Processing method and processing system

By forming a separation region on substrates before bonding using laser irradiation, the method addresses warpage issues in polymerized substrates, ensuring uniform bonding and reducing stress distribution for improved structural integrity.

JP2024149054AInactive Publication Date: 2024-10-18TOKYO ELECTRON LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023062723
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-07
Publication Date
2024-10-18
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods for bonding substrates can lead to warpage in polymerized substrates due to stress generated at the peripheral sagging portions during bonding, which is not effectively addressed by prior surface treatments.

Method used

A method involving forming a separation region on each substrate before bonding by irradiating a laser to separate the laminated film from the substrate's peripheral edge, reducing stress and preventing warpage through controlled separation and bonding processes.

Benefits of technology

The method effectively suppresses warpage in polymerized substrates by minimizing stress distribution and ensuring uniform bonding, thereby improving the integrity of the bonded structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024149054000001_ABST
    Figure 2024149054000001_ABST
Patent Text Reader

Abstract

To suppress a polymerization substrate, formed by joining substrates together, from warping.SOLUTION: The present invention relates to a processing method before a first substrate and a second substrate for forming a polymerization substrate are joined together, and the processing method includes: forming films on the first substrate and the second substrate; and emitting laser light so that the film formed on the first substrate forms an isolation region isolated from the first substrate at a peripheral edge part of the first substrate. The isolation region preferably has its formation width controlled according to a tendency of strain in a circumferential direction of the first substrate.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a processing method and a processing system. [Background technology]

[0002] Patent Document 1 discloses a bonding apparatus for bonding substrates together. Prior to bonding, the substrates to be bonded are subjected to a surface modification treatment for modifying the substrate surfaces and a hydrophilization treatment for making the modified substrate surfaces hydrophilic. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japan Patent No. 6231937 Summary of the Invention [Problem to be solved by the invention]

[0004] The technology according to the present disclosure suppresses the occurrence of warping in a laminated substrate formed by bonding substrates together. [Means for solving the problem]

[0005] One aspect of the present disclosure is a pre-bonding method for a first substrate and a second substrate to form an overlapped substrate, in which a film is formed on each of the first substrate and the second substrate, and laser light is irradiated to form an edge region at a peripheral portion of the first substrate where the film formed on the first substrate is separated from the first substrate. Effect of the Invention

[0006] According to the present disclosure, in a laminated substrate formed by bonding substrates together, the occurrence of warping in the laminated substrate is suppressed. [Brief description of the drawings]

[0007] [Figure 1]1A to 1C are diagrams illustrating the mechanism by which warpage occurs in a wafer according to a conventional method. [Diagram 2] FIG. 2 is an explanatory diagram of a wafer to be processed. [Diagram 3] 1 is a plan view showing an outline of the configuration of a processing system according to an embodiment of the present invention. [Figure 4] FIG. 2 is a plan view showing an outline of the configuration of the separation device. [Diagram 5] FIG. 2 is a cross-sectional view showing an outline of the configuration of a separation device. [Figure 6] FIG. 2 is a cross-sectional view showing an outline of the configuration of a joining unit. [Figure 7] 1A to 1C are explanatory views showing main steps of wafer processing. [Figure 8] 4 is a cross-sectional view for explaining an edge region, a peripheral modification layer, and an adhesive strength reduction region formed on a wafer. FIG. [Figure 9] FIG. 1 is a flow diagram showing main steps of wafer processing. [Figure 10] FIG. 1 is an explanatory diagram of a distortion occurring in a wafer. [Figure 11] 11A to 11C are explanatory diagrams showing other examples of forming the edge region. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] In a three-dimensional integration technology for stacking semiconductor devices three-dimensionally, as disclosed in Patent Document 1, two semiconductor wafers (hereinafter simply referred to as "wafers") are bonded together. A wafer is an example of a substrate. On the surfaces of the wafers to be bonded, for example, an insulating film and a device layer including a plurality of devices are formed. In addition, various pretreatments such as a chemical-mechanical polishing (CMP) process, a surface modification process, or a surface hydrophilization process are performed on the surfaces of the wafers to be bonded prior to bonding the wafers together.

[0009] However, when the wafers are bonded together, the surface condition of each of the two wafers before bonding may cause bonding distortion, which may result in warping of the resulting laminated wafer. Specifically, as shown in FIG. 1(a), the above-mentioned pretreatment may cause the thickness of the laminated film F at the edge portion We to be smaller than the thickness of the laminated film F at the center portion Wc (hereinafter, the portion of the laminated film F with a smaller thickness is referred to as the "sagging portion S"). In this case, the sagging portions S of the laminated film F are bonded together when the wafers W are bonded together, generating stress σ as shown in FIG. 1(b), which then spreads inside the wafer W and causes warping.

[0010] The technology according to the present disclosure has been made in consideration of the above circumstances, and suppresses warping of a laminated substrate formed by bonding substrates together. Hereinafter, a processing method according to the present embodiment and a processing system for realizing the processing method will be described with reference to the drawings. In this specification and the drawings, elements having substantially the same functional configuration are denoted by the same reference numerals, and duplicated explanations will be omitted.

[0011] In the processing system 1 described later, various processes are performed on a wafer W as a substrate shown in FIG. 2. Hereinafter, in the bonding device described later, the wafer placed on the upper side is referred to as the "first wafer W1", and the wafer placed on the lower side is referred to as the "second wafer W2". In addition, the bonding surface of the first wafer W1 to be bonded to the second wafer W2 is referred to as the "front surface W1a", and the opposite surface is referred to as the "back surface W1b". Similarly, the bonding surface of the second wafer W2 to be bonded to the first wafer W1 is referred to as the "front surface W2a", and the opposite surface is referred to as the "back surface W2b". In the following description, the first wafer W1 and the second wafer W2 may be collectively referred to as the "wafer W", the front surface W1a and the front surface W2a may be collectively referred to as the "front surface Wa", and the back surface W1b and the back surface W1b may be collectively referred to as the "back surface Wb".

[0012] The wafer W is a semiconductor wafer such as a silicon substrate, and at least one film is laminated on the front surface Wa. Hereinafter, the film formed on the front surface Wa is referred to as a "laminated film F". In this embodiment, the laminated film F includes a device layer D and a bonding film B as a film. The device layer D includes a plurality of devices. The bonding film B is, for example, an oxide film (THOX film, SiO2 film, TEOS film), a SiC film, a SiCN film, or an adhesive. The first wafer W1 and the second wafer W2 are bonded to each other at their front surfaces Wa via the bonding film B, and a laminated wafer T is formed as a laminated substrate. The peripheral portion We of the wafer W is chamfered, and the cross section of the peripheral portion We becomes thinner toward its tip. The peripheral portion We is a portion to be removed by edge trimming, which will be described later, and is, for example, in the range of 0.5 mm to 3 mm in the radial direction from the outer end of the wafer W. Further, in the peripheral portion We, a sagging portion S is formed where the thickness of the laminated film F (bonding film B) is smaller than that of the central portion Wc.

[0013] 2 illustrates an example in which the first wafer W1 and the second wafer W2 are both device wafers on which a device layer D is formed. However, the configuration of the first wafer W1 and the second wafer W2 is not limited to this, and one of them may be a support wafer on which a device layer D is not formed, for example, a wafer that supports the other wafer W. 2 illustrates an example in which a device layer D and a bonding film B are formed as a laminated film F on the surface of the wafer W. However, the type and number of films formed on the surface Wa of the wafer W are not limited to this, and for example, a laser absorbing film (not shown) for absorbing laser light for separation, which will be described later, may be formed on the interface between the wafer W and the laminated film F illustrated in FIG.

[0014] 3, the processing system 1 has a configuration in which a loading / unloading station 2 and a processing station 3 are integrally connected. In the loading / unloading station 2, for example, a cassette Ct capable of accommodating a plurality of first wafers W1, second wafers W2, or overlapped wafers T is loaded and unloaded between the loading / unloading station 2 and the outside. The processing station 3 includes various processing devices that perform desired processing on the first wafer W1, the second wafer W2, or the overlapped wafer T.

[0015] The carry-in / out station 2 is provided with a cassette mounting table 10 on which a cassette Ct is placed. A wafer transfer device 20 is provided on the X-axis positive side of the cassette mounting table 10. The wafer transfer device 20 moves on a transfer path 21 extending in the Y-axis direction, and is configured to be able to transfer a first wafer W1, a second wafer W2, or a laminated wafer T between the cassette Ct on the cassette mounting table 10 and transition devices 30, 31 described below.

[0016] In the loading / unloading station 2, on the positive X-axis side of the wafer transport device 20, a transition device 30 for transferring the first wafer W1 and the second wafer W2 between the processing station 3, and a transition device 31 for transferring the overlapped wafer T between the processing station 3 are provided.

[0017] In the processing station 3, a wafer transfer device 40, a separating device 50, a bonding device 60, a modifying device 70, an edge removing device 80 and a cleaning device 90 are arranged.

[0018] The wafer transport device 40 is provided on the X-axis positive side of the transition devices 30, 31. The wafer transport device 40 is configured to be freely movable on a transport path 41 extending in the X-axis direction, and is configured to be able to transport the first wafer W1, the second wafer W2, or the overlapped wafer T to the transition devices 30, 31, the separating device 50, the bonding device 60, the modifying device 70, the edge removing device 80, and the cleaning device 90 in the carry-in / out station 2.

[0019] In the separation apparatus 50, a laser beam (laser beam for separation, for example, a CO2 laser) is irradiated to the interface between the wafer W and the laminated film F or the inside of the laminated film F at the peripheral portion We of the wafer W, and the interface between the wafer W and the laminated film F, i.e., the interface between the wafer W and the device layer D or the interface between the wafer W and the bonding film B, is separated. For ease of explanation, the "interface between the wafer W and the laminated film F" may be expressed below to include the interface between the wafer W and the laminated film F and the inside of the laminated film F. The separation apparatus 50 also has a control device 51, which will be described later.

[0020] As shown in FIG. 4 and FIG. 5, the edge separation device 50 has a chuck 100 for holding the wafer W. In order to suppress damage to the bonding film B and the device layer D formed on the front surface Wa of the wafer W, it is preferable that the chuck 100 holds the front surface Wa without contact, or holds the back surface Wb or the side end of the wafer W. The chuck 100 is supported by a slider table 102 via an air bearing 101. A rotation mechanism 103 is provided on the lower surface side of the slider table 102. The rotation mechanism 103 has a built-in motor as a driving source. The chuck 100 is configured to be rotatable around a vertical axis by the rotation mechanism 103 via the air bearing 101. The slider table 102 is configured to be movable on a rail 106 extending in the Y-axis direction on a base 105 via a moving mechanism 104 provided on the lower surface side. The driving source of the moving mechanism 104 is not particularly limited, but a linear motor is used, for example.

[0021] A laser head 110 is provided above the chuck 100. The laser head 110 has a lens 111. The lens 111 is a cylindrical member provided on the lower surface of the laser head 110, and irradiates a laser beam for separation onto the wafer W held by the chuck 100, more specifically, onto the laminated film F formed on the surface Wa of the wafer W, and onto the laser absorbing film formed at the interface between the wafer W and the laminated film F. As a result, a separation region R1 (see FIG. 7) is formed between the wafer W and the laminated film F at the peripheral portion We of the wafer W, which is preferably a separation region where the edge of the wafer W and the laminated film F is cut, and which can reduce at least the stress σ shown in FIG. 1 after the first wafer W1 and the second wafer W2 are bonded. In the separation region R1, as shown in FIG. 7(b) described later, it is preferable to completely separate the laminated film F from the wafer W, but it is sufficient to reduce the stress σ by at least reducing the adhesion force without separating the laminated film F from the wafer W. In other words, in the edge region R1, as long as the stress σ shown in FIG. 1 can be reduced, the laminated film F may be completely peeled off from the wafer W, or a part of it may remain in contact with the wafer W.

[0022] The laser head 110 is supported by a support member 112. The laser head 110 is configured to be movable up and down by an elevating mechanism 114 along a rail 113 extending in the vertical direction. The laser head 110 is also configured to be movable in the Y-axis direction by a moving mechanism 115. The elevating mechanism 114 and the moving mechanism 115 are each supported by a support column 116.

[0023] An imaging mechanism 120 is provided above the chuck 100 on the Y-axis positive side of the laser head 110. The imaging mechanism 120 includes at least one camera. An image captured by the camera is output to a control device 300, which will be described later. The separation device 50 grasps the position of the wafer W on the chuck 100 based on the image obtained by the imaging mechanism 120, and based on this, under the control of the control device 300, aligns the wafer W and determines the irradiation position of the laser light.

[0024] In the bonding apparatus 60, the surfaces Wa of the first wafer W1 and the second wafer W2 are bonded together by van der Waals forces and hydrogen bonds (intermolecular forces). Specifically, the bonding apparatus 60 includes, for example, a modification unit that activates the surfaces Wa of the first wafer W1 and the second wafer W2, a hydrophilization unit that hydrophilizes the surfaces Wa of the first wafer W1 and the second wafer W2, a bonding unit that bonds the first wafer W1 and the second wafer W2, and the like.

[0025] In a modification unit (not shown), for example, in a reduced pressure atmosphere, oxygen gas or nitrogen gas serving as a processing gas is excited to be turned into plasma and ionized. The oxygen ions or nitrogen ions are irradiated onto the surface Wa of the wafer W, so that the surface Wa is subjected to plasma processing and modified (activated) (surface modification processing). In a hydrophilization unit (not shown), a processing liquid is supplied onto a surface Wa of the wafer W while the wafer W held by, for example, a spin chuck is being rotated. Then, the supplied processing liquid is diffused on the surface Wa of the activated wafer W by centrifugal force, and the surface Wa is made hydrophilic (surface hydrophilization processing).

[0026] In the bonding unit, a first wafer W1 and a second wafer W2, whose surfaces Wa have been sequentially subjected to a surface modification treatment and a surface hydrophilization treatment, are bonded to each other. As shown in FIG. 6, the bonding unit includes a processing vessel 200, an upper chuck 210, a lower chuck 220, and a pushing unit 230.

[0027] The processing vessel 200 is configured so that the inside can be sealed. The processing vessel 200 is formed with a loading / unloading port for the wafer W (not shown), and the loading / unloading port is provided with a gate valve (not shown). The upper chuck 210 is provided on the top side of the processing vessel 200, and the lower chuck 220 is provided on the bottom side of the processing vessel 200.

[0028] The upper chuck 210 suction-holds the back surface W1b of the first wafer W1 on its lower surface. The upper chuck 210 is supported by an upper chuck stage 211 provided above the upper chuck 210. The upper chuck 210 is provided with a rotating unit 212. The rotating unit 212 rotates the upper chuck stage 211 and the upper chuck 210 around a vertical axis (θ-axis).

[0029] The lower chuck 220 holds the back surface W2b of the second wafer W2 by suction on its upper surface. The lower chuck 220 is provided below the upper chuck 210 and configured to be able to be arranged opposite the upper chuck 210. That is, the first wafer W1 held by the upper chuck 210 and the second wafer W2 held by the lower chuck 220 can be arranged to face each other. The lower chuck 220 is supported by a lower chuck stage 221 provided below the lower chuck 220. The lower chuck stage 221 is provided with a moving unit 222. The moving unit 222 moves the lower chuck stage 221 and the lower chuck 220 in the horizontal direction. The moving unit 222 also moves the lower chuck 220 in the vertical direction.

[0030] A pressing portion 230 that presses the center portion of the first wafer W1 from the back surface W1b side is provided on the upper surface of the upper chuck 210. The pressing portion 230 has an actuator portion 231 and a cylinder portion 232. The actuator portion 231 is inserted through a through hole 214 that passes through the center of the upper chuck 210 and the upper chuck stage 211 in the thickness direction, and is capable of being raised and lowered in the vertical direction. The actuator portion 231 is supported by a cylinder portion 232. The cylinder portion 232 moves the actuator portion 231 in the vertical direction by a drive portion having a built-in motor, for example. The pushing unit 230 controls the pressing load by the actuator unit 231, and controls the movement of the actuator unit 231 by the cylinder unit 232. The pushing unit 230 can bring the center of the first wafer W1 and the center of the second wafer W2 into contact with each other and press them when bonding the first wafer W1 and the second wafer W2, which will be described later.

[0031] The bonding device 60 may be provided with an inverting device (not shown) for inverting the front and back surfaces of the first wafer W1 that is transported to the bonding device 60 and adsorbed and held by the upper chuck 210. The first wafer W1 is transported to the bonding device 60 with the front surface W1a that has been subjected to the surface modification treatment and the surface hydrophilization treatment facing upward. However, by inverting the front and back surfaces by this inverting device, the back surface W1b can be held by the upper chuck 210.

[0032] In this embodiment, as described above, the modification unit, the hydrophilization unit, and the bonding unit are arranged in the same bonding apparatus 60. However, the configuration of the bonding apparatus 60 is not limited to this, and a surface modification apparatus (not shown) for performing a surface modification process, a surface hydrophilization apparatus (not shown) for performing a surface hydrophilization process, and a bonding apparatus (not shown) for bonding the first wafer W1 and the second wafer W2 may each be configured independently. In addition, in this embodiment, an example will be described in which the surface modification process and the surface hydrophilization process are each performed within the processing system 1, but the surface modification device and the surface hydrophilization device may be disposed outside the processing system 1, and multiple wafers W whose surfaces Wa have previously been subjected to the surface modification process and the surface hydrophilization process may be placed in a cassette Ct and transported into the processing system 1.

[0033] In addition, in this embodiment, an example is described in which the pressing part 230 presses the center of the first wafer W1 against the center of the second wafer W2 in the bonding unit; however, the configuration of the bonding unit is not limited to this, and any configuration may be used as long as it is capable of bonding the first wafer W1 and the second wafer W2.

[0034] In the modifying device 70, a modifying laser beam (e.g., a fiber laser or a YAG laser) is irradiated to the inside of the first wafer W1 to form a peripheral modified layer M (see FIG. 7) that serves as a base point for peeling off the peripheral portion We. The modifying device 70 also has a control device 71, which will be described later.

[0035] The modification device 70 has a similar configuration to the separation device 50, for example. That is, the modification device 70 may include a chuck for holding the overlapped wafer T, a laser head provided above the chuck, and an imaging mechanism. The chuck is configured to be movable in the horizontal direction and rotatable around a vertical axis. The laser head is configured to be movable in the horizontal direction and movable up and down. The laser head is configured to be able to irradiate the above-mentioned modification laser light that is irradiated to the inside of the first wafer W1, instead of the laser light for separation in the separation device 50.

[0036] In the edge removal device 80, the edge portion We of the first wafer W1 is removed, i.e., edge trimmed, using the separation region R1 formed in the separation device 50 and the edge modified layer M formed in the modification device 70 as base points. Any method for edge trimming can be selected. In one example, the edge removal device 80 may insert, for example, a wedge-shaped blade into the interface between the first wafer W1 and the second wafer W2. Also, for example, an air blow or a water jet may be sprayed toward the edge portion We to apply an impact to the edge portion We.

[0037] The cleaning device 90 performs a cleaning process on the first wafer W1 and the second wafer W2 after the edge trimming by the edge removal device 80, and removes particles on these wafers W. The cleaning device 90 also removes the laminated film F (residual film) remaining on the peripheral portion of the second wafer W2 after the edge trimming by the edge removal device 80. Any cleaning method can be selected. In one example, the cleaning device 90 may clean the wafer W by irradiating a desired position of the wafer W with a cleaning laser light (e.g., an IR laser or a solid-state laser). Also, for example, the wafer W may be scrubbed.

[0038] The above-mentioned processing system 1 is provided with a control device 51, a control device 71, and a control device 300. The control device 51 controls the operation of the separation device 50 individually. The control device 71 controls the operation of the modification device 70 individually. The control device 300 controls a series of wafer processing in the processing system 1. The control devices 51, 71, and 300 are, for example, computers and have a program storage unit (not shown). The program storage unit stores programs for controlling various processes in the processing system 1. The above-mentioned programs may be recorded in a computer-readable storage medium H and installed from the storage medium H to the control device 300. The above-mentioned storage medium H may be temporary or non-temporary.

[0039] In this embodiment, the control device 51 and the control device 71 are installed separately for the separation device 50 and the reformer 70, respectively, but these control devices 51 and 71 may be configured integrally with the control device 300. In other words, the operations of the separation device 50 and the reformer 70 may be controlled by the control device 300.

[0040] Next, a method for processing the wafer W using the processing system 1 configured as above will be described.

[0041] First, cassettes Ct each containing a plurality of first wafers W1 and second wafers W2, and an empty cassette Ct are placed on the cassette placement plate 11 of the load / unload station 2. Next, the first wafer W1 is removed from the cassette Ct by the wafer transfer device 22 and transferred to the transition device 30 of the processing station 3.

[0042] Next, the first wafer W1 is transported to the separation apparatus 50 by the wafer transport apparatus 40. In the separation apparatus 50, in one example, the back surface W1b side of the first wafer W1 is held by the chuck 100 with the front surface W1a side facing up. At this time, the chuck 100 holds a portion of the first wafer W1 different from the irradiation position (periphery We) of the modifying laser light, for example, the central portion Wc, and irradiates the laser light from below (the back surface W1b side), thereby suppressing damage to the bonding film B and the device layer D formed on the front surface W1a side.

[0043] It should be noted that the method of holding the first wafer W1 in the separation device 50 and the method of irradiating the laser light are not limited to this, and for example, the laser light may be irradiated from above (the back surface W1b side) by grasping the outer peripheral edge of the first wafer W1 with the back surface W1b side of the first wafer W1 facing upward. Alternatively, for example, with the back surface W1b of the first wafer W1 facing upward, the back surface W1b side of the first wafer W1, for example the central portion Wc, may be held and irradiated with laser light from above (the back surface W1b side). Alternatively, for example, with the front surface W1a of the first wafer W1 facing upward, the outer peripheral edge of the first wafer W1 may be gripped, and the laser light may be irradiated from below (the back surface W1b side).

[0044] Next, in the separation device 50, while rotating the first wafer W1 and moving it horizontally along the Y-axis direction, a laser beam is irradiated onto the laminated film F from the back surface W1b side of the first wafer W1. Preferably, the laser beam is irradiated onto the laminated film F in a range corresponding to the peripheral portion We of the first wafer W1. As a result, as shown in Figs. 7(a) and 8, the laminated film F (bonding film B or device layer D) is detached from the first wafer W1 at the peripheral portion We, and a separation region R1 where the edge of the first wafer W1 and the laminated film F is cut is formed (S1 in Fig. 9).

[0045] In the separation device 50, a separation region R1 is formed in a range corresponding to the peripheral portion We in this manner. In the bonding of the first wafer W1 and the second wafer W2 described below, as described above, the bonding of the sagging portions S may cause stress σ to be generated inside the wafer W, which may lead to warping (see FIG. 1). However, the presence of the separation region R1 in this manner prevents the stress σ from spreading inside the wafer W even if the sagging portions S are bonded to each other, and as a result, warping of the laminated wafer T to be formed can be suppressed.

[0046] The formation range of the edge region R1 is desirably set as an annular region that is approximately the same as or slightly smaller than the trim width of the peripheral portion We in the radial direction from the outer end of the first wafer W1. This makes it possible to at least suppress warping of the formed overlapped wafer T and to suppress chipping in a later process.

[0047] Next, the first wafer W1 is transported to the bonding device 60 by the wafer transport device 40. The first wafer W1 transported into the bonding device 60 is subjected to a surface modification process and a surface hydrophilization process in a modification unit and a hydrophilization unit (not shown) in sequence (S2 in FIG. 9), and then the front and back surfaces are reversed by a reversing device (not shown) (S3 in FIG. 9), and the back surface W1b side is attracted and held by the upper chuck 210.

[0048] While the first wafer W1 is being subjected to the various processes (S1 to S3) described above, the second wafer W2 is being processed following the first wafer W1. First, the second wafer W2 is removed from the cassette Ct by the wafer transfer device 22 and transferred to the transition device 30 in the processing station 3.

[0049] Next, the second wafer W2 is transferred to the separation device 50 by the wafer transfer device 40, and a separation region R1 is formed at the interface between the second wafer W2 and the laminated film F (S4 in FIG. 9). The separation process (S4) for the second wafer W2 is the same as the above-described separation process (S1) for the first wafer W1.

[0050] Next, the second wafer W2 is transported to the bonding device 60 by the wafer transport device 40. The second wafer W2 transported into the bonding device 60 is subjected to a surface modification process and a surface hydrophilization process in a modification unit and a hydrophilization unit (not shown) in sequence (S5 in FIG. 9), and then the back surface W2b side of the second wafer W2 is adsorbed and held by the lower chuck 220.

[0051] Next, a bonding process is performed between the first wafer W1 and the second wafer W2 (S6 in FIG. 9). Specifically, the actuator unit 231 presses the center of the back surface W1b of the first wafer W1 and lowers it, bringing the center of the first wafer W1 and the center of the second wafer W2 into contact and pressing them together. This generates van der Waals forces (intermolecular forces) and hydrogen bonds between the surfaces W1a and W2a, and the surfaces W1a and W2a are bonded together. Thereafter, the bonding between the surfaces W1a and W2a due to van der Waals forces and hydrogen bonds diffuses from the center toward the outer periphery, and when the surface W1a of the first wafer W1 and the surface W2a of the second wafer W2 come into contact with each other over their entire surfaces, the bonding process between the first wafer W1 and the second wafer W2 is completed as shown in FIG. 7(b).

[0052] The overlapped wafer T formed in the bonding device 60 is then transported to the modification device 70 by the wafer transport device 40. In the modification device 70, a laser beam is irradiated onto the overlapped wafer T on the chuck based on a predetermined removal width of the peripheral edge portion We, and a modification process is performed on the overlapped wafer T (S7 in FIG. 9). Specifically, in the modification device 70, an internal laser beam is irradiated to the inside of the first wafer W1 to form a peripheral modified layer M as shown in FIG. 7(c) and FIG. 8. The peripheral modified layer M serves as a base point for removing the peripheral portion We in the edge trimming described below. In addition, a crack C extends from the peripheral modified layer M formed in the thickness direction of the first wafer W1. In the inside of the first wafer W1, the crack C extends from the peripheral modified layer M formed closest to the front surface W1a of the first wafer W1 toward the radially inner end of the separation region R1 formed by the separation device 50. The crack C serves as a base point for removing the peripheral portion We, similar to the peripheral modified layer M.

[0053] In the above, the formation position of the peripheral modified layer M is determined according to the preset removal (trim) width of the peripheral portion We, but the formation position of the peripheral modified layer M may be determined based on the separation region R1 formed by the separation device 50, for example. More specifically, the peripheral modified layer M may be formed by irradiating the inner laser light along the radially inner end of the separation region R1 formed by the separation device 50. In this way, the formation position of the peripheral modified layer M may be determined so that the peripheral modified layer M is not radially outward from the radially inner end of the separation region R1.

[0054] The overlapped wafer T on which the peripheral modified layer M has been formed is then transferred by the wafer transfer device 40 to the peripheral removal device 80. In the edge removing device 80, as shown in Fig. 7(d), the edge We of the first wafer W1 is removed, i.e., edge trimmed (S8 in Fig. 9). At this time, the edge We is peeled from the center (the radially inner side of the edge We) of the first wafer W1 using the peripheral modified layer M as a base point, and is completely peeled from the second wafer W2 using the separation region R1 as a base point. In removing the edge We, for example, a wedge-shaped blade may be inserted into the interface between the first wafer W1 and the second wafer W2 that form the overlapped wafer T.

[0055] The overlapped wafer T from which the peripheral edge portion We of the first wafer W1 has been removed is then transferred by the wafer transfer device 40 to the cleaning device 90. In the cleaning apparatus 90, the first wafer W1 and / or the second wafer W2 after the peripheral portion We has been removed are cleaned (S9 in FIG. 9). More specifically, in the cleaning apparatus 90, a laminated film F (residual film) remaining on the peripheral portion We of the second wafer W2 exposed by the removal of the peripheral portion We of the first wafer W1 is removed. In the cleaning apparatus 90, as shown in FIG. 7(e), for example, a cleaning laser light may be irradiated onto the first wafer W1 and the second wafer W2 to modify and remove the irradiated portions of the laser light, thereby removing (cleaning) the residual film, particles, and the like.

[0056] In the illustrated example, all of the laminate film F remaining on the peripheral portion of the second wafer W2 is removed in the cleaning apparatus 90, but the amount of the laminate film F removed is not limited to this, and the laminate film F may remain on the second wafer W2 depending on the purpose of the wafer processing in the subsequent process, etc.

[0057] Thereafter, the laminated wafer T on which all the processes have been performed is transferred by the wafer transfer device 20 to an empty cassette Ct on the cassette mounting table 10 via the transition device 31. In this manner, a series of substrate processing steps in the processing system 1 is completed.

[0058] As described above, according to the processing system 1 of this embodiment, prior to bonding of the first wafer W1 and the second wafer W2 in the bonding device 60, a separation region R1 where the wafer W and the laminated film F are separated is formed at the peripheral portion We of the wafer W. As a result, even if a sagging portion S occurs at the peripheral portion We of the wafer W and the laminated film F is bonded to each other, the edge of the wafer W and the laminated film F is cut, so that the spread of the stress σ caused by the bonding distortion is suppressed, and as a result, the occurrence of warping in the generated laminated wafer T can be suppressed.

[0059] In the above embodiment, in the separation apparatus 50, the separation region R1 where the wafer W and the laminated film F are separated is formed with a uniform width (see Figure 8) around the entire circumferential direction of the wafer W, but the formation width of the separation region R1 is not limited to this. Specifically, the bonding strain generated during bonding of the first wafer W1 and the second wafer W2 affects the crystal orientation of the first wafer W1 and the second wafer W2 to be bonded and the pattern formed on the front surface Wa. More specifically, the bonding strain generated in the wafer W may increase in a direction in increments of 45 degrees with respect to a notch Wn formed for detecting the orientation of the rotation direction of the wafer W as a reference, as shown in FIG. 10 as an example.

[0060] In view of this, it is desirable to control the width of the edge region R1 formed in the edge separation device 50 according to the tendency of distortion in the circumferential direction of the wafer W caused by the crystal orientation or pattern. Specifically, for example, in the example shown in FIG. 10, it is desirable to make the width of the edge region R1 formed in the direction of 45 degrees where the distortion is large larger than in other directions. This makes it possible to uniformly control the magnitude of the bonding distortion generated over the entire circumference of the generated overlapped wafer T, and more appropriately suppress the occurrence of warping in the overlapped wafer T. In addition, compared to the case where the edge region R1 is formed with a uniform width over the entire circumference of the wafer W, the formation range of the edge region R1 (the irradiation range of the laser light) can be made smaller, and as a result, the time required for the edge separation process in the edge separation device 50 can be shortened.

[0061] Furthermore, even in this way, when the formation width of the isolated region R1 is controlled according to the tendency of distortion in the circumferential direction of the wafer W, the formation position of the peripheral modified layer M may be determined along the radially inner end of the isolated region R1 as described above. Therefore, the removal (trim) width of the peripheral portion We of the first wafer W1 may be determined according to the formation width of the isolated region R1 according to the tendency of distortion in the circumferential direction of the first wafer W1.

[0062] In the above embodiment, as shown in Fig. 7, the separation region R1 is formed in both the first wafer W1 and the second wafer W2 constituting the overlapped wafer T, but the formation of the separation region R1 may be omitted in either the first wafer W1 or the second wafer W2 as shown in Fig. 11. Even when the separation region R1 is formed in only one of the two wafers W to be bonded in this manner, since the edge between the wafer W and the laminated film F is cut in at least one of the wafers W, the spread of the stress σ caused by bonding the sagging portions S to each other is suppressed, and the occurrence of warping in the overlapped wafer T can be suppressed. In addition, by forming the separation region R1 on only one of the wafers W in this manner, the number of wafers to be processed in the separation process in the separation device 50 can be reduced compared to the case where the separation region R1 is formed on both wafers W. Therefore, the number of steps (specifically, S1 or S4 in FIG. 9) in the processing system 1 can be reduced, and the throughput of the wafer processing can be improved.

[0063] In particular, when forming the edge region R1 only on the first wafer W1, which is the target for removing the peripheral portion We, a laminated film F can be left on the surface W2a of the second wafer W2 after edge trimming, and this laminated film F can be used as a protective film in subsequent processes. On the other hand, when forming the edge region R1 only on the second wafer W2, for example, in cases where the laser light cannot pass through the first wafer W1 (the edge region R1 cannot be formed on the first wafer W1 side) due to the influence of the structure of the wafer W, the occurrence of warping in the overlapping wafer T can be appropriately suppressed.

[0064] In the above embodiment, the separation device 50 forms the separation region R1 at the interface between the wafer W and the laminated film F, but for example, when a plurality of films are laminated on the front surface Wa of the wafer W, if at least the film in which the sagging portion S is formed (thickness at the peripheral portion is smaller than that at the central portion) is separated from the wafer W, the occurrence of warpage in the laminated wafer T described above can be suppressed. Therefore, when a plurality of films are laminated on the front surface Wa of the wafer W, the separation region R1 may be formed at the interface between the laminated films instead of at the interface between the wafer W and the laminated film F.

[0065] In this way, when an edge region R1 is formed other than at the interface between the surface Wa of the wafer W and the laminate film F, for example, inside the laminate film F, edge trimming can be performed by extending the crack C to the radially inner end of this edge region R1, thereby reducing the thickness of the laminate film F remaining on the surface W2a of the second wafer W2 after edge trimming, and shortening the time required for the subsequent cleaning process (S9 in Figure 9).

[0066] In the above embodiment, the processing system 1 is provided with the edge separation device 50, the bonding device 60, the modification device 70, the edge removal device 80, and the cleaning device 90. However, the configuration of the processing system 1 is not limited to this, and the edge separation device 50 and the bonding device 60 may be provided independently of the processing system 1. In other words, a first processing system for performing edge separation processing, a second processing system for performing bonding processing, and a third processing system for performing modification processing, edge trimming, and cleaning processing may each be configured independently.

[0067] The embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The above-described embodiments may be omitted, substituted, or modified in various forms without departing from the scope and spirit of the appended claims. For example, the components of the above-described embodiments may be arbitrarily combined. From such an arbitrary combination, the actions and effects of each of the components in the combination can be obtained as a matter of course, and other actions and effects that are obvious to a person skilled in the art from the description of this specification can be obtained.

[0068] In addition, the effects described in this specification are merely explanatory or exemplary and are not limiting. In other words, the technology according to the present disclosure may achieve other effects that are apparent to a person skilled in the art from the description of this specification in addition to or in place of the above effects. [Explanation of symbols]

[0069] 1 Processing System 50 Separation device 300 Control device F Laminated film R1 Remote region T Polymer Wafer W1 First wafer W2 Second wafer Wa Surface We Periphery

Claims

1. 1. A method for treating a first substrate and a second substrate prior to bonding to form a laminated substrate, comprising the steps of: A film is formed on each of the first substrate and the second substrate, A processing method comprising: irradiating a laser beam to form an isolated region in which the film formed on the first substrate is isolated from the first substrate at a peripheral portion of the first substrate.

2. 1. A method for bonding a first substrate and a second substrate to form a laminated substrate, comprising the steps of: A film is formed on each of the first substrate and the second substrate, irradiating a laser beam to form an isolated region in which a film formed on the first substrate is isolated from the first substrate at a peripheral portion of the first substrate; and bonding the first substrate and the second substrate together via the film to form the polymerized substrate.

3. When forming the edge region, The processing method according to claim 1 , further comprising controlling a formation width of the edge region in accordance with a tendency of distortion in a circumferential direction of the first substrate.

4. 3. The processing method according to claim 1, further comprising: irradiating a laser beam to form an isolated region in which the film formed on the second substrate is isolated from the second substrate in a region corresponding to a peripheral portion of the first substrate.

5. When forming the edge region, The processing method according to claim 4 , further comprising controlling a formation width of the edge region in accordance with a tendency of distortion in a circumferential direction of the second substrate.

6. After forming the polymerized substrate, Irradiating a laser beam along a boundary between the peripheral portion of the first substrate and a central portion of the first substrate to form a peripheral modified layer that serves as a base point for peeling off the peripheral portion; The method of claim 2 , further comprising: peeling the peripheral portion from the laminated substrate using the peripheral modification layer and the isolated region as starting points.

7. The method according to claim 6 , wherein a position at which the peripheral modified layer is formed is determined based on a width at which the isolated region is formed.

8. The processing method according to claim 6 or 7, further comprising removing the film remaining on the peripheral edge of the second substrate after removing the peripheral edge.

9. 1. A processing system for processing a first substrate and a second substrate to form a laminated substrate, comprising: A film is formed on each of the first substrate and the second substrate, a separation device that irradiates a laser beam to form a separation region in which the film formed on the first substrate is separated from the first substrate at a peripheral portion of the first substrate; A processing system comprising: a controller.

10. The processing system according to claim 9 , further comprising a bonding device configured to bond the first substrate and the second substrate via the film to form the polymerized substrate.

11. The control device, when forming the edge region, The processing system according to claim 9 or 10, wherein control is executed to change a formation width of the edge region in accordance with a tendency of distortion of the first substrate.

12. The separation device comprises:

11. The processing system according to claim 9, further comprising: a processing unit configured to irradiate a laser beam to form an edge region in which the film formed on the second substrate is separated from the second substrate in a region corresponding to a peripheral portion of the first substrate.

13. The control device, when forming the edge region, The processing system according to claim 12 , further comprising a control for changing a formation width of the edge region in response to a tendency of distortion of the second substrate.

14. a modification device that irradiates a laser beam along a boundary between the peripheral portion of the first substrate and a central portion of the first substrate to form a peripheral modified layer that serves as a base point for peeling off the peripheral portion; The processing system according to claim 10 , further comprising: a peripheral removal device that peels off the peripheral portion from the laminated substrate using the peripheral modification layer and the isolated region as starting points.

15. The control device includes: The processing system according to claim 14 , further comprising a control for determining a position where the peripheral modified layer is formed in the modifying device based on a width of the isolated region formed in the isolated device.

16. The processing system according to claim 14 , further comprising a cleaning device that removes the film remaining on the peripheral edge of the second substrate after the peripheral edge is removed by the peripheral edge removal device.

Citation Information