Method of manufacturing semiconductor device
By aligning film stress directions through PE-CVD or HDP-CVD, the method prevents film peeling between the barrier and metal layers in semiconductor devices, improving manufacturing reliability.
Patent Information
- Application Number
- JP2023056778
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-11
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Film peeling occurs between the barrier layer and the metal layer in semiconductor devices manufactured using the MO-CVD method due to mismatched film stress directions.
The method involves aligning the film stress direction of the barrier layer with that of the outermost surface of the insulating layer by using PE-CVD or HDP-CVD to form the insulating layer, ensuring the film stress directions match, thereby preventing peeling.
This approach effectively suppresses film peeling during semiconductor manufacturing, enhancing the integrity of the semiconductor device structure.
Smart Images

Figure 2024143862000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a semiconductor device, which is capable of preventing film peeling that occurs when using an MO-CVD method. [Background technology]
[0002] The MO-CVD (Metal Organic Chemical Vapor Deposition) method is a type of chemical vapor deposition (CVD) method that forms a thin film on a substrate by chemical reaction.
[0003] For example, in the semiconductor device disclosed in Patent Document 1, in order to prevent interdiffusion of the constituent materials of the metal layers at the contact portions of the metal layers made of different materials, multiple barrier layers are formed between the metal layers (FIG. 6, first titanium layer 5, titanium oxide layer 6, second titanium layer 7, titanium nitride layer 8, third titanium layer 9). Of these barrier layers, titanium nitride layer 8 is formed by MO-CVD.
[0004] However, when a barrier layer is formed using the MO-CVD method in the manufacture of a semiconductor device, peeling can occur between the barrier layer and the metal layer stacked on top of it in contact with it, as shown in Figure 5. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2013-258183 A Summary of the Invention [Problem to be solved by the invention]
[0006] In consideration of the above, the present disclosure has an object to provide a semiconductor manufacturing method that suppresses peeling from an upper metal layer when a barrier layer is formed using an MO-CVD method. [Means for solving the problem]
[0007] A method for manufacturing a semiconductor device according to a first aspect of the present invention includes the steps of stacking an insulating layer on a substrate, forming a contact hole penetrating the insulating layer, and forming a barrier layer in the contact hole, wherein in the step of forming the barrier layer, the barrier layer is formed such that the direction of film stress of the barrier layer coincides with the direction of film stress of an insulating film forming an outermost surface of the insulating layer.
[0008] A second aspect of the present invention relates to a method for manufacturing a semiconductor device according to the first aspect, wherein the barrier layer includes a TiN film formed by an MO-CVD method.
[0009] A manufacturing method of a semiconductor device according to a third aspect of the present invention includes the steps of stacking an insulating layer on a substrate, forming a contact hole penetrating the insulating layer, and forming a barrier layer in the contact hole, wherein in the step of stacking the insulating layer, the insulating layer is formed so that the outermost surface of the insulating layer is a TEOS film formed by PE-CVD, and in the step of forming the barrier layer, a TiN film is formed by MO-CVD. Effect of the Invention
[0010] As described above, according to the present invention, it is possible to provide a semiconductor manufacturing method that, when a barrier layer is formed using an MO-CVD method, prevents the barrier layer from peeling off from an upper metal layer. [Brief description of the drawings]
[0011] [Figure 1] In the case where a Ti / TiN film was formed using an MOCVD apparatus, FIG. 1(A) shows the case where the outermost surface of the insulating layer is an LP-TEOS film, and FIG. 1(B) shows the case where the outermost surface of the insulating layer is a PE-TEOS film. [Diagram 2] This shows the case where a Ti / TiN film was formed using a Ti / TiN-CVD device. [Diagram 3]1 is a schematic diagram showing a part of a semiconductor device manufactured in a Ti / TiN-CVD apparatus and a part of a semiconductor device manufactured in an MO-CVD apparatus. [Figure 4] FIG. 1 is a diagram showing a comparison of manufacturing processes using a Ti / TiN-CVD apparatus and an MO-CVD apparatus. [Diagram 5] FIG. 1 is a schematic diagram showing film peeling. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] First, in this disclosure, a film peeling that actually occurred will be described. Note that in each drawing, the same or similar reference numerals are used for the same or corresponding members, and duplicated explanations will be omitted.
[0013] As shown in Fig. 5, when a multilayer film of Ti / TiN (hereinafter referred to as Ti / TiN film) is formed as a barrier layer 14 using an MO-CVD apparatus in the manufacture of a semiconductor device, film peeling may occur between the barrier layer 14 and a metal layer 18 that is laminated in contact with the barrier layer 14. Fig. 5 is a schematic diagram showing the film peeling that has occurred. The barrier layer 14 may include a film other than a Ti / TiN film.
[0014] The manufacturing process of the semiconductor device shown in Fig. 5 is outlined below. For ease of explanation, the manufacturing process below will mainly describe steps necessary for the present disclosure. (1) PE-TEOS A TEOS (tetraethoxysilane) film 12 was formed as an insulating layer (or intermediate layer) on a Si substrate 11 (and a Co electrode 16 and a gate 17) by PE-CVD (Plasma Enhanced Chemical Vapor Deposition). In the following, the TEOS film formed by PE-CVD is referred to as a PE-TEOS film. In addition, "on" the substrate is not limited to the upper side that contacts the substrate, but also includes the upper side that does not contact the substrate via another layer. The same applies when it is written as "on" a layer. Therefore, another layer may be present as an insulating layer between the Si substrate 11 and the PE-TEOS film 12. (2)CMP The surface was polished flat by CMP. (3) LP-TEOS A TEOS (tetraethoxysilane) film 13 was formed as an insulating layer (or intermediate layer) on the PE-TEOS by LP-CVD (low pressure CVD). In the following, the TEOS film formed by LP-CVD will be referred to as an LP-TEOS film. (4) Photolithography and Etching Contact holes penetrating the insulating layer were formed in the insulating layer by photolithography and etching. (5) Reverse sputtering In order to remove a natural oxide film formed on the surface of the cobalt electrode 16 exposed from the opening of the contact hole, reverse sputtering was performed by sputtering argon (Ar) ions onto the surface of the cobalt electrode 16 . (6) Pre-RTA cleaning (7) RTA RTA (Rapid Thermal Anneal) was performed. (8)MOCVD In the formed contact holes, a Ti / TiN film was formed as a barrier layer 14 using an MO-CVD apparatus. Note that Ti / TiN indicates that the films were formed in this order: Ti, TiN. (9) WCVD The contact holes were filled with tungsten 15 (W) by CVD.
[0015] Hereinafter, in this specification, the barrier layer 14 formed in the contact hole and the tungsten 15 filled in the contact hole will be collectively referred to as a "contact" to distinguish them from each other. 5, film peeling occurred between the LP-TEOS film 13, the barrier layer 14 (Ti / TiN film), and the tungsten 15, and the metal layer 18. The inventors of the present application conducted an investigation under the assumption that film peeling originated from the contact end, because the contacts were densely packed in the area and film peeling did not occur when the barrier layer 14 was formed using another CVD apparatus.
[0016] As a result, the inventors of the present application found that the direction of film stress is different between the PE-TEOS film 12 and the LP-TEOS film 13, that is, tensile (+) and compressive (-). Furthermore, they found that film peeling occurs depending on the direction (+ or -) of the film stress of the film located on the outermost surface of the insulating layer (LP-TEOS film in FIG. 5) and the film stress of the barrier layer 14 (Ti / TiN film). Film stress refers to stress that occurs due to differences in the expansion coefficients of the thin film and the substrate. It is also called film stress.
[0017] Table 1 shows the film stress of LP-TEOS film and PE-TEOS film. In addition, the film stress of Ti / TiN film formed using MO-CVD equipment and the film stress of Ti / TiN film formed using another CVD equipment (hereafter referred to as Ti / TiN-CVD) are shown. The film stress was measured using a thin film stress measurement equipment. [Table 1]
[0018] Figure 1 shows the case where a Ti / TiN film was formed by MO-CVD equipment. Figure 1(A) shows the case where the outermost surface of the insulating layer is an LP-TEOS film, and Figure 1(B) shows the case where the outermost surface of the insulating layer is a PE-TEOS film. As Figure 1(A) shows, when the outermost surface is an LP-TEOS film, the film stress direction of the LP-TEOS film is (+) and the film stress direction of the Ti / TiN film is (-), which is thought to be why film peeling occurred. On the other hand, as Figure 1(B) shows, when the outermost surface is a PE-TEOS film, the film stress direction of the PE-TEOS film is (-) and the film stress direction of the Ti / TiN film is also (-), so film peeling is unlikely to occur.
[0019] Figure 2 shows the case where a Ti / TiN film is formed using a Ti / TiN-CVD device. As shown in Figure 2, it has been confirmed that when a Ti / TiN film is formed using a Ti / TiN-CVD device, no film peeling occurs, even when the outermost surface is an LP-TEOS film. The direction of the film stress of the Ti / TiN film in this case is (+), as shown in Table 1, and is the same as the direction of the film stress of the LP-TEOS film.
[0020] From the above, when forming the Ti / TiN film of the barrier layer 14 using an MO-CVD apparatus, it is advisable to form it so that the direction of the film stress coincides with that of the film located at the top surface of the insulating layer. When forming the Ti / TiN film using an MO-CVD apparatus, it is advisable to set the film stress of the film located at the top surface of the insulating layer to compressive (-) (for example, using PE-CVD or HDP-CVD). The occurrence of film stress is believed to be due to the Si substrate (wafer) warping or becoming flat during subsequent heat-exposed processes. The large arrow in Figure 1 indicates the stress believed to be caused by the wafer.
[0021] As an embodiment according to the present disclosure, a semiconductor device manufactured using an MO-CVD apparatus will be described in comparison with a semiconductor device manufactured using a Ti / TiN-CVD apparatus. 3 is a schematic diagram showing a part of a semiconductor device manufactured by a Ti / TiN-CVD apparatus and a part of a semiconductor device manufactured by an MO-CVD apparatus, both of which include a Ti / TiN film in the barrier layer.
[0022] In a Ti / TiN-CVD apparatus, since the film stress of the Ti / TiN film is (+), it is preferable that the film located on the outermost surface of the insulating layer 20 similarly has a film stress of (+). Therefore, as shown in Fig. 3, it is preferable that the outermost surface of the insulating layer 20 is formed to be an LP-TEOS film.
[0023] On the other hand, in an MO-CVD apparatus, since the film stress of the Ti / TiN film is (-), it is preferable that the film located on the outermost surface of the insulating layer 20 similarly has a (-) film stress. Therefore, it is preferable to form the outermost surface of the insulating layer 20 so that a PE-TEOS film is the outermost surface, without forming an LP-TEOS film.
[0024] Specific manufacturing steps are shown in the flowchart of Figure 4. In the case of a Ti / TiN-CVD device (flowchart A), the steps may be formation of a PE-TEOS film → CMP → formation of an LP-TEOS film → photolithography and etching for contact holes → reverse sputtering → formation of a Ti / TiN film by the Ti / TiN-CVD device → WCVD (filling with tungsten).
[0025] On the other hand, in the case of an MO-CVD apparatus (flow chart B), the process may be PE-TEOS film formation → CMP → photolithography and etching of contact holes → Ti / TiN film formation by MO-CVD apparatus → WCVD (filling with tungsten). In this way, the "LP-TEOS film formation" and "reverse sputtering" can be eliminated, and the process can be simplified compared to the case of a Ti / TiN-CVD apparatus.
[0026] However, even when an MO-CVD apparatus is used, the layer structure of the insulating layer is not limited. It is sufficient that the film stress of the film that is the outermost surface is in the same direction (+ or -) as the film stress of the Ti / TiN film. Therefore, the layer below the outermost film is not particularly limited. Furthermore, the barrier layer includes at least a TiN film, and may be a Ti / TiN film, and may include other films in addition to the Ti / TiN film as necessary, or may include other films instead of the Ti / TiN film.
[0027] As described above, the method for manufacturing a semiconductor device according to the present disclosure can suppress film peeling, not limited to using an MO-CVD device. Note that well-known methods can be used for the processes of the method for manufacturing a semiconductor device other than those described above. [Explanation of symbols]
[0028] 11. Silicon substrate 12 PE-TEOS membrane 13 LP-TEOS membrane 14 Barrier Layer 15 Tungsten 16 Cobalt Electrode 17 Gate 18, 19 Metal layer 20 Insulating layer
Claims
1. depositing an insulating layer on the substrate; forming a contact hole penetrating the insulating layer; forming a barrier layer in the contact hole; In the step of forming the barrier layer, the barrier layer is formed so that a direction of film stress of the barrier layer coincides with a direction of film stress of an insulating film forming an outermost surface of the insulating layer. A method for manufacturing a semiconductor device.
2. The barrier layer includes a TiN film formed by MOCVD. The method for manufacturing a semiconductor device according to claim 1 .
3. depositing an insulating layer on the substrate; forming a contact hole penetrating the insulating layer; forming a barrier layer in the contact hole; In the step of stacking the insulating layer, the insulating layer is formed so that the outermost surface of the insulating layer is a TEOS film formed by PE-CVD; In the step of forming the barrier layer, a TiN film is formed by MOCVD. A method for manufacturing a semiconductor device.
Citation Information
Patent Citations
Semiconductor device, and method of manufacturing the same
JP2013258183A