Wafer processing method

By positioning the laser beam inward and angled relative to the wafer's thickness direction, the method stabilizes the modified layer's position, preventing device damage during grinding by controlling the laser beam's direction and focus.

JP2024152504APending Publication Date: 2024-10-25DISCO CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023066734
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-14
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

The existing methods for forming a laser-modified layer near the outer periphery of a wafer result in processing position shifts due to the laser beam being incident on inclined surfaces, leading to potential device damage during grinding.

Method used

A wafer processing method where the laser beam is positioned inward from the outer periphery and angled to irradiate radially inside the chamfer, forming an annular modified layer to stabilize the processing position and prevent device damage.

Benefits of technology

Stabilizes the processing position of the modified layer, reducing the risk of device damage during grinding by controlling the laser beam's direction and focus relative to the wafer's thickness direction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024152504000001_ABST
    Figure 2024152504000001_ABST
Patent Text Reader

Abstract

To provide a wafer processing method with which it is possible to suppress the processing positional deviation of a modified layer which is formed in order to suppress device breakage during polishing.SOLUTION: The wafer processing method is designed to process a wafer in which a chamfering part is formed along the outer circumferential edge. The method comprises: an annular modified layer formation step 2 in which the focal point of a laser beam of a wavelength permeable to the wafer is located to the inside in a prescribed distance from the outer circumferential edge of the wafer and the laser beam is radiated from the reverse side of the wafter along the outer circumferential edge, and an annular modified layer is thereby formed in the inside of the wafer; and a thinning step 3 in which the reserve side of the wafer is polished until being thinned down to a prescribed thickness after carrying out the annular modified layer formation step 2. In the annular modified layer formation step 2, the laser beam is radiated in a direction inclined a prescribed angle with respect to the thickness direction of the wafer, so that the laser beam enters the wafer on the radially inward of the chamfering part and is headed toward the radially outside.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wafer processing method. [Background technology]

[0002] In recent years, the development of 3D stacked semiconductor wafers has progressed in line with the trend toward lower profile and higher integration of device chips. For example, TSV (Through-Silicon Via) wafers enable the connection of electrodes between two chips by bonding them together using through-hole electrodes.

[0003] Such wafers are ground and thinned while bonded to a support wafer (silicon, glass, ceramics, etc.) that serves as a base. Normally, the outer edge of a wafer is chamfered, so when the wafer is ground to an extremely thin thickness, the outer edge becomes a so-called knife edge, and the edge is likely to chip during grinding. This may cause the chip to extend to the device, leading to damage to the device.

[0004] As a countermeasure against the knife edge, an edge trimming method has been devised in which, after bonding the wafers together, a laser beam is irradiated along the outer edge of the device to form an annular modified layer, thereby preventing chipping of the wafer edge that occurs during grinding from extending into the device (see Patent Document 1). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2020-057709 A Summary of the Invention [Problem to be solved by the invention]

[0006] In the method of Patent Document 1, since the ring-shaped modified layer is formed near the outer periphery of the wafer, the region to be irradiated with the laser beam may be set to the chamfered portion formed on the outer periphery of the wafer. In this case, the position to be irradiated with the laser beam is an inclined surface, which causes problems such as the processing position of the modified layer being shifted.

[0007] The present invention has been made in consideration of such problems, and its object is to provide a wafer processing method that can suppress misalignment of the processing position of a modified layer formed to suppress device damage during grinding. [Means for solving the problem]

[0008] In order to solve the above-mentioned problems and achieve the object, the wafer processing method of the present invention is a wafer processing method for processing a wafer having a chamfered portion formed along an outer circumferential edge, and includes an annular modified layer forming step in which a focal point of a laser beam having a wavelength that is transparent to the wafer is positioned a predetermined distance inside from the outer circumferential edge of the wafer, and the laser beam is irradiated from the back surface side of the wafer along the outer circumferential edge to form an annular modified layer inside the wafer, and after the annular modified layer forming step, a thinning step in which the back surface of the wafer is ground to thin it to a predetermined thickness, and the annular modified layer forming step is characterized in that the laser beam is irradiated in a direction inclined at a predetermined angle with respect to the thickness direction of the wafer so that the laser beam enters the wafer radially inside the chamfered portion and faces radially outward.

[0009] Moreover, the wafer processing method of the present invention may further include a bonding step of bonding the front surface side of the wafer to a support wafer different from the wafer before carrying out the thinning step. Effect of the Invention

[0010] The present invention can suppress misalignment of the processing position of the modified layer formed to suppress damage to the device during grinding. [Brief description of the drawings]

[0011] [Figure 1] FIG. 1 is a perspective view showing an example of a wafer to be processed by the wafer processing method according to the embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along the line II-II shown in FIG. [Diagram 3] FIG. 3 is a flowchart showing a flow of the wafer processing method according to the embodiment. [Figure 4] FIG. 4 is a perspective view showing one state of the bonding step shown in FIG. [Diagram 5] FIG. 5 is an enlarged cross-sectional view of a portion of the wafer after the bonding step of FIG. [Figure 6] FIG. 6 is a side view, partly in section, showing one state of the annular modified layer forming step shown in FIG. [Figure 7] FIG. 7 is an enlarged cross-sectional view showing a part of the wafer in the annular modified layer forming step of FIG. [Figure 8] FIG. 8 is an enlarged cross-sectional view showing a part of a wafer in the annular modified layer forming step of a comparative example. [Figure 9] FIG. 9 is a side view, partially in section, showing one state of the thinning step shown in FIG. [Figure 10] FIG. 10 is an enlarged cross-sectional view of a portion of the wafer after the thinning step of FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] The form (embodiment) for carrying out the present invention will be described in detail with reference to the drawings. The present invention is not limited to the contents described in the following embodiment. Furthermore, the components described below include those that a person skilled in the art can easily imagine and those that are substantially the same. Furthermore, the configurations described below can be appropriately combined. Furthermore, various omissions, substitutions, or modifications of the configurations can be made without departing from the gist of the present invention.

[0013] [Embodiment] A method for processing a wafer 10 according to an embodiment of the present invention will be described with reference to the drawings. Fig. 1 is a perspective view showing an example of a wafer 10 to be processed by the method for processing a wafer 10 according to the embodiment. Fig. 2 is a cross-sectional view taken along line II-II shown in Fig. 1.

[0014] 1 and 2 is a wafer such as a disk-shaped semiconductor wafer or an optical device wafer, which has a substrate 11 made of silicon (Si), sapphire (Al2O3), gallium arsenide (GaAs), silicon carbide (SiC), or the like, and is a silicon wafer in the embodiment. The wafer 10 has a chamfered portion formed along the outer circumferential edge 12, as shown in FIG.

[0015] The wafer 10 has its front surface 13, which is the device surface, bonded to, for example, a support wafer 30 (see FIG. 4, etc.) to form a bonded wafer, and then its back surface 14 is ground to be thinned. In the wafer 10 of the embodiment, the chamfer on the back surface 14 is wider and gentler than the chamfer on the front surface 13. The back surface 14 of the wafer 10 includes an inclined surface 15 of the chamfer and a flat surface 16.

[0016] 1, the wafer 10 includes a device region 17 on the front surface 13 side of the substrate 11, and an outer periphery region 18 surrounding the device region 17. The device region 17 has a plurality of planned division lines 19 set in a lattice pattern on the front surface 13 of the substrate 11, and devices 20 formed in each region partitioned by the planned division lines 19. The outer periphery region 18 is a region surrounding the device region 17 all around, and in which no devices 20 are formed.

[0017] In the embodiment, the device 20 constitutes a 3D NAND flash memory and includes an electrode pad and a through electrode connected to the electrode pad. The through electrode penetrates the back surface 14 of the substrate 11 when the substrate 11 is thinned and the devices 20 are individually separated from the wafer 10. That is, the wafer 10 of the embodiment is a so-called TSV wafer in which the individually separated devices 20 have through electrodes. The wafer 10 of the present invention is not limited to a TSV wafer having through electrodes as in the embodiment, and may be a device wafer without through electrodes.

[0018] Fig. 3 is a flow chart showing the flow of the processing method of the wafer 10 according to the embodiment. As shown in Fig. 3, the processing method of the wafer 10 according to the embodiment includes a bonding step 1, an annular modified layer forming step 2, and a thinning step 3. The processing method of the wafer 10 is a processing method in which an annular modified layer 21 is formed along the outer periphery 12 at a predetermined distance inside the wafer 10 in which a chamfer is formed along the outer periphery 12, and then the back surface 14 side is ground to thin the wafer 10 to a predetermined thickness 23 and the outer periphery region 18 is removed.

[0019] (Lamination step 1) Fig. 4 is a perspective view showing one state of the bonding step 1 shown in Fig. 3. Fig. 5 is an enlarged cross-sectional view showing a part of the wafer 10 after the bonding step 1 of Fig. 4. The bonding step 1 is a step of bonding the front surface 13 side of the wafer 10 to a support wafer 30 different from the wafer 10.

[0020] 4 is a disk-shaped substrate wafer having a substrate 31 made of silicon, glass, ceramics, or the like and the same diameter as the wafer 10, but in the present invention, it may be a TSV wafer similar to the wafer 10. The support wafer 30 has a chamfered portion formed along an outer circumferential edge 32, similar to the wafer 10. Also, in the support wafer 30 of the embodiment, the chamfered portion on the other surface 34 side is wider and gentler than the chamfered portion on one surface 33 side, which is the surface to be bonded to the wafer 10.

[0021] In the bonding step 1, first, the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are opposed to each other with a gap therebetween, as shown in Fig. 4. Next, the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are bonded together. This forms a bonded wafer.

[0022] In this case, when a bonding layer is provided between the wafer 10 and the support wafer 30, the bonding layer is laminated on one of the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30, and then the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are bonded together via the bonding layer. The bonding layer may be a double-sided tape having an adhesive layer laminated on the front and back surfaces of a base layer, an oxide film, or a layer formed by applying an adhesive containing a resin or the like. The wafer 10 and the support wafer 30 may be directly bonded together without using a bonding layer.

[0023] As shown in the flowchart of FIG. 3, in the embodiment, the bonding step 1 is performed before the annular modified layer formation step 2, but it may also be performed after the annular modified layer formation step 2 and before the thinning step 3.

[0024] In the processing method of the wafer 10 of the embodiment, each processing of the wafer 10 is performed in a state where the support wafer 30 is bonded to the front surface 13 side of the wafer 10, but the wafer 10 processed in the present invention is not necessarily limited to the wafer 10 constituting a bonded wafer, and a single wafer 10 may be processed. In other words, the bonding step 1 does not have to be performed.

[0025] (Annular modified layer formation step 2) Fig. 6 is a side view partially in cross section showing one state of the annular modified layer forming step 2 shown in Fig. 3. Fig. 7 is a cross-sectional view showing an enlarged portion of the wafer 10 in the annular modified layer forming step 2 of Fig. 6. The annular modified layer forming step 2 is a step in which a focal point 44 of a laser beam 43 having a wavelength that is transparent to the wafer 10 is positioned a predetermined distance inward from the outer circumferential edge 12 of the wafer 10, and the laser beam 43 is irradiated from the back surface 14 side of the wafer 10 along the outer circumferential edge 12 to form an annular modified layer 21 inside the wafer 10. The annular modified layer forming step 2 of the embodiment is performed after the bonding step 1 is performed.

[0026] Here, the modified layer 21 refers to a region in which the density, refractive index, mechanical strength or other physical properties are different from those of the surrounding area as a result of irradiation with the laser beam 43. The modified layer 21 is, for example, a melting process region, a crack region, a dielectric breakdown region, a refractive index change region, a region in which these regions are mixed, etc. The modified layer 21 has a lower mechanical strength, etc. than other parts of the wafer 10.

[0027] In the annular modified layer formation step 2 of the embodiment, an annular modified layer 21 is formed inside the wafer 10 by stealth dicing using a laser processing device 40. The laser processing device 40 includes a holding table 41, a laser beam irradiation unit 42, a moving unit (not shown) that moves the holding table 41 and the laser beam irradiation unit 42 relatively, and an imaging unit (not shown) that images the wafer 10 held on the holding table 41.

[0028] The holding table 41 holds the wafer 10 on a holding surface (upper surface) via the support wafer 30 and is rotatable around a vertical axis. The laser beam irradiation unit 42 irradiates a laser beam 43 onto the wafer 10 held on the holding table 41 via the support wafer 30. The laser beam irradiation unit 42 has, for example, a laser oscillator, a condenser that condenses and irradiates the laser beam 43 emitted from the laser oscillator onto the wafer 10 held on the holding table 41 via the support wafer 30, and various optical components that propagate the laser beam 43 from the laser oscillator to the condenser. In the laser beam irradiation unit 42, the optical axis of the laser beam 43 passing through the condenser is inclined at a predetermined angle with respect to the thickness direction of the wafer 10 held on the holding table 41 via the support wafer 30.

[0029] In the annular modified layer forming step 2, a laser beam 43 is irradiated from the back surface 14 side of the wafer 10. At this time, the laser beam 43 is irradiated in a direction inclined at a predetermined angle with respect to the thickness direction of the wafer 10 so that the laser beam 43 enters the wafer 10 at the flat surface 16 which is radially inward from the chamfered portion and heads radially outward. The laser beam 43 is a laser beam with a wavelength that is transparent to the wafer 10, for example, infrared rays (IR).

[0030] In the annular modified layer forming step 2, first, the other surface 34 of the support wafer 30 is sucked and held on the holding surface (upper surface) of the holding table 41. Next, the wafer 10 is aligned with the condenser of the laser beam irradiation unit 42. Specifically, the holding table 41 is moved to the processing area below the laser beam irradiation unit 42 by a moving unit (not shown).

[0031] Next, the wafer 10 is photographed and aligned by an imaging unit (not shown), and the irradiation portion of the laser beam irradiation unit 42 is positioned so that the direction of irradiation of the laser beam 43 in a plan view faces the radially outward direction of the wafer 10. Furthermore, the laser beam 43 is aligned so that it is incident on the flat surface 16, which is radially inward from the chamfered portion, on the back surface 14 of the wafer 10, and faces radially outward, so that the focal point 44 is positioned at a position a predetermined distance inward from the outer circumferential edge 12 of the wafer 10.

[0032] In the annular modified layer forming step 2, next, while rotating the holding table 41 about a vertical axis, a laser beam 43 is emitted from a laser beam irradiation unit 42 onto the flat surface 16 side of the back surface 14 of the wafer 10. In this manner, with a focusing point 44 of the laser beam 43 positioned a predetermined distance inside the outer periphery 12 of the wafer 10, the laser beam 43 is annularly irradiated along the outer periphery 12, thereby forming an annular modified layer 21 inside the wafer 10.

[0033] From the modified layer 21 formed by the irradiation of the laser beam 43, the crack 22 extends, and a splitting starting point is formed along the side surface of a truncated cone having a predetermined angle of inclination from the inside of the wafer 10 toward the surface 13. In the annular modified layer forming step 2, it is preferable to irradiate the laser beam 43 so that the crack 22 extending from the modified layer 21 appears on the surface 13. Along the side surface of a truncated cone having a predetermined angle of inclination means that the inclination of an approximation plane, which approximates the entirety of the extended crack 22 to a plane, is within ±5 degrees, preferably within ±2 degrees, with respect to a virtual plane of a body of revolution formed by rotating the optical axis of the laser beam 43 around the axis of the holding table 41.

[0034] In the annular modified layer forming step 2, the height of the focal point 44 of the laser beam 43 may be changed in the optical axis direction of the laser beam 43 and the laser beam 43 may be irradiated multiple times, i.e., after the laser beam 43 having one focal point 44 is irradiated once along an area a predetermined distance inside from the outer peripheral edge 12 of the wafer 10, the position of the focal point 44 may be changed in the optical axis direction of the laser beam 43 and the laser beam 43 may be irradiated multiple times in the same manner to form multiple modified layers 21 along the side surface of the truncated cone having an inclination of a predetermined angle. Alternatively, the laser beam 43 having multiple focal points 44 spaced apart in the optical axis direction of the laser beam 43 may be irradiated to form multiple modified layers 21 along the side surface of the truncated cone having an inclination of a predetermined angle.

[0035] Here, a comparative example of the annular modified layer forming step 2 will be described. Fig. 8 is an enlarged cross-sectional view showing a part of the wafer 10 in the annular modified layer forming step 2 of the comparative example. In the annular modified layer forming step 2 of the comparative example, the laser beam 43 is irradiated in a direction perpendicular to the front surface 13 of the wafer 10, that is, in the thickness direction of the wafer 10. In this case, in order to form the modified layer 21 at the boundary position between the device region 17 and the outer periphery region 18, it is necessary to irradiate the laser beam 43 from the inclined surface 15 on the back surface 14 side of the wafer 10, as shown in Fig. 8.

[0036] The laser beam 43 focused and irradiated by the condenser is refracted when it is incident on the wafer 10, so that the focal point 44 is shifted upward compared to when the laser beam travels straight outside the wafer 10. When positioning the focal point 44 inside the wafer 10 to form the modified layer 21, the position of the focal point 44 is set taking the above into consideration. However, when the laser beam 43 is incident on the inclined surface 15, the height position of incidence is more likely to shift compared to when the laser beam 43 is incident on the flat surface 16, and when the laser beam 43 is incident on a curved surface, it becomes difficult to control the focusing of the laser beam 43, so that the position where the modified layer 21 is formed may be unintentionally shifted.

[0037] (Thinning Step 3) Fig. 9 is a side view, partially in cross section, showing one state of the thinning step 3 shown in Fig. 3. Fig. 10 is an enlarged cross-sectional view showing a part of the wafer 10 after the thinning step 3 of Fig. 9. The thinning step 3 is performed after the annular modified layer forming step 2 is performed. The thinning step 3 is a step of grinding the back surface 14 of the wafer 10 to thin it down to a predetermined thickness 23.

[0038] In the thinning step 3 of the embodiment, the back surface 14 of the wafer 10 is ground by a grinding device 50 to thin the wafer 10 to a predetermined thickness 23. The grinding device 50 includes a holding table 51, a grinding unit 52, and a moving unit (not shown) that moves the holding table 51 and the grinding unit 52 relative to each other.

[0039] The holding table 51 holds the wafer 10 by suction on its holding surface (upper surface) via the support wafer 30, and rotates around a vertical axis. The grinding unit 52 includes a spindle 53 which is a rotating shaft member, a grinding wheel 54 attached to the lower end of the spindle 53, a grinding stone 55 attached to the lower surface of the grinding wheel 54, and a grinding water supply unit (not shown). The spindle 53 and the grinding wheel 54 rotate on a rotation axis parallel to the axis of the holding table 51. The diameter of the grinding wheel 54 is at least larger than the radius of the wafer 10.

[0040] In the thinning step 3, first, the other surface 34 of the support wafer 30 is suction-held on the holding surface (upper surface) of the holding table 51. Next, the wafer 10 held on the holding table 51 and the grinding wheel 54 are aligned via the support wafer 30. Specifically, the holding table 51 is moved to a processing area below the grinding wheel 54 by a moving unit (not shown), and the grinding wheel 55 and the back surface 14 of the wafer 10 are opposed to each other.

[0041] Next, while rotating the holding table 51 about its axis, the grinding wheel 54 is rotated about its axis. Grinding water is supplied to the processing point by a grinding water supply unit (not shown), and the grinding wheel 55 of the grinding wheel 54 is brought closer to the holding table 51 at a predetermined feed speed, whereby the back surface 14 side of the wafer 10 is ground by the grinding wheel 55, thinning the wafer 10 to a predetermined thickness 23 shown in Fig. 10. At this time, the region (outer peripheral region 18) on the outer peripheral edge 12 side of the modified layer 21 of the wafer 10 is removed by the grinding load.

[0042] As described above, the processing method of the wafer 10 according to the embodiment forms the annular modified layer 21 inside the wafer 10, which serves as a division starting point for removing the outer peripheral region 18. Here, the irradiation region onto which the laser beam 43 for forming the modified layer 21 is irradiated is near the outer peripheral edge 12, and therefore may be set to the chamfered portion of the outer peripheral edge 12, i.e., the inclined surface 15.

[0043] When the inclined surface 15 is irradiated with the laser beam 43, the thickness of the wafer 10 in the irradiated area is not constant, so that the height position of the modified layer 21 to be formed may be unintentionally shifted. In addition, when the laser beam 43 is incident on the inclined surface 15, which is a curved surface, it is diffusely reflected, so that the modified layer 21 may not be formed stably.

[0044] In contrast, in the embodiment, in the annular modified layer formation step 2, a laser beam 43 inclined at a predetermined angle is irradiated from the back surface 14 of the wafer 10 so as to be directed from the flat surface 16 radially inward from the chamfered portion toward the radially outward. This makes it possible to avoid problems such as diffuse reflection of the laser beam 43 by the chamfered portion, and has the effect of enabling the modified layer 21 to be stably formed along the outer circumferential edge 12.

[0045] The present invention is not limited to the above-mentioned embodiment and modified examples. That is, various modifications can be made without departing from the gist of the present invention. For example, in the annular modified layer forming step 2, the method is not limited to tilting the optical axis of the laser beam 43 in the embodiment, and the holding table 41 may be tilted, or a spatial light modulator such as LCOS (Liquid-Crystal on Silicon) may be used to control the wavefront to form a predetermined angle.

[0046] Furthermore, in order to facilitate removal of the outer circumferential region 18 in the thinning step 3, laser processing for dividing the outer circumferential region 18 into a plurality of regions in advance may be performed prior to the thinning step 3. In this case, for example, the outer circumferential region 18 may be divided radially by forming a radial modified layer in the outer circumferential region 18 by stealth dicing.

[0047] Alternatively, the outer peripheral region 18 may be removed by applying an external force. The external force may be, for example, a mechanical external force such as an external force in the shear direction caused by pressing the outer peripheral region 18 from above or lifting the outer peripheral region 18, or crushing by a roller, or may be an external force in the radial direction caused by vibration due to ultrasonic waves, a collision force between at least one of a liquid and a solid when sprayed onto the outer peripheral region 18, or expanding an expand tape attached to the ground finish surface of the wafer 10. [Explanation of symbols]

[0048] 10 wafers 11 Substrate 12 Outer rim 13 Surface 14 Back side 15 Slope 16 flat surface 17 Device Area 18 Outer area 19 Division line 20 Devices 21 Modification layer 22 Crack 23 Thickness 30 Support Wafer 43 Laser Beam 44 Focus point

Claims

1. A wafer processing method for processing a wafer having a chamfered portion formed along an outer periphery, comprising: an annular modified layer forming step of positioning a focal point of a laser beam having a wavelength that is transparent to the wafer at a predetermined distance inside from the outer periphery of the wafer, and irradiating the laser beam from the back side of the wafer along the outer periphery to form an annular modified layer inside the wafer; After the annular modified layer forming step is performed, a thinning step of grinding the back surface of the wafer to a predetermined thickness, In the annular modified layer forming step, The laser beam is irradiated in a direction inclined at a predetermined angle with respect to the thickness direction of the wafer so that the laser beam is incident on the wafer radially inward from the chamfered portion and directed radially outward. A wafer processing method comprising the steps of:

2. Prior to carrying out the thinning step, The method further includes a bonding step of bonding the front side of the wafer to a support wafer different from the wafer.

2. The wafer processing method according to claim 1 .

Citation Information

Patent Citations

  • Method for manufacturing silicon carbide semiconductor device and silicon carbide semiconductor device

    JP2014229843A

  • Processing method of wafer

    JP2020057709A

  • Wafer processing method

    JP2021129037A

  • Workpiece processing method

    JP2022059711A