Front edge protective layer construction method for wind turbine blade and protective layer for wind turbine blade

By adjusting thermal spraying directions and positions on wind turbine blades, the method ensures precise and consistent protective layer formation on the leading edge, addressing curvature challenges and maintaining quality and thickness.

JP2024149046AInactive Publication Date: 2024-10-18MITSUBISHI HEAVY IND LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023062708
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-07
Publication Date
2024-10-18
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The challenge of forming a protective layer on the leading edge of a wind turbine blade with a large curvature using thermal spraying is the difficulty in determining the appropriate spraying direction, leading to inconsistencies in thickness and quality.

Method used

A method involving thermal spraying in the blade span direction with positional adjustments in the chord direction to maintain consistent curvature, followed by changing the chord position for adjacent spraying, ensuring precise layer formation.

Benefits of technology

This approach allows for the formation of a protective layer with desired thickness and quality, minimizing fluid loss and maintaining high precision even on large blades.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024149046000001_ABST
    Figure 2024149046000001_ABST
Patent Text Reader

Abstract

To provide a method for manufacturing wind turbine blades capable of improving position accuracy of thermal spraying to obtain a protective layer with a desired thickness and quality.SOLUTION: A manufacturing method for a wind turbine blade 5 in which a protective layer is provided on a tip part 12 and a front edge 16 side in a blade length direction L1 of a wind turbine blade body 5a formed from FRP, comprises: a first thermal spraying process of performing thermal spraying in the blade length direction L1; a blade chord position changing process of changing a position so that a protective layer 30 formed in the first thermal spraying process is sprayed at an adjacent position adjacent in a blade chord direction C1; and a second thermal spraying process of performing thermal spraying in the blade length direction L1 at the adjacent position.SELECTED DRAWING: Figure 8
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for applying a leading edge protective layer to a wind turbine blade and a protective layer for a wind turbine blade. [Background technology]

[0002] As the wind turbine rotor rotates, the wind turbine blades collide with foreign objects in the air (e.g., raindrops, dust, etc.) and are eroded, causing erosion on the leading edge of the wind turbine blade. To protect the wind turbine blades from this erosion, it is known to form an erosion-resistant protective layer on the leading edge of the wind turbine blade (see Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2022-175830 Summary of the Invention [Problem to be solved by the invention]

[0004] When spraying the leading edge of a wind turbine blade, it is difficult to determine the spraying direction appropriately because the leading edge has a large curvature, and there is a risk that the desired thickness and quality of the protective layer will not be obtained.

[0005] The present disclosure has been made in consideration of the above circumstances, and aims to provide a method for applying a leading edge protective layer to a wind turbine blade, and a protective layer for a wind turbine blade, which can improve the positional accuracy of thermal spraying to obtain a protective layer having a desired thickness and quality. [Means for solving the problem]

[0006] A method for applying a leading edge protective layer to a wind turbine blade according to one embodiment of the present disclosure is a method for manufacturing a wind turbine blade in which a protective layer is provided by thermal spraying at the tip and leading edge in the blade span direction of a wind turbine blade body formed of FRP, the method including a first thermal spraying step of performing thermal spraying in the blade span direction, a chordwise position changing step of changing the position so that the protective layer formed in the first thermal spraying step is sprayed at an adjacent position adjacent in the chord direction, and a second thermal spraying step of performing thermal spraying in the blade span direction at the adjacent position.

[0007] A protective layer for a wind turbine blade according to one embodiment of the present disclosure comprises a wind turbine blade body formed of FRP, and a protective layer provided at a tip and leading edge portion in the blade span direction of the wind turbine blade body, wherein the thickness in the chord direction of an end portion of the protective layer formed on the blade surface of the wind turbine blade body is gradually reduced towards the edge. Effect of the Invention

[0008] A protective layer of desired thickness and quality can be applied to the wind turbine blade. [Brief description of the drawings]

[0009] [Figure 1] 1 is a schematic configuration diagram showing a wind power generation device using a wind turbine blade according to an embodiment of the present disclosure. [Diagram 2] FIG. 2 is a plan view showing a wind turbine blade. [Diagram 3] FIG. 3 is a front view of the wind turbine blade of FIG. 2. [Figure 4] FIG. 4 is a cross-sectional view of the wind turbine blade shown in FIGS. 2 and 3. [Diagram 5] FIG. 11 is a front view showing an installed state of the wind turbine blade when a protective layer is formed. [Figure 6] FIG. 6 is a cross-sectional view of the support position of FIG. 5. [Figure 7] FIG. 4 is a partially enlarged front view showing the area in which a protective layer is formed on the tip of a wind turbine blade. [Figure 8] 5A to 5C are partially enlarged front views showing the order of forming protective layers. [Figure 9] FIG. 4 is a partially enlarged cross-sectional view showing the direction in which a protective layer is formed in the chord direction. [Figure 10] FIG. 2 is a cross-sectional view of an end portion in the chord direction of a protective layer formed on the blade surface of a wind turbine blade. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, an embodiment according to the present disclosure will be described with reference to the drawings. As shown in FIG. 1, the wind turbine generator 1 has a tower 3 erected on an installation surface B, a nacelle 6 installed at the upper end of the tower 3, and a rotor head 4 mounted on the nacelle 6 so as to be rotatable around a substantially horizontal axis.

[0011] A number of (e.g., three) wind turbine blades 5 are attached to the rotor head 4 in a radial manner around the rotation axis. This allows the force of the wind hitting the wind turbine blades 5 from the direction of the rotation axis of the rotor head 4 to be converted into power that rotates the rotor head 4 around the rotation axis. The obtained power is converted into electric power by a generator (not shown) and supplied to the outside.

[0012] As shown in Fig. 2, the wind turbine blade 5 includes a blade root portion 10 attached to the rotor head 4, a blade tip portion (tip portion) 12 located farthest from the rotor head 4, and an airfoil portion 14 extending between the blade root portion 10 and the blade tip portion 12. In Fig. 2, the blade span direction L1 is the horizontal direction.

[0013] The wind turbine blade 5 has a leading edge 16 and a trailing edge 18 from the blade root 10 to the blade tip 12. The outer shape of the wind turbine blade 5 is determined by a ventral side surface 20 which is a pressure surface (positive pressure surface) and a suction side surface 22 which is a negative pressure surface facing the ventral side surface 20. The wind turbine blade 5 is made of FRP (Fiber-Reinforced Plastic). Examples of FRP that can be used include carbon fiber reinforced plastic (CFRP) and glass fiber reinforced plastic (GFRP). The entire length of the wind turbine blade 5 from the blade root 10 to the blade tip 12 is in the 100 m class, for example, 80 m or more and 150 m or less. A 200 m class wind turbine blade may be used as the wind turbine blade 5 of this embodiment.

[0014] 3, the wind turbine blade 5 is provided with a pre-bend PB that is bent in advance on the blade tip 12 side. The amount of bending of the pre-bend PB is determined in advance assuming that the wind turbine blade 5 receives wind pressure during operation. Therefore, the pre-bend PB is bent so that the ventral side surface 20 that receives wind pressure is concave and the suction side surface 22 is convex.

[0015] As shown in Fig. 2, a protective layer 30 is formed on the wind turbine blade main body 5a in a predetermined region (leading edge portion) including the blade tip portion 12 and leading edge 16 of the wind turbine blade 5. The formation range of the protective layer 30 is indicated by a thick line in Fig. 2. The formation range of the protective layer 30 in the blade length direction L1 is 20 m to 40 m, preferably about 30 m, from the tip 12a of the blade tip portion 12. Note that the formation range of the protective layer 30 is not limited to this, and for example, in a region where the peripheral speed exceeds 90 m / s, it is set to a range of about 1 / 3 of the total length from the tip of the wind turbine blade 5. The protective layer 30 is made of a material having excellent wear resistance, such as a cermet or a Co (cobalt)-based alloy, etc. The protective layer 30 is formed, for example, by HVOF (High Velocity Oxy-Fuel) thermal spraying.

[0016] Figure 4 shows a cross section of a wind turbine blade 5. In the figure, the horizontal direction indicates the chord direction (cord direction) C1. If the total length of the wind turbine blade 5 is R, (a) is the cross section at a position of 0.9R, and (b) is the cross section at a position of 0.7R.

[0017] The chord length c in the cross section of Figure 4(a) is about 1 m. When the maximum blade thickness is t, the blade thickness ratio t / c is 18%. The chord length c in the cross section of Figure 4(b) is approximately 2 m, and the thickness ratio t / c is 25%.

[0018] 4, the protective layer 30 is formed from the ventral side surface 20 to the suction side surface 22 across the leading edge 16. The formation range of the protective layer 30 is determined in consideration of erosion of the wind turbine blade 5 by raindrops, etc.

[0019] Next, the process of forming the protective layer 30 will be described. As shown in Fig. 5, after the outer shape of the wind turbine blade main body 5a of the wind turbine blade 5 is formed, the wind turbine blade 5 is installed in a posture in which the blade length direction L1 is approximately horizontal and the leading edge 16 faces downward (posture setting process). That is, the wind turbine blade 5 is installed upright so that the blade chord direction C1 of the wind turbine blade main body 5a faces approximately vertically. At this time, the wind turbine blade 5 is supported from below by a plurality of supports 32 provided at predetermined intervals in the blade length direction L1 (support process).

[0020] 6 shows that the leading edge 16 side of the wind turbine blade 5 is supported by a plurality of support bases 32. Each support base 32 is provided on the as-formed installation surface BS. Note that the wind turbine blade 5 may be supported with the leading edge 16 side facing downward. For example, instead of the method of supporting the wind turbine blade 5 from below by the support bases 32 described above, the wind turbine blade 5 may be supported by holding and lifting the leading edge 16 facing downward by a hanging member such as a wire hung from above the wind turbine blade 5.

[0021] As shown in Figures 5 and 6, spraying is performed by the spraying section with the leading edge 16 facing downward. The spraying section accelerates the spraying material, which has been heated and melted or softened, in the form of droplets or particles by a carrier gas and sprays it onto the surface of the wind turbine blade body 5a.

[0022] 7 shows the sprayed area formed on the blade tip 12 of the wind turbine blade 5. As shown in the figure, a protective layer 30 is formed in a predetermined area (leading edge portion) on the leading edge 16 side of the wind turbine blade 5.

[0023] As shown in FIG. 8, the spraying is performed by reciprocating the sprayed part in the blade length direction L1 (the direction indicated by (1) in the figure) (first spraying step). This results in a multi-layered protective layer. The thickness of the protective layer is, for example, about 500 μm to 600 μm. The irradiation width of the sprayed part on the blade surface is, for example, about 10 mm.

[0024] After the above-mentioned first spraying process, the position of the sprayed portion is changed so that spraying is performed at an adjacent position adjacent to the chord direction C1 (the direction shown by (2) in the figure) (chord position changing process). Then, at this adjacent position, spraying is performed by reciprocating the sprayed portion in the chord direction C1 in the spanwise direction L1 (the direction shown by (1) in the figure) in the same manner as in the first spraying process (second spraying process). The first and second spraying processes are formed by scanning the sprayed portion so that it reciprocates in the spanwise direction L1. This is because the change in curvature of the blade surface is smaller in the spanwise direction L1 than in the chord direction C1.

[0025] As shown in Figure 9, the position change direction in the above-mentioned chord position changing process is a direction from one blade surface of the wind turbine blade 5 (e.g., the ventral side surface 20 or the suction side surface 22) through the leading edge 16 to the other blade surface (e.g., the suction side surface 22 or the ventral side surface 20), as indicated by the arrow in the figure.

[0026] 10 shows a cross section of an end 30a in the chord direction C1 of the protective layer 30 formed on the blade surface (ventral side surface 20 or suction side surface 22) of the wind turbine blade 5. As shown in the figure, the thickness of the end 30a of the protective layer 30 is formed to gradually decrease toward its edge (the right side in the figure). This is achieved by gradually shifting the sprayed portion in the chord direction C1 when spraying the end 30a of the protective layer 30 to laminate the protective layer 30 in the thickness direction (end spraying process).

[0027] The effects of the present embodiment described above are as follows. The thermal spraying is performed in the blade length direction L1, in a direction in which the curvature of the wind turbine blade main body 5a does not change significantly, thereby improving the positional accuracy of the thermal spraying. The chord position is changed so that spraying is performed at a position adjacent in the chord direction C1 of the protective layer 30 formed in the first spraying process. Then, spraying is performed in the blade length direction L1 in the second spraying process. By changing the position to an adjacent position in the chord direction C1, it is possible to make the change in curvature of the wind turbine blade main body 5a relatively small. This makes it possible to improve the positional accuracy of spraying.

[0028] When changing the position in the chord direction C1 during thermal spraying, the position is changed from one blade surface 20, 22 of the wind turbine blade body 5a via the leading edge 16 to the other blade surface 22, 20, so that the protective layer 30 can be formed on the leading edge 16 side in a series of processes.

[0029] The protective layer 30 is formed so that the thickness of the end 30a of the protective layer 30 in the chord direction C1 gradually decreases toward the edge. This makes it possible to minimize loss of fluid flowing through the end 30a of the protective layer 30. Note that the thickness of the end of the protective layer 30 in the spanwise direction L1 may also be gradually decreased toward the edge.

[0030] Even in the case of a large wind turbine blade 5 exceeding 80 m, the deflection of the wind turbine blade main body 5a is small, so the protective layer 30 can be formed with high precision.

[0031] The wind turbine blade leading edge protective layer construction method and the wind turbine blade protective layer described in each of the above-described embodiments can be understood, for example, as follows.

[0032] A method for applying a leading edge protective layer to a wind turbine blade (5) according to a first aspect of the present disclosure is a method for manufacturing a wind turbine blade in which a protective layer (30) is provided at a tip portion (12) and a leading edge (16) in a blade length direction (L1) of a wind turbine blade body (5a) formed of FRP, the method including a first thermal spraying step of performing thermal spraying in the blade length direction, a chord position changing step of changing a position so that thermal spraying is performed at an adjacent position adjacent in a chord direction (C1) of the protective layer formed in the first thermal spraying step, and a second thermal spraying step of performing thermal spraying in the blade length direction at the adjacent position.

[0033] The thermal spraying is performed in the blade length direction, in a direction in which the curvature of the wind turbine blade body does not change significantly. This improves the positional accuracy of the thermal spraying. The chord position is changed so that spraying is performed at a position adjacent in the chord direction to the protective layer formed in the first spraying process. Then, spraying is performed in the blade length direction in the second spraying process. By changing the position to an adjacent position in the chord direction, it is possible to make the change in curvature of the wind turbine blade body relatively small. This makes it possible to improve the positional accuracy of spraying.

[0034] In a wind turbine blade leading edge protective layer construction method according to a second aspect of the present disclosure, in the first aspect, the chord position changing step changes the chordwise position from one blade surface (20, 22) of the wind turbine blade body via the leading edge (16) to the other blade surface (22, 20).

[0035] When changing the position in the chord direction during thermal spraying, the position is changed from one blade surface of the wind turbine blade via the leading edge to the other blade surface, so that the protective layer can be formed on the leading edge portion in a series of processes.

[0036] The wind turbine blade leading edge protective layer application method according to a third aspect of the present disclosure includes an end spraying step in the first or second aspect, in which spraying is performed so that the thickness of an end in a chord direction of the protective layer formed on the blade surface of the wind turbine blade body gradually decreases toward the edge.

[0037] The protective layer is formed so that the thickness of the protective layer at the end in the chord direction and / or span direction gradually decreases toward the edge, thereby minimizing the loss of the fluid flowing at the end of the protective layer.

[0038] A wind turbine blade leading edge protective layer construction method according to a fourth aspect of the present disclosure is any one of the first to third aspects, wherein the dimension of the wind turbine blade body in the blade span direction is 80 m or more.

[0039] Even for large wind turbine blades exceeding 80m, the deflection of the wind turbine blade body is small, so the protective layer can be formed with high precision.

[0040] The protective layer of a wind turbine blade according to a first aspect of the present disclosure is a protective layer of a wind turbine blade provided at the tip and leading edge in the blade span direction of a wind turbine blade body formed from FRP, and the thickness of the end in the chord direction of the protective layer formed on the blade surface of the wind turbine blade body is gradually reduced towards the edge.

[0041] The thickness of the protective layer at the end in the chord direction is gradually reduced toward the edge, thereby minimizing loss of the fluid flowing at the end of the protective layer. [Explanation of symbols]

[0042] 1. Wind power generation equipment 3. Tower 4 Rotor Head 5 windmill blade 5a Wind turbine blade body 6. Nacelle 10 Wing root 12 Wing tip (tip) 12a Tip 14 Airfoil section 16 Leading Edge 18 Trailing edge 20 Ventral aspect 22 Dorsal aspect 30 protective layer 30a end 32 Support stand B Installation surface Installation surface when forming BS C1 Chord direction (chord direction) L1 spanwise direction PB Pre-bend

Claims

1. A method for manufacturing a wind turbine blade in which a protective layer is provided at a tip portion and a leading edge portion in a blade span direction of a wind turbine blade body formed of FRP, comprising the steps of: a first thermal spraying step of performing thermal spraying in the blade span direction; a chord position changing step of changing a position so that the protective layer formed in the first thermal spraying step is sprayed at an adjacent position in the chord direction; a second thermal spraying step of performing thermal spraying in the blade span direction at the adjacent position; A method for constructing a leading edge protective layer for a wind turbine blade having the above structure.

2. The wind turbine blade leading edge protective layer construction method according to claim 1 , wherein the chord position changing step changes a position in the chord direction from one blade surface of the wind turbine blade body to the other blade surface via a leading edge.

3. 2. The wind turbine blade leading edge protective layer construction method according to claim 1, further comprising an end thermal spraying step of spraying an end portion of the protective layer formed on the blade surface of the wind turbine blade body in such a manner that the thickness of the end portion in the chord direction and / or the blade length direction becomes gradually smaller toward the edge.

4. 2. The wind turbine blade leading edge protective layer construction method according to claim 1, wherein the dimension of the wind turbine blade body in the blade span direction is 80 m or more.

5. A protective layer for a wind turbine blade provided at a leading edge portion in a blade span direction of a wind turbine blade body formed of FRP, A protective layer for a wind turbine blade, the thickness of an end portion in a chord direction of the protective layer formed on the blade surface of the wind turbine blade body being gradually reduced toward the edge.

Citation Information

Patent Citations

  • Method for coating inner surface of metallic cylinder

    JP1989252762A

  • Blade structure and manufacturing method of blade structure

    JP2022175830A