Wafer processing method

The wafer processing method forms an annular modified layer inside the wafer using a laser beam to stabilize the processing position and prevent device damage, enhancing the yield of producible devices.

JP2024153501APending Publication Date: 2024-10-29DISCO CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023067436
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-17
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

The challenge in processing three-dimensionally stacked semiconductor wafers is the difficulty in forming a modified layer along the outer periphery due to the chamfered portion's curved surface, which can lead to device damage during grinding and reduces the number of producible devices.

Method used

A wafer processing method that forms an annular modified layer inside the wafer by irradiating a laser beam with a transparent wavelength from the back surface, shaping the beam to avoid the chamfered portion and using a support wafer to stabilize the processing position, followed by grinding to a predetermined thickness.

Benefits of technology

This method suppresses device damage during grinding and increases the number of devices that can be produced by stabilizing the modified layer formation and crack control.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024153501000001_ABST
    Figure 2024153501000001_ABST
Patent Text Reader

Abstract

To provide a wafer processing method with which it is possible to suppress the breakage of a device during polishing and increase the number of devices produced.SOLUTION: The wafer processing method comprises: an annular modified layer formation step 3 in which a laser beam of a wavelength transparent to a wafer is radiated from a reverse side along a boundary region between a chamfering section formed along the outer circumference of the wafer and a flat plane constituting the surface or the reverse side, and thereby an annular modified layer is formed in the inside; and a thinning step in which the reserve side is polished until being thinned down to a prescribed thickness after carrying out the annular modified layer formation step 3. In the annular modified layer formation step 3, the cross sectional shape of the laser beam is formed into a semicircular shape, a segmental shape, a circular shape chipped to a crescent shape, or an elliptical shape before being radiated to the wafer in a condensed manner, so that a chamfering part on the radially outward of the boundary region is not irradiated with the laser beam and a flat plane on the radially inward of the boundary region is irradiated with the laser beam.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wafer processing method. [Background technology]

[0002] In recent years, the development of 3D stacked semiconductor wafers has progressed in line with the trend toward lower profile and higher integration of device chips. For example, TSV (Through-Silicon Via) wafers enable the connection of electrodes between two chips by bonding them together using through-hole electrodes.

[0003] Such wafers are ground and thinned while bonded to a support wafer (silicon, glass, ceramics, etc.) that serves as a base. Normally, the outer edge of a wafer is chamfered, so when the wafer is ground to an extremely thin thickness, the outer edge becomes a so-called knife edge, and the edge is likely to chip during grinding. This may cause the chip to extend to the device, leading to damage to the device.

[0004] As a countermeasure against the knife edge, an edge trimming method has been devised in which, after bonding the wafers together, a laser beam is irradiated along the outer edge of the device to form an annular modified layer, thereby preventing chipping of the wafer edge that occurs during grinding from extending into the device (see Patent Document 1). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2020-057709 A Summary of the Invention [Problem to be solved by the invention]

[0006] Incidentally, the processing position when forming the modified layer along the outer periphery is preferably as close to the outer periphery as possible in order to increase the number of devices that can be produced. However, since the chamfered portion formed along the outer periphery is composed of a curved surface, there is a problem that it is difficult to control the formation of the modified layer and the processing position inside the wafer.

[0007] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a wafer processing method capable of suppressing damage to devices during grinding and increasing the number of devices that can be obtained. [Means for solving the problem]

[0008] In order to solve the above-mentioned problems and achieve the object, the wafer processing method of the present invention is a wafer processing method for processing a wafer having a chamfer formed along an outer circumferential edge, and includes an annular modified layer forming step of forming an annular modified layer inside the wafer by irradiating a laser beam having a wavelength that is transparent to the wafer from the back side of the wafer along a boundary region between the chamfer and a flat surface constituting the front or back surface of the wafer, and a thinning step of grinding the back surface of the wafer to a predetermined thickness after performing the annular modified layer forming step, wherein the annular modified layer forming step is characterized in that the laser beam is focused and irradiated onto the wafer in a state in which the cross-sectional shape of the laser beam is shaped into a semicircular shape, a segmented circle shape, a crescent-shaped segmented circle shape, or an elliptical shape so that the laser beam is not irradiated onto the chamfer radially outward from the boundary region, and the laser beam is irradiated onto the flat surface radially inward from the boundary region.

[0009] In addition, the wafer processing method of the present invention may further include a measurement step of measuring the distance from the outer peripheral edge of the wafer to the boundary region between the chamfered portion and the flat surface before performing the annular modified layer formation step.

[0010] Moreover, the wafer processing method of the present invention may further include a bonding step of bonding the front surface side of the wafer to a support wafer different from the wafer before carrying out the thinning step. Effect of the Invention

[0011] The present invention can suppress damage to devices during grinding and increase the number of devices that can be obtained. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a perspective view showing an example of a wafer to be processed by the wafer processing method according to the embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along the line II-II shown in FIG. [Diagram 3] FIG. 3 is a flowchart showing a flow of the wafer processing method according to the embodiment. [Figure 4] FIG. 4 is a perspective view showing one state of the bonding step shown in FIG. [Diagram 5] FIG. 5 is an enlarged cross-sectional view of a portion of the wafer after the bonding step of FIG. [Figure 6] FIG. 6 is a side view, partly in section, showing one state of the annular modified layer forming step shown in FIG. [Figure 7] FIG. 7 is an enlarged cross-sectional view showing a part of the wafer in the annular modified layer forming step of FIG. [Figure 8] FIG. 8 is a plan view showing an example of a cross-sectional shape of a laser beam in the annular modified layer forming step of FIG. [Figure 9] FIG. 9 is a plan view showing another example of the cross-sectional shape of the laser beam in the annular modified layer forming step of FIG. [Figure 10] FIG. 10 is an enlarged cross-sectional view showing a part of a wafer in the annular modified layer forming step of a comparative example. [Figure 11] FIG. 11 is a side view, partially in section, showing one state of the thinning step shown in FIG. [Figure 12] FIG. 12 is an enlarged cross-sectional view of a portion of the wafer after the thinning step of FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] The form (embodiment) for carrying out the present invention will be described in detail with reference to the drawings. The present invention is not limited to the contents described in the following embodiment. Furthermore, the components described below include those that a person skilled in the art can easily imagine and those that are substantially the same. Furthermore, the configurations described below can be appropriately combined. Furthermore, various omissions, substitutions, or modifications of the configurations can be made without departing from the gist of the present invention.

[0014] [Embodiment] A method for processing a wafer 10 according to an embodiment of the present invention will be described with reference to the drawings. Fig. 1 is a perspective view showing an example of a wafer 10 to be processed by the method for processing a wafer 10 according to the embodiment. Fig. 2 is a cross-sectional view taken along line II-II shown in Fig. 1.

[0015] 1 and 2 is a wafer such as a disk-shaped semiconductor wafer or an optical device wafer, which has a substrate 11 made of silicon (Si), sapphire (Al2O3), gallium arsenide (GaAs), silicon carbide (SiC), or the like, and is a silicon wafer in the embodiment. The wafer 10 has a chamfered portion formed along the outer circumferential edge 12, as shown in FIG.

[0016] The wafer 10 has its front surface 13, which is the device surface, bonded to, for example, a support wafer 30 (see FIG. 4, etc.) to form a bonded wafer, and then its back surface 14 is ground to be thinned. In the wafer 10 of the embodiment, the chamfer on the back surface 14 is wider and gentler than the chamfer on the front surface 13. The back surface 14 of the wafer 10 includes an inclined surface 15 of the chamfer and a flat surface 16.

[0017] 1, the wafer 10 includes a device region 17 on the front surface 13 side of the substrate 11, and an outer peripheral region 18 surrounding the device region 17. The device region 17 has a plurality of planned division lines 19 set in a lattice pattern on the front surface 13 of the substrate 11, and devices 20 formed in each region partitioned by the planned division lines 19. The outer peripheral region 18 is a region surrounding the device region 17 all around, in which no devices 20 are formed. The boundary between the device region 17 and the outer peripheral region 18 is located at approximately the same position as a boundary region 21 between the inclined surface 15 and the flat surface 16 of the chamfered portion on the back surface 14 side.

[0018] In the embodiment, the device 20 constitutes a 3D NAND flash memory and includes an electrode pad and a through electrode connected to the electrode pad. The through electrode penetrates the back surface 14 of the substrate 11 when the substrate 11 is thinned and the devices 20 are individually separated from the wafer 10. That is, the wafer 10 of the embodiment is a so-called TSV wafer in which the individually separated devices 20 have through electrodes. The wafer 10 of the present invention is not limited to a TSV wafer having through electrodes as in the embodiment, and may be a device wafer without through electrodes.

[0019] Fig. 3 is a flow chart showing the flow of the processing method of the wafer 10 according to the embodiment. As shown in Fig. 3, the processing method of the wafer 10 according to the embodiment includes a bonding step 1, a measurement step 2, an annular modified layer forming step 3, and a thinning step 4. The processing method of the wafer 10 is a processing method in which an annular modified layer 23 is formed along a boundary region 21 between a chamfered portion (inclined surface 15) of the wafer 10 having a chamfered portion formed along the outer circumferential edge 12 and a flat surface 16, and then the back surface 14 side is ground to thin the wafer 10 to a predetermined thickness 25 and the outer circumferential region 18 is removed.

[0020] (Lamination step 1) Fig. 4 is a perspective view showing one state of the bonding step 1 shown in Fig. 3. Fig. 5 is an enlarged cross-sectional view showing a part of the wafer 10 after the bonding step 1 of Fig. 4. The bonding step 1 is a step of bonding the front surface 13 side of the wafer 10 to a support wafer 30 different from the wafer 10.

[0021] 4 is a disk-shaped substrate wafer having a substrate 31 made of silicon, glass, ceramics, or the like and the same diameter as the wafer 10, but in the present invention, it may be a TSV wafer similar to the wafer 10. The support wafer 30 has a chamfered portion formed along an outer circumferential edge 32, similar to the wafer 10. Also, in the support wafer 30 of the embodiment, the chamfered portion on the other surface 34 side is wider and gentler than the chamfered portion on one surface 33 side, which is the surface to be bonded to the wafer 10.

[0022] In the bonding step 1, first, the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are opposed to each other with a gap therebetween, as shown in Fig. 4. Next, the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are bonded together, as shown in Fig. 5. This forms a bonded wafer.

[0023] In this case, when a bonding layer is provided between the wafer 10 and the support wafer 30, the bonding layer is laminated on one of the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30, and then the front surface 13 of the wafer 10 and one surface 33 of the support wafer 30 are bonded together via the bonding layer. The bonding layer may be a double-sided tape having an adhesive layer laminated on the front and back surfaces of a base layer, an oxide film, or a layer formed by applying an adhesive containing a resin or the like. The wafer 10 and the support wafer 30 may be directly bonded together without using a bonding layer.

[0024] 3, the bonding step 1 in the embodiment is performed before the annular modified layer forming step 3, but may be performed after the measurement step 2 and before the annular modified layer forming step 3. Also, the bonding step 1 may be performed after the annular modified layer forming step 3 and before the thinning step 4.

[0025] In the processing method of the wafer 10 of the embodiment, each processing of the wafer 10 is performed in a state where the support wafer 30 is bonded to the front surface 13 side of the wafer 10, but the wafer 10 processed in the present invention is not necessarily limited to the wafer 10 constituting a bonded wafer, and a single wafer 10 may be processed. In other words, the bonding step 1 does not have to be performed.

[0026] (Measurement step 2) The measuring step 2 is a step of measuring a distance 22 (see FIG. 5 ) from the outer peripheral edge 12 of the wafer 10 to a boundary region 21 between the chamfered portion (inclined surface 15) and the flat surface 16. The measuring step 2 is performed before performing the annular modified layer forming step 3. The measuring step 2 in the embodiment is performed after performing the bonding step 1, but may be performed before performing the bonding step 1.

[0027] The measuring step 2 is performed, for example, in a state where the wafer 10 is held via the support wafer 30 on the holding table 41 of the laser processing device 40 which performs the annular modified layer forming step 3 described later (see FIG. 6). In the measuring step 2, first, the positions of the outer periphery 12 and the boundary region 21 are detected, and then the distance 22 between the outer periphery 12 and the boundary region 21 is calculated. The position of the outer periphery 12 is detected, for example, by using an imaging unit. The position of the outer periphery 12 may be calculated based on a known diameter of the wafer 10 on the premise that the center of the wafer 10 is accurately aligned with the axis of the holding table 41. Note that even if the center of the wafer 10 is not accurately aligned with the axis of the holding table 41, the center and diameter of the wafer 10 can be calculated from the coordinate positions of three or more points of the outer periphery 12 of the wafer 10, and the positional deviation from the axis of the holding table 41 can be detected, so that the subsequent processing can be performed based on the calculated center of the wafer 10.

[0028] An example of a method for detecting the position of the boundary region 21 is a method using an imaging unit. The imaging unit is, for example, mounted on a laser processing device 40 that performs the annular modified layer formation step 3 described below, and is an imaging unit for imaging the wafer 10. The imaging unit images the back surface 14 side of the wafer 10 from a direction perpendicular to the back surface 14, with the focus on the flat surface 16. At this time, the inclined surface 15 of the chamfered portion is out of focus, so the boundary between the in-focus and out-of-focus portions can be recognized as the boundary region 21.

[0029] Also, as a method for detecting the position of the boundary region 21, for example, a method using a non-contact height sensor can be mentioned. The non-contact height sensor is mounted on a laser processing device 40 that performs the annular modified layer formation step 3 described below, and is a non-contact height sensor for measuring the thickness of the wafer 10. The non-contact height sensor measures the height of the back surface 14 of the wafer 10. At this time, since the height of the inclined surface 15 of the chamfered portion is lower than that of the flat surface 16, the boundary between the portion with a substantially constant height and the portion with a lower height can be recognized as the boundary region 21.

[0030] Calculation of distance 22 between outer periphery 12 and boundary region 21 may be performed, for example, by a control device mounted on laser processing device 40 that performs annular modified layer formation step 3 described below and that controls each part. Detection of boundary region 21 and calculation of distance 22 between outer periphery 12 and boundary region 21 may be performed at one point in the circumferential direction of wafer 10, or may be performed at multiple points and averaged.

[0031] (Annular modified layer formation step 3) FIG. 6 is a side view showing, in partial section, one state of the annular modified layer forming step 3 shown in FIG. 3. FIG. 7 is a cross-sectional view showing an enlarged portion of the wafer 10 in the annular modified layer forming step 3 of FIG. 6. FIG. 8 is a plan view showing an example of the cross-sectional shape of the laser beam 43 in the annular modified layer forming step 3 of FIG. 6. FIG. 9 is a plan view showing another example of the cross-sectional shape of the laser beam 43 in the annular modified layer forming step 3 of FIG. 6. The annular modified layer forming step 3 is a step of forming an annular modified layer 23 inside the wafer 10 by irradiating a laser beam 43 having a wavelength that is transparent to the wafer 10 from the back surface 14 side of the wafer 10 along a boundary region 21 between the chamfered portion (inclined surface 15) and the flat surface 16.

[0032] Here, the modified layer 23 means a region in which the density, refractive index, mechanical strength or other physical properties are different from those of the surrounding area as a result of irradiation with the laser beam 43. The modified layer 23 is, for example, a melting process region, a crack region, a dielectric breakdown region, a refractive index change region, a region in which these regions are mixed, etc. The modified layer 23 has a lower mechanical strength, etc. than other parts of the wafer 10.

[0033] In the annular modified layer forming step 3 of the embodiment, an annular modified layer 23 is formed inside the wafer 10 by stealth dicing using a laser processing device 40. The laser processing device 40 includes a holding table 41, a laser beam irradiation unit 42, a moving unit (not shown) that moves the holding table 41 and the laser beam irradiation unit 42 relatively, and an imaging unit (not shown) that images the wafer 10 held on the holding table 41 via the support wafer 30.

[0034] The holding table 41 holds the wafer 10 on a holding surface (upper surface) via the support wafer 30, and is rotatable around a vertical axis. The laser beam irradiation unit 42 irradiates a laser beam 43 onto the wafer 10 held on the holding table 41 via the support wafer 30. The laser beam irradiation unit 42 has, for example, a laser oscillator, a collector that condenses and irradiates the laser beam 43 emitted from the laser oscillator onto the wafer 10 held on the holding table 41 via the support wafer 30, and various optical components that propagate the laser beam 43 from the laser oscillator to the collector.

[0035] The laser beam irradiation unit 42 also has a shaping means between the laser oscillator and the condenser for shaping the cross-sectional shape of the laser beam 43 irradiated onto the wafer 10. The shaping means includes, for example, a spatial light modulator such as LCOS (Liquid-Crystal on Silicon) for controlling the wavefront, and a pinhole for blocking a part of the laser beam 43. The laser beam 43 is shaped into, for example, a semicircular shape (irradiation area 45) shown in Fig. 8 or a segmented circular shape (irradiation area 45-1) shown in Fig. 9.

[0036] In the annular modified layer forming step 3, a laser beam 43 is irradiated from the back surface 14 side of the wafer 10 to form an annular modified layer 23 inside the wafer 10 along the boundary region 21 between the chamfered portion (inclined surface 15) and the flat surface 16. The laser beam 43 is a laser beam having a wavelength that is transparent to the wafer 10, such as infrared rays (IR).

[0037] In the annular modified layer forming step 3, first, the other surface 34 of the support wafer 30 is sucked and held on the holding surface (upper surface) of the holding table 41. If the measurement step 2 is performed on the holding table 41, this procedure is omitted. Next, the wafer 10 is aligned with the condenser of the laser beam irradiation unit 42. Specifically, the holding table 41 is moved to the processing area below the laser beam irradiation unit 42 by a moving unit (not shown).

[0038] Next, the wafer 10 is photographed and aligned by an imaging unit (not shown), and the irradiation portion of the laser beam irradiation unit 42 is vertically opposed to the boundary region 21 between the chamfered portion (inclined surface 15) of the back surface 14 of the wafer 10 and the flat surface 16, and then the focal point 44 of the laser beam 43 is set inside the wafer 10. At this time, in the irradiation region 45 of the laser beam 43, the notches 46, 46-1 that become the chords of the semicircular or notched circular shape are aligned so as to face radially outward of the wafer 10. As shown in FIG. 7, the position of the focal point 44 may be set slightly radially inward of the wafer 10 from the boundary region 21.

[0039] In the annular modified layer forming step 3, next, a laser beam 43 is irradiated from a laser beam irradiation unit 42 onto the back surface 14 of the wafer 10 while rotating the holding table 41 around a vertical axis. In this manner, the laser beam 43 is annularly irradiated along the boundary region 21 with a focal point 44 positioned at a predetermined distance inside the outer circumferential edge 12 of the wafer 10, thereby forming an annular modified layer 23 inside the wafer 10.

[0040] A crack 24 extends from the modified layer 23 formed by the irradiation of the laser beam 43, and a cylindrical splitting starting point having a side perpendicular to the surface 13 is formed from inside the wafer 10. In the annular modified layer forming step 3, it is preferable to irradiate the laser beam 43 so that the crack 24 extending from the modified layer 23 appears on the surface 13. Note that "perpendicular to the surface 13 of the wafer 10" means that the inclination of an approximation plane obtained by approximating the entirety of the extended crack 24 to a plane relative to the vertical plane is within ±5 degrees, preferably within ±2 degrees.

[0041] In the annular modified layer forming step 3, the height of the focal point 44 of the laser beam 43 may be changed in the thickness direction of the wafer 10 and the laser beam 43 may be irradiated multiple times, i.e., after the laser beam 43 having one focal point 44 is irradiated once along the boundary region 21 of the wafer 10, the height of the focal point 44 may be changed in the thickness direction of the wafer 10 and the laser beam 43 may be irradiated similarly multiple times to form multiple modified layers 23 in an annular shape and in a direction perpendicular to the surface 13 of the wafer 10. Alternatively, multiple modified layers 23 may be formed in a direction perpendicular to the surface 13 of the wafer 10 by irradiating the laser beam 43 having multiple focal points 44 spaced apart in the thickness direction of the wafer 10.

[0042] In the above description, as shown in Figs. 8 and 9, an example was given in which the laser beam 43 was shaped into a semicircular or partially circular shape, but the irradiation area 45, 45-1 of the laser beam 43 may have another shape as long as it is a circular shape with a part of the outer periphery 12 side missing. That is, it is preferable that the irradiation area 45, 45-1 of the laser beam 43 is not present on the outer periphery 12 side of the boundary area 21, and the optical axis of the laser beam 43 is as close to the boundary area 21 as possible. Therefore, for example, the irradiation area 45 shown in Fig. 8 is a semicircular shape with a semicircle of the same diameter missing from a perfect circle, and the irradiation area 45-1 shown in Fig. 9 is a partially circular shape with a bow of the same diameter missing from a perfect circle, but it may be a shape with a crescent shape missing from a perfect circle. Alternatively, it may be an elliptical shape having a minor axis in the radial direction of the wafer 10.

[0043] Here, a comparative example of the annular modified layer forming step 3 will be described. Fig. 10 is an enlarged cross-sectional view showing a part of the wafer 10 in the comparative example of the annular modified layer forming step 3. In the comparative example of the annular modified layer forming step 3, the cross-sectional shape of the laser beam 43-1 irradiated to the back surface 14 side of the wafer 10 is a perfect circle.

[0044] In the example shown in Fig. 10, the focal point 44-1 is positioned radially inward from the boundary region 21 so that the laser beam 43-1, which has a circular cross-sectional shape, is not irradiated onto the chamfered portion (inclined surface 15). The position of the focal point 44-1 shown in Fig. 10 is radially inward from the position of the focal point 44 in the embodiment shown in Fig. 7. For this reason, the device region 17, which is the region inside the modified layer 23 to be formed, is smaller than in the embodiment, and the number of devices 20 that can be obtained is reduced.

[0045] For example, when forming the modified layer 23 by setting the focal point 44-1 of the laser beam 43-1 having a circular cross-sectional shape at the same position as the focal point 44 in the embodiment shown in Fig. 7, a part of the laser beam 43-1 irradiated to the rear surface 14 side is also irradiated to the inclined surface 15 radially outward from the boundary region 21. When the laser beam 43-1 is incident on a curved surface in this manner, it becomes difficult to control the focusing of the laser beam 43-1, and the formation position of the modified layer 23 may be unintentionally shifted or an unstable modified layer 23 may be formed, which may cause the crack 24 to extend toward the device region 17 side.

[0046] (Thinning Step 4) Fig. 11 is a side view, partially in cross section, showing one state of the thinning step 4 shown in Fig. 3. Fig. 12 is an enlarged cross-sectional view showing a part of the wafer 10 after the thinning step 4 of Fig. 11. The thinning step 4 is performed after the annular modified layer forming step 3 is performed. The thinning step 4 is a step of grinding the back surface 14 of the wafer 10 to thin it down to a predetermined thickness 25.

[0047] In the thinning step 4 of the embodiment, the back surface 14 of the wafer 10 is ground by a grinding device 50 to thin the wafer 10 to a predetermined thickness 25. The grinding device 50 includes a holding table 51, a grinding unit 52, and a moving unit (not shown) that moves the holding table 51 and the grinding unit 52 relative to each other.

[0048] The holding table 51 holds the wafer 10 by suction on its holding surface (upper surface) via the support wafer 30, and rotates around a vertical axis. The grinding unit 52 includes a spindle 53 which is a rotating shaft member, a grinding wheel 54 attached to the lower end of the spindle 53, a grinding stone 55 attached to the lower surface of the grinding wheel 54, and a grinding water supply unit (not shown). The spindle 53 and the grinding wheel 54 rotate on a rotation axis parallel to the axis of the holding table 51. The diameter of the grinding wheel 54 is at least larger than the radius of the wafer 10.

[0049] In the thinning step 4, first, the other surface 34 of the support wafer 30 is suction-held on the holding surface (upper surface) of the holding table 51. Next, the wafer 10 held on the holding table 51 via the support wafer 30 is aligned with the grinding wheel 54. Specifically, the holding table 51 is moved to the processing area below the grinding wheel 54 by a moving unit (not shown), and the grinding wheel 55 is brought into opposition to the back surface 14 of the wafer 10.

[0050] Next, while the holding table 51 is rotated about its axis, the grinding wheel 54 is rotated about its axis. Grinding water is supplied to the processing point by a grinding water supply unit (not shown), and the grinding wheel 55 of the grinding wheel 54 is brought closer to the holding table 51 at a predetermined feed speed, whereby the back surface 14 side of the wafer 10 is ground by the grinding wheel 55, thinning the wafer 10 to a predetermined thickness 25 shown in Fig. 12. At this time, the region (outer peripheral region 18) on the outer peripheral edge 12 side of the modified layer 23 of the wafer 10 is removed by the grinding load.

[0051] As described above, the processing method of the wafer 10 according to the embodiment forms the annular modified layer 23 inside the wafer 10, which serves as a division starting point for removing the outer peripheral region 18. Here, the irradiation regions 45, 45-1 to which the laser beam 43 for forming the modified layer 23 is irradiated are in the vicinity of the outer peripheral edge 12, and therefore may be set in the chamfered portion of the outer peripheral edge 12, i.e., the inclined surface 15.

[0052] When the inclined surface 15 is irradiated with the laser beam 43, the thickness of the wafer 10 in the irradiated area is not constant, so that the height position of the modified layer 23 to be formed may be unintentionally shifted. In addition, when the laser beam 43 is incident on the inclined surface 15, which is a curved surface, it is diffusely reflected, so that the modified layer 23 may not be formed stably.

[0053] In contrast to this, in the embodiment, in the annular modified layer forming step 3, the cross-sectional shape of the laser beam 43 irradiated to the back surface 14 of the wafer 10 is made semicircular, semicircular, crescent-shaped, or elliptical. That is, the laser beam 43 is shaped so that it is not irradiated to the chamfered portion, and the laser beam 43 is irradiated along the boundary region 21 between the chamfered portion (inclined surface 15) and the flat surface 16.

[0054] This eliminates the influence of unstable modified layer 23 and cracks 24 that may be formed inside wafer 10 when laser beam 43 is irradiated to the chamfered portion, and enables stable formation of modified layer 23 and cracks 24. In addition, since the optical axis of laser beam 43 can be set in the vicinity of boundary region 21, modified layer 23 and cracks 24 can be formed in the vicinity of boundary region 21, which has the effect of suppressing damage to devices 20 while increasing the number of devices 20 that can be obtained.

[0055] It should be noted that the present invention is not limited to the above-described embodiment and modifications, and can be practiced in various forms without departing from the spirit of the present invention.

[0056] For example, in order to facilitate removal of the outer circumferential region 18 in the thinning step 4, laser processing for dividing the outer circumferential region 18 into a plurality of regions in advance may be performed prior to the thinning step 4. In this case, for example, the outer circumferential region 18 may be divided radially by forming a radial modified layer in the outer circumferential region 18 by stealth dicing.

[0057] Alternatively, the outer peripheral region 18 may be removed by applying an external force. The external force may be, for example, a mechanical external force such as an external force in the shear direction caused by pressing the outer peripheral region 18 from above or lifting the outer peripheral region 18, or crushing by a roller, or may be an external force in the radial direction caused by vibration due to ultrasonic waves, a collision force between at least one of a liquid and a solid when sprayed onto the outer peripheral region 18, or expanding an expand tape attached to the ground finish surface of the wafer 10. [Explanation of symbols]

[0058] 10 wafers 11 Substrate 12 Outer rim 13 Surface 14 Back side 15 Slope 16 flat surface 17 Device Area 18 Outer area 19 Division line 20 Devices 21 Boundary area 22 distance 23 Modification layer 24 Crack 25 Thickness 30 Support Wafer 43, 43-1 Laser beam 44, 44-1 Focus point

Claims

1. A wafer processing method for processing a wafer having a chamfered portion formed along an outer periphery, comprising: an annular modified layer forming step of forming an annular modified layer inside the wafer by irradiating a laser beam having a wavelength that is transparent to the wafer from the back side of the wafer along a boundary region between the chamfered portion and a flat surface that constitutes the front or back surface of the wafer; After the annular modified layer forming step is performed, a thinning step of grinding the back surface of the wafer to a predetermined thickness, In the annular modified layer forming step, The laser beam is focused and irradiated onto the wafer in a state in which the cross-sectional shape of the laser beam is formed into a semicircular shape, a partially cut circle shape, a circle cut into a crescent shape, or an elliptical shape, so that the laser beam is not irradiated onto the chamfered portion radially outward from the boundary region, and the laser beam is irradiated onto the flat surface radially inward from the boundary region. A wafer processing method comprising the steps of:

2. Before carrying out the annular modified layer forming step, The method further includes a measuring step of measuring a distance from the outer periphery of the wafer to the boundary region between the chamfer and the flat surface.

2. The wafer processing method according to claim 1 .

3. Prior to carrying out the thinning step, The method further includes a bonding step of bonding the front side of the wafer to a support wafer different from the wafer.

3. The wafer processing method according to claim 1 or 2.

Citation Information

Patent Citations

  • Laser machining method for wafer and device thereof

    JP2006319198A

  • Parting method of semiconductor substrate, and semiconductor chip manufactured thereby

    JP2007258236A

  • Device and method for inspecting test object

    JP2008216054A

  • Wafer processing method

    JP2016076524A

  • Substrate processing system and substrate processing method

    WO2019208359A1