Minute vibrating body, inertia sensor, manufacturing method of minute vibrating body, and manufacturing method of inertia sensor
A micro-vibrator with a Ti-containing nitride surface electrode formed via atomic layer deposition addresses the thickness and bonding issues of existing micro-vibrators, maintaining vibration quality and ensuring reliable adhesion and conductivity.
Patent Information
- Application Number
- JP2023062932
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-07
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2043-04-07
AI Technical Summary
The existing micro-vibrators in inertial sensors, such as those described in Patent Document 1, face issues with increased thickness of the surface electrode due to a laminated structure, leading to decreased Q value of vibration, potential insulation from heat migration, and poor bonding with the mounting board.
A micro-vibrator with a surface electrode made of a nitride film containing Ti as a main component, formed using atomic layer deposition, which ensures adhesion and conductivity without a laminated structure, maintaining the total thickness below a predetermined value.
The solution maintains the Q value of vibration, ensures good adhesion and conductivity, and prevents poor bonding with the mounting board, enhancing the sensitivity and reliability of the inertial sensor.
Smart Images

Figure 2024149200000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a micro-vibrator having a glass structure having a three-dimensional curved surface covered with a conductive film, an inertial sensor using the micro-vibrator, and a method for manufacturing the micro-vibrator and the inertial sensor. [Background technology]
[0002] In recent years, the development of autonomous driving systems for vehicles has progressed, and this type of system requires highly accurate self-location estimation technology. For example, a self-location estimation system equipped with GNSS and IMU is being developed for so-called level 3 autonomous driving. GNSS is an abbreviation for Global Navigation Satellite System. IMU is an abbreviation for Inertial Measurement Unit, and is, for example, a 6-axis inertial force sensor consisting of a 3-axis gyro sensor and a 3-axis acceleration sensor. In order to realize so-called level 4 or higher autonomous driving in the future, an IMU with even higher sensitivity than the current one will be required.
[0003] BRG is considered to be a promising gyro sensor for realizing such a high-sensitivity IMU, and is made up of a micro-vibrator with a roughly hemispherical three-dimensional curved surface that vibrates in wine glass mode, mounted on a mounting board. BRG is an abbreviation for Bird-bath Resonator Gyroscope. This micro-vibrator has a Q value, which represents the state of vibration, of 10 6 This is expected to result in higher sensitivity than before.
[0004] For example, the micro-vibrator described in Patent Document 1 has a base made of glass, the surface of which is covered with a surface electrode. This micro-vibrator has a surface electrode covering the surface made of a material such as Ti (titanium)-Pt (platinum) or Cr (chromium)-Au (gold), and is configured by laminating an adhesive layer and a conductive layer in this order from the base. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] U.S. Pat. No. 1,061,2925 Summary of the Invention [Problem to be solved by the invention]
[0006] The micro-vibrator described in Patent Document 1 requires that the surface electrode be a laminated structure of an adhesive layer and a conductive layer, and the total thickness of the surface electrode is large, which reduces the Q value of the vibration. Furthermore, if the total thickness of the surface electrode with such a structure, particularly the thickness of the adhesive layer, is made thin, it may become insulated due to migration caused by heat in the process of manufacturing the micro-vibrator, or the adhesion with the base may decrease, causing the film to peel off, or poor bonding with the mounting board may occur.
[0007] In view of the above, the present invention aims to provide a micro-vibrator and a manufacturing method thereof that suppresses the thickness of the surface electrode to a predetermined value or less, suppresses a decrease in the Q value of vibration, ensures the conductivity and adhesion of the surface electrode, and suppresses poor bonding to the mounting substrate.The present invention also aims to provide an inertial sensor using a micro-vibrator that simultaneously ensures the conductivity and adhesion of the surface electrode and suppresses poor bonding to the mounting substrate, and a manufacturing method thereof. [Means for solving the problem]
[0008] In order to achieve the above object, the micro-vibrator described in claim 1 is a micro-vibrator capable of vibrating in a wine glass mode, and comprises a base (20) having a curved portion (21) having an annular curved surface, a bottomed cylindrical connection portion (22) recessed from the surface (21a) of the curved portion toward the center of the imaginary hemisphere formed by the curved portion, and a surface electrode (23) covering at least a portion of the surface of the base, the base being made of glass, and the surface electrode being a nitride film formed by atomic layer deposition and containing Ti as its main component.
[0009] This results in a micro-vibrator having a curved surface portion and a connection portion, and a surface electrode made of a nitride mainly composed of Ti formed by atomic layer deposition on the surface of a base made of glass. Since the surface electrode of this micro-vibrator is made of a nitride mainly composed of Ti and has adhesion to the base made of glass, it is not necessary to form an adhesion layer and a conductive layer into a laminated structure, and the adhesion and conductivity of the surface electrode are ensured while the total thickness of the surface electrode is set to a predetermined value or less. Furthermore, since the adhesion and conductivity of the surface electrode are ensured, poor bonding to the mounting board is suppressed.
[0010] The manufacturing method of a micro-vibrator according to claim 4 is a manufacturing method of a micro-vibrator capable of vibrating in a wine glass mode, and includes the steps of: preparing a base (20) made of glass, the base having a curved surface portion (21) having an annular curved surface and a cylindrical connecting portion (22) with a bottom that is recessed from the surface (21a) of the curved surface portion toward the center of a virtual hemisphere formed by the curved surface portion; preparing a jig (J) having a support portion (J1) that is inserted into the connecting portion and can support the base; and forming a surface electrode (23) that covers the surface by an atomic layer deposition method while the support portion is inserted into the connecting portion and the base is held by the jig. In forming the surface electrode, the base is held in a state where it is not in contact with parts of the jig that are different from the support portion, and a nitride film mainly composed of Ti is formed.
[0011] This results in a method for manufacturing a micro-vibrator that includes preparing a base having a curved surface portion and a connection portion and made of glass, setting the base on a jig having a support portion, and forming a nitride film mainly composed of Ti by atomic layer deposition to form a surface electrode. By forming a nitride film mainly composed of Ti on glass, it is possible to ensure the adhesion and conductivity of the surface electrode while keeping the total thickness of the surface electrode below a predetermined value, and to manufacture a micro-vibrator in which poor bonding with a mounting board is suppressed.
[0012] The inertial sensor described in claim 7 comprises a base (20) having a curved portion (21) with an annular curved surface and a cylindrical connection portion (22) with a bottom that is recessed from the surface (21a) of the curved portion toward the center of a virtual hemisphere formed by the curved portion, a surface electrode (23) covering at least a portion of the surface of the base, a micro-vibrator (2) having a curved portion capable of vibrating in a wine glass mode, and a mounting substrate (3) to which the connection portion is joined, the mounting substrate having a rim (211) at the end of the curved portion opposite the connection portion and a plurality of electrode portions (53) arranged to surround the rim while being spaced apart from each other, the base being made of glass, and the surface electrode being a nitride film formed by atomic layer deposition and mainly composed of Ti.
[0013] As a result, the micro-vibrator described in claim 1 is bonded to a mounting substrate, the total thickness of the surface electrodes of the micro-vibrator is set to a predetermined value or less, and a decrease in the Q value of vibration is suppressed while the adhesion and conductivity of the surface electrodes are ensured, resulting in an inertial sensor in which poor bonding with the mounting substrate is suppressed.
[0014] The manufacturing method of an inertial sensor described in claim 8 is a manufacturing method of an inertial sensor in which a micro-vibrator (2) capable of vibrating in a wine glass mode is bonded to a mounting substrate (3), and includes the steps of: preparing a base (20) made of glass and having a curved surface portion (21) having an annular curved surface and a bottomed cylindrical connecting portion (22) recessed from a surface (21a) of the curved surface portion toward the center of a virtual hemisphere formed by the curved surface portion; preparing a jig (J) having a support portion (J1) that is inserted into the connecting portion and can support the base; inserting the support portion into the connecting portion, and forming a surface electrode (23) that covers the surface by atomic layer deposition while the base is held by the jig, thereby forming a micro-vibrator; preparing a mounting substrate and bonding the connecting portion of the micro-vibrator to the mounting substrate, and in forming the surface electrode, a nitride film mainly composed of Ti is formed.
[0015] This results in a method for manufacturing an inertial sensor that includes bonding the micro-vibrator manufactured by the method according to claim 4 to a mounting substrate. Since the total thickness of the surface electrodes of the micro-vibrator is set to a predetermined value or less, it is possible to manufacture an inertial sensor in which the adhesion and conductivity of the surface electrodes are ensured while suppressing a decrease in the Q value of vibration, and bonding defects with the mounting substrate are suppressed.
[0016] The reference symbols in parentheses attached to each component indicate an example of the correspondence between the component and specific components described in the embodiments described below. [Brief description of the drawings]
[0017] [Figure 1] 1 is a perspective view showing an example of an inertial sensor using a micro-vibrator according to an embodiment; [Diagram 2] 1 is a cross-sectional view of a micro-vibrator according to an embodiment. [Diagram 3] FIG. 2 is a cross-sectional view taken along line III-III in FIG. [Figure 4] FIG. 1 is a graph showing the relationship between the Ti—O ratio in a titanium oxynitride film and the bonding strength and resistance value. [Diagram 5] 11 is an explanatory diagram of a jig used in a film-forming process for a surface electrode of a micro-vibrator. FIG. [Figure 6] FIG. 6 is a perspective view showing a tip end surface of the jig in FIG. 5. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In the following embodiments, parts that are the same or equivalent to each other will be denoted by the same reference numerals.
[0019] (First embodiment) An inertial sensor 1 of a first embodiment will be described with reference to the drawings.
[0020] 1, in order to make the configuration of the inertial sensor 1 easier to understand, a lower substrate 4, an upper substrate 5, and a part of the micro-vibrator 2, which will be described later, of the inertial sensor 1 are omitted, and a cross-sectional configuration of the micro-vibrator 2 is partially shown. In FIG. 3, in order to make the configuration of the inertial sensor 1 easier to understand, the outlines of an electrode portion 53 and an electrode film 531, which will be described later and are located in another cross section, are indicated by dashed lines.
[0021] For the sake of convenience, as shown in FIG. 1, one direction in the plane of the mounting substrate 3 is referred to as the "x direction", a direction perpendicular to the x direction on the same plane is referred to as the "y direction", and a normal direction to the xy plane is referred to as the "z direction". The x, y, and z directions in FIG. 2 and subsequent figures correspond to the x, y, and z directions in FIG. 1, respectively. In addition, in this specification, "upper" refers to the direction along the z direction in the figure, and refers to the side indicated by the arrow, and "lower" refers to the opposite side to the upper side. Furthermore, in this specification, a state in which the inertial sensor 1, the micro-vibrator 2, or the mounting substrate 3 is viewed from above in the z direction may be referred to as a "top view".
[0022] 1, the micro-vibrator 2 according to the embodiment is preferably mounted on a mounting substrate 3 and used to configure an inertial sensor such as a gyro sensor like a BRG, but may also be used for other purposes such as a clock device, etc. In this specification, a case where it is used as a component of a BRG will be described as a representative example, but the use is not limited to this.
[0023] [Inertial Sensor] An example of an inertial sensor 1 having a micro-vibrator 2 will be described. As shown in Fig. 1, the inertial sensor 1 includes the micro-vibrator 2 and a mounting substrate 3, and a part of the micro-vibrator 2 is joined to the mounting substrate 3. The inertial sensor 1 is configured to detect an angular velocity applied to the inertial sensor 1 based on a change in electrostatic capacitance between a curved surface portion 21 of the thin-walled micro-vibrator 2 capable of vibrating in a wine glass mode and a plurality of electrode portions 53 of the mounting substrate 3.
[0024] As shown in Fig. 2, the micro-vibrator 2 has a base 20 covered with a surface electrode 23, the base 20 having a curved surface portion 21 including the outline of a three-dimensional curved surface of a substantially hemispherical shape and a connection portion 22 extending from the apex side of the imaginary hemisphere formed by the curved surface portion 21 toward the center side of the hemisphere. The connection portion 22 is a connection portion that is connected to another member such as a mounting board 3, and is, for example, a cylindrical recess with a bottom. The micro-vibrator 2 has, for example, a curved surface portion 21 that has a bowl-shaped three-dimensional curved surface, and the Q value of the vibration is 10 5 That's all.
[0025] The base 20 is made of a reflow material made of glass containing additives such as quartz glass, borosilicate glass, metal glass, silicon, etc. The base 20 is not limited to the above-mentioned material examples as long as it is made of glass capable of forming the curved surface portion 21 and the connection portion 22 having a three-dimensional curved shape and vibrating in wine glass mode. The base 20 is formed, for example, by processing a thin-walled base material made of the above-mentioned material in a forming process described later, so that the curved surface portion 21 and the connection portion 22 are thin members on the order of micrometers, with the thickness of the curved surface portion 21 and the connection portion 22 being 10 μm to 100 μm. The base 20 has a millimeter-sized shape, for example, with the height direction being along the thickness direction of the mounting substrate 3, with the dimension in the height direction being 2.5 mm, and the outer diameter of the surface 2a side of the rim 211 described later being 5 mm.
[0026] The base 20 is formed by, for example, setting a quartz plate having a thickness of 100 μm or less in a mold (not shown) having a recess and a support part that supports a part of the quartz plate at the center of the recess when the quartz plate is heated and softened, and evacuating the recess while softening it with a heating means such as a flame, thereby forming the curved surface part 21. For example, this process forms a connection part 22 in a shape of a bottomed cylinder recessed into the curved surface part 21 of the quartz plate supported by the support part of the mold (not shown), and the part protruding from the recess remains unprocessed, but is removed in a later process. Then, for example, the recess of the mold (not shown) is returned to normal pressure, and the quartz plate with the approximately hemispherical curved surface part 21 formed thereon is removed from the mold, and the quartz plate is sealed with a sealant made of any curable resin material. After that, for example, unnecessary parts of the quartz plate after processing are removed by polishing and CMP together with the sealant, and then the sealant is removed by any method such as heating or chemicals, and the quartz plate is taken out. CMP is an abbreviation for Chemical Mechanical Polishing. The base 20 is manufactured by, for example, the manufacturing process as described above, but is not limited to this manufacturing method example, and other known methods may be adopted. For example, the base 20 may be formed by removing unnecessary parts outside the curved surface portion 21 by laser processing without sealing the quartz plate on which the curved surface portion 21 and the connection portion 22 are formed.
[0027] The end of the curved surface portion 21 opposite to the connection portion 22 is the rim 211, and the rim 211 is, for example, substantially cylindrical. The substantially cylindrical shape here includes not only a cylindrical shape in which the diameter from the upper end to the lower end of the outer surface and the inner surface of the rim 211 is the same, but also a tubular shape in which the diameter from the upper end to the lower end varies. In other words, the curved surface portion 21 has the rim 211 that is an annular portion of an annular curved surface shape. The micro-vibrator 2 is mounted on the mounting board 3 with the surface 2a being the surface with the larger outer diameter and the opposite surface being the back surface 2b, such that the rim 211 faces the multiple electrode portions 53 of the mounting board 3 on the surface 2a side and is mounted so that the distance between the multiple electrode portions 53 is equal. When the micro-vibrator 2 is mounted on the mounting board 3, the curved surface portion 21 including the rim 211 is in a hollow state in which it does not come into contact with other members. The micro-vibrator 2 has a structure in which, when mounted on the mounting substrate 3, the hollow rim 211 can vibrate in a wine glass mode.
[0028] 2 and 3, the micro-vibrator 2 has a surface electrode 23 that covers part or all of the surface 21a and the back surface 21b of the base 20. The surface 21a is the surface of the curved portion 21 that has a larger outer diameter, and the back surface 21b is the opposite surface. The surface of the connection portion 22 on the back surface 21b side of the micro-vibrator 2 serves as a mounting surface 22b that faces the mounting substrate 3. For example, the surface of the bottom of the connection portion 22 opposite to the mounting surface 22b, i.e., the recess bottom surface 22a, can be used as a support surface for a jig J (described later) used when forming the surface electrode 23, and can also be used as an adsorption surface used for adsorbing and transporting the micro-vibrator 2.
[0029] The surface electrode 23 is made of a nitride film mainly composed of Ti (titanium). Specifically, the surface electrode 23 is a film of TiN (titanium nitride) to which O (oxygen) is added, that is, a titanium oxynitride film, and the ratio of Ti-O in the entire film is within a range of 26 to 52 wt%. The surface electrode 23 is formed on the front surface 21a and the back surface 21b of the base 20 by atomic layer deposition (ALD) to a thickness of, for example, 3 to 15 nm. The surface electrode 23 is formed on at least the mounting surface 22b and the front surface 21a of the rim 211, and these parts are electrically connected. The surface electrode 23 is, for example, in a solid shape covering the entire front and back surfaces of the micro-vibration body 2, but may be in a pattern shape covering only a predetermined area. The surface electrode 23 is connected to the mounting board 3 through a bonding member 52 made of a conductive material such as AuSn (gold tin), for example, at least in a predetermined area including a portion covering the mounting surface 22b of the connection portion 22.
[0030] The mounting substrate 3 includes a lower substrate 4 and an upper substrate 5, which are joined together, as shown in FIG. 1, for example. For example, the mounting substrate 3 is obtained by subjecting the lower substrate 4, which is made of borosilicate glass, an insulating material, to etching and wiring film formation, and then an upper substrate 5, which is made of silicon (Si), a semiconductor material, to the lower substrate 4 and performing patterning. The mounting substrate 3 includes, for example, on the upper substrate 5 side, a plurality of inner frame portions 51, a plurality of electrode portions 53 arranged apart from each other so as to surround the inner frame portion 51, and an outer frame portion 54 surrounding the plurality of electrode portions 53 at a distance. The mounting substrate 3 also includes, for example, on the lower substrate 4 side, a ring-shaped groove 41 surrounding the plurality of inner frame portions 51 while separating the inner frame portion 51 from the plurality of electrode portions 53, and a plurality of wirings 42 spanning the inside and outside of the groove 41.
[0031] 3, the groove 41 is provided between the inner frame portion 51 and the plurality of electrode portions 53, and is formed by wet etching. The groove 41 has a dimension corresponding to the outer diameter of the rim 211 of the micro-vibrator 2, and is provided so that the rim 211 does not come into contact with the mounting substrate 3 when the micro-vibrator 2 is mounted on the mounting substrate 3.
[0032] The wiring 42 is made of a conductive material such as Al (aluminum) and is disposed so as to pass between the plurality of electrode portions 53 and is electrically independent from the plurality of electrode portions 53. For example, a plurality of wirings 42 are provided, and one end of the wirings 42 is connected to the inner frame portion 51 and the other end is connected to the outer frame portion 54 while straddling the groove 41 in the lower substrate 4, electrically connecting them. This allows the mounting substrate 3 to apply a voltage to the surface electrode 23 of the micro-vibrator 2 via the outer frame portion 54, the wirings 42, and the inner frame portion 51.
[0033] The inner frame 51 is formed together with the multiple electrode portions 53 and the outer frame 54, for example, by performing dry etching such as DRIE on the upper substrate 5 anodically bonded to the lower substrate 4. DRIE is an abbreviation for Deep Reactive Ion Etching. The inner frame 51 is, for example, annular in shape when viewed from above, and is configured so that the connection portion 22 of the micro-vibrator 2 can be inserted or fitted into the enclosed area. For example, after arranging a bonding member 52 in the area enclosed by the inner frame 51 on the mounting substrate 3, the connection portion 22 of the micro-vibrator 2 is mounted on the bonding member 52 and heated and solidified, whereby the micro-vibrator 2 is mounted on the mounting substrate 3.
[0034] The electrode parts 53 are arranged at a distance from each other, and as shown in FIG. 3, each of the electrode parts 53 has an electrode film 531 formed on its upper surface. The electrode parts 53 are electrically connected to an external circuit board or the like, for example, by connecting a wire (not shown) to the electrode film 531. The electrode parts 53 are arranged at equal intervals from each other to form a ring, for example, when viewed from above, surrounding the rim 211 of the micro-vibration body 2. When the micro-vibration body 2 is mounted, each of the electrode parts 53 is spaced a predetermined distance from the rim 211 of the micro-vibration body 2, and each of the electrode parts 53 forms a capacitor with the micro-vibration body 2. That is, the mounting board 3 can detect the electrostatic capacitance between the micro-vibration body 2 and generate an electrostatic attraction between the micro-vibration body 2 and the mounting board 3 to vibrate the micro-vibration body 2 in a wine glass mode, via the electrode parts 53. In other words, a part of the electrode parts 53 is a detection electrode that detects the electrostatic capacitance, and the remaining part is a drive electrode that drives the micro-vibration body 2.
[0035] The outer frame portion 54 has a frame shape surrounding the inner frame portion 51 and the plurality of electrode portions 53 arranged therearound when viewed from above, for example. The outer frame portion 54 has at least one electrode film 541 made of Al or the like on its upper surface, for example, and a wire (not shown) is connected to the electrode film 541.
[0036] The above is the basic configuration of the inertial sensor 1 including the micro-vibrator 2. The inertial sensor 1 is manufactured, for example, by preparing the micro-vibrator 2 and the mounting board 3, applying a bonding material 52 to the mounting board 3 held by a mounter device (not shown), and then adsorbing and transporting the micro-vibrator 2 by a transport device (not shown) and bonding them by heating. The alignment of the micro-vibrator 2 and the mounting board 3 can be achieved, for example, by capturing an image of the micro-vibrator 2 during transport by an imaging device (not shown), extracting feature points of the curved surface portion 21 by edge detection using a known image recognition technology, and adjusting the relative positions based on these feature points.
[0037] The inertial sensor 1 described above is merely an example, and the number, shape, dimensions, arrangement, etc. of the wiring 42, the inner frame 51, the electrode parts 53, and the outer frame 54 of the mounting substrate 3 on which the micro-vibrator 2 is mounted may be appropriately changed. For example, when the micro-vibrator 2 obtained by removing unnecessary parts of the base 20 by the above-mentioned laser processing is configured such that the lower end of the rim 211 is located above the mounting surface 22b in the z direction, the mounting substrate 3 may be configured without the groove 41. In addition, the outer frame 54 is electrically connected to the micro-vibrator 2 with the multiple electrode parts 53 as first electrodes, and only needs to function as a second electrode part capable of applying a voltage to the surface electrode 23 of the micro-vibrator 2, and does not need to be in a frame shape, and the shape and arrangement may be appropriately changed.
[0038] [Surface electrode] Next, the surface electrode 23 of the micro-vibrator 2 and a method for forming the same will be described.
[0039] The surface electrode 23 is made of a TiN film doped with oxygen, and is a single layer that functions as both an adhesive layer and a conductive layer. The surface electrode 23 has a Ti-O ratio in the range of 26 to 52 wt% in order to achieve both adhesion to the base 20 made of a glass material and the conductivity required for an electrode. According to the inventors' intensive studies, it was found that the bonding strength and resistance value of the TiN film doped with O, as shown in FIG. 4, change depending on the Ti-O ratio. The Ti-O ratio was obtained by measurement using X-ray photoelectron spectroscopy (XPS) analysis.
[0040] For example, when the Ti-O ratio was 40.6 wt%, 43.2 wt%, and 63.5 wt%, the bonding strength with the base 20 was 3.8 MPa, 4.5 MPa, and 6.0 MPa, respectively. The bonding strength is evaluated, for example, by forming a titanium oxynitride film with a thickness of about 3 to 15 nm on a plate material of the glass material constituting the base 20 (for example, a quartz glass plate) and performing a tensile test on the sample. Here, from the viewpoint of ensuring the adhesion between the base 20 and the surface electrode 23, the bonding strength is desirably 1 MPa or more. An approximation line was obtained by the least squares method based on three data of Ti-O ratios of 40.6 wt%, 43.2 wt%, and 63.5 wt%, and the approximation line was extrapolated to the region with a low Ti-O ratio, and the bonding strength was 1 MPa when the Ti-O ratio was 26 wt%. That is, by using titanium oxynitride having a Ti—O ratio of 26 wt % or more for the surface electrode 23, adhesion to the base 20 made of glass can be ensured, and poor bonding with the mounting substrate 3 can be suppressed.
[0041] When the Ti-O ratio was 40.2 wt%, 52.0 wt%, and 97.6 wt%, the resistance values were 150 Ω / □, 950 Ω / □, and 1.02 MΩ / □, respectively, as shown in FIG. 4. The resistance value can be evaluated, for example, by preparing a sample having the same configuration as the evaluation sample for the bonding strength and measuring it by a four-terminal method. Here, it is desirable that the surface electrode 23 has a resistance of at least 1 kΩ / □ or less from the viewpoint of ensuring conductivity. Therefore, conductivity is ensured by making the surface electrode 23 from titanium oxynitride having a Ti-O ratio of 52 wt% or less.
[0042] Therefore, by making the surface electrode 23 a single titanium oxynitride film with a Ti-O ratio in the range of 26 to 52 wt%, it is possible to achieve a configuration that ensures both adhesion to the base 20 and conductivity without a laminated configuration of an adhesive layer and a conductive layer. As a result, the micro-vibrator 2 has a configuration in which the film thickness of the surface electrode 23 is set to a predetermined value or less to suppress a decrease in the Q value of vibration, while ensuring adhesion and conductivity between the base 20 and the surface electrode 23, and suppressing poor bonding with the mounting board 3.
[0043] The surface electrode 23 is formed by ALD using, for example, a jig J shown in FIG. 5. The jig J has a columnar support J1 that is inserted into the connection portion 22 of the base 20 and abuts against the bottom surface 22a of the recess to support the base 20. The jig J has, for example, a plurality of support portions J1 arranged at a predetermined interval, and is configured to be able to hold a plurality of base portions 20 without contacting each other. The diameter of the connection portion 22 on the bottom surface 22a side of the recess is taken as the inner diameter, and the support portion J1 is set to a height such that when the base 20 is set, the base 20 does not contact any portion other than the support portion J1. For example, the support portion J1 is set to a height such that the distance H between the set base 20 and the surface of the jig J on which the support portion J1 is provided is 0.5 mm or more. This ensures a sufficient space when the front surface electrode 23 is formed by ALD, and prevents the material gas from flowing around to the recess bottom surface 22a side of the base 20, thereby preventing uneven film formation on the front surface electrode 23.
[0044] 6, the support J1 has a surface that contacts the bottom surface 22a of the recess as a tip surface J1a, and the outer peripheral edge of the tip surface J1a is, for example, a substantially right-angled corner, i.e., is not chamfered. This stabilizes the contact between the support J1 and the bottom surface 22a of the recess, suppresses the base 20 from tilting during deposition of the surface electrode 23, and stabilizes the deposition process. Note that, in FIG. 6, the support J1 has an example in which the tip surface J1a is a cylinder with no chamfering, but the present invention is not limited to this and may have other columnar shapes such as a polygonal column.
[0045] The surface of the jig J is coated with an oxide (not shown), which suppresses outgassing from the jig during the ALD process and stabilizes the film formation process. x O y , x and y are arbitrary numbers), but any other material may be used as long as it has a predetermined permeability to outgassing such as water or oxygen, that is, has high barrier properties.
[0046] A plurality of bases 20 are set on the jig J described above, and the surface electrode 23 is formed by ALD. In the ALD for forming the surface electrode 23, for example, TiCl4 gas is used as a source gas, NH3 gas is used as a nitriding gas, and N2 gas is used as a purge gas and a carrier gas. For example, the jig J supporting the plurality of bases 20 is set in a chamber of an ALD film forming apparatus (not shown), and the degree of vacuum is adjusted to 1.3 to 1.3×10 3 Pa, and the temperature during film formation is 300 to 500°C. For example, TiCl4 gas is supplied at a flow rate of 200 to 300 sccm, then N2 gas is supplied at a flow rate of 1500 to 2500 sccm to remove residual TiCl4 gas, and then NH3 gas is supplied at a flow rate of 5500 to 6000 sccm. Then, for example, this cycle from supplying TiCl4 gas to supplying NH3 gas is repeated multiple times. Also, for example, a small amount of O2 gas is supplied when supplying N2 gas or NH3 gas in the above film formation cycle, or an oxidation treatment with O3 gas is performed after forming a titanium nitride film in the film formation cycle, thereby obtaining a titanium oxynitride film with a predetermined film thickness. As a result, the surface electrodes 23 made of a titanium oxynitride film with a Ti-O ratio in the range of 26 to 52 wt% can be formed on the front and back surfaces of the base 20, and the above-mentioned micro-vibrator 2 can be obtained.
[0047] According to this embodiment, the micro-vibrator 2 is made of glass, and the base 20 having the curved surface portion 21 and the connection portion 22 is covered with the surface electrode 23 made of an oxynitride film containing Ti as a main component and having a Ti-O ratio within a predetermined range. As a result, the surface electrode 23 of the micro-vibrator 2 is made of a single-layer oxynitride film instead of a laminated structure of an adhesive layer and a conductive layer, so that the total thickness of the surface electrode 23 is set to a predetermined value or less, and the Ti-O ratio is within a range of 26 to 52 wt%, so that adhesion and conductivity are ensured. Therefore, the micro-vibrator 2 is obtained by suppressing a decrease in the Q value of vibration, while achieving both adhesion and conductivity between the base 20 and the surface electrode 23, and suppressing poor bonding to the mounting board 3. Moreover, the inertial sensor 1 using this micro-vibrator 2 is configured to have high sensitivity by ensuring the Q value of vibration, and improved reliability by suppressing poor bonding.
[0048] In addition, the surface electrode 23 that has both adhesion to the base 20 and electrical conductivity can be formed by ALD film formation using a jig J having a columnar support J1 that supports the base 20 having the curved surface portion 21 and the connection portion 22, and the microvibrator 2 can be manufactured. In addition, by using a jig J in which the tip surface J1a of the support J1 is not chamfered and the surface is covered with an oxide, the base 20 can be stabilized during film formation and the influence of outgassing can be reduced. Furthermore, by adjusting the height of the support J1 so that the distance between the base 20 and the jig J is 0.5 mm or more, gas during ALD film formation flows around to the bottom surface 22a of the recess of the connection portion 22, and uneven film formation of the surface electrode 23 can be suppressed.
[0049] (Other embodiments) Although the present disclosure has been described based on the embodiment, it is understood that the present disclosure is not limited to the embodiment or structure. The present disclosure also includes various modifications and modifications within the equivalent range. In addition, various combinations and forms, and other combinations and forms including only one element, more than one, or less than one, are also within the scope and concept of the present disclosure.
[0050] In each of the above embodiments, it goes without saying that the elements constituting the embodiment are not necessarily essential, except when it is specifically stated that they are essential or when it is clearly considered essential in principle. In addition, in each of the above embodiments, when the numbers, values, amounts, ranges, etc. of the components of the embodiment are mentioned, they are not limited to the specific numbers, except when it is specifically stated that they are essential or when it is clearly limited to a specific number in principle. In addition, in each of the above embodiments, when the shapes, positional relationships, etc. of the components are mentioned, they are not limited to the shapes, positional relationships, etc., except when it is specifically stated that they are essential or when it is clearly limited to a specific shape, positional relationship, etc. in principle. [Explanation of symbols]
[0051] 20 base 21 Curved part 21a surface 22 Connection 23 Surface electrode
Claims
1. A micro-vibrator capable of vibrating in a wine glass mode, A base (20) having a curved surface portion (21) having an annular curved surface and a bottomed tubular connecting portion (22) recessed from a surface (21a) of the curved surface portion toward the center of a virtual hemisphere formed by the curved surface portion; a surface electrode (23) covering at least a portion of the surface of the base; The base is made of glass, The surface electrode is a nitride film formed by atomic layer deposition and mainly composed of Ti.
2. 2. The micro-vibrator according to claim 1, wherein the surface electrode is an oxynitride film to which oxygen is added.
3. 3. The micro-vibrator according to claim 2, wherein the surface electrode has a Ti--O composition in the range of 26 to 52 wt %.
4. A method for manufacturing a micro-vibrator capable of vibrating in a wine glass mode, comprising the steps of: A base (20) is provided which is made of glass and has a curved surface portion (21) having an annular curved surface and a bottomed tubular connecting portion (22) recessed from a surface (21a) of the curved surface portion toward the center of a virtual hemisphere formed by the curved surface portion; preparing a jig (J) having a support portion (J1) that is inserted into the connection portion and can support the base portion; and forming a surface electrode (23) covering the surface by atomic layer deposition while inserting the support part into the connection part and holding the base part in the jig. In forming the surface electrode, the base is held in a state where it is not in contact with any part of the jig other than the support portion, and a nitride film mainly composed of Ti is formed.
5. 5. The method for manufacturing a micro-vibrator according to claim 4, wherein the step of preparing the jig includes preparing a jig having a surface covered with aluminum oxide.
6. 6. The method for manufacturing a micro-vibration body according to claim 4, wherein in preparing the jig, an end portion of the tip surface of the support portion is not chamfered.
7. An inertial sensor, a base (20) having a curved surface portion (21) having an annular curved surface, a bottomed cylindrical connection portion (22) recessed from a surface (21a) of the curved surface portion toward the center of a virtual hemisphere formed by the curved surface portion, and a surface electrode (23) covering at least a portion of the surface of the base, the curved surface portion being capable of vibrating in a wine glass mode; a mounting substrate (3) to which the connection portion is joined, the mounting substrate (3) having a rim (211) at an end of the curved portion opposite to the connection portion, the rim being spaced apart from one another and surrounding the rim, The base is made of glass, The surface electrode is formed by atomic layer deposition and is a nitride film mainly composed of Ti.
8. A method for manufacturing an inertial sensor in which a micro-vibrator (2) capable of vibrating in a wine-glass mode is bonded to a mounting substrate (3), A base (20) is provided which is made of glass and has a curved surface portion (21) having an annular curved surface and a bottomed tubular connecting portion (22) recessed from a surface (21a) of the curved surface portion toward the center of a virtual hemisphere formed by the curved surface portion; preparing a jig (J) having a support portion (J1) that is inserted into the connection portion and can support the base portion; inserting the support portion into the connection portion, and forming a surface electrode (23) covering the surface by atomic layer deposition while the base portion is held by the jig, thereby forming the micro-vibrator; preparing the mounting substrate and joining the connection portion of the micro-vibrator to the mounting substrate; In the step of forming the surface electrode, a nitride film containing Ti as a main component is formed.
Citation Information
Patent Citations
MEMS sensor and manufacturing method of MEMS sensor
JP2010155299A
Detection element, minute electromechanical device, and electronic equipment
JP2010169401A
Piezoelectric device and using method thereof
JP2014060330A
Grasping structure of micro-vibration body and method of manufacturing inertial sensor
JP2022095430A
Inertial sensor
JP2022155449A