Wafer processing method

The described wafer processing method forms an annular modified layer inside the wafer by irradiating from the back side and flattening the area, addressing processing position shifts and device damage issues during grinding.

JP2024152435APending Publication Date: 2024-10-25DISCO CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023066623
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-14
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

The existing methods for forming an annular modified layer on the outer periphery of wafers during grinding result in processing position shifts, leading to potential device damage due to knife edges and chamfered edges.

Method used

A wafer processing method that forms an annular modified layer inside the wafer by positioning the laser beam focal point inward from the outer periphery and irradiating from the back side, followed by flattening the irradiation area and grinding the back surface to a predetermined thickness, including a planarization step to stabilize the processing position.

Benefits of technology

This method effectively suppresses processing position shifts, reducing the risk of device damage during grinding by stabilizing the modified layer formation and ensuring precise thickness control.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024152435000001_ABST
    Figure 2024152435000001_ABST
Patent Text Reader

Abstract

To provide a wafer processing method with which it is possible to suppress the positional deviation of a modified layer which is formed in order to suppress the breakage of a device during polishing.SOLUTION: The wafer processing method is designed to process a wafer whose outer circumferential edge is chamfered. The method comprises: an annular modified layer formation step 3 in which the focal point of a laser beam of a wavelength permeable to a wafer is located to the inside in a prescribed distance from the outer circumferential edge of the wafer and the laser beam is radiated from the reverse side of the wafter along the outer circumferential edge, and an annular modified layer is thereby formed in the inside of the wafer; and a thinning step 4 in which the reserve side of the wafer is polished until being thinned down to a prescribed thickness after carrying out the annular modified layer formation step 3. And a flattening step 2 is further included in which at least the irradiation region on the reverse side of the wafer which is irradiated with the laser beam in the annular modified layer formation step 3 is flattened before carrying out the annular modified layer formation step 3.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wafer processing method. [Background technology]

[0002] In recent years, the development of 3D stacked semiconductor wafers has progressed in line with the trend toward lower profile and higher integration of device chips. For example, TSV (Through-Silicon Via) wafers enable the connection of electrodes between two chips by bonding them together using through-hole electrodes.

[0003] Such wafers are ground and thinned while bonded to a support wafer (silicon, glass, ceramics, etc.) that serves as a base. Normally, the outer edge of a wafer is chamfered, so when the wafer is ground to an extremely thin thickness, the outer edge becomes a so-called knife edge, and the edge is likely to chip during grinding. This may cause the chip to extend to the device, leading to damage to the device.

[0004] As a countermeasure against the knife edge, an edge trimming method has been devised in which, after bonding the wafers together, a laser beam is irradiated along the outer edge of the device to form an annular modified layer, thereby preventing chipping of the wafer edge that occurs during grinding from extending into the device (see Patent Document 1). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2020-057709 A Summary of the Invention [Problem to be solved by the invention]

[0006] In the method of Patent Document 1, since the ring-shaped modified layer is formed near the outer periphery of the wafer, the region to be irradiated with the laser beam may be set to the chamfered portion formed on the outer periphery of the wafer. In this case, the position to be irradiated with the laser beam is an inclined surface, which causes problems such as the processing position of the modified layer being shifted.

[0007] The present invention has been made in consideration of such problems, and its object is to provide a wafer processing method that can suppress misalignment of the processing position of a modified layer formed to suppress device damage during grinding. [Means for solving the problem]

[0008] In order to solve the above-mentioned problems and achieve the object, the wafer processing method of the present invention is a wafer processing method for processing a wafer having a chamfered outer peripheral edge, comprising: an annular modified layer formation step in which a focal point of a laser beam having a wavelength that is transparent to the wafer is positioned a predetermined distance inward from the outer peripheral edge of the wafer, and the laser beam is irradiated from the back side of the wafer along the outer peripheral edge to form an annular modified layer inside the wafer; and after performing the annular modified layer formation step, a thinning step in which the back side of the wafer is ground to thin it to a predetermined thickness, and is characterized in that the method further comprises a planarization step in which, before performing the annular modified layer formation step, at least an irradiation area on the back side of the wafer that is irradiated with the laser beam in the annular modified layer formation step is planarized.

[0009] In addition, in the wafer processing method of the present invention, the planarization step may be a grinding step of flat-grinding the entire back surface of the wafer so that the thickness of the wafer is not reduced to less than half.

[0010] Moreover, the wafer processing method of the present invention may further include a bonding step of bonding the front surface side of the wafer to a support wafer different from the wafer before carrying out the thinning step. Effect of the Invention

[0011] The present invention can suppress misalignment of the processing position of the modified layer formed to suppress damage to the device during grinding. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a perspective view showing an example of a wafer to be processed by the wafer processing method according to the embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along the line II-II shown in FIG. [Diagram 3] FIG. 3 is a flowchart showing a flow of the wafer processing method according to the embodiment. [Figure 4] FIG. 4 is a perspective view showing one state of the bonding step shown in FIG. [Diagram 5] FIG. 5 is an enlarged cross-sectional view of a portion of the wafer after the bonding step of FIG. [Figure 6] FIG. 6 is a side view, partially in section, illustrating one state of the flattening step shown in FIG. [Figure 7] FIG. 7 is an enlarged cross-sectional view of a portion of the wafer after the planarization step of FIG. [Figure 8] FIG. 8 is a side view, partly in section, showing one state of the annular modified layer forming step shown in FIG. [Figure 9] FIG. 9 is a side view, partially in section, showing one state of the thinning step shown in FIG. [Figure 10] FIG. 10 is an enlarged cross-sectional view of a portion of the wafer after the thinning step of FIG. [Figure 11] FIG. 11 is a side view, partially in section, showing one state of the flattening step in the modified example. [Figure 12] FIG. 12 is an enlarged cross-sectional view of a portion of the wafer after the planarization step of FIG. [Figure 13] FIG. 13 is a side view, partly in section, showing one state of the annular modified layer forming step in the modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] The form (embodiment) for carrying out the present invention will be described in detail with reference to the drawings. The present invention is not limited to the contents described in the following embodiment. Furthermore, the components described below include those that a person skilled in the art can easily imagine and those that are substantially the same. Furthermore, the configurations described below can be appropriately combined. Furthermore, various omissions, substitutions, or modifications of the configurations can be made without departing from the gist of the present invention.

[0014] [Embodiment] A method for processing a wafer 10 according to an embodiment of the present invention will be described with reference to the drawings. Fig. 1 is a perspective view showing an example of a wafer 10 to be processed by the method for processing a wafer 10 according to the embodiment. Fig. 2 is a cross-sectional view taken along line II-II shown in Fig. 1.

[0015] 1 and 2 is a disk-shaped semiconductor wafer, an optical device wafer, or the like, having a substrate 11 of silicon (Si), sapphire (Al2O3), gallium arsenide (GaAs), silicon carbide (SiC), or the like, and in the embodiment, is a silicon wafer. As shown in FIG. 2, the outer peripheral edge 12 of the wafer 10 is chamfered (beveled).

[0016] The wafer 10 has its front surface 13, which is the device surface, bonded to, for example, a support wafer 30 (see FIG. 4, etc.) to form a bonded wafer, and then its back surface 14 is ground to be thinned. In the wafer 10 of the embodiment, the bevel portion on the back surface 14 is wider and gentler than the bevel portion on the front surface 13. The back surface 14 of the wafer 10 includes an inclined surface 15 of the bevel portion and a flat surface 16.

[0017] 1, the wafer 10 includes a device region 17 on the front surface 13 side of the substrate 11, and an outer periphery region 18 surrounding the device region 17. The device region 17 has a plurality of planned division lines 19 set in a lattice pattern on the front surface 13 of the substrate 11, and devices 20 formed in each region partitioned by the planned division lines 19. The outer periphery region 18 is a region surrounding the device region 17 all around, and in which no devices 20 are formed.

[0018] In the embodiment, the device 20 constitutes a 3D NAND flash memory and includes an electrode pad and a through electrode connected to the electrode pad. The through electrode penetrates the back surface 14 of the substrate 11 when the substrate 11 is thinned and the devices 20 are individually separated from the wafer 10. That is, the wafer 10 of the embodiment is a so-called TSV wafer in which the individually separated devices 20 have through electrodes. The wafer 10 of the present invention is not limited to a TSV wafer having through electrodes as in the embodiment, and may be a device wafer without through electrodes.

[0019] Fig. 3 is a flow chart showing the flow of the processing method of the wafer 10 according to the embodiment. As shown in Fig. 3, the processing method of the wafer 10 according to the embodiment includes a bonding step 1, a flattening step 2, an annular modified layer forming step 3, and a thinning step 4. The processing method of the wafer 10 is a processing method in which an annular modified layer 25 is formed along the boundary between the device region 17 and the outer peripheral region 18 inside the wafer 10 with the outer peripheral edge 12 chamfered, and then the back surface 14 side is ground to thin the wafer 10 to a predetermined thickness 27 and the outer peripheral region 18 is removed.

[0020] (Lamination step 1) Fig. 4 is a perspective view showing one state of the bonding step 1 shown in Fig. 3. Fig. 5 is an enlarged cross-sectional view showing a part of the wafer 10 after the bonding step 1 of Fig. 4. The bonding step 1 is a step of bonding the front surface 13 side of the wafer 10 to a support wafer 30 different from the wafer 10.

[0021] 4 is a disk-shaped substrate wafer having a substrate 31 made of silicon, glass, ceramics, or the like and the same diameter as the wafer 10, but in the present invention, it may be a TSV wafer similar to the wafer 10. The supporting wafer 30 has a chamfered (beveled) outer periphery 32, similar to the wafer 10. In addition, in the supporting wafer 30 of the embodiment, the bevel portion on the other surface 34 side is wider and gentler than the bevel portion on one surface 33 side, which is the surface to be bonded to the wafer 10.

[0022] In the bonding step 1, first, the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are opposed to each other with a gap therebetween, as shown in Fig. 4. Next, the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are bonded together. This forms a bonded wafer.

[0023] In this case, when a bonding layer is provided between the wafer 10 and the support wafer 30, the bonding layer is laminated on one of the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30, and then the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are bonded together via the bonding layer. The bonding layer may be a double-sided tape having an adhesive layer laminated on the front and back surfaces of a base layer, an oxide film, or a layer formed by applying an adhesive containing a resin or the like. The wafer 10 and the support wafer 30 may be directly bonded together without using a bonding layer.

[0024] 3, the bonding step 1 in the embodiment is performed before the planarizing step 2, but may be performed after the planarizing step 2 and before the annular modified layer forming step 3. Also, the bonding step 1 may be performed after the annular modified layer forming step 3 and before the thinning step 4.

[0025] In the processing method of the wafer 10 of the embodiment, each processing of the wafer 10 is performed in a state where the support wafer 30 is bonded to the front surface 13 side of the wafer 10, but the wafer 10 processed in the present invention is not necessarily limited to the wafer 10 constituting a bonded wafer, and a single wafer 10 may be processed. In other words, the bonding step 1 does not have to be performed.

[0026] (flattening step 2) Fig. 6 is a side view, partially in cross section, showing one state of the planarization step 2 shown in Fig. 3. Fig. 7 is an enlarged cross-sectional view showing a part of the wafer 10 after the planarization step 2 of Fig. 6. In Fig. 7, the outline of the wafer 10 before processing is depicted by a dotted line. The planarization step 2 is performed before the annular modified layer formation step 3 described below is performed. The planarization step 2 is a step for planarizing a predetermined region on the back surface 14 side of the wafer 10.

[0027] The predetermined region includes at least an irradiation region 21 to be irradiated with a laser beam 53 in annular modified layer formation step 3 described below. In the embodiment, the predetermined region to be planarized is the entire surface of the back surface 14 of the wafer 10. Planarization step 2 in the embodiment is a grinding step in which the entire surface of the back surface 14 of the wafer 10 is surface-ground so that the thickness 23 of the wafer 10 is not reduced to less than half.

[0028] In the planarization step 2 of the embodiment, the entire surface of the back surface 14 side of the wafer 10 is surface-ground by a grinding device 40 shown in Fig. 6. The grinding device 40 includes a holding table 41, a grinding unit 42, and a moving unit (not shown) that moves the holding table 41 and the grinding unit 42 relatively.

[0029] The holding table 41 holds the wafer 10 by suction on its holding surface (upper surface) via the support wafer 30, and rotates around a vertical axis. The grinding unit 42 includes a spindle 43 which is a rotating shaft member, a grinding wheel 44 attached to the lower end of the spindle 43, a grinding stone 45 attached to the lower surface of the grinding wheel 44, and a grinding water supply unit (not shown). The spindle 43 and the grinding wheel 44 rotate on a rotation axis parallel to the axis of the holding table 41. The diameter of the grinding wheel 44 is at least larger than the radius of the wafer 10.

[0030] In the planarization step 2, first, the other surface 34 of the support wafer 30 is suction-held on the holding surface (upper surface) of the holding table 41. Next, the wafer 10 held on the holding table 41 via the support wafer 30 is aligned with the grinding wheel 44. Specifically, the holding table 41 is moved to the processing area below the grinding wheel 44 by a moving unit (not shown), and the grinding wheel 45 is brought into opposition to the back surface 14 of the wafer 10.

[0031] Next, while rotating the holding table 41 about its axis, the grinding wheel 44 is rotated about its axis. Grinding water is supplied to the processing point by a grinding water supply unit (not shown), and the grinding wheel 45 of the grinding wheel 44 is brought closer to the holding table 41 at a predetermined feed speed, so that the grinding wheel 45 grinds the entire surface of the back surface 14 of the wafer 10. As a result, the entire surface of the back surface 14 of the wafer 10 is flattened, as shown in FIG. 7.

[0032] Here, the entire surface of the back surface 14 side may include the irradiation region 21 to which the laser beam 53 is irradiated in the annular modified layer formation step 3 described later, and may not necessarily include a part of the inclined surface 15 on the outer periphery 12 side from the irradiation region 21. The irradiation region 21 is set at the boundary between the device region 17 and the outer periphery region 18, which is a predetermined distance inside from the outer periphery 12. That is, the outer diameter of the flat surface 22 flattened by grinding may be smaller than the outer diameter of the wafer 10. In the embodiment, since the irradiation region 21 is located on the inclined surface 15, grinding is performed in the flattening step 2 until at least the irradiation region 21 of the inclined surface 15 is flattened. At this time, the thickness 24 of the flattened wafer 10 is larger than half the original thickness 23.

[0033] (Annular modified layer formation step 3) Fig. 8 is a side view, partially in cross section, showing one state of the annular modified layer forming step 3 shown in Fig. 3. The annular modified layer forming step 3 is performed after the planarizing step 2. The annular modified layer forming step 3 is a step in which a focal point 54 of a laser beam 53 having a wavelength that is transparent to the wafer 10 is positioned a predetermined distance inward from the outer circumferential edge 12 of the wafer 10, and the laser beam 53 is irradiated along the outer circumferential edge 12 from the back surface 14 (flat surface 22) side of the wafer 10, thereby forming an annular modified layer 25 inside the wafer 10.

[0034] In annular modified layer formation step 3 of the embodiment, an annular modified layer 25 is formed inside the wafer 10 by stealth dicing using a laser processing device 50. The laser processing device 50 includes a holding table 51, a laser beam irradiation unit 52, a moving unit (not shown) that moves the holding table 51 and the laser beam irradiation unit 52 relatively, and an imaging unit (not shown) that images the wafer 10 held on the holding table 51.

[0035] The holding table 51 holds the wafer 10 on its holding surface (upper surface) and is rotatable around a vertical axis. The laser beam irradiation unit 52 irradiates a laser beam 53 onto the wafer 10 held on the holding table 51. The laser beam irradiation unit 52 has, for example, a laser oscillator, a collector that condenses and irradiates the laser beam 53 emitted from the laser oscillator onto the wafer 10 held on the holding table 51, and various optical components that propagate the laser beam 53 from the laser oscillator to the collector.

[0036] In the annular modified layer forming step 3, a laser beam 53 is irradiated along an irradiation region 21 located a predetermined distance inside the outer circumferential edge 12, specifically, along the boundary between the device region 17 and the outer circumferential region 18 of the wafer 10, to form an annular modified layer 25. The laser beam 53 is a laser beam having a wavelength that is transparent to the wafer 10, such as infrared rays (IR).

[0037] Here, the modified layer 25 means a region in which the density, refractive index, mechanical strength or other physical properties are different from those of the surrounding area as a result of irradiation with the laser beam 53. The modified layer 25 is, for example, a melting process region, a crack region, a dielectric breakdown region, a refractive index change region, a region in which these regions are mixed, etc. The modified layer 25 has a lower mechanical strength, etc. than other parts of the wafer 10.

[0038] In the annular modified layer forming step 3, first, the other surface 34 of the support wafer 30 is sucked and held on the holding surface (upper surface) of the holding table 51. Next, the wafer 10 is aligned with the condenser of the laser beam irradiation unit 52. Specifically, the holding table 51 is moved to the processing area below the laser beam irradiation unit 52 by a moving unit (not shown). Next, the wafer 10 is photographed and aligned by an imaging unit (not shown), so that the irradiation part of the laser beam irradiation unit 52 faces the irradiation area 21 at a predetermined distance inside from the outer circumferential edge 12 of the wafer 10 in the vertical direction, and then the focusing point 54 of the laser beam 53 is set inside the wafer 10.

[0039] In the annular modified layer forming step 3, next, while rotating the holding table 51 about a vertical axis, a laser beam 53 is irradiated from a laser beam irradiation unit 52 onto the back surface 14 (flat surface 22) of the wafer 10. In this manner, the laser beam 53 is irradiated along an irradiation region 21 located a predetermined distance inward from the outer peripheral edge 12 of the wafer 10, thereby forming an annular modified layer 25 inside the wafer 10.

[0040] A crack 26 extends from the modified layer 25 formed by the irradiation of the laser beam 53, forming a cylindrical splitting starting point having a side perpendicular to the surface 13 of the wafer 10. In the annular modified layer forming step 3, it is preferable to irradiate the modified layer 25 with the laser beam 53 so that the crack 26 extending from the modified layer 25 appears on the surface 13. "Perpendicular to the surface 13 of the wafer 10" means that the inclination of an approximation plane obtained by approximating the entirety of the extended crack 26 to a plane relative to the vertical plane is within ±5 degrees, preferably within ±2 degrees.

[0041] In the annular modified layer forming step 3, the height of the focal point 54 of the laser beam 53 may be changed in the thickness direction of the wafer 10 and the laser beam 53 may be irradiated multiple times, i.e., after the laser beam 53 having one focal point 54 is irradiated once along an area a predetermined distance inside from the outer circumferential edge 12 of the wafer 10, the height of the focal point 54 may be changed in the thickness direction of the wafer 10 and the laser beam 53 may be irradiated multiple times in the same manner to form multiple modified layers 25 in an annular shape and in a direction perpendicular to the surface 13 of the wafer 10. Alternatively, multiple modified layers 25 may be formed in a direction perpendicular to the surface 13 of the wafer 10 by irradiating the wafer 10 with a laser beam 53 having multiple focal points 54 spaced apart in the thickness direction of the wafer 10.

[0042] (Thinning Step 4) Fig. 9 is a side view, partially in cross section, showing one state of the thinning step 4 shown in Fig. 3. Fig. 10 is an enlarged cross-sectional view showing a part of the wafer 10 after the thinning step 4 of Fig. 9. The thinning step 4 is performed after the annular modified layer forming step 3 is performed. The thinning step 4 is a step in which the back surface 14 (flat surface 22) of the wafer 10 is ground to thin the wafer 10 to a predetermined thickness 27.

[0043] In the thinning step 4 of the embodiment, the back surface 14 (flat surface 22) of the wafer 10 is ground by a grinding device 40 to thin the wafer 10 to a predetermined thickness 27. The grinding device 40 used in the thinning step 4 may be the same device as the grinding device 40 used in the flattening step 2, or may be a separate device.

[0044] In the thinning step 4, first, the other surface 34 of the support wafer 30 is suction-held on the holding surface (upper surface) of the holding table 41. Next, the wafer 10 held on the holding table 41 via the support wafer 30 is aligned with the grinding wheel 44. Specifically, the holding table 41 is moved to the processing area below the grinding wheel 44 by a moving unit (not shown), and the grinding wheel 45 is brought into opposition to the flat surface 22 of the wafer 10.

[0045] Next, while rotating the holding table 41 about its axis, the grinding wheel 44 is rotated about its axis. Grinding water is supplied to the processing point by a grinding water supply unit (not shown), and the grinding wheel 45 of the grinding wheel 44 is brought closer to the holding table 41 at a predetermined feed speed, whereby the flat surface 22 side of the wafer 10 is ground by the grinding wheel 45, thinning the wafer 10 to a predetermined thickness 27 shown in Fig. 10. At this time, the outer peripheral region 18 of the wafer 10 is removed by the grinding load.

[0046] [Modifications] Next, a modified example of the method for processing the wafer 10 will be described with reference to the drawings.

[0047] (flattening step 2) Fig. 11 is a side view partially in cross section showing one state of the planarization step 2 in the modified example. Fig. 12 is a cross-sectional view partially enlargedly showing the wafer 10 after the planarization step 2 in Fig. 11. The planarization step 2 in the modified example is different from the planarization step 2 in the embodiment in that the entire surface of the back surface 14 side of the wafer 10 is planarized, whereas the planarization step 2 in the modified example planarizes only the vicinity of the outer circumferential edge 12 on the back surface 14 side. That is, in the modified example, the predetermined area to be planarized is an annular area including the irradiation area 28 on the back surface 14 side of the wafer 10 to which the laser beam 53 is irradiated in the annular modified layer formation step 3.

[0048] In the planarization step 2 of the embodiment, the vicinity of the outer peripheral edge 12 on the back surface 14 side of the wafer 10 is surface-ground by a grinding device 60 shown in Fig. 11. The basic configuration of the grinding device 60 is similar to that of the grinding device 40 shown in Fig. 6, and includes a holding table 61, a grinding unit 62, and a moving unit (not shown) that moves the holding table 61 and the grinding unit 62 relatively.

[0049] The holding table 61 holds the wafer 10 by suction on its holding surface (upper surface) via the support wafer 30, and rotates around a vertical axis. The grinding unit 62 includes a spindle 63 which is a rotating shaft member, a grinding wheel 64 attached to the lower end of the spindle 63, a grinding stone 65 attached to the lower surface of the grinding wheel 64, and a grinding water supply unit (not shown). The spindle 63 and the grinding wheel 64 rotate on a rotation axis parallel to the axis of the holding table 61. The diameter of the grinding wheel 64 is smaller than the diameter of the grinding wheel 44 of the grinding device 40 shown in FIG. 6.

[0050] In the planarization step 2 of the modified example, first, the other surface 34 of the support wafer 30 is suction-held on the holding surface (upper surface) of the holding table 61. Next, the wafer 10 held on the holding table 61 via the support wafer 30 is aligned with the grinding wheel 64. Specifically, the holding table 61 is moved to the processing region below the grinding wheel 64 by a moving unit (not shown), and the grinding wheel 65 is opposed to the outer periphery of the device region 17 on the back surface 14 side of the wafer 10 and the inclined surface 15 which is the outer periphery region 18.

[0051] Next, while rotating the holding table 61 about its axis, the grinding wheel 64 is rotated about its axis. Grinding water is supplied to the processing point by a grinding water supply unit (not shown), and the grinding wheel 65 of the grinding wheel 64 is brought closer to the holding table 61 at a predetermined feed speed, so that the grinding wheel 45 grinds the inclined surface 15 on the back surface 14 side of the wafer 10. As a result, as shown in FIG. 12, the inclined surface 15 on the back surface 14 side of the wafer 10 is flattened.

[0052] Here, the inclined surface 15 to be flattened may include the irradiation region 28 to which the laser beam 53 is irradiated in the annular modified layer forming step 3 described later, and may not necessarily include a part of the inclined surface 15 on the outer periphery 12 side from the irradiation region 28. The irradiation region 28 is set at the boundary between the device region 17 and the outer periphery region 18, which is a predetermined distance inside from the outer periphery 12. That is, the outer diameter of the annular flat surface 29 flattened by grinding may be smaller than the outer diameter of the wafer 10. In the embodiment, since the irradiation region 28 is located on the inclined surface 15, grinding is performed in the flattening step 2 until at least the irradiation region 28 of the inclined surface 15 is flattened. At this time, the thickness 24 of the flat surface 29 portion of the flattened wafer 10 is larger than half the original thickness 23.

[0053] (Annular modified layer formation step 3) 13 is a side view, partially in cross section, showing one state of annular modified layer forming step 3 in the modified example. Annular modified layer forming step 3 in the modified example is performed after flattening step 2 in the modified example. The procedure of annular modified layer forming step 3 in the modified example is the same as that in the embodiment, except that "irradiation area 21" and "flat surface 22" are replaced with "irradiation area 28" and "flat surface 29", and therefore a description thereof will be omitted.

[0054] As described above, in the processing method of wafer 10 according to the embodiment and the modified example, in annular modified layer formation step 3, an annular modified layer 25 serving as a division starting point for removing outer peripheral region 18 is formed inside wafer 10. Here, irradiation regions 21, 28 onto which laser beam 53 for forming modified layer 25 is irradiated are in the vicinity of outer peripheral edge 12, and therefore may be set at the chamfered portion of outer peripheral edge 12, i.e., inclined surface 15.

[0055] When the inclined surface 15 is irradiated with the laser beam 53, the thickness of the wafer 10 in the irradiation regions 21, 28 is not constant, so that the height position of the modified layer 25 to be formed may be unintentionally shifted. In addition, when the laser beam 53 is incident on the inclined surface 15, that is, when the laser beam 53 is incident from a direction oblique to the incidence surface, the radial position of the modified layer 25 to be formed may be unintentionally shifted. In contrast, in the embodiment and the modified example, at least the irradiation regions 21, 28 are flattened before the annular modified layer formation step 3, so that the effect of enabling stable laser processing is achieved.

[0056] The present invention is not limited to the above-mentioned embodiment and modified examples. In other words, various modifications can be made without departing from the gist of the present invention. For example, the planarization step 2 is not limited to grinding, and may be performed by laser processing using irradiation of a laser beam or cutting processing using a cutting blade.

[0057] In addition, in the embodiment, in the annular modified layer formation step 3, a cylindrical split starting point having a side perpendicular to the surface 13 of the wafer 10 is formed, but in the present invention, the modified layer 25 and the crack 26 may be formed along a direction having a predetermined inclination from the direction perpendicular to the surface 13 of the wafer 10, to form a split starting point having a truncated cone shape.

[0058] Furthermore, in order to facilitate removal of the outer circumferential region 18 in the thinning step 4, laser processing for dividing the outer circumferential region 18 into a plurality of regions in advance may be performed prior to the thinning step 4. In this case, for example, the outer circumferential region 18 may be divided radially by forming a radial modified layer in the outer circumferential region 18 by stealth dicing.

[0059] Alternatively, the outer peripheral region 18 may be removed by applying an external force. The external force may be, for example, a mechanical external force such as an external force in the shear direction caused by pressing the outer peripheral region 18 from above or lifting the outer peripheral region 18, or crushing by a roller, or may be an external force in the radial direction caused by vibration due to ultrasonic waves, a collision force between at least one of a liquid and a solid when sprayed onto the outer peripheral region 18, or expanding an expand tape attached to the ground finish surface of the wafer 10. [Explanation of symbols]

[0060] 10 wafers 11 Substrate 12 Outer rim 13 Surface 14 Back side 15 Slope 16 flat surface 17 Device Area 18 Outer area 19 Division line 20 Devices 21, 28 Irradiation area 22, 29 flat surface 23, 24, 27 Thickness 25 Modification layer 26 Crack 30 Support Wafer 53 Laser Beam 54 Focus point

Claims

1. A wafer processing method for processing a wafer having a chamfered outer periphery, comprising the steps of: an annular modified layer forming step of positioning a focal point of a laser beam having a wavelength that is transparent to the wafer at a predetermined distance inside from the outer periphery of the wafer, and irradiating the laser beam from the back side of the wafer along the outer periphery to form an annular modified layer inside the wafer; After the annular modified layer forming step is performed, a thinning step of grinding the back surface of the wafer to a predetermined thickness, The method further includes a planarization step of planarizing at least an irradiation area on the back side of the wafer where the laser beam is irradiated in the annular modified layer formation step before the annular modified layer formation step is performed. A wafer processing method comprising the steps of:

2. The planarization step is a grinding step in which the entire back surface of the wafer is flat-ground so that the thickness of the wafer is not reduced to less than half.

2. The wafer processing method according to claim 1 .

3. Prior to carrying out the thinning step, The method further includes a bonding step of bonding the front side of the wafer to a support wafer different from the wafer.

3. The wafer processing method according to claim 1 or 2.

Citation Information

Patent Citations

  • Semiconductor device manufacturing method

    JP2017055089A

  • Substrate processing method and substrate processing apparatus

    WO2021199585A1

  • Processing method of wafer

    JP2020057709A