Mold and method of reclaiming mold

A mold made of unfired ceramics, bonded at low temperatures, addresses the environmental burden of high-temperature reuse methods by enabling energy-efficient reuse.

JP2024143503AInactive Publication Date: 2024-10-11ADVICS CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023056224
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing mold reuse methods involve high-temperature heat treatment, which is environmentally burdensome.

Method used

A mold formed from unfired ceramics made of a mixture of ceramic particles and an alkaline component, bonded using mechanochemical treatment and an alkaline solution at low temperatures.

Benefits of technology

Reduces environmental load by eliminating the need for high-temperature heating during mold reuse, thereby conserving energy and minimizing environmental impact.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143503000001_ABST
    Figure 2024143503000001_ABST
Patent Text Reader

Abstract

To reduce the burden on environment by reclaiming a mold.SOLUTION: A mold is formed of sinter-free ceramic (10) consisting of a mixture of ceramic particles and an alkali component.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to molds and methods for reusing molds. [Background technology]

[0002] Patent Document 1 discloses a method for reusing core sand using water glass as a binder. This method includes a heating step for heating the core at a temperature between 300°C and 550°C. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2018-15813 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, from the viewpoint of reducing the burden on the environment, a method for reusing molds that does not involve heat treatment at such high temperatures is desired. [Means for solving the problem]

[0005] In order to solve the above problems, a mold according to one embodiment of the present disclosure is characterized in that it is formed from a non-fired ceramic that is a mixture of ceramic particles and an alkali component. Effect of the Invention

[0006] According to the present disclosure, it is possible to reduce the burden on the environment when reusing molds. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a schematic diagram of a mold according to an embodiment of the present disclosure. [Diagram 2]1A is a schematic diagram of a non-fired ceramic used in a mold according to an embodiment of the present disclosure, and FIG. 1B is a diagram used to explain bonding of multiple ceramic particles. [Diagram 3] 1 is a flow chart illustrating a method for reusing a mold according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Fig. 1 is a schematic diagram showing an example of a mold according to an embodiment of the present disclosure. The mold 1 shown in Fig. 1 includes a core 2 and a main mold 3. The core 2 and the main mold 3 are formed of unfired ceramics. The core 2 is placed in the main mold 3. A gap 4 is provided between the core 2 and the main mold 3 for pouring a molten material.

[0009] FIG. 2(a) is a schematic diagram of a non-sintered ceramic used in a mold according to an embodiment of the present disclosure. The non-sintered ceramic 10 shown in FIG. 2(a) is formed by bonding a plurality of ceramic particles 11. Examples of the ceramic particles 11 include silica (SiO2), alumina (Al2O3), iron oxide (Fe2O3), calcium oxide (CaO), magnesium oxide (MgO), sodium oxide (Na2O), titania (TiO2), potassium oxide (K2O), zirconia (ZrO2), and composite oxides of any combination thereof, as well as silicon carbide (SiC). The ceramic particles 11 have their particle surfaces activated by mechanochemical treatment.

[0010] Fig. 2(b) is a diagram used to explain bonding of multiple ceramic particles. Ceramic particles 11 shown in Fig. 2(b) have active surfaces 31 formed on their particle surfaces. Multiple ceramic particles 11 are mixed in an alkaline aqueous solution in which alkaline components 20 such as sodium hydroxide and potassium hydroxide are dissolved, and are heated at a temperature of 100°C or less to bond the particles together. In Fig. 2(a), the active surfaces 31 of multiple ceramic particles 11 are bonded to form bonded parts 30. The alkaline components 20 are attached to the portions of the active surfaces 31 of multiple ceramic particles 11 where bonded parts 30 are not formed. The mold 1 shown in FIG. 1 is made of non-fired ceramic 10 formed from an alkaline aqueous solution in which an alkaline component 20 shown in FIG. 2 is dissolved.

[0011] 3 is a flow chart illustrating a method for reusing a mold according to an embodiment of the present disclosure. As shown in FIG. 3, the method for reusing a mold 1 according to an embodiment of the present disclosure includes a crushing step S100, a pH adjustment step S200, a molding step S300, a solidification step S400, a casting step S500, and a recovery step S600.

[0012] 3, the steps from the crushing step S100 to the recovery step S600 are repeatedly executed. The following will explain the steps starting from the casting step S500. In the casting step S500, a casting is cast using the mold 1. The mold 1 used for casting the casting is destroyed when the casting is removed from the mold 1. In the recovery step S600, pieces of the mold 1 destroyed in the casting step S500 are recovered.

[0013] In the crushing step S100, the fragments of the mold 1 recovered in the recovery step S600 are crushed into grains, and the alkali content 20 is peeled off from the particle surfaces of the ceramic particles 11. This reactivates the particle surfaces of the ceramic particles 11, and an active surface 31 is formed.

[0014] The pH adjustment step S200 is an example of a kneading step. In the pH adjustment step S200, the pH of the alkaline aqueous solution is appropriately adjusted to adjust the pH of the mold 1. In the pH adjustment step S200, the mass and pH of the mixture are adjusted by adding water or an alkaline solution to the mold 1 crushed in the crushing step S100 in an amount corresponding to the mass of the crushed mold 1. The pH of the mixture may be adjusted by dissolving the alkali content 20 peeled off from the particle surface of the ceramic particles 11 in the crushing step S100 in an aqueous solution. The pH of the surface of the mold 1 may affect the strength of the mold 1. For example, the strength of the mold 1 may be improved by increasing the pH of the mold 1 above a predetermined value.

[0015] In the casting step S300, the ceramic particles 11 of the unsintered ceramic 10 whose particle surfaces have been reactivated and the decomposed alkali content are obtained from the mold 1 in the pH adjustment step S200, and an alkali mixture mixed with water or an alkaline aqueous solution is placed into the metal mold of the mold 1. The metal mold of the mold 1 is a metal mold for casting the core 2 and the main mold 3 using the unsintered ceramic 10.

[0016] In the solidification step S400, the metal mold of the mold 1 into which the ceramic particles 11 were placed in the molding step S300 is heated to a temperature of 100° C. or less to solidify the unsintered ceramic 10. This forms the mold 1 in which the unsintered ceramic 10 is reused. In the casting step S500, a new casting is cast using the mold 1 formed in the solidification step S400.

[0017] 〔summary〕 A mold according to one embodiment of the present disclosure is formed from non-fired ceramics. In the present disclosure, by forming the mold from non-sintered ceramics, the mold can be reused at a lower temperature than before, thereby reducing the burden on the environment when the mold is reused.

[0018] A method for reusing a mold according to one embodiment of the present disclosure includes a crushing step of crushing the mold to separate the mold into ceramic particles with reactivated particle surfaces and an alkali component, a kneading step of obtaining an alkali mixture by mixing the ceramic particles and the alkali component in an aqueous solution, and a obtaining step of obtaining the unsintered ceramic by heating the alkali mixture kneaded in the kneading step at a low temperature. Since the process for removing the alkali does not include a heating treatment, less energy is consumed when reusing the mold, which reduces the burden on the environment.

[0019] The present disclosure is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present disclosure. [Explanation of symbols]

[0020] 1. Mold 10. Non-fired ceramics 31 Active surface S100 Crushing step S200 pH adjustment step (mixing step) S300 mold insertion step S400 Solidification step

Claims

1. A mold characterized in that it is formed from a non-fired ceramic consisting of a mixture of ceramic particles and an alkali component.

2. A crushing step of crushing the mold according to claim 1 to separate the mold into ceramic particles having reactivated particle surfaces and an alkali component; a kneading step of obtaining an alkali mixture by mixing the ceramic particles and the alkali component in an aqueous solution; a step of obtaining the non-fired ceramic by low-temperature heating the alkali mixture kneaded in the kneading step; A method for reusing a mold, comprising:

Citation Information

Patent Citations

  • Method and apparatus of reusing core sand

    JP2018015813A