Light-emitting element, display unit, and method of manufacturing light-emitting element

A fluorine region with a non-uniform concentration gradient in the semiconductor stacked structure addresses structural defects and enhances luminous efficiency by forming a barrier against external influences in light-emitting devices.

JP2024149354APending Publication Date: 2024-10-18SAMSUNG DISPLAY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023200949
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-07
Filing Date
2023-11-28
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Existing light-emitting devices face structural defects and reduced luminous efficiency due to damage from etching processes, which affect the semiconductor layers.

Method used

A semiconductor stacked structure with a fluorine region adjacent to an insulating layer, featuring a non-uniform fluorine concentration gradient, is used to form a barrier against external influences, reducing structural defects and enhancing luminous efficiency.

Benefits of technology

The fluorine region improves the structural stability and reliability of the light-emitting device by acting as a barrier, reducing defects and enhancing luminous efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024149354000001_ABST
    Figure 2024149354000001_ABST
Patent Text Reader

Abstract

To provide a light-emitting element, a method of manufacturing the light-emitting element, and a display unit such that the light-emitting element can be improved in light emission efficiency and reliability by reducing structural defects of the light-emitting element.SOLUTION: A light-emitting element includes a semiconductor laminate structure including an N type semiconductor layer, a P type semiconductor layer, and an active layer between the N type semiconductor layer and the P type semiconductor layer, and an insulation layer arranged on the side of the semiconductor laminate structure. The semiconductor laminate structure includes a fluorine region formed in a region adjoining the insulation layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a light-emitting element, a display device, and a method for manufacturing a light-emitting element. [Background technology]

[0002] Recently, interest in information displays has increased, and as a result, research and development into display devices has been continuously carried out. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Korean Patent Publication No. 2012-0070809 Summary of the Invention [Problem to be solved by the invention]

[0004] An object of the present disclosure is to provide a light-emitting element capable of reducing structural defects in the light-emitting element, a method for manufacturing the light-emitting element, and a display device.

[0005] An object of the present disclosure is to provide a light-emitting element capable of improving the light-emitting efficiency and reliability of the light-emitting element, a method for manufacturing the light-emitting element, and a display device. [Means for solving the problem]

[0006] A light-emitting device according to an embodiment of the present disclosure includes a semiconductor laminate structure including an N-type semiconductor layer, a P-type semiconductor layer, and an active layer between the N-type semiconductor layer and the P-type semiconductor layer, and an insulating layer disposed on a side of the semiconductor laminate structure, and the semiconductor laminate structure includes a fluorine region formed in an area adjacent to the insulating layer.

[0007] According to one embodiment of the present disclosure, the semiconductor laminate structure includes a GaF x N (1-x) may include:

[0008] According to an embodiment of the present disclosure, in the fluorine region, F (fluorine) may have a non-uniform concentration gradient depending on the depth from the outer surface of the semiconductor stack structure.

[0009] According to an embodiment of the present disclosure, the F may have a peak concentration at a depth of 0.001 μm or more and 0.01 μm or less from the outer side surface of the semiconductor laminate structure.

[0010] According to one embodiment of the present disclosure, the peak concentration is 1.2×10 18 ~1.6×10 18 [pcs / cm 3 ] may be included.

[0011] According to one embodiment of the present disclosure, the fluorine region may entirely cover a side of the semiconductor stack.

[0012] According to one embodiment of the present disclosure, the fluorine region may cover the sides of the P-type semiconductor layer and the active layer, but not the sides of the N-type semiconductor layer.

[0013] According to one embodiment of the present disclosure, the insulating layer may comprise a metal oxide and the fluorine region may be directly adjacent to the insulating layer.

[0014] According to one embodiment of the present disclosure, the insulating layer may include a metal oxide including one or more metals selected from the group consisting of tantalum (Ta), hafnium (HF), zirconium (Zr), lanthanum (La), silicon (Si), titanium (Ti), and aluminum (Al).

[0015] According to one embodiment of the present disclosure, the bond energy between the F and Ga may be greater than the bond energy of the metal oxide.

[0016] According to an embodiment of the present disclosure, the insulating layer includes a first insulating layer disposed on a side of the semiconductor stack and a second insulating layer disposed on the first insulating layer, the first insulating layer is disposed between the fluorine region and the second insulating layer, and the first insulating layer and the second insulating layer each include a metal oxide. The first insulating layer may further include F, and the second insulating layer may not include F.

[0017] A display device according to one embodiment of the present disclosure includes a base layer and a light-emitting element on the base layer, the light-emitting element including a semiconductor laminate structure including an N-type semiconductor layer, a P-type semiconductor layer, and an active layer between the N-type semiconductor layer and the P-type semiconductor layer, and an insulating layer disposed on a side of the semiconductor laminate structure, and the semiconductor laminate structure includes a fluorine region formed in a region adjacent to the insulating layer.

[0018] According to one embodiment of the present disclosure, the display device may further include a first electrode and a second electrode on the base layer, the light-emitting element may include a first end and a second end, and the light-emitting element may be electrically connected to the first electrode at the first end and electrically connected to the second electrode at the second end.

[0019] According to one embodiment of the present disclosure, the display device may further include a first alignment electrode and a second alignment electrode on the base layer, and the light-emitting element may be aligned between the first alignment electrode and the second alignment electrode.

[0020] According to one embodiment of the present disclosure, the semiconductor laminate structure includes a GaF x N (1-x) may include:

[0021] According to an embodiment of the present disclosure, in the fluorine region, F (Fluorine) has a non-uniform concentration gradient according to depth from an outer surface of the semiconductor laminated structure, the F has a peak concentration at a depth of 0.001 μm to 0.01 μm from the outer surface of the semiconductor laminated structure, and the peak concentration is 1.2×10 18~1.6×10 18 [pcs / cm 3 ] may be included.

[0022] A method for manufacturing a light-emitting device according to an embodiment of the present disclosure includes patterning a semiconductor laminate structure on a growth substrate, forming a fluorine region on a side surface of the semiconductor laminate structure, and forming an insulating layer on the side surface of the semiconductor laminate structure.

[0023] According to one embodiment of the present disclosure, forming the fluorine region may include providing F to the semiconductor stack using an ion implantation method or a surface treatment process.

[0024] According to one embodiment of the present disclosure, forming the insulating layer may include forming two or more insulating layers alternately after forming the fluorine region.

[0025] According to one embodiment of the present disclosure, forming the insulating layer includes forming a first insulating layer on a side of the semiconductor stack and forming a second insulating layer on the first insulating layer, and forming the first insulating layer may be performed before forming the fluorine region and forming the second insulating layer after forming the fluorine region. Effect of the Invention

[0026] According to an embodiment of the present disclosure, it is possible to provide a light emitting device capable of reducing structural defects of the light emitting device, a method for manufacturing the light emitting device, and a display device.

[0027] According to an embodiment of the present disclosure, it is possible to provide a light emitting device capable of improving the light emitting efficiency and reliability of the light emitting device, a method for manufacturing the light emitting device, and a display device. [Brief description of the drawings]

[0028] [Figure 1] 1 is a schematic cross-sectional view showing a light-emitting device according to an embodiment of the present disclosure. [Diagram 2] 1 is a schematic cross-sectional view showing a light-emitting device according to an embodiment of the present disclosure. [Diagram 3] 1 is a schematic perspective view showing a light-emitting device according to an embodiment of the present disclosure. [Figure 4] 1 is a schematic cross-sectional view showing a light-emitting device according to an embodiment of the present disclosure. [Diagram 5] 1 is a schematic enlarged cross-sectional view showing a portion of a light-emitting device according to an embodiment of the present disclosure. [Figure 6] 1 is a schematic enlarged cross-sectional view showing a portion of a light-emitting device according to an embodiment of the present disclosure. [Figure 7] 1 is a graph showing a concentration profile of fluorine at each position in a semiconductor laminate structure. [Figure 8] 1 is a schematic flow chart illustrating a method for manufacturing a light-emitting device according to an embodiment of the present disclosure. [Figure 9] 1A to 1C are schematic cross-sectional views illustrating process steps for a method for manufacturing a light-emitting device according to an embodiment of the present disclosure. [Figure 10] 1A to 1C are schematic cross-sectional views illustrating process steps for a method for manufacturing a light-emitting device according to an embodiment of the present disclosure. [Figure 11] 1A to 1C are schematic cross-sectional views illustrating process steps for a method for manufacturing a light-emitting device according to an embodiment of the present disclosure. [Figure 12] 1A to 1C are schematic cross-sectional views illustrating process steps for a method for manufacturing a light-emitting device according to an embodiment of the present disclosure. [Figure 13] 1A to 1C are schematic cross-sectional views illustrating process steps for a method for manufacturing a light-emitting device according to an embodiment of the present disclosure. [Figure 14] 1A to 1C are schematic cross-sectional views illustrating process steps for a method for manufacturing a light-emitting device according to an embodiment of the present disclosure. [Figure 15] 1 is a schematic flow chart showing a method for manufacturing a light-emitting device according to an embodiment of the present disclosure, some of which have been modified; [Figure 16] 5A to 5C are schematic cross-sectional views illustrating process steps of a method for manufacturing a light emitting device according to a modified embodiment. [Figure 17]5A to 5C are schematic cross-sectional views illustrating process steps of a method for manufacturing a light-emitting device according to a partially modified embodiment of the present disclosure. [Figure 18] 1 is a schematic plan view illustrating a display device including a light-emitting device according to an embodiment of the present disclosure. [Figure 19] 1 is a schematic cross-sectional view showing a display device according to an embodiment of the present disclosure. [Figure 20] 1 is a schematic cross-sectional view showing a display device according to an embodiment of the present disclosure. [Figure 21] 1 is a schematic cross-sectional view showing a display device according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0029] Although the present disclosure can be modified in various ways and can be implemented in various forms, only specific examples are illustrated in the drawings and the present disclosure will be described based on these examples. However, the present disclosure is not limited to such specific examples, and it is understood that all modifications, equivalents, or alternatives within the spirit and technical scope of the present disclosure are included in the present disclosure.

[0030] Terms such as first and second are used to describe various components, but the components are not limited by the terms. The terms are used to distinguish one component from another component. For example, the first component may be called the second component without departing from the scope of the present disclosure. Similarly, the second component may be called the first component. A singular expression includes a plural expression unless the context clearly indicates otherwise.

[0031] In this disclosure, the terms "comprise" or "have" refer to features, numbers, steps, operations, components, parts, or combinations thereof described in the specification, and do not preclude the possibility of one or more other features, numbers, steps, operations, components, parts, or combinations thereof or additional features. In addition, when a layer, film, region, plate, or other part is described as being "on" another part, this includes not only the case where it is "directly on" the other part, but also the case where another part is located between them. In addition, in this specification, when a layer, film, region, plate, or other part is described as being formed on another part, the formed direction is not limited to the upper direction, but also includes the case where it is formed on the side or lower direction. In addition, when a layer, film, region, plate, or other part is described as being "under" another part, this includes not only the case where it is "directly under" the other part, but also the case where another part is located between them.

[0032] The present disclosure relates to a light emitting device, a display device, and a method for manufacturing the light emitting device. Hereinafter, a light emitting device, a display device, and a method for manufacturing the light emitting device according to an embodiment of the present disclosure will be described with reference to the accompanying drawings.

[0033] A light emitting device LD according to an embodiment of the present disclosure will be described with reference to FIGS.

[0034] Figures 1, 2, and 4 are schematic cross-sectional views showing a light-emitting device according to an embodiment of the present disclosure. Figure 3 is a schematic perspective view showing a light-emitting device according to an embodiment of the present disclosure. Figures 5 and 6 are schematic enlarged cross-sectional views showing a part of a light-emitting device according to an embodiment of the present disclosure. Figure 7 is a graph showing the concentration of fluorin at each position in a semiconductor laminate structure.

[0035] The light-emitting element LD is configured to emit light. For example, the light-emitting element LD can emit any one of red light, green light, and blue light. The red light can be light including a part of a wavelength band of about 600 nm to 750 nm. The green light can be light including a part of a wavelength band of about 480 nm to 560 nm. The blue light can be light including a part of a wavelength band of about 370 nm to 460 nm.

[0036] The light-emitting element LD may include a semiconductor laminate structure 1 including a fluorine region FA and an insulating layer INF. The semiconductor laminate structure 1 includes an N-type semiconductor layer SCL1, a P-type semiconductor layer SCL2, and an active layer AL disposed between the N-type semiconductor layer SCL1 and the P-type semiconductor layer SCL2.

[0037] The light-emitting element LD may have various sizes. According to an embodiment of the present disclosure, the light-emitting element LD may have a size from a microscale to a nanoscale. For example, the diameter of the light-emitting element LD may be 100 μm or less. Alternatively, according to an embodiment, the diameter of the light-emitting element LD may be 1 μm or less. Here, the diameter of the light-emitting element LD may be determined according to the cross-sectional shape of the light-emitting element LD (e.g., the active layer AL). For example, when the cross-section of the light-emitting element LD is circular, the diameter may be the diameter of the circle. When the cross-section of the light-emitting element LD is elliptical, the diameter may be the length of the long side of the ellipse. When the cross-section of the light-emitting element LD is polygonal, the diameter may be the length of the longest diagonal of the polygon.

[0038] The light emitting element LD may have a first end EP1 and a second end EP2. According to an embodiment of the present disclosure, the first end EP1 of the light emitting element LD may be adjacent to an N-type semiconductor layer SCL1, and the second end EP2 of the light emitting element LD may be adjacent to a P-type semiconductor layer SCL2. The first end EP1 and the second end EP2 may be defined based on the direction of an electrical path formed in the light emitting element LD.

[0039] The light emitting element LD can have various shapes. For example, the light emitting element LD can have a bar shape extending in one direction (FIGS. 1 to 3). In this case, the light emitting element LD can have a shape extending in a direction from the first end EP1 to the second end EP2.

[0040] Alternatively, according to an embodiment of the present disclosure, the light emitting element LD may be a light emitting diode manufactured to have a flip-chip type (FIG. 4), in which case the P-type semiconductor layer SCL2 at the first end EP1 and the N-type semiconductor layer SCL1 at the second end EP2 may face in the same direction.

[0041] The N-type semiconductor layer SCL1 is disposed on the active layer AL and may include a semiconductor layer of a different type from the P-type semiconductor layer SCL2. For example, the N-type semiconductor layer SCL1 may include an N-type semiconductor. The N-type semiconductor layer SCL1 may include a GaN-based material. For example, the N-type semiconductor layer SCL1 may include one or more selected from the group of InAlGaN, GaN, AlGaN, and InGaN, and may include an N-type semiconductor layer doped with a first conductive type dopant such as Si, Ge, and Sn. According to an embodiment, the N-type semiconductor layer SCL1 may include a GaN-based material including F in the fluorine region FA.

[0042] The active layer AL may be disposed between the N-type semiconductor layer SCL1 and the P-type semiconductor layer SCL2. The active layer AL may include a single-quantum well or a multi-quantum well structure. The position of the active layer AL is not limited to a specific example and may be changed in various ways depending on the type of the light emitting device LD.

[0043] The active layer AL may include well layers and barrier layers to form a quantum well structure. For example, the active layer AL may include InGaN as a well layer, and the active layer AL may include GaN as a barrier layer. In some embodiments, the active layer AL may include a GaN-based material containing F in the fluorine region FA.

[0044] The P-type semiconductor layer SCL2 is disposed on the active layer AL and may include a semiconductor layer of a different type from the N-type semiconductor layer SCL1. For example, the P-type semiconductor layer SCL2 may include a P-type semiconductor. The P-type semiconductor layer SCL2 may include a GaN-based material. For example, the P-type semiconductor layer SCL2 may include one or more selected from the group of InAlGaN, GaN, AlGaN, and InGaN, and may include a P-type semiconductor layer doped with a second conductive type dopant such as Ga, B, and Mg. According to an embodiment of the present disclosure, the P-type semiconductor layer SCL2 may include a GaN-based material including F in the fluorine region FA.

[0045] When a voltage equal to or greater than a threshold voltage is applied to the first end EP1 and the second end EP2 of the light emitting device LD, the electron-hole pairs in the active layer AL recombine with each other to form excitons, and the light emitting device LD can emit light. By controlling the emission of the light emitting device LD using this principle, the light emitting device LD can be used as a light source in various devices.

[0046] Experimentally, an etching (e.g., dry etching) process for manufacturing the light-emitting element LD may affect the light-emitting efficiency of the light-emitting element LD, etc. For example, there is a risk that the side of the light-emitting element LD may be broken and the active layer AL may be damaged, and in this case, the light-emitting efficiency of the light-emitting element LD may be hindered (for example, the light-emitting efficiency may decrease due to an increase in non-radiative recombination).

[0047] In this specification, a "side" may refer to a region including a part of the remaining region other than the top and bottom surfaces of an object (e.g., semiconductor stacked structure 1, active layer AL, N-type semiconductor layer SCL1, or P-type semiconductor layer SCL2, etc.). Here, the top and bottom surfaces of the object may refer to surfaces corresponding to the first end EP1 or the second end EP2 of the light-emitting element LD (or semiconductor stacked structure 1). Depending on the embodiment, the side may refer to a part of the outer surface of the object defined by the region between the first end EP1 and the second end EP2 of the light-emitting element LD (or semiconductor stacked structure 1).

[0048] According to an embodiment of the present disclosure, the light emitting device LD is characterized in that a fluorine region FA is formed on a side portion of the semiconductor laminate structure 1. The fluorine region FA may be a region including a crystal structure containing F (Fluorine).

[0049] The fluorine region FA may be formed on a side of the semiconductor stack 1 adjacent to the insulating layer INF. The fluorine region FA may be formed adjacent to a side of the semiconductor stack 1 directly adjacent to the insulating layer INF. The fluorine region FA may be disposed between at least a portion of the interior of the semiconductor stack 1 and the insulating layer INF. For example, the fluorine region FA may be directly adjacent to a metal oxide that forms the insulating layer INF.

[0050] The fluorine region FA may be adjacent to an etching surface where an etching process is performed during patterning of the semiconductor stacked structure 1. For example, when the N-type semiconductor layer SCL1, the active layer AL, and the P-type semiconductor layer SCL2 are etched together, an etching surface may be defined on a side of the semiconductor stacked structure 1, and the fluorine region FA may be adjacent to at least a portion of the defined etching surface.

[0051] The fluorine region FA may be a region formed by doping the side of the semiconductor laminated structure 1 with F. The F supplied to form the fluorine region FA may form at least a part of a crystal structure on the side of the semiconductor laminated structure 1.

[0052] For example, the fluorine region FA may be entirely disposed on a side of the semiconductor laminate structure 1 (FIGS. 1, 3, etc.). Thus, the fluorine region FA may be formed on a side of the N-type semiconductor layer SCL1, on a side of the active layer AL, or on a side of the P-type semiconductor layer SCL2.

[0053] In another embodiment, the fluorine region FA may be formed on a side of the active layer AL without being formed on a side of the N-type semiconductor layer SCL1, and may also be formed on a side of the P-type semiconductor layer SCL2 (FIG. 2). In this case, a fluorine-free region (FFA) that does not contain F may be formed on the side of the N-type semiconductor layer SCL1.

[0054] In the fluorine region FA, F may be distributed in one concentration profile according to depth based on the outer surface of the semiconductor stacked structure 1. This will be described with reference to FIG. 7. Here, the outer surface of the semiconductor stacked structure 1 may refer to an outer surface that is a side of the semiconductor stacked structure 1 and is directly adjacent to the insulating layer INF. The depth described below may refer to the distance between a target position and the outer surface of the semiconductor stacked structure 1.

[0055] The concentration of F increases with depth from the outer surface of the semiconductor laminate structure 1, but may have a profile that decreases from a peak concentration. For example, the concentration of F may have a peak concentration y at a peak position x included in a numerical range of 0.001 μm to 0.01 μm. According to an embodiment of the present disclosure, the peak concentration y is 1.2×10 18 ~1.6×10 18 [pcs / cm 3 That is, in the fluorine region FA, F can be distributed with a non-uniform concentration gradient and can be provided to have a peak concentration at at least some positions. By providing such a concentration gradient of F, the fluorine region FA can function as a barrier layer of the semiconductor laminate structure 1 against external influences.

[0056] The fluorine region FA may include a GaFN-based material. For example, the fluorine region FA may include GaF x N (1-x) However, the present disclosure is not necessarily limited thereto. For example, the GaFN-based material may further include one or more elements. In some embodiments, the GaFN-based material may include In x Al y Ga (1-x-y) F m N n may include.

[0057] According to an embodiment of the present disclosure, in the GaN crystal structure forming the semiconductor laminate structure 1, F can be placed in vacancies where N is not placed, and can form a bond structure with Ga. F ​​has a relatively high electronegativity and can form a bond structure with Ga having high bond energy. This allows GaFN to form a crystal structure with high stability.

[0058] In this case, the risk of elements other than F penetrating into the GaN crystal structure (e.g., wurtzite crystal structure) in the fluorine region FA can be reduced. For example, it has been experimentally shown that when H (hydrogen) and O (oxygen) are provided in the GaN crystal structure, they function as donor elements and may impair the structural stability of the GaN crystal structure. In particular, since the insulating layer INF can contain a metal oxide, there is a risk that a part of O forming the metal oxide is provided in the GaN crystal structure, and when O is provided in the GaN crystal structure, GaON and Ga 2 O 3 There is a possibility that such a crystal structure will be formed, reducing the stability of the GaN crystal structure.

[0059] However, by providing the GaN crystal structure with F capable of forming a bond structure having a bond energy with Ga, the risk of the GaN crystal structure being deformed at the side of the semiconductor laminate structure 1 (for example, an etching interface) can be reduced. For example, the Ga-F bond can have a higher bond energy than the Ga-O bond. The HF bond can have a higher bond energy than the HO bond. The Ga-F bond can have a bond energy of about 6.0 eV. The Ga-O bond can have a bond energy of about 3.9 eV. The HF bond can have a bond energy of about 5.9 eV. The HO bond can have a bond energy of about 4.8 eV. This can reduce the risk of the Ga-F bond and / or the FO bond being strongly formed or H or O penetrating into the GaN crystal structure.

[0060] Ultimately, the fluorine region FA can reduce defects that may occur at the sides of the semiconductor laminate structure 1, reduce the risk of structural mutations due to external influences (e.g., a phenomenon in which excitons are self-trapped, causing lattice vibrations in the lattice of the crystal structure), and reduce the risk of changes in the material properties of GaN. This can improve the light-emitting efficiency of the light-emitting element LD and allow for a reconsideration of the light-emitting reliability of the light-emitting element LD. For example, if the structural stability of the GaN crystal structure is impaired, strains will occur in the GaN crystal structure, making it difficult for the light-emitting element LD to emit light with the intended brightness, but the fluorine region FA can reduce such risks.

[0061] The insulating layer INF can surround the sides of the semiconductor stack 1. The insulating layer INF can be disposed on the semiconductor stack 1 including the N-type semiconductor layer SCL1, the active layer AL, and the P-type semiconductor layer SCL2.

[0062] The insulating layer INF can be disposed on the fluorine region FA. The insulating layer INF can protect the semiconductor stack 1 from external influences and can insulate the N-type semiconductor layer SCL1, the active layer AL, and the P-type semiconductor layer SCL2 from the outside.

[0063] The insulating layer INF may include an insulating material including a metal oxide. For example, the insulating layer INF may include a metal oxide including one or more metals selected from the group consisting of tantalum (Ta), hafnium (HF), zirconium (Zr), lanthanum (La), silicon (Si), titanium (Ti), and aluminum (Al). However, an embodiment of the present disclosure is not limited to a specific example.

[0064] The insulating layer INF may include two or more insulating layers each containing a metal oxide (see FIG. 5). For example, the insulating layer INF may have a structure in which two or more metal oxide insulating layers containing different materials are sequentially stacked. For example, the insulating layer INF may include a metal oxide insulating layer having a thickness of M1. X O Y A first insulating layer including M2 U O Z (M1 and M2 are metals). The number of two or more insulating layers for forming the insulating layer INF is not particularly limited.

[0065] According to one embodiment of the present disclosure, the insulating layer INF may include a first insulating layer INF1 and a second insulating layer INF2 (FIG. 6). Here, the second insulating layer INF2 may be an insulating structure including two or more insulating layers each including a metal oxide, as described above. The first insulating layer INF1 may be a layer formed separately from the second insulating layer INF2.

[0066] According to one embodiment of the present disclosure, the first insulating layer INF1 may be referred to as a preliminary insulating layer.

[0067] For example, the first insulating layer INF1 may be disposed between the fluorine region FA of the semiconductor laminate structure 1 and the second insulating layer INF2. One surface of the first insulating layer INF1 may contact a side of the semiconductor laminate structure 1, and the other surface of the first insulating layer INF1 may contact the second insulating layer INF2. In some embodiments, the first insulating layer INF1 may cover the respective sides of the N-type semiconductor layer SCL1, the active layer AL, and the P-type semiconductor layer SCL2. However, the present disclosure is not necessarily limited thereto. In some embodiments, the first insulating layer INF1 may be disposed on the N-type semiconductor layer SCL1 without being disposed on the active layer AL and the P-type semiconductor layer SCL2.

[0068] The first insulating layer INF1 includes one or more of the metal oxides described above, and may further include F. For example, the first insulating layer INF1 includes a metal oxide manufactured to have an amorphous structure, and at least a portion of the structure formed by the metal oxide may include F. Depending on the embodiment, the second insulating layer INF1 includes one or more of the metal oxides described above, but may not include F.

[0069] During the process for forming the fluorine region FA, the first insulating layer INF1 may cap at least a portion of the semiconductor stack 1. For example, the first insulating layer INF1 may protect the semiconductor stack 1 from the effects of the process for forming the fluorine region FA.

[0070] For example, F doped into the semiconductor laminate structure 1 to form the fluorine region FA may have a certain kinetic energy. For example, when F penetrates into the semiconductor laminate structure 1 using plasma or the like, the kinetic energy of F may cause strain in the semiconductor laminate structure 1. However, according to an embodiment, by preliminarily forming the first insulating layer INF1 before forming the fluorine region FA, the first insulating layer INF1 can reduce the kinetic energy of F, thereby reducing the above-mentioned risk.

[0071] According to an embodiment of the present disclosure, the structure of the light emitting device LD is not limited to the above example, and may further include additional layers. For example, the light emitting device LD may further include an electron blocking layer for preventing overflow of electrons, and the light emitting device LD may further include a superlattice layer for relieving stress in the light emitting device LD. In addition, the light emitting device LD may further include an electrode layer disposed on the P-type semiconductor layer SCL2 and electrically connected to the P-type semiconductor layer SCL2.

[0072] According to an embodiment, when the light emitting device LD is a flip-chip type light emitting diode, the light emitting device LD may include a first connecting electrode CNE1 electrically connected to the N-type semiconductor layer SCL1, a second connecting electrode CNE2 electrically connected to the P-type semiconductor layer SCL2, a growth substrate GS forming a base of the N-type semiconductor layer SCL1, a buffer layer BF disposed between the growth substrate GS and the N-type semiconductor layer SCL1, and an undoped semiconductor layer USCL. The growth substrate GS, the buffer layer BF, and the undoped semiconductor layer USCL will be described in detail later with reference to FIGS. 12 to 14.

[0073] A method for manufacturing a light-emitting element LD according to an embodiment of the present disclosure will be described below with reference to Fig. 8 to Fig. 17. Descriptions of contents that may overlap with those described above may be simplified or omitted.

[0074] First, with reference to FIGS. 8 to 14, an embodiment of the present disclosure in which the insulating layer INF is not formed before the fluorine region FA is formed will be described.

[0075] Fig. 8 is a schematic flow chart showing a method for manufacturing a light-emitting element according to an embodiment of the present disclosure. Figs. 9 to 14 are schematic cross-sectional views showing each process step of a method for manufacturing a light-emitting element according to an embodiment of the present disclosure. Figs. 9 to 11 are diagrams showing a method for manufacturing a light-emitting element LD (e.g., Figs. 1 to 3) having a shape extending in one direction. Figs. 12 to 14 are diagrams showing a method for manufacturing a flip-chip type light-emitting element LD (e.g., Fig. 4).

[0076] Referring to FIG. 8, a method for manufacturing a light emitting device LD according to an embodiment of the present disclosure may include step S120 of patterning a semiconductor stacked structure, step S140 of forming a fluorine region, and step S160 of forming an insulating layer.

[0077] 8, 9 and 12, in step S120 of patterning the semiconductor stacked structure, a buffer layer BF, an undoped semiconductor layer USCL, an N-type base semiconductor layer, a base active layer and a P-type base semiconductor layer may be grown on a growth substrate GS, and at least a portion of each of the N-type base semiconductor layer, the base active layer and the P-type base semiconductor layer may be etched to pattern the semiconductor stacked structure 1. Depending on the embodiment, the etching process may be performed so that a side portion of the semiconductor stacked structure 1 is exposed. Depending on the embodiment, in order to manufacture a flip-chip type light emitting device LD, an etching process may be performed so that one surface of the N-type semiconductor layer SCL1 is exposed (see FIG. 12).

[0078] The growth substrate GS may be a base plate for growing a target material. For example, the growth substrate GS may be a wafer for epitaxial growth of a material. The growth substrate GS may be a substrate including Si, GaAs, etc., but the material for forming the growth substrate GS is not limited to a specific example.

[0079] The buffer layer BF can improve the crystallinity of a semiconductor layer formed on the growth substrate GS. By way of example, the buffer layer BF can include one or more of the following group: InAlGaN, GaN, AlGaN, InGaN, AIN, and InN, although the present disclosure is not necessarily limited thereto.

[0080] The undoped semiconductor layer USCL can reduce defects in a semiconductor layer formed on the growth substrate GS. According to an embodiment, the undoped semiconductor layer USCL may include the same material as the semiconductor material for forming the semiconductor stack 1 as a semiconductor material not including a separate dopant, but the material for forming the undoped semiconductor layer USCL is not limited to a specific example.

[0081] The N-type base semiconductor layer, the base active layer, and the P-type base semiconductor layer can be epitaxially grown in sequence. The N-type base semiconductor layer can include a material for forming the N-type semiconductor layer SCL1. The base active layer can include a material for forming the active layer AL. The P-type base semiconductor layer can include a material for forming the P-type semiconductor layer SCL2.

[0082] 8, 10 and 13, in a step S140 of forming a fluorine region, a fluorine region FA can be formed.

[0083] In this step, the side of the semiconductor laminated structure 1 can be doped with F, and according to an embodiment, a crystal structure containing GaFN can be formed on the side of the semiconductor laminated structure 1.

[0084] For example, the fluorine region FA may be a region produced by implanting F ions using an ion implantation method. When using the ion implantation method, the energy applied to the ions to be doped can be adjusted to control the depth to which the ions penetrate through the outer surface of the semiconductor laminate structure 1. According to an embodiment of the present disclosure, an energy of about 5 keV can be supplied to the ions. In this case, the peak concentration of F in the fluorine region FA is about 1.0×10 15 [pcs / cm 3 By way of example, the peak concentration of F can be greater than 1.2×10 18 [pcs / cm 3 ] or more, and by way of example, the peak concentration of F can be 1.2 x 1018 ~1.6×10 18 [pcs / cm 3 However, the present disclosure is not necessarily limited thereto.

[0085] In another embodiment, the fluorine region FA may be a region produced by supplying F through a surface treatment process. The surface treatment process may be an annealing process or a surface treatment process using plasma. However, an embodiment of the present disclosure is not limited thereto.

[0086] According to an embodiment of the present disclosure, the region where the fluorine region FA is formed may be selectively defined in a portion of the side of the semiconductor stacked structure 1. For example, the fluorine region FA may be formed entirely on the side of the semiconductor stacked structure 1, or may be selectively formed on the side of the active layer AL and the P-type semiconductor layer SCL2 according to the embodiment.

[0087] 8, 11 and 14, in step S160 of forming an insulating layer, the insulating layer INF can be patterned so that the insulating layer INF covers the semiconductor stack structure 1.

[0088] For example, the insulating layer INF can be formed (or deposited) by various methods. For example, an atomic layer deposition (ALD) process or a chemical vapor deposition (CVD) process can be used. However, an embodiment of the present disclosure is not necessarily limited thereto. The formed insulating layer INF can be etched to electrically expose the semiconductor stack structure 1.

[0089] According to an embodiment of the present disclosure, the insulating layer INF may be formed of alternating different materials to include two or more insulating layers. As mentioned above, the insulating layer INF may include a metal oxide.

[0090] According to an embodiment of the present disclosure, although not shown, a step of patterning an electrode layer electrically connected to at least a portion of the semiconductor laminate structure 1 may be further performed.

[0091] According to an embodiment of the present disclosure (e.g., FIGS. 9 to 11), a step of separating the structure including the semiconductor stacked structure 1 and the insulating layer INF to provide an individual light emitting element LD may be further performed. For example, a part of the N-type semiconductor layer SCL1 may be cut. According to an embodiment, a laser lift off (LLO) process may be performed to cut a part of the N-type semiconductor layer SCL1. However, an embodiment of the present disclosure is not necessarily limited thereto. According to an embodiment, it is also possible to manufacture a light emitting element LD by transferring the structure including the semiconductor stacked structure 1 to a backplane layer (e.g., a pixel circuit layer PCL including a pixel circuit (see FIG. 19)) without performing a step of separating the structure including the semiconductor stacked structure 1 and the insulating layer INF, and then removing the growth substrate GS or the like.

[0092] Meanwhile, according to an embodiment of the present disclosure (for example, FIGS. 12 to 14), a step of forming a connecting electrode CNE may be further performed. The connecting electrode CNE may be patterned before forming the insulating layer INF, or may be patterned after forming the insulating layer INF. The connecting electrode CNE may include a first connecting electrode CNE1 and a second connecting electrode CNE2. The first connecting electrode CNE1 may be electrically connected to the N-type semiconductor layer SCL1 and may be configured to electrically connect a cathode electrode of the light emitting device LD and the semiconductor stacked structure 1. The second connecting electrode CNE2 may be electrically connected to the P-type semiconductor layer SCL2 and may be configured to electrically connect an anode electrode of the light emitting device LD and the semiconductor stacked structure 1. According to an embodiment of the present disclosure, since the light emitting device LD is manufactured as a flip-chip type, a structure of the light emitting device LD may be formed without separately removing a layer forming a base of the semiconductor stacked structure 1.

[0093] Next, an embodiment of the present disclosure in which a part of the insulating layer INF is formed before the fluorine region FA is formed will be described with reference to Figures 15 to 17. When comparing with the contents described above with reference to Figures 8 to 14, the manufacturing method of the light-emitting element LD will be described with a focus on the differences.

[0094] Fig. 15 is a schematic flow chart showing a method for manufacturing a light-emitting device according to an embodiment of the present disclosure, which has been partially modified. Figs. 16 and 17 are schematic cross-sectional views of each process step showing a method for manufacturing a light-emitting device according to an embodiment of the present disclosure, which has been partially modified.

[0095] This manufacturing method differs from the above-mentioned manufacturing method in that a step of forming a first insulating layer INF1 is performed before forming the fluorine region FA.

[0096] For example, a manufacturing method of a light-emitting element LD according to one embodiment of the present disclosure may include step S120 of patterning a semiconductor stacked structure, step S240 of forming a first insulating layer, step S260 of forming a fluorine region, and step S280 of forming a second insulating layer.

[0097] According to an embodiment of the present disclosure, before forming the fluorine region FA, a step S240 of forming a first insulating layer can be performed.

[0098] For example, referring to FIG. 16, after patterning the semiconductor laminate structure 1, the first insulating layer INF1 may be patterned on the side of the semiconductor laminate structure 1. Depending on the embodiment, the first insulating layer INF1 may be patterned on the entire side of the semiconductor laminate structure 1, or may be patterned selectively on a part of the side of the semiconductor laminate structure 1. For example, the first insulating layer INF1 may be patterned on the N-type semiconductor layer SCL1 without being patterned on the active layer AL and the P-type semiconductor layer SCL2. In this way, the first insulating layer INF1 may not be disposed on the active layer AL and the P-type semiconductor layer SCL2, which need to have a relatively high concentration of F in the fluorine region FA, and the first insulating layer INF1 may be selectively disposed on the N-type semiconductor layer SCL1, which does not need to have a relatively high concentration of F.

[0099] According to one embodiment of the present disclosure, the first insulating layer INF1 may include one or more of the metal oxides mentioned above with respect to the insulating layer INF1.

[0100] Referring to FIG. 17, after forming the first insulating layer INF1, a step S260 of forming a fluorine region may be performed.

[0101] In this step, the first insulating layer INF1 can reduce physical effects on the semiconductor laminated structure 1 that may occur during the process for forming the fluorine region FA. For example, as described above, the process environment 1000 for forming the fluorine region FA may affect the bonding structure of the semiconductor laminated structure 1, which may reduce the light emission reliability of the semiconductor laminated structure 1. However, according to this embodiment, the first insulating layer INF1 capable of passivating the side of the semiconductor laminated structure 1 is provided in advance before the fluorine region FA is formed, so that the semiconductor laminated structure 1 can be protected from the process environment 1000 for forming the fluorine region FA. In addition, since F ions having high kinetic energy can be doped into the semiconductor laminated structure 1 only after passing through the first insulating layer INF1 and having reduced kinetic energy, the risk of energy generated during the process damaging the structure of the semiconductor laminated structure 1 can be reduced.

[0102] Thereafter, a step S280 of forming a second insulating layer may be performed, and a second insulating layer INF2 may be patterned on the first insulating layer INF1.

[0103] Next, a display device DD including a light emitting element LD according to an embodiment of the present disclosure will be described with reference to Fig. 18 to Fig. 21. Descriptions of contents that may overlap with those described above may be simplified or omitted.

[0104] Fig. 18 is a schematic plan view showing a display device including a light-emitting element according to an embodiment of the present disclosure, Figs. 19 to 21 are schematic cross-sectional views showing display devices according to the embodiment.

[0105] 18 to 21, a display device DD according to an embodiment of the present disclosure may include a base layer BSL and a pixel PXL formed on the base layer BSL.

[0106] According to an embodiment of the present disclosure, the base layer BSL is a member forming a base surface on which the pixels PXL are disposed, and may be a substrate or a film. Depending on the embodiment, the base layer BSL may be a rigid substrate made of a glass material. Alternatively, the base layer BSL may be a flexible substrate capable of bending, folding, rolling, etc. In this case, the substrate may include an insulating material such as a polymer resin such as polyimide.

[0107] According to an embodiment of the present disclosure, the pixel PXL may include the light emitting element LD described above.

[0108] According to an embodiment of the present disclosure, the display device DD may include a pixel circuit layer PCL including a base layer BSL and a driving circuit on the base layer BSL. The display device DD may also include a light emitting element layer EML disposed on the pixel circuit layer PCL and in which a light emitting element LD is disposed.

[0109] According to an embodiment of the present disclosure, the light emitting element LD is transferred onto the pixel circuit layer PCL and can emit light according to electrical signals provided from the first electrode EL1 and the second electrode EL2.

[0110] For example, according to an embodiment of the present disclosure (FIG. 19), the light emitting element LD may be individually separated and transferred onto the first electrode EL1. Alternatively, according to an embodiment (FIG. 20), when the light emitting element LD is manufactured into a flip-chip type light emitting diode, the light emitting element LD may be transferred such that the first connecting electrode CNE1 is electrically connected to the first electrode EL1 and the second connecting electrode CNE2 is electrically connected to the second electrode EL2.

[0111] According to an embodiment of the present disclosure, the light emitting device layer EML may include a first electrode EL1 electrically connected to one end of the light emitting device LD and a second electrode EL2 electrically connected to the other end of the light emitting device LD.

[0112] The light emitting element LD can provide light based on an electrical signal provided by a driving transistor of a driving circuit (e.g., an electrical signal provided from a first electrode EL1 and a second electrode EL2). According to an embodiment, the light emitting element LD can emit light of various colors, and the light emitting elements LD emitting light of the same color can form sub-pixels, and the formed sub-pixels can form one or more pixels PXL (or pixel units).

[0113] Meanwhile, according to an embodiment of the present disclosure (FIG. 21), the light emitting element LD may be aligned (or disposed) between the first alignment electrode ALE1 and the second alignment electrode ALE2 on the pixel circuit layer PCL. For example, in order to dispose the light emitting element LD on the pixel circuit layer PCL, a first alignment signal (e.g., an AC signal) may be provided to the first alignment electrode ALE1, and a second alignment signal (e.g., a ground signal) may be provided to the second alignment electrode ALE2. In this case, an electric field may be formed between the first alignment electrode ALE1 and the second alignment electrode ALE2, and the light emitting element LD may be aligned based on the formed electric field. According to an embodiment of the present disclosure, the first end EP1 of the light emitting element LD aligned between the first alignment electrode ALE1 and the second alignment electrode ALE2 may be electrically connected to an anode electrode (not shown), and the second end EP2 of the light emitting element LD may be electrically connected to a cathode electrode (not shown) to be configured to emit light.

[0114] As described above, the light emitting element LD is manufactured to reduce process risks and have high light emitting efficiency, so that the display device DD including the light emitting element LD according to one embodiment of the present disclosure can be manufactured into a high quality product.

[0115] As described above, each embodiment of the present disclosure has been described with reference to the drawings, but a person skilled in the art or with ordinary knowledge in the art can modify and change the present disclosure in various ways without departing from the concept and technical scope of the present disclosure described in the claims below.

[0116] Therefore, the technical scope of the present disclosure should not be limited to the contents described in the detailed description of the specification, but should be determined by the claims. [Explanation of symbols]

[0117] LD light emitting element 1. Semiconductor stacked structure SCL1, SCL2 N-type semiconductor layer, P-type semiconductor layer AL active layer FL Fluorine region INF insulation layer DD display device EL1, EL2 1st electrode, 2nd electrode ALE1, ALE2 First alignment electrode, second alignment electrode

Claims

1. a semiconductor laminate structure including an N-type semiconductor layer, a P-type semiconductor layer, and an active layer between the N-type semiconductor layer and the P-type semiconductor layer; an insulating layer disposed on a side of the semiconductor stack; The light-emitting device, wherein the semiconductor laminated structure includes a fluorine region formed in a region adjacent to the insulating layer.

2. The semiconductor laminate structure is GaF formed in the fluorine region. x N (1-x) The light-emitting device according to claim 1 ,

3. The light emitting device according to claim 2 , wherein in the fluorine region, F (fluorine) has a non-uniform concentration gradient depending on the depth from the outer surface of the semiconductor laminated structure.

4. The light-emitting device according to claim 3 , wherein the F has a peak concentration at a depth of 0.001 μm to 0.01 μm from the outer side surface of the semiconductor laminated structure.

5. The peak concentration is 1.2×10 18 ~1.6 x 10 18 [pcs / cm 3 5. The light-emitting device according to claim 4, wherein

6. The light emitting device according to claim 1 , wherein the fluorine region entirely covers a side of the semiconductor laminate structure.

7. The light emitting device according to claim 1 , wherein the fluorine region covers sides of the P-type semiconductor layer and the active layer, but does not cover sides of the N-type semiconductor layer.

8. the insulating layer includes a metal oxide; The light emitting device of claim 3 , wherein the fluorine region is directly adjacent the insulating layer.

9. 9. The light-emitting device of claim 8, wherein the insulating layer includes a metal oxide including one or more metals selected from the group consisting of tantalum (Ta), hafnium (HF), zirconium (Zr), lanthanum (La), silicon (Si), titanium (Ti), and aluminum (Al).

10. The light-emitting element according to claim 8 , wherein a bond energy between the F and Ga is greater than a bond energy of the metal oxide.

11. the insulating layer includes a first insulating layer disposed on a side of the semiconductor stack and a second insulating layer disposed on the first insulating layer; the first insulating layer is disposed between the fluorine region and the second insulating layer; the first insulating layer and the second insulating layer each contain a metal oxide; The first insulating layer further contains F, The light emitting device according to claim 8 , wherein the second insulating layer does not contain F.

12. A base layer; a light emitting element on the base layer, The light-emitting element includes a semiconductor laminated structure including an N-type semiconductor layer, a P-type semiconductor layer, and an active layer between the N-type semiconductor layer and the P-type semiconductor layer, and an insulating layer disposed on a side surface of the semiconductor laminated structure; 2. A display device comprising: a semiconductor laminate structure including a fluorine region formed in a region adjacent to the insulating layer.

13. further comprising a first electrode and a second electrode on the base layer; the light emitting element includes a first end and a second end; The display device of claim 12, wherein the light emitting element is electrically connected to the first electrode at the first end and to the second electrode at the second end.

14. further comprising a first alignment electrode and a second alignment electrode on the base layer; The display device of claim 12, wherein the light emitting element is aligned between the first alignment electrode and the second alignment electrode.

15. The semiconductor laminate structure is GaF formed in the fluorine region. x N (1-x) The display device according to claim 12 ,

16. In the fluorine region, F (fluorine) has a non-uniform concentration gradient depending on the depth from the outer surface of the semiconductor laminate structure, the F has a peak concentration at a depth of 0.001 μm or more and 0.01 μm or less from the outer side surface of the semiconductor laminate structure, The peak concentration is 1.2×10 18 ~1.6 x 10 18 [pcs / cm 3 16. The display device according to claim 15, wherein

17. patterning a semiconductor stack on a growth substrate; forming a fluorine region on a side surface of the semiconductor laminate structure; and forming an insulating layer on a side surface of the semiconductor laminated structure.

18. 20. The method of claim 17, wherein forming the fluorine region comprises providing F to the semiconductor stack using an ion implantation method or a surface treatment process.

19. The method of claim 17, wherein the forming of the insulating layer comprises forming the fluorine region followed by alternately forming two or more insulating layers.

20. forming the insulating layer includes forming a first insulating layer on a side of the semiconductor stack and forming a second insulating layer on the first insulating layer; forming the first insulating layer occurs prior to forming the fluorine region; The method of claim 17, wherein the forming of the second insulating layer is performed after the forming of the fluorine region.

Citation Information

Patent Citations

  • KR2012-0070809