Bonding method and bonding system

The bonding method and system address the issue of recess control in metal wiring by using plasma treatment and controlled hydrophilization with pH/ORP adjustments, achieving improved bonding quality and consistency.

JP2024148358APending Publication Date: 2024-10-18TOKYO ELECTRON LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023061426
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-05
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Conventional bonding systems fail to adequately control the recess amount of metal wiring on substrates, leading to insufficient bonding quality and variations in the bonding process.

Method used

A bonding method and system that uses plasma treatment to modify substrate surfaces, followed by hydrophilization with controlled application of a treatment liquid to adjust the recess amount of metal materials, utilizing pH and ORP adjustments to prevent corrosion and ensure precise bonding.

Benefits of technology

Improves the bonding quality between substrates by precisely controlling the recess amount of metal wiring, enhancing the bonding strength and preventing corrosion, thus ensuring consistent and robust intermolecular forces.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024148358000001_ABST
    Figure 2024148358000001_ABST
Patent Text Reader

Abstract

To improve the quality of bonding between substrates forming a polymerized substrate.SOLUTION: A bonding method for bonding substrates with exposed metal material on their surfaces includes the steps of modifying the surfaces of substrates to be bonded by plasma of process gas, hydrophilizing the surface of the modified substrate, and bonding the surfaces of the hydrophilic substrates together, and in the process for hydrophilization, a processing solution is supplied to the surface of the substrate, and the amount of recesses in the metallic material is controlled by the processing solution.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a bonding method and a bonding system. [Background technology]

[0002] Patent Document 1 discloses a bonding system for bonding substrates together by intermolecular forces. The bonding system includes a surface modification device for modifying the surfaces of the substrates, a hydrophilization device for hydrophilizing the modified substrate surfaces, and a bonding device for bonding the hydrophilized substrates together. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-073455 A Summary of the Invention [Problem to be solved by the invention]

[0004] The techniques disclosed herein improve the bonding quality between the substrates that form the laminated substrate. [Means for solving the problem]

[0005] One aspect of the present disclosure is a method for bonding substrates having exposed metal material on their surfaces, comprising the steps of modifying the surfaces of the substrates to be bonded with plasma of a processing gas, hydrophilizing the modified surfaces of the substrates, and bonding the hydrophilized surfaces of the substrates together, wherein the hydrophilization step includes supplying a processing liquid to the surfaces of the substrates and controlling the amount of recess in the metal material by the processing liquid. Effect of the Invention

[0006] According to the present disclosure, the bonding quality between the substrates forming the laminated substrate is improved. [Brief description of the drawings]

[0007] [Figure 1] 1 is an explanatory diagram showing a recess formed on a wafer surface by recess processing; [Diagram 2] 1 is a plan view showing an outline of a configuration of a joining system according to an embodiment of the present invention. [Diagram 3] FIG. 2 is a side view showing an outline of the configuration of an upper wafer and a lower wafer. [Figure 4] 1 is a cross-sectional view showing an outline of the configuration of a surface modification device. [Diagram 5] FIG. 1 is a cross-sectional view showing an outline of the configuration of a surface hydrophilization device. [Figure 6] FIG. 2 is a cross-sectional view showing an outline of the configuration of a joining device. [Figure 7] 1A to 1C are explanatory views showing main steps of wafer processing. [Figure 8] FIG. 1 is an explanatory diagram showing (a) a surface modification treatment and (b) a surface hydrophilization treatment. [Figure 9] FIG. 1 is a Pourbaix diagram of copper as a metal wiring. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] In 3D integration technology for stacking semiconductor devices in three dimensions, two semiconductor wafers (hereinafter simply referred to as "wafers") with insulating films and metal wiring exposed on their surfaces are bonded together. A wafer is an example of a substrate. In a bonding system that performs the bonding process, a surface modification process and a surface hydrophilization process are sequentially performed on the surfaces of the wafers to be bonded, and then the wafers are bonded together, for example, by van der Waals forces and hydrogen bonds (intermolecular forces). The bonding system disclosed in Patent Document 1 is provided with various processing devices for performing the surface modification process, surface hydrophilization process, and bonding process.

[0009] The laminated wafer thus formed by bonding the wafers together is then subjected to a heating (annealing) process to increase the bonding strength between the wafers. In this heating process, the metal wiring exposed on the wafer surface expands thermally, and in order to prevent damage to the metal wiring due to the expansion, the surface height of the metal wiring (Cu in the illustrated example) formed on the surface of the wafer (Si in the illustrated example) is made lower (recessed) in advance compared to the surface height of the insulating film (SiO in the illustrated example), as shown in Fig. 1.

[0010] However, because this recessing is performed in advance outside the bonding system, for example, in the bonding system disclosed in Patent Document 1, even if the recess amount is insufficient or the recess amount varies within the wafer surface, it is not possible to adjust this prior to bonding. Therefore, there is room for improvement in conventional bonding systems.

[0011] The technology disclosed herein improves the bonding quality between substrates that form an overlapped substrate. Hereinafter, a bonding method according to the present embodiment and a bonding system that realizes the bonding method will be described with reference to the drawings. In this specification and the drawings, elements having substantially the same functional configurations are denoted by the same reference numerals, and duplicated descriptions will be omitted.

[0012] <Configuration of the joining system> First, the configuration of the bonding system according to this embodiment will be described. Fig. 2 is a plan view showing an outline of the configuration of the bonding system 1. In the following description, in order to clarify the positional relationship, the X-axis direction, the Y-axis direction, and the Z-axis direction which are mutually orthogonal are defined, and the positive direction of the Z-axis is defined as the vertical upward direction.

[0013] In the bonding system 1, wafers W as substrates shown in FIG. 3 are bonded together. Hereinafter, the wafer placed on the upper side in the bonding apparatus described later is referred to as the "upper wafer W". U The wafer placed on the bottom is called the "lower wafer W L " Also, the upper wafer W U In the lower wafer W L The surface to be joined is called "surface W U1" and the opposite side is called "Back W U2 Similarly, the lower wafer W L In the upper wafer W U The surface to be joined is called "surface W L1 " and the opposite side is called "Back W L2 In the following description, the upper wafer W U Surface of W U1 and the lower wafer W L Surface of W L1 The upper wafer W1 and the lower wafer W2 are sometimes collectively referred to as "front surface W1". U Back of W U2 and the lower wafer W L Back of W L2 In the bonding system 1, the upper wafer W U and the lower wafer W L The surfaces W1 of the two substrates are bonded together to form a laminated wafer W T Form.

[0014] The wafer W is a semiconductor wafer such as a silicon substrate, and has an insulating film F and metal wiring D as a metal material exposed on the surface W1 side. The insulating film F is, for example, a silicon oxide film (SiO2 film or SiO film). The metal wiring D is, for example, copper (Cu) or cobalt (Co). The surface W1 of the wafer W to be carried into the bonding system 1 is previously recessed so that the surface height of the metal wiring D is lower than the surface height of the insulating film F. In one example, this recessing is controlled by a chemical mechanical polishing process (so-called "CMP process") of the wafer W. In one example, the depth (recess amount) of the recess formed by the recessing process is less than 5 nm.

[0015] As shown in FIG. 2, the bonding system 1 has a configuration in which a loading / unloading station 2 and a processing station 3 are integrally connected. In the loading / unloading station 2, for example, a plurality of upper wafers W are transferred between the loading / unloading station 2 and the outside. U , lower wafer W L Or laminated wafer W T Cassette C that can accommodate U , C L , C TThe processing station 3 carries in and out the upper wafer W U , lower wafer W L , laminated wafer W T The system is equipped with various processing devices that perform desired processing on the substrate.

[0016] In the loading / unloading station 2, cassette C U , C L , C T A cassette mounting stage 10 is provided on which a cassette C is mounted. A wafer transfer section 20 is provided adjacent to the cassette mounting stage 10 on the X-axis positive side of the cassette mounting stage 10. The wafer transfer section 20 moves on a transfer path 21 extending in the Y-axis direction to transfer the cassette C from the cassette mounting stage 10 to the U , C L , C T and the transition devices 50 and 51 described later. U , lower wafer W L Or laminated wafer W T A wafer transfer device 22 capable of transferring the wafer is provided.

[0017] The processing station 3 is provided with a plurality of, for example, three, processing blocks G1, G2, and G3 each equipped with various devices. The first processing block G1 is provided with a surface modification device 30 for modifying the surface W1 of the wafer W. The second processing block G2 is provided with a surface hydrophilization device 40 for hydrophilizing the surface W1 of the wafer W and cleaning the surface W1, and a surface hydrophilization device 50 for cleaning the upper wafer W. U and the lower wafer W L The third processing block G3 is provided with a bonding device 41 for bonding the upper wafer W U , lower wafer W L Or laminated wafer W T Transition devices 50 and 51 are provided for temporarily holding the

[0018] In the surface modification device 30, for example, under a reduced pressure atmosphere, oxygen gas or nitrogen gas serving as a processing gas is excited to be turned into plasma and ionized. The oxygen ions or nitrogen ions are irradiated onto the surface W1 of the wafer W, so that the surface W1 is subjected to the plasma processing and modified.

[0019] As shown in FIG. 4, the surface modification apparatus 30 includes a processing vessel 100, a processing gas supply unit 110, a plasma generation unit 120, an ion attraction unit 130, and an exhaust unit 140.

[0020] The processing vessel 100 is configured so that the inside can be sealed. The processing vessel 100 is formed with a loading / unloading port for the wafer W (not shown), and the loading / unloading port is provided with a gate valve (not shown). A stage 101 is disposed on the bottom side of the processing vessel 100, and the stage 101 holds the back surface W2 of the wafer W by suction so that the front surface W1 of the wafer W faces upward. At least a portion of the stage 101 is made of, for example, an insulating material.

[0021] The process gas supply unit 110 supplies a process gas into the process vessel 100. The process gas supply unit 110 includes a gas supply line 111 for introducing the process gas into the process vessel 100, at least one gas supply source 112, and at least one flow rate controller 113. The gas supply line 111 introduces the process gas supplied from the gas supply source 112 into the process vessel 100. The flow rate controller 113 may include, for example, a mass flow controller, a pressure control type, or a flow rate modulation device. Note that the process gas supplied from the gas supply source 112 is not limited to oxygen gas or nitrogen gas, and may be, for example, argon gas or helium gas.

[0022] The plasma generating unit 120 generates plasma of the processing gas inside the processing vessel 100. In the illustrated example, the plasma generating unit 120 includes a surface wave plasma (SWP: Surface Wave Plasma) type plasma generating device, but the configuration of the plasma generating unit 120 is not particularly limited, and may be a capacitively coupled plasma (CCP: Capacitively Coupled Plasma), an inductively coupled plasma (ICP: Inductively Coupled Plasma), or the like. The plasma generating device may be any plasma generating device such as an AC (Alternating Current) plasma generating device, an ECR (Electron-Cyclotron-resonance) plasma generating device, or a Helicon Wave Plasma (HWP) plasma generating device. Also, various types of plasma generating devices may be used, including an AC (Alternating Current) plasma generating device and a DC (Direct Current) plasma generating device.

[0023] The ion drawing unit 130 draws ions distributed inside the plasma generated in the processing vessel 100 to the surface W1 of the wafer W on the stage 101. In one example, the ion drawing unit 130 has at least one electrode 131, a high frequency power supply 132, and a capacitor 133. Note that the high frequency power supply 132 may be used to generate plasma inside the processing vessel 100, in addition to drawing ions to the surface W1 of the wafer W. Therefore, the high frequency power supply 132 supplies at least one of source power and bias power to the electrode 131.

[0024] The exhaust unit 140 is connected to, for example, a gas exhaust port 100e provided at the bottom of the processing vessel 100. The exhaust unit 140 may include a pressure regulating valve and a vacuum pump. The internal pressure of the processing vessel 100 is adjusted by the pressure regulating valve. The vacuum pump may include a turbo molecular pump, a dry pump, or a combination thereof.

[0025] The above is a configuration of the surface modification apparatus 30. Note that the above configuration is just an example, and the surface modification apparatus 30 may have any configuration as long as it can modify the surface W1 of the wafer W.

[0026] The surface hydrophilization device 40 supplies a processing liquid onto the surface W1 of the wafer W while rotating the wafer W held by, for example, a spin chuck. Then, the supplied processing liquid is diffused on the surface W1 of the wafer W by centrifugal force, and the surface W1 is hydrophilized.

[0027] As shown in FIG. 5, the surface hydrophilization apparatus 40 includes a processing vessel 200, a spin chuck 210, a cup 220, a discharge nozzle 230, and a liquid supply mechanism 240.

[0028] The processing vessel 200 is configured so that the inside can be sealed. The processing vessel 200 is formed with a loading / unloading port for the wafer W (not shown), and the loading / unloading port is provided with a gate valve (not shown). A spin chuck 210 is disposed in the center of the processing vessel 200, which holds the wafer W with its front surface W1 facing upward and rotates it around a vertical axis. The spin chuck 210 has a driving mechanism 211 including, for example, a motor. The driving mechanism 211 may also be provided with a lifting / lowering driving source such as a cylinder.

[0029] A cup 220 is provided around the spin chuck 210 to receive and collect liquid scattered or dropped from the wafer W. A discharge pipe 221 for discharging the collected liquid and an exhaust pipe 222 for exhausting the atmosphere inside the cup 220 are connected to the bottom surface of the cup 220.

[0030] Discharge nozzle 230 is provided above spin chuck 210 and is supported by an arm (not shown). Discharge nozzle 230 can move from a waiting section 231 disposed outside cup 220 to above the center of wafer W in cup 220, and can further move in the radial direction above wafer W. Discharge nozzle 230 is configured so that its height with respect to surface W1 of wafer W can be adjusted by a lifting mechanism (not shown).

[0031] A liquid supply mechanism 240 for supplying a processing liquid to the surface of the wafer W on the spin chuck 210 is connected to the discharge nozzle 230. The liquid supply mechanism 240 has a processing liquid supply source 241 that stores the processing liquid therein and supplies the processing liquid to the discharge nozzle 230, and a processing liquid supply pipe 242 that connects the processing liquid supply source 241 and the discharge nozzle 230.

[0032] An adjustment mechanism 242a including a regulator, a pressure gauge, a flow rate detector, a valve, a filter, etc. is disposed in the processing liquid supply pipe 242. This adjustment mechanism 242a can measure and adjust the pressure and / or flow rate of the processing liquid flowing inside the processing liquid supply pipe 242, and can also collect and remove particles in the processing liquid. There are no particular limitations on the types, numbers, and configurations of these regulators, pressure gauges, flow rate detectors, valves, and filters.

[0033] In this embodiment, a weak alkaline solution, for example, diluted ammonia water (dNH4OH), is used for the hydrophilization process of the surface of the wafer W. Therefore, the processing liquid supply source 241 of the liquid supply mechanism 240 stores ammonia water, for example.

[0034] In this embodiment, the liquid supply mechanism 240 is provided with a hydrogen ion concentration (hereinafter referred to as “pH”) adjuster 243 and an oxidation-reduction potential (hereinafter referred to as “ORP”) adjuster 244. The pH adjustment unit 243 adjusts the pH of the processing liquid (ammonia water in this embodiment) to a desired value by controlling, for example, the concentration of the processing liquid supplied to the surface W1 of the wafer W. Note that the configuration of the pH adjustment unit 243 is not limited to this, and may be configured arbitrarily as long as it can adjust the pH of the processing liquid. The ORP adjusting unit 244 adjusts the ORP of the processing liquid to a desired value by changing the amount of dissolved hydrogen in the processing liquid by mixing, for example, hydrogen gas or hydrogen water with the processing liquid supplied to the front surface W1 of the wafer W. Note that the configuration of the ORP adjusting unit 244 is not limited to this, and may be configured arbitrarily as long as it is possible to adjust the ORP of the processing liquid.

[0035] The above-described structure is of the surface hydrophilization device 40. Note that the above-described structure is merely an example, and the surface hydrophilization device 40 may have any structure as long as it can hydrophilize the surface W1 of the wafer W.

[0036] In the bonding device 41, the upper wafer W U and the lower wafer W L and surface W, which has been subjected to surface modification treatment and surface hydrophilization treatment in sequence. U1, surface W L1 And then join them.

[0037] As shown in FIG. 6, the bonding device 41 includes a processing vessel 300 , an upper chuck 310 , a lower chuck 320 , and a pushing unit 330 .

[0038] The processing vessel 300 is configured so that the inside can be sealed. The processing vessel 300 is formed with a loading / unloading port for the wafer W (not shown), and the loading / unloading port is provided with a gate valve (not shown). The upper chuck 310 is provided on the top side of the processing vessel 300, and the lower chuck 320 is provided on the bottom side of the processing vessel 300.

[0039] The upper chuck 310 supports the upper wafer WU Back of W U2 The upper chuck 310 is supported by an upper chuck stage 311 provided above the upper chuck 310. The upper chuck stage 311 supports the lower wafer W held by the lower chuck 320. L Surface of W L1 An upper imaging section 312 is provided to capture an image of the upper portion of the substrate 310. The upper imaging section 312 may be, for example, a CCD camera. The upper chuck 310 is provided with a rotating unit 313. The rotating unit 313 rotates the upper chuck stage 311 and the upper chuck 310 around a vertical axis (θ-axis). The rotating unit 313 may be provided with a measuring unit (e.g., a linear scale) (not shown) for measuring the position of the upper chuck 310 in the θ-axis direction.

[0040] The lower chuck 320 holds the lower wafer W L Back of W L2 The lower chuck 320 is provided below the upper chuck 310 and is configured to be able to be arranged opposite the upper chuck 310. That is, the upper wafer W held by the upper chuck 310 is U and the lower wafer W held by the lower chuck 320. LThe lower chuck 320 is supported by a lower chuck stage 321 provided below the lower chuck 320. The lower chuck stage 321 supports the upper wafer W held by the upper chuck 310. U Surface of W U1 The lower imaging section 322 is provided to capture an image of the object. The lower imaging section 322 is, for example, a CCD camera. Further, the lower chuck 320 is provided with a moving unit 323. The moving unit 323 moves the lower chuck stage 321 and the lower chuck 320 in the horizontal direction. The moving unit 323 moves the lower chuck 320 in the vertical direction. Note that the moving unit 323 may be provided with a measurement unit (e.g., a laser interferometer) (not shown) for measuring the horizontal and vertical positions of the lower chuck 320.

[0041] The upper surface of the upper chuck 310 is provided with an upper wafer W U The center of the back W U2 The pressing portion 330 has an actuator portion 331 and a cylinder portion 332. The actuator part 331 is inserted through a through hole 314 that passes through the center of the upper chuck 310 and the upper chuck stage 311 in the thickness direction, and is movable up and down in the vertical direction. The actuator part 331 is moved by air from an electropneumatic regulator, for example, to move the upper wafer W. U and the upper wafer W U The pressure load applied to the center of the material can be controlled. The actuator portion 331 is supported by a cylinder portion 332. The cylinder portion 332 moves the actuator portion 331 in the vertical direction by a drive portion having a built-in motor, for example. As described above, the pressing unit 330 controls the pressing load by the actuator unit 331, and controls the movement of the actuator unit 331 by the cylinder unit 332. The pressing unit 330 presses the upper wafer W (to be described later) against the upper wafer W (to be described later). U and the lower wafer W L When bonding the upper wafer W U The center of the lower wafer W LThe center of the plate can be brought into contact with the plate and pressed against it.

[0042] The lower chuck 320 is attached to the outer periphery of the upper wafer W. U , lower wafer W L , laminated wafer W T A guide member (not shown) is provided to prevent the lower chuck 320 from jumping out or sliding down from the lower chuck 320. The guide members are provided at a plurality of locations, for example, four locations, at equal intervals on the outer periphery of the lower chuck 320.

[0043] In addition, the bonding device 41 includes an upper wafer W that is transported to the bonding device 41 and is attracted and held by the upper chuck 310. U A reversing device (not shown) may be provided to reverse the front and back sides of the upper wafer W. U is a surface W that has been subjected to surface modification and surface hydrophilization treatment. U1 The reverse side W is conveyed facing up, but the reverse side is reversed by this reversing device, so that the reverse side W is properly conveyed. U2 can be held by the upper chuck 310. However, the location of the inversion device is not limited to this. Instead of inside the bonding device 41, the upper wafer W may be placed at any position in the processing station 3 of the bonding system 1. U A reversing device (not shown) for reversing the front and back sides may be provided separately.

[0044] The bonding apparatus 41 is configured as described above. Note that the above configuration is an example. U Surface of W U1 and the lower wafer W L Surface of W L1 Any configuration can be adopted as long as the above can be joined.

[0045] The transition devices 50 and 51 are stacked in the third processing block G3. U , lower wafer W L and laminated wafer W TIn order to transfer the upper wafer W between the wafer transfer device 22 of the wafer transfer section 20 of the loading / unloading station 2 and the wafer transfer device 62 of the wafer transfer section 60 described later, U , lower wafer W L and laminated wafer W T is temporarily held.

[0046] 2, a wafer transfer section 60 is provided in an area surrounded by the first processing block G1 to the third processing block G3 of the processing station 3. The wafer transfer section 60 moves on a transfer path 61 extending in the X-axis direction to transfer the upper wafer W between the surface modification device 30, the surface hydrophilization device 40, the bonding device 41, and the transition devices 50 and 51. U , lower wafer W L Or laminated wafer W T A wafer transfer device 62 capable of transferring the wafer is provided.

[0047] The bonding system 1 described above is provided with a control device 70. The control device 70 is, for example, a computer equipped with a CPU, a memory, and the like, and has a program storage unit (not shown). A program for controlling wafer processing in the bonding system 1 is stored in the program storage unit. The program may be recorded in a computer-readable storage medium H and installed from the storage medium H to the control device 70. The storage medium H may be temporary or non-temporary.

[0048] <Joining method> Next, the bonding of the upper wafer W is performed using the bonding system 1 configured as above. U and the lower wafer W L 7 is an explanatory diagram showing main steps of wafer processing in the bonding system 1. As shown in FIG.

[0049] First, a plurality of upper wafers W U Cassette C containing U , multiple lower wafers W L Cassette C containing L, and an empty cassette C T are placed on the cassette placement plate 11 of the carry-in / out station 2. Then, the cassettes C U Upper wafer W U is removed and transported to the transition device 50 of processing station 3.

[0050] Next, the upper wafer W U The upper wafer W is transported to the surface modification device 30 by the wafer transport device 62. In the surface modification device 30, the processing gas, oxygen gas or nitrogen gas, is excited to be turned into plasma and ionized in a desired reduced pressure atmosphere. The oxygen ions or nitrogen ions are then ionized into the upper wafer W. U Surface of W U1 is irradiated onto the surface W U1 The upper wafer W is then subjected to plasma processing. U Surface of W U1 In this surface modification process, as shown in FIG. 8(a), the surface W of the wafer W is U1 The insulating film F exposed to the surface of the wafer W is modified to form dangling bonds DB of silicon atoms. U1 The metal wiring D exposed to the surface is not modified.

[0051] Next, the upper wafer W U The upper wafer W is transferred to the surface hydrophilization device 40 by the wafer transfer device 62. In the surface hydrophilization device 40, the upper wafer W held by the spin chuck is U While rotating the upper wafer W U The processing liquid is then supplied to the upper wafer W. U Surface of W U1 The upper wafer W is then diffused and modified in the surface modification device 30. U Surface of W U1 (dangling bond DB) adheres to the hydroxyl group (silanol group) on the surface W U1 Therefore, in this surface hydrophilization treatment, the surface W of the wafer W is hydrophilized as shown in FIG. U1Hydroxyl groups are attached to the insulating film F exposed to the surface of the upper wafer W, but not to the metal wiring D. U Surface of W U1 The surface of the wafer W is then cleaned (step SU2 in FIG. 7). The detailed method of the hydrophilization treatment of the surface of the wafer W will be described later.

[0052] Next, the upper wafer W U The upper wafer W is transferred to the bonding device 41 by the wafer transfer device 62. U After the front and back sides are inverted by an inversion device (not shown), the back side W is placed on the upper chuck 310. U2 At this time, the upper wafer W U The horizontal direction is adjusted by a position adjustment mechanism (not shown).

[0053] Upper wafer W U While the above-mentioned various processes are being performed on the upper wafer W U Next, the lower wafer W L First, the wafer transfer device 22 transfers the wafer to the cassette C. L Lower wafer W L is removed and transported to the transition device 50 of processing station 3.

[0054] Next, the lower wafer W L The lower wafer W is transferred to the surface modification device 30 by the wafer transfer device 62. L Surface of W L1 The lower wafer W in step SL1 is modified (step SL1 in FIG. 7). L Surface of W L1 The modification is the same as in the above-mentioned step SU1.

[0055] Next, the lower wafer W L The lower wafer W is transferred to the surface hydrophilization device 40 by the wafer transfer device 62. L Surface of W L1 is hydrophilized and the surface W L1 The lower wafer W is cleaned (step SL2 in FIG. 7). L Surface of WL1 The hydrophilization and cleaning are the same as those in the above-mentioned step SU2. The detailed method of the hydrophilization treatment of the surface of the wafer W will be described later.

[0056] Next, the lower wafer W L The lower wafer W is transferred to the bonding device 41 by the wafer transfer device 62. L The lower chuck is 320 and the back side is W L2 At this time, the lower wafer W L The horizontal direction is adjusted by a position adjustment mechanism (not shown).

[0057] Upper wafer W U The lower wafer W is attached to the upper chuck 310. L After the upper wafer W held by the upper chuck 310 is sucked and held by the lower chuck 320, U and the lower wafer W held by the lower chuck 320. L Adjust the position with. Specifically, the upper imaging unit 312 captures the lower wafer W held by the lower chuck 320. L Surface of W L1 The upper wafer W held by the upper chuck 310 is imaged by the lower imaging unit 322 in sequence. U Surface of W U1 The control device 70 sequentially captures images of predetermined reference points on the upper wafer W based on the images captured by the upper imaging unit 312 and the images captured by the lower imaging unit 322. U The reference point and the lower wafer W L The upper chuck 310 (upper wafer W) is rotated by the rotating part 313 so that the reference points of the upper chuck 310 and the upper wafer W are aligned with each other. U ) is rotated, and the lower chuck 320 (lower wafer W) is moved by the moving part 323. L In this way, the upper wafer W U and the lower wafer W L The position of the upper wafer W is adjusted. U and the lower wafer W L are disposed opposite each other at a desired position.

[0058] Next, the upper wafer W U and the lower wafer W L Then, a bonding process is performed (step S3 in FIG. 7). Specifically, first, the actuator part 331 is lowered by the cylinder part 332, and the actuator part 331 is placed on the upper wafer W. U Back of W U2 Next, the actuator part 331 continues to move downward until the upper wafer W U The upper wafer W is lowered by pressing the center of the U The center of the lower wafer W L The center of the upper wafer W is pressed against the U The center of the lower wafer W L When the centers of the upper wafer W and the lower wafer W are pressed against each other, U and the lower wafer W L That is, the bonding of the upper wafer W U Surface of W U1 and the lower wafer W L Surface of W L1 Since the surfaces are modified in steps SU1 and SL1, respectively, the surface W U1 , W L1 Van der Waals forces (intermolecular forces) occur between the surfaces W U1 , W L1 The upper wafer W U Surface of W U1 and the lower wafer W L Surface of W L1 Since the surfaces are hydrophilized in steps SU2 and SL2, respectively, the surface W U1 , W L1 Hydrophilic groups between the surfaces form hydrogen bonds (intermolecular forces), U1 , W L1 The two surfaces are firmly joined together. Then, the surface W U1 , surface W L1 The van der Waals forces and hydrogen bonds between the upper and lower wafers diffuse from the center to the periphery. U Surface of W U1 and the lower wafer W L Surface of W L1 When the upper wafer W U and the lower wafer WL The joining process is then completed.

[0059] Upper wafer W U and the lower wafer W L The laminated wafer W T Then, the wafer is transferred to the transition device 51 by the wafer transfer device 62, and the wafer is loaded into the cassette C by the wafer transfer device 22 of the loading / unloading station 2. T In this way, a series of upper wafers W U and the lower wafer W L The joining process is then completed.

[0060] In this way, the upper wafer W U and the lower wafer W L The laminated wafer W formed by bonding T Then, the overlapped wafer W is subjected to a heating (annealing) process in a heating device provided outside the bonding system 1 (step S4 in FIG. 7). T By the heating, the metal wiring D formed on the surface W1 of the wafer W thermally expands along the wall surface of the recess (see FIG. 1), and the upper wafer W U and the lower wafer W L The surfaces of the metal wirings D formed on each of the above are firmly diffusion-bonded to each other and electrically connected.

[0061] Although this heat treatment may be performed outside the bonding system 1, a heating device (not shown) may be provided in the processing station 3 of the bonding system 1 to heat the upper wafer W in the bonding device 41. U and the lower wafer W L Alternatively, the above-mentioned step may be performed after the joining.

[0062] <Surface hydrophilization treatment> Next, the detailed method of the surface hydrophilization treatment according to this embodiment will be described.

[0063] As shown in the Pourbaix diagram in Figure 9, the surface state of copper (Cu) used as metal wiring D changes depending on the hydrogen ion concentration (pH value) and oxidation-reduction potential (ORP value) of the treatment solution supplied in the surface hydrophilization treatment. Specifically, when the reducing power of the supplied treatment liquid is large (the ORP value is a negative value), there is no change in the surface state (composition) of the metal wiring D. On the other hand, when the oxidizing power of the supplied treatment liquid is large (the ORP value is a positive value), the surface state further changes depending on the hydrogen ion concentration of the treatment liquid. That is, when the supplied treatment liquid is acidic (pH value is 7 or less), it corrodes the surface of the metal wiring D and produces copper ions (Cu 2+ ) is generated. In addition, if the processing liquid supplied is strongly alkaline (for example, pH value of 11 or more), coordination bonds are formed between the metal wiring D and the processing liquid, which may generate a highly soluble complex and cause dissolution (corrosion) of the metal wiring D itself. In such cases, the composition of the metal wiring D changes due to corrosion of the metal wiring D, inhibiting bonding between the metal wirings D and degrading the quality of the metal wiring in the product wafer, such as its electrical conductivity. On the other hand, when the processing liquid supplied is weakly alkaline, copper hydroxide or copper oxide (I) is generated on the surface without changing the composition of the metal wiring D (while maintaining the metallic properties). U and the lower wafer W L This can promote bonding between the metal wirings D.

[0064] Therefore, in the bonding system 1 according to the technology of the present disclosure, a weak alkaline solution, such as diluted ammonia water, is used as the processing liquid supplied to the surface W1 of the wafer W in the surface hydrophilization treatment, and the pH value and ORP value of the processing liquid supplied onto the wafer W are adjusted using the pH adjustment unit 243 and the ORP adjustment unit 244. Specifically, in the surface hydrophilization treatment according to this embodiment, the pH value and ORP value of the treatment solution are adjusted using the pH adjustment unit 243 and the ORP adjustment unit 244 so that the relationship between the pH value and the ORP value does not fall within the corrosion region (the shaded region in the figure) on the Pourbaix diagram shown in FIG. 9. More specifically, the amount of dissolved hydrogen in the treatment liquid is adjusted by the ORP adjustment unit 244 to strengthen the reducing power of the treatment liquid (ORP value of 0 or less), or the concentration [ppm] of the treatment liquid is adjusted by the pH adjustment unit 243 to make the hydrogen ion concentration pH of the treatment liquid about 7 to 11. In one example, when the treatment liquid is ammonia water, the concentration at which the hydrogen ion concentration pH becomes 7 to 11 is 1 ppm to 1000 ppm.

[0065] As a result, in the surface hydrophilization device 40, hydroxyl groups (silanol groups) are attached to the insulating film F that has been subjected to a surface modification treatment on the surface W1 of the wafer W, and bonding between the metal wirings D in a heating device (not shown) can be promoted without changing the composition of the metal wirings D.

[0066] Furthermore, the thickness of the copper hydroxide formed on the surface of the metal wiring D by the supply of ammonia water, in other words, the amount of film reduction (i.e., the amount of recess) of copper (Cu) as the metal wiring D, varies depending on the pH value and ORP value of the supplied ammonia water. Specifically, the amount of film reduction (recess amount) increases when the pH value of the ammonia water is high (highly alkaline) and the ORP value is high (high reducing power), whereas the amount of film reduction (recess amount) decreases when the pH value of the ammonia water is low (closer to neutral) and the ORP value is low (weak reducing power). From this viewpoint, by appropriately adjusting the pH value and ORP value within a range that does not fall within the corrosion region on the Pourbaix diagram, the metal wiring D can be recessed to a desired value. In this case, the surface hydrophilization treatment preferably includes a step of controlling the pH value and ORP value of the treatment solution to be constant at a predetermined desired value (a step of maintaining the pH value and ORP value constant at a desired value) at least until a desired recess amount is obtained in the metal wiring D. Therefore, according to the technology disclosed herein, even if the recess amount of the metal wiring D formed on the surface W1 of the wafer W transported to the bonding system 1 is insufficient or there is variation within the surface, the recess amount of the metal wiring D can be adjusted in the surface hydrophilization device 40 prior to bonding in the bonding device 41, and the variation in the recess amount can be suppressed and corrected by locally supplying a processing liquid.

[0067] In the above embodiment, the amount of recess in the metal wiring D is controlled by the pH value and ORP value of the processing liquid supplied to the surface W1 of the wafer W. However, the amount of recess in the metal wiring D may be controlled more precisely by controlling the temperature of the processing liquid supplied, the supply time (time for the surface hydrophilization treatment) and the amount of the processing liquid supplied in addition to the above. Specifically, the amount of recess in the metal wiring D can be increased by increasing the temperature of the processing liquid, and the amount of recess can be decreased by decreasing the temperature. In one example, the temperature of the processing liquid supplied to the front surface W1 of the wafer W is controlled in the range of 20°C to 80°C, preferably 60°C or less. Moreover, the amount of recess in the metal wiring D can be increased by increasing the supply time or amount of the processing liquid, and the amount of recess in the metal wiring D can be decreased by decreasing the supply time or amount of the processing liquid.

[0068] In the above embodiment, the metal wiring D formed on the front surface W1 of the wafer W is copper (Cu), but the type of metal constituting the metal wiring D is not limited thereto. Specifically, for example, as described above, cobalt (Co) may be used as the metal wiring D. Even in this case, by controlling at least the pH value and ORP value of the treatment liquid to be supplied, the bonding between the metal wirings D can be promoted, and the recess amount can be adjusted by the surface hydrophilization device 40 prior to bonding.

[0069] In the above embodiment, diluted ammonia water (dNH4OH) is used as the treatment liquid in the surface hydrophilization treatment, but the type of treatment liquid is not limited to this as long as it can control the surface condition of the metal wiring D by controlling the pH value and ORP value as described above. In addition, the treatment liquid conventionally used in surface hydrophilization treatment, such as carbon dioxide water (CO2 Even if the ORP value is controlled based on a Pourbaix diagram (not shown) so as not to enter the corrosion region of the metal wiring D, the same effect as that of the technology according to the present disclosure can be obtained.

[0070] The embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The above-described embodiments may be omitted, substituted, or modified in various forms without departing from the scope and spirit of the appended claims. For example, the components of the above-described embodiments may be arbitrarily combined. From such an arbitrary combination, the actions and effects of each of the components in the combination can be obtained as a matter of course, and other actions and effects that are obvious to a person skilled in the art from the description of this specification can be obtained.

[0071] In addition, the effects described in this specification are merely explanatory or exemplary and are not limiting. In other words, the technology according to the present disclosure may achieve other effects that are apparent to a person skilled in the art from the description of this specification in addition to or in place of the above effects.

[0072] Note that the following configuration examples also fall within the technical scope of the present disclosure. (1) A method for joining substrates having metal materials exposed on their surfaces, comprising the steps of: modifying the surface of the substrate to be bonded with a plasma of a process gas; making the modified surface of the substrate hydrophilic; and bonding the hydrophilized surfaces of the substrates together, In the hydrophilization step, A bonding method comprising: supplying a treatment liquid to the surface of the substrate; and controlling a recess amount of the metal material by the treatment liquid. (2) The bonding method according to (1) above, wherein the recess depth is controlled by a hydrogen ion concentration of the treatment liquid. (3) The bonding method according to (2) above, wherein the hydrogen ion concentration of the treatment liquid is controlled within a pH value range of 7 to 11. (4) The bonding method according to (3) above, wherein ammonia water is used as the treatment liquid. (5) The bonding method according to (5) above, wherein the concentration of the ammonia water is adjusted to 1 ppm to 1000 ppm. (6) The bonding method according to (2) or (3), further comprising a step of maintaining the hydrogen ion concentration of the treatment liquid at a predetermined constant pH value. (7) The bonding method according to any one of (1) to (6), wherein the recess depth is controlled by an oxidation-reduction potential of the treatment liquid. (8) The bonding method according to (7) above, wherein an oxidation-reduction potential of the treatment liquid is controlled so that the ORP value is 0 or less. (9) The bonding method according to (7) or (8), further comprising a step of maintaining an oxidation-reduction potential of the treatment liquid at a predetermined constant ORP value. (10) The bonding method according to any one of (1) to (9), wherein the recess depth is controlled by at least one of a temperature, a flow rate, and a supply time of the treatment liquid. (11) The bonding method according to (10) above, wherein the temperature of the treatment liquid is controlled within a range of 20°C to 80°C. (12) The bonding method according to any one of (1) to (11), wherein the metal material is copper. (13) The bonding method according to any one of (1) to (12), further comprising a step of heating the laminated substrate formed by bonding the substrates.

[0073] (14) A joining system for joining substrates having metal materials exposed on surfaces, comprising: a surface modification device for modifying the surface to be bonded of the substrate by plasma of a processing gas; a surface hydrophilization device for hydrophilizing the modified surface of the substrate; a bonding device for bonding the hydrophilized surfaces of the substrates together; A control device, The control device includes: a bonding system in which, in the surface hydrophilization device, a treatment liquid is supplied to the surface of the substrate, and a control is performed to adjust a recess amount of the metal material by the treatment liquid. (15) The bonding system according to (14), wherein the surface hydrophilization device includes a pH adjustment unit that adjusts a hydrogen ion concentration of the treatment liquid. (16) The bonding system according to (14) or (15), wherein the surface hydrophilization device includes an ORP adjustment unit that adjusts an oxidation-reduction potential of the treatment liquid. (17) The bonding system according to any one of (14) to (16), wherein the treatment liquid is ammonia water. (18) The joint system according to any one of (14) to (17), wherein the metal material is copper. (19) The bonding system according to any one of (14) to (18), further comprising a heating device for heating the laminated substrate formed by the bonding device. [Explanation of symbols]

[0074] 1 Joining System 30 Surface modification equipment 40 Surface hydrophilization device 41 Joining equipment 70 Control device D Metal wiring W U Upper wafer W L Lower wafer W1 surface

Claims

1. A method for joining substrates having metal materials exposed on their surfaces, comprising the steps of: modifying the surface of the substrate to be bonded with a plasma of a process gas; making the modified surface of the substrate hydrophilic; and bonding the hydrophilized surfaces of the substrates together, In the hydrophilization step, A bonding method comprising: supplying a treatment liquid to the surface of the substrate; and controlling a recess amount of the metal material by the treatment liquid.

2. The bonding method according to claim 1 , wherein the recess depth is controlled by a hydrogen ion concentration of the treatment liquid.

3. 3. The bonding method according to claim 2, wherein the hydrogen ion concentration of the treatment liquid is controlled within a pH range of 7 to 11.

4. 4. The bonding method according to claim 3, wherein the treatment liquid is ammonia water.

5. 5. The bonding method according to claim 4, wherein the concentration of the ammonia water is adjusted to 1 ppm to 1000 ppm.

6. 3. The bonding method according to claim 2, further comprising the step of maintaining the hydrogen ion concentration of the treatment liquid at a predetermined constant pH value.

7. The bonding method according to claim 1 , wherein the recess depth is controlled by an oxidation-reduction potential of the treatment liquid.

8. The bonding method according to claim 7 , wherein the oxidation-reduction potential of the treatment liquid is controlled so that the ORP value is 0 or less.

9. 8. The method of claim 7, further comprising the step of maintaining the oxidation-reduction potential of the treatment solution at a predetermined constant ORP value.

10. The bonding method according to claim 1 , wherein the recess depth is controlled by at least one of a temperature, a flow rate, and a supply time of the treatment liquid.

11. The bonding method according to claim 10, wherein the temperature of the treatment liquid is controlled to be in the range of 20°C to 80°C.

12. The bonding method according to any one of claims 1 to 11, wherein the metal material is copper.

13. The bonding method according to any one of claims 1 to 11, further comprising a step of heating the laminated substrate formed by bonding the substrates.

14. A joining system for joining substrates having metal materials exposed on their surfaces, comprising: a surface modification device for modifying the surface to be bonded of the substrate by plasma of a processing gas; a surface hydrophilization device for hydrophilizing the modified surface of the substrate; a bonding device for bonding the hydrophilized surfaces of the substrates together; A control device, The control device includes: a bonding system in which, in the surface hydrophilization device, a treatment liquid is supplied to the surface of the substrate, and a control is performed to adjust a recess amount of the metal material by the treatment liquid.

15. The bonding system according to claim 14 , wherein the surface hydrophilization device includes a pH adjustment unit that adjusts a hydrogen ion concentration of the treatment liquid.

16. The bonding system according to claim 14 , wherein the surface hydrophilization device includes an ORP adjusting section that adjusts an oxidation-reduction potential of the treatment liquid.

17. The bonding system according to any one of claims 14 to 16, wherein the treatment liquid is aqueous ammonia.

18. The joining system according to any one of claims 14 to 16, wherein the metallic material is copper.

19. The bonding system according to any one of claims 14 to 16, further comprising a heating device for heating the laminated substrate formed by the bonding device.

Citation Information

Patent Citations

  • Joint system

    JP2017073455A