Semiconductor storage device
By integrating a semiconductor layer with specific metal elements and an amorphous second region in the insulating layer, the semiconductor memory device addresses issues of impurity diffusion and resistance, ensuring high-speed and reliable operation of three-dimensional NAND flash memory.
Patent Information
- Application Number
- JP2021146796
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2021-09-09
- Publication Date
- 2024-10-23
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing semiconductor memory devices face challenges in maintaining high-speed operation and preventing leakage current due to impurity diffusion and increased electrical resistance in three-dimensional NAND flash memory structures.
Incorporating a semiconductor layer with specific metal elements and a charge storage layer with aluminum oxide and oxygen, along with an amorphous second region in the insulating layer to suppress impurity diffusion and reduce electrical resistance.
This configuration enhances the operational speed and maintains the integrity of memory cell characteristics by reducing leakage current and electrical resistance, thereby improving the overall performance of three-dimensional NAND flash memory.
Smart Images

Figure 2024149933000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor memory device. [Background technology]
[0002] 3D NAND flash memory, which has memory cells arranged three-dimensionally, achieves high integration and low cost. In 3D NAND flash memory, for example, a memory hole penetrating a stack in which multiple insulating layers and multiple gate electrode layers are alternately stacked is formed. A charge storage layer and a semiconductor layer are formed in the memory hole, forming a memory string in which multiple memory cells are connected in series. Data is stored in the memory cell by controlling the amount of charge held in the charge storage layer. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] U.S. Pat. No. 10,566,280 Summary of the Invention [Problem to be solved by the invention]
[0004] An object of the present invention is to provide a semiconductor memory device capable of improving characteristics. [Means for solving the problem]
[0005] The semiconductor memory device of the embodiment includes a semiconductor layer extending in a first direction, a gate electrode layer containing at least one metal element selected from the group consisting of tungsten (W), molybdenum (Mo), and cobalt (Co), a charge storage layer provided between the semiconductor layer and the gate electrode layer, and a first insulating layer provided between the charge storage layer and the gate electrode layer, including a first region containing aluminum (Al) and oxygen (O), and in contact with the gate electrode layer. [Brief description of the drawings]
[0006] [Figure 1] 1 is a circuit diagram of a memory cell array in a semiconductor memory device according to a first embodiment. [Diagram 2] 1 is a schematic cross-sectional view of a memory cell array in a semiconductor memory device according to a first embodiment. [Diagram 3] 1 is a schematic cross-sectional view of a memory cell in a semiconductor memory device according to a first embodiment. [Figure 4] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Diagram 5] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 6] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 7] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 8] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 9] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 10] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 11] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 12] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 13] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 14] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the first embodiment. [Figure 15] FIG. 4 is a schematic cross-sectional view of a memory cell in a semiconductor memory device as a comparative example of the first embodiment. [Figure 16] FIG. 11 is a schematic cross-sectional view of a memory cell array in a semiconductor memory device according to a second embodiment. [Figure 17] FIG. 11 is a schematic cross-sectional view of a memory cell in a semiconductor memory device according to a second embodiment. [Figure 18] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the second embodiment. [Figure 19] 5A to 5C are schematic cross-sectional views showing an example of a manufacturing method of the semiconductor memory device according to the second embodiment. [Figure 20] FIG. 13 is a schematic cross-sectional view of a memory cell in a semiconductor memory device as a comparative example of the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the following description, the same reference numerals will be used to designate the same or similar components, and the description of components that have already been described will be omitted as appropriate.
[0008] In addition, the terms "upper" and "lower" may be used for convenience in this specification. "Upper" and "lower" are terms that indicate, for example, a relative positional relationship in a drawing. The terms "upper" and "lower" do not necessarily specify a positional relationship with respect to gravity.
[0009] The qualitative and quantitative analysis of the chemical composition of the members constituting the semiconductor memory device in this specification can be performed by, for example, secondary ion mass spectroscopy (SIMS), energy dispersive X-ray spectroscopy (EDX), electron energy loss spectroscopy (EELS), etc. Furthermore, for measuring the thickness of the members constituting the semiconductor memory device and the distance between the members, for example, a transmission electron microscope (TEM) can be used. Furthermore, for identifying the crystal system of the constituent material of the semiconductor memory device and comparing the abundance ratio of the crystal system, for example, a transmission electron microscope, X-ray diffraction analysis (XRD), electron beam diffraction analysis (EBD), X-ray photoelectron spectroscopy (XPS), and synchrotron radiation X-ray absorption fine structure (XAFS) can be used. Moreover, whether a material constituting a semiconductor memory device is crystalline or amorphous can be determined from an image obtained by, for example, a TEM.
[0010] (First embodiment) The semiconductor memory device of the first embodiment includes a semiconductor layer extending in a first direction, a gate electrode layer containing at least one metal element selected from the group consisting of tungsten (W), molybdenum (Mo), and cobalt (Co), a charge storage layer provided between the semiconductor layer and the gate electrode layer, and a first insulating layer provided between the charge storage layer and the gate electrode layer, including a first region containing aluminum (Al) and oxygen (O), and in contact with the gate electrode layer.
[0011] The semiconductor memory device of the first embodiment is a three-dimensional NAND flash memory. The memory cells of the semiconductor memory device of the first embodiment are so-called Metal-Oxide-Nitride-Oxide-Semiconductor (MONOS) type memory cells.
[0012] FIG. 1 is a circuit diagram of a memory cell array in a semiconductor memory device according to the first embodiment.
[0013] The memory cell array 100 of the 3D NAND flash memory of the first embodiment includes a plurality of word lines WL, a common source line CSL, a source select gate line SGS, a plurality of drain select gate lines SGD, a plurality of bit lines BL, and a plurality of memory strings MS, as shown in FIG.
[0014] A plurality of word lines WL are arranged in the z direction and spaced apart from one another. A plurality of word lines WL are arranged in a stacked manner in the z direction. A plurality of memory strings MS extend in the z direction. A plurality of bit lines BL extend, for example, in the x direction.
[0015] Hereinafter, the x direction is defined as a third direction, the y direction as a second direction, and the z direction as a first direction. The x direction, the y direction, and the z direction intersect with each other, for example, are perpendicular to each other.
[0016] As shown in Fig. 1, a memory string MS includes a source select transistor SST, a plurality of memory cells, and a drain select transistor SDT, which are connected in series between a common source line CSL and a bit line BL. One memory string MS is selected by selecting one bit line BL and one drain select gate line SGD, and one memory cell can be selected by selecting one word line WL. The word line WL is the gate electrode of the memory cell transistor MT that constitutes the memory cell.
[0017] 2(a) and 2(b) are schematic cross-sectional views of a memory cell array of a semiconductor memory device according to the first embodiment. Figures 2(a) and 2(b) show cross sections of multiple memory cells in one memory string MS, for example, surrounded by a dotted line, in the memory cell array 100 in Figure 1.
[0018] Fig. 2(a) is a yz cross-sectional view of the memory cell array 100. Fig. 2(a) is a BB' cross-sectional view of Fig. 2(b). Fig. 2(b) is an xy cross-sectional view of the memory cell array 100. Fig. 2(b) is an AA' cross-sectional view of Fig. 2(a). In Fig. 2(a), the area surrounded by a dashed line is one memory cell.
[0019] Fig. 3 is a schematic cross-sectional view of a memory cell in the semiconductor memory device of the first embodiment, and an enlarged cross-sectional view of a portion of the memory cell.
[0020] As shown in Figures 2(a), 2(b), and 3, the memory cell array 100 includes a word line WL, a semiconductor layer 10, an interlayer insulating layer 12, a tunnel insulating layer 14, a charge storage layer 16, a first block insulating layer 18, a second block insulating layer 19, and a core insulating region 20.
[0021] The multiple word lines WL and the multiple interlayer insulating layers 12 form a stack 30. The first block insulating layer 18 includes a first region 18a and a second region 18b.
[0022] The word line WL is an example of a gate electrode layer. The interlayer insulating layer 12 is an example of a fourth insulating layer. The tunnel insulating layer 14 is an example of a third insulating layer. The first block insulating layer 18 is an example of a first insulating layer. The second block insulating layer 19 is an example of a second insulating layer.
[0023] The memory cell array 100 is provided, for example, on a semiconductor substrate (not shown). The semiconductor substrate has a surface parallel to the x-direction and the y-direction.
[0024] The word lines WL and the interlayer insulating layers 12 are alternately stacked in the z direction on the semiconductor substrate. The word lines WL are repeatedly arranged in the z direction at intervals. The word lines WL and the interlayer insulating layers 12 form a stacked body 30. The word lines WL function as control electrodes of the memory cell transistors MT.
[0025] The word line WL is a plate-shaped conductor. The word line WL includes at least one metal element selected from the group consisting of tungsten (W), molybdenum (Mo), and cobalt (Co). The word line WL is, for example, a tungsten layer, a molybdenum layer, or a cobalt layer. The thickness of the word line WL in the z direction is, for example, 5 nm or more and 20 nm or less.
[0026] The interlayer insulating layer 12 electrically separates the word lines WL from one another. The interlayer insulating layer 12 electrically separates the word lines WL from one another.
[0027] The interlayer insulating layer 12 is, for example, an oxide, an oxynitride, or a nitride. The interlayer insulating layer 12 is, for example, silicon oxide. The thickness of the interlayer insulating layer 12 in the z direction is, for example, 5 nm or more and 20 nm or less.
[0028] The semiconductor layer 10 is provided in the stack 30. The semiconductor layer 10 extends in the z direction. The semiconductor layer 10 extends in a direction perpendicular to the surface of the semiconductor substrate.
[0029] The semiconductor layer 10 is provided to penetrate the stacked body 30. The semiconductor layer 10 is surrounded by a plurality of word lines WL. The semiconductor layer 10 has, for example, a cylindrical shape. The semiconductor layer 10 functions as a channel of the memory cell transistor MT.
[0030] The semiconductor layer 10 is, for example, a polycrystalline semiconductor. The semiconductor layer 10 is, for example, polycrystalline silicon.
[0031] The tunnel insulating layer 14 is provided between the semiconductor layer 10 and the word line WL. The tunnel insulating layer 14 is provided between the semiconductor layer 10 and at least one of the multiple word lines WL. The tunnel insulating layer 14 is provided between the semiconductor layer 10 and the charge storage layer 16. The tunnel insulating layer 14 has a function of passing charges in response to a voltage applied between the word line WL and the semiconductor layer 10.
[0032] The tunnel insulating layer 14 includes, for example, silicon (Si), nitrogen (N), and oxygen (O). The tunnel insulating layer 14 includes, for example, silicon oxide, silicon nitride, or silicon oxynitride. The tunnel insulating layer 14 has, for example, a stacked structure of a silicon oxide layer, a silicon nitride layer, and a silicon oxide layer. The thickness of the tunnel insulating layer 14 is, for example, 3 nm or more and 8 nm or less.
[0033] The charge storage layer 16 is provided between the tunnel insulating layer 14 and the first block insulating layer 18. The charge storage layer 16 is provided between the tunnel insulating layer 14 and the second block insulating layer 19.
[0034] The charge storage layer 16 has a function of trapping and storing electric charges. The electric charges are, for example, electrons. The threshold voltage of the memory cell transistor MT changes depending on the amount of electric charges stored in the charge storage layer 16. By utilizing this change in threshold voltage, it becomes possible for one memory cell to store data.
[0035] For example, the voltage at which the memory cell transistor MT turns on changes as the threshold voltage of the memory cell transistor MT changes. If a high threshold voltage state is defined as data "0" and a low threshold voltage state is defined as data "1," the memory cell can store one bit of data, "0" or "1."
[0036] The charge storage layer 16 is an insulating layer. The charge storage layer 16 includes, for example, silicon (Si) and nitrogen (N). The charge storage layer 16 includes, for example, silicon nitride. The charge storage layer 16 is, for example, a silicon nitride layer. The thickness of the charge storage layer 16 is, for example, 3 nm or more and 10 nm or less.
[0037] The first block insulating layer 18 and the second block insulating layer 19 are provided between the tunnel insulating layer 14 and the word line WL. The first block insulating layer 18 and the second block insulating layer 19 are provided between the charge storage layer 16 and the word line WL. The first block insulating layer 18 and the second block insulating layer 19 have the function of blocking a current flowing between the charge storage layer 16 and the word line WL.
[0038] The thickness in the y direction of first block insulating layer 18 is, for example, not less than 1 nm and not more than 8 nm. The thickness in the y direction of second block insulating layer 19 is, for example, not less than 3 nm and not more than 8 nm.
[0039] The first block insulating layer 18 is provided between the charge storage layer 16 and the word line WL. The first block insulating layer 18 is provided between the second block insulating layer 19 and the word line WL. The first block insulating layer 18 contacts the word line WL.
[0040] The interlayer insulating layer 12 is provided in the z direction of the word lines WL. A first block insulating layer 18 is provided between the word lines WL and the interlayer insulating layer 12 in the z direction.
[0041] The first block insulating layer 18 includes a first region 18a and a second region 18b. The second region 18b is provided between the word line WL and the first region 18a.
[0042] The first region 18a is an insulating layer. The first region 18a includes aluminum (Al) and oxygen (O). The first region 18a includes aluminum oxide. The first region 18a is, for example, an aluminum oxide layer.
[0043] The first region 18a is crystalline. The first region 18a is, for example, a crystalline aluminum oxide layer.
[0044] The thickness of the first region 18a in the y direction from the semiconductor layer 10 toward the word line WL is, for example, not less than 1 nm and not more than 5 nm.
[0045] The second region 18b is an insulating layer. The second region 18b is, for example, an oxide, an oxynitride, or a nitride. The second region 18b includes, for example, at least one element of aluminum (Al), hafnium (Hf), or zirconium (Zr). The second region includes, for example, at least one element of oxygen (O) or nitrogen (N).
[0046] The second region 18b includes, for example, aluminum nitride, aluminum oxynitride, aluminum oxide, aluminum silicate, hafnium silicate, nitrogen-doped hafnium silicate, or zirconium silicate. The second region 18b is, for example, an aluminum nitride layer, an aluminum oxynitride layer, an aluminum oxide layer, an aluminum silicate layer, a hafnium silicate layer, a nitrogen-doped hafnium silicate layer, or a zirconium silicate layer.
[0047] The second region 18b is amorphous. The second region 18b is, for example, an amorphous aluminum nitride layer, an amorphous aluminum oxynitride layer, an amorphous aluminum oxide layer, an amorphous aluminum silicate layer, an amorphous hafnium silicate layer, an amorphous nitrogen-doped hafnium silicate layer, or an amorphous zirconium silicate layer.
[0048] The second region 18b includes, for example, boron (B). The boron atomic concentration of the second region 18b is, for example, higher than the boron atomic concentration of the first region 18a.
[0049] The second region 18b contains, for example, fluorine (F). The fluorine atomic concentration of the second region 18b is, for example, higher than the fluorine atomic concentration of the first region 18a.
[0050] The thickness of the second region 18b in the y direction from the semiconductor layer 10 toward the word line WL is thinner than the thickness of the first region 18a in the y direction from the semiconductor layer 10 toward the word line WL. The thickness of the second region 18b in the y direction from the semiconductor layer 10 toward the word line WL is, for example, not less than 0.1 nm and not more than 1 nm.
[0051] The second block insulating layer 19 is provided between the charge storage layer 16 and the first block insulating layer 18. The second block insulating layer 19 is provided between the interlayer insulating layer 12 and the semiconductor layer 10. The second block insulating layer 19 is provided between the interlayer insulating layer 12 and the charge storage layer 16.
[0052] The second block insulating layer 19 is an insulating layer. The second block insulating layer 19 includes, for example, silicon (Si) and oxygen (O). The second block insulating layer 19 includes, for example, silicon oxide.
[0053] The thickness of the second block insulating layer 19 in the y direction is, for example, not less than 3 nm and not more than 8 nm.
[0054] The core insulating region 20 is provided in the stack 30. The core insulating region 20 extends in the z direction. The core insulating region 20 is provided penetrating the stack 30. The core insulating region 20 is surrounded by the semiconductor layer 10. The core insulating region 20 is surrounded by a plurality of word lines WL. The core insulating region 20 is columnar. The core insulating region 20 is, for example, cylindrical.
[0055] The core insulating region 20 is, for example, an oxide, an oxynitride, or a nitride. The core insulating region 20 includes, for example, silicon (Si) and oxygen (O). The core insulating region 20 is, for example, silicon oxide.
[0056] Next, an example of a method for manufacturing the semiconductor memory device of the first embodiment will be described.
[0057] Figures 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, and 14 are schematic cross-sectional views showing an example of a method for manufacturing the semiconductor memory device of the first embodiment. Each of Figures 4 to 14 shows a cross section corresponding to Figure 2(a). Figures 4 to 14 are views showing an example of a method for manufacturing the memory cell array 100 of the semiconductor memory device.
[0058] First, silicon oxide layers 50 and silicon nitride layers 52 are alternately stacked on a semiconductor substrate (not shown) (FIG. 4). A stacked structure 31 is formed in which a plurality of silicon oxide layers 50 and a plurality of silicon nitride layers 52 are alternately stacked in the z direction. A portion of the stacked structure 31 will eventually become the stacked body 30.
[0059] The silicon oxide layer 50 and the silicon nitride layer 52 are formed by, for example, a chemical vapor deposition (CVD) method. A part of the silicon oxide layer 50 will eventually become the interlayer insulating layer 12.
[0060] Next, a memory hole 54 is formed in the silicon oxide layer 50 and the silicon nitride layer 52 (FIG. 5). The memory hole 54 penetrates the stacked structure 31 and extends in the z direction. The memory hole 54 is formed by, for example, a lithography method and a reactive ion etching method (RIE method).
[0061] Next, a silicon oxide film 56 is formed on the inner wall of the memory hole 54 (FIG. 6). The silicon oxide film 56 is formed by, for example, a CVD method. The silicon oxide film 56 will eventually become the second block insulating layer 19.
[0062] Next, a silicon nitride film 58 is formed on the silicon oxide film 56 (FIG. 7). The silicon nitride film 58 is formed by, for example, an atomic layer deposition method (ALD method). The silicon nitride film 58 will eventually become the charge storage layer 16.
[0063] Next, a laminated insulating film 60 is formed on the silicon nitride film 58 (FIG. 8). The laminated insulating film 60 is, for example, a laminated film of a silicon oxide film, a silicon nitride film, and a silicon oxide film.
[0064] The laminated insulating film 60 is formed by, for example, a CVD method. The laminated insulating film 60 will eventually become the tunnel insulating layer 14.
[0065] Next, a polycrystalline silicon film 62 is formed on the laminated insulating film 60 (FIG. 9). The polycrystalline silicon film 62 is formed by, for example, a CVD method. The polycrystalline silicon film 62 will eventually become the semiconductor layer 10.
[0066] Next, the memory hole 54 is filled with a silicon oxide film 64 (FIG. 10). The silicon oxide film 64 is formed on the polycrystalline silicon film 62. The silicon oxide film 64 is formed by, for example, a CVD method. The silicon oxide film 64 will eventually become the core insulating region 20.
[0067] Next, the silicon nitride layer 52 is selectively removed by wet etching using an etching groove (not shown) (FIG. 11). For example, a phosphoric acid solution is used for the wet etching. The silicon nitride layer 52 is selectively etched with respect to the silicon oxide layer 50 and the silicon oxide film 56.
[0068] Next, an aluminum oxide film 66 is formed in the region where the silicon nitride layer 52 has been removed (FIG. 12). The aluminum oxide film 66 is formed by, for example, the ALD method. The aluminum oxide film 66 will eventually become the first region 18a of the first block insulating layer 18.
[0069] Next, crystallization annealing is performed, for example, in an inert gas atmosphere at a temperature of 1000° C. The crystallization annealing makes the aluminum oxide film 66 crystalline.
[0070] Next, an aluminum nitride film 68 is formed on the aluminum oxide film 66 (FIG. 13). The aluminum nitride film 68 is formed by, for example, the ALD method. The aluminum nitride film 68 is amorphous. The aluminum nitride film 68 will eventually become the second region 18b of the first block insulating layer 18.
[0071] Next, a tungsten film 70 is formed on the aluminum nitride film 68 (FIG. 14). The tungsten film 70 is formed by, for example, a CVD method. The tungsten film 70 will eventually become the word lines WL.
[0072] When forming the tungsten film 70, for example, diborane (B2H6) and tungsten hexafluoride (WF6) are used as source gases.
[0073] By the above manufacturing method, the memory cell array 100 of the semiconductor memory device of the first embodiment is manufactured.
[0074] Next, the operation and effects of the semiconductor memory device of the first embodiment will be described.
[0075] Fig. 15 is a schematic cross-sectional view of a memory cell in a semiconductor memory device of a comparative example of the first embodiment, which corresponds to Fig. 3 of the semiconductor memory device of the first embodiment.
[0076] The semiconductor memory device of the comparative example differs from the semiconductor memory device of the first embodiment shown in FIG. 3 in that the first block insulating layer 18 does not include the amorphous second region 18b, and in that a barrier metal layer 21 is provided between the first block insulating layer 18 and the word line WL.
[0077] The barrier metal layer 21 is a metal layer. The barrier metal layer 21 contains, for example, titanium (Ti) and nitrogen (N). The barrier metal layer 21 contains, for example, titanium nitride. The barrier metal layer 21 is, for example, a titanium nitride layer. The thickness of the barrier metal layer 21 is, for example, not less than 1 nm and not more than 5 nm.
[0078] Assuming that the distance between two interlayer insulating layers 12 facing each other in the vertical direction (z direction) is constant, the thickness of the word line WL in the vertical direction is reduced by providing the barrier metal layer 21. The electrical resistivity of the barrier metal layer 21 is higher than that of the word line WL.
[0079] If the thickness of the word line WL in the vertical direction is thin, the electrical resistance of the word line WL increases, and for example, there is a risk of delay in the operation of the memory cell transistor MT. If the operation of the memory cell transistor MT is delayed, for example, high-speed operation of the 3D NAND flash memory becomes difficult. Therefore, it is desirable to omit the barrier metal layer 21 and increase the thickness of the word line WL in the vertical direction.
[0080] However, the barrier metal layer 21 has a function of suppressing the diffusion of impurities from the word line WL side to the charge storage layer 16 side. If impurities diffuse from the word line WL side to the charge storage layer 16 side, for example, a leakage current between the charge storage layer 16 and the word line WL increases.
[0081] When the leakage current between the charge storage layer 16 and the word line WL increases, the characteristics of the memory cell deteriorate. When the leakage current between the charge storage layer 16 and the word line WL increases, for example, the charge retention characteristics, erase characteristics, write characteristics, etc. of the memory cell deteriorate.
[0082] The impurities that diffuse from the word line WL side to the charge storage layer 16 side are, for example, boron (B) or fluorine (F) contained in the source gas when the word line WL is formed.
[0083] In the 3D NAND flash memory of the first embodiment, a barrier metal layer is not provided between the first block insulating layer 18 and the word lines WL. Therefore, it is possible to increase the thickness of the word lines WL in the vertical direction. This reduces the electrical resistance of the word lines WL, enabling, for example, high-speed operation of the 3D NAND flash memory.
[0084] In the 3D NAND flash memory of the first embodiment, the first block insulating layer 18 includes the amorphous second region 18b. By including the amorphous second region 18b, the 3D NAND flash memory of the first embodiment suppresses the diffusion of impurities from the word line WL side to the charge storage layer 16 side. Therefore, for example, it is possible to suppress the leakage current between the charge storage layer 16 and the word line WL from increasing. Therefore, it is possible to suppress the deterioration of the characteristics of the memory cell.
[0085] The mechanism by which the amorphous second region 18b suppresses the diffusion of impurities from the word line WL side to the charge storage layer 16 side is not necessarily clear. However, it is considered that the amorphous second region 18b serves as a diffusion barrier for impurities, for example.
[0086] In order to suppress the diffusion of impurities from the word line WL side to the charge storage layer 16 side, the thickness of the second region 18b in the y direction from the semiconductor layer 10 toward the word line WL is preferably 0.1 nm or more, and more preferably 0.2 nm or more.
[0087] From the viewpoint of reducing the electrical resistance of the word line WL, it is preferable that the thickness of the second region 18b is thin. Therefore, the thickness of the second region 18b in the y direction from the semiconductor layer 10 toward the word line WL is preferably 1 nm or less, and more preferably 0.5 nm or less.
[0088] The second region 18b suppresses the diffusion of impurities from the word line WL side to the charge storage layer 16 side, so that the impurity concentration of the second region 18b is higher than the impurity concentration of the first region 18a. For example, the boron atomic concentration of the second region 18b is higher than the boron atomic concentration of the first region 18a. Also, for example, the fluorine atomic concentration of the second region 18b is higher than the fluorine atomic concentration of the first region 18a.
[0089] As described above, according to the first embodiment, it is possible to provide a semiconductor memory device in which the resistance of the word lines is reduced and characteristics can be improved.
[0090] Second embodiment The semiconductor memory device of the second embodiment includes a semiconductor layer extending in a first direction, a gate electrode layer including at least one metal element selected from the group consisting of tungsten (W), molybdenum (Mo), and cobalt (Co), a charge storage layer provided between the semiconductor layer and the gate electrode layer, a first insulating layer including a first region including aluminum (Al) and oxygen (O) provided between the charge storage layer and the gate electrode layer, and a second region provided between the first region and the gate electrode layer, the first region being crystalline and the second region being amorphous, and a metal layer provided between the first insulating layer and the gate electrode layer, in contact with the second region and the gate electrode layer, and including titanium (Ti) and nitrogen (N). The semiconductor memory device of the second embodiment is different from the first embodiment in that it includes a metal layer provided between the first insulating layer and the gate electrode layer. Hereinafter, some of the contents that overlap with the first embodiment will be omitted.
[0091] 16(a) and 16(b) are schematic cross-sectional views of a memory cell array of a semiconductor memory device according to a second embodiment, which correspond to FIGS. 2(a) and 2(b) of the first embodiment.
[0092] Fig. 16(a) is a yz cross-sectional view of the memory cell array 200. Fig. 16(a) is a DD' cross-section of Fig. 16(b). Fig. 16(b) is an xy cross-sectional view of the memory cell array 200. Fig. 16(b) is a CC' cross-section of Fig. 16(a). In Fig. 16(a), the area surrounded by a dashed line is one memory cell.
[0093] Fig. 17 is a schematic cross-sectional view of a memory cell in the semiconductor memory device of the second embodiment, and an enlarged cross-sectional view of a portion of the memory cell.
[0094] As shown in Figures 16(a), 16(b), and 17, the memory cell array 200 includes a word line WL, a semiconductor layer 10, an interlayer insulating layer 12, a tunnel insulating layer 14, a charge storage layer 16, a first block insulating layer 18, a second block insulating layer 19, a core insulating region 20, and a barrier metal layer 21.
[0095] The multiple word lines WL and the multiple interlayer insulating layers 12 form a stack 30. The first block insulating layer 18 includes a first region 18a and a second region 18b.
[0096] The word line WL is an example of a gate electrode layer. The interlayer insulating layer 12 is an example of a fourth insulating layer. The tunnel insulating layer 14 is an example of a third insulating layer. The first block insulating layer 18 is an example of a first insulating layer. The second block insulating layer 19 is an example of a second insulating layer. The barrier metal layer 21 is an example of a metal layer.
[0097] The first block insulating layer 18 includes a first region 18a and a second region 18b. The second region 18b is provided between the word line WL and the first region 18a.
[0098] The first region 18a is an insulating layer. The first region 18a includes aluminum (Al) and oxygen (O). The first region 18a includes aluminum oxide. The first region 18a is, for example, an aluminum oxide layer.
[0099] The first region 18a is crystalline. The first region 18a is, for example, a crystalline aluminum oxide layer.
[0100] The thickness of the first region 18a in the y direction from the semiconductor layer 10 toward the word line WL is, for example, not less than 1 nm and not more than 5 nm.
[0101] The second region 18b is an insulating layer. The second region 18b is, for example, an oxide, an oxynitride, or a nitride. The second region 18b includes at least one element of aluminum (Al), hafnium (Hf), or zirconium (Zr). The second region includes at least one element of oxygen (O) or nitrogen (N).
[0102] The second region 18b includes, for example, aluminum nitride, aluminum oxynitride, aluminum oxide, aluminum silicate, hafnium silicate, nitrogen-doped hafnium silicate, or zirconium silicate. The second region 18b is, for example, an aluminum nitride layer, an aluminum oxynitride layer, an aluminum oxide layer, an aluminum silicate layer, a hafnium silicate layer, a nitrogen-doped hafnium silicate layer, or a zirconium silicate layer.
[0103] The second region 18b is amorphous. The second region 18b is, for example, an amorphous aluminum nitride layer, an amorphous aluminum oxynitride layer, an amorphous aluminum oxide layer, an amorphous aluminum silicate layer, an amorphous hafnium silicate layer, an amorphous nitrogen-doped hafnium silicate layer, or an amorphous zirconium silicate layer.
[0104] The second region 18b includes, for example, boron (B). The boron atomic concentration of the second region 18b is, for example, higher than the boron atomic concentration of the first region 18a.
[0105] The second region 18b contains, for example, fluorine (F). The fluorine atomic concentration of the second region 18b is, for example, higher than the fluorine atomic concentration of the first region 18a.
[0106] The thickness of the second region 18b in the y direction from the semiconductor layer 10 toward the word line WL is thinner than the thickness of the first region 18a in the y direction from the semiconductor layer 10 toward the word line WL. The thickness of the second region 18b in the y direction from the semiconductor layer 10 toward the word line WL is, for example, not less than 0.1 nm and not more than 1 nm.
[0107] The barrier metal layer 21 is provided between the first block insulating layer 18 and the word line WL. The barrier metal layer 21 is provided between the second region 18b and the word line WL. The barrier metal layer 21 contacts the second region 18b. The barrier metal layer 21 contacts the word line WL.
[0108] The barrier metal layer 21 is a metal layer. The barrier metal layer 21 contains, for example, titanium (Ti) and nitrogen (N). The barrier metal layer 21 contains, for example, titanium nitride. The barrier metal layer 21 is, for example, a titanium nitride layer. The thickness of the barrier metal layer 21 is, for example, not less than 1 nm and not more than 5 nm.
[0109] Next, an example of a method for manufacturing the semiconductor memory device according to the second embodiment will be described.
[0110] Figures 18 and 19 are schematic cross-sectional views showing an example of a method for manufacturing the semiconductor memory device of the second embodiment. Figures 18 and 19 each show a cross section corresponding to Figure 16(a). Figures 18 and 19 are views showing an example of a method for manufacturing the memory cell array 200 of the semiconductor memory device.
[0111] An example of a method for manufacturing a semiconductor memory device according to the second embodiment is similar to the example of a method for manufacturing a semiconductor memory device according to the second embodiment up to the formation of the aluminum nitride film 68 on the aluminum oxide film 66.
[0112] Next, a titanium nitride film 69 is formed on the aluminum nitride film 68 (FIG. 18). The titanium nitride film 69 is formed by, for example, an ALD method. The titanium nitride film 69 will eventually become the barrier metal layer 21.
[0113] Next, a tungsten film 70 is formed on the titanium nitride film 69 (FIG. 19). The tungsten film 70 is formed by, for example, a CVD method. The tungsten film 70 will eventually become the word lines WL.
[0114] When forming the tungsten film 70, for example, diborane (B2H6) and tungsten hexafluoride (WF6) are used as source gases.
[0115] Next, the operation and effects of the semiconductor memory device of the second embodiment will be described.
[0116] Fig. 20 is a schematic cross-sectional view of a memory cell in a semiconductor memory device of a comparative example of the second embodiment, which corresponds to Fig. 17 of the semiconductor memory device of the second embodiment.
[0117] The semiconductor memory device of the comparative example differs from the semiconductor memory device of the second embodiment shown in FIG. 17 in that the first block insulating layer 18 does not include the amorphous second region 18b.
[0118] The barrier metal layer 21 has a function of suppressing the diffusion of impurities from the word line WL side to the charge storage layer 16 side. In the semiconductor memory device of the comparative example, the effect of the barrier metal layer 21 in suppressing the diffusion of impurities may be insufficient.
[0119] This causes a problem that, for example, the leakage current between the charge storage layer 16 and the word line WL becomes large. When the leakage current between the charge storage layer 16 and the word line WL becomes large, the characteristics of the memory cell deteriorate. When the leakage current between the charge storage layer 16 and the word line WL becomes large, for example, the charge retention characteristics, erase characteristics, write characteristics, etc. of the memory cell deteriorate.
[0120] The impurities that diffuse from the word line WL side to the charge storage layer 16 side are, for example, boron (B) or fluorine (F) contained in the source gas when the word line WL is formed.
[0121] The reason why the barrier metal layer 21 is insufficient in its effect of suppressing the diffusion of impurities is believed to be that the flatness of the barrier metal layer 21 is insufficient.
[0122] The 3D NAND flash memory of the second embodiment includes the amorphous second region 18b between the first region 18a of the first block insulating layer 18 and the barrier metal layer 21, thereby suppressing the diffusion of impurities from the word line WL side to the charge storage layer 16 side. Therefore, for example, it is possible to suppress an increase in the leakage current between the charge storage layer 16 and the word line WL. Therefore, it is possible to suppress the deterioration of the characteristics of the memory cell.
[0123] Providing the amorphous second region 18b improves the flatness of the barrier metal layer 21. It is believed that the improvement in the flatness of the barrier metal layer 21 improves the effect of the barrier metal layer 21 in suppressing the diffusion of impurities.
[0124] The second region 18b is preferably thick in order to improve the flatness of the barrier metal layer 21 and suppress the diffusion of impurities from the word line WL side to the charge storage layer 16 side. Therefore, the thickness of the second region 18b in the y direction from the semiconductor layer 10 toward the word line WL is preferably 0.1 nm or more, and more preferably 0.2 nm or more.
[0125] From the viewpoint of reducing the electrical resistance of the word line WL, it is preferable that the thickness of the second region 18b is thin. Therefore, the thickness of the second region 18b in the y direction from the semiconductor layer 10 toward the word line WL is preferably 1 nm or less, and more preferably 0.5 nm or less.
[0126] As described above, according to the second embodiment, it is possible to provide a semiconductor memory device in which the diffusion of impurities from the word lines is suppressed and the characteristics can be improved.
[0127] In the first and second embodiments, the interlayer insulating layer 12 is provided between the word lines WL. However, the space between the word lines WL may be, for example, a cavity.
[0128] In the first and second embodiments, the semiconductor layer 10 is surrounded by the word lines WL, but the semiconductor layer 10 may be sandwiched between two divided word lines WL. In this structure, the number of memory cells in the stack 30 can be doubled.
[0129] In the first and second embodiments, a structure in which one semiconductor layer 10 is provided in one memory hole 54 has been described as an example, but a structure in which a plurality of semiconductor layers 10 divided into two or more are provided in one memory hole 54 is also possible. In the case of this structure, it is possible to more than double the number of memory cells in the stack 30.
[0130] Furthermore, in the first and second embodiments, the charge storage layer is an insulating layer, but the charge storage layer may be a conductive layer.
[0131] Although several embodiments of the present invention have been described above, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. For example, components of one embodiment may be replaced or changed with components of another embodiment. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]
[0132] 10 Semiconductor layer 12 Interlayer insulating layer (fourth insulating layer) 14 Tunnel insulating layer (third insulating layer) 16 Charge storage layer 18 First block insulating layer (first insulating layer) 18a First Area 18b Second Area 19 Second block insulating layer (second insulating layer) 21 Barrier metal layer (metal layer) WL Word line (gate electrode layer)
Claims
1. A semiconductor layer extending in a first direction; a gate electrode layer including at least one metal element selected from the group consisting of tungsten (W), molybdenum (Mo), and cobalt (Co); a charge storage layer provided between the semiconductor layer and the gate electrode layer; a first insulating layer provided between the charge storage layer and the gate electrode layer, the first insulating layer including a first region containing aluminum (Al) and oxygen (O), and in contact with the gate electrode layer; A semiconductor memory device comprising:
2. 2. The semiconductor memory device according to claim 1, wherein the first insulating layer includes a second region provided between the first region and the gate electrode layer and in contact with the gate electrode layer, the first region being crystalline and the second region being amorphous.
3. 3. The semiconductor memory device according to claim 2, wherein the second region contains at least one element selected from the group consisting of aluminum (Al), hafnium (Hf), and zirconium (Zr).
4. 4. The semiconductor memory device according to claim 3, wherein the second region contains at least one element selected from the group consisting of oxygen (O) and nitrogen (N).
5. 3. The semiconductor memory device according to claim 2, wherein the second region contains at least one element selected from the group consisting of boron (B) and fluorine (F).
6. 6. The semiconductor memory device according to claim 5, wherein the second region has a higher boron atomic concentration than the first region, or the second region has a higher fluorine atomic concentration than the first region.
7. 3. The semiconductor memory device according to claim 2, wherein the thickness of said second region in a second direction from said semiconductor layer to said gate electrode layer is not less than 0.1 nm and not more than 1 nm.
8. 2. The semiconductor memory device according to claim 1, wherein the thickness of said first region in a second direction from said semiconductor layer to said gate electrode layer is 1 nm or more and 5 nm or less.
9. 2. The semiconductor memory device according to claim 1, further comprising a second insulating layer provided between said charge storage layer and said first insulating layer, said second insulating layer containing silicon (Si) and oxygen (O).
10. 2. The semiconductor memory device according to claim 1, further comprising a third insulating layer provided between said charge storage layer and said semiconductor layer.
11. 2. The semiconductor memory device according to claim 1, further comprising a fourth insulating layer provided in the first direction of the gate electrode layer, the first insulating layer being provided between the gate electrode layer and the fourth insulating layer.
12. A semiconductor layer extending in a first direction; a gate electrode layer including at least one metal element selected from the group consisting of tungsten (W), molybdenum (Mo), and cobalt (Co); a charge storage layer provided between the semiconductor layer and the gate electrode layer; a first insulating layer including a first region provided between the charge storage layer and the gate electrode layer, the first region including aluminum (Al) and oxygen (O), and a second region provided between the first region and the gate electrode layer, the first region being crystalline and the second region being amorphous; a metal layer provided between the first insulating layer and the gate electrode layer, in contact with the second region and the gate electrode layer, and containing titanium (Ti) and nitrogen (N); A semiconductor memory device comprising:
13. 13. The semiconductor memory device according to claim 12, wherein the second region contains at least one element selected from the group consisting of aluminum (Al), hafnium (Hf), and zirconium (Zr).
14. 14. The semiconductor memory device according to claim 13, wherein the second region contains at least one element selected from the group consisting of oxygen (O) and nitrogen (N).
15. 13. The semiconductor memory device according to claim 12, wherein the thickness of the second region in a second direction from the semiconductor layer to the gate electrode layer is not less than 0.1 nm and not more than 1 nm.
16. 13. The semiconductor memory device according to claim 12, wherein the thickness of the first region in a second direction from the semiconductor layer to the gate electrode layer is not less than 1 nm and not more than 5 nm.
17. 13. The semiconductor memory device according to claim 12, further comprising a second insulating layer provided between the charge storage layer and the first insulating layer, the second insulating layer containing silicon (Si) and oxygen (O).
18. 13. The semiconductor memory device according to claim 12, further comprising a third insulating layer provided between the charge storage layer and the semiconductor layer.
19. 13. The semiconductor memory device according to claim 12, further comprising a fourth insulating layer provided in the first direction of the gate electrode layer, the first insulating layer being provided between the gate electrode layer and the fourth insulating layer.
20. 13. The semiconductor memory device according to claim 12, wherein the thickness of the metal layer in a second direction from the semiconductor layer to the gate electrode layer is not less than 1 nm and not more than 5 nm.
Citation Information
Patent Citations
Semiconductor device and method of manufacturing the same
US10566280B2