Method of piezoelectric element arraying and arrayed piezoelectric element
By forming grooves of varying depths in piezoelectric elements, the method allows multiple frequency outputs from uniform thickness elements, addressing cost and performance limitations in existing arrays.
Patent Information
- Application Number
- JP2023063843
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-11
- Publication Date
- 2024-10-24
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing piezoelectric element arrays require different thicknesses to output multiple frequencies, leading to increased manufacturing costs and limited ablation depth and bandwidth.
Forming parallel grooves of varying depths in piezoelectric elements to adjust frequency output without changing thickness, allowing multiple frequencies from elements of uniform thickness.
Enables multiple frequency outputs from uniform thickness elements, reducing manufacturing costs and achieving wide ablation depth and bandwidth.
Smart Images

Figure 2024150852000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a piezoelectric element arraying method for arraying and dividing a piezoelectric element into a plurality of elements, and to an arrayed piezoelectric element which is a piezoelectric element arrayed and divided into a plurality of elements. [Background technology]
[0002] Ultrasound has been used in a variety of fields for a long time, for example, in the medical field, it is used as High Intensity Focused Ultrasound (HIFU) therapy, which uses ultrasound to heat and destroy tissue deep inside the body to achieve a therapeutic effect. In such cauterization treatments using ultrasound heating, it is required to be able to control the energy level (spot concentration, strength, depth, width) of the cauterization area, and in the future, there is a demand for miniaturization so that it can be inserted into blood vessels and endoscopes.
[0003] In order to meet these demands, arraying and dividing small piezoelectric elements is being considered. In other words, the method involves dividing a polarized piezoelectric element (individual element) into multiple channels by creating grooves using dicing or other methods.
[0004] On the other hand, it has been known for some time that in order to output a plurality of different frequencies from a piezoelectric element, it is necessary to vary the thickness of the piezoelectric element (see, for example, Patent Document 1, etc.). For this reason, even when forming an array of piezoelectric elements, it has been thought that in order to output a plurality of different frequencies, piezoelectric elements with different thicknesses must be used. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Utility Model Application Publication No. 60-40124 Summary of the Invention [Problem to be solved by the invention]
[0006] As described above, in order to array piezoelectric elements to output multiple frequencies, the thickness of the piezoelectric elements must be changed for each frequency, which not only increases manufacturing costs but also makes it impossible to achieve a broadband or broad cauterization depth, since one piezoelectric element can only output one frequency.
[0007] SUMMARY OF THE PRESENT DISCLOSURE An object of the present invention is to provide a piezoelectric element arraying method and an arrayed piezoelectric element that are capable of outputting a plurality of frequencies using piezoelectric elements of the same thickness when arraying piezoelectric elements. [Means for solving the problem]
[0008] In order to achieve the above object, the invention described in claim 1 is a piezoelectric element array method in which a piezoelectric element is divided into a plurality of channels by forming a plurality of grooves in parallel in the piezoelectric element, wherein the depth is defined as the ratio of the depth of the groove to the width of the channel between the grooves, and the depth is adjusted according to the frequency to be output for piezoelectric elements of the same thickness to form the grooves.
[0009] The invention described in claim 2 is an arrayed piezoelectric element in which a plurality of grooves are formed in parallel in a piezoelectric element, dividing the piezoelectric element into a plurality of channels, wherein the depth is defined as the ratio of the depth of the groove to the width of the channel between the grooves, and a single piezoelectric element of the same thickness has a plurality of grooves formed therein with different depths, thereby allowing a plurality of different frequencies to be output.
[0010] The invention described in claim 3 is characterized in that, in the arrayed piezoelectric element described in claim 2, a plurality of the grooves having different depths are arranged so as to obtain predetermined ultrasonic characteristics. Effect of the Invention
[0011] According to the considerations and verifications of the present inventors, it has been confirmed that even if the thickness of the piezoelectric element is the same, different frequencies can be output by changing the ratio of the groove depth to the channel width (width between grooves), i.e., the depth of the groove. For example, when the groove depth is small (the groove is shallow compared to the width), a frequency due to thickness-longitudinal vibration / thickness mode (frequency constant is Nt) is excited and output, and when the groove depth is large (the groove is deep compared to the width), a frequency due to longitudinal vibration / length mode (frequency constant is Nt) is excited and output. 33 ) was excited and output.
[0012] According to the invention described in claim 1, since grooves are formed by adjusting the depth according to the frequency to be output for piezoelectric elements of the same thickness, it becomes possible to output multiple frequencies from piezoelectric elements of the same thickness. Furthermore, when outputting multiple frequencies from an arrayed piezoelectric element, it is not necessary to change the thickness of the piezoelectric element, and it is only necessary to change the depth of the groove, which makes it possible to reduce manufacturing costs.
[0013] According to the invention described in claim 2, since a plurality of grooves with different depths are formed in one piezoelectric element with the same thickness, a plurality of different frequencies are output, so that a single piezoelectric element with a uniform thickness can output a plurality of frequencies. As a result, it is possible to achieve a broadband and a broad cauterization depth by outputting a plurality of frequencies from a single piezoelectric element.
[0014] According to the invention described in claim 3, since a plurality of grooves having different depths are arranged and positioned so as to obtain a predetermined ultrasonic characteristic, it becomes possible to irradiate and use ultrasonic waves having desired characteristics with one piezoelectric element having a uniform thickness. For example, it becomes possible to irradiate ultrasonic waves so that the focal points of a plurality of frequencies coincide with each other, and to effectively cauterize only the treatment area. [Brief description of the drawings]
[0015] [Figure 1]FIG. 1A is a perspective view showing an arrayed piezoelectric element for illustrating a piezoelectric element arraying method according to a first embodiment of the present invention, and FIG. 1B is a front view seen from the direction of the arrow in FIG. [Diagram 2] FIG. 1 is a diagram for explaining a piezoelectric element arraying method according to embodiment 1 of the present invention, showing front views of arrayed piezoelectric elements and impedance values versus frequency in the cases where (a) the groove spacing is wide and the grooves are shallow, (b) the groove spacing is wide and the grooves are deep, (c) the groove spacing is narrow and the grooves are shallow, and (d) the groove spacing is narrow and the grooves are deep. [Diagram 3] FIG. 1 is a diagram for explaining a piezoelectric element array method according to embodiment 1 of the present invention, in which (a) is a perspective view showing the width and height of a channel, and (b) is a diagram showing the relationship between the ratio of the channel height to the width (groove depth) and the output frequency. [Figure 4] FIG. 2 is a diagram showing a front view of an arrayed piezoelectric element when (a) it is caused to output at a first frequency and when (b) it is caused to output at a second frequency in the first embodiment of the present invention, and a diagram showing impedance values versus frequency. [Diagram 5] 10 is a front view showing a first example of an arrayed piezoelectric element in accordance with embodiment 2 of the present invention. FIG. [Figure 6] 10 is a front view showing a second example of an arrayed piezoelectric element in accordance with embodiment 2 of the present invention. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] Hereinafter, the present invention will be described based on the illustrated embodiment.
[0017] (Embodiment 1) 1A is a perspective view of an arrayed piezoelectric element 1 for explaining a piezoelectric element arraying method according to this embodiment, and FIG. 1B is a front view seen from the direction of the arrow in FIG. 1A. The piezoelectric element arraying method is a method of dividing a piezoelectric element 2 into a plurality of channels CH by forming a plurality of grooves 2a in parallel in the piezoelectric element 2, and the arrayed piezoelectric element 1 is a piezoelectric element in which a plurality of grooves 2a are formed in parallel in the piezoelectric element 2, dividing the piezoelectric element 2 into a plurality of channels CH.
[0018] The arrayed piezoelectric element 1 is made of piezoelectric elements (individual elements) 2 made of lead zirconate titanate (PZT) or the like and having a uniform thickness t, which are polarized, and a ground electrode 3 is formed on the lower and lower surfaces of the piezoelectric element 2, and a signal electrode 4 is formed on the upper and upper surfaces of the piezoelectric element 2. A plurality of grooves 2a are formed in parallel on the signal electrode 4 side of the piezoelectric element 2 by dicing or the like, and a channel CH is formed between the grooves 2a.
[0019] Here, the depth of the groove 2a ( The depth of the groove 2a is the ratio (=d / w) of the depth and thickness of the channel CH. Each groove 2a is filled with a resin or the like before use. Note that both ends of the piezoelectric element 2 are not sandwiched between the grooves 2a, but are sandwiched between the groove 2a and the open end, and these both ends also constitute the channel CH.
[0020] In such an arrayed piezoelectric element 1, the inventors of the present application have discovered and confirmed that even if the thickness t of the piezoelectric element 2 is the same, by changing the depth of the grooves 2a, a plurality of different frequencies may be output (the excited frequencies may differ). For example, when the depth of the grooves 2a is small (the grooves 2a are shallow with respect to the width w), a frequency (frequency constant is Nt) due to thickness-longitudinal vibration / thickness mode is excited and output, and when the depth of the grooves 2a is large (the grooves 2a are deep with respect to the width w), a frequency (frequency constant is Nt) due to longitudinal vibration / length mode is excited and output. 33 ) was discovered and confirmed to be excited and output.
[0021] For example, as shown in Fig. 2(a), when the grooves 2a are spaced widely and shallow, i.e., when the depth of the grooves 2a is small, excitation occurs at around 9 MHz. Similarly, as shown in Fig. 2(b), when the grooves 2a are deep but spaced widely, i.e., when the depth of the grooves 2a is small, excitation occurs at around 9 MHz. Furthermore, as shown in Fig. 2(c), when the grooves 2a are spaced narrow but shallow, i.e., when the depth of the grooves 2a is small, excitation occurs at around 9 MHz.
[0022] In contrast, as shown in Fig. 2(d), when the grooves 2a are deep and the interval between them is narrow, that is, when the depth of the grooves 2a is large, the excitation frequency is around 6 MHz. In this way, it was discovered and confirmed that even if the thickness t of the piezoelectric element 2 is the same, two different frequencies can be output by setting the depth of the grooves 2a to a specified value.
[0023] Furthermore, it was verified what value of the depth (d / w) of the groove 2a would result in the output of two different frequencies. That is, as shown in FIG. 3(a), the thickness of the channel CH, i.e., the depth d of the groove 2a, was kept constant, and the width w of the channel CH was changed to change the depth (d / w) of the groove 2a, and the impedance of the channel CH was calculated by simulation to calculate the resonance frequency. As a result, as an example, as shown in FIG. 3(b), it was confirmed that when the depth (d / w) of the groove 2a is 0.4 or less (first depth), a frequency (first frequency) of about 9 MHz is output by thickness longitudinal vibration, and when the depth (d / w) of the groove 2a is 1.5 or more (second depth), a frequency (second frequency) of about 6 MHz is output by longitudinal vibration.
[0024] Based on such considerations and verifications by the inventors of the present application, the piezoelectric element array method according to this embodiment forms grooves 2a by adjusting the depth according to the frequency to be output for piezoelectric elements 2 having the same thickness t. Here, in this embodiment, a case will be described in which the output frequencies are two different frequencies, a first frequency and a second frequency, and thickness longitudinal vibration is excited at the first frequency, and longitudinal vibration is excited at the second frequency. In contrast, the output frequencies may be three or more different frequencies, and vibrations other than thickness longitudinal vibration and longitudinal vibration, such as long side extension vibration and thickness shear vibration, may be excited.
[0025] In this embodiment, when a first frequency is output, the groove 2a is formed at a first depth (for example, a shallow depth), and when a second frequency different from the first frequency is output, the groove 2a is formed at a second depth different from the first depth (for example, a deep depth). For example, as shown in FIG. 4(a), when a first frequency of about 10 MHz is output, the groove 2a is formed at a shallow first depth, and as shown in FIG. 4(b), when a second frequency of about 7 MHz is output, the groove 2a is formed at a deep second depth. Here, as described above, the first depth is set to a value at which thickness longitudinal vibration is performed, and the second depth is set to a value at which longitudinal vibration is performed.
[0026] Thus, according to this piezoelectric element arraying method, when a first frequency is to be output from piezoelectric elements 2 having the same thickness t, grooves 2a are formed at a first depth, and when a second frequency is to be output, grooves 2a are formed at a second depth, making it possible to output two frequencies from piezoelectric elements 2 having the same thickness t. Furthermore, when outputting two frequencies from arrayed piezoelectric elements 1, there is no need to change the thickness t of piezoelectric elements 2, and it is only necessary to change the depth of grooves 2a, making it possible to reduce manufacturing costs.
[0027] That is, when outputting two frequencies by changing the thickness t of the piezoelectric element 2, the piezoelectric elements 2 with different thicknesses t must be polished in two steps, and then the grooves 2a must be formed in each. In contrast, according to this piezoelectric element array method, it is only necessary to polish the piezoelectric elements 2 with the same thickness t in one step, and then form the grooves 2a with different depths, which makes it possible to reduce manufacturing costs.
[0028] (Embodiment 2) 5 is a front view showing an arrayed piezoelectric element 11 according to this embodiment. In this embodiment, a plurality of grooves 2a with different depths are formed in one piezoelectric element 2 having the same (uniform) thickness t, that is, the grooves 2a have a mixture of depths, and the configuration equivalent to that of embodiment 1 is given the same reference numerals and description thereof will be omitted.
[0029] In this embodiment, a case will be described in which grooves 2a of two different depths are formed to output two different frequencies, a first frequency and a second frequency, and thickness longitudinal vibration is excited at the first frequency, and longitudinal vibration is excited at the second frequency. In contrast, grooves 2a of three or more different depths may be formed to output three or more different frequencies, and vibrations other than thickness longitudinal vibration and longitudinal vibration, such as long side extension vibration and thickness shear vibration, may be excited.
[0030] In the arrayed piezoelectric element 11, a groove 2a1 is formed at a first depth (e.g., a shallow depth) in a first channel CH1 that outputs a first frequency, and a groove 2a2 is formed at a second depth (e.g., a deep depth) that is different from the first depth in a second channel CH2 that outputs a second frequency different from the first frequency. In other words, the first channel CH1 in which the groove 2a1 is formed at the first depth outputs the first frequency, and the second channel CH2 in which the groove 2a2 is formed at the second depth outputs the second frequency.
[0031] Furthermore, grooves 2a1 of a first depth and grooves 2a2 of a second depth are arranged so as to obtain a predetermined ultrasonic characteristic. That is, in this embodiment, a plurality of grooves 2a1 of a first depth are formed on one of the left and right sides of the upper surface of the piezoelectric element 2 (left surface) to provide a plurality of first channels CH1, and a plurality of grooves 2a2 of a second depth are formed on the other surface (right surface) to provide a plurality of second channels CH2. This allows for the ultrasonic characteristic of outputting only the first frequency from one side (left surface side) of the piezoelectric element 2 and outputting only the second frequency from the other side (right surface side).
[0032] In contrast to this, depending on the specified / desired ultrasonic characteristics, as in the arrayed piezoelectric element 12 shown in FIG. 6, a plurality of grooves 2a1 of a first depth may be formed in the center of the upper surface of the piezoelectric element 2 to provide a plurality of first channels CH1, and a plurality of grooves 2a2 of a second depth may be formed on both sides of the upper surface to provide a plurality of second channels CH2.
[0033] According to this embodiment, in a single piezoelectric element 2 having the same (uniform) thickness t, a first frequency is output in a first channel CH1 in which grooves 2a1 are formed at a first depth, and a second frequency is output in a second channel CH2 in which grooves 2a2 are formed at a second depth, so that it is possible to output two frequencies with a single piezoelectric element 2 having a uniform thickness t. As a result, it is possible to achieve a broadband and a broad cauterization depth by outputting two frequencies with a single piezoelectric element 2.
[0034] In addition, since grooves 2a1 (first channel CH1 outputting a first frequency) and grooves 2a2 (second channel CH2 outputting a second frequency) are provided at a first depth to obtain predetermined ultrasonic characteristics, it is possible to irradiate and use ultrasonic waves having desired characteristics with a single piezoelectric element 2 having a uniform thickness t. For example, it is possible to irradiate ultrasonic waves so that the focal points of the two frequencies coincide with each other, thereby effectively cauterizing only the treatment area.
[0035] Although the embodiment of the present invention has been described above, the specific configuration is not limited to the above embodiment, and even if there are design changes within the scope of the present invention, they are included in the present invention. For example, in the above embodiment 2, the grooves 2a1 of the first depth and the grooves 2a2 of the second depth may be arranged in an arrangement other than the above. For example, the grooves 2a1 of the first depth and the grooves 2a2 of the second depth may be arranged alternately. [Explanation of symbols]
[0036] 1. Arrayed piezoelectric element 2. Piezoelectric element 2a groove 3 Ground electrode 4 Signal Electrode CH Channel w channel width d Groove depth t Thickness of the piezoelectric element
Claims
1. A method for arraying piezoelectric elements, comprising forming a plurality of parallel grooves in a piezoelectric element to divide the piezoelectric element into a plurality of channels, the method comprising the steps of: The ratio of the depth of the groove to the width of the channel between the grooves is defined as a depth, and the depth is adjusted according to the frequency to be output for the piezoelectric element having the same thickness to form the groove. A method for forming a piezoelectric element array comprising the steps of:
2. An arrayed piezoelectric element in which a plurality of grooves are formed in parallel in a piezoelectric element, dividing the piezoelectric element into a plurality of channels, The ratio of the depth of the groove to the width of the channel between the grooves is defined as a depth, and a plurality of grooves having different depths are formed in one piezoelectric element having the same thickness, so that a plurality of different frequencies are output.
1. An arrayed piezoelectric element comprising:
3. A plurality of the grooves having different depths are arranged so as to obtain predetermined ultrasonic characteristics.
3. The piezoelectric element array according to claim 2 .
Citation Information
Patent Citations
Piezoelectric resonator
JP1985040124U