Semiconductor device

The semiconductor device design with an N+ layer and anode trench structure effectively addresses recovery loss and breakdown voltage issues by managing carrier concentration and discharge, optimizing performance characteristics.

JP2024153183AInactive Publication Date: 2024-10-29WILL SEMICON (SHANGHAI) CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023066921
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-17
Publication Date
2024-10-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods for reducing recovery loss in semiconductor devices using lifetime killers, such as forming crystal defects, require large-scale equipment and cause issues like poor temperature characteristics and increased leakage current.

Method used

A semiconductor device design incorporating an N+ layer with a higher carrier concentration and an anode trench structure to manage carrier discharge during turn-off, reducing recovery loss and improving breakdown voltage.

Benefits of technology

The N+ layer maintains low carrier concentration at turn-off, minimizing recovery loss while the anode trench enhances breakdown voltage, achieving optimal trade-off between forward voltage drop and recovery loss.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024153183000001_ABST
    Figure 2024153183000001_ABST
Patent Text Reader

Abstract

To reduce the recovery loss.SOLUTION: A semiconductor device includes an anode electrode 20 formed on a front surface of a semiconductor base material 12, a cathode electrode 22 formed on a back surface, a P layer 16 formed on the anode electrode side 20, an N layer 14 formed on the cathode electrode 22 side, an N+ layer 26 disposed between the P layer 16 and the N layer 14 and having higher carrier concentration than the N layer 14, and an anode trench 30 extending from the front surface of the semiconductor base material 12 to a back surface thereof, penetrating the P layer 16, extending to the N+ layer 26, having an insulating film 32 between the N+ layer 26 in the periphery and the anode trench, and having a conductive material 34 disposed internally and connected to the anode electrode 20.SELECTED DRAWING: Figure 1A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a semiconductor device, and more particularly to reducing recovery loss. [Background technology]

[0002] Semiconductor devices use current control using PN junctions. A diode has a PN junction and allows current to flow from the anode on the P side to the cathode on the N side, blocking current in the opposite direction. When conducting, a large amount of carriers, holes from the anode and electrons from the cathode, are injected, lowering the forward voltage drop VF when conducting.

[0003] On the other hand, during recovery, the injected holes and electrons (carriers) are discharged to the anode and cathode, respectively, so if there is a large amount of carriers, the recovery loss Err becomes large.

[0004] Patent Document 1 discloses that a lifetime killer is provided to eliminate internal carriers, thereby speeding up the discharge of carriers. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] International Publication No. WO2017 / 146148 Summary of the Invention [Problem to be solved by the invention]

[0006] Here, the lifetime killer is provided by forming crystal defects in the semiconductor, and the processing requires large-scale equipment and work processes. Furthermore, the provision of the lifetime killer also poses the problem of poor temperature characteristics and increased leakage current. [Means for solving the problem]

[0007] The semiconductor device according to the present disclosure includes: A semiconductor substrate; an anode electrode formed on one surface of the semiconductor substrate; a cathode electrode formed on the other surface of the semiconductor substrate; A P layer formed on the anode electrode side in the semiconductor substrate; an N layer formed on the cathode electrode side of the P layer in the semiconductor substrate; an N+ layer disposed between the P layer and the N layer and having a carrier concentration higher than that of the N layer; an anode trench extending from one surface of the semiconductor substrate toward the other surface, penetrating the P layer, and extending to the N+ layer, an insulating film being formed between the N+ layer and a periphery of the anode trench, and a conductive material disposed therein is connected to the anode electrode; Includes. Effect of the Invention

[0008] According to the semiconductor device of the present disclosure, the N+ layer can reduce the concentration of carriers remaining at turn-off, and the loss at turn-off can be reduced. In addition, the electric field created by the anode trench can improve the breakdown voltage. [Brief description of the drawings]

[0009] [Figure 1A] 1 is a schematic diagram showing a cross-sectional configuration of a semiconductor device (diode) according to an embodiment. [Figure 1B] 1 is a schematic diagram showing a planar configuration of a semiconductor device (diode) according to an embodiment. [Diagram 2] The voltage and current waveforms during recovery of a typical diode are shown below. [Diagram 3] FIG. 4 is a diagram showing the relationship between recovery loss Err and forward voltage drop VF of the diode of the embodiment. [Figure 4] FIG. 1 is a diagram showing the relationship between the peak carrier concentration in the N+ layer and VF and the breakdown voltage. [Diagram 5] 1A to 1C are diagrams illustrating a manufacturing process of a semiconductor device according to an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. Note that the following embodiments do not limit the present disclosure, and configurations obtained by selectively combining multiple examples are also included in the present disclosure.

[0011] "Configuration of Semiconductor Device" Fig. 1A is a schematic diagram showing a cross-sectional configuration of a semiconductor device according to an embodiment. Fig. 1B is a plan view of the semiconductor device according to an embodiment. Note that an anode electrode 20 on the upper surface is omitted in Fig. 1B. In this example, the semiconductor device 10 is a diode.

[0012] The semiconductor device 10 includes a semiconductor substrate 12. The semiconductor substrate 12 is, for example, a silicon (Si) wafer, but may be other semiconductors such as SiC or gallium oxide. In this embodiment, an N-type FZ wafer by the FZ (Floating Zone) method doped with N-type impurities is used.

[0013] Since an N-type semiconductor substrate 12 is used, most of the semiconductor substrate 12 becomes an N layer 14. The N layer 14 is usually called an N-drift layer.

[0014] By doping P-type impurities from one surface (hereinafter referred to as the surface), a P layer 16 containing carriers (holes) is formed on the surface side of the N layer 14. The P layer 16 constitutes an anode region. Here, in this embodiment, an N+ layer 26 containing carriers (electrons) is formed on the surface side of the N layer 14 by doping with N-type impurities, and then the P layer 16 is formed. Therefore, the N+ layer 26 is formed between the N layer 14 and the P layer 16. The N+ layer 26 has a higher carrier concentration than the N layer 14.

[0015] An anode electrode 20 is formed on the surface of the semiconductor substrate 12, i.e., on the P layer 16. The anode electrode 20 is preferably made of a metal such as aluminum.

[0016] A cathode electrode 22 is formed on the other surface (hereinafter referred to as the back surface) of the semiconductor substrate 12, i.e., the back surface side of the N layer 14, via a back surface N+ layer 24 having a higher impurity concentration than the N layer 14. The cathode electrode 22 can also be made of metal, similar to the anode electrode 20. The back surface N+ layer 24 facilitates the injection of electrons from the cathode electrode 22.

[0017] Furthermore, an anode trench 30 is provided that extends from the front surface of the semiconductor substrate 12 toward the rear surface. As shown in FIG. 1B, the anode trench 30 surrounds the periphery of the P layer 16 that constitutes the anode region. In this example, the P layer 16 is divided into three parts. The anode trenches 30 are disposed on both sides of the semiconductor substrate 12. The anode trenches 30 are preferably disposed uniformly in a plan view so that a relatively uniform electric field can be applied to the surrounding N+ layer 26.

[0018] The anode trench 30 has a groove-shaped hole extending from the surface of the semiconductor substrate 12 toward the bottom surface, an insulating film 32 is formed around the hole, and a conductive material 34 is embedded inside. The conductive material 34 is directly connected to the anode electrode 20 at the top. The conductive material 34 can be made of a metal such as aluminum like the anode electrode 20, but can also be made of polysilicon or the like. The insulating film 32 can be formed by forming a hole in the semiconductor substrate 12 by anisotropic etching or the like and then oxidizing the surrounding silicon, but it may be formed by other methods. The insulating film 32 is preferably formed on the entire surface except for the top surface (the surface in contact with the anode electrode 20). That is, the insulating film 32 is provided between the P layer 16, the N+ layer 26, and the N layer 14.

[0019] Such a semiconductor device 10 functions as a diode. A forward current flows when a positive forward voltage is applied between the anode electrode 20 and the cathode electrode 22. When a reverse voltage is applied between the anode electrode 20 and the cathode electrode 22, no current flows if the applied voltage is equal to or lower than the breakdown voltage.

[0020] When a forward voltage is applied, holes are supplied from the anode electrode 20 and electrons are supplied from the cathode electrode 22. The holes supplied from the anode electrode 20 recombine with electrons in the N+ layer 26, and some of them disappear before entering the N layer 14. Electrons also flow into the N layer 14 from the cathode electrode 22, causing conductivity modulation and resulting in a low VF. That is, the N+ layer 26 reduces the number of holes moving from the P layer 16 to the N layer 14. The amount of holes entering the N layer 14 can be adjusted by the carrier concentration of the N+ layer 26, and the amount of carriers remaining in the P layer 16 and N layer 14 at the time of turn-off can be set appropriately. Therefore, it is possible to suppress switching loss at the time of turn-off while maintaining an appropriate VF at the time of on.

[0021] The semiconductor device 10 according to this embodiment can be used as a diode as it is, but can also be used in various elements incorporating a diode.

[0022] "Recovery Waveform" Fig. 2 shows the voltage and current waveforms during recovery when a typical diode switches from on to off. First, when conducting, the voltage between the anode electrode 20 and the cathode electrode 22 is a forward voltage drop VF, which is a predetermined small voltage when there are sufficient P-type and N-type carriers, and a predetermined forward current IF flows. In this example, the voltage Vrr is the cathode voltage.

[0023] Here, by applying a reverse voltage, the current IF decreases linearly. This is because holes are drawn from the N layer 14 through the P layer 16 to the anode electrode 20, and electrons are drawn to the cathode electrode 22. At this time, the current Irr once becomes significantly negative and then approaches 0, and the cathode voltage Vrr becomes significantly positive and then settles to the applied voltage.

[0024] The energy loss during recovery is Vrr*Irr*time, and the loss during the period from when Vrr becomes positive to when Irr becomes 0 is the recovery loss Err.

[0025] In this embodiment, since the residual carrier concentration at the time of turn-off is low, the time until the current Irr becomes 0 is short, and therefore the loss Err is small.

[0026] 3 is a diagram showing the relationship between the carrier concentration of the N+ layer 26 in the semiconductor device according to the embodiment and VF and Err. As described above, when the carrier concentration of the N+ layer 26 is low, the loss Err increases, and when the carrier concentration is high, VF increases. In this embodiment, VF and Err are set to appropriate values ​​by appropriately setting the carrier concentration of the N+ layer 26.

[0027] According to various studies, in the semiconductor device 10, the peak carrier concentration of the N+ layer 26 is set to 1e 17 ~3e 17 / cm 3 It has been found that desired characteristics can be obtained by setting the thickness of the insulating film to about 100 nm.

[0028] If the forward voltage is applied for a long period of time under the conditions of use, the carrier concentration of the N+ layer 26 should be lowered, and if on-off switching is repeated, the carrier concentration should be higher.

[0029] "About pressure resistance" Here, if the N+ layer 26 is provided, the breakdown voltage of the diode decreases. This is because the N+ layer 26 makes it easier for carriers to move in the reverse direction.

[0030] In this embodiment, the anode trench 30 is provided. In particular, the anode trench 30 penetrates the N+ layer 26 and extends to the N layer 14. The inside of the anode trench 30 is at the voltage of the anode electrode 20, and therefore, when a reverse voltage is applied, electrons in the N+ layer 26 are drawn away from the anode trench 30 toward the N layer 14, and a depletion layer spreads from the N+ layer 26 to the N layer 14. This can improve the breakdown voltage of the semiconductor device 10.

[0031] 5 is a diagram showing the relationship between the carrier concentration, the breakdown voltage, and VF in the semiconductor device 10 of this embodiment. As described above, in this embodiment, even if the N+ layer 26 is provided, a sufficiently high breakdown voltage can be maintained.

[0032] When the width of the mesa region between the two anode trenches 30 was 1 μm, the depth of the anode trenches 30 was 5 μm, and the bottom end of the anode trench 30 extended to the N layer 14, the breakdown voltage as shown in FIG. 5 was obtained.

[0033] If the depth of the anode trench 30 is insufficient, the depletion layer in the N+ layer 26 is insufficient, resulting in a low breakdown voltage. For this reason, if it is desired to increase the breakdown voltage, the anode trench 30 should penetrate the N+ layer 26 and reach the N layer 14. If the breakdown voltage does not need to be so high, the anode trench 30 may be terminated within the N+ layer 26.

[0034] In this manner, in this embodiment, by providing the N+ layer 26 and adjusting the carrier concentration therein, it is possible to appropriately set the trade-off between VF and Err. Also, by providing the anode trench, it is possible to ensure sufficient withstand voltage.

[0035] <Manufacturing process> 5 is a diagram showing a manufacturing process of the semiconductor device 10 according to the embodiment. First, a semiconductor substrate 12 is prepared (S11). As the semiconductor substrate 12, for example, an FZ (Floating Zone) silicon wafer of N type is used.

[0036] P-type impurities are doped (implanted) from the front surface side (S12) and then diffused (S13) to form a P- P layer 16. N-type impurities are doped (implanted) from the front surface side (S14) and then diffused (S15) to form an N+ layer 26.

[0037] Next, an anode trench 30 is formed (S16). A contact is formed (S17), and a surface electrode, i.e., an anode electrode 20, is formed on the surface (S18).

[0038] Next, the back surface side is polished (S19), and then N-type impurities are doped (S20) to form the back surface N+ layer 24. After the impurities are diffused by laser annealing (S21), the back surface electrode, i.e., the cathode electrode 22, is formed (S22).

[0039] In this manner, the semiconductor device 10 is formed, and then various inspections are carried out on it (S18), and the manufacturing process is completed. [Explanation of symbols]

[0040] 10 semiconductor device, 12 semiconductor substrate, 14 N layer, 16 P layer, 20 anode electrode, 22 cathode electrode, 24 backside N+ layer, 26 N+ layer, 30 anode trench, 32 insulating film, 34 conductive material.

Claims

1. A semiconductor substrate; an anode electrode formed on one surface of the semiconductor substrate; a cathode electrode formed on the other surface of the semiconductor substrate; A P layer formed on the anode electrode side in the semiconductor substrate; an N-layer formed on the cathode electrode side of the P-layer in the semiconductor substrate; an N+ layer disposed between the P layer and the N layer and having a higher carrier concentration than the N layer; an anode trench extending from one surface of the semiconductor substrate toward the other surface, penetrating the P layer, and extending to the N+ layer, an insulating film being formed between the N+ layer and a periphery of the anode trench, and a conductive material disposed therein is connected to the anode electrode; A semiconductor device comprising:

2. 2. The semiconductor device according to claim 1, The anode trench extends through the N+ layer to the N layer, and an insulating film is formed between the N layer and the N+ layer around the anode trench. Semiconductor device.

3. 3. The semiconductor device according to claim 1, The semiconductor substrate is made of a silicon wafer. Semiconductor device.

Citation Information

Patent Citations

  • Semiconductor device

    JP2016096222A

  • Semiconductor device

    JP2021136311A

  • Semiconductor device

    JP2023004072A

  • Semiconductor device

    WO2017146148A1