Crystal formation method, crystal formation apparatus, image formation method, and method for manufacturing three-dimensional object

The optical vortex laser beam-based crystal formation method addresses scattering issues in laser-induced forward transfer by controlling viscosity and shear stress, achieving precise and accurate transfer of light absorbing materials.

JP2024147483APending Publication Date: 2024-10-16RICOH CO LTD +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023184070
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-03
Filing Date
2023-10-26
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

Existing laser-induced forward transfer methods struggle with scattering of high-viscosity light absorbing materials, leading to inaccurate transfer and scattering of the transfer target material.

Method used

A crystal formation method using an optical vortex laser beam to irradiate a donor substrate with a light absorbing material and dispersion medium, applying shear stress and controlling viscosity within specific ranges to achieve precise transfer without scattering.

Benefits of technology

The method enables high-definition and precise transfer of light absorbing materials by forming crystals with controlled viscosity and shear stress, reducing scattering and improving transfer accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147483000018
    Figure 2024147483000018
  • Figure 2024147483000019
    Figure 2024147483000019
  • Figure 2024147483000020
    Figure 2024147483000020
Patent Text Reader

Abstract

To provide a crystal formation method capable of transferring a light-absorbing material with higher precision without scattering the transfer target material containing the light-absorbing material.SOLUTION: A crystal formation method includes a crystal formation step of irradiating a donor substrate with an optical vortex laser beam from a substrate side of the donor substrate to a transfer target material to fly the transfer target material as a flying object and impart it to the target material, thereby forming crystals, wherein the donor substrate includes a substrate and the transfer target material including a light absorbing material and a dispersing medium on the substrate. A complex viscosity of the transfer target material at a shear stress of 200 Pa at 25°C is 1 mPa_s or more and 8.6 mPa_s or less, and a ten-point average roughness Rz of the target material is 4.9 μm or less.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a crystal formation method, a crystal formation apparatus, an image formation method, and a method for manufacturing a three-dimensional object. [Background technology]

[0002] The Laser-Induced Forward Transfer (LIFT) method is a method in which a donor substrate having a transfer target material including a light absorbing material arranged on the substrate is irradiated with a laser beam from the substrate side of the donor substrate to the transfer target material, causing the transfer target material to fly and transfer the transfer target material to a desired position on a recipient (acceptor substrate) arranged opposite the transfer target material.

[0003] As an example of such a LIFT method, an image formation method has been proposed in which an optical vortex laser beam is used as the laser beam, thereby enabling precise transfer without scattering a highly viscous liquid containing a light absorbing material (see, for example, Patent Document 1). Summary of the Invention [Problem to be solved by the invention]

[0004] An object of the present invention is to provide a crystal formation method capable of transferring a light absorbing material with higher resolution without scattering a transfer target material containing the light absorbing material. [Means for solving the problem]

[0005] The crystal formation method of the present invention as a means for solving the above-mentioned problems includes a crystal formation step in which a donor substrate having a substrate and a transfer target material containing a light absorbing material and a dispersion medium arranged on the substrate is irradiated with an optical vortex laser beam from the substrate side of the donor substrate to cause the transfer target material to fly as a transfer body and be applied to an object to be applied, thereby forming crystals, and is characterized in that the complex viscosity of the transfer target material at 25°C and a shear stress of 200 Pa is 1 mPa·s or more and 8.6 mPa·s or less, and the ten-point average roughness of the object to be applied is 4.9 μm or less. Effect of the Invention

[0006] According to the present invention, it is possible to provide a crystal formation method capable of transferring a light absorbing material with higher definition and accuracy without scattering the transfer target material containing the light absorbing material. [Brief description of the drawings]

[0007] [Figure 1A] FIG. 1A is a schematic diagram showing an example of a wavefront (equal phase surface) in a typical laser beam. [Figure 1B] FIG. 1B is a diagram showing an example of a light intensity distribution in a typical laser beam. [Figure 1C] FIG. 1C is a diagram showing an example of a phase distribution in a typical laser beam. [Figure 2A] FIG. 2A is a schematic diagram showing an example of a wavefront (equal phase surface) in an optical vortex laser beam. [Figure 2B] FIG. 2B is a diagram showing an example of the light intensity distribution in an optical vortex laser beam. [Figure 2C] FIG. 2C shows an example of a phase distribution in an optical vortex laser beam. [Figure 3A] FIG. 3A is a photograph showing an example of a light absorbing material being irradiated with a general laser beam. [Figure 3B] Figure 3B is a photograph showing an example of an optical vortex laser beam being irradiated onto a light absorbing material. [Figure 4A]FIG. 4A is an explanatory diagram showing an example of the results of interference measurement of an optical vortex laser beam. [Figure 4B] FIG. 4B is an explanatory diagram showing an example of the result of interference measurement of a laser beam having a point of zero light intensity at its center. [Figure 5A] FIG. 5A is an explanatory diagram showing an example of the projectile transfer device of the present invention. [Figure 5B] FIG. 5B is an explanatory diagram showing another example of the projectile transferring device of the present invention. [Figure 5C] FIG. 5C is an explanatory diagram showing another example of the projectile transferring device of the present invention. [Figure 6A] FIG. 6A is a schematic cross-sectional view showing an example of the image forming apparatus of the present invention. [Figure 6B] FIG. 6B is a schematic cross-sectional view showing another example of the image forming apparatus of the present invention. [Figure 7A] FIG. 7A is a schematic cross-sectional view showing another example of the image forming apparatus of the present invention. [Figure 7B] FIG. 7B is a schematic cross-sectional view showing another example of the image forming apparatus of the present invention. [Figure 7C] FIG. 7C is a schematic cross-sectional view showing another example of the image forming apparatus of the present invention. [Figure 8A] FIG. 8A is a schematic cross-sectional view showing another example of the image forming apparatus of the present invention. [Figure 8B] FIG. 8B is a schematic cross-sectional view showing another example of the image forming apparatus of the present invention. [Figure 9] FIG. 9 is a schematic cross-sectional view showing an example of an apparatus for producing a three-dimensional object. [Figure 10A] FIG. 10A is a schematic diagram showing an example of a laser irradiation device having an optical vortex laser beam used in the examples and comparative examples. [Figure 10B] FIG. 10B is a schematic diagram showing an example of a laser irradiation device having an optical vortex laser beam used in the examples and comparative examples. [Figure 11] FIG. 11 is a graph showing an example of the relationship between the glycerol concentration (mass %) and the complex viscosity (mPa·s) in transfer target materials Nos. 1 to 8. [Figure 12] Figure 12 is a photograph showing an example of the behavior of transfer target material No. 1 (glycerol concentration 43 mass%, complex viscosity 6 mPa·s) at 0 μs, 3 μs, 5 μs, 10 μs, 20 μs, 30 μs, and 40 μs after irradiation with an optical vortex laser beam. [Figure 13A] Figure 13A is a photograph showing an example of the state in which the material to be transferred (hereinafter referred to as a dot) has been transferred to an object to be treated (S1214, water-polished edge, t1.3, manufactured by Matsunami Glass Industry Co., Ltd.) placed 1.5 mm away from the material to be transferred, and then heated at 300°C to remove the dispersion medium in the material to be transferred. [Figure 13B] FIG. 13B is a schematic diagram showing an example of a 3D image obtained by measuring FIG. 13A using a confocal laser microscope. [Figure 14A] Figure 14A is a top photograph showing an example of a dot obtained by irradiating an optical vortex laser beam with total angular momentum J = 2 (L = 1, S = 1). [Figure 14B] Figure 14B is a cross-sectional side photograph showing an example of a dot obtained by irradiating an optical vortex laser beam with total angular momentum J = 2 (L = 1, S = 1). [Figure 15A] Figure 15A is a top photograph showing an example of a dot obtained by irradiating an optical vortex laser beam with total angular momentum J = -2 (L = -1, S = -1). [Figure 15B] Figure 15B is a side cross-sectional photograph showing an example of a dot obtained by irradiating an optical vortex laser beam with total angular momentum J = -2 (L = -1, S = -1). [Figure 16] FIG. 16 shows the relationship between the dot diameter and the core diameter when the total angular momentum J is changed by the spin angular momentum S. [Figure 17A] FIG. 17A is a photograph showing an example of an observed image of dots formed using transfer target material No. 1, observed with a scanning electron microscope (SEM). [Figure 17B] FIG. 17B is an example of an SEM observation image of the processed product of FIG. 17A, in which the core is sliced ​​using a focused ion beam device (FIB). [Figure 18A]FIG. 18A is a photograph showing an example of a bright-field image of FIG. 17A observed using a transmission electron microscope. [Figure 18B] FIG. 18B is an example of an electron diffraction pattern obtained from the position a in FIG. 18A. [Figure 18C] FIG. 18C is an example of a dark-field image obtained from the electron diffraction spot surrounded by the white circle in FIG. 18C. [Figure 18D] FIG. 18D is an example of an electron diffraction pattern obtained from position b in FIG. 18A. [Figure 18E] FIG. 18E is an example of a dark-field image obtained from the electron beam diffraction spot surrounded by the white circle in FIG. 18D. [Figure 18F] FIG. 18F is an example of the correspondence between the areas shown in FIGS. 18C and 18E and FIG. 18A. [Figure 19A] FIG. 19A is an example of an electron diffraction pattern obtained from the region of FIG. 18C. [Figure 19B] FIG. 19B is an example of an electron diffraction pattern of a spinel crystal (iron ferrite) with Miller indices (122), simulated from ReciPro. [Figure 19C] FIG. 19C is an example of an electron diffraction pattern obtained from the region of FIG. 18E. [Figure 19D] FIG. 19D is an example of an electron diffraction pattern of a spinel crystal (iron ferrite) with Miller indices (100) simulated from ReciPro. [Figure 19E] FIG. 19E is an example of a comparison result between the ratios and angles of the diffraction spots a to e shown in FIGS. 19A to 19D. [Figure 19F] FIG. 19F is a schematic diagram showing an example of two spinel crystals with different zone axes. [Figure 20A] FIG. 20A is a photograph showing an example of a bright-field image of FIG. 17A observed using a transmission electron microscope. [Figure 20B] FIG. 20B is an example of an electron diffraction pattern in Miller indices (100) at the white circle a in FIG. 20A. [Figure 21A] FIG. 21A is an example of an electron diffraction pattern in Miller indices (100) at the white circle a in FIG. 20A. [Figure 21B] FIG. 21B is an example of the distribution of iron (Fe) obtained by elemental analysis, which is mapped onto FIG. 21A. [Figure 21C] FIG. 21C is an example of the distribution of manganese (Mn) obtained by elemental analysis, which is mapped onto FIG. 21A. [Figure 22A] FIG. 22A is a diagram showing an example of patterning using the experimental system of FIG. 10A. [Figure 22B] FIG. 22B is a diagram showing the result of adding a laser beam irradiation region to FIG. 22A. [Figure 22C] FIG. 22C is a diagram showing an example of the relationship between the position error and the dot diameter when the distance between the transfer target material and the object is changed. [Figure 23A] FIG. 23A is an example showing the relationship between each fluence and flight speed when transfer target material No. 1 is used. [Figure 23B] FIG. 23B shows an example of a flying object classified as a single droplet flying mode observed when transfer target material No. 1 was used. [Figure 23C] FIG. 23C shows an example of a flying object classified into a multiple droplet flying mode observed when transfer target material No. 1 was used. [Figure 23D] FIG. 23D shows an example of a flying object classified into a flying mode caused by a bulging jet observed when transfer target material No. 1 was used. [Figure 23E] FIG. 23E shows an example of a flying object classified into the scattering mode observed when transfer target material No. 1 was used. [Figure 24A] FIG. 24A shows an example of the relationship between each fluence and the flight speed when transfer target material No. 7 is used. [Figure 24B] FIG. 24B shows an example of a flying object classified as a single droplet flying mode observed when using transfer target material No. 7. [Figure 24C] FIG. 24C shows an example of a flying object classified into a multiple droplet flying mode observed when transfer target material No. 7 was used. [Figure 24D] FIG. 24D shows an example of a flying object classified into a flying mode caused by a bulging jet observed when transfer target material No. 7 was used. [Figure 24E] FIG. 24E shows an example of a flying object classified as a scattering mode observed when transfer target material No. 7 was used. [Figure 25A] FIG. 25A is an example showing the relationship between each fluence and flight speed when transfer target material No. 8 is used. [Figure 25B] FIG. 25B shows an example of a flying object classified as a single droplet flying mode observed when using transfer target material No. 8. [Figure 25C] FIG. 25C shows an example of a flying object classified into a multiple droplet flying mode observed when transfer target material No. 8 was used. [Figure 25D] FIG. 25D shows an example of a flying object classified into a flying mode caused by a bulging jet observed when transfer target material No. 8 was used. [Figure 25E] FIG. 25E shows an example of a flying object classified into the scattering mode observed when transfer target material No. 8 was used. [Figure 26] Figure 26 shows an example showing the relationship between dots transferred to an object placed 1.5 mm away from the material to be transferred using Figures 23B, 24B, and 25B, and the complex viscosity of the material to be transferred after the dots have been heated at 300°C to remove the dispersion medium in the material to be transferred. [Figure 27A] FIG. 27A is a schematic diagram showing an example of an image diagram of an analysis method. [Figure 27B] FIG. 27B is a schematic diagram showing an example of the spatial distribution of dots obtained by using transfer target material No. 1. [Figure 27C] FIG. 27C is a schematic diagram showing an example of the spatial distribution of dots obtained by using transfer target material No. 7. [Figure 27D]FIG. 27D is a schematic diagram showing an example of the spatial distribution of dots obtained by using transfer target material No. 8. [Figure 28A] FIG. 28A is a schematic diagram showing an example of the relationship between the dot diameter and the core diameter when the film thickness is 26 μm and the beam spot diameters are 34 μm, 49 μm, 74 μm, and 97 μm using transfer target material No. 1. [Figure 28B] FIG. 28B is a schematic diagram showing an example of the relationship between the dot volume and the core height when the beam spot diameter is changed in FIG. 28A. [Figure 29A] FIG. 29A is a diagram showing an example of the change in bubble growth over time up to 3.0 μs after irradiation with a laser beam. [Figure 29B] FIG. 29B is a graph showing an example of the relationship between the internal pressure calculated from the Rayleigh-Plesset equation and the elapsed time after laser beam irradiation. [Figure 30A] FIG. 30A is a simplified diagram showing an example of an analysis method. [Figure 30B] FIG. 30B is a graph showing an example of the results of an experiment in which the transfer target material was uniformly No. 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] (Crystallization method and crystallization device) The crystal formation method of the present invention includes a crystal formation step of irradiating an optical vortex laser beam from the substrate side of a donor substrate having a substrate and a transfer target material containing a light absorber and a dispersion medium arranged on the substrate onto the transfer target material, causing the transfer target material to fly as a transfer body and be applied to an object to be applied, thereby forming crystals, wherein the complex viscosity of the transfer target material at 25°C and a shear stress of 200 Pa is 1 mPa·s or more and 8.6 mPa·s or less, and the ten-point average roughness of the object to be applied is 4.9 μm or less, and the method further includes other steps as necessary.

[0009] The crystal formation apparatus of the present invention has a crystal formation means for irradiating an optical vortex laser beam onto a donor substrate having a substrate and a transfer target material containing a light absorber and a dispersion medium arranged on the substrate from the substrate side of the donor substrate, causing the transfer target material to fly as a transfer body and be applied to an object to be applied, thereby forming crystals, wherein the complex viscosity of the transfer target material at 25°C and a shear stress of 200 Pa is 1 mPa·s or more and 8.6 mPa·s or less, and the ten-point average roughness of the object to be applied is 4.9 μm or less, and the apparatus further has other means as necessary.

[0010] The projectile transfer method of the present invention can be suitably carried out by the crystal formation apparatus of the present invention, and the crystal formation step can be carried out by the crystal formation means, and the other steps can be carried out by other means.

[0011] In the prior art, there was no mention of the effect that the surface smoothness of the object to be coated (hereinafter sometimes referred to as "smoothness") has on the shape of the material to be transferred (hereinafter referred to as the transferred object) transferred onto the object to be coated, making it difficult to accurately reproduce the shape of the transferred object.

[0012] Therefore, in the present invention, a donor substrate having a substrate and a transfer target material containing a light absorbing material and a dispersion medium on the substrate is irradiated with an optical vortex laser beam from the substrate side of the donor substrate to fly the transfer target material as a transfer body and apply it to an object to form crystals. Since the complex viscosity of the transfer target material at 25°C and a shear stress of 200 Pa is 1 mPa·s or more and 8.6 mPa·s or less, the light absorbing material that absorbs light of a predetermined wavelength can be concentrated at a high density at one point in the formation of the flying object using the optical vortex laser. This high-density aggregate (hereinafter sometimes referred to as "core") is melted and aggregated in a state having the crystallinity of the light absorbing material, and can promote the synthesis of the material. Therefore, the thickness of the transfer target increases in the height direction, and it is possible to transfer in a three-dimensional shape. In addition, since the ten-point average roughness of the object to which the projectiles are to be attached is 4.9 μm or less, the core can be formed near the center of the object with good reproducibility, making it possible to transfer the core with high precision.

[0013] <Crystallization process and crystallization means> The flying process is a process in which a donor substrate having a substrate and a transfer target material containing a light absorbing material and a dispersion medium arranged on the substrate is irradiated with an optical vortex laser beam from the substrate side of the donor substrate to cause the transfer target material to fly as a flying object and be applied to an object to form a crystal, and can be performed by a crystal formation means.

[0014] <<Donor Substrate>> The donor substrate has a substrate and a transfer target material, which contains a light absorbing material and a dispersion medium, disposed on the substrate. In the present invention, "flying" means moving through the air or traveling through the air. In the present invention, "scattering" means scattering by flying away.

[0015] -substrate- The substrate is not particularly limited in shape, structure, size, material, etc., and may be appropriately selected depending on the purpose.

[0016] The shape of the substrate is not particularly limited and can be appropriately selected according to the purpose, and examples thereof include a flat plate, a cylindrical shape such as a perfect circle or ellipse, a surface cut out from a cylindrical shape, and an endless belt shape. Among these, it is preferable that the substrate is cylindrical and has a supplying means for supplying the transfer target material to the surface of the substrate rotating in the circumferential direction. When the transfer target material is supported on the surface of the cylindrical substrate, it can be supplied regardless of the size of the object in the circumferential direction. In this case, a flying means is arranged inside the cylindrical shape, and the optical vortex laser beam can be irradiated from the inside toward the periphery, and continuous irradiation can be performed by rotating the substrate in the circumferential direction. The flat substrate may be, for example, a glass slide.

[0017] The structure of the substrate is not particularly limited and can be appropriately selected depending on the purpose.

[0018] The size of the substrate is not particularly limited and can be appropriately selected depending on the purpose, but it is preferable that the size of the substrate is set to match the width of the object to which the transfer material is to be applied.

[0019] The material of the substrate is not particularly limited as long as it transmits light, and can be appropriately selected depending on the purpose. However, inorganic materials such as various glasses containing silicon oxide as a main component, and organic materials such as transparent heat-resistant plastics and elastomers are preferred in terms of transmittance and heat resistance.

[0020] The transmittance of the optical vortex laser beam in the substrate is not particularly limited and can be appropriately selected according to the purpose, but is preferably 75% or more, more preferably 85% or more. If the transmittance is within the preferred range, the energy of the optical vortex laser beam absorbed in the substrate is not easily converted into heat, so that the transfer target material is less likely to be changed, such as dried or melted, and the energy given to the transfer target material is less likely to decrease, which is advantageous in that the position where the transferred material is applied is less likely to vary. The transmittance can be measured, for example, using a spectrophotometer (V-660DS, manufactured by JASCO Corporation).

[0021] The surface roughness Ra of the substrate is not particularly limited and can be appropriately selected according to the purpose, but it is preferable that both the front and back surfaces are 1 μm or less in order to suppress refraction and scattering of the optical vortex laser beam and not to reduce the energy applied to the transfer target material. In addition, when the surface roughness Ra is within a preferred range, it is advantageous in that it is possible to suppress the variation in the average thickness of the transfer target material applied to the object to which the transfer target material is applied, and it is possible to apply the desired amount of the transfer target material. The surface roughness Ra can be measured in accordance with JIS B0601, for example, using a stylus-type surface profiler (Dektak150, manufactured by Bruker AXS K.K.). Furthermore, when the substrate is made of a soft material such as cloth, the surface roughness Ra can be estimated and measured in a non-contact manner, for example, by using a confocal microscope (H1200, Lasertec Corporation).

[0022] -Transfer target material- The material to be transferred contains a light absorbing material and a dispersion medium, and further contains other components as required. The transfer target material has a complex viscosity of 1 mPa·s or more and 8.6 mPa·s or less at 25° C. and a shear stress of 200 Pa. When the complex viscosity is 1 mPa·s or more and 8.6 mPa·s or less, the light absorbing material melts and aggregates while maintaining its crystallinity, facilitating the synthesis of the material. The complex viscosity can be measured under the following conditions using a dynamic viscoelasticity measuring device by a stress control method in which the applied stress is changed and the amount of strain generated at that time is measured. -Measurement conditions- - Instrument name: Rheometer, HAAKE RheoStress 600, Thermo Fisher Scientific ·Temperature: 25℃ Shear stress: 200Pa

[0023] --Light absorbing material-- The light absorbing material preferably has an absorbance for a light wavelength of greater than 1, and more preferably greater than 2. When the light absorbing material has an absorbance for a light wavelength of greater than 2, it is advantageous in that energy efficiency can be improved.

[0024] The light absorbing material is not particularly limited as long as it absorbs light of a predetermined wavelength, and can be appropriately selected depending on the purpose. For example, inorganic materials can be used.

[0025] The inorganic material is not particularly limited with respect to its shape, size, material, etc., and can be appropriately selected depending on the purpose. The form of the inorganic material may be, for example, a solid, a powder, etc. The term "solid" refers to a material that retains its shape at 25° C. regardless of the shape of the container.

[0026] Examples of the inorganic material include manganese ferrite, iron ferrite, magnesium ferrite, strontium ferrite, triiron tetroxide, titanium oxide, zinc sulfide, black iron oxide, black copper oxide, black chromium oxide, yellow iron oxide, yellow nickel titanium, cadmium sulfide, selenium, cadmium selenide, lead chromate, lead molybdate, red iron oxide, cobalt oxide, hydrous chromium oxide, chromium oxide, gold, lead antimony, nickel oxide, manganese oxide, neodymium oxide, erbium oxide, cerium oxide, aluminum oxide, aluminum, bronze, mica, carbon black, carbon, zeolite, calcium carbonate, barium sulfate, zinc oxide, antimony trioxide, mercury cadmium sulfide, Prussian blue, ultramarine, etc. These may be used alone or in combination of two or more.

[0027] When the light absorbing material contains two or more different inorganic materials, it is preferable that the two or more different inorganic materials are made of substances having the same crystal structure. The crystal structure is not particularly limited and may be appropriately selected depending on the purpose. For example, a spinel type crystal structure may be mentioned. Examples of the light absorbing material include light absorbing materials made of iron ferrite and manganese ferrite, which have the same spinel type crystal structure.

[0028] The median diameter (D 50 ) is preferably 50 nm or more and 500 nm or less, and more preferably 50 nm or more and 240 nm or less. The median diameter (D 50 The median diameter (D) is measured, for example, using a scanning electron microscope (SU8200 series, manufactured by Hitachi High-Technologies Corporation). The obtained image is binarized using image processing software A-zo-kun (manufactured by Asahi Kasei Engineering Co., Ltd.) to obtain the median diameter (D 50 ) can be calculated. Alternatively, for example, a transmission electron microscope (JEM-2100, manufactured by JEOL Ltd.) is used for the measurement. For the observation sample, an ethanol dispersion containing 0.4% by mass of inorganic material is prepared, and the dispersion is dispersed in an ultrasonic cleaner for about 1 hour. The measurement is then performed using a collodion film-attached mesh (manufactured by Nissin EM Co., Ltd.). The obtained image is binarized using image processing software A-zo-kun (manufactured by Asahi Kasei Engineering Co., Ltd.), and the median diameter (D 50 ) can be calculated.

[0029] --Dispersion medium-- The dispersion medium is not particularly limited as long as it can disperse the light absorbing material, and can be appropriately selected according to the purpose, and examples thereof include water, organic solvents, wax, and resin varnish. These may be used alone or in combination of two or more. Among these, pure water and an aqueous glycerol solution are preferred because a dispersion medium having an ignition residue of 0.1% or less or an evaporation residue of 1.0 or less allows the transfer of a transfer target material with high purity. The glycerol concentration in the glycerol aqueous solution is not particularly limited and may be appropriately selected depending on the purpose, but is preferably less than 52% by mass, and more preferably 43% by mass or less. When the glycerol concentration is less than 52% by mass, the complex viscosity of the transfer target material at 25°C and a shear stress of 200 Pa is easily controlled to be 1 mPa s or more and 8.6 mPa s or less.

[0030] Examples of the water include pure water such as ion-exchanged water, ultrafiltered water, reverse osmosis water, and distilled water, and ultrapure water. The organic solvent is not particularly limited and can be appropriately selected depending on the purpose. Examples of the organic solvent include glycerol, ethanol, and acetone.

[0031] The wax is not particularly limited and may be appropriately selected depending on the purpose. Examples of the wax include hydrocarbon waxes, ester waxes, and ketone waxes.

[0032] The resin varnish is not particularly limited and can be appropriately selected depending on the purpose. Examples of the resin varnish include acrylic, polyester, styrene, polyurethane, alkyd, epoxy, amber, and rosin varnishes.

[0033] The dispersion medium may contain a surfactant from the viewpoint of dispersibility of the light absorbing material. The surfactant is not particularly limited and can be appropriately selected depending on the purpose. Examples of the surfactant include anionic surfactants, cationic surfactants, nonionic surfactants, and amphoteric surfactants.

[0034] Examples of the anionic surfactant include fatty acid soap, alkyl succinate, sodium alkylbenzene sulfonate, sodium alkylnaphthalene sulfonate, sodium alkyl sulfate, sodium polyoxyethylene alkyl ether sulfate, sodium dialkyl sulfosuccinate, sodium alkyl phosphate, polycarboxylic acid type polymer surfactant, etc. In addition to the above-mentioned sodium salts, any metal salt, ammonium salt, etc. may also be used. Examples of the cationic surfactant include alkyltrimethylammonium chloride and alkyldimethylbenzylammonium chloride. Examples of the nonionic surfactant include polyoxyethylene alkyl ether, polyoxyethylene alkyl allyl ether, and sorbitan fatty acid ester. Examples of the amphoteric surfactant include alkyl betaines and amido betaines.

[0035] -Other ingredients- Examples of other components include colorants, dispersants, heat stabilizers, antioxidants, anti-reducing agents, preservatives, pH adjusters, antifoaming agents, wetting agents, and penetrating agents.

[0036] The material to be transferred in the donor substrate disposed on the substrate may be in the form of a layer or a film, and can be appropriately selected depending on the purpose. The material to be transferred may form an integral (continuous) layer (film) on the substrate, or may form an intermittent layer (film).

[0037] The average thickness of the transfer target material (transfer target layer) when it is liquid at 25° C. is not particularly limited and can be appropriately selected depending on the purpose, but is preferably 10 μm or more, more preferably 10 μm to 50 μm, and even more preferably 20 μm to 50 μm. When the transfer target layer is liquid at 25° C., if the average thickness of the transfer target layer is 10 μm or more, scattering of the transfer target material when irradiated with light can be suppressed, and when the material is continuously supplied in a layer form, the strength of the layer on the substrate can be ensured even when the material is continuously flown, so that the transfer target material can be continuously flown. Furthermore, when the layer to be transferred is liquid at 25°C, if the average thickness of the layer to be transferred is 50 μm or less, the light energy required to make the material to be transferred fly does not become too large, which is advantageous in that deterioration and decomposition are less likely to occur, particularly when the light absorbing material is organic. Depending on the application method, it may be possible to supply the material as a layer that maintains a certain pattern. The average thickness of the transfer target layer when it is solid at 25° C. is not particularly limited and can be appropriately selected depending on the purpose, but is preferably 40 μm or less, more preferably 0.2 μm to 20 μm, and even more preferably 5 μm to 18 μm. When the transfer target layer is solid at 25° C., if the average thickness of the transfer target layer is 40 μm or less, transfer is possible with relatively weak light energy, and damage to the light absorbing material can be suppressed.

[0038] The method for measuring the average thickness of the transfer target layer is not particularly limited and can be appropriately selected according to the purpose, and examples thereof include a method of selecting multiple arbitrary points on the transfer target layer and calculating the average thickness of the multiple points. The average thickness is preferably an average thickness of 5 points, more preferably an average thickness of 10 points, and particularly preferably an average thickness of 20 points. The measuring device for the average thickness is not particularly limited and can be appropriately selected depending on the purpose. For example, a laser displacement meter, a micrometer, or the like can be used for a non-contact or contact method.

[0039] In the present invention, the donor substrate is used, and an optical vortex laser beam is irradiated onto a material to be transferred from the substrate side of the donor substrate, causing the material to be transferred to fly. In the present invention, the term "flying" means that at least a part of the material to be transferred is detached from the donor substrate. By using an optical vortex laser beam, it is possible to prevent the flying transfer target material from scattering.

[0040] The optical vortex laser beam is described in detail below. A typical laser beam has a uniform phase, and therefore has a planar equiphase surface (wavefront) as shown in Figure 1A. The direction of the Poynting vector of the laser beam is perpendicular to the planar equiphase surface, and therefore the direction is the same as the direction of the laser beam irradiation. Therefore, when the laser beam is irradiated onto a light-absorbing material in the transfer target material, a force acts on the light-absorbing material in the irradiation direction. However, the light intensity distribution on the cross section of the laser beam is a normal distribution (Gaussian distribution) with the strongest intensity at the center of the beam as shown in Figure 1B, so the transfer target material is likely to scatter. In addition, when the phase distribution is observed, it is confirmed that there is no phase difference as shown in Figure 1C. In contrast, the optical vortex laser beam has a helical equiphase surface as shown in Figure 2A. Since the direction of the Poynting vector of the optical vortex laser beam is perpendicular to the helical equiphase surface, when the optical vortex laser beam is irradiated to the light absorbing material in the transfer target material, a force acts in the perpendicular direction. Therefore, as shown in Figure 2B, the light intensity distribution becomes a concave donut-shaped distribution with zero at the center of the beam, and the donut-shaped energy is applied as radiation pressure to the light absorbing material irradiated with the optical vortex laser beam. Then, the light absorbing material irradiated with the optical vortex laser beam flies along the irradiation direction of the optical vortex laser beam and is applied to the object in a state where it is difficult to scatter. In addition, when the phase distribution is observed, it is confirmed that a phase difference occurs as shown in Figure 2C.

[0041] Figure 3A is a photograph showing an example of a typical laser beam irradiated onto a light absorbing material in a transfer target material. Figure 3B is a photograph showing an example of a light vortex laser beam irradiated onto a light absorbing material in a transfer target material. Comparing Figure 3A and Figure 3B, it can be seen that the transfer target material is scattered more in Figure 3A than in Figure 3B. This shows that the light absorbing material in the transfer target material irradiated with the optical vortex laser beam is applied with doughnut-shaped energy as radiation pressure, so that it flies along the irradiation direction of the optical vortex laser beam and is applied to the target object in a state that is less likely to scatter.

[0042] There are no particular limitations on the method for determining whether or not an optical vortex laser beam is present, and it can be selected appropriately depending on the purpose. For example, the method can include the aforementioned observation of the phase distribution and interferometry, with interferometry being the most common. The interference measurement can be observed using a laser beam profiler (such as a laser beam profiler manufactured by Spiricon or a laser beam profiler manufactured by Hamamatsu Photonics KK), and examples of the results of the interference measurement are shown in FIG. 4A and FIG. 4B. FIG. 4A is an explanatory diagram showing an example of the results of interferometry on an optical vortex laser beam, and FIG. 4B is an explanatory diagram showing an example of the results of interferometry on a laser beam having a point with zero light intensity at its center. When an optical vortex laser beam is subjected to interferometric measurement, it can be confirmed that the energy distribution is donut-shaped, as shown in Figure 4A, and that the laser beam has a point of zero light intensity in the center, as in Figure 1C. On the other hand, when an interferometric measurement of a typical laser beam with a point of zero light intensity at the center is performed, as shown in Figure 4B, it is similar to the interferometric measurement of the optical vortex laser beam shown in Figure 4A. However, the energy distribution in the donut-shaped part is not uniform, confirming the difference from the optical vortex laser beam.

[0043] -Flight means- The flying means irradiates light onto the material to be transferred from the substrate side of the donor substrate, in other words, irradiates light onto the surface of the substrate opposite the side on which the material to be transferred is arranged, thereby causing the material to be transferred to fly in the direction of light irradiation.

[0044] The flying means includes a laser light source, an optical vortex converter, and a wavelength converter, and may further include other components as necessary.

[0045] --Laser light source-- The laser light source is not particularly limited and can be appropriately selected depending on the purpose. Examples of the laser light source include solid-state lasers, gas lasers, and semiconductor lasers that generate laser beams, and those capable of pulse oscillation are preferable. Examples of the solid-state laser include a YAG laser and a titanium sapphire laser. Examples of the gas laser include an argon laser, a helium-neon laser, and a carbon dioxide laser. Among these, a semiconductor laser with an output of about 30 mW is preferable from the viewpoint of miniaturization and cost reduction of the device, however, in this embodiment, a titanium sapphire laser is used. The wavelength of the laser beam is not particularly limited and can be appropriately selected depending on the purpose, but is preferably 300 nm or more and 11 μm or less, and more preferably 350 nm or more and 1100 nm or less. The beam diameter of the laser beam is not particularly limited and can be appropriately selected depending on the purpose, but is preferably from 10 μm to 10 mm, and more preferably from 10 μm to 1 mm. The pulse width of the laser beam is not particularly limited and can be appropriately selected depending on the purpose, but is preferably from 2 nanoseconds to 100 nanoseconds, and more preferably from 2 nanoseconds to 10 nanoseconds. The pulse frequency of the laser beam is not particularly limited and can be appropriately selected depending on the purpose, but is preferably from 10 Hz to 200 Hz, and more preferably from 20 Hz to 100 Hz. The laser light source may be a laser light source capable of outputting an optical vortex laser beam.

[0046] --Optical vortex converter-- The optical vortex converter is not particularly limited as long as it can convert a laser beam into an optical vortex laser beam, and can be appropriately selected depending on the purpose. Examples of the optical vortex converter include a diffractive optical element, a multimode fiber, and a liquid crystal phase modulator. Examples of the diffractive optical element include a spiral phase plate, a hologram element, etc. Among these, a spiral phase plate is preferable. The method of generating the optical vortex laser beam is not limited to the method using the optical vortex converter, but may include, for example, a method of oscillating an optical vortex as an eigenmode from a laser resonator, a method of inserting a hologram element into a resonator, etc. Other methods of generating the optical vortex laser beam include, for example, a method of using excitation light converted into a doughnut beam, a method of using a resonator mirror with a dark spot, and a method of oscillating in an optical vortex mode using the thermal lens effect generated by a side-excited solid-state laser as a spatial filter.

[0047] --Wavelength conversion section-- The optical vortex laser beam is characterized by a helical equiphase surface, a circular beam intensity distribution, and a phase singularity in the optical wavefront. In the present invention, there are no particular limitations as long as it has these characteristics, and an appropriate wavelength conversion section can be selected according to the purpose, such as a circularly polarized optical vortex laser beam obtained by providing a circularly polarized optical vortex laser beam. A circularly polarized optical vortex laser beam has a total angular momentum J consisting of orbital angular momentum and spin angular momentum due to circular polarization, and is expressed by the following equation (1). Examples of the wavelength conversion unit include a quarter-wave plate. In the case of a quarter-wave plate, the optical axis may be set at an angle other than +45° or -45° to impart elliptical circular polarization (elliptical polarization) to the optical vortex laser beam, but it is preferable to set the optical axis at +45° or -45° to impart true circular circular polarization to the optical vortex laser beam and satisfy the above conditions. This allows the projectile transfer device to stably fly the light absorbing material and increase the effect of imparting it to the object in a shape that suppresses scattering.

[0048]

number

number

[0049] L is a parameter determined by the number of turns of the helical wavefront in the wave plate. S is a parameter determined by the direction of circular polarization in the wave plate. Both L and S are integers. The signs of L and S indicate the direction of rotation (clockwise, counterclockwise), respectively. The total angular momentum J of an optical vortex laser beam can be expressed as J = L + S.

[0050] The flying object transfer device of the present invention is equipped, for example, with an optical vortex conversion unit that converts a laser beam into an optical vortex laser beam, and a wavelength conversion unit that imparts circular polarization to the optical vortex laser beam.By converting the optical vortex laser beam into a circularly polarized optical vortex laser beam, it is possible to express linear directionality of flying objects of highly viscous material to be transferred, thereby improving the effect of suppressing scattering of the material to be transferred.

[0051] --Other materials-- The other members are not particularly limited and can be appropriately selected depending on the purpose. Examples of the other members include a beam diameter changing member, a beam wavelength changing element, and an output adjustment unit.

[0052] ---Beam diameter change parts--- There are no particular limitations on the beam diameter changing member as long as it can change the beam diameter of the optical vortex laser beam, and it can be selected appropriately depending on the purpose, such as a focusing lens. The beam diameter (irradiation diameter) of the optical vortex laser beam is not particularly limited and can be selected appropriately depending on the purpose, but it is preferably 100 μm or less. If the irradiation diameter of the optical vortex laser beam is 100 μm or less, it is preferable because it is easy to form a high-resolution image. The beam diameter can be changed by, for example, the laser spot diameter and the condenser lens. In addition, when the material to be transferred is a dispersion, the beam diameter is preferably equal to or larger than the maximum volume average particle diameter of the material to be transferred, and more preferably three times the maximum volume average particle diameter of the dispersion. If the beam diameter is within the more preferred range, it is advantageous in that the material to be transferred can be stably ejected.

[0053] ---Beam wavelength changing element--- The beam wavelength changing element is not particularly limited as long as it can change the wavelength of the optical vortex laser beam to a wavelength that can be absorbed by the light absorbing material in the transfer target material and can be transmitted through the substrate described below, and can be appropriately selected according to the purpose. Examples of the beam wavelength changing element include KTP crystal, BBO crystal, LBO crystal, and CLBO crystal.

[0054] ---Output adjustment section--- The output adjustment unit is not particularly limited as long as it can adjust the laser beam or optical vortex laser beam to an appropriate output value, and can be appropriately selected depending on the purpose. For example, glass can be used.

[0055] The output value of the optical vortex laser beam irradiated onto the transfer target material is not particularly limited, and can be appropriately selected according to the purpose, as long as it can produce a state in which a liquid column that converges to a diameter smaller than the irradiation diameter while rotating around the central axis of the irradiation diameter with the irradiation direction as the axis, or a state in which a part of the liquid column is detached and a droplet is produced. Note that hereinafter, "output value" may also be referred to as "irradiation energy". The irradiation energy of the optical vortex laser beam is preferably adjusted appropriately since the appropriate value varies depending on the viscosity and film thickness of the material to be transferred, but specifically, 100 μJ / dot or less is more preferable, and 60 μJ / dot or less is even more preferable. If the irradiation energy of the optical vortex laser beam is 60 μJ / dot or less, it is advantageous in that it is easy to realize a state in which a liquid column that converges to a diameter smaller than the irradiation diameter while rotating around the central axis of the irradiation diameter with the irradiation direction as the axis can be generated, or a state in which a part can be detached and a droplet can be generated.

[0056] The means for applying the flying object to the object to be applied is not particularly limited and can be appropriately selected depending on the purpose, and examples thereof include a means having a mechanism for contacting the liquid column or droplets of the material to be transferred with the object to be applied, etc. Specifically, examples of the applying means include a mechanism for adjusting the gap between the object to be applied and the material to be transferred, and a mechanism for transporting the object to be applied. The term "imparting" is almost synonymous with "attaching."

[0057] -Granted object- The ten-point average roughness Rz (surface smoothness) of the object to be treated is 4.9 μm or less, preferably 2.3 μm or less, from the viewpoint of forming the core near the center of the transferred object with good reproducibility, and more preferably 0.007 μm or more and 1.5 μm or less from the viewpoint of higher accuracy. When the ten-point average roughness Rz is 4.9 μm or less, the core can be formed near the center of the transferred object with good reproducibility, and the shape of the transferred object can be reproduced with high accuracy. The ten-point average roughness Rz can be measured in accordance with JIS B0601, for example, using a stylus-type surface profiler (Dektak150, manufactured by Bruker AXS K.K.).

[0058] The shape of the object to be applied is not particularly limited and can be appropriately selected depending on the purpose, and examples thereof include recording media and intermediate transfer belts conventionally used in image forming apparatuses, object support substrates for forming three-dimensional objects, etc. In this specification, the object to be applied is sometimes referred to as an image receiving medium. To prepare the cross section, an ultramicrotome ULTRACUT-S (Leica Corporation) or a focused ion beam device (FIB) can be used, and an appropriate device can be selected as necessary. The recording medium is not particularly limited and can be appropriately selected depending on the purpose. Examples of the recording medium include coated paper, wood-free paper, film, cloth, and fiber.

[0059] The gap (gap, distance) between the object to be applied and the transfer target material is not particularly limited as long as the object to be applied and the transfer target material are not in contact with each other, and can be appropriately selected according to the purpose, but is preferably 0.05 mm or more and 5 mm or less, more preferably 0.10 mm or more and 2 mm or less, and particularly preferably 0.50 mm or more and 1.50 mm or less. If the gap between the object to be applied and the transfer target material is within a preferred range, it is advantageous in that the accuracy of the application position of the transfer target material to the object to be applied is unlikely to decrease. In addition, by not contacting the object to be applied and the transfer target material, it is possible to apply the transfer target material to the object to be applied regardless of the composition of the light absorbing material and the object to be applied. Further, it is preferable that the gap is kept constant by, for example, a position control means for maintaining the position of the object to be applied constant. In this case, it is important to arrange each part in consideration of the positional fluctuation of the transfer target material and the object to be applied and the variation in the average thickness.

[0060] The average diameter (average dot diameter) of the transfer target material applied to the substrate is not particularly limited and may be appropriately selected depending on the purpose. For example, it is preferable to set the average diameter to 100 μm or less, since this can further improve the resolution of the image or three-dimensional object to be formed. In addition, the average dot diameter can be obtained, for example, by obtaining a dot image of the material to be transferred using a microscope or the like, detecting a dot area from image brightness information, calculating the area of ​​each dot from the number of pixels in the detected dot area, and averaging the diameter when converted into a circle as the dot diameter.

[0061] Furthermore, the variation in the average diameter (dot diameter) of the transfer target material applied to the object is preferably 10% or less, and more preferably 6% or less. By setting the variation in the average diameter of the transfer target material applied to the object to the preferred range described above, it is possible to further improve the accuracy in forming an image or a three-dimensional object. In addition, the value of the variation in the average diameter of the material to be transferred applied to the object to be transferred can be obtained, for example, by acquiring a dot image of the material to be transferred using a microscope or the like, detecting a dot area from image brightness information, calculating the area of ​​each dot from the number of pixels in the detected dot area, defining the diameter when converted into a circle as the dot diameter, and calculating it from the average particle size and standard deviation of the particle size distribution of each dot.

[0062] In addition, the value of the variation in the position (dot position) of the transfer target material applied to the object to be applied is preferably 10 μm or less, more preferably 5 μm or less. By setting the value of the variation in the position of the transfer target material applied to the object to be applied within the above-mentioned preferred range, the accuracy of forming an image or a three-dimensional object can be further improved. Note that, for example, when dots of the transfer target material are applied in a row, the value of the variation in the position of each of the transfer target materials in a direction perpendicular to the row of dots can be used as the value of the variation in the position of each of the transfer target materials applied to the object to be applied. For example, the dot image of the material to be transferred is obtained using a microscope or the like, and dot areas are detected from image brightness information. The coordinates of the center of gravity of each detected dot area are then calculated, and the deviation of each center of gravity from an approximate straight line using the least squares method is calculated to obtain the value.

[0063] The average thickness of the transfer target material applied to the object to be applied is not particularly limited and can be appropriately selected according to the purpose, but is preferably 100 μm or less. If the average thickness of the transfer target material applied to the object to be applied is 100 μm or less, the energy required to fly the transfer target material can be reduced, which is advantageous in terms of the durability of the transfer target material and the fact that decomposition of the composition when the light absorbing material is an organic material is unlikely to occur. The average thickness of the transfer target material applied to the object to be applied can be appropriately selected according to the recording medium, purpose, etc.

[0064] <Other processes> Examples of the other steps include a supplying step, a light scanning step, and a control step.

[0065] <<Supply process and supply means>> The supplying step is not particularly limited as long as it is a step of supplying the transfer target material to the optical path between the flying means and the object to be transferred, and can be appropriately selected depending on the purpose. For example, it can be suitably performed using the supplying means. The supplying means is not particularly limited as long as it is a means for supplying the transfer target material to the optical path between the flying means and the object to be transferred, and can be appropriately selected depending on the purpose.

[0066] The supplying means may be, for example, a cylindrical substrate, etc. In the case where the cylindrical substrate is used, the cylindrical substrate may be disposed on an optical path, and the transfer target material may be supplied to the donor substrate via the cylindrical substrate. More specifically, when the material to be transferred is liquid and is supplied to the donor substrate, it is preferable to provide a supply roller and a regulating blade as the supply means, since this is a very simple configuration that allows the material to be supplied to the surface of the substrate at a constant average thickness. In this case, the supply roller is partially immersed in a storage tank that stores the transfer target material, rotates while carrying the transfer target material on its surface, and abuts against the donor substrate to supply the transfer target material. The regulating blade is disposed downstream of the storage tank in the rotation direction of the supply roller, and regulates the transfer target material carried by the supply roller to make the average thickness uniform and stabilize the amount of the transfer target material to be scattered. By making the average thickness of the transfer target material to be supplied very thin, the amount of the transfer target material to be scattered can be reduced, so that the transfer target material can be applied to the object to be applied as minute dots with reduced scattering, and dot gain, which causes the halftone dots to thicken, can be suppressed. The regulating blade may be disposed downstream of the supply roller in the rotation direction of the supply roller.

[0067] In addition, when the material to be transferred has a high viscosity, the material of the supply roller is preferably one having at least an elastic surface so as to ensure contact with the donor substrate. When the material to be transferred has a relatively low viscosity, examples of the supply roller include a gravure roll, a microgravure roll, and a forward roll, which are used in precision wet coating.

[0068] Furthermore, as a supply means that does not include a supply roller, the donor substrate may be directly contacted with the material to be transferred in the storage tank, and then excess material to be transferred is scraped off with a wire bar or the like to form a layer of the material to be transferred on the surface of the donor substrate. The storage tank may be provided separately from the supply means, and the transfer target material may be supplied to the supply means by a hose or the like.

[0069] <<Optical scanning process and optical scanning means>> The optical scanning process is not particularly limited as long as it is a process of scanning the optical vortex laser beam onto the transfer target material, and can be appropriately selected depending on the purpose. For example, it can be suitably performed using the optical scanning means. The optical scanning means is not particularly limited as long as it can scan the optical vortex laser beam on the transfer target material, and can be appropriately selected according to the purpose. For example, the optical scanning means may have a reflector that reflects the light irradiated from the flying means toward the transfer target material, and a reflector driving unit that changes the angle and position of the reflector to scan the optical vortex laser beam on the transfer target material.

[0070] <<Control process>> The control step is a step of controlling each step and can be suitably performed by a control means. The control means is not particularly limited as long as it can control the movement of each means and can be appropriately selected depending on the purpose. Examples of the control means include devices such as a sequencer and a computer.

[0071] Next, an example of a projectile transfer device according to the present invention will be described with reference to the drawings. The number, positions, shapes, etc. of the members of the projectile transfer device of the present invention are not limited to those in this embodiment, and the number, positions, shapes, etc. may be any number, positions, shapes, etc. that are preferable for implementing the present invention.

[0072] FIG. 5A is an explanatory diagram showing an example of the projectile transfer device of the present invention. 5A, the flying object transfer device 300 has a flying means 1, a transfer target material (transfer target layer) 20, an object to be applied 30, and a donor substrate 40. The donor substrate 40 is provided on the upper surface of the transfer target layer 20 on the opposite side to the donor substrate 40. The flying object transfer device 300 irradiates the transfer target layer 20 carried on the donor substrate 40 with a laser beam 112 by the flying means 1, and causes the transfer target layer 20 to fly in the irradiation direction by the energy of the laser beam 12. In Fig. 5A, an object to be treated 30 is an object to which the flown transfer target layer 20 is to be treated. By arranging the object to be treated 30 opposite the transfer target layer 20, the transfer target layer 20 can be treated on the object to be treated 30.

[0073] The flying means 1 has a laser light source 2, beam diameter changing members 3 and 7, a beam wavelength changing member 4, an optical vortex converting unit 5, and a wavelength converting unit 6.

[0074] The laser light source 2 is, for example, a titanium sapphire laser, which generates a pulsed laser beam 11 and irradiates the beam diameter changing member 3 with the laser beam. The beam diameter changing member 3 is, for example, a condenser lens, and is disposed downstream of the laser light source 2 in the optical path of the laser beam 11 generated by the laser light source 2 to change the diameter of the laser beam 11. The beam wavelength changing member 4 is, for example, a KTP crystal, and is disposed downstream of the beam diameter changing member 3 in the optical path of the laser beam 11 to change the wavelength of the laser beam 11 to a wavelength that can be absorbed by the layer 20 to be transferred. The optical vortex converter 5 is, for example, a spiral phase plate, and is arranged downstream of the beam wavelength changing member 4 in the optical path of the laser beam 11 , and converts the laser beam 11 into an optical vortex laser beam 12 . The wavelength conversion section 6 is, for example, a quarter-wave plate, and provides the optical vortex laser beam 12 with circular polarization.

[0075] The transfer target layer 20 is irradiated with the optical vortex laser beam 12 from the flying means 1, and flies by receiving energy within the range of the diameter of the optical vortex laser beam 12. By placing an object 30 opposite the transfer target layer 20, the transfer target layer 20 can be applied to the object 30. In addition, the flying transfer target layer 20 is twisted while converging near the central axis of the beam diameter due to the forward propulsion and gyro effect caused by the moderate energy imparted by the optical vortex laser beam 12, thereby being applied to the object 30 while preventing it from scattering to the surrounding area. At this time, the flying amount of the transfer target layer 20 is a portion of the area of ​​the transfer target layer 20 irradiated with the optical vortex laser beam 12, and can be adjusted by the wavelength conversion unit 6, etc.

[0076] FIG. 5B is an explanatory diagram showing another example of the projectile transferring device of the present invention. In FIG. 5B, the flying object transfer device 301 has an optical scanning means 60 in addition to the various means of the flying object transfer device 300 shown in FIG. 5A. In FIG. 5B, the donor substrate 40 is arranged such that the long axis direction of the donor substrate 40 is perpendicular to the irradiation direction of the optical vortex laser beam 12. In this flying object transfer device 301, the optical scanning means 60 scans the optical vortex laser beam 12 generated by the flying means 1 onto the donor substrate 40. As a result, the flying object transfer device 301 can irradiate an arbitrary position on the donor substrate 40 and fly the transfer target material (transfer target layer) 20. As a result, when the object to be applied 30 is placed opposite the transfer target layer 20, the transfer target layer 20 can be applied to an arbitrary position on the object to be applied 30.

[0077] The optical scanning means 60 is disposed downstream of the flying means 1 in the optical path of the optical vortex laser beam 12, and has a reflecting mirror 61. The reflecting mirror 61 is movable in the scanning direction indicated by the arrow S in FIG. 5B by a reflecting mirror driving means, and reflects the optical vortex laser beam 12 to an arbitrary position on the transfer target layer 20 . The optical scanning means 60 may, for example, move the flying means 1 itself or rotate the flying means 1 to change the irradiation direction of the optical vortex laser beam 12. Alternatively, the optical scanning means 60 may use the polygon mirror as the reflecting mirror 61 to scan the optical vortex laser beam 12 at any position.

[0078] The donor substrate 40 is disposed downstream of the optical scanning means 60 in the optical path of the optical vortex laser beam 12, and is used for the purpose of applying and fixing the layer to be transferred 20 when the layer to be transferred 20 is a high-viscosity liquid, for example. The donor substrate 40 is transmissive to the light, and supports the layer to be transferred 20 on the surface opposite to the surface irradiated with the optical vortex laser beam 12. Furthermore, at the stage where the transfer target layer 20 is supported on the donor substrate 40, the flying amount of the transfer target layer 20 can be stabilized by controlling the average thickness of the layer formed by the transfer target layer 20 to be constant. The combination of the flying means 1 and the optical scanning means 60 is referred to as a laser beam irradiation unit 100.

[0079] FIG. 5C is an explanatory diagram showing another example of the projectile transferring device of the present invention. In Fig. 5C, flying object transfer device 301a has galvanometer scanners (galvanometer mirrors) 62a and 62b as the optical scanning means 60 in the flying object transfer device 301 shown in Fig. 5B. The galvanometer scanners 62a and 62b are each movable in an independent scanning direction (two-dimensionally) and can reflect the optical vortex laser beam 12 to any position on the transfer target layer 20. By using the galvanometer scanners 62a and 62b as the optical scanning means 60, the scanning speed and scanning accuracy of the optical vortex laser beam 12 can be further improved. Furthermore, the flying object transfer device 301a may be configured such that light is passed through a galvano scanner and then focused by an fθ lens (hereinafter, sometimes referred to as a "focusing lens"). The focusing lens may be appropriately selected according to the purpose of the experiment, and since the theoretical limit of the minimum beam spot diameter obtained when focused is proportional to the focal length of the lens, an appropriate focusing lens may be selected. As a result, when a lens with a long focal length is selected, the area of ​​the laser beam irradiated on the transfer target material also becomes larger, and the volume of the transferred object increases. In the flying object transfer device 301a, it is also preferable to place an fθ lens between the galvano scanner 62b and the substrate 40, for example.

[0080] Applications of the crystal formation method and crystal formation apparatus of the present invention are not particularly limited and can be appropriately selected depending on the purpose. Examples thereof include image formation, production of three-dimensional objects, and printable circuit formation.

[0081] (Image forming method) The image forming method of the present invention forms an image by the crystal forming method of the present invention, and further includes other steps as necessary. Specifically, the image forming method of the present invention includes a crystal forming step, and further includes other steps as necessary. The crystal formation step is the same as the crystal formation step in the crystal formation method of the present invention.

[0082] When forming an image, a colorant is used as the material to be transferred. The colorant is not particularly limited with respect to its shape, material, etc., and may be appropriately selected depending on the purpose.

[0083] The liquid colorant is not particularly limited and can be appropriately selected depending on the purpose, but for example, an aqueous ink in which a coloring material such as a dye, pigment, colored particles, or colored oil droplets is dispersed in water as a solvent can be used. In addition to aqueous ink, a colorant containing a relatively low boiling point liquid as a solvent, such as a hydrocarbon organic solvent or various alcohols, can also be used. Among these, aqueous ink is preferred from the standpoint of safety of volatile components and risk of explosion.

[0084] In addition, the image forming device can also form images using process inks for offset printing, which uses plates, JAPAN COLOR compatible inks, and special color inks, making it easy to reproduce digital images that match the colors used in offset printing without plates. Furthermore, since images can also be formed using UV-curable ink, by curing the ink by irradiating it with ultraviolet light in the fixing process, blocking, where overlapping recording media stick together, can be prevented and the drying process can be simplified.

[0085] Examples of the coloring material include organic pigments, inorganic pigments, dyes, etc. These may be used alone or in combination of two or more.

[0086] Examples of the organic pigments include dioxazine violet, quinacridone violet, copper phthalocyanine blue, phthalocyanine green, sap green, monoazo yellow, disazo yellow, polyazo yellow, benzimidazolone yellow, isoindolinone yellow, fast yellow, chromophthalic yellow, nickel azo yellow, azomethine yellow, benzimidazolone orange, alizarin red, quinacridone red, naphthol red, monoazo red, polyazo red, perylene red, anthraquinonyl red, diketopyrrolopyrrole red, diketopyrrolopyrrole orange, benzimidazolone brown, sepia, and aniline black. Examples of metal lake pigments among the organic pigments include rhodamine lake, quinoline yellow lake, and brilliant blue lake.

[0087] Examples of the inorganic pigments include cobalt blue, cerulean blue, cobalt violet, cobalt green, zinc white, titanium white, titanium yellow, chrome titanium yellow, light red, chrome oxide green, mars black, viridian, yellow ocher, alumina white, cadmium yellow, cadmium red, vermilion, lithopone, ultramarine, talc, white carbon, clay, mineral violet, rose cobalt violet, silver white, calcium carbonate, magnesium carbonate, Examples of suitable pigments include zinc oxide, zinc sulfide, strontium sulfide, strontium aluminate, brass, gold powder, bronze powder, aluminum powder, brass pigments, ivory black, peach black, lamp black, carbon black, Prussian blue, aureolin, titanium mica, yellow ochre, terre belt, raw sienna, raw umber, Cassel earth, chalk, gypsum, burnt sienna, burnt umber, lapis lazuli, azurite, malachite, orpiment, cinnabar, coral powder, chalk powder, red ocher, ultramarine, Prussian blue, fish phosphorus foil, and iron oxide-treated pearls.

[0088] Among these, carbon black is preferred as the black pigment from the viewpoints of hue and image storage stability. As the cyan pigment, CI Pigment Blue 15:3, which is copper phthalocyanine blue, is preferred from the standpoints of hue and image storage stability.

[0089] As the magenta pigment, CI Pigment Red 122, which is quinacridone red, CI Pigment Red 269, which is naphthol red, and CI Pigment Red 81:4, which is rhodamine lake, are preferred, and these may be used alone or in combination of two or more. Among these, from the viewpoint of hue and image storage stability, a mixture of CI Pigment Red 122 and CI Pigment Red 269 is more preferred, and as a mixture of CI Pigment Red 122 (PR122) and CI Pigment Red 269 (PR269), a mixture of PR122:PR269 of 5:95 or more and 80:20 or less is particularly preferred. When PR122:PR269 is within the particularly preferred range, the hue does not deviate from magenta color.

[0090] As the yellow pigment, preferred are CI Pigment Yellow 74, which is a monoazo yellow, CI Pigment Yellow 155, which is a disazo yellow, CI Pigment Yellow 180, which is a benzimidazolone yellow, and CI Pigment Yellow 185, which is an isoindoline yellow. Among these, CI Pigment Yellow 185 is more preferred in terms of hue and image storage stability. These may be used alone or in combination of two or more.

[0091] When the transfer target material is used as a process color ink as a colorant, it is preferable to use it as a four-color ink set.

[0092] The inorganic pigment is often composed of particles having a volume average particle size of more than 10 nm. When an inorganic pigment having a volume average particle size of 10 nm or more is used as a colorant, the colorant is preferably a liquid. If the colorant is a liquid, it is advantageous in that the colorant can be maintained in a stable state without using forces other than non-electrostatic adhesion forces such as electrostatic forces. In addition, in this case, the image forming method of the present invention is very effective compared to the inkjet recording method in which nozzle clogging and ink sedimentation are likely to become significant, making it difficult to achieve a stable continuous printing process. Furthermore, the image forming method of the present invention is very effective compared to the electrophotographic method in which a sufficient amount of charge cannot be obtained when the surface area of ​​the colorant particles becomes small, and therefore a stable continuous printing process cannot be achieved.

[0093] Examples of the dyes include monoazo dyes, polyazo dyes, metal complex azo dyes, pyrazolone azo dyes, stilbene azo dyes, thiazole azo dyes, anthraquinone derivatives, anthrone derivatives, indigo derivatives, thioindigo derivatives, phthalocyanine dyes, diphenylmethane dyes, triphenylmethane dyes, xanthene dyes, acridine dyes, azine dyes, oxazine dyes, thiazine dyes, polymethine dyes, azomethine dyes, quinoline dyes, nitro dyes, nitroso dyes, benzoquinone dyes, naphthoquinone dyes, naphthalimide dyes, and perinone dyes.

[0094] The viscosity of the colorant is not particularly limited and may be appropriately selected depending on the purpose. When a liquid colorant that permeates into the recording medium is used, the colorant applied to the recording medium may cause feathering or bleeding, but when a high-viscosity colorant that can be handled by the projectile transfer method of the present invention is used, the colorant dries faster than it permeates into the recording medium, and thus the reduction in bleeding in particular leads to improved color development and sharper edges, making it possible to form high-quality images. Also, when performing gradation expression by applying colorant in layers, bleeding due to an increase in the amount of colorant can be reduced. Furthermore, since this projectile transfer method involves applying a liquid colorant by projecting it, it is possible to perform recording well even if the recording medium has minute irregularities, as compared with, for example, a so-called thermal transfer method in which a colorant is melt-transferred from a film-like donor substrate by heat.

[0095] <Other manual processes and other means> Examples of the other steps include a step of transporting an object to be treated and a fixing step.

[0096] The object transporting step is not particularly limited as long as it is a step of transporting the object, and can be appropriately selected depending on the purpose. For example, it can be suitably performed using an object transport means. The object transport means is not particularly limited as long as it can transport the object, and can be appropriately selected depending on the purpose. For example, a pair of transport rollers can be used.

[0097] The fixing means is not particularly limited as long as it can fix the light absorbing material contained in the transfer target material applied to the object, and can be appropriately selected depending on the purpose. For example, a thermocompression method using a heating and pressing member can be used. The heating and pressing member is not particularly limited and can be appropriately selected depending on the purpose, and examples thereof include a heating roller, a pressure roller, a combination of a heating roller and a pressure roller, etc. Other heating and pressing members include, for example, a combination of these with a fixing belt, and a heating block in place of the heating roller.

[0098] The pressure roller is preferably one whose pressure surface moves at the same speed as the object to be applied, which is transported by the object transport means, in order to suppress image deterioration due to friction. Among these, one having an elastic layer formed near the surface is more preferable in order to easily apply pressure to the object to be applied. Furthermore, the pressure roller having a water-repellent surface layer formed on the outermost surface using a low surface energy material such as a silicone-based water-repellent material or a fluorine compound is particularly preferable in order to suppress image distortion caused by the application of the transfer target material to the surface. Examples of the water-repellent surface layer made of the silicone-based water-repellent material include a film of a silicone-based release agent, a baked film of silicone oil or various modified silicone oils, a film of silicone varnish, a film of silicone rubber, and a film made of a composite of silicone rubber and various metals, rubber, plastic, ceramic, or the like. Examples of the water-repellent surface layer made of a fluorine compound include a fluororesin film, an organic fluorine compound film, a baked film or adsorption film of fluorine oil, a fluororubber film, and a film made of a composite of fluororubber and various metals, rubber, plastic, ceramic, etc.

[0099] The heating temperature of the heating roller is not particularly limited and can be appropriately selected depending on the purpose, but is preferably 80° C. or more and 200° C. or less.

[0100] The fixing belt is not particularly limited as long as it has heat resistance and high mechanical strength, and can be appropriately selected according to the purpose, and examples thereof include films such as polyimide, PET, and PEN. In addition, the fixing belt is preferably made of the same material as that forming the outermost surface of the pressure roller in order to suppress image disturbance caused by the transfer target material being applied to the surface. Since the thickness of the fixing belt can be reduced, the energy required to heat the belt itself can be reduced, so that the fixing belt can be used immediately after turning on the power. The temperature and pressure at this time vary depending on the composition of the light absorbing material to be fixed, but a temperature of 200°C or less is preferable from the viewpoint of energy saving, and a pressure of 1 kg / cm or less is preferable from the viewpoint of the rigidity of the device.

[0101] In the image forming method and image forming apparatus of the present invention, the flying means, the supplying means, and the optical scanning means may be integrally treated as a flying unit. For example, an example will be described in which a colorant containing a coloring material is used as the transfer target material. Four of the flying units may be provided in the image forming apparatus, and the colorants of yellow, magenta, cyan, and black, which are process colors, may be flown. The number of colors of the colorants is not particularly limited and may be appropriately selected according to the purpose, and the number of flying units (hereinafter, colorant flying units) may be increased or decreased as necessary. In addition, by disposing the flying unit having a white colorant upstream of the flying unit having the colorant of the process color in the conveying direction of the recording medium, it is possible to provide a white concealing layer, so that an image with excellent color reproducibility can be formed on a transparent recording medium. However, in particular for yellow, white, and transparent colorants, there are cases in which the laser light source must be appropriately selected, for example, a blue laser beam, an ultraviolet laser beam, or the like, so that the light transmittance (absorbance) of the wavelength of the laser beam is appropriate.

[0102] Furthermore, in the image forming apparatus relating to the image forming method of the present invention, a highly viscous colorant can be used. Therefore, even if an image is formed by sequentially overlapping colorants of different colors on a recording medium, the occurrence of bleeding, in which the colorants seep out and mix, can be suppressed, and a high-quality color image can be obtained. For the purpose of miniaturizing the image forming apparatus relating to the image forming method of the present invention, only one flying unit may be provided, and a multi-color image may be formed by switching the colorant itself supplied to the supply roller and the donor substrate.

[0103] Next, an example of an image forming apparatus according to the image forming method of the present invention will be described with reference to the drawings. The number, position, shape, etc. of the members of the image forming apparatus relating to the image forming method of the present invention are not limited to those in this embodiment, and may be any number, position, shape, etc. that is preferable for implementing the present invention.

[0104] FIG. 6A is an explanatory diagram showing an example of an image forming apparatus in which a supplying unit and a target transporting unit are added to the flying object transferring device shown in FIG. 5B. In Fig. 6A, image forming apparatus 302 has supply means 50 and object transport means 70 in addition to the various means of projectile transfer apparatus 301 shown in Fig. 5B, and is obtained by replacing flat substrate 40 with a cylindrical support roller 41. A laser beam irradiation unit 100 is disposed inside support roller 41, and irradiates optical vortex laser beam 12 onto transfer target material (transfer target layer) 20 carried on the outer periphery of support roller 41.

[0105] The supplying means 50 includes a storage tank 51 , a supplying roller 52 , and a regulating blade 53 . The storage tank 51 is disposed below and in the vicinity of the supply roller 52 and stores the transfer target material 20 . Supply roller 52 is disposed so as to abut against carrier roller 41, and is partially immersed in transfer target material 20 in storage tank 51. Supply roller 52 applies transfer target material 20 to its surface while rotating in the rotation direction indicated by arrow R2 in FIG. 6A by a rotation drive means or following the rotation of carrier roller 41. The applied transfer target material 20 is made uniform in average thickness by regulating blade 53, and is transferred to carrier roller 41 and supplied as a layer. Transfer target material 20 supplied to the surface of carrier roller 41 is continuously supplied to the position irradiated with optical vortex laser beam 12 as carrier roller 41 rotates. The regulating blade 53 is positioned upstream of the carrier roller 41 in the rotation direction indicated by the arrow R2 in Figure 6A, and regulates the transfer target material 20 applied to its surface by the supply roller 52, thereby making the average thickness of the transfer target material 20 supplied to the carrier roller 41 uniform.

[0106] The object transport means 70 is disposed near the carrying roller 41 so that the object 30 to be transported does not come into contact with the carrying roller 41, and has an object transport roller 71 and an object transport belt 72 stretched around the object transport roller 71. The object transport means 70 rotates the object transport roller 71 by a rotary drive means, and transports the object 30 by the object transport belt 72 in the transport direction shown by the arrow C in FIG. 6A. At this time, the laser beam irradiation unit 100 irradiates the optical vortex laser beam 12 from the inside of the carrier roller 41 in accordance with the image information, causing the transfer target material 20 to be applied to the object 30. By performing an application operation in which the transfer target material 20 is applied to the object 30 while the object 30 is moved by the object conveyor belt 72, a two-dimensional image can be formed on the object 30.

[0107] The transfer target material (transfer target layer) 20 that is supported on the surface of the support roller 41 but not caused to fly accumulates as the support roller 41 rotates and comes into contact with the supply roller 52, and eventually drops and is collected in the storage tank 51. The method of collecting the transfer target material 20 is not limited to this, and a scraper that scrapes off the transfer target layer 20 on the surface of the support roller 41 may be provided.

[0108] FIG. 6B is an explanatory diagram showing another example of an image forming apparatus in which a supplying unit and a target transporting unit are added to the flying object transferring device shown in FIG. 5B. In FIG. 6B, image forming device 303 is a modification of image forming device 302 in which cylindrical support roller 41 in image forming device 302 shown in FIG. 6A is divided into two support sections 42 along the axial direction, and the arrangement of image forming device 302 is changed.

[0109] The support portion 42 is a partial surface of a cylinder, and has a shape with no surface on the opposite side of the center line of the cylinder. By making the support body without an opposing surface in this way, it is easier to ensure the optical path of the optical vortex laser beam 12 without providing the laser beam irradiation unit 100 on the cylindrical support roller 41, and therefore the device can be simplified.

[0110] FIG. 7A is an explanatory diagram showing an example of the image forming apparatus shown in FIG. 6A to which a fixing unit is added. In Fig. 7A, the image forming apparatus 305 has a fixing means 80 in addition to the various means of the image forming apparatus 302 shown in Fig. 6A, so as to fix and smooth the transfer target layer 20 applied to the object 30. Note that the object transport means 70 is located on the side of the carrier roller 41 in Fig. 6A, but is located above the carrier roller 41 in Fig. 7A for the sake of convenience.

[0111] The fixing means 80 is a pressure-applying fixing means, which is disposed downstream of the carrying roller 41 in the transport direction of the object 30 indicated by the arrow C in Fig. 7A, and includes a pressure roller 83 and an opposing roller 84. The fixing means 80 fixes the object 30, to which the transfer target layer 20 has been applied, by applying pressure to the object 30 by conveying the object 30 while sandwiching it.

[0112] The pressure roller 83 is biased toward the opposing roller 84, and its surface comes into contact with the object 30 to which the pressure is to be applied, and the object 30 is pressed while being sandwiched between the opposing roller 84 and the pressure roller 84. The counter roller 84 is disposed at a position where it comes into contact with the pressure roller 83 , and the object 30 is sandwiched between the pressure roller 83 and the object conveying belt 72 .

[0113] For example, if the transfer target material 20 has a very high viscosity of 1,000 mPa·s or more, the transfer target material 20 is likely to penetrate or wet the object 30 to which the transfer target material 20 is applied slowly. If the transfer target material 20 dries in its original state, the surface roughness of the image may become rough and the gloss of the image may decrease. In such a case, the fixing means 80 presses the object 30 to which the transfer target material 20 is applied with the pressure roller 83, and can push the transfer target material 20 into the object 30 to which the transfer target material 20 is applied or crush the transfer target material 20, thereby reducing the surface roughness of the object 30 to which the transfer target material 20 is applied.

[0114] FIG. 7B is an explanatory diagram showing another example of the image forming apparatus shown in FIG. 6A to which a fixing unit is added. In FIG. 7B, an image forming apparatus 306 is obtained by changing the pressure fixing unit 80 in the image forming apparatus 305 shown in FIG. 7A to a heat and pressure fixing unit 81 . Fixing means 81 is disposed downstream of carrying roller 41 in the transport direction of object 30 indicated by arrow C in Fig. 7B, and includes heat and pressure roller 85, fixing belt 86, driven roller 87, halogen lamp 88, and opposing roller 84. This fixing means 81 is used when a target image cannot be obtained by applying pressure alone in the case where a dispersion liquid in which a material that needs to be melted is used as transfer target material 20.

[0115] The heating and pressing roller 85 is biased toward the opposing roller 84, and applies heat and pressure to the object 30 while sandwiching it with the opposing roller 84 via the fixing belt 86. The fixing belt 86 is an endless belt that is stretched around a heating and pressure roller 85 and a driven roller 87 and has a surface that comes into contact with the object 30 to which the toner is applied. The driven roller 87 is disposed below the heating and pressure roller 85 and rotates in accordance with the rotation of the heating and pressure roller 85 . The halogen lamp 88 is disposed inside the heating and pressure roller 85 and generates heat for fixing the transfer target layer 20 onto the object 30 . The counter roller 84 is disposed at a position where it contacts the fixing belt 86 , and the object 30 is sandwiched between the pressure roller 83 and the object conveying belt 72 .

[0116] FIG. 7C is an explanatory diagram showing another example of the image forming apparatus shown in FIG. 6A to which a fixing unit is added. In FIG. 7C, an image forming apparatus 307 is obtained by changing the pressure fixing unit 80 in the image forming apparatus 305 shown in FIG. 7A to a UV irradiation fixing unit 82 . The fixing means 82 is disposed downstream of the carrying roller 41 in the transport direction of the object 30 indicated by the arrow C in FIG. 7C, and has a UV lamp 89. This fixing means 81 is used when an ultraviolet-curable material is used as the transfer target layer 20, and fixes the material 30 to the object 30 by irradiating UV light from the UV lamp 89.

[0117] FIG. 8A is an explanatory diagram showing an example of an image forming apparatus of the present invention. In FIG. 8A, image forming apparatus 400 has four flying units 120 in addition to the various means of image forming apparatus 306 shown in FIG. 7B, and is modified for use when colorant 21 containing color material is used as transfer target material 20. The flying unit 120 is composed of a supplying means 50, a flying means 100, a beam scanning means 60 (not shown), a carrying roller 41, and a transfer target material 20 (colorant 21).

[0118] The flying units 120Y, 120M, 120C, and 120K store, as colorants 21, toners of four process colors, yellow (Y), magenta (M), cyan (C), and black (K), respectively. This makes it possible to apply the toner to a color process in which images of each color are formed in sequence on a recording medium 31 as an object 30 to which toner is to be applied, thereby obtaining a color image.

[0119] FIG. 8B is an explanatory diagram showing another example of the image forming apparatus of the present invention. In FIG. 8B, an image forming apparatus 401 has an intermediate transfer means 90 as an object to which a toner is applied, in addition to the various means of the image forming apparatus 400 shown in FIG. 8A.

[0120] The intermediate transfer means 90 includes an intermediate transfer body 91 , an intermediate transfer body drive roller 92 , and an intermediate transfer body driven roller 93 . The intermediate transfer body 91 is, for example, an endless belt, and is disposed above the four flying units 120 and is stretched between an intermediate transfer body drive roller 92 and an intermediate transfer body driven roller 93 . The intermediate transfer body drive roller 92 is rotated by a rotation drive means in the direction indicated by the arrow R2 in FIG. The intermediate transfer member driven roller 93 rotates in accordance with the rotation of the intermediate transfer member drive roller 92 . In this way, an image may first be formed on the intermediate transfer body 91, and then transferred to a desired recording medium 31. This image forming apparatus 201 can also obtain a high-quality color image, similar to the image forming apparatus 400. Furthermore, when the image formed on the intermediate transfer body 91 is transferred to the recording medium 31, it is pressed by the intermediate transfer body drive roller 92, so that, similar to the image forming apparatus 200, the surface roughness of the recording medium 31 to which the colorant 21 has been applied can be reduced.

[0121] In addition, in Figure 5B, the direction in which the laser beam is irradiated is the direction of gravity, but in Figures 5A and 6A to 8B, it is shown that the direction in which the laser beam is irradiated is the opposite direction to the direction of gravity or is horizontal. In this manner, in the image forming method of the present invention, the direction of irradiation of the laser beam onto the surface of the substrate may be the non-gravity direction, and the liquid column or droplets may be generated in the non-gravity direction, which increases the degree of freedom in the design of the apparatus.

[0122] The image forming method and the image forming apparatus of the present invention can also be applied to a manufacturing method and an apparatus for manufacturing a three-dimensional object as described below.

[0123] (Method of manufacturing three-dimensional objects) The method for producing a three-dimensional object of the present invention produces a three-dimensional object by the crystal formation method of the present invention, and further includes other steps as necessary. Specifically, the method includes a crystal formation step, and further includes other steps as necessary. The crystal formation step is the same as the crystal formation step in the crystal formation method of the present invention. In the crystal formation step in the method for producing a three-dimensional object, the transfer target material as a three-dimensional modeling agent is stacked in layers on the object to be transferred, and is applied three-dimensionally.

[0124] -3D modeling agent- The three-dimensional modeling agent is not particularly limited in shape, material, etc., as with the transfer target material, and can be appropriately selected depending on the purpose. Hereinafter, differences when using a three-dimensional modeling agent as the transfer target material in the manufacturing method of the three-dimensional object will be described.

[0125] The average thickness of each layer of the three-dimensional modeling agent applied to the object to be applied is not particularly limited and can be appropriately selected according to the purpose, and varies depending on the required precision, etc., but is preferably 5 μm or more and 500 μm or less. If the average thickness of each layer of the three-dimensional modeling agent applied to the object to be applied is 5 μm or more and 500 μm or less, it is advantageous in terms of the precision, texture, smoothness, production time, etc. of the three-dimensional modeling object. In addition, the average thickness of each layer of the three-dimensional modeling agent applied to the object to be applied is more preferably 5 μm or more and 100 μm or less. If the average thickness of each layer of the three-dimensional modeling agent applied to the object to be applied is within the more preferred range, it is advantageous in terms of suppressing the energy of the laser beam to be low and suppressing the deterioration of the three-dimensional modeling agent.

[0126] The three-dimensional modeling agent contains at least a curable material, and further contains other components as required.

[0127] --Curable material-- The curable material is not particularly limited as long as it is a compound that undergoes a polymerization reaction and is cured by irradiation with active energy rays (ultraviolet rays, electron beams, etc.), heating, etc., and can be appropriately selected depending on the purpose, and examples thereof include active energy ray curable compounds, thermosetting compounds, etc. Among these, materials that are liquid at room temperature are preferred. The active energy ray-curable compound is a monomer having a relatively low viscosity and a radically polymerizable unsaturated double bond in the molecular structure, and examples of the monomer include a monofunctional monomer and a polyfunctional monomer.

[0128] --Other ingredients-- The other components are not particularly limited and can be appropriately selected depending on the purpose. Examples of the other components include water, organic solvents, photopolymerization initiators, surfactants, colorants, stabilizers, water-soluble resins, low-boiling alcohols, surface treatment agents, viscosity modifiers, adhesion promoters, antioxidants, age resistors, crosslinking accelerators, ultraviolet absorbers, plasticizers, preservatives, and dispersants.

[0129] <Other steps and other means> The other steps are not particularly limited and may be appropriately selected depending on the purpose. Examples of the other steps include a supplying step, a three-dimensional modeling head unit scanning step, a step of adjusting the position of the object to be coated, and a control step.

[0130] <<Curing process and curing means>> The hardening step is a step of hardening a three-dimensional modeling agent serving as the transfer target material. The hardening means is a means for hardening a three-dimensional modeling agent serving as the transfer target material. The curing means is not particularly limited and can be appropriately selected depending on the purpose. For example, when the three-dimensional modeling agent is an ultraviolet curable material, an ultraviolet irradiator can be used. The curing step is not particularly limited and can be appropriately selected depending on the purpose. For example, if the three-dimensional modeling agent is an ultraviolet curable material, an ultraviolet ray irradiation step can be mentioned, and can be suitably carried out using an ultraviolet ray irradiation means.

[0131] <<3D modeling agent supplying process and 3D modeling agent supplying means>> The three-dimensional modeling agent supplying step is the same as the supplying step in the image forming method of the present invention, except that the transfer target material is a three-dimensional modeling agent, and therefore a description thereof will be omitted. The supplying means is the same as the supplying means in the image forming apparatus of the present invention, except that the transfer target material is a three-dimensional modeling agent, and therefore a description thereof will be omitted.

[0132] <<3D Modeling Head Unit Scanning Process and 3D Modeling Head Unit Scanning Means>> The three-dimensional modeling head unit scanning step is a step of scanning a three-dimensional modeling head unit, which is an integral unit of a flying unit and the curing means, in the width direction (X-axis) of the device above an object to be coated. The three-dimensional modeling head unit scanning means is a means for scanning a three-dimensional modeling head unit, which is an integral combination of a flying unit and the curing means, in the width direction (X-axis) of the device above an object to be coated. Furthermore, a plurality of the three-dimensional modeling head units may be provided.

[0133] <<Object position adjustment process and object position adjustment means>> The object position adjusting step is a step of adjusting the position of the object in the depth direction (Y axis) and height direction (Z axis) of the apparatus. The object position adjustment means is a means for adjusting the position of the object in the depth direction (Y axis) and height direction (Z axis) of the device. The object position adjusting means may be, for example, a base (stage) capable of adjusting the position of the object in the depth direction (Y axis) and height direction (Z axis) of the device.

[0134] <<Control process and control means>> The control process is the same as that of the image forming apparatus described above. The control means is the same as the control means of the image forming apparatus described above.

[0135] Next, an example of the apparatus for manufacturing a three-dimensional object will be described with reference to the drawings. The number, positions, shapes, etc. of the members of the apparatus for manufacturing a three-dimensional object are not limited to those in this embodiment, and may be any number, position, shape, etc. that is preferable for implementing the present invention.

[0136] FIG. 9 is an explanatory diagram showing an example of a manufacturing apparatus for a three-dimensional object. 9, the apparatus 500 for manufacturing a three-dimensional object includes a support substrate 122 for a model as an object to be treated, a stage 123, and a three-dimensional modeling head unit 130. The apparatus 500 for manufacturing a three-dimensional object manufactures a three-dimensional object 124 by laminating the applied three-dimensional modeling agent 22 while curing it. The three-dimensional modeling head unit 130 is disposed on the top of the three-dimensional object manufacturing apparatus 500, and can be scanned by a driving means in the direction indicated by the arrow L in Fig. 9. The three-dimensional modeling head unit 130 has a flying unit 120 and an ultraviolet irradiator 121 as a curing means.

[0137] The flying unit 120 is disposed at the center of the three-dimensional modeling head unit 130, and causes the transfer target material 20 to fly downward and be applied to the object support substrate 122 or the transfer target layer 20 that has already been hardened. The ultraviolet irradiators 121 are disposed on both sides of the flying unit 120 and irradiate the transfer target material 20 that has been flown by the flying unit 120 with ultraviolet light, thereby hardening the transfer target layer 20 . The object support substrate 122 is disposed at the bottom of the three-dimensional object manufacturing apparatus 500, and serves as a substrate when the three-dimensional object forming head unit 130 forms a layer of the three-dimensional object forming agent 22. The stage 123 is disposed below the object support substrate 122, and can move the object support substrate 122 in the vertical direction in Fig. 9 by a driving means. In addition, the stage 123 can be moved in the direction indicated by the arrow H in Fig. 9, and the gap between the 3D object modeling head unit 130 and the 3D object 124 can be adjusted.

[0138] In the image forming apparatus and the three-dimensional object manufacturing apparatus, an example in which the object to be treated (recording medium) is transported or moved has been shown, but the present invention is not limited to this. The object to be treated, etc. may be kept stationary and the flying unit, etc. may be moved. Alternatively, both the object to be treated and the flying unit, etc. may be moved. In addition, when an image is simultaneously formed over the entire surface of the object, both may be stationary at least during recording, with only the laser operating. EXAMPLES

[0139] Examples of the present invention will be described below, but the present invention is not limited to these examples.

[0140] (Example 1 of manufacturing material to be transferred) Transfer target material No. 1 (glycerol concentration 43% by mass) was prepared by adding 1 part by mass of spherical nano ferrite powder_M001 (manufactured by Powder Tech Co., Ltd.) as inorganic particles to a dispersion medium of the following composition for a total of 100 parts by mass of the dispersion liquid and inorganic particles and stirring. [Composition of dispersion medium] Vegetable glycerin 98% or more (manufactured by Natural Cosmetics Laboratory Co., Ltd.): 44 parts by weight ·Pure water: 56 parts by mass

[0141] (Example 2 of manufacturing material to be transferred) Transfer target material No. 2 (glycerol concentration 0% by mass) was prepared by adding 1 part by mass of spherical nano ferrite powder_M001 (manufactured by Powder Tech Co., Ltd.) as inorganic particles to a dispersion medium of the following composition for a total of 100 parts by mass of the dispersion medium and inorganic particles and stirring. [Composition of dispersion medium] ·Pure water: 100 parts by mass

[0142] (Example 3 of manufacturing transfer target material) Transfer target material No. 3 (glycerol concentration 32% by mass) was prepared by adding 1 part by mass of spherical nano ferrite powder_M001 (manufactured by Powder Tech Co., Ltd.) as inorganic particles to a dispersion medium of the following composition for a total of 100 parts by mass of the dispersion liquid and inorganic particles and stirring. [Composition of dispersion medium] Vegetable glycerin 98% or more (manufactured by Natural Cosmetics Laboratory Co., Ltd.): 33 parts by weight ·Pure water: 67 parts by mass

[0143] (Example 4 of manufacturing a transfer target material) Transfer target material No. 4 (glycerol concentration 52% by mass) was prepared by adding 1 part by mass of spherical nano ferrite powder_M001 (manufactured by Powder Tech Co., Ltd.) as inorganic particles to a dispersion medium of the following composition for a total of 100 parts by mass of the dispersion liquid and inorganic particles and stirring. [Composition of dispersion medium] Vegetable glycerin 98% or more (manufactured by Natural Cosmetics Laboratory Co., Ltd.): 53 parts by weight ·Pure water: 47 parts by mass

[0144] (Transfer target material manufacturing example 5) Transfer target material No. 5 (glycerol concentration 43% by mass) was prepared by adding 3 parts by mass of spherical nano ferrite powder_M001 (manufactured by Powder Tech Co., Ltd.) as inorganic particles to a dispersion medium of the following composition for a total of 100 parts by mass of the dispersion liquid and inorganic particles and stirring. [Composition of dispersion medium] Vegetable glycerin 98% or more (manufactured by Natural Cosmetics Laboratory Co., Ltd.): 44 parts by weight ·Pure water: 56 parts by mass

[0145] (Example 6 of manufacturing a transfer target material) Transfer target material No. 6 (glycerol concentration 43% by mass) was prepared by adding 5 parts by mass of spherical nano ferrite powder_M001 (manufactured by Powder Tech Co., Ltd.) as inorganic particles to a dispersion medium of the following composition for a total of 100 parts by mass of the dispersion liquid and inorganic particles and stirring. [Composition of dispersion medium] Vegetable glycerin 98% or more (manufactured by Natural Cosmetics Laboratory Co., Ltd.): 44 parts by weight ·Pure water: 56 parts by mass

[0146] (Example 7 of manufacturing a transfer target material) Transfer target material No. 7 (glycerol concentration 87% by mass) was prepared by adding 1 part by mass of spherical nano ferrite powder_M001 (manufactured by Powder Tech Co., Ltd.) as inorganic particles to a dispersion medium of the following composition for a total of 100 parts by mass of the dispersion liquid and inorganic particles, and stirring. [Composition of dispersion medium] Vegetable glycerin 98% or more (manufactured by Natural Cosmetics Laboratory Co., Ltd.): 88 parts by weight ·Pure water: 12 parts by mass

[0147] (Example 8 of manufacturing material to be transferred) Transfer target material No. 8 (glycerol concentration 98% by mass) was prepared by adding 1 part by mass of spherical nano ferrite powder_M001 (manufactured by Powder Tech Co., Ltd.) as inorganic particles to a dispersion medium of the following composition for a total of 100 parts by mass of the dispersion liquid and inorganic particles, and stirring. [Composition of dispersion medium] Vegetable glycerin 98% or more (manufactured by Natural Cosmetics Laboratory Co., Ltd.): 99 parts by weight ·Pure water: 1 part by mass

[0148] Next, for each of the transfer target materials prepared, the median diameter (D 50 ) and complex viscosity at 25° C. and a shear stress of 200 Pa were measured. The results are shown in Table 1.

[0149] <Median diameter (D 50 ) Measurement> Median diameter (D 50 The median diameter (D) was measured using a scanning electron microscope (SU8200 series, Hitachi High-Technologies Corporation). The obtained image was binarized using image processing software A-zo-kun (Asahi Kasei Engineering Co., Ltd.) and the median diameter (D 50 ) was calculated.

[0150] <Complex viscosity measurement at 25℃ and shear stress of 200Pa> The complex viscosity was measured under the following conditions using a dynamic viscoelasticity measuring device with a stress control method in which the applied stress is changed and the amount of strain generated is measured. Figure 11 shows the relationship between the glycerol concentration (mass%) and the complex viscosity (mPa s) for transfer target materials No. 1 to 8. -Measurement conditions- - Instrument name: Rheometer, HAAKE RheoStress 600, Thermo Fisher Scientific ·Temperature: 25℃ Shear stress: 200Pa

[0151] [Table 1]

[0152] Details of each component in Table 1 are as follows. *M001: Spherical nano ferrite powder_M001, iron ferrite, manganese ferrite, manufactured by Powder Tech Co., Ltd. *Glycerol: 98% or more vegetable glycerin, manufactured by Natural Cosmetics Laboratory Co., Ltd.

[0153] The results in Table 1 and Figure 11 show that as the glycerol concentration increases, the complex viscosity of the material to be transferred increases, and that the complex viscosity of the material to be transferred at 25°C and a shear stress of 200 Pa varies in the range of 1 mPa·s to 752 mPa·s.

[0154] (Donor Substrate Manufacturing Examples 1 to 8) Next, each of the obtained transfer target materials was applied using a bar coater onto one side of a slide glass (micro slide glass S7213, manufactured by Matsunami Glass Industry Co., Ltd.; transmittance of 532 nm wavelength light is 99%) to produce donor substrates 1 to 8 having a transfer target layer with an average thickness of 26 μm (variation range: 20 to 29 μm).

[0155] (Examples 1 to 7 and Comparative Examples 1 to 3) Next, a transfer method was carried out by combining the transfer target material and laser irradiation shown in Table 2. In this example, a laser beam having a pulse width of 10 ns and a pulse frequency of 50 Hz was used. In addition, the experiment was carried out with the distance between the object and the transfer target material being 1.2 mm or more and 1.5 mm or less. In some of the present examples, measurements were performed using the experimental apparatus shown in Figures 10A and 10B. Here, a Canon galvanometer scanner GM-1015 was installed between the focal length of the condenser lens and the light was scanned through the condenser lens, and the focus was set to coincide with the transfer target layer. 10A and 10B are schematic diagrams showing an example of a laser irradiation device having an optical vortex laser beam used in the examples and comparative examples. The experimental apparatus shown in FIGS. 10A and 10B includes a pulsed laser 131 (wavelength: 532 nm, 50 Hz, 10 ns), a spatial light modulator 132, a mirror 133, a quarter-wave plate 134, a focusing lens 135, a galvano scanner 136, glass 137, and a receptor 138. In Figure 10A, a pulsed laser with a wavelength of 532 nm and a nanosecond pulse (approximately 10 ns) was used as the laser light source, and an optical vortex laser beam was generated by controlling the orbital angular momentum and spin angular momentum with a spatial light modulator (SLM) and a quarter-wave plate (QWP). The optical vortex laser beam was focused with a focusing lens, and a Canon galvanometer scanner GM-1015 was placed between the focusing lens and the focal length and set to focus on the layer to be transferred. The optical vortex laser beam was then irradiated onto the layer to be transferred from the substrate side of the donor substrate. In Figure 10B, a pulsed laser with a wavelength of 532 nm and a nanosecond pulse (approximately 10 ns) was used as the laser light source. This was then converted into an optical vortex laser beam by a spatial light modulator (SLM), which was then bounced into the air by a mirror and passed through a quarter-wave plate (QWP) to control the spin angular momentum to generate an optical vortex laser beam. The optical vortex laser beam was then focused by a focusing lens so that it was focused on the layer to be transferred, and the optical vortex laser beam was irradiated onto the layer to be transferred from the substrate side of the donor substrate. The only difference between the two is whether or not optical scanning is performed using a galvano scanner device, and there is no effect on the special properties of the light, etc. Therefore, it can be selected appropriately according to the purpose. In this study, a condenser lens was placed in front of the galvano scanner, and lenses with focal lengths of 125 mm to 300 mm were used.

[0156] Figure 12 shows the behavior of the transfer target material No. 1 (glycerol concentration 43 mass%, complex viscosity 6 mPa·s) when irradiated with an optical vortex laser beam. The optical vortex laser beam is irradiated upward from the bottom surface of Figure 12. From the results in Figure 12, after 3.0 μsec of laser irradiation, the inorganic particles in the transfer target material gather in the center and a liquid column grows with high directionality while rotating, a phenomenon known as a "spin jet." This "spin jet" is thought to be generated by the circular intensity profile of the optical vortex laser beam and the transfer of orbital angular momentum.

[0157] Figure 13A is a photograph showing an example of the state in which the material to be transferred (hereinafter referred to as a dot) has been transferred to an object to be treated (S1214, water-polished edge, t1.3, manufactured by Matsunami Glass Industry Co., Ltd.) placed 1.5 mm away from the material to be transferred, and then heated at 300°C to remove the dispersion medium in the material to be transferred. FIG. 13B is a schematic diagram showing an example of a 3D image obtained by measuring FIG. 13A using a confocal laser microscope.

[0158] In this example, experiments were conducted using a circularly polarized optical vortex laser beam, and the total angular momentum J could be changed arbitrarily. No effect of the value of J on the accuracy of the core formation position was confirmed. On the other hand, changes in the total angular momentum caused differences in the shape of the core and the shape of the transferred dots. Figures 14A and 14B show dots obtained by irradiating an optical vortex laser beam with a total angular momentum of J = 2 (L = 1, S = 1). Figure 14A is a top photograph of the dot, and Figure 14B is a cross-sectional photograph of the side of the dot. The arrow in Figure 14A indicates the direction of rotation of the dot core. Figures 15A and 15B show dots obtained by irradiating an optical vortex laser beam with a total angular momentum of J = -2 (L = -1, S = -1). Figure 15A is a top photograph of the dot, and Figure 15B is a cross-sectional photograph of the side of the dot. The arrow in Figure 15A indicates the direction of rotation of the dot's center (core). In both cases, the core located in the center of the dot is twisted and rotates in opposite directions, which is thought to be the effect of the optical vortex laser beam. Although the experimental conditions are different from those of this example, Figure 16 shows the relationship between the dot diameter (△) and the core diameter (○) when the total angular momentum J is changed by the spin angular momentum S. It can be confirmed that a core is formed under all conditions, but as J becomes smaller, there is a tendency for disturbance to occur on the periphery of the dot, which is due to the influence of the momentum of the optical vortex laser beam.

[0159] Figure 17A shows an example of an observation image using a scanning electron microscope (SEM) of a dot transferred to an object placed 1.5 mm away from the transfer target material using the transfer target material No. 1, after the dispersion medium in the transfer target material was removed by heat treatment at 300°C. A core can be confirmed in the center of the dot in Figure 17A. FIG. 17B is an example of an SEM observation image of the processed product of FIG. 17A, in which the core is sliced ​​using a focused ion beam device (FIB). FIG. 18A is an example of a bright-field image of FIG. 17A observed using a transmission electron microscope. FIG. 18B is an example of an electron diffraction pattern obtained from the position a in FIG. 18A. FIG. 18C is an example of a dark-field image obtained from the electron beam diffraction spot surrounded by the white circle in FIG. 18B, which shows crystalline regions having the same zone axis. FIG. 18D is an example of an electron diffraction pattern obtained from position b in FIG. 18A. FIG. 18E is an example of a dark-field image obtained from the electron diffraction spot circled in FIG. 18D, which shows crystalline regions with identical zone axes. FIG. 18F shows the correspondence between the regions shown in FIGS. 18C and 18E and FIG. 18A. The core is formed from two single crystals, and the crystal with the most region has more than 90% of the crystals having the same zone axis.

[0160] The crystal structure of the obtained core was analyzed using the open source software (ReciPro) for indexing and simulation of single crystal electron diffraction patterns, which was released by Professor Seto of Hokkaido University. FIG. 19A is an electron diffraction pattern obtained from the area of ​​FIG. 18C. FIG. 19B is an electron diffraction pattern of a spinel crystal (iron ferrite) with Miller indices (122) simulated from ReciPro. FIG. 19C is an electron diffraction pattern obtained from the area of ​​FIG. 18E. FIG. 19D is an electron diffraction pattern of a spinel crystal (iron ferrite) with Miller indices (100) simulated from ReciPro. Figure 19E shows a comparison of the ratios and angles between the diffraction spots a to e shown in Figures 19A to D, which match with a very high degree of accuracy, indicating that the core is composed of two spinel crystals (Figure 19F) with different zone axes.

[0161] FIG. 20A is a photograph showing an example of a bright-field image of FIG. 17A observed using a transmission electron microscope. The white circle a in FIG. 20A is located on the boundary between the regions of different zone axes shown in FIG. 18C and FIG. 18E, and indicates the region from which FIG. 20B, which is an electron diffraction pattern in Miller indices (100), was obtained. If the axes a and b inserted in FIG. 20B are taken as axes, the diffraction spots that should be aligned in a square lattice are tilted by about ±4°, and it can be seen that the crystals grow in a distorted state with respect to the b-axis direction. On the other hand, the a-axis direction is aligned at equal intervals. This is thought to have occurred because the two crystals that form the core have a flat reference on a very fine scale, and it is assumed that the object to which the coating is applied may play this role. From these points of view, it is preferable that the surface of the object to which the coating is applied is smooth.

[0162] FIG. 21A is an image of dots formed using transfer target material No. 1, observed with a scanning electron microscope. Fig. 21B is an example of the distribution of iron (Fe) obtained by elemental analysis, which is mapped on Fig. 21A. Fig. 21C is an example of the distribution of manganese (Mn) obtained by elemental analysis, which is mapped on Fig. 21A. While iron is detected throughout the sample, manganese tends to be detected only in the outer frame, which is likely due to differences in crystallinity.

[0163] FIG. 22A is a diagram showing an example of patterning using the experimental system of FIG. 10A. First, using the experimental system of Figure 10A, the galvano scanner 136 was scanned in the X-axis direction in Figure 10A, and the dots were continuously transferred to a recipient (receiver 138) placed 0.6 mm away from the material to be transferred so that the dot spacing was 100 μm. FIG. 22A shows an example of a state in which the above transfer is repeated for two rows, and the resulting dots are heat-treated at 300° C. to remove the dispersion medium from the transfer target material.

[0164] Figure 22B is a photograph showing the beam irradiation position in Figure 22A with a dashed circle. From this result, the center of gravity of the dot and the center of gravity of the beam irradiation position can be determined, and the deviation of the dot from the beam irradiation position (hereinafter referred to as position error) can be estimated.

[0165] FIG. 22C shows an example of the relationship between the position error of an optical vortex and the dot diameter when the distance between the material to be transferred and the object to be coated is changed from 0.6 mm to 1.4 mm, and for comparison, the relationship between the position error of a general laser beam and the dot diameter when the distance between the material to be transferred and the object to be coated is set to 1.2 mm. According to Figure 22C, when using an optical vortex, the position error is about half that of when using a general laser beam. Furthermore, with an optical vortex, the position error can be suppressed to a few μm by setting the distance between the transfer material and the object to be transferred to 0.6 mm or less, enabling transfer with extremely high precision. It was also confirmed that the emission angle when using an optical vortex is approximately 0.8 deg, independent of the distance between the material to be transferred and the object to be annexed.

[0166] Below, a comparison is shown using transfer target material No. 1 in which a core is formed and transfer target materials No. 7 and No. 8 in which a core is not formed. FIG. 23A shows the relationship between each fluence and flight speed (flight speed of the jet head or leading droplet within the field of view) when using the No. 1 transfer target material, the film thickness of the transfer target material is 20 μm, and the beam spot diameter is 49 μm. Figure 23B-E shows the four confirmed flight modes (B: single droplet flight, C: multiple droplet flight, D: jet flight with expansion, E: scattering), and the fluence was 0.16 [J / cm 2 ], 0.21 [J / cm 2 ], 0.42 [J / cm 2 ], 0.72 [J / cm 2 In this case, the core is formed reproducibly in the case of single droplet flight and multiple droplet flight, and the fluence is 0.16 [J / cm 2 ] or more 0.27[J / cm 2 ] or less, and the condition for no dust to occur around the transferred dot is a single droplet flight, and the fluence is 0.16 [J / cm 2 ] or more 0.18[J / cm 2 ] or less is more preferable. In addition, the fluence range for single droplet flight for a film thickness of 20 μm is approximately 0.02 to 0.03 [J / cm 2 ], but as the film thickness increases, the width of the fluence at which a single droplet can fly remains almost unchanged, and the threshold fluence shifts in the larger direction. When the film thickness is 28 μm, the fluence threshold for a single droplet to fly is 0.27 [J / cm 2 ] or more 0.28[J / cm 2 ] or less, and it can be seen that the width of the valid fluence does not change significantly, and only the threshold value shifts. This change is predicted to change continuously with film thickness, and the same tendency is observed for other flight modes.

[0167] FIG. 24A shows the relationship between each fluence and the flight speed (the flight speed of the jet head or the leading droplet within the field of view) when using the No. 7 transfer target material, the film thickness of the transfer target material is 20 μm, and the beam spot diameter is 49 μm. Figure 24B-E shows the four confirmed flight modes (B: single droplet flight, C: multiple droplet flight, D: jet flight with expansion, E: scattering), and the fluence was 0.36 [J / cm 2 ], 0.51 [J / cm 2 ], 1.52 [J / cm 2 ], 4.08 [J / cm 2 In this case, the core is formed reproducibly in the case of single droplet flight and multiple droplet flight, and the fluence is 0.36 [J / cm 2 ] or more 0.72[J / cm 2 ] or less, and the condition for no dust to occur around the transferred dot is a single droplet flight, and the fluence is 0.36 [J / cm 2 ] or more 0.42[J / cm 2 ] or less is more preferable. In addition, the fluence range for single droplet flight for a film thickness of 20 μm is approximately 0.05 to 0.06 [J / cm 2 ], but as the film thickness increases, the range of fluences at which a single droplet can fly remains almost unchanged, and the threshold fluence shifts toward a larger value. When the film thickness is 29 μm, the fluence threshold for single droplet flight is 0.57 [J / cm 2 ] or more 0.65[J / cm 2 ] or less, and it can be seen that the width of the valid fluence does not change significantly, and only the threshold value shifts. This change is predicted to change continuously with film thickness, and the same tendency is observed for other flight modes.

[0168] Figure 25A shows the relationship between each fluence and flight speed (flight speed of the jet head or the leading droplet within the field of view) when using the No. 8 transfer target material, the film thickness of the transfer target material is 20 μm, and the beam spot diameter is 49 μm. Figures 25B to 25E show the four confirmed flight modes (B: single droplet flight, C: multiple droplet flight, D: flight by a jet with expansion, E: scattering), and the fluence is 0.53 [J / cm 2 ], 0.65 [J / cm 2 ], 0.99 [J / cm 2 ], 4.08 [J / cm 2In this case, the core is formed reproducibly in the case of single droplet flight and multiple droplet flight, and the fluence is 0.53 [J / cm 2 ] or more 0.72[J / cm 2 ] or less, and the condition for no dust to occur around the transferred dot is a single droplet flight, and the fluence is 0.53 [J / cm 2 ] or more 0.58[J / cm 2 ] or less is more preferable. In addition, the fluence range for single droplet flight for a film thickness of 20 μm is approximately 0.05 to 0.06 [J / cm 2 ], but as the film thickness increases, the width of the fluence at which a single droplet can fly remains almost unchanged, and the threshold fluence shifts in the larger direction. When the film thickness is 29 μm, the threshold fluence for a single droplet to fly is 0.87 [J / cm 2 ] or more 0.93[J / cm 2 ] or less, and it can be seen that the width of the valid fluence does not change significantly, and only the threshold value shifts. This change is predicted to change continuously with film thickness, and the same tendency is observed for other flight modes.

[0169] Figure 26 shows an example of the relationship between the complex viscosity of the material to be transferred and dots transferred to an object placed 1.5 mm away from the material to be transferred using Figures 23B, 24B, and 25B, after the dots have been heat-treated at 300°C to remove the dispersion medium in the material to be transferred.

[0170] The dot formed in FIG. 23B has a diameter of about 14 μm, and inorganic particles gather in the center to form a core with a diameter of about 4 μm, forming a dot that is much smaller than the beam spot.

[0171] The dots formed in the donor of FIG. 24B were approximately 25 μm in diameter, with a domain of loosely aggregated inorganic particles in the center.

[0172] In the donor of Fig. 25B, dots were obtained in which inorganic particles were uniformly distributed in a circular area with a diameter of about 20 [μm] and a radius of 10 μm. It can be seen that the lower the complex viscosity of the material to be transferred, the more the inorganic particles are concentrated near the center of the dot.

[0173] Here, the spatial distribution of inorganic particles in the three dots shown in FIG. 26 was quantitatively evaluated.

[0174] Figure 27A shows an image of the analysis method, where RD [μm] is the distance from the center of gravity of the dot to the outer periphery of the dot, RGn [μm] is the distance from the center of the dot to the center of gravity of each magnetic particle (filled domain), and (RGn / RD)*100[%] is defined. This defined region was divided into circular regions with 5% intervals (circular regions in Figure 27A), the sum of the magnetic particle domains with the center of gravity in this region was calculated, and the area ratio of the magnetic particle domains in each region was calculated to create a histogram.

[0175] Figure 27B shows the spatial distribution of dots obtained using transfer target material No. 1, Figure 27C shows the spatial distribution of dots obtained using transfer material No. 7, and Figure 27D shows the spatial distribution of dots obtained using transfer material No. 8. From this result, it is understood that as the complex viscosity of the material to be transferred decreases, the position at which the ratio of the inorganic particle domains reaches its peak shifts to the center of the dot. For a more specific comparison, we calculated (RGn / RD)*100[%], where the accumulation of inorganic particle domains would be 60% of the total, and the results were ~8[%] for transfer material No. 1, ~40[%] for transfer material No. 7, and ~53[%] for transfer material No. 8. It should be noted that in the transfer material No. 8, 60% of the cumulative area of ​​the inorganic particle domain is located at the center of the dot radius, and the inorganic particles are distributed relatively uniformly, while in the transfer material No. 1, more than half of the inorganic particles are concentrated near the center and localized. From this result, it is clear that the lower the complex viscosity of the transfer target material, the more the inorganic particles are concentrated near the center of the dot. This is thought to be because a spiral central force acts on the inorganic particles due to the in-plane radiation force caused by the forward scattering force of the optical vortex laser beam and the radial radiation force caused by the total angular momentum, which promotes the movement of the inorganic particles, but the movement of the inorganic particles is hindered by the increase in the complex viscosity of the transfer target material.

[0176] The spatial distribution of inorganic particles in a droplet of the material to be transferred can be analyzed as follows. The area S of the dot in FIG. All [μm 2 The area of ​​the dot [μm] was calculated by selecting the edge of the droplet using the polygon selection tool of the image analysis software ImageJ. 2 ] and the center of gravity of the dot [X DG , Y DG ] was decided. The area of ​​each inorganic particle in FIG. 27A was measured using the binary image creation function of ImageJ or the binary processing function of the image analysis software "A-zo-kun" manufactured by Asahi Kasei Engineering Corporation. The area of ​​each inorganic particle obtained [μm 2 ], and the center of gravity position is [X Gn , Y Gn ]. The image analysis software used was the free image analysis software ImageJ and the image analysis software "Azo-kun" manufactured by Asahi Kasei Engineering Corporation.

[0177] R G is the center of gravity of the droplet [X DG , Y DG ] and the center of gravity of each inorganic particle [X Gn , Y Gn ] is calculated using Pythagoras' theorem and is expressed by the following formula (A).

number

[0178] The radius of the dot RD [μm] is the area of ​​the dot S All [μm 2 ] and is expressed by the following formula (B).

number

[0179] The center of gravity of the inorganic particle domain [X Gn , Y Gn The degree of distance from the dot is defined as (RGn / RD)*100, and the farthest position where the magnetic particles are distributed corresponds to the outer periphery of the dot, and is expressed as (RGn / RD)*100=100[%]. Here, to compare the spatial distribution of magnetic particles within a dot, we set a circular region (the circular region in Fig. 27A) represented by r≦(RGn / RD)*100 < r+5 [%], and defined the circular region in increments of r=5n (n=0 to 19). We calculated the area ratio for each circular region by adding the area of ​​the magnetic particle domain with the center of gravity in the circular region and normalizing it by the area of ​​the circular region.

[0180] The above formulas (A) and (B) are used to create the histograms in Figures 13B to 15B. Below, a method for calculating the accumulation and a method for calculating the histogram will be described.

[0181] - Calculation of cumulative amount - Dot centroid [X DG , Y DG The length from the radius RGn to the circle equivalent diameter RD is defined as 100%, and (RGn / RD)*100 is defined. Inorganic particle area [μm 2 The sum of these values ​​was set to 100%, and the (RGn / RD)*100 values ​​were added in order from the smallest to the largest, and the (RGn / RD)*100 value corresponding to the particle with a cumulative total of 60% was evaluated.

[0182] --Histogram calculation-- The sum of the areas of magnetic particle domains having their center of gravity in a circular region represented by r≦(RGn / RD)*100 < r+5 [%] is calculated for each circular region, and then normalized by the area of ​​the circular region to calculate the area ratio for each circular region, thereby obtaining the histograms in Figures 27B to 27D.

[0183] Therefore, it can be seen that the LIFT method using an optical vortex laser (OV-LIFT) makes it possible to control the spatial distribution of inorganic particles in droplets of the material to be transferred by controlling the complex viscosity of the material to be transferred.

[0184] Figure 28A shows the relationship between the dot diameter and the core diameter when the No. 1 transfer material is used, the film thickness of the transfer target material is 26 μm, and the beam spot diameter is 34 μm, 49 μm, 74 μm, and 97 μm. At this time, the focusing lens is changed from f = 125 to 300 mm to obtain the target beam spot size. Here, the beam diameter is the interval between the peak positions with the singular point of the energy density distribution as the target center, and was calculated based on the following formulas (C) and (D) for the radial intensity distribution in the optical vortex, and the following formula (E) for the intensity peak position.

number

number

number

[0185] Figure 28B shows an example of the relationship between the volume of dots and the height of the magnetic core obtained when the beam spot diameter is set to 34 μm, 49 μm, 74 μm, and 97 μm. As shown in Figure 28B, it can be seen that the volume of the dot is proportional to the square of the beam spot diameter (irradiation area). On the other hand, the height of the magnetic core changes depending on the beam spot diameter, but the variation is very small at less than 1 μm. From these results, it can be confirmed that the dots and magnetic cores obtained change depending on the beam spot diameter.

[0186] Figure 29A shows an example of the time change of bubble growth (cavitation) up to 3.0 μs after laser irradiation. Figure 29B shows the change in internal pressure during this cavitation process calculated from the Rayleigh-Plesset equation (equation (G) below).

number

[0187] <Displacement of the core dot from the center of gravity> The droplets on the object were observed using a microscope, and the values ​​were calculated using the method shown below. Figure 30A shows a simplified diagram of the analysis method. The dot images obtained by microscopy were analyzed by selecting the edges of the dots using the polygon selection tool of the image analysis software ImageJ, and the area of ​​the dots [μm 2 ] and the center of gravity of the dot [X ドット , Y ドット The radius of the dot was calculated using formula (B). Next, the center of gravity of the core was determined by selecting the edge of the core using the polygon selection tool of the image analysis software ImageJ from the dot image obtained by microscopy [X コア , Y コア ] was decided.

[0188] The deviation of the core from the center of gravity of the dot was calculated using the following formula (F).

number

[0189] FIG. 30B shows the results of an experiment conducted uniformly using transfer material No. 1, comparing Example 1, Example 5, Example 6, Example 7, Comparative Example 1, Comparative Example 2, and Comparative Example 3.

[0190] [Table 2]

[0191] The results in Table 2 reveal that the crystal formation method of the present invention using an optical vortex laser beam can strongly focus an optical absorber that absorbs an optical vortex laser beam of a specified wavelength, and place the core formed at the center of the dot, making it possible to align the cores with greater precision.

[0192] For example, aspects of the present invention are as follows. <1> A crystal formation process includes irradiating a light vortex laser beam from the substrate side of a donor substrate, the donor substrate having a substrate and a transfer target material including a light absorbing material and a dispersion medium disposed thereon, onto the transfer target material, so that the transfer target material is caused to fly as a flying object and applied to an object to be applied, thereby forming a crystal; the complex viscosity of the material to be transferred at 25°C and a shear stress of 200 Pa is 1 mPa s or more and 8.6 mPa s or less; The crystal formation method is characterized in that the ten-point average roughness Rz of the object to be treated is 4.9 μm or less. <2> The ten-point average roughness Rz of the object to be treated is 0.007 μm or more and 1.5 μm or less. <1> The crystal formation method is as described above. <3> The light absorbing material comprises an inorganic material. <1> from <2> The present invention relates to a method for producing crystals according to any one of the above. <4> The median diameter (D 50 ) is 50 nm or more and 500 nm or less. <3> The crystal formation method is as described above. <5> The light absorbing material comprises two or more different inorganic materials; The two or more different inorganic materials are made of substances having the same crystal structure. <1> from <4> The present invention relates to a method for forming crystals according to any one of the above. <6> The dispersion medium is an aqueous glycerol solution. <1> from <5> The present invention relates to a method for forming crystals according to any one of the above. <7> 80% or more of the formed crystals are single crystals, <1> from <6> The present invention relates to a method for forming crystals according to any one of the above. <8> a crystal forming means for forming a crystal by irradiating an optical vortex laser beam from the substrate side of the donor substrate to the transfer target material, the transfer target material being transferred as a transfer body to a target object, the transfer target material being transferred to the target object by flying the transfer target material as a transfer body; the complex viscosity of the material to be transferred at 25°C and a shear stress of 200 Pa is 1 mPa s or more and 8.6 mPa s or less; A crystal forming apparatus, characterized in that the ten-point average roughness Rz of the object to be treated is 4.9 μm or less. <9> The ten-point average roughness Rz of the object to be treated is 0.007 μm or more and 1.5 μm or less. <8> The crystal formation apparatus according to claim 1 . <10> The above <1> from <7> 2. An image forming method, comprising forming an image by the crystal forming method according to any one of claims 1 to 11. <11> The above <1> from <7> 13. A method for producing a three-dimensional object, comprising the steps of:

[0193] The above <1> from <7> The crystal formation method according to any one of the preceding claims. <8> from <9> The crystal formation apparatus according to any one of the preceding claims. <10> The image forming method according to the <11> According to the method for manufacturing a three-dimensional object described above, the conventional problems can be solved and the object of the present invention can be achieved. [Explanation of symbols]

[0194] 1 Flight means 11 Laser Beam 12. Optical Vortex Laser Beam 20 Transfer target material (transfer target layer) 30 Grantee 31 Recording media 32 Substrate 40 Donor Substrate 300, 301, 301a Projectile transfer device 302~307 Image forming equipment 400, 401 Image forming apparatus 500 Three-dimensional object manufacturing equipment [Prior art documents] [Patent documents]

[0195] [Patent Document 1] Patent No. 6455588

Claims

1. A crystal formation process includes irradiating a light vortex laser beam from the substrate side of a donor substrate, the donor substrate having a substrate and a transfer target material including a light absorbing material and a dispersion medium disposed thereon, onto the transfer target material, so that the transfer target material is caused to fly as a flying object and applied to an object to be applied, thereby forming a crystal; The complex viscosity of the material to be transferred at 25° C. and a shear stress of 200 Pa is 1 mPa·s or more and 8.6 mPa·s or less; The method for forming crystals, characterized in that the ten-point average roughness Rz of the object to be treated is 4.9 μm or less.

2. 2. The method for forming crystals according to claim 1, wherein the ten-point average roughness Rz of the object to be treated is 0.007 μm or more and 1.5 μm or less.

3. The crystal formation method according to claim 1 , wherein the light absorbing material comprises an inorganic material.

4. The median diameter (D 50 4. The method for forming crystals according to claim 3, wherein the diameter of the crystal is 50 nm or more and 500 nm or less.

5. The light absorbing material comprises two or more different inorganic materials; 3. The method for forming crystals according to claim 1, wherein the two or more different inorganic materials are made of substances having the same crystal structure.

6. The method for forming crystals according to claim 1 , wherein the dispersion medium is an aqueous glycerol solution.

7. 3. The method for forming crystals according to claim 1, wherein 80% or more of the formed crystals are single crystals.

8. a crystal forming means for forming a crystal by irradiating an optical vortex laser beam from the substrate side of the donor substrate to the transfer target material, the transfer target material being transferred as a transfer body to a target object, the transfer target material being transferred to the target object by flying the transfer target material as a transfer body; The complex viscosity of the material to be transferred at 25° C. and a shear stress of 200 Pa is 1 mPa·s or more and 8.6 mPa·s or less; A crystal forming apparatus, characterized in that the ten-point average roughness Rz of the object to be treated is 4.9 μm or less.

9. The crystal formation apparatus according to claim 8, wherein the ten-point average roughness Rz of the object to be treated is 0.007 μm or more and 1.5 μm or less.

10. 3. An image forming method, comprising forming an image by the crystal forming method according to claim 1.

11. A method for producing a three-dimensional object, comprising the steps of: producing the three-dimensional object by the crystal formation method according to claim 1 or 2.

Citation Information

Patent Citations

  • Driving of liquid crystal display device

    JP1989055588A