Elastic wave device and method for manufacturing the same
By incorporating a resin support layer with higher thermal conductivity and a structured internal space, the acoustic wave device addresses poor heat dissipation, ensuring efficient operation and manufacturability.
Patent Information
- Application Number
- JP2023067605
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-18
- Publication Date
- 2024-10-30
AI Technical Summary
Existing acoustic wave devices with a Wafer Level Package (WLP) structure face poor heat dissipation due to the low thermal conductivity of piezoelectric materials like lithium tantalate and lithium niobate, which are commonly used.
A resin support layer with higher thermal conductivity is introduced, comprising a lower layer made of non-photosensitive resin and an upper layer made of photosensitive resin, with a structured internal space to enhance heat dissipation, and a through hole for improved thermal pathways.
The improved thermal conductivity of the support layer enhances heat dissipation in the device chip, allowing for efficient operation and easier manufacturing through photolithography.
Smart Images

Figure 2024154027000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an acoustic wave device suitable for use as a frequency filter in mobile communication devices and the like, and to an improvement in a manufacturing method thereof. [Background technology]
[0002] A surface acoustic wave (SAW) device having a wafer level package (WLP) structure has a structure disclosed in Patent Document 1. In the device disclosed in Patent Document 1, a cover is provided on one surface of a device chip, and an IDT electrode formed on the one surface is positioned in an internal space formed by the cover. Here, the input of signals to the acoustic wave device generates heat in the device chip, but the piezoelectric material that makes up the device chip has low thermal conductivity and poor heat dissipation. The thermal conductivity of lithium tantalate and lithium niobate used as piezoelectric materials is approximately 4 to 6 W / mK. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2002-217673 A Summary of the Invention [Problem to be solved by the invention]
[0004] The main problem that the present invention aims to solve is to provide a new structure and a manufacturing method thereof that can rationally improve the heat dissipation of the device chip that constitutes this type of WLP structure acoustic wave device. [Means for solving the problem]
[0005] In order to achieve the above object, from a first aspect, the present invention provides an acoustic wave device comprising: An acoustic wave device comprising a device chip having a functional element including an IDT electrode formed on one surface thereof, a resin cover layer supported on the one surface thereof via a resin support layer, and the functional element being positioned in an internal space formed between these three elements, the support layer is composed of a lower layer portion in contact with the one surface of the device chip, and an upper layer portion located between the cover layer and the lower layer portion in contact with both of them, The lower layer is made of a resin having a higher thermal conductivity than a resin constituting the upper layer and being non-photosensitive; The upper layer is made of a photosensitive resin.
[0006] One aspect of the present invention is to form a bump within a through hole that penetrates the cover layer and the support layer and positions at the bottom of the hole a bump pad formed on one surface of the device chip and connected to the functional element.
[0007] Another aspect of the present invention is that, in a cross section along the one surface of the device chip, the cross-sectional area of the internal space is made larger at the formation level of the lower layer than at the formation level of the upper layer.
[0008] In order to achieve the above object, from a second standpoint, the present invention provides a method for manufacturing an acoustic wave device, comprising the steps of: A method for manufacturing the acoustic wave device, comprising the steps of: a first step of forming the functional elements, wiring, and bump pads on one surface of a wafer that will become the device chip; a second step of forming a first resin layer that will become the lower layer portion on the one surface of the wafer that has been subjected to the first step; a third step of forming a second resin layer to be the upper layer portion on the first resin layer formed in the second step; a fourth step of exposing a region of the second resin layer formed in the third step other than a region located on a formation region of the functional element; a fifth step of removing an area of the second resin layer other than the exposed area by development; and a sixth step of etching the first resin layer using the exposed area of the second resin layer as a mask after the fifth step to form a space that becomes the internal space at the formation level of the lower layer portion. Effect of the Invention
[0009] In the present invention, the lower layer portion of the support layer can be used to rationally improve the heat dissipation of the device chip, and an acoustic wave device including such a lower layer portion of the support layer can be easily and appropriately manufactured. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a plan configuration diagram of an acoustic wave device (first example) according to an embodiment of the present invention, in which bumps are omitted. [Diagram 2] FIG. 2 is a cross-sectional view taken along line AA in FIG. 1, with bumps indicated by dashed lines. [Diagram 3] FIG. 3 is a configuration diagram showing an example of a functional element formed on a device chip constituting the first example. [Figure 4] FIG. 4 is a configuration diagram showing an example of a circuit formed on the device chip of the first example. [Diagram 5] FIG. 5 is a cross-sectional view showing the main part of the manufacturing process of the first example. [Figure 6] FIG. 6 is a cross-sectional view showing the main part of the manufacturing process of the first example. [Figure 7] FIG. 7 is a cross-sectional view showing the main part of the manufacturing process of the first example. [Figure 8] FIG. 8 is a cross-sectional view showing the main part of the manufacturing process of the first example. [Figure 9] FIG. 9 is a cross-sectional view showing the main part of the manufacturing process of the first example. [Figure 10]FIG. 10 is a cross-sectional view showing the main part of the manufacturing process of the first example. [Figure 11] FIG. 11 is a cross-sectional view showing the main part of the manufacturing process of the first example. [Figure 12] FIG. 12 is a cross-sectional view showing the main part of the manufacturing process of the first example. [Figure 13] FIG. 13 is a cross-sectional view of a second example of an acoustic wave device having a support layer with a different structure from that of the first example, in which bumps are indicated by dashed lines. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, exemplary embodiments of the present invention will be described with reference to Figures 1 to 13. An acoustic wave device 1 according to this embodiment is suitable for use as a frequency filter in a mobile communication device or the like.
[0012] The acoustic wave device 1 has: A device chip 2; A functional element 6 such as an IDT electrode 6b formed on one surface 2a of the device chip 2; A support layer 3 (wall) formed on the surface 2a so as to surround the functional element 6; The device chip 2 is formed on the support layer 3, and the cover layer 4 (roof) cooperates with the support layer 3 to form an internal space 5 (cavity, hollow structure) that hermetically seals the functional element 6.
[0013] Typically, the device chip 2 is configured in the shape of a square (rectangular in the illustrated example) plate with a side measuring 0.5 to 1 mm and a thickness of 0.15 to 0.2 mm. Furthermore, typically, the support layer 3 is configured to have a thickness in a direction perpendicular to one surface 2a of the device chip 2 (the height of the support layer 3 based on one surface 2a of the device chip 2) of 10 to 30 μm. Typically, the cover layer 4 is configured to have a thickness of 15 to 35 μm. The acoustic wave device 1 constructed from these components typically has a thickness of about 0.25 to 0.35 mm.
[0014] As shown in FIG. 1, the acoustic wave device 1 has a square or rectangular outline when viewed from a direction perpendicular to the surface 2a of the device chip 2. That is, the acoustic wave device 1 has a flat hexahedral shape having two rectangular faces 1a, 1b and four side faces 1c extending between the two faces 1a, 1b. In each drawing, the thickness of each component of the acoustic wave device 1 is exaggerated to make the configuration of the device easier to understand.
[0015] The cross-sectional structure of the acoustic wave device 1 is shown in Fig. 2. In the figure, reference numeral 6 denotes a functional element, reference numeral 5 denotes an internal space, reference numeral 3 denotes a support layer, reference numeral 4 denotes a cover layer, and reference numeral 7 denotes a bump for connecting the functional element 6 to the outside via wiring 9 (see Fig. 4) and bump pads 10.
[0016] A plurality of functional elements 6 are formed on one surface 2a of the device chip 2. The formation area of each functional element 6 on one surface 2a of the device chip 2 is surrounded by a support layer 3 and is covered with a cover layer 4 formed on the support layer 3. This gives the acoustic wave device 1 a plurality of internal spaces 5. The support layer 3 and the cover layer 4 are made of an insulating synthetic resin.
[0017] The device chip 2 has a function of propagating elastic waves. Typically, lithium tantalate or lithium niobate is used as a piezoelectric material in the device chip 2, and the device chip 2 may be configured by laminating sapphire, silicon, alumina, spinel, quartz crystal, glass, or the like on the piezoelectric material.
[0018] 3 shows a resonator 6a as an example of the functional element 6. The resonator 6a has an IDT electrode 6b and a reflector 6e formed to sandwich the IDT electrode 6b. The IDT electrode 6b is composed of an electrode pair, and each electrode pair is formed by connecting a plurality of electrode fingers 6c arranged in parallel so that their length direction crosses the propagation direction x of the elastic wave with one end side of the electrode fingers by a bus bar 6d. The reflector 6e is formed by connecting ends of a plurality of electrode fingers 6f arranged in parallel so that their length direction crosses the propagation direction x of the elastic wave with a bus bar 6g. Such a functional element 6 is typically made of a conductive metal film formed by photolithography.
[0019] Fig. 4 shows the concept of an example of a circuit provided on one device chip 2. Reference numeral 6aa denotes a resonator 6a connected in series between input and output ports, reference numeral 6ab denotes a resonator 6a connected in parallel between input and output ports, and reference numeral 8 denotes a ground. The number and arrangement of functional elements 6 can be changed as necessary. In other words, a ladder-type filter is configured by the circuit in Fig. 4. The bump pads 10 are connected to wiring 9 that constitutes the circuit. The wiring 9 and the bump pads 10 are also typically formed on one surface 2a of the device chip 2 by a conductive metal film formed by photolithography technology.
[0020] In the acoustic wave device of this embodiment, the support layer 3 is composed of a lower layer 3a that contacts the one surface 2a of the device chip 2, and an upper layer 3b that is located between the cover layer 4 and the lower layer 3a and contacts both of them. At the same time, the lower layer 3a is made of a resin that has a higher thermal conductivity than the resin that constitutes the upper layer 3b and is non-photosensitive. On the other hand, the upper layer 3b is made of a photosensitive resin.
[0021] When a signal is input to the acoustic wave device, heat is generated in the device chip 2. However, the piezoelectric material constituting the device chip 2 has low thermal conductivity and poor heat dissipation properties. If the entire support layer 3 is made of a resin with high thermal conductivity, the heat dissipation properties of the device chip 2 can be improved. Such resins with high thermal conductivity contain fillers made of highly thermally conductive materials in the range of 70wt% to 90wt% of the base resin. Such fillers are typically formed as granules with a diameter of about 10μm. However, the resin with increased thermal conductivity has reduced photosensitivity, so if the entire support layer 3 is made of a resin with high thermal conductivity, it becomes difficult to form the internal space 5 above the formation region of the functional element in the device chip 2 by using photolithography technology. In the acoustic wave device of this embodiment, a first resin layer 12, which will become the lower layer 3a, described below is formed on one surface 2a of the device chip 2, and then a second resin layer 13, which will become the upper layer 3b, described below is formed.The second resin layer 13 is then patterned by exposure and development, and the first resin layer 12 is then etched using the patterned second resin layer 13 as a mask, so that the internal space 5 can be formed using photolithography technology, while increasing the thermal conductivity of the lower layer 3a of the support layer 3, which is in direct contact with one surface 2a of the device chip 2, and improving the heat dissipation properties of the device chip 2.
[0022] The resin constituting the lower layer 3a can typically be an epoxy resin containing a filler or a phenolic resin containing a filler. The filler can typically be alumina, aluminum nitride, or diamond powder. On the other hand, the resin constituting the upper layer portion 3b can typically be a photosensitive epoxy resin or a photosensitive phenol resin.
[0023] In this embodiment, the acoustic wave device 1 has a through hole 11 that penetrates the cover layer 4 and the support layer 3 and that positions at the bottom of the through hole a bump pad 10 that is formed on the one surface 2a of the device chip 2 and connected to the functional element 6. A metallic bump 7 is formed in the through hole 11. In the illustrated example, the through holes 11 are formed at the four corners of the acoustic wave device 1. The upper hole portion 11a of each of the through holes 11 is formed by removing a part of the upper layer portion 3b by the patterning, and the lower hole portion 11b is formed by removing a part of the lower layer portion 3a by etching using the upper hole portion 11a. A heat dissipation path from the device chip 2 is formed by the bumps 7 formed in the passing holes 11 thus formed and the lower layer portions 3 a of the support layer 3 that contact the bumps 7 in the passing holes 11 .
[0024] In the first example shown in FIGS. 1 to 12, the cross-sectional area of the internal space 5 is made substantially equal in any position in the cross section in the direction perpendicular to one surface 2a of the device chip 2. That is, in the first example, the side surface 3e facing the internal space 5 extending between the lower surface 3c fixed to one surface 2a of the device chip 2 in the support layer 3 and the upper surface 3d fixed to the roof layer is positioned on a virtual surface y (see Figure 2) perpendicular to one surface 2a of the device chip 2.
[0025] In contrast, in the second example shown in Figure 13, in a cross section along the one surface 2a of the device chip 2, the cross-sectional area of the internal space 5 is larger at the formation level L2 of the lower layer 3a (see Figure 13) than at the formation level L1 of the upper layer 3b (see Figure 13). That is, in the second example, at any position around the center z of the internal space 5 (see Figure 13), the upper layer side surface 3g extending between the upper surface 3d of the support layer 3 and the fixing portion 3f of the upper layer portion 3b to the lower layer portion 3a is located closer to the center z of the internal space 5 than the lower layer side surface 3h extending between the lower surface 3c of the support layer 3 and the fixing portion 3f, so that a step surface 3i facing one surface 2a of the device chip 2 is formed between this upper layer side surface 3g and the lower layer side surface 3h. This second example can be achieved by using the second resin layer 13 patterned as described above as a mask, so to speak, to etch the first resin layer 12 while adjusting conditions such as time and temperature. In the case of this second example, the bonding area between the support layer 3 and the cover layer 4 can be secured as wide as possible to enhance the mechanical integrity of the two, while the cross-sectional area of the internal space 5 below, i.e., the area of the formation region of the functional element 6, can be secured as wide as possible.
[0026] The acoustic wave device 1 described above can be appropriately and efficiently manufactured by a manufacturing method including the following steps.
[0027] First, the functional elements 6, wiring 9 (not shown), and bump pads 10 are formed on one surface of a wafer 14 that will become the device chip 2 (FIG. 5 / first step).
[0028] Next, a first resin layer 12 that becomes the lower layer portion 3a is formed on the one surface of the wafer 14 that has been subjected to the first step (FIG. 6 / second step). The first resin layer 12 can be formed by laminating a sheet (film) made of a resin that has high thermal conductivity and is non-photosensitive on one surface of the wafer 14 and integrating the two. Alternatively, the first resin layer 12 can be formed by applying a resin having high thermal conductivity, being non-photosensitive, and having coatable properties to one surface of the wafer 14 .
[0029] Next, a second resin layer 13 which becomes the upper layer portion 3b is formed on the first resin layer 12 formed in the second step (FIG. 7 / third step). The second resin layer 13 can be formed by laminating a sheet (film) made of a photosensitive resin on the first resin layer 12 and integrating the two together. Alternatively, the second resin layer 13 can be formed on the first resin layer 12 by applying a resin that is photosensitive and has coatable properties.
[0030] Next, a region 16 of the second resin layer 13 formed in the third step other than the region located above the formation region of the functional element 6 is exposed (FIG. 8 / fourth step). In FIG. 8, reference numeral 15 denotes a mask covering the region located above the formation region. At this time, the portion where the through hole 11 of the bump 7 is to be formed is also excluded from the exposure target.
[0031] Next, the areas of the second resin layer 13 other than the exposed area 16 are removed by development (FIG. 9 / fifth step). That is, the second resin layer 13 on the region where the functional element 6 is formed and the second resin layer 13 directly above the bump pad 10 (the portion where the through hole 11 is formed) are dissolved in a developer and removed.
[0032] Next, after the fifth step, the first resin layer 12 is etched using the exposed area 16 of the second resin layer 13 as a mask to form a space 5a that will become the internal space 5 at the formation level of the lower layer portion 3a (Figure 10 / sixth step).
[0033] After the sixth step, the first resin layer 12 and the second resin layer 13 are hardened by a reflow treatment or the like, and the formation of the support layer 3 is completed.
[0034] Thereafter, the cover layer 4 is formed on the support layer 3 to form the internal space 5 (FIG. 11). The cover layer 4 is typically formed by laminating a sheet (film) made of a photosensitive resin on the support layer 3 and integrating it with the support layer 3. At the location where the passing holes 11 for the bumps 7 are to be formed, a part of the cover layer 4 is removed by photolithography.
[0035] Cream solder is typically applied and filled into the through hole 11 thus formed using a printer, and a columnar bump 7 is formed by a subsequent reflow process, which is tall enough to protrude from the outer surface of the cover layer 4 (Figure 12).
[0036] Thereafter, the wafer 14 is diced to produce acoustic wave devices 1 having a plurality of the above-described structures from the wafer 14.
[0037] Of course, the present invention is not limited to the above-described embodiments, but includes all embodiments that can achieve the object of the present invention. [Explanation of symbols]
[0038] 1. Acoustic Wave Devices 1a, 1b side 1c side 2. Device chip 2a one side 3 Support layer 3a Lower part 3b upper management 3c Bottom surface 3d top view 3e side 3f Fixation part 3g Upper side 3h Lower side 3i Step surface 4 Cover Layer 4a Exterior 4b Inner surface 5. Interior Space 5a Space 6 Functional elements 6a, 6aa, 6ab resonator 6b IDT electrode 6c electrode finger 6d Busbar 6e reflector 6f electrode finger 6g busbar 7. Bump 8 Grand 9 Wiring 10 Bump Pad 11 Passing hole 11a Upper hole 11b Lower hole 12 First resin layer 13 Second resin layer 14 Wafer 15 Mask 16 areas x Propagation direction y One imaginary surface z Center of the inner space L1, L2 formation levels
Claims
1. An acoustic wave device comprising a device chip having a functional element including an IDT electrode formed on one surface thereof, a resin cover layer supported on the one surface thereof via a resin support layer, and the functional element being positioned in an internal space formed between these three elements, the support layer is composed of a lower layer portion in contact with the one surface of the device chip, and an upper layer portion located between the cover layer and the lower layer portion in contact with both of them, The lower layer is made of a resin having a higher thermal conductivity than a resin constituting the upper layer and being non-photosensitive; The upper layer of the acoustic wave device is made of a photosensitive resin.
2. 2. The acoustic wave device according to claim 1, wherein a bump is formed in a through hole that penetrates the cover layer and the support layer and positions a bump pad formed on the one surface of the device chip at the bottom of the hole and connected to the functional element.
3. 2. The acoustic wave device according to claim 1, wherein in a cross section along the one surface of the device chip, a cross-sectional area of the internal space is larger at a formation level of the lower layer than at a formation level of the upper layer.
4. A method for manufacturing the acoustic wave device according to any one of claims 1 to 3, comprising the steps of: a first step of forming the functional elements, wiring, and bump pads on one surface of a wafer that will become the device chip; a second step of forming a first resin layer that will become the lower layer portion on the one surface of the wafer that has been subjected to the first step; a third step of forming a second resin layer to be the upper layer portion on the first resin layer formed in the second step; a fourth step of exposing a region of the second resin layer formed in the third step other than a region located on a region where the functional element is formed; a fifth step of removing an area of the second resin layer other than the exposed area by development; A method for manufacturing an acoustic wave device, comprising: a sixth step of etching the first resin layer using the exposed area of the second resin layer as a mask after the fifth step to form a space that becomes the internal space at the formation level of the lower layer.
Citation Information
Patent Citations
Saw device, manufacturing method thereof, and electronic component using the same
JP2002217673A