Thermocompression bonding device
The thermocompression bonding apparatus addresses flux deterioration and alignment issues by using a die block with escape grooves and non-contact bonding, ensuring efficient and high-quality semiconductor chip bonding with integrated inspection.
Patent Information
- Application Number
- JP2024061509
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-11-21
- Filing Date
- 2024-04-05
- Publication Date
- 2024-10-18
AI Technical Summary
Conventional thermocompression bonding devices face issues such as flux deterioration due to residual heat, inefficient flux application, reduced productivity, and poor bonding quality, along with challenges in inspecting for foreign substances and aligning semiconductor chips, leading to decreased UPH and potential mechanical deformation.
A thermocompression bonding apparatus with a die picker that immerses semiconductor chips in flux using a die block with escape grooves, a bonding head that applies heat and pressure non-contactually, and integrated inspection systems to ensure precise alignment and continuous bonding, minimizing heat transfer and mechanical impact.
Enhances bonding efficiency by maintaining flux quality, reducing mechanical deformation, and enabling continuous inspection and alignment, thereby improving productivity and bonding quality while minimizing defects.
Smart Images

Figure 2024149461000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a thermocompression bonding apparatus for thermocompression bonding a semiconductor chip onto a substrate. [Background technology]
[0002] Generally, a process of bonding individual semiconductor chips obtained by cutting a wafer to a bonding substrate is called a semiconductor chip bonding process.
[0003] The semiconductor chip bonding process may include the steps of picking up a number of semiconductor chips, which are separated by cutting or dicing a wafer, using a flip-over picker and flipping them upside down, picking up the semiconductor chips using a bonding head, transporting the bonding head and dipping the bottom surface of the semiconductor chip in flux so that the flux is applied to the bumps (solder balls) formed on the bottom surface of the semiconductor chip, inspecting the condition of the bottom surface of the semiconductor chip to which the flux is applied, and bonding the semiconductor chip to a bonding substrate. An apparatus in which such a semiconductor chip bonding process is performed may be defined as a bonding device.
[0004] Bonding devices can be divided into flip-chip bonding devices, which apply flux to the bumps of a semiconductor chip and attach the bumps to the connection terminals of a substrate to bond them, and thermocompression bonding devices, which apply heat and pressure while the underside of the semiconductor chip is connected to the substrate.
[0005] Such bonding equipment can be used in through-silicon via (TSV) package stacking processes to realize 3D packaging that vertically connects multiple packages to realize high-performance memory materials for data centers that process massive amounts of data based on artificial intelligence (AI) and big data.
[0006] TSV packaging is an advanced stacking technique in which multiple identical semiconductor chips are vertically stacked after drilling tiny holes in them and filling them with a conductive material such as copper to form electrodes. Individual packages can be stacked in multiple layers on a substrate, and the packages are then stacked and bonded by applying heat and pressure using a thermocompression method.
[0007] A through silicon via package can be constructed by stacking and bonding semiconductor packages using advanced lamination techniques, such as drilling tiny holes in a semiconductor chip and stacking multiple semiconductor chips vertically, then filling the holes with copper to form electrodes, or stacking multiple copper-filled semiconductor chips to form electrodes, and applying heat and pressure to the semiconductor package using a thermocompression bonding device.
[0008] In the case of thermocompression bonding equipment, if flux is used, the heat of the bonding head accumulates in the flux as it is repeatedly immersed in the flux, activating the flux and causing problems such as hardening of the flux.As a result, conventional thermocompression bonding equipment does not use flux, but uses semiconductor packages with bumps coated with NCF (Non Conductive Film) for thermocompression bonding.
[0009] However, as the pitch of semiconductor bumps becomes smaller and smaller to achieve faster signal transmission, lower power consumption, and higher performance, it is difficult to manufacture a film having the required functions while limiting the height so that it can be attached to the bumps that are lowered due to the fine pitch.Additional film attachment and removal processes are required, which causes an increase in manufacturing costs.
[0010] If flux is used in bonding equipment, it has the advantages of removing contaminants and oxides on the metal that interfere with the soldering process, improving the surface tension of the solder (bump), and improving the wetting effect by allowing the solder to diffuse smoothly into the metal to be soldered, so the use of flux is also required in thermocompression bonding equipment.
[0011] With the trend of semiconductor chips becoming smaller and thinner, in a situation where package bumps are formed with fine pitches, it is becoming important to immerse the bumps in a resin-like flux rather than a film in order to provide good wettability to the bumps overall without voids during bonding. Therefore, it is necessary to immerse the bumps in flux during bonding to remove oxides from the bumps, improve electrical contact, and improve lead flow.
[0012] On the other hand, when performing thermocompression bonding using flux, the bonding head immerses the bump-formed surface of the semiconductor chip in flux while adsorbing the semiconductor chip, then moves to the board and thermocompresses the semiconductor chip to attach it to the board. In order to apply a fixed amount of flux to the bumps, the flux contained in the flux section is adjusted to a certain height (flattened flux) before the flux immersion work is performed. Next, the bonding head heats the bumps and flux of the adsorbed semiconductor chip using the built-in heating member and performs thermocompression bonding on the board to attach them. At this time, the heating member is heated to about 180°C to melt the bumps and flux, and cooling air is applied to the heating member to solidify the molten bumps and flux, cooling them to about 100°C, and work on the subsequent semiconductor chip is performed.
[0013] Even after cooling, the bonding head maintains a temperature of approximately 100°C, and when working on the subsequent semiconductor chip, the next semiconductor chip is picked up and its bump-forming surface is immersed in flux in a state of residual heat.
[0014] In this case, residual heat remaining in the joining head is transferred to the flux provided in the flux section, and the transferred residual heat accumulates and can cause a problem of altering the flux. In the case of flux, activation is initiated by heat, so the flux on the flux section can be activated and altered before joining. Altered flux cannot function properly during joining, which can lead to poor joining.
[0015] Furthermore, the altered flux makes it difficult to flatten the flux, and even if it is determined that the flux has been flattened within the flux portion, a portion of the flux may harden, resulting in a problem that the amount of flux actually applied to the bumps is insufficient.
[0016] In addition, even if the bonding head immerses the bump-forming surface of the semiconductor chip in a fixed amount of flux, the residual heat of the bonding head can vaporize the flux during the process of transporting the semiconductor chip from the flux section to the substrate, which makes it difficult to maintain a fixed amount of flux applied to the bump-forming surface, which can lead to a deterioration in bonding quality.
[0017] If the heating element is cooled to a lower temperature so as not to transfer the residual heat to the flux, it will take a long time to cool, which will increase the time required to bond each semiconductor chip, resulting in poor productivity. It will also take a long time to reheat the heating element to perform thermocompression bonding to the subsequent semiconductor chip, resulting in reduced efficiency.
[0018] Therefore, the bonding apparatus must be equipped with a separate picker in addition to the bonding head, and the semiconductor chip must be immersed in the flux. A table on which the semiconductor chip can be temporarily placed is also required in order to transfer the flux-coated semiconductor chip to the bonding head.
[0019] In addition, in the case of a TSV package, since the presence or absence of foreign matter in each layer of stacked semiconductor chips can determine whether the package is defective, foreign matter inspection is required for the substrate to which the semiconductor chips are bonded and the surface of each semiconductor chip to be sequentially stacked. With the existing bonding device, when the bonding process of a specific layer is completed, before stacking and bonding the subsequent semiconductor chip, the substrate is taken out of the bonding device and a separate foreign matter inspection is performed, and then the substrate is again carried into the bonding device to perform the bonding process for stacking the subsequent semiconductor chips. As the bonding process and the foreign matter inspection process are separated, the work of carrying out and carrying out the substrate to and from the bonding device and the inspection device is repeated, which causes a problem of a decrease in UPH.
[0020] Another existing bonding machine is equipped with a Particle Vision that inspects for foreign objects on the surfaces of the substrate and semiconductor chip together with a Slit Vision driver within the bonding machine. However, the Slit Vision driver must move to the substrate every time a foreign object inspection is performed after or during bonding, which delays the process. In addition, the more inspections are performed, the longer the delay time becomes, making the inspection inefficient and resulting in a reduction in UPH.
[0021] In addition, frequent driving of the slit vision driving unit for foreign body inspection can accelerate mechanical deformation, which can cause alignment errors between the substrate and the semiconductor chip, resulting in a deterioration in bonding quality.In addition, foreign bodies can be introduced into the substrate during the substrate transport process, contaminating the substrate and the surfaces of the stacked semiconductor chips.
[0022] Also, there is a problem that the semiconductor chip may be subjected to impact or damage in the process in which the bonding head comes into contact with the semiconductor chip to pick up the thin semiconductor chip. Summary of the Invention [Problem to be solved by the invention]
[0023] In order to solve the above problems, the present invention provides a thermocompression bonding apparatus that includes a die picker that picks up a semiconductor chip and immerses it in flux, and when a semiconductor chip coated with flux is transferred, the device transfers the flux to a die block having an escape groove for allowing the flux coated on the underside of the semiconductor chip to escape. This prevents the heat of the bonding head from being transferred to the flux, prevents the flux from changing and vaporizing, and improves the efficiency of thermocompression bonding using flux.
[0024] Another object of the present invention is to provide a thermocompression bonding apparatus capable of inspecting whether or not a foreign object has been introduced into a substrate within the bonding apparatus and continuously bonding semiconductor chips.
[0025] Another object of the present invention is to provide a thermocompression bonding apparatus capable of picking up a semiconductor chip in a non-contact manner during the process of picking up the semiconductor chip, thereby minimizing impact and damage to the semiconductor chip.
[0026] Another object of the present invention is to provide a thermocompression bonding apparatus having a die block capable of supporting and seating a semiconductor chip in a parallel manner without tilting the semiconductor chip during the transfer process.
[0027] Another object of the present invention is to provide a thermocompression bonding apparatus that can minimize the amount of Z-axis movement by managing a die picker that needs to repeatedly move while working in each area in two height modes: the moving height and the working height.
[0028] Another object of the present invention is to provide a thermocompression bonding apparatus that can realize a low bonding pressure by minimizing frictional force generated when a shaft of a bonding head moves vertically, and can realize a desired bonding force precisely and quickly.
[0029] Another object of the present invention is to provide a thermocompression bonding apparatus that includes a reject picker that directly separates and removes the defective semiconductor chip from the bonding head that is sucking the defective semiconductor chip, thereby reliably separating the defective semiconductor chip from the bonding head and accurately loading the separated defective semiconductor chip onto a collection section.
[0030] Another object of the present invention is to provide a thermocompression bonding apparatus that can ensure uniform bonding quality and temperature uniformity regardless of the position of the substrate by providing a heat diffusion area on a heating table that diffuses heat transferred from a heating plate or a bonding head during the thermocompression bonding process, thereby preventing heat accumulation on the outer periphery of the substrate and matching thermal equilibrium conditions between the center and the outer periphery of the substrate.
[0031] Another object of the present invention is to provide a thermocompression bonding apparatus capable of minimizing frictional force generated when a shaft of a bonding head moves vertically to achieve low force.
[0032] Another object of the present invention is to provide a thermocompression bonding apparatus in which a flux tank for supplying flux and flattening is movably installed on the immersion plate while the immersion plate is fixed, thereby ensuring the stability of the immersion plate.
[0033] Another object of the present invention is to provide a thermocompression bonding apparatus that can increase the amount of tape expansion through an expanding section that prevents the tape from falling off the ring frame during the tape expansion process, thereby ensuring a sufficient separation distance for semiconductor chips. [Means for solving the problem]
[0034] In order to achieve the above object, a thermocompression bonding apparatus according to an embodiment of the present invention includes a flip-over picker that picks up individualized semiconductor chips from a tape having the individualized semiconductor chips attached thereto and turns the semiconductor chips upside down, a die picker that receives the semiconductor chips from the flip-over picker, a flux unit that contains flux for immersing a bottom surface of the semiconductor chip in the flux, and an up-looking vision that inspects the bottom surface of the semiconductor chip for the presence or absence of cracks. a slit vision that simultaneously photographs the upper surface of the semiconductor chip picked up by the bonding head and the upper surface of the substrate to which the semiconductor chip is to be bonded, to inspect the alignment of the semiconductor chip; and a die block that is fixedly disposed below the moving path of the die picker and the bonding head, to which the semiconductor chip coated with flux is transferred, and that has an escape groove for allowing the flux coated on the lower surface of the semiconductor chip to escape, wherein the die picker immerses the lower surface of the semiconductor chip in the flux and transfers it to the die block, and the bonding head picks up the semiconductor chip coated with flux from the die block and bonds it to the substrate by thermocompression.
[0035] In addition, according to a thermocompression bonding apparatus according to an embodiment of the present invention, the die picker forms a negative pressure while spaced apart from the semiconductor chip to suck and adsorb the semiconductor chip from the flip-over picker, and the bonding head forms a negative pressure while spaced apart from the semiconductor chip to suck and adsorb the semiconductor chip coated with flux from the die block.
[0036] In addition, according to an embodiment of the thermocompression bonding apparatus of the present invention, the working areas of the flip-over picker, the flux unit, the apple picking vision, and the die block are arranged in a row so as to be located on the same line along the movement direction of the die picker, and the die picker moves to the same preset height when moving to the top of each working area of the flip-over picker, the apple picking vision, and the die block, and the preset height is the same as the height corresponding to the working distance of the apple picking vision when inspecting the underside of the semiconductor chip with the apple picking vision.
[0037] In addition, according to a thermocompression bonding apparatus according to an embodiment of the present invention, the die picker includes a picker body having a pickup arm formed thereon and movably mounted to pick up the semiconductor chip; a mounting member to which the picker body is mounted so as to be able to rise and fall; a first rotating shaft extending along the movement direction of the picker body and into which the mounting member is inserted and coupled to move the mounting member in the movement direction of the picker body by rotating; a second rotating shaft extending in a direction parallel to the first rotating shaft at an upper or lower part of the first rotating shaft and rotatably mounted in the axial direction; and a switching member mounted on the second rotating shaft and raising and lowering the picker body from the mounting member as the second rotating shaft rotates.
[0038] In addition, according to a thermocompression bonding device according to an embodiment of the present invention, the switching member comprises a link that is connected to the second rotating shaft and can rotate together with the second rotating shaft, and a cam follower that is attached to the other side of the link and is connected to a bracket extending to a lower part of the picker body, the bracket being a "C" shaped bracket, and the cam follower is connected while being housed inside the "C" shaped bracket.
[0039] In addition, according to the thermocompression bonding apparatus according to an embodiment of the present invention, the working areas of the flip-over picker, the flux part, the apple picking vision, and the die block are arranged in a row so as to be located on the same line along the moving direction of the die picker, the flip-over picker, the flux part, the apple picking vision, the die block, and the die picker are each provided in pairs, the pickup arm is formed to protrude from a picker body to a position corresponding to an upper part of each working area of the flip-over picker, the flux part, the apple picking vision, and the die block, the die picker further includes a fixed frame having the first rotation shaft and the second rotation shaft mounted on one side thereof and guiding the movement of the picker body, the pair of die pickers are provided on one side and the other side of the fixed frame, respectively, and the pair of the flip-over picker, the flux part, the apple picking vision, and the die block are formed symmetrically with respect to the fixed frame.
[0040] In addition, according to an embodiment of the thermocompression bonding apparatus of the present invention, the flux unit includes an immersion plate having a flux accommodating groove formed therein for accommodating flux, a flux tank movably installed on the immersion plate and having a container for accommodating flux opened downward, a moving bracket attached to one side of the flux tank, and a flux tank transport unit including a guide member for guiding movement of the flux tank and a moving block for transporting the flux tank along the guide member, wherein an accommodating groove is formed in one of the moving bracket and the moving block, and an insertion part to be inserted into the accommodating groove is formed in the other, so that the flux tank is transported according to the transport of the moving block, and when an accommodating groove is formed in one of the moving bracket and the moving block, the moving bracket or the moving block includes a frame and a guide member coupled to upper portions on both sides of the frame, and the accommodating groove is formed by the frame and the guide member.
[0041] In addition, according to the thermocompression bonding apparatus of an embodiment of the present invention, the appleooking vision is characterized in that it inspects the presence or absence of cracks in the semiconductor chip when the flux is not applied, and inspects the underside of the semiconductor chip when the flux is applied.
[0042] According to the thermocompression bonding apparatus of the embodiment of the present invention, the bonding head includes a bonding tool having a heating member for heating the semiconductor chip and bonding the semiconductor chip by thermocompression bonding, a shaft provided on the upper part of the bonding tool and mounted so as to be movable up and down, a load control unit that supports the shaft and applies a predetermined load to the weight of the shaft, a pressing unit provided on the upper part of the load control unit and includes a mover fixed to an outer circumferential surface of the shaft and a driver that drives the mover to be movable in a vertical direction to press the bonding tool with a predetermined force, and The semiconductor chip may include a first load measuring unit that is provided between the pressing unit and the pressing unit and that measures the load applied to the semiconductor chip in real time; a rotary motor that is provided above the pressing unit and that rotates the shaft; and a low-friction coupling that connects the rotary motor and the shaft and transmits the rotational force of the rotary motor to the shaft, wherein the low-friction coupling has an upper portion connected to the rotary motor and a lower portion connected to the shaft, forming a space between the rotary motor and the shaft, and the shaft may be raised and lowered by the movable element between the space.
[0043] In addition, a thermocompression bonding apparatus according to an embodiment of the present invention further includes a heating table to which a substrate to which the semiconductor chip is to be bonded is transferred, and a second load measuring unit provided on one side of the heating table and contacting the bonding head to measure the load of the bonding head, wherein the first load measuring unit is set so that a measurement value of the first load measuring unit is equal to a measurement value of the second load measuring unit.
[0044] In addition, according to the thermocompression bonding apparatus according to an embodiment of the present invention, the shaft passes through the movable element of the pressing unit, and the shaft and the movable element are rotated together by the rotary motor to rotate the bonding tool.
[0045] In addition, according to the thermocompression bonding apparatus according to an embodiment of the present invention, the low-friction coupling is capable of expanding and contracting in the vertical direction with its upper portion fixed when the shaft is raised and lowered in the space separated by the mover.
[0046] In addition, according to a thermocompression bonding apparatus according to an embodiment of the present invention, the escape groove of the die block has an open upper portion and an inwardly sloping surface formed thereon, and a side surface of the semiconductor chip is supported by the inclined surface so that a bottom surface of the escape groove is spaced apart from a bottom surface of the escape groove.
[0047] In addition, according to a thermocompression bonding apparatus according to an embodiment of the present invention, the escape groove of the die block has an open upper portion and an inwardly sloping surface formed thereon, and a protruding end extending horizontally is formed at a lower portion of the inclined surface to support a bottom surface of the semiconductor chip, and an edge of the bottom surface of the semiconductor chip is supported by the protruding end to space the bottom surface of the semiconductor chip from the bottom surface of the escape groove.
[0048] In addition, according to a thermocompression bonding apparatus according to an embodiment of the present invention, the escape groove is formed by a plurality of protruding blocks, each protruding block is formed to be inclined inward, and adjacent protruding blocks are spaced apart from each other.
[0049] In addition, according to a thermocompression bonding apparatus according to an embodiment of the present invention, the die block is rotatably provided, and the die picker transfers the semiconductor chip to the escape groove of the die block in a state in which the die block is rotated by an angle of twist of the semiconductor chip in accordance with an inspection result of the appleooking vision.
[0050] In addition, according to the thermocompression bonding apparatus of an embodiment of the present invention, after the semiconductor chip is transferred to the die block, the die block rotates and returns to its initial position before the rotation, and the bonding head picks up the semiconductor chip coated with flux from the die block.
[0051] In addition, a thermocompression bonding apparatus according to an embodiment of the present invention further includes a reject picker that removes from the bonding head a defective semiconductor chip that is determined to be defective as a result of the inspection by the appleooking vision, and a collection unit in which the defective semiconductor chip is discarded by the reject picker, and the reject picker is formed with a duct for sucking or discharging air and includes a suction unit that sucks up a semiconductor chip and a rotating member that rotates the suction unit 180 degrees to invert the top and bottom surfaces of the semiconductor chip sucked to the suction unit, and the suction unit discharges air into the semiconductor chip inverted upside down by the rotating member and drops the semiconductor chip toward the collection unit.
[0052] In addition, a thermocompression bonding apparatus according to an embodiment of the present invention may further include a heating table to which a substrate to be bonded with a semiconductor chip is transferred, the heating table including a chuck plate on which the substrate to be bonded is placed, a base provided under the chuck plate and connected to a vacuum generator for forming a negative pressure on the chuck plate, and a heating plate provided between the chuck plate and the base for transferring heat to the chuck plate, the chuck plate including an adsorption region for adsorbing the substrate and a thermal diffusion region for diffusing heat transferred from the heating plate or the bonding head.
[0053] In addition, a thermocompression bonding apparatus according to an embodiment of the present invention further includes a particle vision device attached to one side of the bonding head for detecting the presence or absence of foreign matter on an upper surface of a substrate to be bonded, and the particle vision device detects the presence or absence of foreign matter on the upper surface of the substrate to which the semiconductor chip is bonded or on the upper surface of a lower semiconductor chip to which the semiconductor chip is bonded.
[0054] In addition, a thermocompression bonding apparatus according to an embodiment of the present invention further includes an expanding unit that expands the tape of a ring frame having a tape with individualized semiconductor chips attached thereto adhered to its underside, the expanding unit including a support member that supports the underside of the tape, a pressure plate that presses downward the upper surface of the ring frame to which the tape is adhered and is arranged to be movable up and down, and a peel-off prevention plate that presses the underside of the tape adhered to the ring frame in a direction opposite to the pressing direction of the pressure plate, the elastic member supporting the tape, supporting the tape in the direction opposite to the pressing direction of the pressure plate due to the pressure of the pressure plate, and deforming so that the pressure plate and the peel-off prevention plate descend together, thereby expanding the tape. Effect of the Invention
[0055] The thermocompression bonding apparatus of the present invention is equipped with a particle vision on one side of the bonding head that can inspect the top surface of the substrate for foreign objects, and after performing a foreign object inspection using the particle vision before bonding a semiconductor chip to the substrate, a new semiconductor chip can be bonded to the top of a substrate or semiconductor chip for which no foreign objects are detected, thereby having the advantage that bonding and inspection can be performed continuously without any additional movement of the mechanical parts.
[0056] In addition, the thermocompression bonding apparatus of the present invention realizes two-mode height control so that the die picker moves from a first height, which is in an elevated state, to each work area and inspects the semiconductor chip, and then moves to a second height, which is in a lowered state, to perform multiple tasks such as receiving the semiconductor chip, dipping it in flux, and transferring it to the die block, thereby minimizing the up and down movement of the die picker and increasing the UPH.
[0057] In addition, by independently providing the first drive unit and the second drive unit which guide the horizontal and vertical movement of the die picker externally, the thermocompression bonding apparatus of the present invention can miniaturize the structure of the die picker and accommodate the die picker within the limited space of the bonding apparatus, thereby making it possible to realize a compact device.
[0058] In addition, the thermocompression bonding apparatus of the present invention has the effect of minimizing the impact on the semiconductor chip when the die picker or the bonding head picks up the semiconductor chip by attracting and suctioning the semiconductor chip with air while the die picker and the bonding head are not in contact with the top surface of the semiconductor chip.
[0059] In addition, in the thermocompression bonding apparatus of the present invention, the die picker is specialized in the processes of receiving the semiconductor chip, immersing it in flux, inspecting it, and transferring it to the die block, and the bonding head only performs the task of picking up the semiconductor chip transferred to the die block and bonding it to the substrate, thereby shortening the work path and movement path of the bonding head and improving the bonding speed of the entire bonding apparatus.
[0060] In addition, in the thermocompression bonding apparatus of the present invention, the die picker immerses the die in flux and temporarily places it on the die block, and the bonding head transports the semiconductor chip temporarily placed on the die block to the substrate and thermocompresses it, thereby preventing the problem of the heat of the bonding head altering the flux on the flux portion. Also, since the moving path of the bonding head is shortened, the amount of flux scattered by the residual heat of the bonding head in the process of the bonding head transporting the semiconductor chip can be reduced, thereby maintaining the fixed amount of applied flux.
[0061] In addition, the thermocompression bonding apparatus of the present invention has an escape groove formed in the die block, which prevents the flux applied to the underside of the semiconductor chip from adhering to the bottom surface of the die block, thereby maintaining a constant amount of flux and preventing contamination of the bottom surface of the die block by flux.
[0062] In addition, the joining head of the thermocompression joining apparatus of the present invention connects a rotary motor to the upper part of a low-friction coupling and connects a shaft to the lower part, and forms a separation space between the upper part connecting the rotary motor and the lower part connecting the shaft, thereby enabling the shaft to be raised and lowered with low friction while transmitting the rotational force of the rotary motor to the shaft, and the load control part supports the shaft without contact and supports the shaft so that it does not vibrate, thereby minimizing the supporting friction force and achieving no load on the z-axis.
[0063] In addition, the thermocompression bonding apparatus according to the present invention has a heat diffusion area on the heating plate, which prevents heat accumulation on the outer periphery of the substrate, thereby ensuring temperature uniformity regardless of the position on the substrate, ensuring bonding quality and reducing the defect rate. When multiple vertically stacked semiconductor chips are thermocompression bonded, there is no difference in the bonding state of the semiconductor chips and the hardening state of the flux between the upper and lower parts of the stacked semiconductor chips, improving the bonding quality.
[0064] In addition, the thermocompression bonding apparatus of the present invention can reliably remove defective semiconductor chips by sucking them from the bonding head using a reject picker, thereby minimizing the problem of picking up or bonding other semiconductor chips while a defective semiconductor chip remains on the bonding head, which can lead to defects. Since the defective semiconductor chips coated with flux can be easily dropped into a collection section and removed, the defective semiconductor chips do not scatter around and contaminate other components of the bonding apparatus or the surrounding area, and the reliable removal of the defective semiconductor chips has the effect of preventing mass defects.
[0065] In addition, the thermocompression bonding apparatus of the present invention can adopt a structure in which the flux tank can move freely in the vertical direction when the flux section is connected between the flux tank and the flux tank transport section, and can perform leveling work to flatten the immersion plate even if there is mechanical deformation or processing error. Furthermore, the distance between the moving bracket attached to one side of the flux tank and the moving block that moves along the guide member that guides the movement of the flux tank is adjustable, which has the effect of making it possible to adjust the parallelism of the squeegee of the flux tank and the immersion plate without being affected by the lower structure.
[0066] In addition, the thermocompression bonding apparatus of the present invention has an expanding section that can uniformly expand the tape in a radial direction over the entire area of the ring frame, thereby ensuring a sufficient separation distance between semiconductor chips and allowing the semiconductor chips to be easily picked up from a flip-over picker without interference between the semiconductor chips. [Brief description of the drawings]
[0067] [Figure 1] FIG. 1 is a plan view of a thermocompression bonding apparatus according to an embodiment of the present invention. [Diagram 2] FIG. 1 is a front view of a thermocompression bonding apparatus according to an embodiment of the present invention. [Diagram 3] FIG. 2 illustrates a die picker in an embodiment of the present invention. [Figure 4] FIG. 4(a) is a diagram showing a lowered state of the die picker in the embodiment of the present invention, and FIG. 4(b) is a diagram showing an elevated state of the die picker in the embodiment of the present invention. [Diagram 5]FIG. 5(a) is a diagram showing a state in which the die picker in an embodiment of the present invention is positioned at a second height and receives a semiconductor chip from a flip-over picker, (b) is a diagram showing a state in which the die picker in an embodiment of the present invention is positioned at a second height and immerses a semiconductor chip, (c) is a diagram showing a state in which the die picker in an embodiment of the present invention is positioned at a first height and inspects the semiconductor chip using an apple picking vision, and (d) is a diagram showing a state in which the die picker in an embodiment of the present invention is positioned at a second height and provides a semiconductor chip with flux applied to the die block. [Figure 6] FIG. 2 is a diagram showing a flux section in an embodiment of the present invention. [Figure 7] FIG. 7(a) is a view showing a state in which a semiconductor chip is mounted on a die block according to an embodiment of the present invention, and FIG. 7(b) is a view showing a cross section taken along line AA' of FIG. 7(a). [Figure 8] FIG. 8(a) is a view showing a state in which a semiconductor chip is mounted on a die block according to another embodiment of the present invention, and FIG. 8(b) is a view showing a cross section taken along line BB' of FIG. 8(a). [Figure 9] FIG. 2 is a diagram showing a bonding head according to an embodiment of the present invention. [Figure 10] 13 is a diagram showing a state in which a reject picker receives a defective semiconductor chip from a bonding head in an embodiment of the present invention. FIG. [Figure 11] 1 is a diagram showing a state in which a reject picker provides a defective semiconductor chip to a reject box in an embodiment of the present invention. FIG. [Figure 12] FIG. 12(a) is a diagram showing a conventional heating table, and (b) is a diagram showing the heat transfer state of the heating table on the CC' cross section of FIG. 12(a). [Figure 13] FIG. 2 shows a plan view of a heating table according to an embodiment of the present invention. [Figure 14] FIG. 2 shows a cross-sectional view of a heating table according to an embodiment of the present invention. [Figure 15] FIG. 2 illustrates a bottom view of a chuck plate according to an embodiment of the present invention. [Figure 16] FIG. 16(a) is a diagram showing a heating table formed with a heat dissipation portion in an embodiment of the present invention, and FIG. 16(b) is a diagram showing the heat transmission state of the heating table on the D-D' cross section of FIG. 16(a). [Figure 17] 17(a) to (c) are diagrams showing an expanding section and an operating process of the expanding section in an embodiment of the present invention.
[0068] The following merely illustrates the principles of the present invention. Thus, those skilled in the art will be able to invent various devices that embody the principles of the invention and fall within the concept and scope of the invention, although not explicitly described or illustrated herein. Furthermore, all conditional terms and embodiments listed herein are expressly intended only to allow the concept of the invention to be understood in principle, and should not be understood as being limited to the embodiments and conditions specifically listed in this manner.
[0069] The above objects, features and advantages will become more apparent from the following detailed description taken in conjunction with the accompanying drawings, which will enable those skilled in the art to easily understand the technical concept of the invention.
[0070] The embodiments described herein are described with reference to cross-sectional views and / or perspective views which are ideal exemplary views of the present invention. The thicknesses of films and regions and the diameters of holes shown in such drawings are exaggerated for the purpose of effectively explaining the technical contents. The shapes of the exemplary views may be deformed due to manufacturing techniques and / or tolerances.
[0071] A thermocompression bonding apparatus 10 according to an embodiment of the present invention will now be described in detail.
[0072] In the thermocompression bonding apparatus 10 described below, the length direction refers to the ±x direction, the width direction refers to the ±y direction, the lifting direction refers to the ±z direction, and the θ direction refers to the direction in which the apparatus can rotate clockwise or counterclockwise on the xy plane.
[0073] Fig. 1 is a plan view of a thermocompression bonding apparatus 10 according to an embodiment of the present invention, and Fig. 2 is a front view of the thermocompression bonding apparatus 10 according to an embodiment of the present invention.
[0074] 1 and 2, a thermocompression bonding apparatus 10 according to an embodiment of the present invention includes a flip-over picker 100 that picks up a semiconductor chip separated from a wafer and turns it upside down, a die picker 200 that receives the semiconductor chip from the flip-over picker 100, a flux unit 300 that contains flux for immersing the bottom surface of the semiconductor chip picked up by the die picker 200 in the flux, an approching vision 400 that inspects the bottom surface of the semiconductor chip or the presence or absence of cracks, and a heating member provided inside. The bonding head 700 includes a bonding head 910 for bonding the semiconductor chip to the substrate by thermocompression bonding, a heating table 910 to which the substrate to be bonded is transferred, a slit vision 800 for simultaneously photographing the semiconductor chip picked up by the bonding head and the top surface of the substrate to which the semiconductor chip is bonded, and a die block 500 fixedly disposed below the moving path of the die picker 200 and the bonding head 700, to which the semiconductor chip coated with flux is transferred and which has an escape groove for allowing the flux coated on the bottom surface of the semiconductor chip to escape. Here, the die picker 200 immerses the bottom surface of the semiconductor chip in flux and transfers it to the die block 500, and the bonding head 700 picks up the semiconductor chip coated with flux from the die block 500 and bonds it to the substrate by thermocompression bonding.
[0075] First, the flip-over picker 100 can move up and down in the Z-axis direction to pick up the semiconductor chips attached on the tape t in an expanded state and deliver them to a bonding head, and includes a suction unit that can suction the semiconductor chips by vacuum pressure. Also, the flip-over picker 100 can be configured to be rotatable to flip the top and bottom surfaces of the semiconductor chips suctioned by the flip-over picker 100.
[0076] At this time, the semiconductor chips are supplied in a state where they are attached to a tape t, and in order to facilitate operations such as transportation, the edge of the upper surface of the tape t is attached to a ring frame rf made of a ring-shaped plate material. Also, the flip-over picker 100 can vacuum-suck the semiconductor chips attached to the tape t to separate the semiconductor chips from the tape t, and an ejector (not shown) may be further provided under the tape t to separate the semiconductor chips from the tape t. The ejector slides the semiconductor chips upwards while the semiconductor chips are sucked by the flip-over picker 100, so that the semiconductor chips can be easily separated from the tape t.
[0077] An ejector (not shown) pushes up the semiconductor chips without interference from surrounding semiconductor chips, and the tape t is expanded by the expanding section 101 of the present invention so that the flip-over picker 100 can easily pick up the semiconductor chips attached to the tape t, thereby increasing the spacing between the semiconductor chips.
[0078] As shown in FIG. 17, the expanding section 101 for expanding the tape t of the ring frame rf to which the tape t having the individualized semiconductor chips attached thereto is attached includes a support member 130 for supporting the underside of the tape t, a pressure plate 110 for pressing either the ring frame rf or the tape t downward and arranged to be movable up and down, and a peeling prevention plate 120 having an elastic member for pressing the underside of the tape attached to the ring frame rf in the direction opposite to the pressing direction of the pressure plate 110, the elastic member supporting the tape and supporting the tape in the direction opposite to the pressing direction of the pressure plate due to the pressure of the pressure plate, and deforming so that the pressure plate and the peeling prevention plate descend together, thereby expanding the tape.
[0079] 17a to 17c, the expanding unit 101 of the present invention can be seen to have an operating process of expanding the tape t of a ring frame rf having individualized semiconductor chips attached thereto and bonded to its underside.
[0080] The expanding section 101 of the present invention includes a support member 130 that supports the underside of the tape t, a pressure plate 110 that is movable up and down by pressing the ring frame rf, a peel-off prevention plate 120 that presses the tape t in the direction opposite to the pressing direction of the pressure plate 110, and an elastic member 140 provided on the lower part of the peel-off prevention plate 120.
[0081] At this time, the pressing plate 110 includes a pressing member 111 for pressing the ring frame rf downward, a seating member 112 on which the ring frame rf is seated, and a connecting member 113 for connecting the pressing member 111 and the seating member 112, and the semiconductor chip is supported by the ring frame rf in a state where it is attached to the tape t, and a wafer supply unit (not shown) seats the ring frame rf on the seating member 112 of the pressing plate 110. As shown in Fig. 17a, the seating member 112 can support the edge of the ring frame rf attached to the tape t.
[0082] When the pressing plate 110 is lowered with the ring frame rf seated on the seating member 112, the peeling prevention plate 120 can come into contact with the lower surface of the tape t, as shown in Fig. 17b. The tape t attached to the ring frame rf is supported with the pressing plate 110 in contact with the upper surface of the ring frame rf to which the tape t is attached, and the peeling prevention plate 120 in contact with the lower surface of the tape t attached to the ring frame rf.
[0083] In this state, when the pressure plate 110 further descends, the tape t expands as shown in Fig. 17c. That is, the pressure plate 110 descends and can press the ring frame rf downward with the lower surface of the pressing member 111 in contact with the upper surface of the ring frame rf. At the same time, the upper surface of the peeling prevention plate 120 can press the tape t in the opposite direction to the pressing direction of the pressure plate 110, i.e., upward, by the elastic force of the elastic member 140, with the upper surface of the peeling prevention plate 120 in contact with the lower surface of the tape t.
[0084] The pressing plate 110 and the peeling prevention plate 120 can clamp the ring frame rf and the tape t at the upper and lower parts, respectively, with the ring frame rf and the tape t positioned therebetween. At this time, the outer region of the tape t is clamped by the pressing plate 110 and the peeling prevention plate 120 and moves relatively downward based on the support member 130, and the central region of the tape t is prevented from moving by the support member 130, so that the tape t can expand in the radial direction based on the center point to separate the semiconductor chips.
[0085] In the embodiment of the present invention, the pressure plate 110 is provided so as to be able to rise and fall, and the support member 130 may be provided so as to be fixed, but both the pressure plate 110 and the support member 130 may be provided so as to be able to rise and fall.
[0086] 17, the tape t having the individualized semiconductor chips attached thereto is attached to the lower surface of the ring frame rf, the pressing plate 110 presses the upper surface of the ring frame rf, and the peeling prevention plate 120 presses the lower surface of the tape t attached to the ring frame rf. However, the tape t may be attached to the upper surface of the ring frame rf. In this case, the tape t and the ring frame rf are clamped by the pressing plate 110 and the peeling prevention plate 120 so that the pressing plate 110 presses the tape t and the peeling prevention plate 120 presses the ring frame rf, thereby preventing the tape t from expanding and coming off the ring frame rf.
[0087] The flip-over picker 100 can move up and down in the Z-axis direction to pick up the semiconductor chips attached on the tape t in an expanded state and deliver them to a bonding head, and includes a suction unit that can suction the semiconductor chips by vacuum pressure. Also, the flip-over picker 100 can be configured to be rotatable in order to flip the top and bottom surfaces of the semiconductor chips suctioned to the flip-over picker 100.
[0088] The flip-over picker 100 can pick up the semiconductor chip from the tape on which the individualized semiconductor chip is attached and turn it upside down. For this purpose, the flip-over picker 100 is provided so as to be able to rise and fall in the lifting direction (±z direction) and rotate 180° based on the lifting direction (±z direction). The flip-over picker 100 is located on the upper part of the adhesive tape and picks up the bump formation surface of the semiconductor chip on the adhesive tape. At this time, the molding surface of the semiconductor chip faces downward based on the lifting direction (±z direction). The flip-over picker 100 rotates 180° in the lifting direction (±z direction) while picking up the semiconductor chip. As a result, the semiconductor chip is turned upside down with the molding surface facing upward based on the lifting direction (±z direction).
[0089] The die picker 200 creates negative pressure while spaced apart from the semiconductor chip to pick up the upside-down semiconductor chip from the flip-over picker, and is configured to rise and fall in the elevation direction (±z direction) and move in the longitudinal direction (±x direction).
[0090] The die picker 200 of the present invention will now be described in more detail with reference to Figures 3, 4a and 4b.
[0091] FIG. 3 is a diagram showing a die picker 200 in an embodiment of the present invention, FIG. 4a is a diagram showing the die picker 200 in a lowered state in an embodiment of the present invention, and FIG. 4b is a diagram showing the die picker 200 in an raised state in an embodiment of the present invention.
[0092] In an embodiment of the present invention, the die picker 200 may include a picker body 210 having a pickup arm 211 for picking up semiconductor chips and movably mounted thereon, a mounting member 220 to which the picker body 210 is mounted so as to be capable of being raised and lowered, a first rotating shaft 230 extending along the movement direction of the picker body and to which the mounting member 220 is coupled and which moves the mounting member 220 in the movement direction of the picker body by rotating, a second rotating shaft 240 extending in a direction parallel to the first rotating shaft at the upper or lower part of the first rotating shaft 230 and rotatably mounted in the axial direction, and a switching member 250 mounted on the second rotating shaft 240 and which raises and lowers the picker body 210 from the mounting member 220 as the second rotating shaft 240 rotates.
[0093] With such a structure, the die picker 200 of the present invention can rise and fall in the lifting direction (±z-axis direction), and can move in the movement direction of the picker body, i.e., the longitudinal direction (±x-axis direction) in Figure 1.
[0094] The die picker 200 of the present invention is capable of moving a semiconductor chip in the longitudinal direction (±x-axis direction) and raising and lowering in the lifting direction (±z-axis direction) without increasing its volume, so that the first drive unit 231 can rotate the first rotating shaft 230 to move the picker body 210 in the x-axis direction, and the second drive unit 241 can rotate the second rotating shaft 240 to move (lift) the picker body 210 in the z-axis direction.
[0095] Referring again to FIG. 2, the first driving unit 231 is connected to one end of the first rotating shaft 230 to move the picker body 210, and the second driving unit 241 is connected to one end of the second rotating shaft 240 to enable the picker body 210 to move stably while allowing the picker body to be raised and lowered.
[0096] To explain each component of the die picker of the present invention in more detail, first, a picker body 210 is provided with a pick-up arm 211 for picking up semiconductor chips and is movably installed. The pick-up arm 211 of the die picker 200 may be formed to protrude from the picker body up to a position corresponding to the upper part of each working area of the flip-over picker 100, the flux unit 300, the appick vision 400, and the die block 500.
[0097] An adsorption member 210a is formed at one end of the pickup arm 211, and the adsorption member 210a can adsorb the semiconductor chip to pick it up. At this time, the adsorption member 210a can suck and adsorb the semiconductor chip by forming a negative pressure while separated from the semiconductor chip. By picking up the semiconductor chip by air pressure without contacting the semiconductor chip through the adsorption member 210a, it is possible to minimize the impact and damage applied to the semiconductor chip when the die picker picks up the semiconductor chip.
[0098] The picker body 210 may be provided to be capable of ascending and descending on the mounting member 220. The die picker 200 includes a lift guide 260 between the mounting member 220 and the picker body 210, and the picker body 210 can move (rise and descend) relative to the mounting member 220 along the lift guide 260.
[0099] The mounting member 220 may be coupled to a first rotating shaft 230. The first rotating shaft 230 extends along the moving direction of the picker body, to which the mounting member is coupled, and the mounting member may be moved in the moving direction of the picker body by rotating. A spiral groove is formed on the outer circumferential surface of the first rotating shaft, and the mounting member may be moved in the moving direction of the picker body, i.e., in the x-axis direction shown in FIG. 1, along the first rotating shaft 230 rotated by the first driving unit 231.
[0100] The first rotating shaft 230 is rotated by a first driving unit 231, which may be a motor.
[0101] The second rotating shaft 240 extends in a direction parallel to the first rotating shaft above or below the first rotating shaft and is rotatable in the axial direction. The second rotating shaft 240 is rotated by a second driving unit 241, which may be a motor.
[0102] The first driving unit 231 and / or the second driving unit 241 may be a ball screw motor. The types of the first driving unit 231 and the second driving unit 241 are not limited to the above examples.
[0103] One or more linear grooves may be formed along the length direction on the outer circumferential surface (surface) of the second rotating shaft 240. The grooves are formed on the outer circumferential surface of the second rotating shaft, and the switching member 250 has a protrusion that is inserted into the groove of the second rotating shaft, so that when the second rotating shaft rotates, the switching member 250 can also rotate together.
[0104] Here, the protrusion is configured to be coupled to the groove of the second rotating shaft 240 to transmit the rotational motion of the second rotating shaft 240 to the switching member 250, and the function of the protrusion can also be performed by providing a ball between the switching member 250 and the linear groove of the second rotating shaft 240.
[0105] Of course, at least one protrusion parallel to the length direction is provided on the outer circumferential surface (surface) of the second rotating shaft 240, and a groove is formed in the switching member 250, so that the protrusion can be inserted into and coupled to the groove of the switching member 250.
[0106] Here, the second rotating shaft 240 may be a spline, but is not limited to this.
[0107] The second rotating shaft 240 rotates the switching member 250 while rotating, and can move the picker body 210 up and down. In other words, the switching member 250 can switch the rotational motion of the second rotating shaft 240 with the translational motion of the picker body 210.
[0108] When the mounting member 220 moves in the x-axis, the switching member 250 can move in the x-axis together along the second rotating shaft 240. When the second rotating shaft 240 rotates, the switching member 250 can guide the lifting and lowering movement of the picker body 210, and when the first rotating shaft 230 rotates, the switching member 250 can guide the longitudinal movement of the picker body 210.
[0109] For this purpose, the switching member 250 of the present invention may include a link 251 connected to a second rotating shaft and rotatable together with the second rotating shaft, and a cam follower 252 attached to the other side of the link 251 and connected to a bracket 253 extending to the lower part of the picker body.
[0110] Moreover, the switching member 250 may include a link 251 having one side coupled to the second rotating shaft 240 and rotatable together with the second rotating shaft 240, a bracket 253 attached to the other side of the link 251 and coupled to the lower part of the picker body 210, and a cam follower 252 coupled to the bracket 253. The configuration of the switching member 250 is not limited to the above example, and other configurations capable of raising and lowering the picker body 210 by rotation may be used.
[0111] In this case, the first and second rotating shafts may be mounted on a fixed frame 290. The fixed frame 290 is configured to mount the first and second rotating shafts and extends in a length direction along the moving direction of the picker body to guide the movement of the picker body.
[0112] On the other hand, when the die pickers of the present invention are provided in a pair as shown in FIG. 1, each die picker may be attached to one side and the other side of the fixed frame and be provided so as to be independently movable in the longitudinal direction.
[0113] In the thermocompression bonding apparatus 10 according to the embodiment of the present invention, the first rotating shaft 230 and the second rotating shaft 240 may be provided at different heights or at the same height. As an example, as shown in Fig. 3, the first rotating shaft 230 may be provided at a higher position than the second rotating shaft 240, but the first rotating shaft 230 may also be provided at a lower position than the second rotating shaft 240, and there is no restriction on the relative heights of the first rotating shaft 230 and the second rotating shaft 240.
[0114] The bracket 253 may include a first horizontal frame 253b, a second horizontal frame 253c facing the first horizontal frame 253b in the lifting direction, and a connecting frame 253a connecting the first horizontal frame 253b and the second horizontal frame 253c. The first horizontal frame 253b, the second horizontal frame 253c, and the connecting frame 253a may form a U-shaped bracket 253. The cam follower 252 may be coupled to the U-shaped bracket 253 while being housed therein.
[0115] The connecting frame 253a can connect the first horizontal frame 253b and the second horizontal frame 253c on one side of the first horizontal frame 253b and the second horizontal frame 253c.
[0116] An upper portion of the connection frame 253a may be coupled to a lower portion of the picker body 210, or may be formed integrally with the picker body 210. A pick-up arm extends from an upper portion of the picker body 210, and an adsorption member 210a formed at one end of the pick-up arm creates negative pressure without contacting the semiconductor chip, thereby sucking and adsorbing the semiconductor chip.
[0117] The bracket 253 may form an accommodation space 253d surrounded by the first horizontal frame 253b, the second horizontal frame 253c, and the connecting frame 253a. The cam follower 252 may be positioned in the accommodation space 253d.
[0118] 4a, the cam follower 252 can contact the inner surface of the connecting frame 253a in the accommodation space 253d when the attraction member 210a is in the lowered state. The cam follower 252 can contact the first horizontal frame 253b, the second horizontal frame 253c, and the connecting frame 253a.
[0119] 4b, when the attraction member 210a is in the raised state, the cam follower 252 can be separated from the inner surface of the connection frame 253a in the accommodation space 253d. The cam follower 252 can be in contact with the first horizontal frame 253b and the second horizontal frame 253c.
[0120] The link 251 can rotate with the second rotating shaft 240 connected to one side as the rotating shaft, with the cam follower 252 connected to the hole on the other side. The link 251 can raise the cam follower 252 while rotating.
[0121] The cam follower 252, while positioned in the accommodation space 253d of the bracket 253, can move in the lifting and lowering direction (or make a circular motion) in response to the rotation of the link 251. The cam follower 252 can move the bracket 253 upward by moving in the lifting and lowering direction (±z direction), and can move away from the connecting frame 253a by moving in the width direction (±y direction). The cam follower 252 can move together with the bracket 253 in the lifting and lowering direction by making a circular motion, and can move relatively from the bracket 253 in the width direction.
[0122] The cam follower 252 may be provided so as to be drivable integrally with the bracket 253 in the lifting direction via the accommodation space 253d. The cam follower 252 performs circular motion together with the bracket 253 by rotation of the second rotating shaft 240, and moves relatively in a direction away from the inner surface of the connecting frame 253a within the accommodation space 253d of the bracket 253 fixed in the width direction (±y direction), and can move upward together with the first horizontal frame 253b while pushing it up in the upward direction.
[0123] As the second rotating shaft 240 rotates, the cam follower 252 can move in a direction away from the inner surface of the connecting frame 253a, lifting the bracket 253 and rising together with the bracket 253. At this time, in order to prevent the problem of the cam follower 252 coming out of the accommodation space 253d, the first horizontal frame 253b and the second horizontal frame 253c can be formed to be longer than the distance between the cam follower 252 and the connecting frame 253a.
[0124] Furthermore, the bracket 253 may be provided in a U-shape, a square shape, or an O-shape. The bracket 253 may be provided so as to form an elongated hole-shaped accommodation space 253d. The elongated hole-shaped accommodation space 253d can accommodate the movement of the cam follower 252 but prevent it from coming off.
[0125] With this configuration, the die picker 200 of the present invention can rise and fall in the lifting direction and move horizontally along the first rotation axis.
[0126] The die picker 200 of the present invention is capable of moving in the longitudinal direction (±x-axis direction) without increasing its size or volume, and is capable of rising and falling in the lifting direction (±z-axis direction), so that the first drive unit 231 can rotate the first rotating shaft 230 to move the picker body 210 in the x-axis direction, and the second drive unit 241 can rotate the second rotating shaft 240 to move (lift) the picker body 210 in the z-axis direction.
[0127] As a result, the first drive unit 231 and the second drive unit 241 are not directly connected to the picker body 210, the mounting member 220 and the switching member 250, but are connected via the first rotating shaft 230 and the second rotating shaft 240, so that the height and position of the die picker 200 can be changed, thereby achieving weight reduction and compactness.
[0128] The die picker 200 moves in the length direction (±x direction) to the upper part of the flip-over picker 100. The die picker 200 descends toward the semiconductor chip adsorbed to the flip-over picker 100 and adsorbs the upper surface (molding surface) of the semiconductor chip. When the semiconductor chip is adsorbed to the die picker 200, the bump formation surface faces downward based on the ascending and descending directions (±z directions) and is exposed to the outside.
[0129] The die picker 200 moves to above the flux section 300 with the semiconductor chip picked up.
[0130] The flux section 300 includes a flux containing groove for containing the flux so that the lower surface of the semiconductor chip is immersed in the flux.
[0131] As shown in FIG. 6, the flux unit 300 of the present invention includes an immersion plate 310 having a flux receiving groove formed therein for receiving flux, a flux tank 320 movably installed on the immersion plate 310 and formed by opening a container for receiving flux downward, a moving bracket 350 attached to one side of the flux tank 320, and a flux tank transport unit including a guide member 380 for guiding the movement of the flux tank 320 and a moving block 360 for transporting the flux tank 320 along the guide member 380, wherein one of the moving bracket 350 and the moving block 360 has a receiving groove formed therein and the other has an insertion part to be inserted into the receiving groove, and the flux tank 320 is transported in accordance with the transport of the moving block 360.
[0132] Here, the flux tank 320 is provided with a container for accommodating the flux that is open downward and can supply the flux to the immersion plate 310 side, and can include a squeegee for flattening the flux accommodated in the flux accommodation groove.
[0133] The flux tank 320 can move horizontally in the y-axis direction above the immersed plate 310 along the transport rails formed on both sides of the upper part of the base 330, and can flatten the flux using a squeegee while supplying flux to the flux receiving groove of the immersed plate 310. This allows the flux having a predetermined viscosity to be provided in a flat state so as to maintain a constant height on the immersed plate 310 based on the ascending and descending direction of the bonding head.
[0134] The flux tank 320 is mounted on the top of the immersion plate 310 so that it can move back and forth. Therefore, when the flux tank 320 moves forward (to one side), the flux tank 320 is positioned on top of the immersion plate 310 and the flux stored in the container of the flux tank 320 can be supplied to the flux storage groove of the immersion plate 310. When the flux tank 320 moves backward (to the other side), the top surface of the flux becomes flat and the top of the flux storage groove is exposed, allowing the semiconductor chip to be immersed in the flux.
[0135] Therefore, when the underside of the semiconductor chip is immersed in flux, it is preferable that the flux tank 320 is moved backward so as to avoid the flux containing groove of the immersion plate 310.
[0136] In the present invention, the moving bracket 350 fastened to the flux tank 320 side is constrained in the transport direction via the guide member 340, but since the moving bracket 350 and the moving block 360 are not constrained or fastened to each other in the vertical direction, the moving bracket 350 can move in the y-axis direction even if the distance between the moving bracket 350 and the moving block 360 varies. Therefore, even if the transport rail is deformed during the process of transporting the flux tank 320, the moving bracket 350 transporting the flux tank 320 can be allowed to move in the vertical direction, and the drive of the flux tank 320 is not restricted.
[0137] Furthermore, even when adjusting the flatness based on the immersion plate 310, the moving bracket 350 and the moving block 360 are not constrained to each other, and the distance between them can be freely changed in the vertical direction. Therefore, even if there is structural twisting or mechanical deviation, it can be easily corrected without having to disassemble structures such as the flux tank 320, the moving bracket 350, and the moving block 360.
[0138] If the base 330 on which the immersion plate 310 is mounted cannot maintain a horizontal state due to overheating, external impact, or processing tolerances, resulting in a difference in height between the left and right sides, when the moving bracket 350 mounted on the flux tank 320 and the moving block 360 of the flux tank transport unit are fastened and fixed, the upper surface of the immersion plate 310 will be inclined, making it impossible to apply a fixed amount of flux uniformly when immersing the semiconductor chips in the flux, and twisting between the mechanical parts may occur.
[0139] However, in the present invention, even if the base 330 cannot be kept horizontal, the level of the base 330 can be adjusted to adjust the flatness of the immersion plate 310 through the flatness adjustment member, and in this case, the distance between the moving bracket 350 and the moving block 360 can be changed in the process of adjusting the flatness of the immersion plate 310.
[0140] Of course, even if the separation distance is variable, the insertion portion of the moving bracket 350 remains inserted into the accommodating groove of the moving block 360, and the movement of the moving block 360 is transmitted to the moving bracket 350 via the guide member 340, so that the moving bracket 350 can move in the same direction as the movement direction of the moving block 360.
[0141] With this structure, the immersion plate 310 is fixed with the flatness of the flux receiving groove adjusted, and the flux tank 320 can move back and forth on the immersion plate 310, so that the shaking and vibration of the immersion plate 310 can be minimized and stability can be ensured.
[0142] In addition, since the moving bracket 350 and the moving block 360 are not vertically separated and constrained during the process of transporting the flux tank 320, structural distortion between the flux tank 320 and the flux tank transport unit that drives the flux tank 320 due to a height deviation of the immersion plate 310 or the base 330 can be prevented, and even if there is a height deviation, the height of the flux tank 320 can be flexibly adjusted to prevent pinching.
[0143] Meanwhile, the die picker 200 receives the semiconductor chip from the flip-over picker 100 and then moves to the top of the flux receiving groove of the immersion plate 310. Then, it descends by a preset height to immerse the bottom surface of the semiconductor chip in the flux. Since the flux has a certain viscosity, an indentation is formed on the top surface of the flux received in the flux receiving groove during the immersion of the semiconductor chip in the flux. If the indentation remains when the bottom surface of the next semiconductor chip is immersed in the flux, the flux cannot be applied evenly and in a fixed amount to the bottom surface of the semiconductor chip. Therefore, the flux tank 320 reciprocates over the immersion plate 310 at a predetermined interval to supply flux to the flux receiving groove and flatten the top surface of the flux received in the flux receiving groove.
[0144] After the bottom surface of the semiconductor chip is immersed in flux by the die picker, it is moved to the top of the Apple Picking Vision 400.
[0145] The Apple Picking Vision 400 performs an upward vision inspection to check for the presence or absence of cracks on the underside of the semiconductor chip picked up by the die picker 200. At this time, the Apple Picking Vision 400 can inspect the presence or absence of cracks on the semiconductor chip in a state where the flux is not applied, and can inspect the underside of the semiconductor chip in a state where the flux is applied.
[0146] Specifically, the Apple Picking Vision 400 can inspect the condition of the underside of a semiconductor chip immersed in flux while the surface of the semiconductor chip is adsorbed to the die picker 200, and can not only inspect the application state of flux to see whether it has been applied properly to the underside of the semiconductor chip, but also inspect the condition of the underside for contamination, foreign matter, chipping, cracks, bump defects, etc.
[0147] In addition, the Apple Picking Vision 400 of the present invention can inspect not only the bottom surface state of the semiconductor chip immersed in the flux, but also the presence or absence of cracks in the semiconductor chip. The inspection of the presence or absence of cracks in the semiconductor chip by the Apple Picking Vision 400 can be performed before the semiconductor chip sucked by the die picker 200 is immersed in flux.
[0148] At this time, the inspection for cracks can be selectively performed as necessary, and when the inspection for cracks is performed, the die picker receives the semiconductor chip from the flip-over picker and checks whether the semiconductor chip has cracks using the Apple Picking Vision 400. After that, the bottom surface of the semiconductor chip that is determined to have no cracks is immersed in flux and moved to the Apple Picking Vision 400 again to inspect the bottom surface of the semiconductor chip coated with flux.
[0149] The die picker 200 inspects the underside of the semiconductor chip with the approching vision 400, and then moves to the upper part of the die block 500. The die block 500 is fixedly disposed below the moving path of the die picker 200 and the bonding head 700, and is provided with an escape groove 510 to support the semiconductor chip and to allow the flux applied to the underside of the semiconductor chip to escape.
[0150] The escape groove 510 of the die block 500 has an open upper portion and an inclined surface that is inclined inward, so that the semiconductor chip is supported on the inclined surface and the bottom surface of the escape groove can be spaced apart from the bottom surface of the escape groove.
[0151] 7 and 8, the die block 500 of the present invention includes an escape groove 510 for supporting the semiconductor chip and allowing the flux applied to the lower surface of the semiconductor chip to escape, the escape groove 510 has an open upper portion and an inclined surface inclined inward, the semiconductor chip is supported on the inclined surface, and the lower surface of the semiconductor chip is separated from the bottom surface of the escape groove 510. In this case, the side of the semiconductor chip may be supported by the inclined surface so that the lower surface of the semiconductor chip is separated from the bottom surface of the escape groove, or an edge of the lower surface of the semiconductor chip may be supported by a protruding end formed at the lower portion of the inclined surface so that the lower surface of the semiconductor chip is separated from the bottom surface of the escape groove.
[0152] In the present invention, the die block 500 can be provided rotatably, and the semiconductor chip 20 to which the flux 50 is applied can be provided by the die picker 200. The die block 500 can include an escape groove 510 for allowing the flux 50 on the underside of the semiconductor chip 20 to escape.
[0153] For reference, bumps are formed on the underside of the semiconductor chip, and the edge (frame) of the underside is a region where no bumps are formed. When the underside of the semiconductor chip is immersed in flux, the flux is applied to the bump-formed surface 20b of the underside of the semiconductor chip, and the edge is not applied with flux.
[0154] Since flux 50 is applied to the bump forming surface 20b of the semiconductor chip 20, the distance between the bump forming surface 20b and the bottom surface of the escape groove 510 prevents the flux 50 applied to the underside of the semiconductor chip from sticking to the escape groove 510.
[0155] In the present invention, even when the semiconductor chip 20 is transferred to the escape groove of the die block 500, the side and bottom surfaces of the semiconductor chip are supported by the inclined surface, so that the bottom surface of the semiconductor chip can be separated from the bottom surface of the escape groove. The flux 50 applied to the semiconductor chip 20 can be retained at a constant amount, and the bottom surface of the escape groove can be prevented from being contaminated by the flux.
[0156] If the bump forming surface 20b of the semiconductor chip 20 is placed in contact with the bottom surface of the escape groove 510, the flux 50 may be attached to the bottom surface of the escape groove 510 when the semiconductor chip 20 is temporarily placed on the die block 500, resulting in a loss of some of the flux 50. This may cause a problem that the amount of the flux 50 applied to the bump forming surface 20b is insufficient, which may deteriorate the electrical connection of the semiconductor chip 20 and cause the semiconductor chip 20 to easily peel off from the substrate 40. In addition, the die block 500 may be easily contaminated by the flux 50 attached to the bottom surface of the die block 500, which may affect the bonding quality of the semiconductor chip 20 to be transferred subsequently.
[0157] In the thermocompression bonding apparatus 10 according to an embodiment of the present invention, when a semiconductor chip 20 is transferred onto a die block 500, in order to prevent a problem in which flux from the underside of the semiconductor chip adheres to the die block and causes a shortage of flux 50 applied to the bump forming surface 20b of the semiconductor chip, the die block of the present invention is provided with an escape groove 510 for allowing the flux applied to the underside of the semiconductor chip to escape.
[0158] The escape groove 510 of the die block 500 may be formed integrally with the die block 500 by machining a groove in the die block 500, or the escape groove 510 may be formed by a plurality of protruding blocks 520. Each of the plurality of protruding blocks 520 may be formed so that at least a portion thereof is inclined inward. The inner side of each of the protruding blocks 520 may be inclined from the upper end of the protruding block 520 to at least a portion of the height.
[0159] In addition, the protruding blocks 520 may be formed to the smallest size possible without distorting the position of the semiconductor chip 20, and only the edges of the semiconductor chip 20 may be supported by the protruding blocks 520, thereby preventing the flux 50 applied to the underside of the semiconductor chip 20 from adhering to the protruding blocks 520. The adjacent protruding blocks 520 are spaced apart from each other, thereby keeping the apex of the semiconductor chip 20 out of contact with the protruding blocks 520. Therefore, it is possible to minimize the impact on the semiconductor chip when the semiconductor chip is transferred to the escape groove formed by the protruding blocks.
[0160] In addition, even if there is an error in the edge of the semiconductor material due to a processing error that may occur during the process of cutting the semiconductor chip, there is no contact at the apex, and the semiconductor chip can slide down smoothly along the inclined surface.
[0161] Of course, it may be configured as one protruding block having an escape groove formed inside the protruding block. The upper surface of the protruding block 520 may form a surface with which a part of the bonding head 700 described later comes into contact.
[0162] Furthermore, when forming an escape groove in one protruding block, a groove may be machined in the corner of the protruding block 520 so that the apex of the semiconductor chip does not come into contact with the corner.
[0163] In addition, the protruding blocks 520 may move backward from the center of the die block 500 in an outward direction to increase the distance between the opposing protruding blocks, and may move forward toward the center of the die block 500 to decrease the distance between the opposing protruding blocks 520. The multiple protruding blocks 520 may further include a driving unit such as a driving cylinder or a motor.
[0164] Therefore, it is possible to accommodate semiconductor chips of various sizes by accommodating semiconductor chips outside the range of sizes that can be accommodated via the inclined surface.
[0165] In an embodiment of the present invention, the escape groove 510 has an open upper portion and an inwardly inclined surface. In this case, the inclined surface may have a step 540 formed by a protruding end 550 extending horizontally downward.
[0166] The escape groove 510 may be formed with only an inclined surface 530 inclined inward, or may be formed with both the inclined surface 530 and a protruding end 550. When a protruding end is formed on the inclined surface, a step 540 formed by the inclined surface 530 and the protruding end 550 can support the edge of the lower surface of the semiconductor chip 20 to separate the semiconductor chip 20 from the bottom surface of the escape groove 510.
[0167] The die block 500 can provide a space that separates the lower surface of the semiconductor chip 20 to which the flux 50 is applied and the bumps 21 from the bottom surface via the escape groove 510. That is, the upper part of the escape groove is open, and the lower part is separated from the lower surface of the semiconductor chip, forming an area that allows the flux of the semiconductor chip to escape.
[0168] First, referring to Figures 7a and 7b, a die block according to one embodiment of the present invention will be described. The escape groove of the die block has an open upper portion and a sloped lower portion, so that the side of the semiconductor chip is supported by the sloped surface and the bottom surface of the escape groove is spaced apart.
[0169] At this time, the semiconductor chip 20 can be seated in a state in which the outer edge of the lower surface, i.e., the side surface of the semiconductor chip, is in contact with and supported by the inner inclined surface of the escape groove 510. As a result, the semiconductor chip 20 is transferred to the escape groove 510, and the bottom surface of the escape groove 510 can be separated from the lower surface (bump forming surface 20b) of the semiconductor chip 20 and the bumps 21.
[0170] Here, a cross-sectional shape can be formed in which the horizontal cross-sectional area decreases from the upper open area (opening) toward the bottom via the inwardly inclined inclined surface 530 of the escape groove 510 of the die block.
[0171] The escape groove 510 can be formed such that the horizontal cross-sectional area becomes continuously smaller from the opening toward the bottom surface due to the inclined surface 530 .
[0172] At this time, the inclined surface guides the semiconductor chip downward and induces the seating of the semiconductor chip, and the angle of the inclined surface can be appropriately changed as required.
[0173] For example, the inclined surface 530 may be formed to have a high angle (slope), thereby improving the guiding effect of the semiconductor chip 20 and achieving smooth seating.
[0174] However, if the angle of the inclined surface is too high, the semiconductor chip may move on the surface that it previously contacted before being guided and aligned horizontally, and the semiconductor chip may be seated in an inclined state. Therefore, by forming the inclined surface at an appropriate angle, the semiconductor chip can be seated in a fixed position in the seating groove while easily maintaining a horizontal state.
[0175] Therefore, as shown in FIGS. 8a and 8b, the die block 500 of the present invention may have an escape groove 510 having a protruding end 550 formed thereon so that the semiconductor chip can be seated in a fixed position in the seating groove in a horizontal state.
[0176] The escape groove 510 has a protruding end 550 extending horizontally below the inclined surface 530. The protruding end may have a stepped shape. Due to the inclined surface and the protruding end, the escape groove 510 may be formed such that the horizontal cross-sectional area is continuously reduced from the opening to the bottom surface by the inclined surface 530, but the horizontal cross-sectional area is maintained constant from the protruding end 550 to the bottom surface.
[0177] The semiconductor chip 20 is guided by the inclined surface and can move to the protruding end 550. The protruding end 550 allows the semiconductor chip to be seated at the same height in the horizontal direction, and when the semiconductor chip is transferred to the escape groove 510 by the die picker, the semiconductor chip 20 can be seated while maintaining a horizontal state so as not to be biased or tilted to one side.
[0178] In particular, the horizontal region of the protruding end 550 comes into surface contact with the edge of the lower surface of the semiconductor chip 20, so that the semiconductor chip 20 can be more stably seated while maintaining a horizontal state.
[0179] The semiconductor chip coated with the flux transferred to the die block 500 is picked up by the bonding head 700 .
[0180] The bonding head 700 attracts and adsorbs the semiconductor chip using air without contacting the top surface of the semiconductor chip transferred to the die block 500, thereby minimizing impact and damage to the semiconductor chip when the bonding head 700 picks up the semiconductor chip coated with flux from the die block 500.
[0181] The bonding head 700 of the present invention has a heating member installed therein, is movable horizontally on the xy plane, is movable up and down in the z-axis direction by an elevation drive unit, and is rotatable clockwise or counterclockwise on the xy plane.
[0182] The bond head 700 of the present invention will now be described in more detail with reference to FIG.
[0183] The bonding head 700 of the present invention includes a bonding tool 770 having a heating member 780 for heating the semiconductor chip and for thermocompression bonding the semiconductor chip, a shaft 790 provided on the upper part of the bonding tool 770 and mounted so as to be movable up and down, a load control unit 750 for supporting the shaft 790 and adjusting a predetermined load to the weight of the shaft 790, a pressing unit 730 provided on the upper part of the load control unit 750 and including a mover 732 fixed to the outer circumferential surface of the shaft 790 and a driver 731 for driving the mover 732 to be movable in the vertical direction to press the bonding tool 770 with a predetermined force, and a pressing unit 730 between the load control unit 750 and the pressing unit 730. a rotation motor 710 provided on the upper part of the pressing part 730 and rotating the shaft 790; and a low-friction coupling 720 connecting the rotation motor 710 and the shaft 790 and transmitting the rotational force of the rotation motor 710 to the shaft 790, the low-friction coupling 720 having an upper part connected to the rotation motor 710 and a lower part connected to the shaft 790, forming a space between the rotation motor 710 and the shaft 790, and the shaft 790 can be raised and lowered by the movable element 732 between the space.
[0184] Although not shown, the bonding head 700 of the present invention is attached to one side of a lifting drive unit and is arranged so as to be movable up and down by the lifting drive unit, and the lifting drive unit is attached to a moving unit via a separate mounting member and can move on the xy plane.
[0185] The lifting drive unit is configured to lower the joining tool 770 to a predetermined height to pick up a semiconductor chip, and then move in a raised state to a predetermined height after picking up the semiconductor chip, so that the lifting drive unit can be raised and lowered as needed in each working area (semiconductor chip pick-up, semiconductor chip inspection, semiconductor chip joining, etc.).
[0186] Moreover, the moving part is moved on the xy plane so that the bonding head 700 can be positioned at each working area.
[0187] The joining tool 770 of the present invention is configured to be able to adsorb and heat a semiconductor chip, and includes a heating member 780 for heating the semiconductor chip, an suction hole 700a for adsorbing the semiconductor chip, an air suction port 771 that communicates with the suction hole and sucks in air to adsorb the semiconductor chip, an air supply port 772 that supplies air to cool the heating member 780, and an air discharge port 773 that discharges the air supplied by the air supply port 772.
[0188] At this time, a through hole communicating with the suction hole 700a may be formed in the heating member 780. A plurality of through holes may be formed at positions corresponding to the suction holes, or the through hole may be formed in an area larger than the suction hole so that the suction hole and the through hole communicate with each other.
[0189] The heating member 780 of the bonding tool 770 may be heated to a preset temperature when the substrate and the semiconductor chip come into contact with each other, and after heating to the preset temperature for a preset time, air is supplied to the heating member 780 through an air supply port 772 to cool the molten bumps and bond the substrate and the semiconductor chip, and the air supplied at this time may be cooled air or room temperature air.
[0190] The air supplied through the air supply port 772 may be discharged through the air discharge port 773 .
[0191] A horizontal leveler 760 for aligning the surface of the substrate and the semiconductor chip parallel to each other may be provided on the upper portion of the bonding tool 770. The horizontal leveler 760 may adjust the horizontal state of the bonding tool 770 via a gyroscope so that the lower surface of the bonding tool 770 and the surface of the substrate or the semiconductor chip at the stacking position are parallel to each other.
[0192] Therefore, during bonding, a uniform force can be applied to the semiconductor chip in a horizontal state with the substrate without being biased to either side.
[0193] The shaft 790 is provided on the upper part of the joining tool 770, the joining tool 770 is attached to the lowest part of the shaft 790, and the low-friction coupling 720 is provided on the upper part of the shaft 790.
[0194] The load control unit 750 supports the shaft 790 with a configuration for controlling the load, and can add or subtract a predetermined load to the weight of the shaft 790. Specifically, the load can be increased by applying a force in the same direction as the weight of the joining head 700, or can be decreased by applying a force in the opposite direction to the weight of the joining head 700, i.e., in a direction that offsets the weight.
[0195] In this case, any configuration that applies force can be used to realize the force, but in the present invention, the force can be realized by fluid pressure, and the load can be increased or decreased by determining the amount of fluid (fluid pressure) and the direction in which the fluid is supplied.
[0196] When fluid is supplied in one direction (upward in the lifting direction (±z direction)) of the load control unit 750, the weight of the joining head 700 can be attenuated, and when fluid is supplied to the other side (downward in the lifting direction (±z direction)), a predetermined load can be applied to the weight of the joining head 700 by the amount of fluid supplied.
[0197] The load control unit 750 supports the shaft 790 in a non-contact manner in the vertical direction, thereby enabling the semiconductor chip to be bonded at an accurate position, and may minimize frictional force that may occur due to the non-contact support of the load control unit 750 when the shaft 790 ascends and descends. That is, the shaft 790 may penetrate the load control unit 750, and the inner peripheral surface of the load control unit 750 and the outer peripheral surface of the shaft 790 may be spaced apart from each other by a predetermined distance to form a gap. Here, the term "formed through" refers to the purpose of transmitting the ascending and descending motion and the rotational motion of the shaft 790 to the bonding tool 770, and the shaft 790 may directly penetrate the load control unit 750 and the bonding tool 770 may be attached to the tip of the shaft 790. Alternatively, a separate load control unit shaft may be provided inside the load control unit 750, and the shaft 790 may be connected to one side of the load control unit shaft and the bonding tool 770 may be connected to the other side to form a bonding head 700 having a shaft that can be separated individually. In this case, the gap may be formed between the inner peripheral surface of the load control unit 750 and the outer peripheral surface of the load control unit shaft.
[0198] A fluid can be supplied to the gap to support the shaft 790 without contact and to minimize frictional forces on the shaft 790 as it rises or falls.
[0199] The pressing unit 730 is provided on the upper part of the load control unit 750 and includes a movable element 732 fixed to the outer peripheral surface of the shaft 790, and a driver 731 that drives the movable element 732 to be movable in the vertical direction, thereby controlling the pressing force that presses the semiconductor chip with a predetermined force via the joining tool 770.
[0200] The pressing unit 730 may preferably be configured with a motor. The pressing unit 730 may be directly connected to the load control unit 750 via a shaft 790, and preferably, the shaft 790 may pass through the mover 732 of the pressing unit 730. In particular, when the rotational force of the rotation motor 710 is transmitted to the shaft 790 via the low-friction coupling 720, the mover 732 of the pressing unit 730 through which the shaft 790 is fixed rotates together with the shaft 790 to rotate the joining tool 770 provided under the shaft 790.
[0201] Further, the pressing section 730 can press the joining tool 770 with a predetermined joining force by driving the mover 732 so that the mover 732 can move up and down within the driver 731 in accordance with the control of the control section.
[0202] In addition, the force applied to the bonding tool 770 can be controlled by using the advancement and retreat of the mover 732, and a desired force can be obtained by driving the driver 731 to move the mover 732 in the vertical direction according to an input value input to the pressing unit 730. That is, the pressing unit 730 can apply different magnitudes of force to the bonding tool 770 according to the input value. At this time, the force applied by the pressing unit 730 may be a force provided to the semiconductor chip sucked to the bonding tool 770.
[0203] A control method for moving the mover 732 forward and backward will be described by taking the pressing unit 730 as an example, in which a motor is used. When a necessary current value is input to the control unit, a current is passed through a coil around the mover 732, and the mover 732 moves forward and backward in the vertical direction within the driver 731, and the coil current is monitored so that the input current flows through the coil so that the mover 732 can press the semiconductor chip with a desired force. Here, the input value for generating a desired force can be obtained by measuring the load value of the bonding head 700 while sequentially varying the input value of the pressing unit 730 in a state where the weight of the bonding head 700 is offset by the load control unit 750, and then converting the load value of the bonding head relative to the input value into data in advance. The input value can be determined through the data to set the force to be applied to the semiconductor chip.
[0204] The pressing unit 730 of the present invention can perform torque control to control the force applied to the joining tool 770, and can also perform position control to control the position of the mover 732 by controlling the amount of vertical movement of the mover 732.
[0205] In addition, the pressing unit 730 can perform torque control when the mover 732 moves up and down to apply a force to the bonding tool 770, and can perform position control when transmitting the rotational force of the rotation motor 710 to the bonding tool 770. For example, if the semiconductor chip sucked to the bonding head 700 is distorted in the θ direction on the xy plane, the rotation motor 710 must correct it, so the pressing unit 730 performs position control when correcting the semiconductor chip of the bonding head 700, and can perform torque control when the semiconductor chip after correction must be pressed with a desired force when bonding the semiconductor chip to the substrate.
[0206] In order to measure the position of the mover 732, a pressing portion height measuring portion 733 and a fixing portion for mounting the pressing portion height measuring portion 733 may be further provided.
[0207] The fixed part may have any configuration as long as it is capable of mounting the pressure part height measuring part 733, and the fixed part may be disposed between the movable part 732 and the load control part 750, and an axis 790 may be provided so that the fixed part can rise and fall together with the movable part 732 when it is raised and lowered by the movable part 732.
[0208] 9, the fixing portion may be composed of a frame 734 formed eccentrically from the center of the shaft 790 and a locking jaw 735 coupled to the upper surface of the frame 734. In this case, the frame 734 and the locking jaw 735 may be formed in a combined form or may be formed as a single unit.
[0209] At this time, the lower end of the pressing portion height measuring portion 733 may be inserted and fixed between the frame 734 and the locking jaw 735, and the upper end of the pressing portion height measuring portion 733 may be inserted and fixed between the frame 734 and the locking jaw 735. Due to the structure in which the pressing portion height measuring portion 733 is attached to a fixing portion penetrating the shaft 790 and inserted and mounted between the frame 734 and the locking jaw 735, it can be stably fixed to the shaft 790 and move integrally with the shaft 790, and the position of the mover 732 can be measured more precisely.
[0210] In this case, a scale or graduations can be further provided to enable confirmation of the height of the pressing portion height measuring portion.
[0211] The pressing part height measuring part 733 can measure the position of the mover 732 to determine the position of the mover 732 which moves back and forth within the driver 731, and can calculate from the position of the mover 732 the relative position of the driver 731 and the joining tool 770 which is directly connected to the shaft 790 fixed to the mover 732.
[0212] A first load measuring unit 740 is provided between the load control unit 750 and the pressing unit 730. The first load measuring unit 740 can measure the load applied to the semiconductor chip in real time. This makes it possible to verify whether a preset load is applied to the semiconductor chip when bonding the semiconductor chip.
[0213] For reference, the bonding head 700 of the present invention can apply a predetermined force by the pressing unit 730 in a state where the load control unit 750 offsets the weight of the shaft 790. When the semiconductor chip is bonded to the substrate, the pressing unit 730 presses the semiconductor chip with a preset load, and the reaction force applied during bonding is measured in real time by the first load measuring unit 740, so that the bonding pressure, i.e., the load of the bonding head 700, can be monitored.
[0214] For reference, the present invention may set a load measuring unit of the bonding head 700 so that the load applied from the bonding head 700 to the semiconductor chip is the same as the bonding pressure for bonding the semiconductor chip.
[0215] For this purpose, a second load measuring unit that comes into contact with the bonding head 700 to measure the load of the bonding head 700 can be provided on one side of the heating table 910, and the first load measuring unit 740 is set so that the measurement value when the bonding head 700 is brought into contact with the second load measuring unit is equal to the measurement value of the first load measuring unit 740.
[0216] For reference, when the bonding head 700 and the second load measuring unit contact each other, the load control unit 750 of the bonding head 700 cancels the weight applied to the shaft 790, and when the pressing unit 730 of the bonding head 700 does not apply force, there is no value measured by the second load measuring unit. However, when the bonding head 700 comes into contact with the second load measuring unit of the heating table 910 and stops descending, the load of the bonding head 700 measured by the second load measuring unit in the absence of external force and the load measured by the first load measuring unit 740 due to the reaction force caused by the contact should be the same as the load of the second load measuring unit. Therefore, it is preferable to set the measurement value of the first load measuring unit 740 and the measurement value of the second load measuring unit to be the same so that the same measurement value can be obtained, and at this time, the set value is based on the measurement value of the second load measuring unit installed on the heating table 910. Of course, at this time, the second load measuring unit may be one that has been verified using a setting weight.
[0217] The measurement value of the first load measuring unit 740 is set by an operator in the process of setting up the equipment before bonding. The second load measuring unit verifies whether the bonding head presses the semiconductor chip with a preset force. By setting the first load measuring unit to reflect the error value of the second load measuring unit in the first load measuring unit 740, the bonding pressure (load) when bonding the semiconductor chip can be accurately monitored in real time.
[0218] In particular, in the case of the thermocompression bonding apparatus 10, the semiconductor chip and the substrate are heated and pressurized, so that the bumps melt at a preset temperature. Since the bonding tool 770 crushes the bumps and descends due to the pressing force of the bonding head 700 that presses the semiconductor chip when the bumps melt, thereby inducing a short circuit, various controls and settings can be performed, such as controlling the height or position of the bonding head or bonding tool 770 based on the melting start point of the bumps by sensing the load applied to the semiconductor chip in real time, or changing the bonding force applied by the pressing unit 730.
[0219] The rotation motor 710 is provided on the upper part of the pressing part 730 and rotates the shaft 790. When the shaft 790 rotates, the mover 732 of the pressing part 730 connected to the shaft 790 and the joining tool 770 provided on the lower part of the shaft 790 rotate together. When there is an angle deviation of the joining head 700 according to the inspection result of the slit vision 800 shown in FIG. 1, the rotation motor 710 can rotate the joining head 700 for correction.
[0220] That is, the Slit Vision 800 simultaneously photographs the semiconductor chip picked up by the bonding head 700 and the top surface of the substrate to which the semiconductor chip is to be bonded, thereby inspecting the alignment of the semiconductor chip and the substrate, and according to the inspection results, the bonding head 700 is moved in the x-axis and y-axis directions by the moving unit to correct the amount of twist of the semiconductor chip in the x- and y-axis directions so that the semiconductor chip picked up by the bonding head 700 can be bonded to the bonding position on the substrate, and the rotation motor 710 rotates the bonding head 700 about an angle θ to correct the amount of twist in the θ direction.
[0221] At this time, it is preferable that the motor of the pressing part 730 performs position control to fix the position of the mover so that the rotational force of the rotation motor 710 is quickly transmitted to the joining head 700 without loss.
[0222] The low-friction coupling 720 of the present invention is configured to connect the rotary motor 710 and the shaft 790, and can transmit the rotational force of the rotary motor 710 to the shaft 790. In this case, the low-friction coupling 720 is connected at an upper portion to the rotary motor 710 and at a lower portion to the shaft 790, forming a space between the rotary motor 710 and the shaft 790.
[0223] The shaft 790 can be raised and lowered between the separated spaces, and the low-friction coupling 720 can be configured to be extendable and contractible so that the lower part can move up and down while the upper part is fixed when the shaft 790 is raised and lowered within the separated space.
[0224] The low friction coupling 720 of the present invention may be made of a metal material to minimize friction, and may also use a bellows configured to be expandable and contractible, but is not limited thereto.
[0225] In the bonding head 700 according to an embodiment of the present invention, when moving or rotating to each working area, the motor of the pressing unit 730 can be in a position controlled state, and when pressing the semiconductor chip against the substrate with a predetermined force above the bonding position of the substrate, the motor can be in a torque controlled state.
[0226] In particular, the pressing unit 730 can cause the driver 731 to move the movable element 732 in an up and down direction so as to press the semiconductor chip with a predetermined joining force via the joining tool 770, and when the driver 731 moves the movable element 732 downward on the z-axis, the force applied to the joining tool 770 increases, and when the driver 731 moves the movable element 732 upward on the z-axis, the force applied to the joining tool decreases.
[0227] Therefore, the pressing unit 730 can apply a preset bonding force, and if the preset bonding force is greater than the capacity of the pressing unit 730, the load control unit 750 can supply fluid pressure downward in an amount sufficient to realize a force equal to the insufficient load, thereby adding a predetermined load to the weight of the shaft 790, or control the load control unit 750 so that the weight of the shaft 790 can be utilized without offsetting it, thereby applying the preset bonding force to the semiconductor chip.
[0228] In addition, in order to minimize the bonding force applied to the bonding tool 770, the pressing unit 730 is set to apply no bonding force or only a minimum bonding force, and the load control unit 750 supplies fluid pressure from above to offset the weight of the shaft 790 and reduce the load of the bonding tool 770, thereby applying a minimum bonding force to the semiconductor chip.
[0229] As a result, the present invention may realize a low-pressure bonding force by offsetting the weight of the shaft 790, or may realize a high-pressure bonding force greater than the capacity of the pressing section 730 by applying a predetermined load to the shaft 790 via the load control section 750 without being restricted by the capacity of the pressing section 730.
[0230] At this time, as the shaft 790 rises or falls, the load control unit 750 supports the shaft 790 in a non-contact manner in the vertical direction, and by supplying fluid to the gap between the inner surface of the load control unit 750 and the outer surface of the shaft 790, the frictional force acting on the shaft 790 can be minimized, and the semiconductor chip can be bonded in an accurate position while achieving low force by offsetting the resistance caused by friction.
[0231] In particular, when bonding thin or fragile semiconductor chips, if a large load is applied to the semiconductor chip, the damage to the semiconductor chip becomes large, and the semiconductor chip may crack or become broken. However, according to the present invention, the weight of the bonding head 700 can be offset, which has the advantage of enabling low-pressure bonding.
[0232] In addition, when setting the bonding force, it is possible to determine which mode the previously set bonding force belongs to and set the bonding force to one of low mode, middle mode, and high mode. In each mode, the load control unit 750 supplies the same amount of fluid pressure to achieve a predetermined load, and then further change the input value of the pressing unit 730 by the required amount to set the corresponding bonding force.
[0233] For example, a predetermined load is reached by supplying a preset amount of fluid pressure to each bonding force by the load control unit 750, and the bonding force that is insufficient at the predetermined load is adjusted by the pressing unit 730 to achieve the desired bonding force. The load control unit 750 realizes a corresponding mode based on fluid pressure for realizing a low mode load, a middle mode load, or a high mode load for each mode, and can more precisely and quickly control the force provided to the semiconductor chip according to an input value of the pressing unit 730.
[0234] Therefore, the load can be offset without increasing the capacity of the pressing unit 730, and a load larger than the capacity of the pressing unit 730 can be realized by using the load control unit 750 capable of applying an additional load. Therefore, a pressing unit 730 with a small capacity can be used, and by reducing the weight of the joining head 700, the joining head 700 can be moved at high speed, and the UPH of the device is not lowered.
[0235] In addition, both low pressure bonding and high pressure bonding can be achieved without the need to replace components or parts of the bonding head 700, and the pressing force can be finely controlled by the pressing unit 730 with the mode of the load control unit 750 selected, thereby enabling high-speed and precise load control. For reference, with the load control unit 750 supplying a fluid pressure corresponding to the corresponding mode to fix the load, the pressing unit 730 can quickly and precisely add and control a desired force, and a motor can be used in the pressing unit 730, enabling fast force setting.
[0236] In addition, in the bonding head 700 of the present invention, the rotation motor 710, the low-friction coupling 720, the shaft 790, the pressing unit 730, and the load control unit 750 are directly connected to each other, so that the position of the shaft 790 can be controlled by the pressing unit 730, and the bonding tool can be elevated separately from the elevation drive unit of the bonding head 700. In particular, the rotation motor 710 is connected in series to the shaft 790 via the low-friction coupling 720, so that the shaft 790 can rotate without loss of rotational force, which has the effect of enabling precise position correction of the semiconductor chip, and the rotation motor 710 and the pressing unit 730 can be quickly driven in response to control commands.
[0237] In addition, the joining head 700 of the present invention has an advantage that each component minimizes resistance due to frictional force, thereby realizing low force when driving the shaft 790 up and down. In particular, the low-friction coupling 720 is configured to transmit the rotational force of the rotation motor 710 to the shaft 790 while allowing the shaft 790 to move up and down, and the shaft 790 moves up and down in a space separated by the low-friction coupling 720, thereby minimizing frictional force.
[0238] Here, the low-friction coupling 720 may be configured to be expandable in order to transmit a rotational force and guide the lifting and lowering movement, and in this case, if the shaft 790 is supported only by the low-friction coupling 720, the position may be twisted, and the position of the shaft 790 may be supported in a non-contact manner using the load control unit 750, so that the semiconductor chip can be bonded to the exact position of the substrate, and the frictional resistance of the configuration supporting the shaft 790 during the lifting and lowering movement of the shaft 790 may be minimized to realize no load on the z-axis, and the force can be precisely controlled without considering the friction of the shaft 790 during low force control. Here, no load can be considered to be a case where there is no load, but in this specification, it also includes a case where there is a small frictional resistance that does not affect the force used during bonding.
[0239] In addition, the bonding head 700 of the present invention can measure in real time the load applied to the semiconductor chip between the load control unit 750 and the pressing unit 730, thereby not only verifying whether an appropriate pressing force is applied to the semiconductor chip during bonding, but also being useful for controlling the height of the bonding tool 770 and the bonding head so as to prevent the bumps from being crushed in the process of melting due to the pressing force, thereby improving the bonding quality.
[0240] On the other hand, the movement of the die picker of the present invention and the work performed by the die picker in each work area will be described with reference to Figs. 5a to 5d.
[0241] Fig. 5a is a diagram showing a state in which the die picker 200 according to the embodiment of the present invention is located at the second height L2 and receives a semiconductor chip from the flip-over picker 100. Fig. 5b is a diagram showing a state in which the die picker 200 according to the embodiment of the present invention is located at the second height L2 and immerses a semiconductor chip. Fig. 5c is a diagram showing a state in which the die picker 200 according to the embodiment of the present invention is located at the first height L1 and inspects the semiconductor chip by the apple picking vision 400. Fig. 5d is a diagram showing a state in which the die picker 200 according to the embodiment of the present invention is located at the second height L2 and delivers a semiconductor chip coated with flux to the die block 500.
[0242] The raised and lowered states of the die picker 200 described below may specifically mean the raised and lowered states of the picker body 210.
[0243] The die picker 200 (or the picker body 210) is located at a first height L1 in an elevated state, and can move from the first height L1 to each working area. The first height L1 can be an inspection height in the up-picking vision. The die picker 200 can be located at a second height L2 in a lowered state, and at this time, the second height L2 can be the working height of the die picker in the flip-over picker, the flux section, and the die block. The first height L1 can mean a position higher than the second height L2.
[0244] The die picker 200 can be moved to a die picker work area in an elevated state located at a first height L1 by a control unit (not shown). The die picker 200 can be lowered from the first height L1 to a second height L2 and can be elevated from the second height L2 to the first height L1 by the control unit. The die picker 200 can perform work in the flip-over picker, flux unit, and die block at the second height L2 by the control unit. The control unit can switch between the elevated state and the lowered state of the die picker 200.
[0245] 5a, a semiconductor chip pick-up process can be performed. The die picker 200 can move from a first height L1 in an elevated state to an upper region of the flip-over picker 100.
[0246] In order to pick up individual semiconductor chips from a wafer, the flip-over picker 100 descends toward the semiconductor chip, adsorbs the top surface of the semiconductor chip to be bonded, i.e., the bump-formed surface of the semiconductor chip, rises to a predetermined height, and then rotates 180 degrees to flip the top and bottom surfaces of the semiconductor chip.
[0247] With the semiconductor chips inverted by the flip-over picker, the die picker 200 may be lowered from the first height L1 to the second height L2 to switch to a lowered state. The die picker 200 may receive the semiconductor chips from the flip-over picker 100 at the second height L2, which is the lowered state. At this time, the die picker 200 may form a negative pressure while separated from the semiconductor chips to suck and adsorb the semiconductor chips. After that, the die picker 200 is elevated from the second height L2 to the first height L1 while picking up the semiconductor chips, and is then converted to an elevated state, and the die picker 200 moves to an upper portion of the flux section while maintaining the first height L1.
[0248] Referring to Fig. 5b, a process of immersing a semiconductor chip in the flux unit can be performed. The die picker 200 moves to an upper region of the flux unit 300 at a first height L1, which is an elevated state, and when it reaches the upper portion of the flux unit, it descends from the first height L1 to a second height L2, thereby switching to a descending state. The die picker 200 can immerse the lower surface of the semiconductor chip in the flux at the second height L2, which is the descending state. After immersing in the flux, the flux tank can move back and forth above the immersion plate to flatten the upper surface of the flux in the flux receiving groove in which the flux is received.
[0249] The die picker 200 can be raised from the second height L2 to the first height L1 and switched to an elevated state after picking up the semiconductor chip coated with flux. After that, the die picker moves to the upper part of the appropriation vision while maintaining the first height L1, and when the die picker 200 moves to the upper part of the appropriation vision, the flux tank moves back and forth above the immersion plate to flatten the upper surface of the flux accommodated in the flux accommodation groove.
[0250] 5c, the inspection process of the semiconductor chip can be performed in the Apple Picking Vision. The die picker 200 moves to the upper area of the Apple Picking Vision 400 at a first height L1 in an elevated state, and when it reaches the upper part of the Apple Picking Vision 400, it can inspect the underside of the semiconductor chip without a separate lifting and lowering operation.
[0251] The preset same height when the die picker 200 moves from the flip-over picker to the flux section, when it moves from the flux section to the apple picking vision, and when it moves from the apple picking vision to the die block is the same height as the height corresponding to the preset working distance (wd) of the apple picking vision when inspecting the semiconductor chip picked up by the die picker from the apple picking vision.
[0252] The working distance means the physical distance from the lens of the Apple Looking Vision to the semiconductor chip when inspecting the semiconductor chip with the Apple Looking Vision, and means the distance at which the Apple Looking Vision is focused so that the semiconductor chip can be inspected. In order to reduce the time required for height adjustment by the die picker, the moving height of the die picker can be set to a height that matches the focus of the Apple Looking Vision, thereby minimizing the lifting and lowering operation of the die picker during inspection by the Apple Looking Vision.
[0253] At this time, the appropriate working distance of the up-looking vision is a state that has been preset by the operator when setting up the joining device before driving the joining device.
[0254] In other words, by moving the die picker to the inspection height of the semiconductor chip by Apple Picking Vision, no additional lifting or lowering is required for inspection by Apple Picking Vision, and the underside of the semiconductor chip picked up by the die picker can be inspected by Apple Picking Vision as the die picker moves to the top of Apple Picking Vision, thereby shortening the inspection time for inspecting the underside of the semiconductor chip by Apple Picking Vision.
[0255] In this case, the Apple Picking Vision may inspect the underside condition of the semiconductor chip while the die picker is stopped above the Apple Picking Vision, or may inspect the underside condition of the semiconductor chip in a flying type manner while the die picker moves from the Apple Picking Vision to the die block.
[0256] At this time, the Apple Picking Vision can inspect the condition of the underside of the semiconductor chip to which flux has been applied while the top surface of the semiconductor chip is adsorbed to the die picker, and can not only inspect the application condition of flux to see whether it has been applied properly to the underside of the semiconductor chip, but also inspect the condition of the underside for contamination, foreign matter, chipping, cracks, bump defects, etc.
[0257] In addition, Apple Picking Vision can inspect not only the condition of the bottom surface of the semiconductor chip immersed in the flux, but also the presence or absence of cracks in the semiconductor chip. The inspection of the presence or absence of cracks in the semiconductor chip using Apple Picking Vision can be performed before the semiconductor chip adsorbed on the die picker is immersed in flux.
[0258] At this time, the inspection for the presence or absence of cracks can be selectively performed as necessary. When the inspection for the presence or absence of cracks is performed, after the die picker transfers the semiconductor chip from the flip-over picker, the die picker checks for the presence or absence of cracks in the semiconductor chip using the apple picking vision, and if it is determined that there is no crack, the underside of the semiconductor chip that has been immersed in flux can be inspected again using the apple picking vision.
[0259] In addition, Apple Picking Vision can also inspect the pick-up state of the semiconductor chip picked up by the die picker. If the inspection result shows that the positional alignment between the escape groove of the die block and the semiconductor chip is distorted, the die picker or the die block can be rotated by the angle of the twist of the semiconductor chip to align them, and then the semiconductor chip can be seated in the escape groove of the die block.
[0260] Of course, the die picker may inspect the underside of the semiconductor chip at the second height L2, which is the lowered state of the die picker in the apple picking vision 400, but from the viewpoint of minimizing the transportation path and lifting and lowering operation of the die picker, it is more preferable to move to a height corresponding to the working distance of the apple picking vision and immediately inspect the underside of the semiconductor chip for the presence or absence of cracks using the apple picking vision. After inspecting the semiconductor chip using the apple picking vision, a process is performed in which the flux-coated semiconductor chip picked up by the die picker is transferred to the die block.
[0261] 5d, a semiconductor chip placement process can be performed. The die picker 200 can move from a first height L1, which is an elevated state, to an upper region of the die block 500, and then move down from the first height L1 to a second height L2 to switch to a lowered state. The die picker 200 can deliver the flux-coated semiconductor chip to the die block 500 at the second height L2, which is the lowered state.
[0262] The die block is fixedly positioned below the movement paths of the die picker and the bonding head, and has an escape groove through which the flux-coated semiconductor chips picked up by the die picker are transferred and through which the flux coated on the underside of the semiconductor chips can escape.
[0263] The semiconductor chip may be seated inside the escape groove in a state in which the lower surface and the bumps of the semiconductor chip are supported and spaced apart from the bottom surface via the escape groove.
[0264] Thereafter, the die picker 200 rises from the second height L2 to the first height L1 and switches to an elevated state, returning to the flip-over picker side to pick up a new semiconductor chip, and the semiconductor chip transferred to the die block is picked up by the bonding head and moved to the top of the substrate to be bonded.
[0265] As described above, the die picker can move to the same preset height when moving to the top of each of the working areas of the flip-over picker, the flux unit, the app-picking vision, and the die block. At this time, the same preset height to which the die picker moves is set to a height (first height) corresponding to the working distance of the app-picking vision when inspecting the bottom surface of a semiconductor chip with the app-picking vision, and since each of the working areas of the flip-over picker, the flux unit, and the die block has the same height (second height), the die picker descends by the same height in the working area, minimizing the Z-axis movement amount of the die picker, thereby improving the accuracy of the die picker.
[0266] If the height at which the die picker 200 works differs for each work area, height errors in control may occur, reducing the accuracy of the die picker and resulting in poor quality semiconductor chips, and the amount of movement of the die picker 200 in the lifting and lowering direction may increase, causing a delay in the bonding time UPH.
[0267] The control unit performs two-mode height control that divides the die picker 200 into an ascending state and a descending state, thereby minimizing the amount of movement of the die picker 200 in the ascending and descending direction and the height error, thereby improving accuracy and UPH.
[0268] The bonding head 700 of the present invention creates negative pressure while being spaced apart from the semiconductor chip transferred to the escape groove of the die block 500, and sucks and adheres the semiconductor chip.
[0269] At this time, among the semiconductor chips picked up by the bonding head 700, normal semiconductor chips are bonded to the substrate according to the inspection results of the appleooking vision 400, and defective semiconductor chips 22 must be removed so as not to be bonded to the substrate.
[0270] For this reason, there is provided a reject picker 600 which picks up and removes from the bonding head 700 defective semiconductor chips 22 which have been determined to be defective as a result of the inspection by the appleooking vision 400, and a collection section 650 which discards the defective semiconductor chips 22 picked up by the reject picker 600.
[0271] The reject picker 600 is disposed below the transport path of the bonding head 700 , and is capable of receiving the defective semiconductor chips 22 from the bonding head 700 and dropping the defective semiconductor chips 22 into the collection section 650 .
[0272] 10 and 11, the reject picker 600 may include a suction unit 610 having a duct for sucking or discharging air and suctioning the defective semiconductor chip 22, and a rotating member 620 for rotating the suction unit 610 180 degrees to invert the top and bottom surfaces of the defective semiconductor chip 22 adsorbed to the suction unit 610.
[0273] The reject picker 600 may further include an air supply device connected to the duct of the suction unit 610 to supply air, and a switching member for switching between intake and exhaust of air on the duct.
[0274] The suction unit 610 can suck air while facing upward and in contact with the lower surface of the defective semiconductor chip 22 sucked by the bonding head 700 to suck the defective semiconductor chip 22 from the bonding head 700 .
[0275] At this time, the suction unit 610 is in a state of suctioning the bump-formed surface of the defective semiconductor chip 22, and the bump-formed surface is in a state of being coated with flux.
[0276] After the suction unit 610 has sucked the defective semiconductor chip 22, the suction unit 610 can rotate the defective semiconductor chip 22 by the rotating member 620 so that the molding surface of the defective semiconductor chip faces downward and the defective semiconductor chip 22 can be dropped into the collecting section 650.
[0277] As described above, the control unit can generate the inspection result of the Apple Taking Vision 400 and can determine the quality of the underside of the semiconductor chip according to the inspection result. If the control unit determines that the semiconductor chip is defective based on the inspection result of the Apple Taking Vision 400, the control unit can discard the defective semiconductor chip 22 to the collection unit 650 via the reject picker 600.
[0278] The collecting part 650 is disposed below the suction unit 610 of the reject picker 600 and includes a collecting container 651 that is detachably installed and collects the defective semiconductor chips 22, a first sensor (not shown) for checking whether the collecting container 651 is attached or not, and a second sensor 652 for checking whether the number of the defective semiconductor chips 22 collected in the collecting container 651 exceeds a preset amount. Here, the first sensor may be a touch sensor, and the second sensor may be an optical sensor.
[0279] A part or the whole of the collection container 651 is made of a transparent material, so that it is easy to visually check how full the collection container 651 is with the defective semiconductor chips 22. Of course, it may be made of an opaque material, and a second sensor 652 for detecting the amount of defective semiconductor chips 22 filled in the collection section may be attached. Whether or not the defective semiconductor chips 22 exceed a preset amount is detected through the second sensor 652, and if the preset amount is exceeded, the collection container 651 can be detached from the collection section, the inside of the collection container 651 can be emptied, and the collection container 651 can be reinstalled in an empty state.
[0280] In order to prevent the defective semiconductor chips 22 from being discarded when the collection container 651 is not attached, the collection unit 650 may be provided with a first sensor (not shown) for checking whether the collection container 651 is attached or not.
[0281] Meanwhile, when the reject picker 600 removes the defective semiconductor chip 22 from the bonding head based on the inspection result of the approving vision 400, the suction unit 610 suctions the bump formation surface of the defective semiconductor chip 22 to which the flux is applied.
[0282] When the suction unit 610 receives the defective semiconductor chip 22 from the bonding head 700, the suction unit 610 sucks the bump-forming surface of the defective semiconductor chip by sucking it with air while in direct contact with or spaced apart from the defective semiconductor chip, and then, after rotating the suction unit 610 180 degrees using the rotating member 620, the suction of the suction unit 610 is released, allowing the defective semiconductor chip 22 to fall toward the collection section.
[0283] The suction unit 610 can suck the defective semiconductor chip 22 by air pressure when facing upward, and can drop the defective semiconductor chip 22 into the collector 650 when facing downward.
[0284] The suction unit 610 may be located above the collector 650, and the rotating member 620 may rotate the suction unit 610 to invert the top and bottom surfaces of the defective semiconductor chip 22 sucked by the suction unit. The rotating member 620 is rotatably connected to the suction unit 610 and may rotate the suction unit 610 by 180° around the x-axis or y-axis as a rotation axis.
[0285] When the suction unit 610 is turned upside down by the rotating member 620, the air suction of the suction unit 610 is released, and the defective semiconductor chip 22 can be dropped into the collection container 651. However, since the bump-formed surface of the defective semiconductor chip 22 may have adhesive force due to the flux 50, the semiconductor chip may not be easily separated from the suction unit 610.
[0286] Therefore, the suction unit 610 can discharge air onto the defective semiconductor chip 22 that has been turned upside down by the rotating member 620, allowing the defective semiconductor chip 22 to drop more easily onto the removal section side.
[0287] Since air must be sucked in when the suction unit 610 picks up the defective semiconductor chip 22 from the bonding head 700, and air must be exhausted when the defective semiconductor chip 22 is dropped from the suction unit 610 to the collecting section side, the present invention may further include an air supply device and a switching member. The air supply device and the switching member may be an ejector, and suction air may be formed via the ejector, or exhaust air may be formed.
[0288] For reference, the suction unit 610 of the reject picker 600 may have any configuration as long as it is capable of both sucking and discharging air. As an example, the reject picker 600 may include a suction unit 610 having a pipe for sucking or discharging air and suctioning the defective semiconductor chips 22, a suction pipe having one end connected to the pipe and the other end connected to a vacuum generator, a discharge pipe having one end connected to the pipe and the other end connected to a compressed air generator, and a switching member for switching on / off the suction pipe and the discharge pipe.
[0289] As another example, the reject picker 600 may include a suction unit 610 having a pipeline for sucking or discharging air and for suctioning defective semiconductor chips 22, a vacuum generator connected to the pipeline to generate negative pressure, a discharge pipeline having one end connected to the pipeline and the other end connected to a compressed air generator, and an opening / closing member installed in the pipeline or the discharge pipeline to turn the pipeline on and off.
[0290] Meanwhile, the reject picker 600 can separate the defective semiconductor chip 22 in a state where the inverted defective semiconductor chip is located lower than the upper end of the collection unit 650. This can prevent the defective semiconductor chip 22 from being discarded in a place other than the collection unit 650.
[0291] First, in the embodiment, an example has been described in which the reject picker 600 receives the defective semiconductor chip 22 adsorbed to the bonding head 700 and drops it into the collection section, but if the reject picker 600 is positioned below the transport path of the die picker 200, the defective semiconductor chip 22 may be provided directly from the die picker 200.
[0292] Of course, at this time, the method of directly sucking and removing the defective semiconductor chip 22 and the method of spraying air onto the defective semiconductor chip while it is turned upside down so that the defective semiconductor chip 22 falls reliably into the removal section can be applied in the same way.
[0293] According to the inspection result of the up-cutting vision 400, the normal semiconductor chip is moved by the bonding head 700 of the present invention to above the heating table 910 on which the substrate is placed.
[0294] 13 to 16, the heating table 910 of the present invention is a table for applying heat to the substrate 40 so that the semiconductor chip is thermocompression bonded to the substrate 40, and includes a chuck plate 911 on which the substrate to be bonded is placed, a base 913 provided under the chuck plate 911 and connected to a vacuum generator for forming a negative pressure on the chuck plate 911, and a heating plate 912 provided between the chuck plate 911 and the base 913 for transferring heat to the chuck plate 911, and the chuck plate 911 includes a suction region 911a for suctioning the substrate, and a thermal diffusion region 911b provided on the outer periphery of the suction region 911a for diffusing heat transferred from the heating plate 912 or the bonding head 700. Here, the substrate may be a wafer.
[0295] First, a substrate to be bonded is placed on the chuck plate 911, preferably on the upper part of the suction area 911a of the chuck plate 911. For this purpose, suction holes 911d for suctioning the substrate are formed on the upper surface of the suction area 911a, and a plurality of suction holes 911d are provided so as to stably suction the substrate. The suction holes 911d of the chuck plate 911 may be formed at a position corresponding to the area of the substrate, or may be located in an area slightly smaller than the size of the substrate to prevent air leakage during the process of suctioning the substrate.
[0296] A fourth air pressure passage 911e for adsorbing a substrate is formed on the lower surface of the suction region 911a of the chuck plate 911, and a fifth air pressure passage 911f for adsorbing the chuck plate 911 to a heating plate 912 (described later) is formed. At this time, the fourth air pressure passage 911e is provided so as to communicate with the suction hole 911d.
[0297] One or more reference objects f may be formed on the upper surface of the thermal diffusion region 911b of the chuck plate 911. The reference objects f may be marks or holes having a shape that makes it easy to detect the center as a reference point for inspecting the state in which the substrate is seated on the chuck plate 911.
[0298] The reference object f is located within the thermal diffusion region 911b, but can be located outside and adjacent to the adsorption region 911a, and may be located anywhere so long as the substrate and the reference object f can be inspected simultaneously.
[0299] The reference object f of the present invention can be used to inspect the seating state of the substrate, and can also be used to separate the regions of the substrate transferred to the chuck plate 911.
[0300] At this time, the substrate is transferred to the upper surface of the suction area 911a of the chuck plate 911 by the transmission member. When the substrate is transferred by the transmission member, the lift member 950 provided on the outside of the heating table 910 rises to support the boundary area of the underside of the substrate, and the lift member 950 descends to transfer the substrate to the upper surface of the suction area 911a of the chuck plate 911.
[0301] When the lift member 950 seats the substrate on the chuck plate 911 by a transfer member (not shown), the lift member 950 is raised to support a boundary region of the lower surface of the substrate, and then lowers to seat the substrate on the chuck plate 911. When lowered, the lift member 950 can be inserted into an insertion groove 911c formed on the upper surface of the thermal diffusion region 911b.
[0302] Here, the transmission member is provided separately from the wafer supply unit and can supply either the wafer or the ring frame, and if the holding methods of the wafer and the ring frame are similar, one transmission member can be responsible for both the wafer supply and the ring frame supply.
[0303] Thereafter, after the bonding of each semiconductor chip to the bonding area of the substrate is completed, the substrate is removed from the chuck table, and a new substrate to be bonded is transferred. At this time, when the lift member 950 rises to remove the substrate from the chuck table, the substrate rises from the chuck plate 911, and the substrate that has been raised can be removed with the transfer member supporting its lower surface. The lift member 950 may also rise when correcting the position of the substrate transferred to the chuck plate 911.
[0304] The heating plate 912 of the present invention is provided below the chuck plate 911, but is provided above the base 913 and can apply heat to the chuck plate 911. The heating plate 912 is preferably formed of a material that has excellent thermal conductivity, is heat resistant, and does not expand easily. Since the heat applied by the heating plate 912 is transferred to the chuck plate 911 provided above the heating plate 912, the chuck plate 911 is preferably formed of the same material as the heating plate 912. Among them, it is more preferable that the heating plate 912 and the chuck plate 911 are formed of a ceramic material.
[0305] A plurality of through holes may be formed in the heating plate 912. In this case, the through holes include a first through hole 912a and a second through hole 912b. The first through hole 912a is a through hole that transmits a negative pressure for adsorbing and supporting the chuck plate 911, and communicates with a fifth air pressure passage 911f of the chuck plate 911 and a second air pressure passage 913b of the base 913. The second through hole 912b is a through hole that transmits a negative pressure for adsorbing the substrate, which is transmitted to the chuck plate 911, and communicates with a fourth air pressure passage 911e of the chuck plate 911 and a third air pressure passage 913c of the base 913. One or more of each of the first through hole 912a and the second through hole 912b may be formed.
[0306] In the heating plate 912 of the present invention, when no substrate is seated on it, negative pressure is applied from a vacuum generator to the first air pressure flow path 913a and the second air pressure flow path 913b of the base 913, so that the chuck plate 911 and the heating plate 912 are constantly held in a state of being adsorbed by the base 913. When a substrate is seated on the chuck plate 911, negative pressure is also applied from the vacuum generator to the third air pressure flow path 913c of the base 913 so that negative pressure is applied to the suction hole 911d of the chuck plate 911, and the substrate can be adsorbed via the second through hole 912b of the heating plate 912 and the suction hole 911d of the chuck plate 911.
[0307] The heating plate 912 of the present invention can be formed to be smaller than the size of the chuck plate 911 and larger than the size of the substrate to be bonded.
[0308] The base 913 is provided under the heating plate 912 and can be connected to a vacuum generator (not shown) for forming a negative pressure on the chuck plate 911. The base 913 can be formed with three types of air pressure passages, a first air pressure passage 913a for adsorbing the heating plate 912, and a second air pressure passage 913b for adsorbing the chuck plate 911. In addition, a third air pressure passage 913c for adsorbing the substrate, and a negative pressure can be formed independently through each air pressure passage.
[0309] A heating table 910 of the present invention has a heating plate 912 provided on an upper portion of a base 913, and a chuck plate 911 provided on an upper portion of the heating plate 912. In this case, the size of the chuck plate 911 provided on the uppermost end of the heating table 910 is formed to be larger than the base 913 and the heating plate 912, as shown in Fig. 16, and a part of a thermal diffusion region 911b provided on the outer periphery of an adsorption region 911a may protrude horizontally beyond the base 913 and the heating plate 912.
[0310] Also, the chuck plate 911 may be formed larger than the base 913 and the heating plate 912 and may be provided interchangeably depending on the size of the substrate. The base 913 and the heating plate 912 may be shared. Therefore, when the size of the substrate is variable, the area of the chucking region 911a may be changed according to the size of the substrate, and the area of the thermal diffusion region 911b may be changed depending on the size of the substrate.
[0311] That is, when the size of the substrate becomes smaller, the area of the adsorption region 911a also becomes smaller, and the area of the thermal diffusion region 911b may become even larger; when the size of the substrate becomes larger, the area of the adsorption region 911a also becomes larger, but the area of the thermal diffusion region 911b may become smaller.
[0312] However, the area of the thermal diffusion region 911b with respect to the size of the substrate may be at least about 10 to 30%. For example, if the substrate is a 300 mm wafer, the chucking region 911a may be formed to 300 mm corresponding to the substrate, and the remaining region may be formed as the thermal diffusion region 911b, and the size of the chuck plate 911 may be manufactured to 330 mm to 390 mm. However, if the size of the chuck plate 911 is too large, the volume occupied by the chuck plate 911 may become large, so the size may be preferably manufactured to about 15 to 25%. Therefore, if the substrate is a 300 mm wafer, the chucking region 911a may be formed to 300 mm corresponding to the substrate, and the remaining region may be formed as the thermal diffusion region 911b, and the size of the chuck plate 911 may be manufactured to 345 mm to 375 mm.
[0313] In this regard, in comparison with the conventional heating table 910 shown in FIGS. 12a and 12b, the conventional heating table 910 is formed such that the size of a chuck plate 911 on which a substrate is placed is smaller than or equal to the size of a heating plate 912 and a base.
[0314] At this time, the size of the chuck plate 911 is formed to correspond to the size of the substrate, so that the heating plate 912 and the base can also be formed to correspond to the size of the substrate or to be slightly larger.
[0315] For example, when a heating table as shown in Fig. 12 is used, when the high heat of the bonding head heats the semiconductor chip and bumps during the thermocompression bonding process, the heat of the bonding head is transferred to the heating table from the position where the semiconductor chip is bonded to the substrate, and the heat transferred to the heating table spreads in the radial direction. In particular, as shown in Fig. 12, the periphery of the heating table is insulated by air, so the temperature difference between the center of the heating table and the periphery of the heating table becomes large, which causes a problem of an increase in the defective rate of semiconductor chips on the substrate located above the periphery of the heating table.
[0316] That is, the heat distribution and amount of heat of the bonding head and heating table, which are involved in melting and hardening of the solder balls and flux of the semiconductor chip, are different between the center and the periphery of the heating table, which creates differences in the heat transfer characteristics and the phase change time of the solder balls and flux at the two points, making it impossible to bond with uniform quality and causing problems such as poor bonding of semiconductor chips. For example, on the board located on the upper part of the periphery of the heating table, the flux may be heated above the hardening start temperature before thermocompression bonding, resulting in differences in bonding quality.
[0317] For example, when bonding to a substrate, the bonding head 700 heats the semiconductor chip to a temperature of about 300° C. and presses it with a predetermined force to bond the chip to the substrate. The heating table 910 can heat the chuck plate 911 to a temperature of about 100° C. to compensate for the temperature of the semiconductor chip located on the side farther from the bonding head 700, i.e., the side closer to the chuck plate 911.
[0318] That is, when the semiconductor chip is bonded to the substrate by thermocompression bonding, the heat transferred from the heating plate 912 and the heat transferred from the bonding head 700 act on the chuck plate 911 together, generating a temperature difference between the heat at the top and the heat at the bottom, and the heat at the top, which is higher, moves to the lower, which is lower, resulting in a thermal equilibrium state. Therefore, the thermocompression bonding is accumulated on the chuck plate 911 side, and the heat from the bonding head 700 acts continuously, and the heat transferred to the chuck plate 911 can be diffused.
[0319] In particular, heat transferred from the bonding head 700 is transferred to the chuck plate 911 in all radial directions, but the heat is not radiated from the periphery of the chuck plate 911 and is insulated by contact with air, resulting in heat accumulation. Therefore, the temperature of the periphery of the conventional chuck plate 911 is about 10 to 15°C higher than that of the center region, and the temperature difference causes a problem of poor bonding in the bonding region of the substrate located at the periphery of the chuck plate 911.
[0320] In response to this, in order to minimize the temperature difference between the center and the outer periphery of the substrate during the thermocompression bonding process and suppress the difference in bonding quality depending on the position on the substrate, the heating table of the present invention is provided with a thermal diffusion area 911b outside the suction area 911a that suctions the substrate, as shown in FIG. 13.
[0321] Therefore, the heating table 910 of the present invention is such that the size of the chuck plate 911 is expanded so that the outer periphery of the substrate is located inside the chuck plate 911. That is, since the outer periphery of the chuck plate 911 may have a possibility of generating a heat pool due to heat insulation by air, the chuck plate 911 of the present invention is provided with a heat diffusion region 911b in which heat transferred from the bonding head 700 is diffused so that heat is transferred to all radial directions of the chuck plate 911 without generating a heat pool on the side where the outer periphery of the substrate is located.
[0322] The heat flowing out from the bonding head 700 due to the thermal diffusion region 911b is accumulated on the outer periphery side of the thermal diffusion region 911b of the chuck plate 911, so that the center and the outer periphery of the substrates to be bonded can ensure temperature uniformity during thermocompression bonding. Therefore, when the heating table 910 of the present invention is applied, a temperature difference of 1 to 2 degrees Celsius occurs between the center and the outer periphery of the substrate.
[0323] That is, by providing the thermal diffusion region 911b, it is possible to prevent the outer periphery of the substrate from being positioned at the outer periphery of the chuck plate 911, thereby improving the temperature difference between the center and the outer periphery of the substrate and ensuring temperature uniformity regardless of the position of the substrate. Therefore, the bonding height of the substrate to which the semiconductor chip is bonded can be made uniform, ensuring bonding quality and reducing the defect rate.
[0324] In the embodiment of the present invention shown in FIG. 16b, the chuck plate 911 is formed to extend and protrude horizontally from the heating plate 912 and the base, and a thermal diffusion region 911b is formed on the outer periphery of the suction region 911a, so that the heat transferred from the heating plate 912 or the bonding head 700 is diffused, and the heat is not accumulated in the outer periphery region of the substrate but is conducted and led to the outer periphery of the thermal diffusion region 911b.
[0325] Therefore, in an embodiment of the present invention, when the bonding head 700 bonds the semiconductor chip 20 to the central region of the substrate 40, heat can be transferred in all radial directions of the chuck plate 911 based on the semiconductor chip 20. When the bonding head 700 bonds the semiconductor chip 20 to the peripheral region of the substrate 40, heat can be transferred in all radial directions of the chuck plate 911 based on the semiconductor chip 20.
[0326] The chuck plate 911 extends to the edge of the heating plate 912 to form a heat spreading region, so that heat can be transferred in the direction of the edge of the chuck plate 911 relative to the semiconductor chip 20 .
[0327] The heat diffusion region prevents heat from accumulating in the region of the chuck plate 911 corresponding to the edge of the substrate 40, thereby preventing defects in the semiconductor chips 20 bonded to the peripheral region of the substrate 40.
[0328] Meanwhile, before the bonding head 700 bonds the semiconductor chip to the substrate, the Slit Vision 800 can simultaneously photograph the semiconductor chip picked up by the bonding head 700 and the top surface of the substrate to which the semiconductor chip will be bonded, thereby inspecting the alignment of the semiconductor chip.
[0329] For this purpose, the slit vision 800 is movably installed in the x-axis and y-axis directions above the substrate on which the semiconductor chip is to be bonded, and may include an up-looking lens that checks the position of the semiconductor chip picked up by the bonding head 700, and a down-looking lens that checks the bonding position of the substrate on which the semiconductor chip picked up by the bonding head 700 is to be bonded.
[0330] The slit vision 800 is composed of a two-eye optical system, with an up-looking lens and a down-looking lens arranged coaxially in the z-axis direction, so that it can simultaneously inspect the semiconductor chip picked up by the bonding head 700 and the bonding position of the substrate to which the semiconductor chip is bonded.
[0331] Therefore, the Slit Vision 800 can compare the position of the semiconductor chip picked up by the bonding head 700 photographed by the up-looking lens with the predetermined bonding position of the substrate photographed by the down-looking lens to simultaneously inspect the bonding position where the semiconductor chip and the semiconductor chip are bonded, thereby inspecting the alignment state of the substrate and the semiconductor chip.
[0332] According to the inspection results of the slit vision 800, the position error of the semiconductor chip picked up by the bonding head 700 can be corrected so that the bonding position and the position of the semiconductor chip coincide with each other, and the preset bonding position and the position of the bonding head 700 can be aligned coaxially.
[0333] In addition, the slit vision 800 may inspect both the reference object and the substrate installed on the heating table 910 to inspect the placement state of the substrate placed on the heating table 910. Depending on the result of the inspection of the placement state of the substrate by the slit vision 800, the position of the substrate may be corrected and realigned so that the substrate can be attracted to the attraction area 911a of the heating table 910.
[0334] At this time, the position of the substrate can be corrected by a transmission member (not shown), and the transmission member can pick up and re-seat the substrate so that the center of the substrate can be aligned with the center of the chuck plate 911 by inspecting both the substrate and the reference object formed in the thermal diffusion region 911b using slit vision.
[0335] Hereinafter, a bonding method using the thermocompression bonding apparatus 10 of the present invention will be described with reference to FIGS.
[0336] First, the flip-over picker 100 picks up the individualized semiconductor chips from the wafer and flips them upside down. At this time, the individualized semiconductor chips may be in a state where the semiconductor chips are spaced apart from each other, and the flip-over picker descends toward the semiconductor chips to adsorb the upper surfaces of the semiconductor chips to be bonded, i.e., the bump-formed surfaces of the semiconductor chips, and then rises to a predetermined height, and then rotates 180° in the ascending / descending direction to flip the upper and lower surfaces of the semiconductor chips. At this time, the die picker 200 can move in the length direction to the top of the flip-over picker 100.
[0337] With the top and bottom surfaces of the semiconductor chip inverted by the flip-over picker, the die picker moves to above the flip-over picker, and while spaced a predetermined distance from the top surface of the semiconductor chip, the semiconductor chip is sucked from the flip-over picker with air to pick up the semiconductor chip in a non-contact state.
[0338] The die picker 200 can move down toward the semiconductor chip sucked by the flip-over picker 100 and suck the semiconductor chip through the molding surface 20a. When the semiconductor chip is sucked by the die picker 200, the bump forming surface of the semiconductor chip faces downward based on the lifting direction, so that the bumps can be exposed to the outside.
[0339] If the semiconductor chip needs to be inspected for cracks, the die picker moves to the appleooking vision and inspects the semiconductor chip picked up by the die picker for cracks. If the semiconductor chip does not need to be inspected for cracks, the die picker moves to the top of the flux section and descends a certain height to immerse the underside of the semiconductor chip in flux. After the flux is immersed, the flux tank moves back and forth above the immersion plate to flatten the top surface of the flux in the flux receiving groove where the flux is received.
[0340] Meanwhile, after dipping the underside of the semiconductor chip in flux, the die picker moves to the top of the apple picking vision. The apple picking vision inspects the underside condition of the semiconductor chip picked up by the die picker. The die picker 200 then transfers the semiconductor chip to the die block 500, and the bonding head 700 picks up the flux-coated semiconductor chip on the die block 500 and bonds it to the substrate 40 by thermocompression bonding.
[0341] If the control unit determines that the semiconductor chip is defective based on the inspection result of the approving vision 400, the die picker 200 transfers the defective semiconductor chip to the die block 500, and the bonding head 700 picks up the defective semiconductor chip on the die block 500 and provides it to the reject picker 600. The reject picker 600 may pick up the defective semiconductor chip from the bonding head 700 and drop it into the collection unit 650.
[0342] The control unit can control the die picker 200, which does not have a semiconductor chip attached thereto, to move to the flip-over picker 100 side and execute a step of receiving a new semiconductor chip. After going through the same method (receiving a semiconductor chip, immersing in flux, and inspecting the bottom surface), the die picker 200 can move in the length direction while adsorbing a semiconductor chip and be positioned above the die block 500.
[0343] The die picker 200 can move down to transfer the semiconductor chip to the escape groove of the die block 500 .
[0344] At this time, in order to transfer the semiconductor chip 20 picked up by the die picker 200 to a fixed position in the escape groove 510, it is necessary to compensate for the twisted angle of the semiconductor chip 20 picked up by the die picker 200 according to the inspection results of the approching vision 400.
[0345] In particular, in the case of a die block, since an escape groove is formed, if the position of the semiconductor chip is distorted, a problem may occur in that the semiconductor chip cannot be properly seated in the escape groove.
[0346] Therefore, the die block of the present invention is rotatably provided and can compensate for the twisted angle of the semiconductor chip 20 picked up by the die picker. That is, the die block 500 is rotatably provided in the θ direction on the xy plane, and the semiconductor chip 20 can be transferred to the escape groove 510 of the die block 500 in a state in which the die block 500 is rotated by the twisted angle of the semiconductor chip 20 according to the inspection result of the approching vision 400.
[0347] The die block rotates so that the direction of the semiconductor chip 20 being adsorbed by the die picker 200 matches the direction of the escape groove 510 of the die block 500, thereby aligning the semiconductor chip 20 with the escape groove 510 of the die block. This makes it possible to prevent the flux 50 applied to the underside of the semiconductor chip 20 from adhering to the side of the die block 500 that forms the escape groove 510 when the semiconductor chip is seated, and prevents a problem of insufficient flux 50 on the underside of the semiconductor chip 20 causing poor bonding during the bonding process.
[0348] After the semiconductor chip 20 is transferred to the die block 500, the die block rotates and returns to its initial position before the rotation, and the bonding head 700 picks up the semiconductor chip to which the flux has been applied from the die block.
[0349] Therefore, when the die block receives the semiconductor chip from the die picker, the die block rotates by the twisted angle of the semiconductor chip, and transfers the semiconductor chip to the escape groove of the die block, and when transferring the transferred semiconductor chip to the bonding head, the die block returns to its initial position and can rotate to transfer the semiconductor chip in an aligned state with the bonding head.
[0350] After the die block 500 rotates to align the semiconductor chip 20 in a desired direction, the bonding head 700 picks up the semiconductor chip 20 in a non-contact state, thereby reducing the alignment range of the bonding head 700 and achieving more precise and rapid bonding. That is, since the twist of the semiconductor chip 20 is pre-compensated by the die block 500, the bonding head 700 can pick up the aligned semiconductor chip 20, and the amount of correction of the semiconductor chip 20 picked up by the bonding head 700 can be minimized when bonding the semiconductor chip 20 to the substrate 40.
[0351] Of course, if the die picker or joining head is rotatably arranged, the die block does not have to be rotatably arranged. However, since the die picker must be able to rise and fall and move, providing a drive unit for rotation may result in the die picker structure becoming large, so it is preferable to rotate the die block 500.
[0352] Meanwhile, when the bonding head picks up the semiconductor chip transferred to the die block 500, the bonding head can create negative pressure while spaced apart from the semiconductor chip transferred to the die block 500 to suck and adsorb the semiconductor chip.
[0353] At this time, the bonding head sucks and holds the semiconductor chip in a non-contact manner, minimizing the impact and damage to the semiconductor chip.
[0354] However, because the semiconductor chip is sucked and attached without contact, if there is a difference in the suction force applied to the semiconductor chip during the process in which the semiconductor chip transferred to the die block 500 is attached to the suction member of the bonding head or if there is an inclination due to the way the semiconductor chip is seated on the die block, there is a problem that the semiconductor chip may be attached to a position other than that permitted by the bottom surface of the suction member.
[0355] The bottom surface of the suction member is formed with suction holes for suctioning the semiconductor chip and a reference object for inspecting the position of the semiconductor chip suctioned to the bonding head. However, if the semiconductor chip suctioned to the bonding head moves from the designated suction position and blocks the reference object, there is a problem that the position of the semiconductor chip suctioned to the bonding head cannot be detected when aligning the semiconductor chip to be bonded to a substrate later.
[0356] Furthermore, if the semiconductor chip deviates significantly from the suction surface of the bonding head, the transport stability decreases, which may cause a problem in that heat cannot be uniformly transferred to the plurality of bumps 21 when the semiconductor chip is bonded to the substrate.
[0357] Therefore, the area of the top end of the escape groove of the die block is formed smaller than the area of the bottom surface of the suction member, and when the semiconductor chip is transferred from the die block to the bonding head, the suction member of the bonding head is brought close to the upper open area of the escape groove, so that even if the semiconductor chip is tilted and sucked, the semiconductor chip can be attached within the allowable range of the bottom surface of the suction member due to the space formed by the bottom surface of the suction member and the escape groove. For example, when the suction member of the bonding head creates negative pressure while covering the upper open area of the escape groove, the suction member of the bonding head can act as a lid to prevent the semiconductor chip from escaping from the escape groove, and the semiconductor chip can be stably sucked within the allowable range of the suction member.
[0358] In this case, covering the upper open area of the escape groove means that the bonding head covers the upper area of the escape groove, which includes both the suction member of the bonding head contacting the upper area of the escape groove to completely close the upper area of the escape groove and the suction member being spaced a predetermined distance from the upper area of the escape groove so that there is a slight gap between the upper area of the escape groove, and the gap is spaced so that the movement range of the semiconductor chip can be limited within the allowable range of the escape groove and the suction member when the semiconductor chip is sucked in a non-contact state.
[0359] For reference, even if there is no complete contact and coverage, and the upper surface distance (gap) between the suction member of the bonding head and the inclined surface of the die block is thinner than the thickness of the semiconductor chip, the movement of the semiconductor chip is restricted by the covering, so that the semiconductor chip can be secured to the bottom surface of the suction member without escaping from the gap.
[0360] Of course, when a protruding end is formed in the escape groove and the edge of the underside of the semiconductor chip is supported by the protruding end, the semiconductor chip is horizontally seated on the protruding end even if the suction member of the joining head does not cover the upper open area of the escape groove, so the semiconductor chip can be easily attracted to the suction position of the suction member and adsorbed.
[0361] That is, in this case, a negative pressure can be generated in a state separated from the upper portion of the escape groove of the die block, and the semiconductor chip can be attracted to the suction position of the suction member and suctioned. At this time, if the control unit determines that the semiconductor chip or the flux application state is defective based on the inspection result of the appleooking vision 400, the die picker 200 transfers the defective semiconductor chip 22 to the die block 500, and the bonding head 700 picks up the defective semiconductor chip 22 on the die block 500 and provides it to the reject picker 600. The suction unit 610 of the reject picker 600 suctions the lower surface of the defective semiconductor chip 22 picked up by the bonding head 700, and removes the defective semiconductor chip from the bonding head 700.
[0362] Thereafter, the suction unit 610 is rotated 180° by the rotating member 620 of the reject picker 600 to invert the top and bottom surfaces of the defective semiconductor chip 22, and then the defective semiconductor chip 22 can be discarded into a collection container 651 located at the bottom of the reject picker 600. When discarding the defective semiconductor chip 22, the suction state of the suction unit 610 is released and switched to an exhaust state so that the defective semiconductor chip 22 can easily drop from the suction unit 610 of the reject picker 600, and air is sprayed toward the semiconductor chip side to reliably introduce the defective semiconductor chip 22 into the collection container 651.
[0363] If the control unit determines that the semiconductor chip or the flux application state is normal based on the inspection results of the appleooking vision 400, the die picker 200 transfers the normal semiconductor chip to the die block 500 side, and the bonding head 700 picks up the normal semiconductor chip on the die block 500 by sucking it with air while being spaced apart (non-contact state), and then thermocompression bonds it to the substrate 40.
[0364] The bonding head 700 picks up a normal semiconductor chip coated with flux from the die block 500, and then moves to above the bonding position where the semiconductor chip is to be bonded. Then, the slit vision 800 simultaneously inspects the semiconductor chip picked up by the bonding head 700 and the bonding position of the substrate to which the semiconductor chip is to be bonded, and inspects whether the center of the semiconductor chip sucked by the bonding head 700 and the center of the bonding position of the substrate are aligned.
[0365] At this time, if the center of the semiconductor chip does not coincide with the center of the bonding position of the substrate, the bonding head 700 can compensate for the positional distortion value of the semiconductor chip in the x-axis, y-axis, and θ-axis directions to bond the semiconductor chip to a preset bonding position of the substrate in an aligned state. The bonding head 700 can perform thermocompression bonding to the substrate by heating and pressing the semiconductor chip to a predetermined temperature.
[0366] To this end, the bonding head 700 picks up a semiconductor chip and then moves to above the bonding position where the semiconductor chip is to be bonded. Then, the slit vision 800 simultaneously inspects the semiconductor chip picked up by the bonding head 700 and the bonding position of the substrate to which the semiconductor chip is to be bonded, thereby inspecting whether the center of the semiconductor chip adsorbed to the bonding head 700 coincides with the center of the bonding position of the substrate.
[0367] At this time, if the center of the semiconductor chip does not coincide with the center of the bonding position of the substrate, the bonding head 700 can compensate for the positional torsion values of the semiconductor chip in the x-axis, y-axis, and θ-axis directions to bond the semiconductor chip to the bonding position of the substrate in an aligned state.
[0368] For reference, before inspecting the alignment state of the semiconductor chip and the substrate with the slit vision 800, it is also possible to inspect whether or not foreign matter is attached to the substrate to which the semiconductor chip is to be bonded or the semiconductor chip with the particle vision 890 mounted on one side of the bonding head 700. Of course, the inspection of the presence or absence of foreign matter at the bonding position with the particle vision 890 may be performed immediately before the semiconductor chip is bonded to the substrate, or the presence or absence of foreign matter may be inspected for the entire substrate to be bonded when the substrate to which the semiconductor chip is to be bonded is seated on the heating table 910. Also, the presence or absence of foreign matter may be inspected after each semiconductor chip is bonded to the substrate and before the next semiconductor chip is stacked on the bonded semiconductor chip.
[0369] A semiconductor chip can be bonded in an area of the bonding position of the substrate that is determined to be free of foreign matter, and as the bonding head 700 moves to the bonding position of the substrate, the slit vision 800 can also move to the bonding position of the semiconductor chip of the bonding head 700 and wait in the bonding area in advance.
[0370] For reference, in the joining apparatus of the present invention, the flip-over picker 100, the flux section 300, the up-picking vision 400, the die block 500, the die picker 200, the joining head 700, and the slit vision 800 are each provided in pairs, and are formed symmetrically on both sides of the axis along which the die picker 200 moves.
[0371] Therefore, a pair of bonding heads 700 and a pair of slit visions can share the substrate to be bonded placed on the heating table 910, inspecting the bonding area and performing bonding on the inspected area.
[0372] In particular, the center of the heating table 910 can be calculated by inspecting a reference object formed on the heating table 910, and the area of the substrate can be divided into a first area and a second area based on the center of the heating table 910.
[0373] In this case, the first region of the substrate may be covered by the first slit vision and the first bonding head, and the second region of the substrate may be covered by the second slit vision and the second bonding head. In this case, the first region and the second region may be half each based on the center of the substrate, or the number of pieces to be bonded may be halved based on the substrate to be bonded. If a part of the substrate to be bonded is found to be defective as a result of inspection by the slit vision or the particle vision, bonding is not performed on that part. Therefore, the remaining region excluding such defective region may be divided in half to define the first region and the second region, and the first region of the substrate may be covered by the first slit vision and the first bonding head, and the second region of the substrate may be covered by the second slit vision and the second bonding head.
[0374] Preferably, a first slit vision may inspect a region to be bonded in a first region of a substrate and the semiconductor chip adsorbed to the first bonding head, and bond the semiconductor chip adsorbed to the first bonding head to a bonding position in the first region of the substrate, and simultaneously or sequentially, a second slit vision may inspect a region to be bonded in a second region of a substrate and the semiconductor chip adsorbed to the second bonding head, and bond the semiconductor chip adsorbed to the second bonding head to a bonding position in the second region of the substrate.
[0375] Therefore, the pair of bonding heads 700 and the slit vision can perform inspection and bonding continuously without waiting for semiconductor chips.
[0376] On the other hand, after the bonding position of the semiconductor chip is inspected by the slit vision, the bonding head 700 performs thermocompression bonding.
[0377] Specifically, the bonding head 700 descends toward the substrate while being aligned with the substrate by the slit vision 800. The bonding head 700 is heated by a heating member mounted inside the bonding head while the bump-formed surface of the semiconductor chip is in contact with the upper surface of the substrate. At this time, the heating temperature may be set differently depending on the type of semiconductor chip to be bonded, but the temperature is raised to about 170°C to 300°C, which is a temperature that can sufficiently melt the bumps formed on the lower surface of the semiconductor chip, and the bonding head 700 is heated for several seconds. At this time, the substrate is in a state of being adsorbed to the adsorption area 911a of the heating table 910, and the heating table 910 may be in a state of being heated to a temperature of about 100°C. During the process of bonding due to the difference in temperature between the bonding head 700 and the heating table 910 during thermocompression bonding, the heat of the bonding head 700 is transferred to the chuck plate 911 of the heating table 910, and the heat transferred to the chuck plate 911 is diffused to the thermal diffusion area 911b.
[0378] In the chuck plate 911 of the present invention, the substrate adsorbed to the adsorption area 911a maintains a uniform temperature both at the center and at the periphery. In the case of the outermost region of the thermal diffusion area 911b provided on the outer periphery of the adsorption area 911a, heat cannot be diffused due to insulation by air, and a heat pool may occur.
[0379] However, since the suction area 911a of the chuck plate 911 is located inside the outer periphery, heat can be conducted in the radial direction, a uniform temperature can be maintained without heat accumulation, and uniform bonding quality can be ensured regardless of the position of the bonding area within the substrate.
[0380] After performing thermocompression bonding by the bonding head 700 for a preset time, cooling air is applied to the heating element to cool it to a temperature of about 100° C. for several seconds. The cooling solidifies the molten bumps, thereby fixing the semiconductor chip to the substrate.
[0381] The bonding head 700 may be cooled with the heating member attached to the bonding head 700 turned off, but since turning off the heating member requires a lot of time to turn on the heating member and raise the temperature to a desired temperature, it is preferable to lower the temperature of the heating member or to lower the temperature of the heating member to a preset cooling temperature by spraying cooling air onto the heating member while maintaining the temperature of the heating member. As a result, the bonding head 700 is cooled while decreasing in temperature, and the semiconductor chip in contact with the bonding head 700 is also cooled while decreasing in temperature. As a result, the flux and bumps melted on the upper surface of the substrate are hardened and the semiconductor chip is bonded to the substrate. Of course, the temperature of the heating table 910 may be heated and maintained at a temperature of about 100° C. during the thermocompression bonding.
[0382] In this manner, the heating table of the bonding apparatus of the present invention has a thermal diffusion region 911b on the outer peripheral edge of the suction region 911a which suctions the substrate to be bonded to the heating plate 912, thereby preventing heat accumulation on the outer periphery of the substrate and ensuring temperature uniformity regardless of the position of the substrate, thereby ensuring bonding quality and reducing the defect rate.
[0383] In particular, when multiple semiconductor chips stacked vertically are thermocompression bonded using the heating table 910, there is no difference in the bonding state of the semiconductor chips and the hardening state of the flux between the upper and lower parts of the stacked semiconductor chips, thereby improving the bonding quality.
[0384] Furthermore, when bonding a semiconductor chip to a substrate, the bonding position must be aligned for each semiconductor chip, and thermocompression bonding must be performed by heating and cooling. This requires a lot of time to be spent on bonding in the thermocompression bonding method.
[0385] Therefore, in the thermocompression bonding apparatus 10 of the present invention, the bonding head 700 moves back and forth between only the die block 500 and the substrate while concentrating only on bonding, and the die picker 200 can prepare the subsequent semiconductor chip to be bonded to the substrate via the flip-over picker 100, the flux unit 300, the up-picking vision 400, and the die block 500.
[0386] In addition, according to the bonding device of the present invention, the path along which the bonding head 700 moves to adsorb the semiconductor chip is shorter than in existing bonding devices, so that the amount of flux scattered by the heat remaining in the bonding head 700 can be reduced.
[0387] Therefore, according to the thermocompression bonding apparatus 10 of the present invention, the bonding head 700, which still has residual heat, does not perform the flux dipping operation of the semiconductor chip, so that heat is not transferred to the flux part 300, and deterioration or alteration of the flux due to heat accumulation can be prevented. Also, the flux can be prevented from hardening inside the flux part 300, so that the flux can be flattened to a desired thickness, and a fixed amount of flux can be applied to the semiconductor chip when the semiconductor chip is dipped.
[0388] In addition, in the conventional thermocompression bonding apparatus 10, the semiconductor chip is immersed in flux in the flux section 300, inspected by the approching vision 400, and then the semiconductor chip is brought into contact with the bonding head for bonding, and the travel distance and contact time are somewhat long. However, according to the present invention, the flux immersion and inspection of the semiconductor chip are already performed by the die picker 200, so the travel distance and contact time of the bonding head and the semiconductor chip until the delivered semiconductor chip is bonded to the substrate are shortened, and the amount of evaporation of flux that occurs during the movement process can be reduced.
[0389] In addition, by forming an escape groove in the die block 500 to prevent the flux from sticking to the die block 500 when the semiconductor chip coated with the flux is transferred, the problem of the flux being reduced when the amount of the flux applied to the semiconductor chip is reduced can be prevented.
[0390] In addition, in order to prevent the defective semiconductor chips 22 coated with flux from being bonded to the substrate, the defective semiconductor chips 22 are sucked up and reliably removed from the bonding head 700, and air is sprayed onto the defective semiconductor chips 22 to drop them toward the collection unit 65. This prevents the defective semiconductor chips 22 from scattering around during the removal process and accidentally attaching to the substrate, or from being unable to be separated from the bonding head, thereby preventing mass defects due to overlapping bonding of expensive semiconductor chips.
[0391] As described above, the present invention has been described with reference to the preferred embodiments. However, those skilled in the art can implement the present invention with various modifications and variations without departing from the spirit and scope of the present invention as set forth in the following claims. [Explanation of symbols]
[0392] 10 thermocompression bonding device; 20 semiconductor chip; 21 bump; 22 defective semiconductor chip; 20a molding surface; 20b bump forming surface; 100 flip-over picker; 101 expanding section; 110 pressing plate; 111 pressing member; 112 seating member; 113 connecting member; 120 peeling prevention plate; 130 support member; 140 elastic member; 200 die picker; 210 picker body; 211 pickup arm; 210a suction member; 220 mounting member; 230 first rotating shaft; 231 first driving section; 240 second rotating shaft; 241 second driving section; 250 switching member; 251 link; 252 cam follower; 253 bracket; 253a connecting frame; 253b first horizontal frame; 253c second horizontal frame; 253d Storage space;290 fixed frame;300 flux section;310 immersion plate;320 flux tank;330 base;340 guide member;350 moving bracket;360 moving block;380 guide member;400 up-picking vision;500 die block;600 reject picker;610 suction unit;620 rotating member;650 collection section;651 collection container;652 second sensor;700 joining head;710 rotating motor;720 low-friction coupling;730 pressing section;731 driving element;732 moving element;735 locking jaw;740 first load measuring section;750 load control section;760 horizontal leveler;770 joining tool;771 air suction port;772 air supply port;773 air exhaust port;733 Pressing portion height measuring portion; 780 heating member; 790 axis; 800 slit vision; 910 heating table; 911 chuck plate; 890 particle vision; 950 lift member; 911a suction area; 911b thermal diffusion area; 911c insertion groove; 911d suction hole; 911e fourth air pressure passage; 911f fifth air pressure passage; 912 heating plate; 912a first through hole; 912b second through hole; 913 base; 913a first air pressure passage; 913b second air pressure passage; 913c third air pressure passage; t tape; F reference object; rf frame.
Claims
1. a flip-over picker that picks up individualized semiconductor chips from a tape to which the individualized semiconductor chips are attached and turns the semiconductor chips upside down; a die picker that receives the semiconductor chip from the flip-over picker; a flux portion for accommodating flux for immersing the lower surface of the semiconductor chip in the flux; an appleooking vision for inspecting the underside or cracks of the semiconductor chip; a bonding head having a heating member mounted therein for thermocompression bonding of the semiconductor chip to the substrate; a slit vision for simultaneously photographing the semiconductor chip picked up by the bonding head and the top surface of the substrate to which the semiconductor chip is bonded, thereby inspecting the alignment of the semiconductor chip; a die block fixedly disposed under a moving path of the die picker and the bonding head, to which a semiconductor chip coated with flux is transferred, and having an escape groove for allowing the flux coated on the underside of the semiconductor chip to escape; the die picker immerses the bottom surface of the semiconductor chip in the flux and transfers it to the die block; A thermocompression bonding apparatus, characterized in that the bonding head picks up a semiconductor chip coated with flux from the die block and bonds it to the substrate by thermocompression bonding.
2. the die picker forms a negative pressure while being spaced apart from the semiconductor chip to suck and adsorb the semiconductor chip from the flip-over picker; 2. The thermocompression bonding apparatus according to claim 1, wherein the bonding head creates a negative pressure while separated from the semiconductor chip to suck and adsorb the semiconductor chip coated with the flux from the die block.
3. The flip-over picker, the flux section, the up-picking vision, and the die block are arranged in a line so that their working areas are aligned on the same line along the moving direction of the die picker; The die picker moves to the same height as previously set when moving to the top of each of the working areas of the flip-over picker, the apple picking vision, and the die block; 2. The thermocompression bonding apparatus of claim 1, wherein the preset height is the same as a height corresponding to a working distance of the apple picking vision when inspecting the bottom surface of the semiconductor chip with the apple picking vision.
4. The die picker includes: a picker body having a movably mounted pick-up arm for picking up the semiconductor chip; a mounting member to which the picker body is mounted so as to be capable of ascending and descending; a first rotation shaft extending along a moving direction of the picker body, the mounting member being inserted and coupled to the first rotation shaft, and the first rotation shaft rotating to move the mounting member in the moving direction of the picker body; a second rotation shaft extending in a direction parallel to the first rotation shaft at an upper or lower part of the first rotation shaft and rotatably provided in an axial direction; 2. The thermocompression bonding apparatus according to claim 1, further comprising: a switching member that is attached to the second rotating shaft and raises and lowers the picker body from the mounting member as the second rotating shaft rotates.
5. The switching member is a link coupled to the second rotation shaft and rotatable together with the second rotation shaft; a cam follower attached to the other side of the link and coupled to a bracket extending to a lower portion of the picker body; The bracket is a U-shaped bracket, 5. The thermocompression bonding apparatus according to claim 4, wherein the cam follower is connected to a U-shaped bracket in a state of being housed therein.
6. The flip-over picker, the flux unit, the apple picking vision, and the die block are arranged in a line so that their working areas are aligned on the same line along the moving direction of the die picker, and the flip-over picker, the flux unit, the apple picking vision, the die block, and the die picker are each provided in pairs, The pick-up arm is formed to protrude from the picker body to a position corresponding to an upper portion of each of the working areas of the flip-over picker, the flux part, the up-picking vision, and the die block, the die picker further includes a fixed frame to which the first rotating shaft and the second rotating shaft are attached and which guides the movement of the picker body; The pair of die pickers are provided on one side and the other side of the fixed frame, respectively, 5. The thermocompression bonding apparatus according to claim 4, wherein the pair of flip-over pickers, the flux section, the appleooking vision, and the die block are formed symmetrically with respect to the fixed frame.
7. The flux portion is an immersion plate having a flux receiving groove formed therein for receiving flux; a flux tank that is movably installed on the immersion plate and has a container for containing flux that is open downward; a moving bracket attached to one side of the flux tank; a flux tank transport unit including a guide member that guides the movement of the flux tank and a moving block that transports the flux tank along the guide member, a receiving groove is formed on one of the moving bracket and the moving block, and an insertion part to be inserted into the receiving groove is formed on the other of the moving bracket and the moving block, and the flux tank is transported in accordance with the transportation of the moving block; When a receiving groove is formed in either the moving bracket or the moving block, The moving bracket or the moving block is The frame includes guide members coupled to upper portions of both sides of the frame, 2. The thermocompression bonding apparatus according to claim 1, wherein a receiving groove is formed by the frame and the guide member.
8. 2. The thermocompression bonding apparatus according to claim 1, wherein the appleooking vision inspects the presence or absence of cracks in the semiconductor chip when the flux is not applied, and inspects the underside of the semiconductor chip when the flux is applied.
9. The joining head includes: a bonding tool that includes a heating member for heating the semiconductor chip and bonds the semiconductor chip by thermocompression bonding; A shaft provided on an upper portion of the joining tool and mounted so as to be movable up and down; a load control unit that supports the shaft and adjusts a predetermined load to the weight of the shaft; a pressing unit including a mover provided on an upper portion of the load control unit and fixed to an outer circumferential surface of the shaft, and a driver that drives the mover to be movable in a vertical direction to press the welding tool with a predetermined force; a first load measuring unit that is provided between the load control unit and the pressing unit and that measures the load applied to the semiconductor chip in real time; A rotary motor provided on an upper portion of the pressing portion and configured to rotate the shaft; a low-friction coupling that connects the rotary motor and the shaft and transmits a rotational force of the rotary motor to the shaft; the low-friction coupling has an upper portion connected to the rotary motor and a lower portion connected to the shaft, forming a space between the rotary motor and the shaft; 2. The thermocompression bonding apparatus according to claim 1, wherein the shaft can be raised and lowered by the mover between the separated spaces.
10. The thermocompression bonding apparatus includes: a heating table to which a substrate to which the semiconductor chip is bonded is transferred; a second load measuring unit provided on one side of the heating table and contacting the welding head to measure a load of the welding head, 10. The thermocompression bonding apparatus according to claim 9, wherein the first load measuring section is set so that a measurement value of the first load measuring section is equal to a measurement value of the second load measuring section.
11. The shaft passes through the movable element of the pressing portion, The thermocompression bonding apparatus according to claim 9, wherein the shaft and the movable element are rotated together by the rotary motor to rotate the bonding tool.
12. 10. The thermocompression bonding apparatus according to claim 9, wherein the low-friction coupling is extendable in the up-down direction with an upper portion fixed when the shaft is raised and lowered in the space separated by the movable member.
13. 2. The thermocompression bonding apparatus according to claim 1, wherein the escape groove of the die block has an open top and an inwardly inclined surface, and a side surface of the semiconductor chip is supported by the inclined surface so that a bottom surface of the escape groove is spaced from a bottom surface of the escape groove.
14. the escape groove of the die block has an open upper portion and an inclined surface inclined inwardly, and a protruding end extending in a horizontal direction is formed at a lower portion of the inclined surface to support a lower surface of the semiconductor chip; 2. The thermocompression bonding apparatus according to claim 1, wherein the protruding end supports an edge of the lower surface of the semiconductor chip, so that the lower surface of the semiconductor chip is spaced from a bottom surface of the escape groove.
15. 2. The thermocompression bonding apparatus according to claim 1, wherein the escape groove is formed by a plurality of protruding blocks, each protruding block being inclined inwardly, and adjacent protruding blocks being spaced apart from each other.
16. The die block is rotatably mounted, 2. The thermocompression bonding apparatus according to claim 1, wherein the die picker transfers the semiconductor chip to the escape groove of the die block in a state where the die block is rotated by an angle corresponding to a twisted angle of the semiconductor chip in response to an inspection result of the appleooking vision.
17. 17. The thermocompression bonding apparatus according to claim 16, wherein after the semiconductor chip is transferred to the die block, the die block rotates and returns to its initial position before the rotation, and the bonding head picks up the semiconductor chip coated with flux from the die block.
18. The thermocompression bonding apparatus includes: The method further includes a reject picker that removes a defective semiconductor chip determined to be defective by the inspection result of the AppleKingVision from the bonding head, and a collection unit that discards the defective semiconductor chip by the reject picker, The reject picker includes: a suction unit that is formed with a duct for sucking or discharging air and that sucks the semiconductor chip; a rotating member for rotating the suction unit by 180° to invert the top and bottom surfaces of the semiconductor chip suctioned by the suction unit; 2. The thermocompression bonding apparatus according to claim 1, wherein the suction unit discharges air onto the semiconductor chip turned upside down by the rotating member, thereby causing the semiconductor chip to fall toward the removal section.
19. The thermocompression bonding apparatus includes: a heating table to which a substrate to which the semiconductor chip is bonded is transferred; The heating table is a chuck plate on which a substrate to be bonded is placed, a base provided under the chuck plate and connected to a vacuum generating device for generating a negative pressure in the chuck plate, and a heating plate provided between the chuck plate and the base for transferring heat to the chuck plate, 2. The thermocompression bonding apparatus according to claim 1, wherein the chuck plate is provided with an adsorption area for adsorbing the substrate and a thermal diffusion area for diffusing heat transferred from the heating plate or the bonding head.
20. The thermocompression bonding apparatus includes: The bonding head further includes a particle vision device for detecting the presence or absence of foreign matter on the upper surface of the substrate to be bonded, the particle vision device being attached to one side of the bonding head, 2. The thermocompression bonding apparatus according to claim 1, wherein the particle vision detects the presence or absence of foreign matter on an upper surface of the substrate to which the semiconductor chip is bonded or on an upper surface of a lower semiconductor chip to which the semiconductor chip is bonded.
21. The thermocompression bonding apparatus includes: The tape having the individual semiconductor chips attached thereto is further provided with an expanding section for expanding the tape of the ring frame having the individual semiconductor chips attached thereto on its underside, The expanding section is A support member for supporting a lower surface of the tape; a pressing plate that is provided so as to be movable up and down and presses downward the upper surface of the ring frame to which the tape is attached; and an elastic member that presses the lower surface of the tape adhered to the ring frame in a direction opposite to the pressing direction of the pressing plate, The thermocompression bonding apparatus according to claim 1, characterized in that the elastic member supports the tape, and supports the tape in a direction opposite to the pressing direction of the pressure plate when pressed by the pressure plate, and deforms to expand the tape by causing the pressure plate and the peel prevention plate to descend together.