Method for manufacturing resin molded product
Incorporating recycled thermoplastic resin fiber scraps with higher fluidity into the base resin for molding enhances moldability and reduces waste in resin products.
Patent Information
- Application Number
- JP2023057148
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-03-31
AI Technical Summary
The generation of fiber scraps during the manufacturing of filter elements and other textile products made of thermoplastic resin leads to waste disposal issues, which is environmentally undesirable due to carbon dioxide emissions.
A method involving the use of recycled thermoplastic resin fiber scraps with higher fluidity than the base resin, mixed with the base resin, followed by heating and molding to form a resin molded product, enhancing moldability while reducing waste.
The method improves moldability of resin products and reduces waste fiber scraps by incorporating fiber scraps with higher fluidity, achieving a balance between moldability and waste reduction.
Smart Images

Figure 2024144954000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a resin molded product. [Background technology]
[0002] Patent Document 1 discloses a filter element used in an air conditioner for an automobile. The filter element has a so-called panel shape with an overall outline of a rectangular parallelepiped. The filter element also includes a filtering portion that filters foreign matter contained in the air.
[0003] The filter material forming the filtration portion is a nonwoven fabric produced by a melt-blowing method. The filtration portion is formed by cutting the nonwoven fabric to a predetermined length and width and then pleating the fabric. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2014-213242 A Summary of the Invention [Problem to be solved by the invention]
[0005] In the manufacture of such filter elements, fiber scraps are generated when the nonwoven fabric is cut. Such fiber scraps are usually discarded and incinerated because they are difficult to recycle.
[0006] However, in recent years, there has been a demand to reduce the amount of waste fiber scraps from the standpoint of reducing carbon dioxide emissions. Furthermore, these problems are not limited to the recycling of fiber scraps generated during the manufacture of filter elements, but also arise when recycling fiber scraps generated during the manufacture of other fiber products made of thermoplastic resins. [Means for solving the problem]
[0007] A method for manufacturing a resin molded product to solve the above problems includes a mixing step of mixing a thermoplastic resin base resin with a recycled fiber scrap material made of thermoplastic resin that has higher fluidity than the base resin in a molten state to form a mixture, a heating step of heating and melting the mixture, and a molding step of injecting the molten mixture into a mold to form a resin molded product.
[0008] According to this method, by mixing fiber scraps, which have a higher fluidity than the base resin, with the base resin, the fluidity of the mixture in a molten state is increased. This improves the moldability of the resin molded product. In addition, by using the fiber scraps in the production of the resin molded product, the amount of waste fiber scraps can be reduced. Therefore, it is possible to achieve both a reduction in the amount of waste fiber scraps and an improvement in the moldability of the resin molded product. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a flow chart showing the steps of manufacturing a resin molded product according to one embodiment. [Diagram 2] FIG. 2 is an exploded perspective view of a filtering section and fiber ends according to the embodiment. [Diagram 3] FIG. 3(a) is a cross-sectional view of a first fiber according to the embodiment, and FIG. 3(b) is a cross-sectional view of a second fiber according to the embodiment. [Figure 4] FIG. 4 is a cross-sectional view showing a mixing step according to the embodiment. [Diagram 5] FIG. 5 is a cross-sectional view of the injection device according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, one embodiment of a method for producing a resin molded product will be described with reference to FIGS. The manufacturing method for a resin molded product is a method of manufacturing a resin molded product using a base resin 10 made of new thermoplastic resin and a recycled material, fiber scrap material 11 made of thermoplastic resin that has higher fluidity than the base resin 10 in a molten state.
[0011] As shown in FIG. 1, the method for producing a resin molded product includes, in order, a first heating step, a cooling step, a crushing step, a mixing step, a second heating step, and a molding step. First, the base resin 10 and the fiber ends 11 will be described.
[0012] The base resin 10 is a thermoplastic resin. The base resin 10 is, for example, polypropylene. The melting point of polypropylene is about 200°C. As shown in FIG. 2, fiber scraps 11 are generated during the manufacture of filter elements used in air conditioners for automobiles.
[0013] More specifically, the fiber scraps 11 are generated when the rectangular sheet-shaped filtering portion 30 of the filter element is cut from a nonwoven fabric sheet. 3(a) and 3(b), the fiber end material 11 includes first fibers 12 and second fibers 13 having a fiber diameter larger than that of the first fibers 12. The fiber diameter R1 of the first fibers 12 is, for example, 1 μm or more and 15 μm or less. The fiber diameter R2 of the second fibers 13 is, for example, 85 μm or more and 95 μm or less.
[0014] The first fibers 12 and the second fibers 13 are made of the same type of thermoplastic resin as the base resin 10. In this embodiment, the first fibers 12 and the second fibers 13 are made of polypropylene. The first fibers 12 and the second fibers 13 are made of fibers spun by a melt-blowing method.
[0015] The polymerization degrees of polypropylene molecules of the first fibers 12, the second fibers 13, and the base resin 10 are small in the same order. Therefore, the MFR (Melt Flow Rate), which is an index of fluidity of the first fibers 12, the second fibers 13, and the base resin 10, are large in the same order. The MFRs of the first fibers 12, the second fibers 13, and the base resin 10 are, for example, about 1200 g / 10 min, about 125 g / 10 min, and about 21 g / 10 min.
[0016] The weight of the second fibers 13 in the fiber end material 11 is greater than the weight of the first fibers 12. The weights of the first fibers 12 and the second fibers 13 are each, for example, about 12 g / m 2 and about 90 g / m 2 It is.
[0017] Next, each step of the method for producing a resin molded product will be described in detail. <First heating step> In the first heating step, the fiber ends 11 are crushed by a crushing and heating device (not shown), and then heated and melted, and the molten resin is extruded and stored in an external tray.
[0018] <Cooling process> In the cooling step, the resin extruded onto the tray (hereinafter, referred to as recycled resin 14) is cooled and solidified.
[0019] <Crushing process> In the pulverizing step, the recycled resin 14 is pulverized by a pulverizer (not shown). <Mixing process> As shown in Fig. 4, in the mixing step, granular base resin 10 and crushed recycled resin 14 are mixed to form a mixture 15. Note that talc 16 is mixed in advance as a filler into the base resin 10. The MFR of the mixture 15 is smaller than the MFR of the first fibers 12 and the second fibers 13, and is larger than the MFR of the base resin 10. The MFR of the mixture 15 is, for example, about 35 g / 10 min.
[0020] <Second heating process> As shown in FIG. 5, in the second heating step, the mixture 15 fed into the injection device 20 is heated.
[0021] The injection device 20 is a device that injects the mixture 15 into a mold (not shown) while heating it. The injection device 20 includes a cylinder 21, a screw 22, a hopper 23, a drive device 24, and a heater 25.
[0022] The cylinder 21 extends horizontally. An injection port 26 is provided at the tip of the cylinder 21 in the extension direction (the left end in FIG. 5). The screw 22 is rotatably accommodated within the cylinder 21 .
[0023] The hopper 23 is disposed above the cylinder 21 and communicates with the inside of the cylinder 21 . An output shaft of a motor of a drive unit 24 is connected to the base end of the screw 22 .
[0024] A heater 25 is disposed on the outer periphery of the cylinder 21, on the tip side (left side in FIG. 5) of the portion where the hopper 23 is disposed. 5, the mixture 15 fed into the hopper 23 enters the cylinder 21 by its own weight. In the cylinder 21, the mixture 15 moves toward the injection port 26 by the rotation of the screw 22. In addition, the mixture 15 is heated by the heater 25 to a temperature equal to or higher than the melting points of the base resin 10 and the recycled resin 14, so that the base resin 10 and the recycled resin 14 melt.
[0025] <Forming process> 5, in the molding process, the molten mixture 15 is injected from the injection port 26 of the injection device 20 into a mold (not shown). Then, the mixture 15 is cooled together with the mold to form a resin molded product.
[0026] The second heating step in this embodiment corresponds to the heating step described in the "Summary of the Invention." Next, the effects of this embodiment will be described.
[0027] (1) In the mixing step, fiber scraps 11, which are recycled materials and have higher fluidity than the base resin 10 in a molten state, are mixed with a base resin 10 to form a mixture 15. The mixture 15 is then heated and melted, and injected into a mold to form a resin molded product.
[0028] According to this method, the fiber end 11, which has a higher fluidity than the base resin 10, is mixed with the base resin 10, thereby increasing the fluidity of the mixture 15 in a molten state. This improves the moldability of the resin molded product. Furthermore, by using the fiber end 11 in the production of the resin molded product, the amount of waste fiber end 11 can be reduced. Therefore, it is possible to achieve both a reduction in the amount of waste fiber end 11 and an improvement in the moldability of the resin molded product.
[0029] (2) Before the mixing step, the recycled resin 14 is crushed. According to this method, the recycled resin 14 is mixed with the base resin 10 in a pulverized state, so that the recycled resin 14 is easily mixed with the base resin 10. Therefore, the recycled resin 14 is less likely to be unevenly distributed in the mixture 15. This makes it possible to prevent the mixture 15 from having parts with high and low fluidity, and thus the moldability can be further improved.
[0030] (3) The fiber end material 11 includes first fibers 12 and second fibers 13 having a fiber diameter larger than that of the first fibers 12 . When spinning fibers made of a thermoplastic resin, the smaller the fiber diameter of the fiber, the narrower the passage through which the molten resin flows in the spinning die. For this reason, generally, the smaller the fiber diameter of the fiber, the more a resin with high fluidity is used.
[0031] According to the above method, since the fiber end material 11 contains the first fibers 12 and the second fibers 13 having different fiber diameters, the fluidity of the mixture 15 can be improved compared to, for example, a case in which the fiber end material 11 is composed only of the second fibers 13.
[0032] However, when the fiber end material 11 is composed only of the first fibers 12, there is a risk of a problem in that the fluidity of the mixture 15 becomes too high. Therefore, if one tries to avoid such a problem, the amount of the fiber end material 11 mixed into the base resin 10 is naturally limited, and there is room for improvement in improving the recycling efficiency of the fiber end material 11.
[0033] In this regard, according to the above method, since the fiber end material 11 contains the first fibers 12 and the second fibers 13 having different fiber diameters, it is possible to increase the amount of the fiber end material 11 mixed into the base resin 10 while preventing the fluidity of the mixture 15 from becoming too high. By increasing the amount of the fiber end material 11 in the mixture 15, the amount of the base resin 10 used can be reduced.
[0034] Therefore, it is possible to achieve both a reduction in the amount of waste fiber ends 11 and an improvement in the moldability of the resin molded product at an even higher level. (4) The weight per unit area of the second fibers 13 is greater than the weight per unit area of the first fibers 12 .
[0035] According to this method, it is possible to prevent the fluidity of the mixture 15 from becoming too high due to the inclusion of a large amount of the first fibers 12, which have a smaller fiber diameter than the second fibers 13, and therefore to prevent molding defects from occurring in the resin molded product. Also, compared to the case where the basis weight of the second fibers 13 is equal to or less than the basis weight of the first fibers 12, it is possible to increase the amount of fiber ends 11 mixed into the base resin 10 while preventing the fluidity of the mixture 15 from becoming too high.
[0036] Therefore, it is possible to achieve both a reduction in the amount of waste fiber ends 11 and an improvement in the moldability of the resin molded product at an even higher level. (5) The first fibers 12, the second fibers 13, and the base resin 10 are made of the same type of thermoplastic resin, and the degree of polymerization of the molecules of the thermoplastic resin decreases in the order of the first fibers 12, the second fibers 13, and the base resin 10.
[0037] According to this method, the first fibers 12, the second fibers 13, and the base resin 10 are easily mixed together in the molten mixture 15. Therefore, the moldability of the resin molded product can be further improved.
[0038] <Example of change> This embodiment can be modified as follows: This embodiment and the following modifications can be combined with each other to the extent that there is no technical contradiction.
[0039] The talc 16 does not have to be premixed with the base resin 10. In the mixing step, the pulverized recycled resin 14, the base resin 10, and the talc 16 may be mixed at the same time.
[0040] The resin molded product may not contain talc 16. The first fibers 12, the second fibers 13, and the base resin 10 are not limited to being made of the same type of thermoplastic resin. As long as the fluidity of the fiber end material 11 in a molten state is higher than the fluidity of the base resin 10, for example, the base resin 10 may be polycarbonate and the fiber end material 11 may be another thermoplastic resin such as polyethylene terephthalate.
[0041] The weight of the second fibers 13 in the fiber end material 11 may be equal to or less than the weight of the first fibers 12 in the fiber end material 11 . The fiber end material 11 may be made up of only fibers having the same fiber diameter.
[0042] The fiber ends 11 crushed in the first heating step may be mixed into the base resin 10 in the crushed state. In the first heating step, the fiber ends 11 may be heated and melted without being crushed.
[0043] The first heating step, the cooling step, and the pulverizing step may be omitted, and the fiber ends 11 that have not been pulverized may be mixed into the base resin 10. The base resin 10 does not have to be new, but may be a recycled material. [Explanation of symbols]
[0044] 10...Base resin 11…Fiber scraps 12…First fiber 13...Second fiber 14…Recycled resin 15...Mixture 16...Talc 20...Injection device 21...Cylinder 22...Screw 23…Hopper 24...Drive unit 25…Heater 26…Ejection port 30…filtration section R1, R2…Fiber diameter
Claims
1. A mixing step of mixing a thermoplastic resin fiber scrap, which is a recycled material and has a higher fluidity than the base resin in a molten state, with a thermoplastic resin base resin to form a mixture; a heating step for heating and melting the mixture; a molding step of injecting the molten mixture into a mold to form a resin molded product; Equipped with A method for manufacturing a resin molded product.
2. A grinding step of grinding the fiber end material is provided before the mixing step, In the mixing step, the pulverized fiber end material and the base resin are mixed together. A method for producing the resin molded product according to claim 1.
3. The fiber end material includes fibers having different fiber diameters. A method for producing the resin molded product according to claim 1 or 2.
4. The fiber end material includes first fibers and second fibers having a fiber diameter larger than that of the first fibers, The weight per unit area of the second fibers is greater than the weight per unit area of the first fibers. A method for producing the resin molded product according to claim 3.
5. the first fibers, the second fibers, and the base resin are made of the same type of thermoplastic resin, and the degrees of polymerization of the molecules of the thermoplastic resin are smaller in the order of the first fibers, the second fibers, and the base resin; A method for producing the resin molded product according to claim 4.
Citation Information
Patent Citations
Environment-friendly type injection molded body and its manufacture
JP1998029222A
Recycle molding method of plastic waste material
JP1998151629A
Manufacture of part for regenerated synthetic resin slide fastener
JP1999070588A
Method for manufacturing exterior parts for car
JP2001341173A
Thermoplastic article and method of making same using improved masterbatch
JP2009542475A
Cited By
Cavity-containing polyester film and method for manufacturing the same
JP2026132665A
Cavity-containing polyester film and method for manufacturing the same
JP2026132666A