film" includes a TD stretching process and a diagonal stretching process.
[0030] (Film roll manufacturing device 100) The film roll manufacturing apparatus 100 shown in FIG. 1 is also called an offline stretching apparatus, and it pays out and splices films from a plurality of original rolls 80, stretches the spliced film, and manufactures a film roll. As shown in FIG. 1, the film roll manufacturing apparatus 100 has a film delivery section 01, a splicing section 02, an accumulation section 03, a stretching section 04, a trimming section 05, a cooling section 06, and a winding section 07. The film delivery section 01 and the splicing section 02 function as a supply section 10. These components 01-07 are arranged in this order along the transport direction of the film F8. The manufacturing conditions of the components 01-07 are controlled by a control device 09 (see FIG. 3 described later).
[0031] The film delivery section 01 is equipped with a raw roll 80 manufactured in a film-forming facility. The raw roll 80 is formed by winding a film around a core into a roll shape. This core is loaded on a mounting shaft r1. The film is delivered from the raw roll 80 equipped in the film delivery section 01, and the film is stretched while being heated in an oven in the stretching section 04. The stretched film passes through the cooling section 06 to have its temperature lowered and is wound up in the winding section 07. The film delivery section 01, the stretching section 04, the cooling section 06, the winding section 07, etc. are provided with an EPC (edge position controller) that controls the film to suppress meandering and transport it accurately. The EPC is not shown.
[0032] In the film roll manufacturing apparatus 100, a detection device 90 is disposed between the splicing position of the splicing processing unit 02 and the gripping position of the gripping unit of the stretching unit 04. In particular, the detection device 90 is disposed between the accumulation unit 03 and the stretching unit 04. The detection device 90 monitors the surface of the film F8 being transported in the production line, photographs the film surface, and analyzes the obtained frame image to detect the splicing state of the film F8 at the splicing processing unit 02. The configuration of the detection device 90 will be described later (FIGS. 4 and 5). In FIG. 1, the outlined arrow indicates the transport direction of the film F8 (the same applies to FIGS. 2, 3, etc.).
[0033] (Film Outlet 01) The film delivery section 01 has a turret-type film delivery device 13. The film delivery device 13 has a turret arm 131 with mounting shafts r1 at both ends. An original web roll 80 is attached to each mounting shaft r1. The turret arm 131 rotates 180 degrees to position one mounting shaft r1 at the delivery position (the side of the splicing processing section 02) and the other mounting shaft r1 at the core replacement position. The film F8 is delivered from the original web roll 80 attached to the mounting shaft r1 at the delivery position to the splicing process of the subsequent splicing processing section 02. When all the film F8 has been delivered, the turret arm 131 rotates, and the empty core is removed from the mounting shaft r1 positioned at the core replacement position, and a new film roll (original web roll 80) is attached.
[0034] (Joining processing section 02) In the joining process, in order to supply a continuous film F8 to the stretching section 04, the joining section 02, which uses a thermal welding method, joins two adjacent films F8 by welding. More specifically, as described below, the joining section 02 overlaps and joins the rear end of the preceding film F8 sent out in advance with the front end of the following film F8 sent out in the following direction.
[0035] FIG. 2 is a schematic diagram showing the configuration of the bonding processing section 02. As shown in FIG. 2, the bonding processing section 02 includes an upper head 21 and a lower head 22. The upper head 21 includes a heater 212 such as a resistance heating element or a heating means of an electromagnetic induction heating (IH) type, a heating member 213 that incorporates the heater 212 and is adjusted to a predetermined temperature, and a holding member 211 that houses the heating member 213. The entire upper head 21 is moved vertically by a driving mechanism (none of which are shown) having power such as a motor. The lower head 22 also has a similar configuration. Normally, the upper and lower heads 21 and 22 are in the retracted position shown in FIG. 2. During bonding, the upper head 21 moves downward and the lower head 22 moves upward to move to the heating position. As a result, the heating members 213 of the upper and lower heads 21 and 22 press against each other with a predetermined bonding pressure to form a nip region, and the film F8 placed in the nip region is heated and melt-bonded while being pressed with the predetermined bonding pressure. In FIG. 2, the range Lx2 corresponds to the nip region. For example, the length of the nip width Lx2 is 10 mm.
[0036] In the joining process, the leading edge of the trailing film F82 is placed so that it overlaps the trailing edge of the leading film F81 that has stopped just before the nip region. The overlapping range in which the two films F81 and F82 overlap is made slightly longer than the length of the nip width Lx2. For example, in the example shown in FIG. 2, the overlapping width Lx1 is 20 mm, and the overlapping region is placed so as to straddle the nip region. Of the overlapping regions in which the leading and trailing edges of the two films F81 and F82 overlap, the nip region is pressurized and heated to form a joining portion. The placement of the films F81 and F82 in the nip region as shown in FIG. 2 may be performed manually by a human being, or may be performed automatically by the control device 09 by detecting the stopping positions of the films F81 and F82 with a sensor and stopping them.
[0037] In the bonding process, the leading film F81 is stopped at a position straddling the nip region as shown in FIG. 2. The trailing film F82, which is then transported, has its leading end overlapped on the trailing end of the leading film F81 so as to have an overlap width Lx1. Then, the upper and lower heads 21 and 22 are moved to the nip position. At this time, the heating members 213 of the upper and lower heads 21 and 22 are heated to a predetermined temperature. For example, the temperature of the heating member 213 is adjusted to a predetermined bonding temperature (for example, within a range of 160 to 250°C). After heating at a predetermined bonding pressure for a predetermined bonding time, the upper and lower heads 21 and 22 are moved to the retreat position, and the bonding process is completed. As a result, both films F81 and F82 are melt-bonded at the bonding portion g1.
[0038] In the joining processing section 02, instead of the above-mentioned thermal welding method, an ultrasonic welding method or a laser welding method may be adopted. For example, in the ultrasonic method, the overlapping parts of both films F81 and F82 are mechanically vibrated by a vibration section at 20,000 to 28,000 times per second while applying pressure, so that the interface between both films is melted by frictional heat and joined. In addition, in the joining processing section 02, it is preferable that the rear end part of the leading film F81 after joining and the front end part of the following film F82, which are the remaining parts around the joining part g1, are cut by a laser or the like so as to be parallel to the joining line of the joining part g1. Here, the joining line corresponds to the joining part g1, and is located between the line (line) forming the end of the rear end part of the leading film F81 and the line (line) forming the end of the front end part of the following film F82 (before the joining process), and refers to the line (line) along which the two films are actually joined by welding.
[0039] (Accumulation Section 03) An accumulation unit 03 is provided between the splicing unit 02 and the stretching unit 04. This accumulation unit 03 has a buffer function to prevent the subsequent process from being stopped while the splicing process is being performed in the splicing unit 02. This accumulation unit 03 forms a film loop that is equal to or longer than the length of the film F8 transported in the time required for the film splicing process. Therefore, during the splicing process in the splicing step, the film F8 stored in the accumulation unit 03 is sent to the stretching unit 04. This allows the splicing process of the film F8 to be performed without stopping the stretching unit 04 when the raw roll 80 is replaced.
[0040] (Extending section 04, Trimming section 05) FIG. 3 is a perspective view showing a schematic configuration of a stretching process (also referred to as a tenter process) and a trimming process of the production line in FIG.
[0041] The stretching unit 04 performs at least one of an MD stretching process, a TD stretching process, and an oblique stretching process. It may also perform simultaneous biaxial stretching, which simultaneously performs biaxial stretching in the MD and TD directions. In the following example, the stretching unit 04 will be described as performing the MD stretching process and the TD stretching process. The stretching unit 04 stretches the unstretched film F8 that is fed and transported from the film delivery unit 01. As shown in FIG. 3, the stretching unit 04 uses a plurality of pairs of left and right gripping units 401 to grip both side ends of the film F8. The stretching unit 04 includes the gripping units 401, a chain, a driving unit, a closer, an opener, and the like (not shown are units other than the gripping units 401).
[0042] In the MD stretching process on the upstream side, the film accelerates as it is transported downstream, and the moving speed in the transport direction gradually increases (indicated by the black arrows in Figures 3 and 4). As a result, in the MD stretching process, the unstretched film F8 is transported while being stretched in the MD direction.
[0043] In the next TD stretching process, the film F8 is transported by the gripping parts 401. The gripping parts 401 are, for example, clips, and the left and right gripping parts 401 are connected to, for example, endless chains. The chains wound around sprockets are rotated by a drive unit, so that the gripping parts 401 move in the transport direction, etc. A closer is disposed on the most upstream side of the TD stretching process of the stretching part 04, and an opener is disposed on the most downstream side. When the gripping parts 401 reach the closer position, the open gripping parts 401 are sequentially closed, and when they reach the opener position, they are sequentially opened. The side ends of the unstretched film F8 are gripped by the gripping parts 401 in the closed state, and the film is transported. In this TD stretching process, the pair of left and right gripping parts 401 gripping the unstretched film F8 move in the transport direction and gradually move outward in the width direction (indicated by black arrows in FIG. 3). As a result, in the TD stretching step, the distance (spacing) in the width direction between the pair of gripping parts 401 gradually increases, and the unstretched film F8 gripped by them is transported while being stretched in the TD direction.
[0044] The cutting unit 05a includes two slitters 511, one on the left and one on the right, and multiple rollers 512, 513. The slitter 511 is, for example, a circular blade or a dish-shaped blade rotatably supported on a shaft, and is rotated by a drive unit (not shown). The slitter 511 may be rotated in the forward direction of the transport direction of the film F8 at the cutting position at a speed approximately equal to that of the transport direction of the film F8, or may be rotated in the opposite direction.
[0045] The two slitters 511 separate the film F8 after the cutting positions x1 and x2 into the central film F8 and the trimmed films F801 and F802 (also called ears or selvages) which are the side ends on both sides. The cutting position x1 of the right slitter 511 and the cutting position x2 of the left slitter 511 may be configured to be at the same position in the conveying direction, or may be arranged alternately with a predetermined interval (for example, several mm to several m) in the conveying direction. In the example shown in FIG. 3, the cutting position x2 is set about 2 m upstream of the cutting position x1. By arranging them alternately, the stress applied to the film F8 when slitting both ends in the width direction can be released to the opposite side of each slitter 511, so that small wrinkles are not generated during cutting, and thus the generation of scratches is also reduced.
[0046] The central portion of the film F8 is the area that will become the product, and its width is in the range of 1000 mm to 2500 mm. The widths (also called trim widths) of the trimmed films F801, F802 are both several tens to several hundred mm (for example, 170 mm). The central portion of the film F8 is transported downstream in the transport direction and supplied to a winding process in the subsequent stage. Meanwhile, the trimmed films F801, F802 are turned 90 degrees downward by roller 512, transported, and collected by collection unit 05b in the subsequent stage.
[0047] The collecting unit 05b has a duct, a rotary cutter disposed inside the duct, and a vacuum cleaner (none of which are shown). The vacuum cleaner is equipped with a suction fan and creates negative pressure inside the vacuum cleaner and the duct. The tip of the trimming film F801 (or F802) is cut into fine chips of a few millimeters in size by the collecting unit 05b, and is collected in a dust box inside the vacuum cleaner.
[0048] The central portion of the film F8 is transported to the downstream winding section 07. A knurling process may be performed by providing a knurling step between the trimming section 05 and the winding section 07. In the knurling step, knurls are formed on both ends of the trimmed film F8.
[0049] (Cooling section 06) The cooling section 06 is equipped with a number of rollers, and the stretched film F8 is transported through the cooling section 06 by the rollers. In the process preceding the cooling section 06 (thermal relaxation process), air at a desired temperature is blown in from an air blower to heat-treat the film. The temperature of the air at this time is preferably 20 to 250°C. After being thermally relaxed in the preceding process, the film F8 is sent to the subsequent cooling process and cooled to 30°C or lower.
[0050] (Winding section 07) A winding shaft r2 and a press roller are provided inside the winding unit 07. The film sent to the winding unit 07 is wound up by the rotating winding shaft r2. At this time, the film is pressed by the press roller while being wound up.
[0051] The material of the film F8 produced as shown in Figures 1 to 3 is not particularly limited, but generally includes polycarbonate resin, polysulfone resin, acrylic resin, polyolefin resin, cyclic olefin resin, polyether resin, polyester resin, polyamide resin, polysulfide resin, unsaturated polyester resin, epoxy resin, melamine resin, phenol resin, diallyl phthalate resin, polyimide resin, urethane resin, polyvinyl acetate resin, polyvinyl alcohol resin, styrene resin, cellulose acetate resin, vinyl chloride resin, etc. In addition, for example, the width of the film F8 is preferably 1000 mm to 2500 mm in consideration of productivity, quality, etc. In consideration of quality, handling, etc., the thickness is preferably 15 μm to 50 μm.
[0052] The length of the optical film F8 in the film roll 85 wound around the winding shaft r2 is preferably 2000 m to 8000 m, taking into consideration productivity, winding quality, and the like. The winding shaft r2 is shown in FIG. 1. The winding shaft is also called the winding core. The winding length indicates a value calculated from the speed and time. The winding speed is, for example, 100 m / min.
[0053] (Manufacturing management system 200) Next, the configuration of the detection device 90 and the hardware configuration of the manufacturing management system 200 including the same will be described with reference to FIGS. 4 to 7. FIG. 5 is a schematic diagram showing the configuration of the detection device 90 and the manufacturing management system 200 including the same. The manufacturing management system 200 includes a film roll manufacturing device 100 and the detection device 90. The detection device 90 or the film roll manufacturing device 100 is connected to a display 81, a PC (personal computer) 82, and an alarm unit 83. The detection device 90 (output unit 95) outputs the determination result of the joining condition of the film F8 by the joining processing unit 02 to at least one of the display 81, the PC 82, and the control device 09. The display 81 or the display of the PC 82 functions as a display unit. In addition, when the detection device 90 (output unit 95) detects an abnormality in the joining condition of the film F8, it outputs the result to the display 81, the PC 82, and the control device 09, and the control device 09 that receives the result warns the user through the alarm unit 83. The alarm unit 83 is, for example, at least one of a patrol lamp, a speaker, a siren, and a display arranged on the production line.
[0054] (Film roll manufacturing device 100) As described above, the film roll manufacturing apparatus 100 has the film delivery section 01, the joining section 02, the accumulation section 03, the stretching section 04, the trimming section 05, the cooling section 06, and the winding section 07. These sections 01 to 07 execute the delivery process, joining process, accumulation process, stretching process, cooling process, trimming process, thermal relaxation / cooling process, and winding process.
[0055] The film roll manufacturing apparatus 100 also includes a control device 09 that sets manufacturing conditions for each of these components 01 to 06. The control device 09 is composed of a CPU, a memory, etc. For example, the manufacturing conditions controlled by the control device 09 include the following. - Adjustment of film F8 (F8) conveying speed common to each process, - The unwinding conditions such as the unwinding speed of film F8 in the unwinding process, - Bonding conditions such as bonding temperature, bonding time, and bonding pressure in the bonding process - Film F8 intake and discharge conditions in the accumulation process; - Winding conditions of film F8 in the winding process, Clipping conditions of the gripping portion 401 in the stretching process.
[0056] (Detection device 90) The detection device 90 detects an abnormality in the splicing condition of the film F8 being transported. The detection device 90 includes one or more imaging units 91 that capture images of a monitoring area, a light source 92 that irradiates the monitoring area with light, a processing unit 93 that processes frame images obtained from the imaging units 91 to determine the splicing condition (the degree of splicing), a storage unit 94, and an output unit 95.
[0057] (Processing unit 93, storage unit 94) The processing unit 93 is composed of a CPU, a RAM, etc., reads out various processing programs stored in the storage unit 94, loads them into the RAM, and performs various processes in cooperation with the programs. The determination process of the processing unit 93 will be described later.
[0058] The storage unit 94 is composed of an HDD, an SSD (Solid State Drive), etc., and stores various processing programs, data required for executing the programs, etc. The storage unit 94 has a function of a camera recorder, and stores time-series frame images (moving images) obtained by shooting with the imaging unit 91 in real time. The storage unit 94 also records a manufacturing history. The manufacturing history is recorded by linking the manufacturing conditions of the film roll, and data on the approximation line, ideal line, and degree of joining of the end near the joint a2 at the time of manufacturing.
[0059] (imaging unit 91, light source 92) 5 is a diagram for explaining a monitoring area arranged immediately upstream of the stretching process. The monitoring area photographed by the detection device 90 is preferably arranged immediately downstream of the joining processing unit 02 or immediately upstream of the stretching process. However, the monitoring area is not limited to this, and may be arranged at any position within the range from the joining process to the winding process.
[0060] The imaging unit 91 is composed of an imaging element such as a CCD or CMOS, and an optical system such as a lens, and outputs frame images in a time series. The imaging unit 91 may also be provided with a buffer memory for temporarily storing the captured frame images. The imaging unit 91 may also be a network camera equipped with a control unit and a network I / F. For example, a 1 / 2-inch CMOS is used as the imaging element of the imaging unit 91. The imaging unit 91 outputs images of 1920×1080 pixels at a maximum frame rate of 100 to 120 fps. The frame rate can be set appropriately within the maximum rate range. For example, the frame rate can be set to 120, 100, 60, or 30 fps.
[0061] As shown in FIG. 3, the monitoring area is arranged so as to capture the edge in the width direction of the surface of the film F8 being transported. In particular, the monitoring area has the imaging unit 91 arranged at a position where one edge of the film F8 being transported can be captured. In the following, an example will be described in which the right edge in the width direction of the film F8 is captured, but a second imaging unit 91 may be arranged so as to capture the left edge on the opposite side. The imaging unit 91 detects diffuse light from the light irradiated by the light source 92 and reflected in the monitoring area of the film F8. Here, a color camera is used as the imaging unit 91. The imaging unit 91 and the light source 92 may irradiate and detect light in the visible light region, or may irradiate and detect light in the infrared region. In the following, the imaging unit 91 will be described as detecting light in the visible light region, and the light source 92 as a light source that irradiates visible light other than white. For example, the light source 92 is a red surface light source.
[0062] (monitoring area) As shown in Fig. 5, the monitoring area is set downstream of the joining process so as to photograph the surface of the film F8 including the joint g1 (see Fig. 2) and the side edge on the near side (right side). In the width direction, the monitoring area encompasses the vicinity of the side edge, including the side edge (edge) on the near side of the film F8, which is about 2 m wide.
[0063] As shown in FIG. 5, the imaging unit 91 is disposed so as to capture the side edge e1 of the film F8. The optical axis c1 of the imaging unit 91 intersects with the surface of the film F8 at the intersection p1. The optical axis c1 is also called the shooting direction and is the optical axis of the lens of the imaging unit 91. The intersection p1 is located approximately at the center of the monitoring area. The shooting angle α1 is the angle between the optical axis c1 and the surface of the film F8 (the surface when ideally transported). The shooting angle α1 corresponds to the complementary angle of the incident angle. The preferred range of the shooting angle α1 is 10 degrees or more and 30 degrees or less. More preferably, the shooting angle α1 is 20 degrees. The preferred range of the distance from the imaging unit 91 to the intersection p1, more specifically, the distance from the outer surface of the lens of the imaging unit 91 to the intersection p1, is 50 mm or more and 2000 mm or less. The more preferred distance is 100 mm.
[0064] The light source 92 is arranged and configured so that direct light does not enter the imaging unit 91, i.e., so that direct light does not enter the lens of the imaging unit 91 and is not received by an optical element. Also, it is preferable that the light source 92 is arranged so that specularly reflected light from the surface of film F8 of the light emitted from the light source 92 does not enter the imaging unit 91, and only scattered reflected light from the surface enters the imaging unit 91. The light source 92 is preferably configured as a surface light source or a set of multiple single light sources. In the example shown in Fig. 5, the light source 92 is a surface light source that emits red light.
[0065] (Detection process of the joining condition of the joining part g1) Fig. 6 is a flow chart showing a process for detecting the degree of splicing by the detection device 90. In the process shown in Fig. 6, a set monitoring area is photographed by the imaging unit 91 to detect the degree of splicing. When photographing a plurality of monitoring areas, for example, when photographing both the right and left ends, the same process is performed in parallel to detect the degree of splicing in each monitoring area, but the process content is the same. In addition, the process shown in Fig. 6 is performed in synchronization with the splicing process that is performed when a new raw fabric roll 80 is replenished.
[0066] (Step S01) The film roll manufacturing apparatus 100 stops the transport of the film F8 before the leading original roll 80 of film F8 is completely fed. Specifically, the film roll manufacturing apparatus 100 continues the transport of the film F8 downstream of the accumulation unit 03, and stops the transport of the film F8 upstream of the accumulation unit 03. The leading film F8 (F81) is cut, and its rear end is set in the nip area (see FIG. 2). The film delivery device 13 moves a new original roll 80 to the delivery position, and the film F8 is delivered from this original roll 80. The leading end of the newly delivered trailing film F8 (F82) is stopped at a position where it passes the nip area and the overlap width is Lx1. Thereafter, the joining process is performed by the joining process unit 02. During the joining process, the rear end of the preceding film F8 is stopped, but by releasing the film F8 accumulated in the accumulation section 03, the process continues without stopping in the stretching process and subsequent processes.
[0067] After the joining process is completed, the film F8 that has been joined together starts to be transported and is sent to the accumulation unit 03 and subsequent units.
[0068] (Step S02) The imaging unit 91 captures an image of an end area of the film F8. During the production of the film roll, the imaging unit 91 captures an image of a monitoring area. Time-series frame images are obtained by capturing the images. The time-series frame images are stored in a buffer memory of the imaging unit 91 or in a storage unit 94.
[0069] (Step S03) After the joining process is completed, the processing unit 93 recognizes the joint g1 by performing image analysis on frame images obtained within a predetermined time after the film F8 near the joining process starts to be transported. Then, from among the multiple frame images in which the joint g1 is recognized, a frame image to be processed (hereinafter, the target frame image) is extracted. For example, if the shooting is performed at 100 fps and the transport speed of the film F8 is 1 to 2 m / sec, the film F8 moves 10 to 20 mm in the transport direction for each frame (10 msec). In this case, the joint (10 mm width) is captured in frame images of several frames to 10 and several frames. From the chronological order of frame images in which the joint g1 is recognized, the processing unit 93 extracts the center frame image as the target frame image, or extracts a frame image in which the joint g1 is located at a predetermined position (center area) of the image as the target frame image. FIG. 7A is an example of the extracted target frame image. In the example shown in FIG. 7A, the film F8 moves from the upper left to the lower right. A red light source is used as the light source 92, and the film F8 is a light-transmitting film. The irradiated light is diffusely reflected inside the joint g1, or at the interface between the two joined films F8. Therefore, as shown in Fig. 7A, the joint g1 (joint line) is recognized as a streak of red light. The processing unit 93 can recognize the joint g1 by extracting a cluster of pixels whose color corresponds to the light source 92.
[0070] (Step S04) The processing unit 93 recognizes the side ends (end points) by performing image processing on the target frame image. For example, the processing unit 93 recognizes end points corresponding to the side ends (edges) of the film by performing edge processing in the film width direction based on pixel values. The processing unit 93 then calculates an approximation line connecting the multiple end points.
[0071] (Step S05) Furthermore, the processing unit 93 removes end points near the junctions from among the end points, and calculates an ideal straight line from the end points after removal. The range to be removed is the end points that overlap the junction g1. Note that the range to be removed may be set to a range included in a predetermined range from the junction g1 (e.g., a pixel distance of 50 mm). As a method of calculating the ideal line, for example, the processing unit 93 may calculate a regression line from the end points after removal using the least squares method, and use this as the ideal line.
[0072] (Step S06) The processing unit 93 calculates the degree of bonding by evaluating the deviation between the approximation line refined in steps S04 and S05 and the ideal straight line. For example, the processing unit 93 uses the deviation angle between the approximation line and the ideal straight line as the degree of bonding. As another example, the processing unit 93 calculates the area caused by the deviation between the approximation line and the ideal straight line, that is, the area (number of pixels) surrounded by the approximation line and the ideal straight line, as the degree of bonding. The area is calculated within a predetermined range from the bonding part g1. For example, the area is calculated within a range equivalent to several tens of mm before and after the bonding part g1 in the conveying direction. The degree of bonding is determined to be poorer as the value is larger.
[0073] (Step S07) The processing unit 93 detects uneven regions by performing image processing on the frame images. The uneven regions are generated by bending of the surrounding film F8 due to the heating process when generating the joint g1. For example, the processing unit 93 extracts pixels whose pixel values are equal to or less than a predetermined threshold, performs clustering processing on the extracted pixels, and recognizes clusters with a predetermined area or more as uneven regions. The predetermined threshold may be set based on the average pixel value of the surface of the film F8, or the average value and variance value.
[0074] (Step S08) The processing unit 93 generates a display image in which the approximation line, the ideal straight line, and the uneven area are superimposed on the target frame image. The output unit 95 causes the display unit to display the display image generated by the processing unit 93. For example, the processing unit 93 displays it on the display 81 or transmits it to the PC 82.
[0075] Fig. 7B is an example of a display screen displayed by the output unit 95 on the display 81. In Fig. 7B, images showing the calculated or recognized ideal line (ideal straight line), approximation line, and uneven area are displayed together with the target frame image. The degree of bonding is also shown. By using such a display screen, the user (manager of the production line) can easily recognize whether or not bonding has been performed appropriately in the bonding process. Note that in Fig. 7B, the target frame image shown in Fig. 7A would normally be displayed as is in the central area, but in Fig. 7B, it is shown with a lighter density for ease of viewing.
[0076] Furthermore, on the display screen, ideal lines and / or approximation lines in the past history may be displayed superimposed. For example, when the user operates the history ON button on the display screen of FIG. 7B, ideal lines and approximation lines in the past history under the same production conditions are further superimposed and displayed on the display screen. Furthermore, if there are multiple histories, data selected by the user from among them may be displayed. It is preferable that the ideal lines and approximation lines related to the history are color-coded so that they can be distinguished from the current ideal lines and approximation lines. By displaying the ideal lines and approximation lines of the history together, the current level of bonding can be easily confirmed.
[0077] (Step S09) The processor 93 determines whether or not the alarm condition is satisfied depending on the degree of bonding determined in step S06. For example, the processor 93 determines that the alarm condition is satisfied when the difference in angle between the ideal line (ideal straight line) and the approximation line as the degree of bonding is equal to or greater than a predetermined threshold.
[0078] (Step S10) The output unit 95 performs a reporting process. For example, the output unit 95 notifies the control device 09 of a warning as reporting information, or displays the warning on the display 81. Furthermore, upon receiving the warning, the control device 09 reports the warning to the user via the reporting unit 83. Furthermore, depending on the level of the degree of splicing, for example, if the level is worse than a predetermined threshold level, the control device 09 stops the ongoing production of the film roll 85.
[0079] (Step S17) The user changes the manufacturing conditions of the production line in response to the warning display. The change in the manufacturing conditions may be automatically performed by the control device 09, or the recommended manufacturing conditions may be output to a display or the like. For example, when the control device 09 automatically performs the change, the control device 09 changes at least one of the clip conditions in the stretching process, the conveying conditions in each process, and the winding conditions in the winding process in order to reduce the influence of poor splicing. In addition, in order to improve the level of the next production or the next splicing process, the control device 09 changes at least one of the payout conditions in the film sending unit 01 and the splicing conditions in the splicing processing unit 02, and stores the changed conditions in the storage unit 94. The stored changed manufacturing conditions are read out in the next production or the next splicing process, and the film is manufactured under the changed conditions.
[0080] In this way, the detection device according to the present embodiment includes an imaging unit that captures the film being conveyed, and a processing unit that calculates the degree of splicing of the film by the splice by analyzing a frame image of the film including the splice obtained by the imaging unit. The processing unit then calculates an approximation line connecting multiple end points of the detected film and an ideal line calculated from multiple end points of the film excluding the end points of the film that are on the splice, and calculates the degree of splicing based on the approximation line and the ideal line. This allows the detection device 90 to appropriately detect the splice condition in the splicing process when manufacturing the film, thereby preventing the occurrence of defects in the optical properties of the film and also preventing the occurrence of events that lead to production stoppages, such as film cracks and breakages, in the stretching process.
[0081] In addition, in the detection device according to this embodiment, the output unit outputs the bonding degree, and the display unit displays the calculated approximation line and ideal line superimposed on the display image of the frame image. This allows a user who manages the production line to easily recognize the level of the bonding degree and the state of the bonding degree.
[0082] The above-described configurations of the manufacturing management system 200 and the detection device 90 are the main configurations described in order to explain the features of the above embodiment, but are not limited to the above configurations and can be modified in various ways within the scope of the claims. Furthermore, configurations of general manufacturing management systems and detection devices are not excluded.
[0083] In addition, the manufacturing management system 200 and the means and methods for performing various processes in the detection device 90 according to the above-mentioned embodiment can be realized by either a dedicated hardware circuit or a programmed computer. The above-mentioned program may be provided by a computer-readable recording medium such as a USB memory or a DVD (Digital Versatile Disc)-ROM, or may be provided online via a network such as the Internet. In this case, the program recorded in the computer-readable recording medium is usually transferred to and stored in a storage unit such as a hard disk. In addition, the above-mentioned program may be provided as a standalone application software, or may be incorporated into the software of the device as one of its functions. EXAMPLES
[0084] The present invention will be specifically described below with reference to examples, but the present invention is not limited to these.
[0085] <Production Example 1> <Preparation of roll-shaped raw film 1> (Preparation of Polyester A) Under a nitrogen atmosphere, 4.85 g of dimethyl terephthalate, 4.4 g of 1,2-propylene glycol, 6.8 g of p-toluic acid, and 10 mg of tetraisopropyl titanate were mixed and stirred at 140° C. for 2 hours, and then further stirred at 210° C. for 16 hours. Next, the temperature was lowered to 170° C., and the unreacted 1,2-propylene glycol was distilled off under reduced pressure to obtain Polyester A.
[0086] Acid value: 0.1 Number average molecular weight: 490 Dispersion degree: 1.4 Molecular weight 300-1800 component content: 90% Hydroxyl value: 0.1 Hydroxyl group content: 0.04% In polyester A, the monocarboxylic acid is used in a molar ratio of twice that of the dicarboxylic acid, and therefore the terminal end is a toluic acid ester.
[0087] <Fine particle dispersion liquid 1> Fine particles (Aerosil R812, manufactured by Nippon Aerosil Co., Ltd.) 11 parts by weight Ethanol 89 parts by weight The above was mixed by stirring for 50 minutes using a dissolver, and then dispersed using a Manton-Gaulin mixer.
[0088] <Fine particle additive liquid 1> The microparticle dispersion liquid 1 was slowly added to a dissolution tank containing methylene chloride while stirring thoroughly. The mixture was then dispersed in an attritor so that the secondary particles had a predetermined particle size. The mixture was filtered through Finemet NF manufactured by Nippon Seisen Co., Ltd. to prepare microparticle additive liquid 1.
[0089] Methylene chloride 99 parts by mass Fine particle dispersion liquid 1 5 parts by mass A main dope solution with the following composition was prepared. First, methylene chloride and ethanol were added to a pressurized dissolution tank. Cellulose ester was added to the pressurized dissolution tank containing the solvent while stirring. This was heated and stirred until it was completely dissolved. This was filtered using Azumi Filter Paper No. 244 manufactured by Azumi Filter Paper Co., Ltd. to prepare the main dope solution.
[0090] <Composition of main dope> Methylene chloride 340 parts by mass Ethanol 64 parts by weight Cellulose ester (cellulose diacetate: acetyl group substitution degree 2.4, propionyl group 0, total substitution degree 2.4) 100 parts by mass 7.0 parts by mass of sugar ester compound A shown below Polyester A 2.5 parts by weight TINUVIN928 (BASF Japan) 1.5 parts by weight Fine particle additive liquid 1 1 part by mass
[0091] [ka]
[0092] The above ingredients were placed in a sealed container and dissolved under stirring to prepare a dope solution.
[0093] Next, using an endless belt casting apparatus, the dope solution was uniformly cast onto a stainless steel belt support having a width of 1500 mm at a temperature of 33° C. The temperature of the stainless steel belt was controlled at 30° C.
[0094] The solvent was evaporated on the stainless steel belt support until the residual solvent content in the cast film was 75%, and then the film was peeled off from the stainless steel belt support with a peeling tension of 110 N / m.
[0095] The peeled cellulose ester film was stretched by 5% in the width direction using a tenter while being heated at 160° C. The residual solvent content at the start of stretching was 15%.
[0096] Next, the drying was completed while the film was conveyed through a drying zone by multiple rolls. The drying temperature was 130° C., and the conveying tension was 100 N / m.
[0097] In this manner, a roll of raw film F8 having an average dry thickness of 75 μm was obtained.
[0098] The thickness unevenness in the longitudinal direction of the obtained raw film F8 was 0.15 μm, and the thickness unevenness in the transverse direction was 0.15 μm. When the in-plane retardation and the retardation in the thickness direction at a wavelength of 550 nm were measured by the above-mentioned method, Ro(550) was 10 nm, and Rt(550) was 120 nm.
[0099] <Example 1> The film F8 of the raw film 1 produced by the method of Production Example 1 described above was stretched using the film roll production apparatus 100 shown in FIG.
[0100] First, the original roll 80 was attached to the roll mounting shaft r1 of the film delivery device 13 and set at the delivery position, and then the film roll manufacturing apparatus 100 transported the original roll 80 through the accumulation section 03, the stretching section 04 (TD stretching process), the trimming section 05, and the cooling section 06 so that it was wound into a roll in the winding section 07. In the accumulation section 03, a sufficient loop was made. In the TD stretching process of the stretching section 04, the original roll 80 was stretched at 175°C and a stretch ratio of 1.5.
[0101] The average thickness of the obtained retardation film was 50 μm.
[0102] A new roll of original film 1 (original roll 80) is attached to the mounting shaft r1 at the core replacement position, and just before the film of the original roll 80 at the delivery position runs out, the transportation of the preceding original roll 80 is stopped and the film rear end is cut so that it is at the joining position. After that, the turret arm is rotated 180 degrees, and a new roll of original film 1 (original roll 80) that was previously attached to the other mounting shaft r1 is set at the delivery position and transported to the joining process. A heat welding machine was used in the joining process. The rear end of the preceding film and the front end of the following film after joining were cut so that they were parallel to the joining line of the joining part g1. The widthwise ends that were chucked by the gripping part 401 in the later stretching part 04 were processed by a heat welding machine along the same joining line, and the total thickness was set to 94 μm.
[0103] During the splicing operation, the stretching section 04 did not stop because the film stored in the accumulation section 03 was sent to the stretching section 04. The spliced film F8 was transported to the stretching section 04 via the accumulation section 03.
[0104] <Example 2> A film was produced by the same process as in Example 1. However, in the stretching section 04, an oblique stretching process was applied in which the film was heated, both ends were held by a plurality of grippers, and the film was stretched in an oblique direction at an angle of 40 to 50° relative to the width direction of the film. In the oblique stretching process in the stretching section 04, the film was stretched at 175°C and a stretch ratio of 1.5.
[0105] The average thickness of the obtained retardation film was 50 μm, the in-plane retardation value Ro (550) at a wavelength of 550 nm was 140 nm, and the angle θ between the in-plane slow axis and the film width direction was 45°. Here, the in-plane slow axis of the optical film refers to the axis on the film surface where the refractive index is maximum. The in-plane slow axis of the optical film can be confirmed by an automatic birefringence meter Axoscan (Axo Scan Mueller Matrix Polarimeter: manufactured by Axometrics).
[0106] A new roll of original film 1 (original roll 80) is attached to the mounting shaft r1 at the core replacement position, and just before the film of the original roll 80 at the delivery position runs out, the transportation of the preceding original roll 80 is stopped and the film rear end is cut so that it is at the joining position. After that, the turret arm is rotated 180 degrees, and a new roll of original film 1 (original roll 80) that was previously attached to the other mounting shaft r1 is set at the delivery position and transported to the joining process. A heat welding machine was used in the joining process. The rear end of the preceding film and the front end of the following film after joining were cut so that they were parallel to the joining line of the joining part g1. The widthwise ends that were chucked by the gripping part 401 in the later stretching part 04 were processed by a heat welding machine along the same joining line, and the total thickness was set to 94 μm.
[0107] During the splicing operation, the stretching section 04 did not stop because the film stored in the accumulation section 03 was sent to the stretching section 04. The spliced film F8 was transported to the stretching section 04 via the accumulation section 03. [Explanation of symbols]
[0108] 200 Manufacturing Management System 90 Detection Device 91 Imaging section 92 Light source 93 Processing section 94 Memory section 95 Output section 100 Film roll manufacturing equipment 01 Film sending section 02 Joining section 03 Stretching section 05 Trimming Department 05a Cutting section 05b Recovery Section 06 Cooling section 07 Winding section 09 Control device 81 Display 82 PC 83 Reporting Department
Claims
1. A detection device used in a production line for a film roll, which is manufactured by the steps of: a delivery process for paying out a film; a stretching process for stretching the film by gradually increasing the distance in the width direction between a plurality of pairs of gripping sections while gripping both side ends of the film being transported and heated; a winding process for winding the stretched film around a core; and a joining process for joining a leading film and a trailing film at a joint where the leading and trailing ends of the films are overlapped, prior to the stretching process, an imaging unit that captures an image of the film being transported; A processing unit that calculates a degree of bonding of the film by the bonding portion by analyzing a frame image of the film including the bonding portion obtained by the imaging unit, The processing unit calculates an approximation line connecting multiple end points of the detected film and an ideal line calculated from multiple end points excluding the end points of the film that overlap the joint, and calculates the degree of joint based on the approximation line and the ideal line.
2. 2. The detection device according to claim 1, wherein the degree of bonding is determined by evaluating a deviation between the ideal line and the approximation line.
3. 3. The detection device according to claim 2, wherein the deviation between the ideal line and the approximation line is a difference in angle between the ideal line and the approximation line, or a size of an area between the ideal line and the approximation line in a predetermined length before and after the joint in the conveying direction.
4. An output unit that outputs the degree of bonding is further provided. The detection device according to claim 1 , wherein the output section causes the display section to display the approximation line and the ideal line superimposed on a display image of the frame image.
5. The processing unit detects unevenness of the film by analyzing the frame images, The detection device according to claim 4 , wherein the output section displays the detected irregularities on a display image of the frame image in a superimposed manner.
6. Further, a storage unit is provided for storing data on a manufacturing history of the film roll, The detection device described in claim 4, wherein the output unit superimposes the approximation line and / or the ideal line calculated during a past film roll production stored in the production history on a display image of the frame image of the film roll currently being produced.
7. 7. The detection device according to claim 1, further comprising a light source for irradiating light onto the monitoring area of the film.
8. The detection device according to claim 4 , wherein the output unit outputs alarm information when the degree of bonding exceeds a threshold value.
9. a film roll manufacturing device for manufacturing a film roll by the following steps: a delivery step for paying out a film; a stretching step for stretching the film by gradually increasing the distance in the width direction between a plurality of pairs of gripping parts while gripping both side ends of the film being transported and heated; a winding step for winding the stretched film around a core; and a joining step for joining a leading film and a trailing film at a joint where the leading and trailing ends of the films are overlapped prior to the stretching step; A manufacturing control system including a detection device, The detection device includes: an imaging unit that captures an image of the film being transported; A processing unit that calculates a degree of bonding of the film by the bonding portion by analyzing a frame image of the film including the bonding portion obtained by the imaging unit, the processing unit calculates an approximation line connecting the detected side ends of the film and an ideal line connecting the side ends of the film excluding the end point of the film related to the joint, and calculates the degree of joint based on the approximation line and the ideal line. Manufacturing management system.
10. The manufacturing management system according to claim 9 , further comprising an output unit that outputs an alarm when the degree of bonding exceeds a threshold value.
11. The film roll manufacturing apparatus includes a control device, The manufacturing management system according to claim 9 or claim 10, wherein the control device changes clip conditions of the gripping parts in the stretching process or stops production of the film roll in progress when the degree of joining exceeds a threshold value.
12. The film roll manufacturing apparatus includes a control device, 11. The manufacturing management system according to claim 9, wherein the control device changes a preceding film transport condition or a winding condition in a winding process when the degree of splicing exceeds a threshold value.
13. The film roll manufacturing apparatus includes a control device, When the degree of joining exceeds a threshold value, the manufacturing conditions related to the feeding of the subsequent film in the sending step and / or the joining in the joining step are changed as the manufacturing conditions, and the changed manufacturing conditions are stored.
11. The manufacturing management system according to claim 9, wherein the film roll is manufactured under the stored changed manufacturing conditions during the next film roll manufacturing or during the next joining process in the joining step.
14. A method for detecting a state of bonding at a bonding portion used in a production line for a film roll manufactured by the steps of: a delivery step of paying out an unstretched film; a stretching step of stretching the film by holding both side ends of the film being transported and heated with a plurality of pairs of gripping portions while gradually increasing the distance between the pairs of gripping portions in the width direction; a winding step of winding the stretched film around a core; and a bonding step of bonding a preceding film and a following film at a bonding portion where the leading and trailing ends of the films are overlapped, prior to the stretching step, the method comprising: (a) photographing a film being transported; (b) calculating a degree of bonding of the film by the bonding portion by analyzing a frame image of the film including the bonding portion obtained by photographing. In the step (b), an approximation line connecting the detected side edges of the film and an ideal line connecting the side edges of the film excluding the end point of the film related to the joint are calculated, and the degree of joint is calculated based on the approximation line and the ideal line.
15. A control program for controlling a detection device for detecting a state of bonding at a bonding portion, which is used in a production line for a film roll manufactured by a delivery process for unwinding a film, a stretching process for stretching the film by gradually increasing a distance in a width direction between a plurality of pairs of gripping portions while gripping both side ends of the film being transported and heated, a winding process for winding the stretched film around a core, and a bonding process for bonding a leading film and a trailing film at a bonding portion where the leading and trailing ends of the films are overlapped, prior to the stretching process, the control program comprising: (a) photographing a film being transported; (b) calculating a degree of bonding of the film by the bonding portion by analyzing a frame image of the film including the bonding portion obtained by photographing. A control program for causing a computer to execute a process in which, in step (b), an approximation line connecting the detected side ends of the film and an ideal line connecting the side ends of the film excluding the end point of the film related to the joint are calculated, and the degree of joint is calculated based on the approximation line and the ideal line.
Citation Information
Patent Citations
Device for detecting joints in rubber sheets
JP2007530962A
Method and apparatus for jointing polymer film
JP2009029080A
Method for inspecting adhesive section of film and apparatus for inspecting adhesive section of film
JP2010023922A
Appearance inspection device, appearance inspection method, and program
JP2015068739A
Method for producing long-sized polymer film, î» / 4 plate, polarizing plate, and stereoscopic image display device
JP2012088592A