Semiconductor device
The semiconductor device utilizes a top-gate transistor structure with ion-doped CAAC-OS and aligned source/drain regions to address mobility and resistance issues in existing transistors, achieving stable electrical performance and miniaturization.
Patent Information
- Application Number
- JP2024118681
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2010-12-28
- Filing Date
- 2024-07-24
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2031-12-20
AI Technical Summary
Existing transistors on glass substrates, particularly those using amorphous silicon and polycrystalline silicon, suffer from low field-effect mobility and are not suitable for large-area applications, while oxide semiconductors like zinc oxide and In-Ga-Zn-O based transistors face challenges with short channel effects and contact resistance, affecting electrical characteristics and on-current.
A semiconductor device is developed using a top-gate transistor structure with a CAAC-OS (C-Axis Aligned Crystalline Oxide Semiconductor) film as the channel, where source and drain regions are formed by ion doping, reducing parasitic capacitance and contact resistance, and employing a gate electrode as a mask to align these regions, thereby minimizing short channel effects.
The semiconductor device exhibits stable electrical characteristics with reduced fluctuations, improved on-current, and miniaturization, enhancing performance and reliability.
Smart Images

Figure 2024150662000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device having a circuit including a semiconductor element such as a transistor, and a manufacturing method thereof. For example, power devices, memories, thyristors, and and semiconductor integrated circuits including image sensors, electro-optical devices such as liquid crystal display panels. The present invention relates to electronic equipment incorporating components such as optical devices and light-emitting display devices having light-emitting elements.
[0002] In this specification, a semiconductor device is a device that can function by utilizing semiconductor characteristics. This generally refers to electro-optical devices, light-emitting display devices, semiconductor circuits, and electronic devices, all of which are semiconductor devices. be. [Background technology]
[0003] As typified by liquid crystal display devices, transistors formed on glass substrates are amorphous. It is made of amorphous silicon, polycrystalline silicon, etc. Although the resulting transistor has low field-effect mobility, it can be used on large glass substrates. In addition, although the field effect mobility of a transistor using polycrystalline silicon is high, the glass substrate is However, it has a drawback that it is not suitable for large area applications.
[0004] A transistor using an oxide semiconductor is manufactured in place of a transistor using silicon. Technologies that can be applied to electronic and optical devices are attracting attention. For example, oxide semiconductors Then, transistors were fabricated using zinc oxide and In-Ga-Zn-O oxide, and a display device was The technology used for the switching element of the pixel is disclosed in Patent Document 1 and Patent Document 2. do.
[0005] In Patent Document 3, a staggered transistor using an oxide semiconductor is described. A highly conductive nitride layer is provided between the source and drain regions and the source and drain electrodes as a buffer layer. An oxide semiconductor containing an element is provided, and contacts between the oxide semiconductor and a source electrode and a drain electrode are formed. Techniques for reducing contact resistance have been disclosed.
[0006] In Non-Patent Document 1, a channel region, a source region, and a drain region are formed by self-alignment. A top-gate oxide semiconductor transistor is disclosed. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] JP 2007-123861 A [Patent Document 2] JP 2007-96055 A [Patent Document 3] JP 2010-135774 A [Non-patent literature]
[0008] [Non-Patent Document 1] Jae Chul Park et al., “High performance amorphous oxide thin film transistors with self-aligned top-gate structure” IEDM2009, p191-194 Summary of the Invention [Problem to be solved by the invention]
[0009] To provide a semiconductor device using transistors in which fluctuations in electrical characteristics due to short channel effects are unlikely to occur. One of our goals is to provide
[0010] Another object is to provide a miniaturized semiconductor device.
[0011] Another object is to provide a semiconductor device with improved on-state current. [Means for solving the problem]
[0012] One embodiment of the present invention is a semiconductor device including a pair of second oxide semiconductor regions which are amorphous regions and a pair of second oxide semiconductor regions which are amorphous regions. a first oxide semiconductor region sandwiched between two oxide semiconductor regions; a gate insulating film and a gate electrode provided on the first oxide semiconductor region via the gate insulating film; , and is a semiconductor device having the same.
[0013] The first oxide semiconductor region is non-single crystal and has a triangular shape when viewed from a direction perpendicular to the ab plane. The metal atoms are arranged in a layered structure, and the metal atoms are arranged in a hexagonal or square shape when viewed perpendicular to the c-axis. A material that contains a phase in which metal atoms and oxygen atoms are arranged in layers (also called c-axis orientation). be.
[0014] In this specification, the term "crystals" refers to crystals that are non-single crystals and have a triangular or , has a hexagonal atomic arrangement, and metal atoms are arranged in layers when viewed from a direction perpendicular to the c-axis, or The oxide semiconductor film containing a phase in which metal atoms and oxygen atoms are arranged in layers is called CAAC-OS (C Axis Aligned Crystalline Oxide Semiconductor This is called the uctor membrane.
[0015] CAAC-OS is not a single crystal, but it is also not composed only of amorphous matter. CAAC-OS also contains crystallized parts (crystalline parts), but one crystalline part and another In some cases, the boundaries of the crystal parts cannot be clearly distinguished. may be substituted with nitrogen. The c-axes of the individual crystal parts constituting the CAAC-OS are aligned in the same direction. The direction of the CAAC-OS is determined by the surface of the substrate supporting the CAAC-OS, the surface of the CAAC-OS, the film surface, the boundary, etc. Alternatively, the individual bonds constituting the CAAC-OS may be aligned in a direction perpendicular to the surface. The normal to the ab plane of the crystal part is in a certain direction (for example, perpendicular to the substrate surface, surface, film surface, interface, etc.) ) may be facing in the opposite direction.
[0016] CAAC-OS can be a conductor, a semiconductor, or an insulator depending on its composition. Also, depending on the composition, etc., they may be transparent or opaque to visible light. An example of such a CAAC-OS is a film-like CAAC-OS that is formed on the film surface or substrate. When observed from a direction perpendicular to the plate surface or interface, a triangular or hexagonal atomic arrangement is observed. When the cross section of the film is observed, metal atoms, or metal atoms and oxygen atoms (or Also included are materials in which a layered arrangement of atoms (atoms) such as nitrogen atoms is observed.
[0017] The oxide semiconductor film contains two or more elements selected from the group consisting of In, Ga, Sn, and Zn. This can be done.
[0018] The pair of second oxide semiconductor regions serves as a source region and a drain region of the transistor. The oxide semiconductor region 1 serves as a channel region of a transistor.
[0019] In a top-gate transistor using an oxide semiconductor film for a channel region, The source region and the drain region are formed by adding ions to the oxide semiconductor film using the gate electrode as a mask. The source and drain regions are formed by using the gate electrode as a mask. As a result, the source region and the drain region do not overlap with the gate electrode. This reduces parasitic capacitance, enabling the transistor to operate at high speed. .
[0020] In a bottom-gate transistor using an oxide semiconductor film for a channel region, The source and drain regions are formed by etching an oxide semiconductor using an insulating film as a channel protection film as a mask. The insulating film that serves as the channel protection film is made of an oxide semiconductor. The back channel portion of the film is protected by a silicon oxide, silicon nitride, or oxide. A material selected from aluminum, aluminum nitride, etc. is used as a single layer or laminated layer. It is preferable to use it in this manner.
[0021] Furthermore, by forming the source region and the drain region as described above, an oxide semiconductor To reduce the contact resistance between the body film and wiring materials such as source and drain electrodes. This makes it possible to improve the on-state current of the transistor.
[0022] The ion doping for forming the source and drain regions of the transistor is carried out by ion doping. The doping method or the ion implantation method can be used. The ions used are one or more of the group 15 elements such as nitrogen, phosphorus, or arsenic. There can be.
[0023] Furthermore, by adding the ions, the ions contained in the source region and the drain region are The amount of on is 5 x 10 18 atoms / cm 3More than 1×10 22 atoms / cm 3 below As the concentration of the added ions increases, the second oxide semiconductor region The carrier density can be increased, but if the concentration of added ions is too high, the carriers This inhibits the movement of the metal, and actually reduces the conductivity.
[0024] In addition, ions are added to the oxide semiconductor film when the oxide semiconductor film is exposed or when the oxide semiconductor film is in an oxidized state. The process can be carried out in either a state where an insulating film or the like is formed to cover the semiconductor film. .
[0025] Furthermore, the ion addition may be performed by an ion doping method or an ion implantation method. For example, the element to be added can be added in a gas atmosphere containing the element to be added. By generating plasma in the atmosphere and treating the additive with plasma, The plasma generating device may be a dry etchant. A CVD apparatus, a plasma CVD apparatus, a high density plasma CVD apparatus, or the like can be used.
[0026] After the ion addition, a heat treatment may be performed. A temperature at which the in-region does not crystallize is preferred.
[0027] The band gap of the second oxide semiconductor region to which ions are added may be narrowed. In that case, the second oxide semiconductor region is used for the source region and the drain region. Therefore, the band edge of the channel made of the first oxide semiconductor region to which ions are not added is On the other hand, the source and drain regions are made of metal. In the case where the first oxide semiconductor region is provided at the first gate electrode, the band edge of the channel is bent. This tendency is seen in transistors where the effective channel length becomes shorter. This is more pronounced when the channel length is short. By using the region as the source region and the drain region, the short channel effect can be suppressed. This can be done.
[0028] The second oxide semiconductor region to which ions are added is used as a source region and a drain region of a transistor. By forming the source and drain regions as the contact regions, the contact between the wiring and the source and drain regions can be improved. Since the resistance of the transistor can be reduced, the on-state current of the transistor can be increased. Effect of the Invention
[0029] According to one embodiment of the present invention, a transistor in which fluctuations in electrical characteristics due to short channel effects are unlikely to occur is provided. It is also possible to provide a semiconductor device using the same. Furthermore, it is possible to provide a semiconductor device with improved on-state current. [Brief description of the drawings]
[0030] [Figure 1] 1A and 1B are a top view and a cross-sectional view illustrating an example of a semiconductor device which is one embodiment of the present invention. [Diagram 2] 1A to 1C are cross-sectional views illustrating an example of a manufacturing process of a semiconductor device according to one embodiment of the present invention. [Diagram 3] FIG. 1 is a cross-sectional view illustrating an example of a semiconductor device according to one embodiment of the present invention. [Figure 4] 1A to 1C are cross-sectional views illustrating an example of a manufacturing process of a semiconductor device according to one embodiment of the present invention. [Diagram 5] FIG. 1 is a cross-sectional view illustrating an example of a semiconductor device according to one embodiment of the present invention. [Figure 6]1A to 1C are cross-sectional views illustrating an example of a manufacturing process of a semiconductor device according to one embodiment of the present invention. [Figure 7] FIG. 1 is a cross-sectional view illustrating an example of a semiconductor device according to one embodiment of the present invention. [Figure 8] FIG. 1 is a cross-sectional view illustrating an example of a semiconductor device according to one embodiment of the present invention. [Figure 9] 1A to 1C are diagrams illustrating band structures of an oxide semiconductor and a metal material. [Figure 10] FIG. 1 is an example of a circuit diagram illustrating one embodiment of the present invention. [Figure 11] FIG. 1 is an example of a circuit diagram illustrating one embodiment of the present invention. [Figure 12] FIG. 1 is an example of a circuit diagram illustrating one embodiment of the present invention. [Figure 13] FIG. 1 is an example of a circuit diagram illustrating one embodiment of the present invention. [Figure 14] FIG. 2 is a block diagram showing a specific example of a CPU and a circuit diagram of a portion thereof. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] The present invention will be described in detail with reference to the drawings. The present invention is not limited to the above embodiment, and various modifications and variations in form and detail are possible without departing from the spirit and scope of the present invention. It will be readily understood by those skilled in the art that various modifications may be made thereto. The present invention is not limited to the description of the embodiments. In the configuration, the same parts or parts having similar functions are denoted by the same reference numerals in different drawings. These are commonly used, and their repeated explanations will be omitted.
[0032] In each figure described in this specification, the size, thickness, or area of each component is not clearly indicated. may be exaggerated for clarity and are not necessarily limited to scale .
[0033] In addition, the terms "first," "second," "third," etc., used in this specification are used interchangeably to avoid confusion of components. The number is not limited to the number of the first one. For example, "first one" can be changed to " The terms "second" or "third" can be used interchangeably to explain the present invention.
[0034] (Embodiment 1) In this embodiment, a first oxide semiconductor to which ions are not added will be described with reference to FIGS. In a top-gate transistor having a channel region made of a region, The source region and the drain region are formed in a second oxide semiconductor region to which ions are added. An example of the configuration of the rain region will be described.
[0035] FIG. 1 is a top view and a cross-sectional view of a transistor having a top gate structure. 1(B) and 1(C) are cross-sectional views taken along the line AB in FIG. 1(A), respectively. In FIG. 1(A), the cross-sectional view is taken along the plane C and the plane D to avoid complication. In order to achieve this, some of the components of the transistor 151 (for example, the gate insulating film 112, the interlayer insulating film The membrane 124, etc. are omitted.
[0036] The transistor 151 illustrated in FIG. 1 includes a first oxide semiconductor region 126 and a pair of The oxide semiconductor film 190 includes the second oxide semiconductor region 122. a gate insulating film 112 on the upper side, a gate electrode 114 on the gate insulating film 112, and a gate insulating film 112 and the gate electrode 114, and an interlayer insulating film 124 provided thereon. A wiring that connects the pair of second oxide semiconductor regions 122 in the contact hole 130 In this embodiment, the insulating surface is a substrate 10. 1. A case where a base insulating film 102 is provided on the insulating film 100 will be described.
[0037] Here, the pair of second oxide semiconductor regions 122 corresponds to the source region and the drain region of the transistor 151. The first oxide semiconductor region 126 serves as a drain region, and the first oxide semiconductor region 126 serves as a channel region of the transistor 151. It becomes an area.
[0038] The oxide semiconductor region includes a first oxide semiconductor region and a pair of second oxide semiconductor regions. The conductive film 190 is made of a material containing two or more elements selected from the group consisting of In, Ga, Sn, and Zn. For example, the oxide semiconductor film 190 may be an In—Ga—Zn—O-based oxide semiconductor. .
[0039] The first oxide semiconductor region 126 is made of CAAC-OS.
[0040] The pair of second oxide semiconductor regions 122 are amorphous regions. The region 122 contains at least one of the group 15 elements such as nitrogen, phosphorus, or arsenic. It contains 5×10 18 atoms / cm 3 More than 1×10 22 atom s / cm 3 It is preferable that:
[0041] The pair of second oxide semiconductor regions 122 has a conductivity of 10 S / cm or more and 1000 S / cm or more. The electrical conductivity is too low, and preferably 100 S / cm to 1000 S / cm. If the conductivity is too high, the on-state current of the transistor will decrease. This reduces the influence of an electric field generated in the pair of second oxide semiconductor regions 122, thereby reducing the short circuit. The channel effect can be suppressed.
[0042] The material of the interlayer insulating film 124 is, for example, silicon oxide, silicon oxynitride, or silicon nitride oxide. Silicon nitride, aluminum oxide, or the like may be used, and the insulating film may be provided as a laminated layer or a single layer. For example, it may be formed by a thermal oxidation method, a CVD method, a sputtering method, or the like. Preferably, the interlayer insulating film 124 is a silicon nitride film or a silicon oxynitride film.
[0043] The wiring 116 may have a structure similar to that of the gate electrode 114 described later.
[0044] With such a structure, the gate electrode 114 and the pair of second oxide semiconductor regions There is almost no parasitic capacitance between the transistor and the region 122, and the transistor can be miniaturized and the channel length can be reduced. Even if the size of the second oxide film is reduced, the variation in the threshold voltage can be reduced. The contact resistance between the semiconductor region 122 and the wiring 116 is reduced, and the on-state voltage of the transistor is increased. In addition, the hydrogen concentration in the first oxide semiconductor region 126 can be reduced. As a result, the electrical characteristics and reliability of the transistor can be improved.
[0045] Although not shown, the gate insulating film 112 is formed only on the first oxide semiconductor region 126. In addition, a structure in which the second oxide semiconductor regions 122 are not covered by the insulating film 122 may be used.
[0046] <An example of how to fabricate a transistor> Next, a manufacturing method of the transistor shown in FIGS. 1A to 1C will be described with reference to FIGS.
[0047] First, as shown in FIG. 2(A), a base insulating film 102 is formed on a substrate 100.
[0048] There is no particular restriction on the material of the substrate 100, but it should be at least strong enough to withstand the subsequent heat treatment. It is necessary to have heat resistance. For example, glass substrate, ceramic substrate, quartz substrate, surface treatment substrate, etc. A single crystal semiconductor substrate such as silicon or silicon carbide may also be used. , polycrystalline semiconductor substrates, compound semiconductor substrates such as silicon germanium and gallium nitride, S It is also possible to use OI substrates, and semiconductor elements are provided on these substrates. may be used as the substrate 100.
[0049] A flexible substrate may be used as the substrate 100. In this case, the transistors may be fabricated directly on the flexible substrate, or may be attached to another substrate. After the transistor is formed, it may be peeled off and transferred to a flexible substrate. In order to peel off the transistor and transfer it to a flexible substrate, a peeling layer is provided between the transistor and the other substrate. It is advisable to set up the following.
[0050] The base insulating film 102 may be a silicon oxide film, a silicon oxynitride film, a silicon nitride oxide film, or a nitride A single layer or a multilayer of a silicon film or an aluminum oxide film may be used.
[0051] Here, silicon oxynitride is a material whose composition contains more oxygen than nitrogen. For example, oxygen is 50 atomic % or more and 70 atomic % or less, nitrogen is 0.5 atomic % or more and 15 atomic % or less. % or less, silicon is 25 atomic % to 35 atomic % or less, and hydrogen is 0 atomic % to 10 atomic % or less Silicon nitride oxide is a material that contains more oxygen than silicon dioxide in its composition. Also indicates that the nitrogen content is high. For example, oxygen is 5 atomic % or more and 30 atomic % or less, and nitrogen is 20 atomic % to 55 atomic %; silicon is 25 atomic % to 35 atomic %; hydrogen is 10 atomic % % or more and 25 atomic % or less. However, the above range is based on the Rutherford method. Rutherford Backscattering Spectrum (RBS) rometry and Hydrogen Forward Scattering (HFS) The content ratio of the constituent elements is , the total of which does not exceed 100 atomic %.
[0052] The base insulating film 102 may be a film from which oxygen is released by heating.
[0053] "Oxygen is released by heating" refers to TDS (Thermal Desorption Spectroscopy: Thermal Desorption Spectroscopy) analysis, oxygen converted to oxygen atoms The emission rate is 1.0×10 18 atoms / cm 3 More than 3.0×10 20 at oms / cm 3 This means that the above is the case.
[0054] Here, the method for measuring the amount of released oxygen converted into oxygen atoms in TDS analysis is as follows: will be explained.
[0055] The amount of gas released during TDS analysis is proportional to the integral value of the spectrum. The amount of gas released is calculated based on the ratio of the integral value of the film spectrum to the reference value of the standard sample. The reference value of the standard sample is the integral of the spectrum of the sample containing a specific atom. is the ratio of the atomic density to the value.
[0056] For example, the results of a TDS analysis of a silicon wafer containing a specific density of hydrogen as a standard sample, From the results of TDS analysis of the insulating film, the amount of oxygen molecules released from the insulating film (N O2 ) is calculated using formula 1. Here, all of the spectra detected at mass number 32 obtained by TDS analysis are It is assumed that the mass number of the molecule is 32. There is CH3OH, but there is no known The oxygen atom isotope with mass number 17, which is not considered here. The abundance ratio of oxygen molecules, including the atomic and mass number 18 oxygen atoms, in nature is Not taken into consideration as it is a very small amount.
[0057] N O2 =N H2 / S H2 ×S O2 ×α (Formula 1)
[0058] N H2 is the density of hydrogen molecules desorbed from the standard sample. H2 is a standard test The integral value of the spectrum obtained when the sample was subjected to TDS analysis. H2 / S H2 Let us assume that S O2 is the integral value of the spectrum obtained by TDS analysis of the insulating film. α is a coefficient that affects the spectral intensity in the TDS analysis. For details of Equation 1, For details, see Japanese Patent Application Laid-Open No. 6-275697. The amount of oxygen released from the insulating film is A thermal desorption analyzer EMD-WA1000S / W manufactured by Electron Science Corporation was used to measure the standard sample and 1×10 16 atoms / cm 3 The measurement was performed using a silicon wafer containing hydrogen atoms. .
[0059] In addition, some of the oxygen is detected as oxygen atoms in the TDS analysis. The ratio of the oxygen molecules can be calculated from the ionization rate of the oxygen molecules. Since the ionization rate of oxygen molecules is included in the calculation, the amount of oxygen atoms released can be calculated by evaluating the amount of oxygen molecules released. It is possible to estimate even if
[0060] In addition, N O2 is the amount of oxygen molecules released. In the case of an insulating film, when converted into oxygen atoms, The amount of oxygen released is twice as much as the amount of oxygen molecules released.
[0061] In the above-mentioned structure, the insulating film from which oxygen is released by heating is silicon oxide (S iO X (X>2)) or silicon oxide (SiO X (X>2) It contains more than twice as many oxygen atoms as silicon atoms per unit volume. The number of silicon atoms and oxygen atoms per volume were measured by Rutherford backscattering spectrometry. value.
[0062] Oxygen is supplied from the base insulating film to the oxide semiconductor film, so that the oxide semiconductor film The interface state of the film can be reduced. As a result, the charge that may be generated due to the operation of the transistor, etc. or the like can be prevented from being trapped at the interface between the base insulating film and the oxide semiconductor film. As a result, a transistor with little deterioration in electrical characteristics can be obtained.
[0063] Furthermore, charges may be generated due to oxygen vacancies in the oxide semiconductor film. Oxygen vacancies in the conductive film cause some of them to become donors and generate electrons as carriers. The threshold voltage of the transistor shifts in the negative direction. This tendency is due to the back channel This is particularly noticeable in the case of oxygen vacancies occurring on the side of the back channel in this embodiment. The oxide semiconductor film is located near the interface between the base insulating film and the oxide semiconductor film. The threshold voltage shifts in the negative direction when sufficient oxygen is released into the membrane. The oxygen vacancies in the oxide semiconductor film, which are the cause of the problem, can be compensated for.
[0064] That is, when oxygen vacancies occur in the oxide semiconductor film, It is difficult to suppress the capture of charges in the insulating film. By providing the insulating film, the interface state between the oxide semiconductor film and the base insulating film and the oxide semiconductor film can be reduced. The oxygen vacancies in the oxide semiconductor film are reduced, and charge trapping at the interface between the oxide semiconductor film and the base insulating film is suppressed. The influence of the above can be reduced.
[0065] Next, the oxide semiconductor film 140 is formed over the base insulating film 102.
[0066] The oxide semiconductor film 140 is formed by sputtering an oxide semiconductor film having a thickness of 1 nm to 50 nm. A mask is formed on the oxide semiconductor film, and then an oxide semiconductor film is formed on the oxide semiconductor film using the mask. It is formed by selectively etching a nitride semiconductor film.
[0067] The mask for etching the oxide semiconductor film is formed by a photolithography process, an inkjet process, and a photolithography process. A deposition method, a printing method, or the like can be used as appropriate. Hot etching or dry etching can be used as appropriate.
[0068] Here, a sputtering apparatus for forming an oxide semiconductor film will be described in detail below. .
[0069] The leakage rate of the treatment chamber for forming the oxide semiconductor film is set to 1×10 -10 Pa·m 3 / second or less It is preferable to set the above to the above, so that impurities in the film are prevented from being introduced during film formation by a sputtering method. It is possible to reduce the contamination.
[0070] To reduce the leak rate, it is necessary to reduce not only external leaks but also internal leaks. An external leak is when gas enters the vacuum system from outside due to a tiny hole or poor seal. Internal leaks are leaks from partitions such as valves in the vacuum system or leaks from internal components. Caused by released gas. Leak rate is 1×10 -10 Pa·m 3 To achieve a maximum of 1 / second Therefore, measures must be taken to prevent both external and internal leaks.
[0071] To reduce external leakage, it is advisable to seal the opening and closing parts of the processing chamber with metal gaskets. Tal gaskets are coated with iron fluoride, aluminum oxide, or chromium oxide. Metal gaskets are preferable. Metal gaskets have higher adhesion than O-rings and are suitable for external rings. In addition, the passivation of iron fluoride, aluminum oxide, chromium oxide, etc. By using a metal material coated with fluorine, the gas released from the metal gasket, including hydrogen, is reduced. This suppresses the internal leakage and reduces the internal leakage.
[0072] The materials that make up the inner walls of the processing chamber are aluminum and chromium, which emit less gas, including hydrogen. , titanium, zirconium, nickel or vanadium. Also, the above materials may be replaced with iron, It may be used by coating an alloy material containing chromium and nickel. The alloy material containing the alloy is rigid, heat resistant, and easy to process. In order to reduce the area, reducing the surface irregularities of the components by polishing, etc., will reduce the amount of gas released. Alternatively, the components of the above-mentioned film forming apparatus can be replaced with iron fluoride, aluminum oxide, chromium oxide, etc. Alternatively, the material may be covered with a passivating material such as SiO 2 .
[0073] Furthermore, a sputtering gas refiner can be provided immediately before the sputtering gas is introduced into the processing chamber. In this case, the length of the pipe from the refiner to the treatment chamber is 5 m or less, preferably 1 m or less. By keeping the length of the piping to 5m or less or 1m or less, the effect of gas released from the piping is reduced. The reverberation can be reduced depending on the length.
[0074] The exhaust of the processing chamber is performed by a roughing pump such as a dry pump, a sputter ion pump, and a turbo pump. It is advisable to use a suitable combination of a sub-pump and a high vacuum pump such as a cryopump. While the polymer pump is excellent at pumping large molecules, it has a low ability to pump hydrogen and water. Therefore, a cryopump with high water pumping capacity and a sputter ion pump with high hydrogen pumping capacity are Combining these groups is effective.
[0075] Adsorbates present inside the treatment chamber are adsorbed to the inner wall and do not affect the pressure in the treatment chamber. However, this causes gas emission when the processing chamber is evacuated. Therefore, the leak rate and the exhaust speed are Although there is no correlation, a pump with high exhaust capacity is used to remove as much of the adsorbed matter as possible from the treatment chamber. It is important to evacuate the treatment chamber beforehand. Baking is also possible. Baking increases the desorption rate of adsorbed substances by about 10 times. Baking can be performed at temperatures between 100°C and 450°C. By removing adsorbed substances while introducing gas, water and other substances that are difficult to remove by exhausting alone can be removed. The speed can be further increased.
[0076] In the sputtering method, the power supply for generating plasma is an RF power supply, A A C power supply unit, a DC power supply unit, etc. can be used as appropriate.
[0077] The target may be a metal oxide target containing zinc. Examples of the oxides include the quaternary metal oxide In-Sn-Ga-Zn-O system and the ternary metal oxide In-Ga-Zn-O metal oxide and In-Sn-Zn-O metal oxide are compound, In-Al-Zn-O metal oxide, Sn-Ga-Zn-O metal oxide, Al- Ga-Zn-O metal oxides, Sn-Al-Zn-O metal oxides, and binary metal oxides The targets used are In-Zn-O metal oxide and Sn-Zn-O metal oxide. There can be.
[0078] As an example of the target, a metal oxide target containing In, Ga, and Zn is used. The composition ratio is O3:Ga2O3:ZnO=1:1:1 [molar ratio]. In2O A target having a composition ratio of 3:Ga2O3:ZnO=1:1:2 [molar ratio], The target has a composition ratio of In2O3:Ga2O3:ZnO=1:1:4 [molar ratio]. The composition ratio of In2O3:Ga2O3:ZnO=2:1:8 [molar ratio] A target can also be used.
[0079] The sputtering gas is a rare gas (typically argon), oxygen, or a mixture of a rare gas and oxygen. A mixed gas is appropriately used. The sputtering gas may contain hydrogen, water, hydroxyl or hydrogen. It is preferable to use a high-purity gas from which impurities such as ions have been removed.
[0080] The substrate temperature during film formation is 150° C. or higher and 450° C. or lower, preferably 200° C. or higher and 350° C. or lower. The substrate is heated to 150° C. or higher and 450° C. or lower, preferably 200° C. or higher and 350° C. or lower. By forming the film while heating, it is possible to prevent moisture (including hydrogen) from entering the film. In addition, a CAAC-OS film, which is an oxide semiconductor film containing crystals, can be formed. can.
[0081] Furthermore, after the oxide semiconductor film is formed, the substrate 100 is subjected to a heat treatment to remove oxide from the oxide semiconductor film. At the same time, part of the oxygen contained in the base insulating film 102 is converted into the oxide semiconductor It is preferable that the oxide semiconductor film is diffused in the vicinity of the interface between the oxide semiconductor film and the base insulating film 102. In addition, by performing the heat treatment, a CAAC-OS film with higher crystallinity is formed. It is possible.
[0082] The heat treatment is performed at a temperature such that hydrogen is released from the oxide semiconductor film and the base insulating film 102 is The temperature at which part of the oxygen contained in the oxide semiconductor film is released and diffused into the oxide semiconductor film is preferably set to 100° C. Typically, the temperature is 200° C. or higher and lower than the distortion point of the substrate 100, and preferably 250° C. or higher and 450° C. or higher. Below.
[0083] The heat treatment is carried out using a rapid thermal annealing (RTA) device. By using an RTA device, the temperature of the substrate can be raised above the distortion point for a short period of time. Therefore, the ratio of crystalline regions to amorphous regions is high. The time required to form the compound semiconductor film can be shortened.
[0084] The heat treatment can be carried out in an inert gas atmosphere, typically helium, neon, or arsenic. It is preferable to carry out the treatment in an atmosphere of a rare gas such as argon, xenon, or krypton, or in a nitrogen atmosphere. The treatment may be performed in an oxygen atmosphere or a reduced pressure atmosphere. The treatment time is 3 minutes to 24 hours. As the distance between the electrodes is increased, the ratio of crystalline regions to amorphous regions in the oxide semiconductor film is increased. However, heat treatment for more than 24 hours is not preferred because it leads to a decrease in productivity.
[0085] The method for forming the CAAC-OS film is not limited to the method described in this embodiment. .
[0086] In this manner, in the process of forming the oxide semiconductor film, the pressure in the process chamber and the leak rate in the process chamber are In the above, by suppressing the inclusion of impurities as much as possible, The inclusion of impurities such as hydrogen in the film can be reduced. The diffusion of impurities such as hydrogen into the oxide semiconductor film can be reduced. The hydrogen in the mixture reacts with the oxygen that is bonded to the metal atom to form water, and the oxygen is removed from the lattice. (or the area where oxygen has been removed) will result in defects.
[0087] Therefore, by extremely reducing impurities in the process of forming the oxide semiconductor film, the oxide It is therefore possible to reduce defects in the semiconductor film. The highly purified CAAC-OS is used as the channel region, and a transistor is The change in threshold voltage before and after light irradiation and BT testing is small, so stable electrical properties are achieved. It can have properties.
[0088] Note that a metal oxide that can be used for the oxide semiconductor film has a band gap of 2 eV or more. The band gap is preferably 2.5 eV or more, and more preferably 3 eV or more. By using metal oxide with a wide gap, the off-current of a transistor can be reduced. do.
[0089] Next, the gate insulating film 112 and the gate electrode 114 are formed over the oxide semiconductor film 140 . The gate electrode 114 is formed by forming a conductive film, forming a mask on the conductive film, and then removing the mask. The conductive film is selectively etched using the etching gas.
[0090] The gate insulating film 112 is made of, for example, silicon oxide, silicon oxynitride, silicon nitride oxide, or nitride. Silicon oxide, aluminum oxide, hafnium oxide, gallium oxide, etc. may be used. For example, it is formed by thermal oxidation, CVD, sputtering, etc. The gate insulating film 112 may be a film that releases oxygen when heated. By using a film that releases oxygen by heating as the insulating film 112, the amount of oxygen generated in the oxide semiconductor The element defects can be repaired, and degradation of the electrical characteristics of the transistor can be suppressed.
[0091] The gate insulating film 112 is made of hafnium silicate (HfSiO x ), nitrogen is added Hafnium Silicate (HfSi x O y N z ), nitrogen-doped hafnium aluminium minate (HfAl x O y N z ), hafnium oxide, yttrium oxide and other high- By using high-k materials, gate leakage can be reduced. Silicon, silicon oxynitride, silicon nitride, silicon nitride oxide, aluminum oxide, oxide The laminated structure can be made of one or more of aluminum nitride, gallium oxide, or gallium oxide. The thickness of the gate insulating film 112 is preferably 1 nm or more and 300 nm or less, more preferably 5 nm or less. It is preferable to set the thickness to 50 nm or more.
[0092] The gate electrode 114 may be made of any of a variety of materials including aluminum, chromium, copper, tantalum, titanium, molybdenum, and titanium. or an alloy containing the above-mentioned metal elements, It can be formed by using an alloy of a combination of metal elements. The metal element may be selected from one or more of the following: The electrode 114 may have a single-layer structure or a laminated structure of two or more layers. A single-layer structure of an aluminum film containing titanium, a two-layer structure of a titanium film laminated on an aluminum film, and a titanium nitride structure. A two-layer structure in which a titanium film is laminated on a tungsten film, and a two-layer structure in which a tungsten film is laminated on a titanium nitride film A two-layer structure in which a tungsten film is laminated on a tantalum nitride film, a titanium film and its For example, a three-layer structure is used in which an aluminum film is laminated on a titanium film, and then a titanium film is formed on top of that. do.
[0093] The gate electrode 114 is made of indium tin oxide or indium oxide containing tungsten oxide. oxide, indium zinc oxide with tungsten oxide, indium oxide with titanium oxide Indium tin oxide, indium zinc oxide, silicon oxide are added. A light-transmitting conductive material such as indium tin oxide can also be used. A laminate structure of the above-mentioned light-transmitting conductive material and the above-mentioned metal element may also be used.
[0094] In addition, a material in contact with the gate insulating film 112 is provided between the gate electrode 114 and the gate insulating film 112. As the material layer, a nitrogen-containing In-Ga-Zn-O film, a nitrogen-containing In-Sn-O film, and a nitrogen-containing In-Ga-Zn-O film are used. In-Ga-O films containing nitrogen, In-Zn-O films containing nitrogen, Sn-O films containing nitrogen, It is preferable to provide an In-O film containing nitrogen or a metal nitride film (InN, ZnN, etc.). These films have a work function of 5 eV, preferably 5.5 eV or more, and are suitable for transistor current regulation. The threshold voltage of the switching element can be made positive, so that it is a so-called normally-off switching element. For example, when an In-Ga-Zn-O film containing nitrogen is used, at least The oxide semiconductor film 140 has a higher nitrogen concentration, specifically, an In-Ga-Zn- O membrane is used.
[0095] Next, as shown in FIG. 2B, a process of adding ions 150 to the oxide semiconductor film 140 is performed. conduct.
[0096] The ions 150 are added to the oxide semiconductor film 140 by ion doping or The ion implantation method can be used. At least one of the group 15 elements such as nitrogen, phosphorus, or arsenic is selected. As shown in FIG. 1B, the gate electrode 114 becomes a mask by adding ions 150. In order to dope the ions 150 in a self-aligned manner, the second oxide semiconductor region The first oxide semiconductor region 122 and the first oxide semiconductor region 126, which is a region to which ions are not added, are formed. (See Figure 2(C)).
[0097] Furthermore, the second oxide semiconductor region 122 to which the ions 150 are added is The crystallinity is reduced by the addition of ions, resulting in an amorphous region. By adjusting the conditions of addition, the amount of damage to the oxide semiconductor can be reduced. In this case, the second oxide layer may be formed so as not to be a completely amorphous region. The oxide semiconductor region 122 has a larger amorphous region than the first oxide semiconductor region 126. The area where the overlap is large is called the "area where the overlap is large."
[0098] In addition, the addition of the ions 150 to the oxide semiconductor film 140 causes the oxide semiconductor film 140 to be covered. Although the structure in which an insulating film or the like is formed is shown, the oxide semiconductor film 140 is exposed. In this state, ions 150 may be added.
[0099] Furthermore, the addition of the ions 150 is performed by ion doping or ion implantation. It is also possible to carry out the implantation by a method other than the implantation by the ion implantation method. For example, By generating plasma in a gas atmosphere and performing plasma treatment on the material to be treated, The plasma can be generated by a dry air device. An etching device, a plasma CVD device, a high-density plasma CVD device, etc. can be used. do.
[0100] After the ions 150 are added, a heat treatment may be performed. The temperature is preferably such that the oxide semiconductor region 122 in FIG. 2 is not crystallized.
[0101] Next, as shown in FIG. 2D, an interlayer insulating film is formed on the gate insulating film 112 and the gate electrode 114. A film 124 is formed, and a contact hole 130 is provided in the interlayer insulating film 124. The wiring 116 that connects the pair of second oxide semiconductor regions 122 to the through hole 130 is Form.
[0102] The material of the interlayer insulating film 124 is silicon oxide, silicon oxynitride, silicon nitride oxide, or nitride. Silicon, aluminum oxide, and aluminum nitride can be used as single layers or in laminated layers. The film can be formed by sputtering or CVD. It is preferable to use a material that is difficult to be removed by etching. Specifically, the CVD method is used to deposit silane gas as the main material. Then, a suitable source gas is mixed from nitrogen oxide gas, nitrogen gas, hydrogen gas, and rare gas to form a film. The substrate temperature may be set to 300°C or higher and 550°C or lower. By using silane gas, it is possible to make the material less likely to release oxygen when heated. By using the film as the main material, hydrogen remains in the film, and the hydrogen diffuses to form a pair of second oxide semiconductors. The conductivity of the conductive region 122 can be further increased. The hydrogen concentration in the interlayer insulating film 124 is , 0.1 atomic % or more and 25 atomic % or less may be used.
[0103] The material of the wiring 116 may be similar to that of the gate electrode 114 .
[0104] By using the above process, it is possible to miniaturize transistors and maintain their electrical characteristics even when the channel length is reduced. It is possible to manufacture a transistor using an oxide semiconductor, which has good properties and high reliability. do.
[0105] This embodiment mode can be combined with other embodiment modes as appropriate.
[0106] (Embodiment 2) In this embodiment, an example of a transistor different from the transistor described in Embodiment 1 will be described. This will be explained with reference to FIG. 3 and FIG.
[0107] The transistor 152 shown in FIG. 3 includes a base insulating film 102 on a substrate 100 and a base insulating film 10 2, the source electrode and the drain electrode 216 on the base insulating film 102, and the first oxide semiconductor A pair of second oxide semiconductors connected to the region 226 and the source and drain electrodes 216 The oxide semiconductor film 290 including the region 222 and the gate insulating film 21 on the oxide semiconductor film 290 2, a gate electrode 214 on the gate insulating film 212, and a gate insulating film 212 and a gate electrode The transistor has an interlayer insulating film 224 on the transistor 214 .
[0108] The channel length of the transistor is determined by the distance between the pair of second oxide semiconductor regions 222. When the channel length and the width of the gate electrode 214 are equal to each other, a pair of second oxide semiconductor regions 222 and This is preferable because there is no overlap with the gate electrode 214. However, the channel length and the gate electrode 214 For example, the width of the gate electrode 214 may be greater than the channel length. When the width is narrow, the short channel effect can be reduced by mitigating the concentration of the electric field. .
[0109] <An example of how to fabricate a transistor> Next, a manufacturing method of the transistor shown in FIGS. 3A to 3C will be described with reference to FIGS.
[0110] As shown in FIG. 4(A), a base insulating film 102 is formed on a substrate 100 .
[0111] Next, a source electrode and a drain electrode 216 are formed on the base insulating film 102. An oxide semiconductor film 240 is formed over the oxide semiconductor film 102 and the source and drain electrodes 216. The oxide semiconductor film 240 can be formed in the same manner as the oxide semiconductor film 140 in the first embodiment. Cut.
[0112] Next, a gate insulating film covering the source electrode and drain electrode 216 and the oxide semiconductor film 240 is 212 is formed, and a gate electrode 214 is formed on the gate insulating film 212 .
[0113] Next, as shown in FIG. 4B, a process of adding ions 150 to the oxide semiconductor film 240 is performed. The addition of ions 150 can be performed in the same manner as in the first embodiment. By using the pole 214 as a mask to add ions 150, ions 1 are self-aligned. The second oxide semiconductor region 222 to which the ions 150 are added and the first oxide semiconductor region 223 to which the ions 150 are not added are An oxide semiconductor region 226 can be formed (see FIG. 4C).
[0114] In addition, the addition of the ions 150 to the oxide semiconductor film 240 causes the oxide semiconductor film 240 to be covered. Although the structure in which an insulating film or the like is formed is shown, the oxide semiconductor film 240 is exposed. In this state, ions 150 may be added.
[0115] After the ions 150 are added, a heat treatment may be performed. The temperature is preferably such that the oxide semiconductor region 222 in No. 2 is not crystallized.
[0116] Next, as shown in FIG. 4(D), an interlayer insulating film is formed on the gate insulating film 212 and the gate electrode 214. Although not shown in the figure, a contact hole is formed in the interlayer insulating film 224. In the contact holes, wiring that connects to the source electrode and the drain electrode 216 is formed. A line may be formed.
[0117] By using the above process, it is possible to miniaturize transistors and maintain their electrical characteristics even when the channel length is reduced. It is possible to manufacture a transistor using an oxide semiconductor, which has good properties and high reliability. do.
[0118] This embodiment mode can be combined with other embodiment modes as appropriate.
[0119] (Embodiment 3) In this embodiment, a transistor different from the transistors described in Embodiments 1 and 2 is used. An example of the register will be described with reference to FIGS.
[0120] The transistor 153 shown in FIG. 5 includes a substrate 100 having an insulating surface and a gate electrode on the substrate 100. A gate electrode 314, a gate insulating film 312 on the gate electrode 314, and a gate insulating film 312 The first oxide semiconductor region 326 and the pair of second oxide semiconductor regions 326 are provided over the gate electrode 314. The oxide semiconductor film 390 includes the first oxide semiconductor region 322 and the second oxide semiconductor region 326. and an insulating film 319 provided to overlap the pair of second oxide semiconductor regions 322. The source electrode and drain electrode 316, the insulating film 319 and the source electrode and drain electrode 316 and an interlayer insulating film 324 on the substrate 100. A structure having a base insulating film 102 may also be used.
[0121] The channel length of the transistor is determined by the distance between the pair of second oxide semiconductor regions 322. When the channel length and the width of the gate electrode 314 are equal to each other, a pair of second oxide semiconductor regions 322 and This is preferable because there is no overlap with the gate electrode 314. However, the channel length and the gate electrode 314 For example, the width of the gate electrode 314 may be shorter than the channel length. When the width is narrow, the short channel effect can be reduced by mitigating the concentration of the electric field. .
[0122] <An example of how to fabricate a transistor> Next, a manufacturing method of the transistor shown in FIGS. 5A to 5C will be described with reference to FIGS.
[0123] As shown in FIG. 6(A), a base insulating film 102 is formed on a substrate 100 .
[0124] Next, a gate electrode 314 is formed on the base insulating film 102, and a gate electrode 315 is formed on the base insulating film 102. An insulating film 312 is formed.
[0125] Next, the oxide semiconductor film 340 is formed on the gate insulating film 312. The oxide semiconductor film 140 can be formed in a manner similar to that of the oxide semiconductor film 140 in Embodiment 1. An insulating film 319 overlapping with the gate electrode 314 is formed over the semiconductor film 340 .
[0126] Next, as shown in FIG. 6B, a process of adding ions 150 to the oxide semiconductor film 340 is performed. The addition of the ions 150 can be performed in the same manner as in the first embodiment. By using 19 as a mask and adding 150 ions, the self-aligned ion 15 The second oxide semiconductor region 322 to which ions 150 are added and the first oxide semiconductor region 323 to which ions 150 are not added are Next, a second oxide semiconductor region 322 may be formed on the second oxide semiconductor region 326. Then, a source electrode and a drain electrode 316 are formed on the insulating layer 314 (see FIG. 6C).
[0127] After the ions 150 are added, a heat treatment may be performed. The temperature is preferably such that the oxide semiconductor region 322 in FIG. 2 is not crystallized.
[0128] Next, as shown in FIG. 6D, the insulating film 319, the second oxide semiconductor region 322, the source An interlayer insulating film 324 is formed on the electrode and drain electrode 316. A contact hole is formed in the interlayer insulating film 324, and a source A wiring may be formed to connect to the drain electrode 316 .
[0129] By using the above process, it is possible to miniaturize transistors and maintain their electrical characteristics even when the channel length is reduced. It is possible to manufacture a transistor using an oxide semiconductor, which has good properties and high reliability. do.
[0130] This embodiment mode can be combined with other embodiment modes as appropriate.
[0131] (Embodiment 4) In this embodiment, a resistor element using an oxide semiconductor to which ions are added will be described with reference to FIG. He explains.
[0132] FIG. 7A shows a substrate 100 having an insulating surface and an ion-doped semiconductor device provided on the substrate 100. The oxide semiconductor film 401 is used as a resistor, and a conductive film 403 is formed in contact with the oxide semiconductor film 401. The resistor element 410 is formed by providing an oxide semiconductor having ions added thereto. The film 401 is formed in a manner similar to that of the second oxide semiconductor region 222 described in Embodiment 2. The conductive film 403 can be formed of the same material as the source and drain electrodes 216. In this embodiment, the base insulating film 102 is formed on the substrate 100. has been formed.
[0133] FIG. 7B shows a substrate 100 having an insulating surface and an ion-doped semiconductor layer provided on the substrate 100. The oxide semiconductor film 421 is used as a resistor, and an insulating film 425 is formed in contact with the oxide semiconductor film 421. The insulating film 425 and part of the oxide semiconductor film 421 are in contact with each other to form a conductive film 42 3. The resistor element 420 formed by providing an ion-doped oxide semiconductor The conductive film 421 is formed in a manner similar to that of the second oxide semiconductor region 222 described in Embodiment 2. The insulating film 425 can be formed using the same material as the gate insulating film 212. The conductive film 423 can be formed using a material similar to that of the source and drain electrodes 216. By forming the resistor element 420 in this manner, The distance between the conductive films in the resistor element can be made constant, and the resistance value of the resistor element can be set with higher accuracy. In this embodiment, a base insulating film 10 is formed on the substrate 100. 2 is formed.
[0134] (Embodiment 5) In this embodiment, a method for forming an oxide semiconductor film, which is a CAAC-OS film, will be described. Methods other than those used in the first to fourth embodiments will be described below.
[0135] First, a first oxide semiconductor film is formed in contact with an insulating film on a substrate. is from one atomic layer to 10 nm, preferably from 2 nm to 5 nm.
[0136] When the first oxide semiconductor film is formed, the substrate temperature is set to 150° C. or higher and 450° C. or lower, preferably 20 The temperature is preferably 0° C. or more and 350° C. or less. It is possible to reduce the amount of impurities such as moisture (including hydrogen) contained in the film. In addition, the crystallinity of the first oxide semiconductor film can be improved. A compound semiconductor film can be formed.
[0137] Next, after the first oxide semiconductor film is formed, a first heat treatment may be performed. This allows moisture (including hydrogen) to be released from the first oxide semiconductor film. By carrying out the first heat treatment, the crystallinity can be improved. The first heat treatment can form a CAAC-OS film. The temperature is set to be lower than the strain point of the plate, preferably 250°C or higher and 450°C or lower.
[0138] The first heat treatment is performed using a rapid thermal anneal (RTA) device. By using an RTA device, the temperature of the substrate can be raised above the distortion point for a short period of time. Therefore, the ratio of crystalline regions to amorphous regions is high. The time required to form the compound semiconductor film can be shortened.
[0139] The first heat treatment can be performed in an inert gas atmosphere, typically, helium, neodymium, or the like. It is preferable to carry out the treatment in an atmosphere of a rare gas such as argon, xenon, or krypton, or in a nitrogen atmosphere. The treatment may be performed in an oxygen atmosphere or a reduced pressure atmosphere. The treatment time is 3 minutes to 24 hours. As the treatment time is increased, an oxide semiconductor film having a higher ratio of crystalline regions to amorphous regions is formed. However, heat treatment for more than 24 hours is not recommended because it reduces productivity. .
[0140] Next, a second oxide semiconductor film is formed over the first oxide semiconductor film to form an oxide semiconductor stack. The second oxide semiconductor film is formed by a method similar to that for the first oxide semiconductor film. can be done.
[0141] When the second oxide semiconductor film is formed, the substrate is heated during the film formation, so that the first oxide semiconductor film is The second oxide semiconductor film can be crystallized using the conductive film as a seed crystal. The first oxide semiconductor film and the second oxide semiconductor film are formed of the same elements, which is called homoepitaxial growth. Alternatively, the first oxide semiconductor film and the second oxide semiconductor film are grown at least partially. When a layer is made up of at least one different element, it is called heteroepitaxial growth.
[0142] Note that a second heat treatment may be performed after the second oxide semiconductor film is formed. The treatment may be performed in the same manner as the first heat treatment. In this case, the ratio of crystalline regions to amorphous regions in the oxide semiconductor stack can be increased. Alternatively, the second heat treatment is performed to grow a second oxide semiconductor film using the first oxide semiconductor film as a seed crystal. At this time, the first oxide semiconductor film and the second oxide semiconductor film can be crystallized. The compound semiconductor film may be homoepitaxially grown by being composed of the same elements. Alternatively, the first oxide semiconductor film and the second oxide semiconductor film have at least one different element. Heteroepitaxial growth composed of elements may also be used.
[0143] Through the above method, an oxide semiconductor film that is a CAAC-OS film can be formed.
[0144] (Embodiment 6) In this embodiment, a transistor using the oxide semiconductor film described in any of Embodiments 1 to 3 will be described. The effect of this on the electrical characteristics of the transistor will be explained using a band diagram.
[0145] FIG. 9 is a schematic diagram showing an energy band diagram of the transistor shown in FIG. FIG. 8 is the same as or equivalent to FIG. 3 shown in the second embodiment. In contrast, Figure 9(B) shows the case where the voltage between the source and drain is equipotential (Vd = 0V). FIG. 8 illustrates a first oxide semiconductor region (referred to as OS1) and a pair of second oxide semiconductor regions. The oxide semiconductor film is made of a body region (referred to as OS2), and the source electrode and the drain electrode (me The transistor is formed of a GaN-type GaN layer.
[0146] The channel of the transistor in FIG. 8 is formed by OS1. By removing and desorbing as much impurities as possible, such as moisture (including hydrogen), The semiconductor is made of an oxide semiconductor that is more intrinsic (I-type) or as close to intrinsic as possible. By doing so, the Fermi level (Ef) is the same as the intrinsic Fermi level (Ei). It can be made into a level.
[0147] In addition, the source and drain regions of the transistor in FIG. Like the OS1, the OS2 is formed by removing impurities such as moisture (including hydrogen) from the film. It is made to be true (type I) by removing and desorbing as many impurities as possible to make it highly purified, or The first step is to make the oxide semiconductor as close to intrinsic as possible, and then to add nitrogen, phosphorus, arsenic, or other The alloy is formed by adding ions selected from at least one of the group elements. As a result, the carrier density in OS2 is higher than that in OS1, and the Fermi The position of the potential is close to the conduction band.
[0148] FIG. 9A shows a state where a first oxide semiconductor region (OS1) is in a vacuum state (Evac). , a second oxide semiconductor region (referred to as OS2), and a source electrode and a drain electrode (met al), where IP is the ionization potential and Ea is Electron affinity, Eg is the band gap, Wf is the work function, and Ec is the bottom of the conduction band. , Ev is the top of the valence band, and Ef is the Fermi level. The symbols at the end of each symbol are , 1 indicates OS1, 2 indicates OS2, and m indicates metal. The Wf_m is assumed to be 4.1 eV (e.g., titanium).
[0149] OS1 is a highly purified oxide semiconductor with extremely low carrier density, so Ef_1 is The Ec and Ev are approximately in the middle. Also, OS2 is an n-type oxide with high carrier density. Since it is a semiconductor, Ec_2 and Ef_2 are roughly equal.
[0150] The oxide semiconductor shown in OS1 has a band gap (Eg) of 3.15 eV and an electron affinity (E a) is said to be 4.3 eV. The oxide semiconductor shown in OS2 has a The band gap (Eg) can be made smaller than 3.15. Since there is almost no change in the ionization potential, the electron affinity increases as a result. In 9(A), we show the case where Eg is smaller than that of OS1 (i.e., Eg_ 1>Eg_2.)
[0151] As shown in FIG. 9B, the channel OS1 and the source and drain regions When OS2 comes into contact, carriers move so that their Fermi levels match, and The band edge is bent. Furthermore, the metal of the source and drain electrodes, OS2, When they come into contact, the carriers move so that the Fermi levels match, and the OS2 band The end is bent.
[0152] In this way, the OS1 that becomes the channel and the metal that becomes the source electrode and the drain electrode The n-type oxide semiconductor OS2 is formed between the oxide semiconductor and the metal. The contacts can be made ohmic and the contact resistance can be reduced. As a result, the on-state current of the transistor can be increased. This reduces the bending of the band edge of the It can be reduced.
[0153] (Embodiment 7) FIG. 10A is a circuit diagram of a memory element (hereinafter also referred to as a memory cell) constituting a semiconductor device. An example of a memory cell is shown in FIG. A transistor 1160 and a transistor 1162 in which an oxide semiconductor is used for a channel formation region are It is composed of:
[0154] The transistor 1162 in which an oxide semiconductor is used for a channel formation region is It can be produced according to the second embodiment.
[0155] As shown in FIG. 10A, the gate electrode of the transistor 1160 and the The first transistor is electrically connected to one of the source electrode and the drain electrode of the second transistor. What is the wiring (1st Line: also called the source line) and the source electrode of the transistor 1160? , electrically connected to the second wiring (also called the bit line) and the transistor The drain electrode of the capacitor 1160 is electrically connected to the third wiring (3rd Line: also called the first signal line) and the source electrode or drain electrode of the transistor 1162 The other electrode is electrically connected to a fourth wiring (also called a second signal line). The gate electrode of the transistor 1162 is electrically connected to the first gate electrode of the transistor 1162 .
[0156] A transistor using a material other than an oxide semiconductor, for example, single crystal silicon, in the channel formation region. Since the transistor 1160 can operate at a sufficiently high speed, It is possible to read out the stored contents at high speed. The transistor 1162 used in the formation region has a smaller off-state current than the transistor 1160. Therefore, by turning off the transistor 1162, Therefore, the potential of the gate electrode of the transistor 1160 can be held for a very long time. It is Noh.
[0157] By utilizing the feature that the potential of the gate electrode can be maintained, information can be written, It is possible to store and read the information.
[0158] First, writing and holding of information will be described. The transistor 1162 is turned on as a potential at which the transistor 1162 is turned on. As a result, the potential of the third wiring is applied to the gate electrode of the transistor 1160 ( After that, the potential of the fourth wiring is set to a potential at which the transistor 1162 is turned off. By turning off the transistor 1162, the gate of the transistor 1160 is turned on. The potential of the port electrode is maintained (retained).
[0159] Since the off-state current of the transistor 1162 is smaller than that of the transistor 1160, The potential of the gate electrode of the transistor 1160 is maintained for a long time. If the potential of the gate electrode of 1160 is a potential that turns on the transistor 1160, The transistor 1160 is maintained in an on state for a long period of time. If the potential of the gate electrode of the transistor 1160 is a potential that turns off the transistor 1160, For example, transistor 1160 is held off for a long period of time.
[0160] Next, the reading of information will be described. As described above, when the transistor 1160 is in the on state, When the transistor is in the on or off state, a predetermined potential (low potential) is applied to the first wiring. When the transistor 1160 is turned on or off, the potential of the second wiring changes depending on whether the transistor 1160 is turned on or off. For example, when the transistor 1160 is on, the first wiring The potential of the second wiring is lowered relative to the potential of the transistor 1160. In the off state, the potential of the second wiring does not change.
[0161] In this manner, in a state in which the information is held, the potential of the second wiring is compared with a predetermined potential. This allows the information to be read out.
[0162] Next, rewriting of information will be described. Rewriting of information is the same as writing and storing the above information. That is, the potential of the fourth wiring is changed when the transistor 1162 is turned on. This causes the transistor 1162 to be turned on. A potential (a potential related to new information) is applied to the gate electrode of transistor 1160. After that, the potential of the fourth wiring is set to a potential at which the transistor 1162 is turned off. By turning off the starter 1162, the new information is held.
[0163] In this way, the memory cell according to the disclosed invention can directly rewrite information. It is possible to rewrite information. This is why it is necessary for flash memory etc. This eliminates the need for an erase operation, and makes it possible to suppress a decrease in operation speed caused by the erase operation. That is, high speed operation of the semiconductor device having memory cells is realized.
[0164] FIG. 10B shows an example of a circuit diagram of a memory cell which is an extension of the memory cell shown in FIG. 10A. As shown in.
[0165] The memory cell 1100 shown in FIG. 10B includes a first wiring SL (source line) and a second wiring BL (bit line), a third line S1 (first signal line), and a fourth line S2 (second signal line) a fifth wiring WL (word line), a transistor 1164 (first transistor), A transistor 1161 (a second transistor) and a transistor 1163 (a third transistor) The transistor 1164 and the transistor 1163 are A material other than an oxide semiconductor is used for a channel formation region. A semiconductor is used for the channel formation region.
[0166] Here, the gate electrode of the transistor 1164 and the source electrode of the transistor 1161 The first wiring SL is electrically connected to one of the drain electrodes. The source electrode of the transistor 1164 is electrically connected to the drain electrode of the transistor 1164. The electrode and the source electrode of the transistor 1163 are electrically connected to each other. The second wiring BL and the drain electrode of the transistor 1163 are electrically connected to each other. The wiring S1 and the other of the source electrode and the drain electrode of the transistor 1161 are electrically The fourth wiring S2 and the gate electrode of the transistor 1161 are electrically connected to each other. The fifth wiring WL and the gate electrode of the transistor 1163 are electrically connected to each other. do.
[0167] Next, the operation of the circuit will be specifically described.
[0168] When writing data to the memory cell 1100, the first wiring SL is set to 0 V, and the fifth wiring WL is set to The first wiring BL is set to 0 V, the second wiring BL is set to 0 V, and the fourth wiring S2 is set to 2 V. When data "0" is written, the third line S1 is set to 0V. At this time, the transistor 1163 is in an off state and the transistor 1161 is in an on state. Note that, when writing is completed, before the potential of the third wiring S1 changes, The wiring S2 is set to 0 V, so that the transistor 1161 is turned off.
[0169] As a result, after writing data "1", the node connected to the gate electrode of the transistor 1164 After writing data "0", the potential of the node A is about 2V. 0 V. Charges corresponding to the potential of the third wiring S1 are stored in the node A, but The off-state current of the transistor 1161 is a transistor that uses single crystal silicon for the channel formation region. is small compared to the potential of the gate electrode of transistor 1164, and the potential is maintained for a long time. do.
[0170] Next, when reading the memory cell, the first line SL is set to 0 V and the fifth line WL is set to 2 V. V, the fourth wiring S2 is set to 0V, the third wiring S1 is set to 0V, and it is connected to the second wiring BL. At this time, the transistor 1163 is in an on state, and the transistor Start 1161 is turned off.
[0171] If the data is "0", that is, if node A is at about 0V, the transistor 1164 is in an off state. Therefore, the resistance between the second wiring BL and the first wiring SL is high. When the voltage at node A is "1", that is, when the voltage at node A is about 2 V, the transistor 1164 is in an on state. Therefore, the resistance between the second wiring BL and the first wiring SL is low. The data "0" or "1" can be read out based on the difference in the resistance state of the recell. The second wiring BL was set to 0V when the input was made, but it may be in a floating state or charged to a potential of 0V or higher. The third wiring S1 was set to 0V during readout, but it can be set to a floating state. or may be charged to a potential of 0 V or higher.
[0172] Note that data "1" and data "0" are defined for convenience, and may be reversed. The above-mentioned operating voltage is an example. When the data is "1", the transistor 1164 is turned on. In this way, the transistor 1161 is turned on during writing and turned off during other times. Also, if the transistor 1163 is selected to be in the on state during reading, In particular, instead of 2V, the power supply potential VDD of the peripheral logic circuits may be used.
[0173] In this embodiment, for ease of understanding, a memory cell having a minimum storage unit (1 bit) will be described. However, the configuration of the memory cells is not limited to this. For example, the memory cells described above can be connected together to form a more advanced semiconductor device. By using these, it is possible to configure a NAND type or NOR type semiconductor device. The configuration is not limited to that shown in FIG. 10(A) or 10(B) and can be changed as appropriate.
[0174] FIG. 11 shows a block diagram of a semiconductor device according to one embodiment of the present invention having a memory capacity of m×n bits. The circuit diagram is shown.
[0175] The semiconductor device shown in FIG. 11 includes m fifth wirings and fourth wirings, n second wirings and A third wiring and a plurality of memory cells 1100(1, 1) to 1100(m, n) are arranged vertically (in rows and columns). A memory cell array 11 arranged in a matrix of n rows and n columns (m and n are natural numbers). 10, the second wiring and the third wiring driving circuit 1111, the fourth wiring and the fifth wiring driving circuit It is composed of peripheral circuits such as a circuit 1113 and a read circuit 1112. A refresh circuit or the like may be provided as a side circuit.
[0176] Consider memory cell 1100(i, j) as a representative of each memory cell. Rule 1100(i, j) (i is an integer between 1 and m, and j is an integer between 1 and n) is the second The wiring BL(j), the third wiring S1(j), the fifth wiring WL(i) and the fourth wiring S2(i ) and the first wiring. A first wiring potential Vs is applied to the first wiring. In addition, the second wirings BL(1) to BL(n) and the third wirings S1(1) to S 1(n) is a second wiring and a third wiring driver circuit 1111 and a read circuit 1112, The wirings WL(1) to WL(m) and the fourth wirings S2(1) to S2(m) are the fourth wirings and They are each connected to a fifth wiring driver circuit 1113 .
[0177] The operation of the semiconductor device shown in FIG. 11 will be described. In this configuration, writing and reading are performed row by row. Make a payment.
[0178] When writing to the memory cells 1100(i, 1) to 1100(i, n) in the i-th row, The potential Vs of the first wiring WL(i) is set to 0 V, the potential of the fifth wiring WL(i) is set to 0 V, and the potentials of the second wirings BL(1) to BL( The fourth wiring S2(i) is set to 0 V, and the fourth wiring S2(i) is set to 2 V. At this time, the transistor 1161 is turned on. The third wiring S1(1) to S1(n) are in a 2V The column to which data "0" is written is set to 0V. Before the potential of the lines S1(1) to S1(n) changes, the fourth line S2(i) is set to 0 V, The transistor 1161 is turned off. The unselected fifth wiring WL is set to 0 V. The fourth wiring S2 is set to 0V.
[0179] As a result, the gate voltage of the transistor 1164 of the memory cell in which data "1" is written The potential of the node connected to the pole (hereinafter, node A) is about 2V, and data “0” is written. The potential of node A of the selected memory cell is about 0V. The position remains unchanged.
[0180] When reading data from the memory cells 1100(i, 1) to 1100(i, n) in the i-th row, The first wiring potential Vs is 0V, the fifth wiring WL(i) is 2V, and the fourth wiring S2(i) is 0V. The third wirings S1(1) to S1(n) are set to 0 V, and the second wirings BL(1) to BL(n) are set to The connected read circuit is put into an operating state. In the read circuit, for example, the resistance of the memory cell is Depending on the difference in resistance state, data "0" and "1" can be read out. The wiring WL of the first line is set to 0 V, and the unselected fourth line is set to 0 V. Note that the second wiring BL Although the voltage is set to 0V, it may be floating or charged to a potential higher than 0V. The third wiring S1 was set to 0V at the time of discharge, but it may be in a floating state or charged to a potential of 0V or higher. It doesn't matter if it is.
[0181] Note that data "1" and data "0" are defined for convenience, and may be reversed. The above-mentioned operating voltage is an example. When the data is "1", the transistor 1164 is turned on. In this way, the transistor 1161 is turned on during writing and turned off during other times. Also, if the transistor 1163 is selected to be in the on state during reading, In particular, instead of 2V, the power supply potential VDD of the peripheral logic circuits may be used.
[0182] (Embodiment 8) In this embodiment, an example of a circuit diagram of a memory cell having a capacitor is shown. The memory cell 1170 shown in FIG. 1 includes a first wiring SL, a second wiring BL, a third wiring S1, a fourth wiring S2, and a A wiring S2, a fifth wiring WL, a transistor 1171 (a first transistor), and a transistor The transistor 1172 (second transistor) and a capacitor element 1173 . The transistor 1171 includes a material other than an oxide semiconductor in a channel formation region. The transistor 1172 has a channel formation region formed using an oxide semiconductor.
[0183] Here, the gate electrode of the transistor 1171 and the source electrode of the transistor 1172 One of the drain electrodes is electrically connected to one of the electrodes of the capacitor 1173. The first wiring SL and the source electrode of the transistor 1171 are electrically connected to each other. The second wiring BL and the drain electrode of the transistor 1171 are electrically connected to each other. The third wiring S1 and the other of the source electrode and the drain electrode of the transistor 1172 are connected to each other. The fourth wiring S2 and the gate electrode of the transistor 1172 are electrically connected to each other. The fifth wiring WL and the other electrode of the capacitor 1173 are electrically connected to each other. There are.
[0184] Next, the operation of the circuit will be specifically described.
[0185] When writing data to the memory cell 1170, the first wiring SL is set to 0 V, and the fifth wiring WL is set to The first wiring BL is set to 0 V, the second wiring BL is set to 0 V, and the fourth wiring S2 is set to 2 V. When data "0" is written, the third line S1 is set to 0V. At this time, the transistor 1172 is turned on. In this case, before the potential of the third wiring S1 changes, the fourth wiring S2 is set to 0 V, and the transistor The controller 1172 is turned off.
[0186] As a result, after writing data "1", The potential of the node (hereinafter referred to as node A) is about 2V. After writing data “0”, the potential of node A becomes approximately 0V.
[0187] When reading the memory cell 1170, the first wiring SL is set to 0 V, and the fifth wiring WL is set to 2V, the fourth wiring S2 is 0V, the third wiring S1 is 0V, and it is connected to the second wiring BL. The read circuit is put into an operating state. At this time, the transistor 1172 is turned off. .
[0188] The state of the transistor 1171 when the fifth wiring WL is set to 2 V will be described. The potential of the node A that determines the state of the transistor 1171 is determined by the capacitance between the fifth wiring WL and the node A. C1 and the capacitance C2 between the gate electrode, source electrode, and drain electrode of the transistor 1171 It depends.
[0189] Although the third wiring S1 was set to 0V during reading, it may be set to a floating state or a potential of 0V or more. Data "1" and data "0" are just definitions for convenience, and the opposite is true. That's fine.
[0190] The potential of the third wiring S1 during writing is such that the transistor 1172 is turned off after writing. When the WL potential of the fifth wiring is 0 V, the transistor 1171 is in an off state. The potentials of the data "0" and "1" can be selected within the range. When the potential is data "0", the transistor 1171 is turned off, and when the potential is data "1", In this case, the transistor 1171 is selected to be in the on state. The threshold voltage of the transistor 1171 is also an example. Any threshold value may be used as long as it is within the range.
[0191] Also, a selection transistor having a first gate electrode and a second gate electrode; FIG. 12B shows an example of a NOR type semiconductor memory device using a memory cell having He explains.
[0192] The semiconductor device according to one embodiment of the present invention shown in FIG. 12B has a structure in which the i-th row (i is a natural number of 2 or more) A memory cell array having a plurality of memory cells arranged in a matrix in columns (j is a natural number). It is equipped with (i).
[0193] The memory cell array shown in FIG. 12B has i rows (i is a natural number of 3 or more) and j columns (j is a natural number of 3 or more). A plurality of memory cells 1180 arranged in a matrix (a natural number of 1180 x 1180 x 1180 ) and i word lines W L (word lines WL_1 to WL_i), and i capacitance lines CL (capacitance lines CL_1 to a capacitance line CL_i) and i gate lines BGL (gate lines BGL_1 to BGL _i), j bit lines BL (bit lines BL_1 to BL_j), and a source line SL and.
[0194] Further, each of the plurality of memory cells 1180 (memory cell 1180(M,N) (where , N is a natural number between 1 and j, and M is a natural number between 1 and i) is a transistor 1181(M,N), a capacitance element 1183(M,N), and a transistor 1182(M,N ) and.
[0195] In the semiconductor memory device, the capacitance element includes a first capacitance electrode, a second capacitance electrode, and The capacitance element is composed of a dielectric layer overlapping the first capacitance electrode and the second capacitance electrode. Charge is accumulated between the first capacitive electrode and the second capacitive electrode in response to a voltage applied between the first capacitive electrode and the second capacitive electrode.
[0196] The transistor 1181 (M, N) is an N-channel transistor, and has a source electrode, The semiconductor device has a drain electrode, a first gate electrode, and a second gate electrode. In the semiconductor memory device, the transistor 1181 is not necessarily an N-channel transistor. You don't have to.
[0197] One of the source electrode and the drain electrode of the transistor 1181(M,N) is connected to the bit line BL _N, and the first gate electrode of the transistor 1181(M,N) is connected to the word line WL _M, and the second gate electrode of the transistor 1181(M,N) is connected to the gate line BG The source and drain electrodes of the transistor 1181(M,N) are connected to By configuring one of the terminals to be connected to the bit line BL_N, the de- The data can be read out.
[0198] The transistor 1181(M,N) is a selected transistor in the memory cell 1180(M,N). It functions as a register.
[0199] The transistor 1181 (M, N) is a transistor in which an oxide semiconductor is used for a channel formation region. A transistor can be used.
[0200] The transistor 1182 (M, N) is a P-channel transistor. In the semiconductor memory device of the present embodiment, the transistor 1182 is not necessarily a P-channel transistor. It doesn't have to be sta.
[0201] One of the source electrode and the drain electrode of the transistor 1182(M,N) is connected to the source line SL The other of the source electrode and the drain electrode of the transistor 1182(M,N) is connected to The gate electrode of the transistor 1182(M,N) is connected to the bit line BL_N. The other of the source electrode and drain electrode of the transistor 1181(M,N) is connected to the other of the source electrode and drain electrode of the transistor 1181(M,N).
[0202] The transistor 1182(M,N) is an output transistor in the memory cell 1180(M,N). The transistor 1182 (M, N) has a function as a single-ended transistor. A transistor using crystalline silicon for a channel formation region can be used.
[0203] The first capacitance electrode of the capacitance element 1183(M,N) is connected to the capacitance line CL_M. The second capacitance electrode of 1183(M,N) is the source electrode of the transistor 1181(M,N). The other of the drain electrodes is connected to the drain electrode of the capacitor 1183 (M,N). It has the function as follows.
[0204] The voltages of the word lines WL_1 to WL_i are, for example, driven by a decoder. It is controlled by an automatic circuit.
[0205] The voltages of the bit lines BL_1 to BL_j are, for example, It is controlled by an automatic circuit.
[0206] The voltages of the capacitance lines CL_1 to CL_i are respectively controlled by a driving circuit using a decoder, for example. It is controlled by the path.
[0207] The voltages of the gate lines BGL_1 to BGL_i are respectively set by, for example, a gate line driving circuit. It is controlled using a path.
[0208] The gate line driving circuit includes, for example, a diode and a first capacitance electrode, It is configured with a circuit having a capacitive element electrically connected to the gate line BGL.
[0209] By adjusting the voltage of the second gate electrode of the transistor 1181, the transistor 1 The threshold voltage of the transistor 181 can be adjusted. The threshold voltage of the transistor 1181 is adjusted to reduce the source voltage of the transistor 1181 in the off state. Therefore, the current flowing between the source electrode and the drain electrode can be minimized. The data retention period in the circuit can be extended. The voltage required for readout can be made lower than that of conventional semiconductor devices, reducing power consumption. It is possible.
[0210] (Embodiment 9) In this embodiment, an example of a semiconductor device including the transistor described in the above embodiment will be described. This will be explained with reference to FIG.
[0211] FIG. 13(A) shows a so-called DRAM (Dynamic Random Access Memory). An example of a semiconductor device having a structure corresponding to a memory cell shown in FIG. The memory array 1120 has a configuration in which a plurality of memory cells 1130 are arranged in a matrix. The memory cell array 1120 includes m first wirings and n second wirings. In this embodiment, the first wiring is called a bit line BL, and the second wiring is called a The line is called the word line WL.
[0212] The memory cell 1130 includes a transistor 1131 and a capacitor 1132. The gate electrode of the transistor 1131 is connected to the first wiring (word line WL). In addition, one of the source electrode and the drain electrode of the transistor 1131 is connected to the second line (bit line BL), and the source electrode or drain electrode of the transistor 1131 The other of the electrodes is connected to one of the electrodes of the capacitance element. The transistor 1131 is connected to a capacitance line CL and is given a constant potential. The transistor shown in the embodiment is applied.
[0213] The transistor in which an oxide semiconductor is used for a channel formation region, which is described in the above embodiment, The off-state current is smaller than that of a transistor using single crystal silicon for the channel formation region. For this reason, the so-called DRAM shown in FIG. When the transistor is applied to a semiconductor device, a substantially non-volatile memory can be obtained. It is possible.
[0214] Figure 13(B) shows a so-called SRAM (Static Random Access Memory). An example of a semiconductor device having a structure corresponding to the memory cell shown in FIG. The array 1140 is configured such that a plurality of memory cells 1150 are arranged in a matrix. In addition, the memory cell array 1140 includes a first wiring (word line WL), a second The pixel has a plurality of wirings (bit lines BL) and a plurality of third wirings (inverted bit lines / BL).
[0215] The memory cell 1150 includes a first transistor 1151, a second transistor 1152, and a third transistor 1153. A third transistor 1153, a fourth transistor 1154, and a fifth transistor 1155 The first transistor 1151 and the second transistor 1152 are connected to the first and second transistors 1153 and 1154. The transistor 1152 functions as a selection transistor. One of the first transistor 1153 and the fourth transistor 1154 is an n-channel transistor (herein Here, the fourth transistor 1154) and the other is a p-channel transistor (here The third transistor 1153 is the third transistor 1154. The fifth transistor 1154 constitutes a CMOS circuit. A CMOS circuit is formed by a sixth transistor 1155 and a sixth transistor 1156.
[0216] A first transistor 1151, a second transistor 1152, and a fourth transistor 115 The fourth and sixth transistors 1156 are n-channel transistors, and are the same as in the previous embodiment. The third transistor 1153 and the transistor shown in the embodiment can be used. The fifth transistor 1155 is a p-channel transistor including a semiconductor other than an oxide semiconductor. A material such as single crystal silicon is used for the channel formation region.
[0217] The structures, methods, and the like described in this embodiment may be combined as appropriate with the structures, methods, and the like described in other embodiments. They can be used in combination.
[0218] (Embodiment 10) A CPU using at least a part of a transistor in which an oxide semiconductor is used for a channel formation region (Central Processing Unit) can be configured.
[0219] FIG. 14A is a block diagram showing a specific configuration of a CPU. The PU is a logic unit (ALU) on a board 1190. nit) 1191, ALU controller 1192, instruction decoder 1193 , an interrupt controller 1194, a timing controller 1195, and a register 11 96, register controller 1197, bus interface (Bus I / F) 119 8, rewritable ROM 1199, and ROM interface (ROM I / F) 1 The substrate 1190 may be a semiconductor substrate, an SOI substrate, a glass substrate, or the like. The ROM 1199 and the ROM I / F 1189 may be provided on a separate chip. The CPU shown in 14(A) is merely a simplified example of its configuration. There are a wide variety of configurations depending on the application.
[0220] The instructions input to the CPU via the bus interface 1198 are The signal is input to the decoder 1193, decoded, and then passed to the ALU controller 1192, the interface Rupture Controller 1194, Register Controller 1197, Timing Controller Entered into 1195.
[0221] ALU controller 1192, interrupt controller 1194, register controller The controller 1197 and the timing controller 1195 control various Specifically, the ALU controller 1192 controls the operation of the ALU 1191. The interrupt controller 1194 also generates signals for the CPU program. During system execution, interrupt requests from external I / O devices and peripheral circuits are handled according to their priority and mask. The register controller 1197 determines the address of the register 1196 and processes it. It generates addresses and reads and writes to register 1196 depending on the state of the CPU.
[0222] The timing controller 1195 also includes the ALU 1191 and the ALU controller 119 2, an instruction decoder 1193, an interrupt controller 1194, and It generates a signal that controls the operation timing of the register controller 1197. The timing controller 1195 generates an internal clock signal C based on the reference clock signal CLK1. The internal clock generator generates the clock signal CLK2. Supply to the road.
[0223] In the CPU shown in FIG. 14A, a register 1196 is provided with a memory element. The memory element of the master 1196 may be the memory element described in the seventh embodiment. Cut.
[0224] In the CPU shown in FIG. 14A, the register controller 1197 controls the ALU 1191. The holding operation in the register 1196 is selected according to the instruction from the register. In the memory element of the 1196, data is held by a phase inversion element or a capacitance Select whether to hold data by the element. Data retention by the phase inversion element is selected. If the capacitance is set to 0, the power supply voltage is supplied to the storage element in the register 1196. When data retention in the element is selected, data is rewritten to the capacitive element. This allows the supply of power supply voltage to the storage element in the register 1196 to be stopped.
[0225] Regarding the power supply cutoff, as shown in FIG. 14(B) or FIG. 14(C), A switching element is installed between the nodes to which the power supply potential VDD or VSS is applied. The circuits in Fig. 14(B) and Fig. 14(C) are explained below. conduct.
[0226] In FIG. 14B and FIG. 14C, a switch that controls the supply of a power supply potential to a memory element is shown. A memory circuit including a transistor in which an oxide semiconductor is used for a channel formation region, An example is shown below.
[0227] The memory device shown in FIG. 14B includes a switching element 1141 and a memory element 1142. Specifically, each of the memory elements 1142 includes The memory element described in the seventh embodiment can be used. The memory element 1142 is supplied with a high-level power supply potential VD Further, each memory element 1142 in the memory element group 1143 is supplied with a signal D. The potential of the signal IN and the potential of the low-level power supply potential VSS are applied.
[0228] In FIG. 14B, a switching element 1141 is formed by using an oxide semiconductor as a channel formation region. The transistor has a gate electrode connected to the signal Switching is controlled by signal SigA.
[0229] In FIG. 14B, the switching element 1141 has only one transistor. However, there is no particular limitation and a plurality of transistors may be included. When the switching element 1141 has a plurality of transistors functioning as switching elements, The plurality of transistors may be connected in parallel or in series. Alternatively, a combination of series and parallel connections may be used.
[0230] In FIG. 14B, the switching element 1141 changes the The supply of a high-level power supply potential VDD to each memory element 1142 is controlled. Even if the supply of the low-level power supply potential VSS is controlled by the switching element 1141, good.
[0231] In addition, in FIG. 14C, a switch is provided in each memory element 1142 included in the memory element group 1143. A low-level power supply potential VSS is supplied through the switching element 1141. An example is shown in FIG. 1. Each memory element included in the memory element group 1143 is switched by the switching element 1141. The supply of a low-level power supply potential VSS to 1142 can be controlled.
[0232] A switch is provided between the memory element group and a node to which the power supply potential VDD or VSS is applied. When a switching element is provided to temporarily stop the CPU operation and the supply of power voltage is stopped, It is possible to retain data even in a low power state, and power consumption can be reduced. Specifically, for example, a user of a personal computer may input commands to an input device such as a keyboard. Even when you stop inputting information, the CPU can be stopped, reducing power consumption. The power consumption can be reduced.
[0233] Here, we have taken the CPU as an example, but the same can also be said for DSP (Digital Signal Processor). processor), custom LSI, FPGA (Field Programmable Gauge It can also be applied to LSIs such as MOSFET's (MOSFET gate arrays).
[0234] This embodiment mode can be implemented in appropriate combination with any of the above embodiment modes. [Explanation of symbols]
[0235] 100 Substrates 102 Undercoat insulating film 112 Gate insulating film 114 Gate electrode 116 Wiring 122 Oxide Semiconductor Region 124 Interlayer insulating film 126 Oxide Semiconductor Region 130 Contact Hole 140 Oxide Semiconductor Film 150 ions 151 Transistor 152 Transistor 153 Transistor 190 Oxide Semiconductor Film 212 Gate insulating film 214 Gate electrode 216 Drain electrode 222 Oxide semiconductor region 224 Interlayer insulating film 226 Oxide Semiconductor Region 240 Oxide Semiconductor Film 290 Oxide Semiconductor Film 312 Gate insulating film 314 Gate electrode 316 Drain electrode 319 Insulating Film 322 Oxide Semiconductor Region 324 Interlayer insulating film 326 Oxide Semiconductor Region 340 Oxide Semiconductor Film 390 Oxide Semiconductor Film 401 Oxide Semiconductor Film 403 Conductive Film 410 Resistance element 420 Resistance element 421 Oxide Semiconductor Film 423 Conductive Film 425 Insulating Film 1100 memory cells 1110 Memory Cell Array 1111 Wiring drive circuit 1112 Circuit 1113 Wiring drive circuit 1120 Memory Cell Array 1130 Memory Cells 1131 Transistor 1132 Capacitive element 1140 Memory Cell Array 1141 Switching element 1142 Memory element 1143 Memory Element Group 1150 memory cells 1151 Transistor 1152 Transistor 1153 Transistor 1154 Transistor 1155 Transistor 1156 Transistor 1160 Transistor 1161 Transistor 1162 Transistor 1163 Transistor 1164 Transistor 1170 Memory Cells 1171 Transistor 1172 Transistor 1173 Capacitive element 1180 memory cells 1181 Transistor 1182 Transistor 1183 Capacitive element 1189 ROM Interface 1190 Board 1191 ALU 1192 ALU Controller 1193 Instruction Decoder 1194 Interrupt Controller 1195 Timing Controller 1196 Registers 1197 Register Controller 1198 Bus Interface 1199 ROM
Claims
1. A semiconductor device including a first transistor and a second transistor having a channel formation region in silicon, a first oxide semiconductor film and a second oxide semiconductor film each having a single layer are provided over a substrate; the first oxide semiconductor film has a first region, a second region, and a third region; the first region is a channel formation region of the first transistor, the second region does not overlap with a gate electrode of the first transistor and has a higher concentration of nitrogen, phosphorus, or arsenic than the first region; the third region does not overlap with a gate electrode of the first transistor and has a higher concentration of nitrogen, phosphorus, or arsenic than the first region; a source electrode of the first transistor electrically connected to the second region; a drain electrode of the first transistor electrically connected to the third region; the second oxide semiconductor film has a fourth region, the fourth region overlaps with a conductive film via an insulator and has a higher concentration of nitrogen, phosphorus, or arsenic than a channel formation region of the first transistor; the conductive film has the same conductive material as a source electrode of the first transistor and a drain electrode of the first transistor; a source electrode or a drain electrode of the first transistor is electrically connected to the second oxide semiconductor film or the conductive film.
2. A semiconductor device including a first transistor and a second transistor having a channel formation region in silicon, a first oxide semiconductor film and a second oxide semiconductor film each having a single layer are provided over a substrate; the first oxide semiconductor film has a first region, a second region, and a third region; the first region is a channel formation region of the first transistor, The second region does not overlap with the gate electrode of the first transistor, and the concentration of nitrogen, phosphorus, or arsenic is 5×10 18 atoms / cm 3 Above 1 x 10 22 atoms / cm 3 A region where: The third region does not overlap with the gate electrode of the first transistor, and the concentration of nitrogen, phosphorus, or arsenic is 5×10 18 atoms / cm 3 Above 1 x 10 22 atoms / cm 3 A region where: a source electrode of the first transistor electrically connected to the second region; a drain electrode of the first transistor electrically connected to the third region; the second oxide semiconductor film has a fourth region, The fourth region overlaps with the conductive film via an insulator, and the concentration of nitrogen, phosphorus, or arsenic is 5×10 18 atoms / cm 3 Above 1 x 10 22 atoms / cm 3 A region where: the conductive film has the same conductive material as a source electrode of the first transistor and a drain electrode of the first transistor; a source electrode or a drain electrode of the first transistor is electrically connected to the second oxide semiconductor film or the conductive film.
3. A semiconductor device including a first transistor and a second transistor having a channel formation region in silicon, a first oxide semiconductor film having a single layer containing two or more elements selected from In, Ga, Sn, and Zn over a substrate; and a second oxide semiconductor film having a single layer containing two or more elements selected from In, Ga, Sn, and Zn, the first oxide semiconductor film has a first region, a second region, and a third region; the first region is a channel formation region of the first transistor, the second region does not overlap with a gate electrode of the first transistor and has a higher concentration of nitrogen, phosphorus, or arsenic than the first region; the third region does not overlap with a gate electrode of the first transistor and has a higher concentration of nitrogen, phosphorus, or arsenic than the first region; a source electrode of the first transistor electrically connected to the second region; a drain electrode of the first transistor electrically connected to the third region; the second oxide semiconductor film has a fourth region, the fourth region overlaps with a conductive film via an insulator and has a higher concentration of nitrogen, phosphorus, or arsenic than a channel formation region of the first transistor; the conductive film has the same conductive material as a source electrode of the first transistor and a drain electrode of the first transistor; a source electrode or a drain electrode of the first transistor is electrically connected to the second oxide semiconductor film or the conductive film.
4. A semiconductor device including a first transistor and a second transistor having a channel formation region in silicon, a first oxide semiconductor film having a single layer containing two or more elements selected from In, Ga, Sn, and Zn over a substrate; and a second oxide semiconductor film having a single layer containing two or more elements selected from In, Ga, Sn, and Zn, the first oxide semiconductor film has a first region, a second region, and a third region; the first region is a channel formation region of the first transistor, The second region does not overlap with the gate electrode of the first transistor, and the concentration of nitrogen, phosphorus, or arsenic is 5×10 18 atoms / cm 3 Above 1 x 10 22 atoms / cm 3 A region where: The third region does not overlap with the gate electrode of the first transistor, and the concentration of nitrogen, phosphorus, or arsenic is 5×10 18 atoms / cm 3 Above 1 x 10 22 atoms / cm 3 A region where: a source electrode of the first transistor electrically connected to the second region; a drain electrode of the first transistor electrically connected to the third region; the second oxide semiconductor film has a fourth region, The fourth region overlaps with the conductive film via an insulator, and the concentration of nitrogen, phosphorus, or arsenic is 5×10 18 atoms / cm 3 Above 1 x 10 22 atoms / cm 3 A region where: the conductive film has the same conductive material as a source electrode of the first transistor and a drain electrode of the first transistor; a source electrode or a drain electrode of the first transistor is electrically connected to the second oxide semiconductor film or the conductive film.
Citation Information
Patent Citations
Semiconductor device, and method of manufacturing semiconductor device
JP2010141230A
Logic circuit and semiconductor device
JP2010171394A
Semiconductor device and method for manufacturing the same
JP2010258434A
Semiconductor device and method for manufacturing the same
JP2007096055A
Semiconductor device and its manufacturing method
JP2007123861A