Hydrogen transport hose
The hydrogen transport hose with a thermoplastic resin and organic fiber reinforcing layer addresses durability and desorption rate issues, providing enhanced handleability and durability in high-pressure hydrogen environments.
Patent Information
- Application Number
- JP2023056038
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-11
AI Technical Summary
The existing hydrogen transport hoses suffer from significant damage due to low hydrogen desorption rates and inadequate durability, particularly in high-pressure hydrogen environments.
A hydrogen transport hose comprising an inner layer made of a thermoplastic resin composition with a specific elastomer and a reinforcing layer of organic fibers, designed to maintain a controlled hydrogen desorption rate and enhance durability.
The hose exhibits excellent handleability and durability, with a hydrogen desorption rate of 3.7 to 7.1 mass ppm/min and a volume expansion ratio of 5.0 or less, ensuring minimal material damage and extended lifespan.
Smart Images

Figure 2024143389000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a hose for transporting hydrogen. More specifically, the present invention relates to a hose for transporting hydrogen that is excellent in handling ability and durability. [Background technology]
[0002] In recent years, the development of fuel cell vehicles and the like has been active. Accordingly, the development of hoses that transport hydrogen gas from dispensers installed at hydrogen stations to fuel cell vehicles and the like is also progressing. These hydrogen transport hoses are required to have hydrogen gas barrier properties, flexibility in low-temperature environments, durability, and the like.
[0003] International Publication No. 2018 / 155491 (Patent Document 1) discloses a hose for transporting hydrogen, which has a hydrogen gas barrier layer made of a resin composition containing polyamide 11 and a modified olefin-based elastomer, a reinforcing layer disposed on the outside of the hydrogen gas barrier layer, and an outer cover layer containing a polyamide resin disposed on the outside of the reinforcing layer. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Publication No. 2018 / 155491 Summary of the Invention [Problem to be solved by the invention]
[0005] The hydrogen transport hose disclosed in Patent Document 1 is susceptible to significant damage from hydrogen due to the low hydrogen desorption rate of the hydrogen gas barrier layer, and therefore does not necessarily have sufficient durability.
[0006] The present invention provides a hose for transporting hydrogen that is easy to handle and has excellent durability by using a material having an appropriate hydrogen desorption rate for the inner layer and at least one layer made of organic fiber as a reinforcing layer. [Means for solving the problem]
[0007] The present invention is a hose for transporting hydrogen comprising an inner layer, a reinforcing layer and an outer layer, wherein the inner layer comprises a thermoplastic resin composition (A) comprising a thermoplastic resin (Aa) and an elastomer (Ab), the reinforcing layer comprises at least one layer made of organic fibers, and is characterized in that when the thermoplastic resin composition (A) is held in a hydrogen atmosphere of 90 MPa at 30°C for 24 hours or more and then reduced to atmospheric pressure, the hydrogen desorption rate from 30 to 90 minutes after reduction in pressure is 3.7 to 7.1 mass ppm / min.
[0008] The present invention includes the following embodiments. [1] A hose for transporting hydrogen comprising an inner layer, a reinforcing layer and an outer layer, wherein the inner layer comprises a thermoplastic resin composition (A) comprising a thermoplastic resin (Aa) and an elastomer (Ab), and the reinforcing layer comprises at least one layer made of organic fibers, and wherein when the thermoplastic resin composition (A) is held in a hydrogen atmosphere of 30°C and 90 MPa for 24 hours or more and then depressurized to atmospheric pressure, the hydrogen desorption rate v from 30 to 90 minutes after depressurization is 3.7 to 7.1 mass ppm / min. [2] The hose for transporting hydrogen according to [1], characterized in that the ratio T / v of the thickness T [mm] of the inner layer to the hydrogen desorption rate v [mass ppm / min] is 0.16 to 0.30. [3] The maximum volume V of the elastomer (Ab) when it is exposed to a hydrogen atmosphere of 90 MPa at 30°C for more than 24 hours and then depressurized to atmospheric pressure. MAX and the volume before exposure V O Ratio of V MAX / V O The hose for transporting hydrogen according to [1], wherein the resistance is 5.0 or less. [4] The hose for transporting hydrogen according to [1], wherein the thermoplastic resin (Aa) has a flexural modulus of 500 to 2000 MPa. [5] The hose for transporting hydrogen according to [1], characterized in that the thermoplastic resin composition (A) has an island-in-a-sea structure consisting of a matrix and domains dispersed in the matrix, the matrix contains a thermoplastic resin (Aa), and the domains contain an elastomer (Ab). [6] The hose for transporting hydrogen according to [5], characterized in that the domains have an average particle size of 2.0 μm or less. Effect of the Invention
[0009] The hose for transporting hydrogen of the present invention is excellent in handleability and durability. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a partially cutaway perspective view of a hose for transporting hydrogen according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The present invention is a hose for transporting hydrogen, comprising an inner layer, a reinforcing layer and an outer layer, wherein the inner layer comprises a thermoplastic resin composition (A) comprising a thermoplastic resin (Aa) and an elastomer (Ab), the reinforcing layer comprises at least one layer made of organic fibers, and is characterized in that when the thermoplastic resin composition (A) is held in a hydrogen atmosphere of 30°C and 90 MPa for 24 hours or more and then reduced to atmospheric pressure, the hydrogen desorption rate v from 30 to 90 minutes after reduction in pressure is 3.7 to 7.1 mass ppm / min.
[0012] A hydrogen transport hose is a hose used to transport hydrogen from a tank or cylinder to another tank or cylinder, and is preferably a hose that transports hydrogen gas from a dispenser installed at a hydrogen station to a fuel cell vehicle or the like.
[0013] 1 is a perspective view of a hose for transporting hydrogen according to the present invention, with a portion cut away to clearly show the layer structure, although the present invention is not limited to that shown in the drawing. The hydrogen transport hose 1 includes an inner layer 2, a reinforcing layer 3, and an outer layer 4. The reinforcing layer 3 is disposed on the outside of the inner layer 2. The outer layer 4 is disposed on the outside of the reinforcing layer 3. The reinforcing layer 3 includes at least one layer 5 made of organic fibers. The reinforcing layer 3 of the hydrogen transport hose in FIG. 1 includes three layers 5 made of organic fibers and further includes one layer 6 made of metal wires, but the reinforcing layer 3 of the hydrogen transport hose of the present invention may include only one layer 5 made of organic fibers, and the layer 6 made of metal wires is not essential.
[0014] The inner layer contains a thermoplastic resin composition (A).
[0015] When the thermoplastic resin composition (A) is maintained in a hydrogen atmosphere of 90 MPa at 30°C for 24 hours or more and then reduced to atmospheric pressure, the hydrogen desorption rate v is 3.7 to 7.1 mass ppm / min 30 to 90 minutes after reduction in pressure. Here, the hydrogen desorption rate 30 to 90 minutes after pressure reduction is the amount of hydrogen (g) desorbed from the thermoplastic resin composition during the 60 minutes between 30 and 90 minutes after pressure reduction, divided by the mass (g) of the thermoplastic resin composition, expressed in parts per million, and further converted to a rate per minute (unit: mass ppm / min). Hereinafter, the term "hydrogen desorption rate 30 to 90 minutes after pressure reduction to atmospheric pressure from a state in which the hydrogen atmosphere at 30°C and 90 MPa has been maintained for 24 hours or more" is also simply referred to as "hydrogen desorption rate". The hydrogen desorption rate is preferably 3.9 to 7.0 mass ppm / min, and more preferably 4.1 to 6.9 mass ppm / min. When the hydrogen desorption rate is within the above range, the thermoplastic resin composition (A) is only slightly damaged by hydrogen even when exposed to hydrogen, and the fatigue resistance does not decrease.
[0016] The ratio T / v of the thickness T [mm] of the inner layer to the hydrogen desorption rate v [mass ppm / min] is preferably 0.16 to 0.30, more preferably 0.17 to 0.28, and even more preferably 0.18 to 0.26. If T / v is within the above numerical range, damage to the thermoplastic resin composition (A) due to exposure to hydrogen is small. If T / v is too large, hydrogen does not escape from the system and defects are likely to occur, and if T / v is too small, the material cannot follow the deformation accompanying hydrogen desorption and defects are likely to occur.
[0017] The thermoplastic resin composition (A) contains a thermoplastic resin (Aa) and an elastomer (Ab).
[0018] The thermoplastic resin (Aa) is not limited as long as the thermoplastic resin composition (A) has a desired hydrogen desorption rate, but is preferably a polyamide, a polyester, an ethylene-vinyl alcohol copolymer resin, a polyacetal, a modified polyphenylene ether, a polyketone, or a polyphenylene sulfide. Examples of polyamides include polyamide 6, polyamide 66, polyamide 6 / 66 copolymer, polyamide 11, polyamide 12, polyamide 610, polyamide 612, polyamide 46, polyamide 410, polyamide 1010, polyamide 1012, polyamide MXD6, polyamide 6T, polyamide 9T, polyamide 10T, polyamide 11 / 10T, and the like, with polyamide 11, polyamide 12, polyamide 1010, and polyamide 6 / 66 copolymer being preferred.
[0019] The thermoplastic resin (Aa) has a flexural modulus of preferably 500 to 2000 MPa, more preferably 600 to 1800 MPa, and further preferably 700 to 1600 MPa. When the flexural modulus of the thermoplastic resin is within the above range, the hose flexibility and hose processability are excellent.
[0020] The elastomer (Ab) is not limited as long as the thermoplastic resin composition (A) has a desired hydrogen desorption rate, but is preferably a styrene-based thermoplastic elastomer, a butyl-based elastomer, or an ionomer-based thermoplastic elastomer.
[0021] Styrenic thermoplastic elastomers are block copolymers that use polystyrene as the hard segment and polydiene as the soft segment. Examples of styrenic thermoplastic elastomers include styrene-butadiene-styrene block copolymers (SBS), styrene-ethylene / butylene-styrene block copolymers (SEBS), styrene-isoprene-styrene block copolymers (SIS), styrene-ethylene / propylene block copolymers (SEP), styrene-ethylene / propylene-styrene block copolymers (SEPS), and their acid-, amine-, or epoxy-modified products. Among these, maleic anhydride-modified styrene-butadiene-styrene block copolymers (MahSBS) and maleic anhydride-modified styrene-ethylene / butylene-styrene block copolymers (MahSEBS) are preferred in terms of volume change when decompressed after exposure to high-pressure hydrogen and dispersibility in polyamide resins.
[0022] Butyl elastomers are those with a polyisobutylene structure (-[-CH2-C(CH3)2-] n - (where n is an integer of 2 or more). Examples of butyl-based elastomers include butyl rubber (IIR), halogenated butyl rubber, isobutylene-p-methylstyrene copolymer, and halogenated isobutylene-p-methylstyrene copolymer, with brominated isobutylene-p-methylstyrene copolymer being preferred.
[0023] An ionomeric thermoplastic elastomer is a network polymer in which a linear polymer with a carboxyl group (or organic acid group) introduced into the side chain is crosslinked by a metal bond via a metal ion. An example of an ionomeric thermoplastic elastomer is an ionomer in which the molecules of an ethylene-methacrylic acid copolymer are crosslinked by a metal ion.
[0024] The maximum volume V of the elastomer (Ab) when it is exposed to a hydrogen atmosphere of 90 MPa at 30°C for 24 hours or more and then depressurized to atmospheric pressure. MAXand the volume before exposure V O Ratio of V MAX / V O is preferably 5.0 or less. MAX / V O is more preferably 0.9 to 4.0, and further preferably 1.0 to 3.0. The smaller the volume expansion of the elastomer alone due to exposure to hydrogen, the more excellent the durability. "Maximum volume V when exposed to 30℃, 90MPa hydrogen atmosphere for 24 hours or more and then decompressed to atmospheric pressure MAX and the volume before exposure V O Hereinafter, this volume ratio will also be referred to as the "volume ratio before and after hydrogen exposure."
[0025] The thermoplastic resin composition (A) preferably has an island-in-a-sea structure consisting of a matrix and domains dispersed in the matrix, the matrix containing the thermoplastic resin (Aa) and the domains containing the elastomer (Ab). When the thermoplastic resin composition (A) has such a phase structure, it can achieve both hydrogen barrier properties and flexibility.
[0026] The average particle size of the domains is not limited as long as the effects of the present invention are achieved, but is preferably 2.0 μm or less, more preferably 0.05 to 1.6 μm, and even more preferably 0.1 to 1.2 μm. When the average particle size of the domains is within the above numerical range, damage due to hydrogen exposure is small, and low-temperature durability is particularly excellent.
[0027] The thickness T of the inner layer is not limited as long as the ratio T / v is within the above numerical range, but is preferably 0.4 to 2.0 mm, more preferably 0.5 to 1.8 mm, and even more preferably 0.6 to 1.5 mm.
[0028] The reinforcing layer is a layer provided between the inner layer and the outer layer, and is usually a braided layer or a spiral layer formed by braiding organic fibers or metal wires. Examples of the organic fibers include polyparaphenylene benzbisoxazole (PBO) fibers, aramid fibers, and carbon fibers, with PBO fibers being preferred. The wire diameter of the organic fibers is preferably 0.25 to 0.30 mm. Examples of the metal wires include steel wires, copper and copper alloy wires, aluminum and aluminum alloy wires, magnesium alloy wires, titanium and titanium alloy wires, with steel wires being preferred. The wire diameter of the metal wires is preferably 0.25 to 0.40 mm. The hose for transporting hydrogen of the present invention includes at least one layer made of organic fibers. The hose for transporting hydrogen of the present invention preferably includes three layers made of organic fibers and further includes one layer made of a metal wire on the outside thereof, as shown in Figure 1.
[0029] Examples of materials constituting the outer layer 4 include, but are not limited to, thermoplastic elastomers, vulcanized rubbers, and the like, and are preferably thermoplastic elastomers. Examples of thermoplastic elastomers include, but are not limited to, polyester elastomers, polyamide elastomers, and polyurethane elastomers.
[0030] The thickness of the outer layer is not limited as long as the effects of the present invention are achieved, but it is preferably 0.2 to 1.2 mm, more preferably 0.3 to 1.0 mm, and even more preferably 0.4 to 0.8 mm.
[0031] The method for producing the hydrogen transport hose is not particularly limited, but it can be produced as follows: First, the inner layer (inner tube) is extruded into a tubular shape by extrusion molding, then fibers that will become a reinforcing layer are braided on the tube, and further the outer layer (outer tube) is covered on the fibers by extrusion molding, thereby producing a hydrogen transport hose. EXAMPLES
[0032] [raw materials] The raw materials used in the following examples and comparative examples are as follows. PA11: Polyamide 11 "RILSAN" (registered trademark) BESN OTL manufactured by Arkema PA12: Polyamide 12 "UBESTA" (registered trademark) 3020U manufactured by UBE Corporation PA1010: Polyamide 1010 "VESTAMID" (registered trademark) Terra DS16 manufactured by Polypla-Evonik Co., Ltd. PA6 / 66: Polyamide 6 / 66 copolymer "UBE NYLON" (registered trademark) 5023B manufactured by UBE Corporation EVOH: Ethylene-vinyl alcohol copolymer "Soarnol" (registered trademark) E3808 manufactured by Mitsubishi Chemical Corporation MahSEBS: Maleic anhydride modified styrene-ethylene-butylene-styrene block copolymer "TUFTECH" (registered trademark) M1943 manufactured by Asahi Kasei Corporation MahEBR: Maleic anhydride modified ethylene-1-butene copolymer "Tafmer" (registered trademark) MH7010 manufactured by Mitsui Chemicals, Inc. SIBS: Kaneka Corporation styrene-isobutylene-styrene block copolymer "SIBSTAR" (registered trademark) 102T-UC BrIPMS: Brominated isobutylene-p-methylstyrene copolymer "EXXPRO" (registered trademark) 3745 manufactured by ExxonMobil Chemical Ionomer: SURLYN (registered trademark) 1855, an ionomer manufactured by Dow Mitsui Polychemicals Co., Ltd. PBO: Polyparaphenylene benzbisoxazole fiber with a diameter of 0.28 mm Steel wire: 0.35mm diameter steel wire TPC: Thermoplastic polyester elastomer "Hytrel" (registered trademark) 4057N manufactured by Toray DuPont Co., Ltd.
[0033] (1) Preparation of Thermoplastic Resin Composition The raw materials were introduced into a twin-screw kneading extruder (manufactured by Japan Steel Works, Ltd.) with the cylinder temperature set to 260°C according to the recipes shown in Tables 1 to 4, melt-kneaded for a residence time of about 5 minutes, and the molten mixture was extruded in a strand shape from a die attached to the discharge port. The resulting strand-shaped extrudate was pelletized with a resin pelletizer to obtain a pelletized thermoplastic resin composition.
[0034] (2) Measurement of hydrogen desorption rate of thermoplastic resin composition The pellet-shaped thermoplastic resin composition prepared in (1) was molded into a sheet having an average thickness of 2.0 mm using a 40 mmφ single-screw extruder with a 200 mm wide T-shaped die (manufactured by Plagiken Co., Ltd.) under the conditions of setting the cylinder and die temperatures to the melting point of the thermoplastic resin + 20°C, a cooling roll temperature of 50°C, and a take-up speed of 1 m / min. This sheet was cut into a disk shape with a diameter of 13 mm, and the cut disk-shaped sample was placed in a pressure-resistant container and exposed to hydrogen at 30°C and 90 MPa for 24 hours. Immediately after decompressing to atmospheric pressure, the disk-shaped sample was placed in a quartz tube at 30°C with argon gas flowing from one end. The other end of the quartz tube was connected to a path that was exhausted after passing through a measuring tube and a path that led to gas chromatography. The gas in the measuring tube was always connected to the exhaust path, but the path was switched once every 5 minutes to introduce the gas in the measuring tube into the gas chromatography for a specified time (about 5 seconds) to quantify the amount of hydrogen desorbed from the disk-shaped sample per time and calculate the amount of hydrogen desorbed every 5 minutes. The measurement was continued until hydrogen was no longer detected, and the total amount of hydrogen (ppm by mass) dissolved in the disk-shaped sample was calculated by integrating the amount of hydrogen desorbed every 5 minutes in each measurement. The time when the pressure was reduced was set to 0 minutes, and the hydrogen desorption rate (ppm by mass / min) was calculated from the amount of hydrogen desorbed in the 60 minutes between the time when 30 minutes had elapsed and the time when 90 minutes had elapsed after the time when the pressure was reduced.
[0035] (3) Volume ratio V of elastomer before and after hydrogen exposure MAX / V O Measurement As in (2), the disk-shaped sample was exposed to hydrogen, and immediately after depressurizing to atmospheric pressure, the area of the disk-shaped sample was measured using a Keyence Corporation TM-3000 two-dimensional multipoint dimension measuring instrument. The apparent volume was calculated as the cube of the square root of the area of the disk-shaped sample. The volume decreases as hydrogen is desorbed, and the largest apparent volume (maximum value) during this process was V MAX , the apparent volume V before exposure measured in the same way. O The volume ratio V before and after hydrogen exposure is calculated by dividing the value by MAX / V O It was decided.
[0036] (4) Measurement of the average particle size of the domain A sheet of the thermoplastic resin composition having an average thickness of 2.0 mm molded in the same manner as in (2) was cut out, and a surface perpendicular to the extrusion direction was cut with a razor. After cooling with liquid nitrogen, a smooth surface was made with a diamond knife. This surface was used as a phase image in tapping mode with an atomic force microscope AFM MFP3D manufactured by Asylum Research, and an image with contrast between the matrix and the domain was obtained. After binarizing the obtained image, particle analysis was performed on approximately 500 domains using image analysis software to determine the number average particle size, which was taken as the average particle size of the domain.
[0037] (5) Measurement of bending modulus Thermoplastic resin was molded using a Moldlock benchtop injection molding machine to prepare dumbbell-shaped test pieces of type A1 multipurpose test pieces for resins. Using these test pieces, the flexural modulus was determined at 23°C and 50% RH in accordance with JIS K7171:2016 "Determination of bending properties of plastics."
[0038] (6) Making the hose The pellet-shaped thermoplastic resin composition prepared by the procedure of (1) was extruded into a tube having an inner diameter of 8 mm and a thickness of 1 mm. This tube was used as the inner layer, and on the outside of the inner layer, three braided layers of PBO fiber were braided as a reinforcing layer, and further on the outside, one braided layer of steel wire was braided (Examples 1 to 8 and 10 to 18 and Comparative Examples 1, 3 and 4), or four braided layers of PBO fiber were braided as a reinforcing layer (Example 9), or four braided layers of steel wire were braided as a reinforcing layer (Comparative Examples 2 and 5). Furthermore, a thermoplastic polyester elastomer (Hytrel (registered trademark) 4057N manufactured by Toray DuPont Co., Ltd.) was extruded to a thickness of 0.7 mm on the outside of the reinforcing layer to form an outer layer, to prepare a hose.
[0039] (7) Measurement of hose bending rigidity The hose prepared in (6) was cut to a predetermined length, and the bending stiffness was measured at room temperature at a bending radius of 180 mm in accordance with JIS K6330-9 "Rubber and plastic hose test methods - Part 9 Bending properties of hoses and pipes." The bending stiffness is an index of the handleability of a hose, and if the bending stiffness is 5 to 20 N, the hose has excellent handleability.
[0040] (8) Ratio of the number of times to fatigue failure at a constant strain for the inner layer material with / without hydrogen exposure R As in (2), the take-up speed in the extrusion molding was appropriately changed to produce sheets with inner layer thicknesses corresponding to those shown in Tables 1 to 4. 24 strips with a width of 5 mm and a length of 200 mm were cut from the sheet, 12 of which were left as they were, while the remaining 12 were exposed to hydrogen at 30°C and 90 MPa for 24 hours. They were then placed in a constant strain, constant load fatigue testing machine manufactured by Ueshima Seisakusho Co., Ltd. and subjected to repeated elongation deformation under conditions of a temperature of -35°C, a strain of 13.5%, and a speed of 100 rpm. The number of times that 7 or more of the 12 strips were subjected to break was calculated, and the ratio of the number of breaks between those exposed to hydrogen and those not exposed to hydrogen, R, was calculated. R = number of fractures of sample after hydrogen exposure / number of fractures of untreated sample The closer R is to 1, the less damage caused by hydrogen exposure and the longer the hose lifespan is expected to be. R of 0.90 or more was rated as "excellent," R of 0.80 or more but less than 0.90 was rated as "good," R of 0.70 or more but less than 0.80 was rated as "passable," and R of less than 0.70 was rated as "unacceptable." Materials rated as "unacceptable" showed a significant decrease in physical properties due to hydrogen exposure and were deemed unsuitable for practical use as the inner layer of a hose.
[0041] [Table 1]
[0042] [Table 2]
[0043] [Table 3]
[0044] [Table 4]
[0045] The present disclosure includes the following inventions. Invention [1] A hose for transporting hydrogen comprising an inner layer, a reinforcing layer and an outer layer, wherein the inner layer comprises a thermoplastic resin composition (A) comprising a thermoplastic resin (Aa) and an elastomer (Ab), and the reinforcing layer comprises at least one layer made of organic fibers, and wherein when the thermoplastic resin composition (A) is held in a hydrogen atmosphere of 30°C and 90 MPa for 24 hours or more and then reduced to atmospheric pressure, the hydrogen desorption rate v for 30 to 90 minutes after reduction in pressure is 3.7 to 7.1 ppm by mass / min. Invention [2] A hose for transporting hydrogen according to invention [1], characterized in that the ratio T / v of the inner layer thickness T [mm] to the hydrogen desorption rate v [mass ppm / min] is 0.16 to 0.30. Invention [3] The maximum volume V of the elastomer (Ab) when it is exposed to a hydrogen atmosphere of 30°C and 90 MPa for 24 hours or more and then reduced to atmospheric pressure. MAX and the volume before exposure V O Ratio of V MAX / V O The hose for transporting hydrogen according to the invention [1] or [2], characterized in that Invention [4] A hose for transporting hydrogen according to any one of inventions [1] to [3], characterized in that the thermoplastic resin (Aa) has a flexural modulus of 500 to 2000 MPa. Invention [5] A hose for transporting hydrogen according to any one of inventions [1] to [4], characterized in that the thermoplastic resin composition (A) has a sea-island structure consisting of a matrix and domains dispersed in the matrix, the matrix contains a thermoplastic resin (Aa), and the domains contain an elastomer (Ab). Invention [6] A hose for transporting hydrogen according to invention [5], characterized in that the average particle size of the domains is 2.0 μm or less. [Industrial Applicability]
[0046] The hydrogen transport hose of the present invention can be suitably used as a hose for transporting hydrogen gas from a dispenser installed at a hydrogen station to a fuel cell vehicle or the like. [Explanation of symbols]
[0047] 1. Hydrogen transport hose 2. Inner layer 3 Reinforcement layer 4 Outer layer 5 Layer made of organic fibers 6 Layers made of metal wires
Claims
1. A hose for transporting hydrogen comprising an inner layer, a reinforcing layer and an outer layer, wherein the inner layer comprises a thermoplastic resin composition (A) comprising a thermoplastic resin (Aa) and an elastomer (Ab), and the reinforcing layer comprises at least one layer made of organic fibers, and wherein when the thermoplastic resin composition (A) is held in a hydrogen atmosphere of 30°C and 90 MPa for 24 hours or more and then reduced to atmospheric pressure, the hose for transporting hydrogen has a hydrogen desorption rate v of 3.7 to 7.1 mass ppm / min at 30 to 90 minutes after reduction in pressure.
2. 2. The hydrogen transport hose according to claim 1, wherein the ratio T / v of the thickness T [mm] of the inner layer to the hydrogen desorption rate v [mass ppm / min] is 0.16 to 0.
30.
3. The maximum volume V of the elastomer (Ab) when it is exposed to a hydrogen atmosphere of 90 MPa at 30° C. for 24 hours or more and then reduced to atmospheric pressure. MAX and the volume before exposure V O Ratio of V MAX / V O 2. The hose for transporting hydrogen according to claim 1, wherein the tensile strength is 5.0 or less.
4. 2. The hose for transporting hydrogen according to claim 1, characterized in that the thermoplastic resin (Aa) has a flexural modulus of elasticity of 500 to 2000 MPa.
5. 2. The hose for transporting hydrogen according to claim 1, characterized in that the thermoplastic resin composition (A) has a sea-island structure consisting of a matrix and domains dispersed in the matrix, the matrix contains a thermoplastic resin (Aa), and the domains contain an elastomer (Ab).
6. 6. The hose for transporting hydrogen according to claim 5, wherein the domains have an average particle size of 2.0 μm or less.
Citation Information
Patent Citations
Hydrogen transport component
WO2018155491A1