Battery and manufacturing method of battery
By designing the battery with an inclined end surface and a specific angle relationship for the insulating layer, the battery addresses insulating layer peeling, improving durability and preventing short circuits.
Patent Information
- Application Number
- JP2023056111
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-11
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional batteries face issues with insulating layers peeling off from the end face, leading to potential short circuits.
The battery design features an electrode body with an inclined end surface and an insulating layer applied in an arc shape, where the angles formed by tangents at the obtuse and acute ends of the insulating layer satisfy a specific relationship (θ1<θ2), increasing adhesive strength and reducing peeling.
This design effectively suppresses insulating layer peeling, enhancing durability and preventing short circuits by increasing the contact area and adhesive strength of the insulating layer.
Smart Images

Figure 2024143433000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to batteries and methods for manufacturing batteries. [Background technology]
[0002] Conventionally, batteries having an electrode assembly in which a positive electrode layer, an electrolyte layer, and a negative electrode layer are laminated in this order have been used. In such batteries, insulating layers are formed on end faces of the electrode assembly to prevent short circuits.
[0003] For example, Patent Document 1 describes a method for producing a laminated all-solid-state battery, which includes preparing a first laminate in which a solid electrolyte layer, a first active material layer, a first current collector layer having a first current collector tab extending to a side of the laminated all-solid-state battery, a first active material layer, and a solid electrolyte layer are laminated in this order; applying an insulator coating liquid to an end of the first laminate to form an insulating portion; and laminating the first laminate in which the insulating portion has been formed, a second active material layer, and a second current collector layer having a second current collector tab extending to a side of the laminated all-solid-state battery to prepare a battery structure having a plurality of second laminates in which a second current collector layer having a second current collector tab, a second active material layer, a solid electrolyte layer, a first active material layer, a first current collector layer having a first current collector tab, a first active material layer, a solid electrolyte layer, and a second active material layer are laminated in this order. and joining a plurality of second current collecting tabs respectively extending from a plurality of second current collectors in the battery structure, wherein an end portion forming the insulating portion of the first laminate is located at a position corresponding to the second current collecting tab when viewed from the stacking direction in the all-solid-state battery, and the insulator coating liquid is applied by immersing the end portion forming the insulating portion of the first laminate in the portion of the insulator coating liquid with the use of a coating device having two plate-like members arranged closely opposite each other in a container body containing the insulator coating liquid, the coating device being configured so that a liquid level of the insulator coating liquid in a portion sandwiched between the two plate-like members becomes higher than a liquid level of the insulator coating liquid in other portions of the container body by capillary action.
[0004] Patent Document 2 discloses an electrode for a lithium ion secondary battery comprising: a current collector; and an electrode active material layer provided on the current collector and containing an electrode active material and a binder, wherein at least a part of the edge of the electrode active material layer is constituted by an inclined portion whose thickness decreases with increasing distance from the center of the electrode active material layer, wherein an edge factor expressed by the ratio (W / T) of the width (W) of the inclined portion to the thickness (T) of the electrode active material layer is 3 or more, and the width (W) of the inclined portion is less than 1000 μm, and further comprising an insulating resin layer provided on the current collector, wherein the insulating resin layer is disposed so as to be adjacent to the inclined portion of the electrode active material layer and to cover the inclined portion. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent No. 6729236 [Patent Document 2] International Publication No. 2020 / 067379 Summary of the Invention [Problem to be solved by the invention]
[0006] In order to prevent the occurrence of short circuits in batteries, insulating layers have been formed on the end faces of electrode bodies in the past. However, the insulating layers are prone to peeling off from the end faces, which can result in short circuits in the batteries.
[0007] The present disclosure has been made in consideration of the above-mentioned circumstances, and aims to provide a battery in which peeling of an insulating layer from an end face of an electrode body is suppressed, and a method for manufacturing such a battery. [Means for solving the problem]
[0008] <1> A battery having an electrode assembly in which at least a positive electrode layer, an electrolyte layer, and a negative electrode layer are laminated in this order, At least one end surface of the electrode body is an inclined surface having an inclination with respect to the stacking direction, an insulating layer formed in an arc shape in contact with the inclined surface and covering at least a portion of the inclined surface; In the inclination direction of the inclined surface, when the side where the inclined surface forms an obtuse angle with the electrode body is defined as the obtuse angle side, and the side where the inclined surface forms an acute angle with the electrode body is defined as the acute angle side, a battery in which an angle θ1 formed by a tangent passing through the end portion of the insulating layer on the obtuse angle side and the inclined surface and an angle θ2 formed by a tangent passing through the end portion of the insulating layer on the acute angle side and the inclined surface satisfy the relationship θ1<θ2. <2> an angle θ1 between a tangent line passing through the end portion on the obtuse angle side of the insulating layer and the inclined surface is 20° or more and 40° or less; the angle θ2 between the tangent line passing through the end portion on the acute angle side of the insulating layer and the inclined surface is 50° or more and 70° or less; <1> 2. The battery according to claim 1 . <3> The angle θ3 on the side where the inclined surface forms an obtuse angle with the electrode body is 100° or more and 130° or less, The angle θ4 on the side where the inclined surface forms an acute angle with the electrode body is 50° or more and 80° or less. <1> or <2> 2. The battery according to claim 1 . <4> a preparation step of preparing an electrode assembly in which at least a positive electrode layer, an electrolyte layer, and a negative electrode layer are laminated in this order; a cutting step of cutting at least one end surface of the electrode body so as to form an inclined surface having an inclination with respect to the stacking direction; and forming an insulating layer on the surface of the inclined surface to cover at least a portion of the inclined surface and have an arc-shaped insulating layer, and curing the insulating material to form an insulating layer, In the inclination direction of the inclined surface, when the side where the inclined surface forms an obtuse angle with the electrode body is defined as the obtuse angle side, and the side where the inclined surface forms an acute angle with the electrode body is defined as the acute angle side, the insulating layer forming process is a process of applying an insulating material such that an angle θ1 formed by a tangent passing through the end portion of the insulating layer on the obtuse angle side and the inclined surface and an angle θ2 formed by a tangent passing through the end portion of the insulating layer on the acute angle side and the inclined surface satisfy the relationship θ1<θ2. Effect of the Invention
[0009] According to the present disclosure, it is possible to provide a battery in which peeling of an insulating layer from an end face of an electrode assembly is suppressed, and a method for manufacturing the battery. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a schematic cross-sectional view illustrating an example of a battery according to an embodiment of the present disclosure. [Diagram 2] FIG. 1 is a schematic cross-sectional view showing an example of a conventional battery. [Diagram 3] FIG. 2 is a schematic cross-sectional view showing another example of a battery according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The battery and the method for manufacturing the battery according to the present disclosure will be described in detail below with reference to the drawings. The drawings shown below are schematic, and the size and shape of each part are appropriately exaggerated for ease of understanding.
[0012] <Battery> The battery according to the embodiment of the present disclosure has an electrode assembly in which at least a positive electrode layer, an electrolyte layer, and a negative electrode layer are laminated in this order. The battery may further have a positive electrode foil on the side of the positive electrode layer opposite the electrolyte layer, and may also have a negative electrode foil on the side of the negative electrode layer opposite the electrolyte layer. At least one end face of the electrode body is an inclined surface having an inclination with respect to the stacking direction (the direction in which the positive electrode layer, the electrolyte layer, and the negative electrode layer are stacked). The battery has an insulating layer formed in an arc shape so as to contact the inclined surface and cover at least a portion of the inclined surface. In the inclination direction of the inclined surface, if the side of the inclined surface that forms an obtuse angle with the electrode body is defined as the obtuse angle side, and the side of the inclined surface that forms an acute angle with the electrode body is defined as the acute angle side, the angle θ1 made by a tangent passing through the end of the insulating layer on the obtuse angle side and the inclined surface, and the angle θ2 made by a tangent passing through the end of the insulating layer on the acute angle side and the inclined surface satisfy the relationship θ1<θ2.
[0013] Here, an example of a battery according to an embodiment of the present disclosure will be described with reference to FIG. The battery shown in FIG. 1 has an electrode body 100, in which a positive electrode layer 8, an electrolyte layer 6, and a negative electrode layer 4 are laminated in this order. The electrode body 100 further has a positive electrode foil 10 on the side of the positive electrode layer 8 opposite the electrolyte layer 6, and has a negative electrode foil 2 on the side of the negative electrode layer 4 opposite the electrolyte layer 6. On both sides of the negative electrode foil 2, a negative electrode layer 4, an electrolyte layer 6, a positive electrode layer 8, and a positive electrode foil 10 are laminated in this order from the negative electrode foil 2 side. In other words, the battery shown in FIG. 1 is a battery in which two pairs of the negative electrode layer 4, the electrolyte layer 6, the positive electrode layer 8, and the positive electrode foil 10 are arranged in pairs, one on each side of the negative electrode foil 2.
[0014] However, the electrode assembly in the battery according to the embodiment of the present disclosure is not limited to this form, and may be any electrode assembly in which a positive electrode layer, an electrolyte layer, and a negative electrode layer are laminated in this order.
[0015] An end surface of the electrode body 100 is an inclined surface 102. This inclined surface 102 is inclined with respect to the stacking direction (the vertical direction in FIG. 1) and extends in a direction having an angle of more than 0° with respect to the stacking direction. One end side of the inclined surface 102 in the inclination direction (the direction in which the inclined surface 102 has an angle of more than 0° with respect to the stacking direction) forms an obtuse angle with the electrode body 100, and the angle of this obtuse angle is θ3. The other end side of the inclined surface 102 in the inclination direction forms an acute angle with the electrode body 100, and the angle of this acute angle is θ4. The side of the inclined surface 102 that forms an obtuse angle with the electrode body 100 is referred to as the "obtuse angle side", and the side that forms an acute angle with the electrode body 100 is referred to as the "acute angle side".
[0016] The electrode body 100 has an insulating layer 14 arranged to be in contact with the inclined surface 102. The insulating layer 14 covers at least a part of the inclined surface 102. The electrode body 100 shown in FIG. 1 is arranged to cover the negative electrode foil 2, and a part of the negative electrode layer 4, the electrolyte layer 6, and the positive electrode layer 8 formed on both sides of the negative electrode foil 2. The insulating layer 14 is formed to rise from the inclined surface 102 and has an arc shape. However, the shape of the insulating layer 14 is not a perfect arc shape, but an irregular arc shape in which the angle on the obtuse side of the inclined surface 102 is small, while the angle on the acute side is large. In other words, when the angle formed by the tangent passing through the end of the insulating layer 14 on the obtuse angle side and the inclined surface 102 is θ1, and the angle formed by the tangent passing through the end of the insulating layer 14 on the acute angle side and the inclined surface 102 is θ2, the relationship of "θ1<θ2" is satisfied.
[0017] According to the battery according to the embodiment of the present disclosure, peeling of the insulating layer from the end faces can be suppressed, and as a result, short circuits caused by peeling of the insulating layer can be effectively suppressed. This effect is due to the following findings.
[0018] First, a conventional battery will be described with reference to FIG. The conventional battery shown in FIG. 2 has an electrode body 200. The electrode body 200 has a configuration in which an anode foil 22 is laminated on both sides of the anode foil 22, in that order from the anode foil 22 side, an anode layer 24, an electrolyte layer 26, a cathode layer 28, and a cathode foil 30. End face 202 of electrode body 200 is not inclined with respect to the stacking direction (the vertical direction in FIG. 2), and is a surface that extends parallel to the stacking direction. Therefore, angle θ3 that one end side of end face 202 makes with electrode body 200 and angle θ4 that the other end side makes with electrode body 200 are both the same angle, 90°. The electrode body 200 has an insulating layer 34 arranged in contact with the end face 202 and so as to cover at least a part of the end face 202. At one end side and the other end side in the stacking direction of the insulating layer 34, the angles θ1 and θ2 formed by the tangent lines passing through the ends and the end face 202 satisfy the relationship θ1=θ2.
[0019] In the electrode body 200 of a conventional battery, the insulating layer 34 is also formed in contact with the end face 202 as described above in order to suppress the occurrence of a short circuit. However, the insulating layer 34 is prone to peeling from the end face 202, which can result in a short circuit.
[0020] In contrast, the battery according to the embodiment of the present disclosure has an inclined surface on the end surface, and the insulating layer arranged to contact this inclined surface satisfies the relationship θ1<θ2 between the angle θ1 on the obtuse angle side and the angle θ2 on the acute angle side. Since the end surface is an inclined surface, the contact area with the insulating layer can be increased, and the adhesive strength of the insulating layer can be increased. In addition, since the angle θ1 on the obtuse angle side and the angle θ2 on the acute angle side satisfy the relationship θ1<θ2, the material on the obtuse angle side, which is more likely to be subjected to stress, becomes thinner, and even if stress is applied, the resin easily follows the electrode body and is less likely to peel off, so that the adhesive strength of the insulating layer can be increased. As a result, in the battery according to the embodiment of the present disclosure, peeling from the end surface of the insulating layer can be suppressed.
[0021] In addition, since the end faces are inclined, the coating accuracy of the insulating material for forming the insulating layer can be reduced. Furthermore, since the end faces are inclined, the stress caused by the current collector (for example, the current collector foil 12 shown in FIG. 3 described later) is less likely to be received, and durability can be improved.
[0022] (Angles θ1 and θ2 between the insulating layer and the inclined surface) In the battery according to the embodiment of the present disclosure, in the electrode body, the angle θ1 formed by the tangent line passing through the obtuse-angle end of the insulating layer and the inclined surface and the angle θ2 formed by the tangent line passing through the acute-angle end of the insulating layer and the inclined surface satisfy the relationship of "θ1<θ2". This can increase the adhesive strength of the insulating layer and suppress peeling from the end surface of the insulating layer.
[0023] In addition, the angle θ1 formed by the tangent passing through the obtuse-angle end of the insulating layer and the inclined surface is preferably 20° or more and 40° or less, and more preferably 25° or more and 35° or less, in order to further suppress peeling of the insulating layer from the end face. In addition, the angle θ2 formed by the tangent passing through the acute-angle end of the insulating layer and the inclined surface is preferably 50° or more and 70° or less, and more preferably 55° or more and 65° or less, in order to further suppress peeling of the insulating layer from the end face.
[0024] (Angles θ3 and θ4 between the inclined surface and the electrode body) The angle θ3 on the side where the inclined surface forms an obtuse angle with the electrode body is preferably 100° or more and 130° or less, and more preferably 105° or more and 120° or less, from the viewpoint of increasing the contact area between the inclined surface and the insulating layer and further suppressing peeling of the insulating layer from the end face. For the same reason, the angle θ4 on the side where the inclined surface forms an acute angle with the electrode body is preferably 50° or more and 80° or less, and more preferably 60° or more and 75° or less.
[0025] (insulation layer thickness t) The thickness t of the insulating layer, i.e., the distance perpendicular to the inclined surface from the apex of the insulating layer, is preferably 0.05 mm or more and 1.0 mm or less, and more preferably 0.1 mm or more and 0.5 mm or less, in order to ensure the insulation provided by the insulating layer while further suppressing peeling from the end face of the insulating layer.
[0026] (Other forms) The battery according to the embodiment of the present disclosure may be a stacked battery (i.e., a stack of a plurality of unit electrodes) in which a plurality of electrode assemblies 100, for example, as shown in Fig. 1, are stacked. Here, a stacked battery will be described with reference to Fig. 3, giving a specific example.
[0027] The battery 300 shown in FIG. 3 has a configuration in which three electrode bodies, a first electrode body 100A, a second electrode body 100B, and a third electrode body 100C, each having the same configuration as the electrode body 100 shown in FIG. 1, are stacked. Between the first electrode body 100A and the second electrode body 100B, and between the second electrode body 100B and the third electrode body 100C, current collector foils 12 are arranged so as to be interposed between the positive electrode foils of each electrode body. In addition, a current collector foil 12 is also arranged on the opposite side of the first electrode body 100A from the second electrode body 100B so as to be in contact with the positive electrode foil. Each current collector foil 12 extends beyond the end face (inclined face) of each electrode body and is collected in one place, and serves as a terminal for taking out the current generated from each electrode body to the outside. The stacked type battery shown in FIG. 3 may be further housed in an exterior body such as a laminate or a can.
[0028] Although an example of the battery according to the embodiment of the present disclosure has been illustrated and described in each of FIGS. 1 and 3, the battery according to the embodiment of the present disclosure is not limited to these aspects, and various modifications are possible as long as the effects of the present disclosure are achieved.
[0029] <Battery manufacturing method> Next, a method for manufacturing a battery according to an embodiment of the present disclosure will be described.
[0030] A method for manufacturing a battery according to an embodiment of the present disclosure includes the following steps. (1) A preparation step of preparing an electrode assembly having at least a positive electrode layer, an electrolyte layer, and a negative electrode layer laminated in this order. (2) A cutting step of cutting at least one end surface of the electrode body so as to form an inclined surface having an inclination with respect to the lamination direction. (3) an insulating layer forming step of applying an insulating material to the surface of the inclined surface so as to cover at least a portion of the inclined surface and have an arc-shaped shape, and then hardening the material to form an insulating layer; In the inclination direction of the inclined surface, the side of the inclined surface that forms an obtuse angle with the electrode body is defined as the obtuse angle side, and the side of the inclined surface that forms an acute angle with the electrode body is defined as the acute angle side. (3) The insulating layer formation process is a process of applying an insulating material so that the angle θ1 made by a tangent passing through the end of the insulating layer on the obtuse angle side and the inclined surface and the angle θ2 made by a tangent passing through the end of the insulating layer on the acute angle side and the inclined surface satisfy the relationship θ1<θ2.
[0031] (1) Preparation process In the preparation step, an electrode body is prepared in which at least a positive electrode layer, an electrolyte layer, and a negative electrode layer are laminated in this order. Furthermore, the electrode body may have a positive electrode foil on the side of the positive electrode layer opposite the electrolyte layer, and may have a negative electrode foil on the side of the negative electrode layer opposite the electrolyte layer. Details of the configuration of the electrode body are as described above in the section on <Battery> and will not be repeated here.
[0032] (2) Cutting process In the cutting step, at least one end surface of the electrode body is cut so as to form an inclined surface that is inclined with respect to the stacking direction.
[0033] The cutting angle is not particularly limited, but it is preferable to cut at an angle such that, for example, the angle θ3 on the side where the inclined surface forms an obtuse angle with the electrode body, and the angle θ4 on the side where the inclined surface forms an acute angle with the electrode body, are in the aforementioned range.
[0034] The cutting method can be a known method, for example, a method using a rotary blade cutter (a method in which a rotary blade is placed on the end of the electrode body and cut while moving the rotary blade in the longitudinal direction of the electrode body), a method in which the electrode is sheared while being tilted, etc. can be mentioned.
[0035] (3) Insulation layer formation process In the insulating layer forming step, an insulating material is applied to the surface of the inclined plane so as to cover at least a portion of the inclined plane and have an arcuate shape, and is then cured to form an insulating layer.
[0036] The insulating material can be applied to the surface of the inclined plane by a known method, such as a nozzle application method (a method in which the insulating material is applied by discharging the insulating material from the nozzle while moving the nozzle in the longitudinal direction of the electrode body) or a dip application method.
[0037] In order to adjust the shape of the inclined surface so as to cover at least a part of the inclined surface and to have an arc-like shape, for example, a method of adjusting the inclination angle of the inclined surface, a method of selecting an insulating material application method and adjusting application conditions, etc. In the case of the above-mentioned nozzle application method, for example, the application conditions include adjustment of the amount of the insulating material discharged from the nozzle, the discharge speed, the moving speed of the nozzle, the distance between the nozzle and the inclined surface, the viscosity of the insulating material to be applied, etc.
[0038] In the insulating layer forming process, the coating is performed so that the angle θ1 formed by the tangent line passing through the obtuse-angle end of the insulating layer and the inclined surface and the angle θ2 formed by the tangent line passing through the acute-angle end of the insulating layer and the inclined surface satisfy the relationship θ1<θ2. In order to adjust the relationship of θ1<θ2, for example, a method of adjusting the inclination angle of the inclined surface, a method of adjusting the viscosity of the applied insulating material, a method of adjusting the time until the applied insulating material hardens, etc. For example, by adjusting the viscosity of the insulating material and the time until hardening so that the applied insulating material hangs down in the direction of gravity due to gravity and then hardens, a shape that satisfies the relationship of θ1<θ2 can be obtained.
[0039] The method for curing the applied insulating material is selected depending on the insulating material used.
[0040] By the above method, a battery according to an embodiment of the present disclosure can be manufactured.
[0041] Examples of insulating materials used to form the insulating layer include copolymers such as styrene-ethylene-butylene-styrene block copolymer (SEBS), styrene-ethylene-propylene-styrene block copolymer (SEPS), styrene-ethylene-ethylene-propylene-styrene block copolymer (SEEPS), styrene-butadiene-styrene block copolymer (SBS), and styrene-isoprene-styrene block copolymer (SIS); elastomers such as styrene butadiene rubber (SBR), butadiene rubber (BR), and nitrile rubber (NBR); and polyvinylidene fluoride (PVdF). Fluorine-containing resins such as polyvinylidene fluoride-hexafluoropropylene copolymer (PVdF-HFP) and polytetrafluoroethylene (PTFE); acrylic resins such as polymethyl acrylate (PMA) and polymethyl methacrylate resin (PMMA); polyvinyl acetate, polyimide (PI), polyamide (PA), polyvinyl chloride (PVC), polyether nitrile (PEN), polyethylene (PE), polypropylene (PP), polyacrylonitrile (PAN), poly(meth)acrylic acid, carboxymethyl cellulose (CMC), hydroxyethyl cellulose, and polyvinyl alcohol. These insulating materials may be used alone or in combination of two or more.
[0042] The insulating material may further contain additives, the type and content of which are not particularly limited. For example, insulating particles may be blended, and examples of the insulating particles include inorganic particles and organic particles.
[0043] (Steel components of batteries / positive electrode layer, negative electrode layer, electrolyte layer The positive electrode layer contains at least a positive electrode active material and may further contain at least one of a conductive material, an electrolyte, and a binder.
[0044] The negative electrode layer contains at least a negative electrode active material and may further contain at least one of a conductive material, an electrolyte, and a binder.
[0045] The electrolyte layer is disposed between the positive electrode layer and the negative electrode layer. The electrolyte layer preferably contains a solid electrolyte. The solid electrolyte preferably contains at least one solid electrolyte species selected from the group of solid electrolytes consisting of sulfide solid electrolytes, oxide solid electrolytes, and halide solid electrolytes.
[0046] The present disclosure is not limited to the above-described embodiments. The above-described embodiments are merely examples, and anything that has substantially the same configuration as the technical idea described in the claims of the present disclosure and exhibits similar effects is included in the technical scope of the present disclosure. EXAMPLES
[0047] Here, the effects of the solid-state battery according to the present disclosure were confirmed by experiments.
[0048] Comparative Example 1 First, a negative electrode foil was prepared, and an electrode body having a configuration in which a negative electrode layer, an electrolyte layer, a positive electrode layer, and a positive electrode foil were laminated on both sides of the negative electrode foil in this order from the negative electrode foil side was prepared (preparation step). Next, one end surface of the electrode body was cut so that the end surface of the electrode body did not have an inclination with respect to the stacking direction, that is, the end surface was cut so as to have a surface extending parallel to the stacking direction (the aspect shown in FIG. 2) (cutting step). Next, an insulating material was applied to the surface of the end face and cured to form an insulating layer (insulating layer forming step). In this manner, an electrode body was obtained.
[0049] For the electrode body obtained in Comparative Example 1, Table 1 shows angles θ1 and θ2 between the tangents passing through both ends of the insulating layer and the end faces, and angles θ3 and θ4 between the end faces and the electrode body.
[0050] Comparative Example 2 In Comparative Example 1, the cutting of the end faces in the cutting step was performed so as to have a surface inclined with respect to the lamination direction, that is, extending in a direction having an angle of more than 0° with respect to the lamination direction (the embodiment shown in FIG. 1). Thereafter, an electrode body was obtained in the same manner as in Comparative Example 1, except that the viscosity of the insulating material and the curing time were adjusted so that the shape of the insulating layer after curing was adjusted to a desired shape.
[0051] For the electrode body obtained in Comparative Example 2, Table 1 shows the angle θ1 between the tangent line passing through the obtuse-angle end of the insulating layer and the inclined surface, the angle θ2 between the tangent line passing through the acute-angle end of the insulating layer and the inclined surface, the angle θ3 on the side where the inclined surface forms an obtuse angle with the electrode body, and the angle θ4 on the side where the inclined surface forms an acute angle with the electrode body.
[0052] Example 1 In Comparative Example 1, the cutting of the end faces in the cutting step was performed so as to have a surface inclined with respect to the lamination direction, that is, extending in a direction having an angle of more than 0° with respect to the lamination direction (the embodiment shown in FIG. 1). Thereafter, an electrode body was obtained in the same manner as in Comparative Example 1, except that the viscosity of the insulating material and the curing time were adjusted so that the shape of the insulating layer after curing was adjusted to a desired shape.
[0053] For the electrode body obtained in Example 1, Table 1 shows the angle θ1 between the tangent line passing through the obtuse-angle end of the insulating layer and the inclined surface, the angle θ2 between the tangent line passing through the acute-angle end of the insulating layer and the inclined surface, the angle θ3 on the side where the inclined surface forms an obtuse angle with the electrode body, and the angle θ4 on the side where the inclined surface forms an acute angle with the electrode body.
[0054] Table 1 also shows the thickness t of the insulating layer of the obtained electrode body (the distance from the end face (inclined face) to the apex of the insulating layer in the direction perpendicular to the end face (inclined face)).
[0055] -Thermal shock test (durability)- Four electrode assemblies obtained in Comparative Examples 1 and 2 and Example 1 were stacked, and metal foil was placed on the top and bottom surfaces of each electrode assembly to prepare an evaluation test cell. This evaluation test cell was subjected to a thermal shock test for 100 hours, in which one cycle consisted of heating the cell from room temperature to 80° C., then cooling it to −20° C., and then returning it to room temperature. A total of 2,000 cycles of the test were then performed. Evaluation criteria A: No peeling of the insulating layer B: Some insulation layers (2 or less) peeled off C: Many insulation layers (more than two) peeled off
[0056] [Table 1]
[0057] As shown in Table 1, in the electrode body of Example 1, in which the end face of the electrode body is an inclined surface and the angle θ1 formed by the tangent passing through the obtuse-angle end of the insulating layer and the inclined surface and the angle θ2 formed by the tangent passing through the acute-angle end of the insulating layer and the inclined surface satisfy the relationship "θ1 < θ2", peeling of the insulating layer from the end face of the electrode body is suppressed compared to the electrode body of Comparative Example 1 in which the end face is not an inclined surface and the electrode body of Comparative Example 2 which does not satisfy the relationship "θ1 < θ2". [Explanation of symbols]
[0058] 2, 22 negative electrode foil, 4, 24 negative electrode layer, 6, 26 electrolyte layer, 8, 28 positive electrode layer, 10, 30 positive electrode foil, 12 current collector foil, 14, 34 insulating layer, 100, 100A, 100B, 100C electrode body, 102 inclined surface, 202 end surface
Claims
1. A battery having an electrode assembly in which at least a positive electrode layer, an electrolyte layer, and a negative electrode layer are laminated in this order, At least one end surface of the electrode body is an inclined surface having an inclination with respect to the stacking direction, an insulating layer formed in an arc shape in contact with the inclined surface and covering at least a portion of the inclined surface; In the inclination direction of the inclined surface, when the side where the inclined surface forms an obtuse angle with the electrode body is defined as the obtuse angle side, and the side where the inclined surface forms an acute angle with the electrode body is defined as the acute angle side, a battery, wherein an angle θ1 formed by a tangent passing through the end portion of the insulating layer on the obtuse angle side and the inclined surface, and an angle θ2 formed by a tangent passing through the end portion of the insulating layer on the acute angle side and the inclined surface satisfy the relationship θ1 < θ2.
2. an angle θ1 between a tangent line passing through the end portion on the obtuse angle side of the insulating layer and the inclined surface is equal to or greater than 20° and equal to or less than 40°; The battery according to claim 1 , wherein an angle θ2 between a tangent line passing through the acute-angle end of the insulating layer and the inclined surface is equal to or greater than 50° and equal to or less than 70°.
3. An angle θ3 on the side where the inclined surface forms an obtuse angle with the electrode body is 100° or more and 130° or less, The battery according to claim 1 , wherein an angle θ4 on the side where the inclined surface forms an acute angle with the electrode body is equal to or greater than 50° and equal to or less than 80°.
4. a preparation step of preparing an electrode assembly in which at least a positive electrode layer, an electrolyte layer, and a negative electrode layer are laminated in this order; a cutting step of cutting at least one end surface of the electrode body so as to form an inclined surface having an inclination with respect to the stacking direction; and forming an insulating layer on the surface of the inclined surface to cover at least a portion of the inclined surface and have an arc-shaped insulating material, and hardening the insulating material to form an insulating layer, In the inclination direction of the inclined surface, when the side where the inclined surface forms an obtuse angle with the electrode body is defined as the obtuse angle side, and the side where the inclined surface forms an acute angle with the electrode body is defined as the acute angle side, the insulating layer forming process is a process of applying an insulating material so that an angle θ1 formed by a tangent passing through the end portion of the insulating layer on the obtuse angle side and the inclined surface and an angle θ2 formed by a tangent passing through the end portion of the insulating layer on the acute angle side and the inclined surface satisfy the relationship θ1 < θ2.
Citation Information
Patent Citations
Manufacturing method for stacked all-solid-state battery
JP6729236B2
Electrode for lithium ion secondary batteries, and lithium ion secondary battery
WO2020067379A1
Cited By
End coating material and all-solid-state battery
CN122772498A
Battery cell, method for coating battery cell, and method for assembling battery cell
CN122843450A
End coating material, all-solid-state battery
JP2026154333A
Battery cell, method for coating a battery cell, and method for assembling a battery cell
JP2026160560A