Method of sealing additively manufactured channel and port
By integrating ports for external access and using dedicated tools to remove residual powder from internal channels, the method addresses the challenge of uneven channel sizes and damage in complex internal features, ensuring effective and intact manufacturing of additively manufactured parts.
Patent Information
- Application Number
- JP2024006565
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-10
- Filing Date
- 2024-01-19
- Publication Date
- 2024-10-25
AI Technical Summary
Existing additive manufacturing methods face challenges in efficiently and effectively removing unbonded powder from complex internal channels with bends and tortuous paths in additively manufactured parts, leading to uneven channel sizes and potential damage during the debinding and sintering processes.
Incorporating ports that extend from the exterior surface to internal channels, allowing for the use of pressure gradients, ultrasonic wands, or abrasive brushes to remove residual powder, followed by sealing the ports with a brazing material after sintering to maintain structural integrity.
Enables reliable and complete removal of residual powder from intricate internal channels, preserving the structural integrity of the manufactured parts with complex geometries, even after sintering.
Smart Images

Figure 2024152599000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates generally to additive manufacturing systems and, more specifically, to methods for sealing additively manufactured ports and channels. [Background technology]
[0002] Binder jetting additive manufacturing (BJAM) selectively sprays a binder solution (such as a liquid adhesive) in a CAD-defined pattern onto a powder bed to form the target part. That layer is then overcoated with a new layer of powder, and the jetting process is repeated until the target part is completed. The printed target part is typically subjected to a curing process that solidifies the binder solution within the powder to form a green (e.g., as-printed, unfired) target part. The green target part is then subjected to a debinding process that uses heat to break down and remove the binder from the green target part so that a brown (e.g., partially fired) target part is formed. The brown target part is then subjected to a sintering process that consolidates the powder particles to form the final target part.
[0003] Certain target parts may include internal features, such as cooling channels, to enhance the performance and / or durability of the target part. Such channels are formed during the jetting and printing process, and unbound powder is removed from the channels defined within the green target part (in a process known as "depowdering") prior to debinding and sintering. For example, to depowder the internal channels of a green target part, a pressure gradient (e.g., positive pressure or vacuum) may be applied or induced to a first external opening of the internal channel of the green target part to rapidly move a gas (e.g., air) through the internal channel to remove the unbound powder from a second external opening of the channel. Alternatively, a vacuum probe, ultrasonic wand, and / or an abrasive wire brush may be inserted into the external opening to remove the unbound powder.
[0004] Depending on the complexity of the internal features of the green target part and / or the orientation of the channels, de-powdering can be a difficult and / or time-consuming process. For example, the internal channels can be circuitous (e.g., serpentine and / or winding), which can cause unbound powder to become trapped in portions of the internal channels, resulting in inconsistencies in the size and shape of the internal channels after sintering. Furthermore, because unbound powder is typically removed from the external openings of the internal channels during de-powdering, the external openings can be damaged during de-powdering. As a result, the internal channels so produced have previously been limited in their internal features and / or size.
[0005] Therefore, there is a need for improved additive manufacturing systems and methods of operation for obtaining target parts with complex internal channels defined therein. Summary of the Invention
[0006] In one aspect, a method for manufacturing a target part is disclosed. The method includes inputting instructions for manufacturing a desired target part into a binder jetting additive manufacturing system. The target part includes one or more internal channels defined at least by a circuitous path including one or more bends. The method further includes printing the target part by a binder jet additive manufacturing process to form a green body target part. During printing, one or more ports are formed that extend from an outer surface of the target part to the one or more internal channels. The method further includes de-powdering the one or more internal channels by accessing the one or more ports formed on the green body target part.
[0007] In another aspect, a method for manufacturing a target part is disclosed. The method includes inputting instructions into an additive manufacturing system for additively manufacturing a desired target part. The target part includes one or more internal channels. The method further includes inputting locations of one or more ports to be formed, the one or more ports extending from an outer surface of the target part to the one or more internal channels. The method further includes printing the target part to form a green body target part. The method further includes de-powdering the one or more internal channels by accessing the one or more ports of the green body target part to facilitate removal of residual powder from the one or more internal channels. [Brief description of the drawings]
[0008] In the following detailed description, the disclosed technology will be more fully described with reference to exemplary embodiments illustrated in the accompanying drawings. [Figure 1] FIG. 1 is a schematic diagram of an exemplary binder jetting additive manufacturing system. [Diagram 2] 1 is a schematic diagram of an exemplary target part before sintering. [Diagram 3] 3 is a detailed view of Detail A (shown in FIG. 2) of the target part of FIG. 2. [Figure 4] 3 is a detailed view of Detail A (shown in FIG. 2) including the tapered port of the target part of FIG. 2. [Diagram 5] 3 is a detailed view of Detail A (shown in FIG. 2) including the angled port of the target part of FIG. 2; [Figure 6] 1 is a schematic diagram of an exemplary target part after brazing a preformed plug to a port. [Figure 7] 7 is a flow diagram of an exemplary method for manufacturing the target part of FIGS.
[0009] The symbols used in the drawings and their meanings are summarized in the Brief Explanation of Symbols section. In principle, the same target parts are given the same symbols as in the drawings. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] In the following specification and claims, reference will be made to a number of terms that shall be defined to have the following meanings.
[0011] As used herein, the singular includes the plural unless otherwise clear from the context. As used herein, the terms "comprises," "includes," and "having" are inclusive and mean that there may be additional elements other than the recited components. The term "optional" or "optionally" means that the recited event or circumstance may or may not occur, and such a description encompasses both the occurrence and non-occurrence of the event.
[0012] Unless otherwise stated, approximate expressions such as "approximately", "substantially" and "about" in this specification indicate that the modified terms are not absolute or precise, but are merely approximate as would be obvious to one skilled in the art. Thus, values modified with terms such as "approximately", "substantially" and "about" are not limited to the exact numerical value, but are meant to include numerical values within a range of ±10% of the numerical value. In at least some cases, the approximate expression corresponds to the accuracy of the instrument that measures the value. In the present specification and claims, ranges may be limited. Such ranges are mutually combinable and / or interchangeable, and include any subranges contained within the ranges unless otherwise clear from the context.
[0013] Moreover, unless otherwise indicated, the terms "first," "second," etc. are used herein merely as labels and do not impose numerical, positional, or hierarchical requirements on what they are attached to. Furthermore, the reference to "second," for example, does not require or preclude the presence of, for example, a "first" or more, or a "third" or more.
[0014] As used herein, the term "additive manufacturing" or "additive manufacturing technique or process" refers to a manufacturing process in which a three-dimensional part is built up layer by layer by depositing layers of material on top of each other in a sequential manner. Successive layers are then partially melted or fused together to form a monolithic or integral part.
[0015] As used herein, the term "binder jetting" or "binder jet additive manufacturing" refers to an additive manufacturing technique in which a binder (e.g., an adhesive) is used to bind powder particles together to form a three-dimensional object. In particular, a binder is selectively deposited (or jetted) onto successive layers of powder within a build volume, where the layers of powder and binder adhere to each other to form the three-dimensional object. The powder may be, for example, particles of a material such as a polymer, metal, metal alloy, ceramic, etc. The binder-printed target part, also referred to as a "green target part," may later be subjected to a heat treatment to obtain a densified final target part. For example, the green target part may be inserted into a sintering furnace where the green target part is heated to a high temperature (e.g., about 500° C. or higher) to remove the binder material and to cause the powder particles to coagulate together.
[0016] As used herein, the term "green target part" refers to a binder printed target part or workpiece that has not been subjected to a heat treatment to remove the binder. A green target part can include particulate matter that has not been consolidated by heating the particulate matter to a sintering temperature. The green target part consolidates upon heating to a sufficient temperature during sintering to form a densified sintered target part that has strong mechanical properties. As such, the green target part can have a relatively lower solid density and higher porosity (e.g., 50% to 70%) than the sintered target part (e.g., 92% or more, or even 98% or more).
[0017] As used herein, the term "sintering" refers to heating a green target part to an elevated temperature. Sintering of a green target part may be performed in one or more stages. For example, in some embodiments, sintering may include heating the green target part to a first elevated temperature to induce pyrolysis of at least a portion of the binder used to print the green target part. The green target part may then be further heated to a second elevated temperature, higher than the first elevated temperature, to consolidate the powder particles together to form a sintered consolidated target part.
[0018] The methods, systems, and devices described herein relate to a method for manufacturing a target part. The method includes providing a target part with a binder jetting system, the target part including one or more internal channels and a circuit path defined by one or more bends in the internal channels. A port extending from an outer surface of the target part is then provided in fluid communication with the one or more internal channels to facilitate de-powdering of the one or more internal channels. The one or more internal channels are then de-powdered through the port of the target part. The method further includes sintering the green target part and then brazing the port to seal the preformed plug in the port with a brazing material. It is noted that the embodiments described herein may also be used to de-powder channels that do not include bends or circuitous paths.
[0019] 1 is a schematic diagram of an exemplary additive manufacturing system 100 used to manufacture (or print) a green body target part 150 by binder jetting. In an exemplary embodiment, the target part 150 includes one or more interior channels 152 having two or more openings 154 and a circuitous (e.g., serpentine, meandering) path 156 that extends at least partially between the two openings 154. The circuitous path 156 is defined by one or more bends 158 in the interior channel 152.
[0020] The methods described herein may be applied to a variety of components. As an example, the target component 150 may be an inner or outer endwall of a gas turbine nozzle, such as may be used in the expander turbine section of a gas turbine engine. Similarly, the target component 150 may be a turbine shroud for use in the expander turbine section of a gas turbine engine.
[0021] As shown, the additive manufacturing system 100 includes a housing 102, a print head 104, a powder feed assembly 106, and a build chamber 116 within the housing 102. The powder feed assembly 106 includes a source of powder 108. The powder feed assembly 106 also includes a powder piston 110 located within a feed chamber 112 that contains the powder 108. The powder piston 110 can be selectively raised within the feed chamber 112 to push a portion of the powder 108 from the powder feed chamber 112 through a powder feed port 114. A recoater 120, such as a roller or blade / wiper, can be operable to move across the powder feed port 114 to push the powder 108 discharged from the powder feed chamber 112 across a work surface 122 and through an opening 118 into the build chamber 116.
[0022] The additive manufacturing system 100 also includes a build platform 124 in the build chamber 116. The build platform 124 has a flat build surface 126 that supports the green body target part 150 being printed, and a powder bed 128 that contains excess powder 108 from the powder supply chamber 112 (powder 108 that is delivered into the build chamber 116 but is not used to print the green body target part 150). The build platform 124 is movable along a build direction relative to the print head 104 (i.e., the build platform 124 can be raised and lowered by a platform actuator 130 operably coupled to the build platform 124) to selectively vary the height of the green body target part 150 during printing. During printing of the green body target part 150, the recoater 120 smoothes a layer of powder 108 discharged from the powder supply chamber 112 across the build surface 126 of the build platform 124 (or across the existing powder bed 128, in the case of a subsequent layer). The printhead 104 selectively deposits binder solution 140 onto a layer of powder 108 that represents a layer of green body target part 150 to be printed.
[0023] The additive manufacturing system 100 may include any suitable number of print heads 104. For example, in the illustrated embodiment, the additive manufacturing system 100 includes a single print head 104. However, in alternative embodiments, the additive manufacturing system 100 may include two or more print heads 104. Multiple layers of powder 108 are laid down on the build surface 126, and the print head 104 selectively deposits a pattern of binder solution 140 on each layer of powder 108 in sequence. The build platform 124 is lowered before each layer of powder 108 is laid down and after the selective deposition of binder solution 140.
[0024] The additive manufacturing system 100 also includes a computing system 142 coupled to one or more system components of the additive manufacturing system 100 (e.g., the print head 104, the powder piston 110, the recoater 120, and / or the platform actuator 130), whose operation may be electronically or automatically controlled by the computing system 100. In general, the computing system 142 may include one or more processor units (e.g., a controller or computing device, or a suitable combination of multiple controllers or computing devices). For example, in some embodiments, the computing system 142 may include one or more processors 144 and one or more associated memory devices 146 configured to perform various computer-implemented functions.
[0025] As used herein, the term "processor" refers to integrated circuits referred to in the art as included in computers, as well as controllers, microcontrollers, microcomputers, programmable logic circuits (PLCs), application specific integrated circuits, and other programmable circuits. Additionally, the one or more memory devices 146 of the computing system 142 may generally include one or more memory elements, such as, but not limited to, a computer-readable medium (e.g., random access memory (RAM)), a computer-readable non-volatile medium (e.g., flash memory), a floppy disk, a compact disk read only memory (CD-ROM), a magneto-optical disk (MOD), a digital versatile disk (DVD), and / or other suitable memory elements. Such one or more memory devices 146 may generally be configured to store suitable computer-readable instructions that, when executed by the one or more processors 144, cause the computing system 142 to perform various computer-implemented functions, such as one or more aspects of the methods and algorithms described herein. Additionally, the computing system 142 may include various other suitable components, such as a user interface, communication circuits or modules, one or more input / output channels, data / control buses, and the like.
[0026] Various functions of computing system 142 may be performed on a single processor device or may be distributed across any number of processor devices, in which case such multiple processor devices may cooperate to form a target part. For example, functions of computing system 142 may be distributed across multiple application-specific controllers, such as additive manufacturing device controllers, one or more controllers / computing devices of one or more remote devices (e.g., laptops, desktops, servers, etc.), etc.
[0027] In an exemplary embodiment, computing system 142 is coupled to each of powder piston 110, recoater 120, and platform actuator 130 via communications link 143. System 142 controls the operation of components of additive manufacturing system 100 during printing of green body target part 150. For example, computing system 142 may cause powder piston 110 and recoater 120 to cooperate in dispensing powder 108 from powder feed chamber 112 to be laid down across build surface 126. Similarly, system 142 may control platform actuator 130 to selectively raise and lower build platform 124 while selectively depositing binder solution 140 with print head 104 onto layers of powder 108 laid down across build surface 126.
[0028] The computing system 142 may, for example, store a CAD model of the green body target part 150 in one or more memory devices 146 and control the print head to print the green body target part 150 based on the CAD model. Additionally or alternatively, the computing system 142 may receive one or more inputs (e.g., from a user interface) of a desired geometric shape of the green body target part 150.
[0029] After the intended overall structure of the green target part 150 is formed using the additive manufacturing system 100, the binder solution 140 deposited on and within the layers of powder 108 may be heated to a curing temperature (e.g., about 25° C. or higher and about 100° C. or lower) to evaporate at least a portion of the solvent in the binder solution 140. The printed green target part 150 may be heated using IR lamps and / or a heating plate (e.g., on-board) or by placing the printed green target part 150 in an oven (e.g., off-board). After curing, the binder bonds the layers of powder 108 together. Suitable binders include, but are not limited to, thermoplastic binders, thermosetting binders, and non-polymeric binders such as waxes and sugars (e.g., glucose, fructose, derivatives thereof, or combinations thereof).
[0030] After molding and curing, the green target part 150 (which may at this stage be referred to as the brown target part 150) may be inserted into a sintering furnace (not shown) for consolidation of the brown target part 150. To sinter the brown target part 150, the brown target part 150 is heated in the sintering furnace (not shown) to a suitable elevated temperature for a suitable time. In various embodiments, sintering of the body target part 150 may be performed in multiple stages. For example, in some embodiments, sintering may include heating the brown target part 150 (for a suitable first period of time) to a suitable first elevated temperature to cause thermal decomposition of at least a portion of the binder used to print the target part 150 (e.g., to "de-grease" the brown target part 150). The brown target part 150 may then be heated to a temperature above a second elevated temperature, which is higher than the first elevated temperature, to consolidate the powder particles to form a consolidated target part after sintering.
[0031] Prior to sintering and debinding, the target part 150 is depowdered to remove unbonded powder 108 from one or more internal channels 152 of the target part 150. In some embodiments, a pressure gradient (e.g., positive pressure or vacuum) is applied to at least one of two openings 154 at either end of the internal channel 152 to rapidly move a gas (e.g., air) through the internal channel 152. The rapid flow of gas through the internal channel 152 facilitates the removal of the unbonded powder 108 from the internal channel 152. Alternatively, an ultrasonic wand or an abrasive wire brush may be inserted into at least one of the two or more openings 154 to expel the unbonded powder 108 from the one or more internal channels 152.
[0032] FIG. 2 is a schematic diagram of the target part 150 before sintering and degreasing, and FIG. 3 is a detailed diagram of Detail A (shown in FIG. 2). As shown in the exemplary embodiment, the ports 160 extend substantially perpendicular to the internal channels 152 and / or the outer surface 151 of the target part 150 to facilitate de-powdering of the internal channels 152. The ports 160 are incorporated into the CAD model and are manufactured with the target part 150 during the build-up and printing process. The ports 160 each have a first opening 162 defined in the outer surface 151 of the target part 150 and a second opening 164 in fluid communication with one or more of the internal channels 152. In the illustrated embodiment, the first openings 162 of the ports 160 each extend from the top surface 153 of the target part 150.
[0033] In some embodiments, the first openings 162 of the ports 160 each extend from the underside 155 or side 157 of the target part 150. In some embodiments, the port openings 162 extend from multiple surfaces depending on the geometry and complexity of the target part 150 and depending on the geometry and complexity of the internal channels 152. It is noted that while the figures show a two-dimensional view, the target part 150 is a three-dimensional solid object and the first openings 162 of the ports 160 may extend from any surface such that the internal channels 152 extend between the second openings 164 and the first openings 162 and one or more openings 162 or 164 of each channel 152 are accessible by an operator or user for use in de-powdering the internal channels 152. As shown most clearly in FIG. 3, in an exemplary embodiment, each of the ports 160 has a diameter D and is spaced apart from an adjacent port 160 by a separation distance L. The separation distance L is measured from the central axis of each port 160.
[0034] As described in more detail below, the ports 160 are plugged and brazed after sintering of the target part 150. However, when the ports 160 are plugged, the plugged ports 160 create stress points in the target part 150. Therefore, the number of ports 160, the diameter D of the ports 160, and the distance L between the ports 160 are each optimized to provide adequate access to the internal channels 152 for de-powdering without adversely affecting the structural integrity of one or more of the parts 150. The ports 160 ensure that even internal channels 152 with complex geometries, narrow diameters, and sharp bends 158 can be de-powdered.
[0035] In some embodiments, the ports 160 each have the same diameter D. In some embodiments, the diameter D of the ports may vary relative to one another depending on the complexity of the target part 150 and the surface 151 on which the first opening 162 is defined. By way of example, the narrow region 169 of the target part 150 may have ports 160 formed with a smaller diameter D than the diameter D of the ports formed in the wide region 167 of the target part 150. In some embodiments, the diameter D of the ports 160 may be in the range of about 0.03 inches (about 0.7 mm) to about 0.8 inches (about 20 mm). It will be appreciated that areas of the target part 150 that are less stressed under normal operating conditions may have ports 160 formed with larger diameters D. It will also be appreciated that larger target parts 150 may have larger ports 160.
[0036] Similarly, in some embodiments, the spacing L between adjacent ports 160 (also referred to as the pitch distance) is substantially the same (i.e., substantially equally spaced) throughout the entire target part 150 or a portion of the target part 150. In other embodiments, the spacing L may vary depending on the complexity of the target part 150 and the complexity of each of the internal channels 152 within the part 150. As an example, a channel 152 having a circuitous path 156 may require more ports 160 in the circuitous portion of the path 156 to provide adequate access for de-powdering, and the spacing L between adjacent ports 160 may be smaller, as compared to a portion of the internal channel 152 having fewer bends 158 within the target part 150. In some embodiments, the spacing L between adjacent ports 160 may range from about 0.5 inches (about 12 mm) to about 4 inches (about 100 mm). In some embodiments, the spacing L between adjacent ports 160 is preferably about 1.2 inches (about 30 mm). As will be appreciated, areas of the target component 150 that experience less stress under normal operating conditions may have ports 160 with greater spacing L therebetween.
[0037] As shown in FIG. 4, the ports 160 are preferably tapered to improve the pluggability and brazing of the ports 160. Specifically, in an exemplary embodiment, the ports 160 are formed in a frustoconical shape, with a diameter D1 of the first opening 162 being wider than a diameter D2 of the second opening 164. The diameter D2 is sized and oriented to provide adequate access to the one or more internal channels 152 for de-powdering. As shown in FIG. 5, in some embodiments, at least one of the ports 160 is formed obliquely at an angle θ to the internal channel 152 to facilitate de-powdering. The obliquely oriented ports 160 may be utilized to facilitate improved access to the internal channel 152 for de-powdering. In some embodiments, the ports 160 are both inclined and tapered. As shown in FIG. 6, after de-powdering, the ports 160 are plugged with preformed plugs 161 and fixed in the ports by brazing. As a result, the bypass path 156 is open only through the access openings 154 located on both sides.
[0038] An exemplary method 300 for producing a target part 150 is described with reference to FIG. 7 and further with reference to FIGS. 1-6. In an exemplary embodiment, the method 300 includes inputting 302 instructions to a binder jetting system for producing a desired target part, such as part 150, the desired target part 150 including one or more internal channels 152 defined therein. The one or more internal channels 152 include two or more access openings 154, as described above, and, in an exemplary embodiment, a bypass path 156 extending at least partially between two openings 154. The method 300 further includes providing 304 a plurality of access ports (such as port 160), each extending from an exterior surface of the target part 150 and in fluid communication with the one or more internal channels 152, to facilitate de-powdering of the internal channels 152.
[0039] The method 300 further includes printing 306 the green body target part 150 by a binder jet additive manufacturing process. Binder jet additive manufacturing to print the green body target part 150 can be performed using additive manufacturing system 100 or any other suitable additive manufacturing system. As described above, the green body target part 150 is printed on a build surface, such as surface 126. A recoater, such as recoater 120, spreads a layer of powder 108 across the build surface 126, and a print head, such as head 104, selectively deposits binder solution 140 across the layer of powder 108. The process is repeated to lay successive layers of powder 108 across the build surface 126 and selectively deposit binder solution 140 on each layer of powder 108.
[0040] After printing 306 the green body target part 150, the method 300 includes de-powdering 308 the green body target part 150. De-powdering 308 is performed by at least one of: directing 310 pressurized air or pulling a vacuum through the ports 160 of the one or more internal channels 152 to dislodge any residual powder within the internal channels 152, inserting an ultrasonic wand into the ports 160 of the one or more internal channels 152 to dislodge any residual powder within the one or more internal channels 152, and inserting a wire brush into the ports 160 of the one or more internal channels 152 to dislodge any residual powder within the one or more internal channels 152.
[0041] After de-powdering 308 the one or more internal channels 152, the method 300 further includes a step 316 of sintering the green body target part 150 and a step 318 of brazing the port 160 to seal the preformed plug 161 in the port 160 using a brazing material.
[0042] The embodiments described herein may successfully address at least some of the shortcomings of binder jet additive manufacturing in producing parts containing internal circuit channels. The target part is printed with ports formed in fluid communication with the circuit channels. In some embodiments, the ports may be tapered and / or angled to allow easy access to the bypass channel to be de-powdered after printing. The inclusion of access ports for de-powdering of such bypass channels allows intricate internal channels with complex geometries, narrow diameters, and sharp turns to be produced and reliably de-powdered without the risk of inadvertently sintering powder residue remaining in the channel after printing into the channel. The reliable de-powdering technique described herein effectively maintains the overall structural integrity of parts produced with complex internal channels.
[0043] The above description is illustrative and not limiting. For example, the above-described embodiments (and / or aspects thereof) may be used in combination with each other. Furthermore, numerous modifications may be made to the teachings of the technology described herein to adapt to a particular situation or material without departing from the scope thereof. The dimensions and types of materials described herein define the parameters of the technology disclosed herein, but they are illustrative and not limiting. Many other embodiments will be apparent to those skilled in the art upon reading the description herein. The technical scope of the technology disclosed herein should be determined based on the claims and their equivalents. In the claims, the terms "first", "second" and "third" are merely appended and do not impose numerical requirements on what they are appended to. Furthermore, unless the phrase "means for" a function is expressly used as a limitation of the claim without specifying the structure, limitations recited in a means-plus-function form are not to be construed under § 112(f).
[0044] This specification discloses several embodiments of the disclosed technology, including the best mode thereof, and has described by way of example, in order to enable those skilled in the art to practice the disclosed technology, including making and using a device or system and practicing a method. The patentable scope of the disclosed technology is defined by the claims, and includes other examples that are obvious to those skilled in the art. Such other examples are within the scope of the claims if they have elements that are not literally different from the claims, or have equivalent elements that are only insubstantial different from the claims.
[0045] The methods, systems, and compositions disclosed herein are not limited to the specific embodiments described herein, and the method steps, system components, and / or composition components may be utilized independently and separately from other steps and / or components described herein. For example, the methods, systems, and compositions are not limited to practice with the rotating machines described herein. The methods, systems, and compositions may be implemented and utilized in connection with many other applications.
[0046] Although specific features of various embodiments may be shown in some drawings and not in others, this is for convenience only. Moreover, references to "one embodiment" in the above description should not be interpreted as excluding the existence of additional embodiments that possess the recited features. Consistent with the principles of the present disclosure, features shown in one drawing may be referenced and / or claimed in combination with features shown in other drawings.
[0047] While the present systems and methods have been described in various specific embodiments, it will be apparent to those skilled in the art that the present techniques may be modified and practiced within the spirit and scope of the appended claims.
[0048] The present system and method may be defined in the following exemplary embodiment section.
[0049] In a first embodiment, a method for manufacturing a target part includes inputting instructions for manufacturing a desired target part into a binder jetting additive manufacturing system, the target part including one or more internal channels defined at least by a circuitous path including one or more bends; printing the target part by a binder jet additive manufacturing process to form a green body target part, where during printing, one or more ports are formed extending from an outer surface of the target part to the one or more internal channels; and de-powdering the one or more internal channels by accessing the one or more ports formed on the green body target part.
[0050] In the above aspects, the method includes at least one of: directing pressurized air through one or more ports to facilitate dislodging residual powder remaining in the one or more internal channels; inserting an ultrasonic wand into one or more ports to facilitate dislodging residual powder remaining in the one or more internal channels; and inserting a wire brush into one or more ports to facilitate dislodging residual powder remaining in the one or more internal channels.
[0051] In any of the above embodiments, the method further includes sintering the green body target part after removing residual powder from the one or more internal channels.
[0052] In any of the above aspects, the method further includes brazing the one or more ports to seal the one or more ports with a braze material after removing residual powder from the one or more internal channels and after sintering the green body target part.
[0053] In any of the above aspects, the method further includes forming one or more ports oriented substantially perpendicular to an exterior surface of the target part to facilitate de-powdering of one or more internal channels.
[0054] In any of the above aspects, the method further includes forming one or more ports oriented obliquely relative to an exterior surface of the target part to facilitate de-powdering of one or more internal channels.
[0055] In any of the above aspects, the method further includes forming the ports having a tapered shape such that a first end of each port has a diameter larger than a diameter of a second end of each port, the second ends being in fluid communication with the one or more internal channels.
[0056] In any of the above aspects, the step of printing the target part further includes forming a plurality of ports, each extending from an outer surface of the target part to an internal channel formed in the target part, the plurality of ports being substantially equally spaced apart.
[0057] In any of the above aspects, the step of printing the target part further includes forming a plurality of ports each extending from an outer surface of the target part to an internal channel formed in the target part, the plurality of ports being spaced apart a variable distance across the target part.
[0058] In any of the above aspects, the step of printing the target part further includes forming a plurality of ports spaced apart at intervals within a range of about 0.5 inches (about 12 mm) to about 4 inches (100 mm) and forming a plurality of ports having diameters within a range of about 0.03 inches (about 0.7 mm) to about 0.8 inches (about 20 mm).
[0059] In a second embodiment, a method for manufacturing a target part includes inputting instructions into an additive manufacturing system for additively manufacturing a desired target part, the target part including one or more internal channels; inputting the locations of one or more ports to be formed, the one or more ports extending from an outer surface of the target part to the one or more internal channels; printing the target part to form a green body target part; and de-powdering the one or more internal channels by accessing the one or more ports of the green body target part to facilitate removal of residual powder from the one or more internal channels.
[0060] In the above aspect, the method includes at least one of: directing pressurized air through one or more ports to facilitate dislodging of residual powder remaining within the one or more internal channels; inserting an ultrasonic wand into one or more ports to facilitate dislodging of residual powder remaining within the one or more internal channels; and inserting a wire brush into one or more ports to facilitate dislodging of residual powder remaining within the one or more internal channels.
[0061] In any of the above embodiments, the method further includes sintering the green body target part after removing residual powder from the one or more internal channels.
[0062] In any of the above aspects, the method further includes brazing the one or more ports to seal the one or more ports with a braze material after removing residual powder from the one or more internal channels and after sintering the green body target part.
[0063] In any of the above aspects, the method further includes forming one or more ports oriented substantially perpendicular to an exterior surface of the target part to facilitate de-powdering of one or more internal channels.
[0064] In any of the above aspects, the method further includes forming one or more ports oriented obliquely relative to an exterior surface of the target part to facilitate de-powdering of one or more internal channels.
[0065] In any of the above aspects, the method further includes forming the ports having a tapered shape such that a first end of each port has a diameter larger than a diameter of a second end of each port, the second ends being in fluid communication with the one or more internal channels.
[0066] In any of the above aspects, the step of printing the target part further includes forming one or more channels having a circuitous path including one or more bends, and forming a plurality of ports each extending from an outer surface of the target part to one or more internal channels formed in the target part, the plurality of ports being substantially equally spaced apart.
[0067] In any of the above aspects, printing the target part further includes forming one or more channels having a circuitous path including one or more bends, and forming a plurality of ports each extending from an outer surface of the target part to one or more internal channels formed in the target part, the plurality of ports being spaced apart a variable distance across the target part.
[0068] In any of the above aspects, the step of printing the target part further includes forming a plurality of ports spaced apart by a spacing distance within a range of about 0.5 inches (about 12 mm) to about 20 inches (508 mm), and forming a plurality of ports having a diameter within a range of about 0.03 inches (about 0.7 mm) to about 0.8 inches (about 20 mm). [Explanation of symbols]
[0069] 100 Additive Manufacturing System 104 Printhead 128 Powder bed 140 Binder Solution 150 Target Parts 151 Outer surface of target part 152 Internal Channel 156 Detour Route 158 Bend 160 Port 162 First Opening 164 Second Opening
Claims
1. A method for manufacturing a target part (150), the method comprising: Inputting (302) instructions into an additive manufacturing system (100) for additive manufacturing of a desired target part (150), the target part (150) including one or more internal channels (152); inputting the locations of one or more ports (160) to be formed, the one or more ports (160) extending from an outer surface (151) of said target part (150) to said one or more internal channels (152); printing (306) the target part (150) including the one or more ports (160) using the additive manufacturing system (100) to form a green body target part (150); de-powdering (308) the one or more internal channels (152) by accessing one or more ports (160) of the green body target part (150) to facilitate removal of residual powder from the one or more internal channels (152); The method includes:
2. The method of claim 1 , wherein the additive manufacturing system is a binder jetting system.
3. directing (310) pressurized air through one or more ports (160) to facilitate dislodging residual powder remaining within said one or more internal channels (152); inserting (312) an ultrasonic wand into one or more ports (160) to facilitate dislodging any residual powder remaining within said one or more internal channels (152); and Inserting (314) a wire brush into one or more ports (160) to facilitate dislodging any residual powder remaining within said one or more internal channels (152). The method of claim 1 , comprising at least one of the following:
4. The method of claim 1, further comprising sintering (316) the green body target part (150) after removing residual powder from the one or more internal channels (152).
5. 5. The method of claim 4, further comprising the step of brazing (318) one or more ports (160) to seal the one or more ports (160) with a braze material after removing residual powder from the one or more internal channels (152) and after sintering the green body target part (150).
6. forming one or more ports (160) oriented substantially perpendicular to an exterior surface (151) of the target part (150) to facilitate de-powdering of the one or more internal channels (152); and forming one or more ports (160) oriented obliquely relative to the outer surface (151) of the target part (150) to facilitate de-powdering of the one or more internal channels (152); The method of claim 1 , comprising at least one of:
7. 2. The method of claim 1, further comprising forming ports (160) having a tapered shape such that a first end (162) of each port (160) has a diameter (D1) greater than a diameter (D2) of a second end (164) of each port (160), the second ends (164) being in fluid communication with the one or more internal channels (152).
8. The step of printing (306) the target part (150) comprises: forming one or more interior channels (152) having a circuitous path (156) including one or more bends (158); forming a plurality of ports (160) each extending from an outer surface (151) of the target part (150) to a respective one of one or more internal channels (152) formed in the target part (150), the plurality of ports (160) being substantially equally spaced apart; The method of claim 1 further comprising:
9. The step of printing (306) the target part (150) comprises: forming one or more interior channels (152) having a circuitous path (156) including one or more bends (158); forming a plurality of ports (160) each extending from an exterior surface (151) of the target part (150) to a respective one of one or more interior channels (152) formed in the target part (150), the plurality of ports (160) being spaced apart a variable distance (L) across the target part (150); The method of claim 1 further comprising:
10. 2. The method of claim 1, wherein printing (306) the target part (150) further comprises forming a plurality of ports (160) spaced apart by a separation distance (L) within a range of about 12 mm to about 100 mm, and forming a plurality of ports (160) having a diameter (D) within a range of about 0.7 mm to about 20 mm.
11. 11. A turbine component having at least one internal channel (152) and at least one port (160) in communication with the at least one internal channel (152), the turbine component being manufactured by the method of any one of claims 1 to 10.
12. The turbine component of claim 11 , wherein the turbine component is one of an inner endwall of a turbine nozzle, an outer endwall of a turbine nozzle, or a turbine shroud.