Method for estimating impact energy to blast furnace burden

The method estimates impact energy on blast furnace charges by calculating circularity and correcting for particle size, addressing the challenge of accurately determining impact energy and improving blast furnace management.

JP2024154034APending Publication Date: 2024-10-30NIPPON STEEL CORPORATION
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023067623
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-30

AI Technical Summary

Technical Problem

Existing methods fail to accurately estimate the impact energy received by blast furnace charges during transportation, which affects their properties and operational management in blast furnaces.

Method used

A method to estimate impact energy by calculating the circularity of blast furnace charge particles based on photographed images, using a correlation between circularity and impact energy, and correcting for particle size, allowing estimation of impact energy through drum rotation speed.

Benefits of technology

Enables accurate estimation of impact energy, facilitating better management of blast furnace operations by assessing the strength and particle size distribution of the charge, thereby optimizing operational actions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154034000001_ABST
    Figure 2024154034000001_ABST
Patent Text Reader

Abstract

To estimate impact energy given to a blast furnace burden.SOLUTION: In a method for estimating the impact energy given to a blast furnace burden, the circularity of particles of the blast furnace burden is calculated based on the photographed image of the blast furnace burden. Based on the correlation between the pre-specified circularity and the impact energy, the impact energy corresponding to the calculated circularity is calculated. In the correlation, the greater the impact energy, the greater the circularity. The impact energy can be expressed as the number of drum revolutions on the drum testing machine.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention is a method for estimating impact energy received by a blast furnace charge, during transportation, etc., when the charge is charged into a blast furnace. [Background technology]

[0002] Iron raw materials (sintered ore, iron ore, etc.) and coke are charged into a blast furnace, and these blast furnace charge materials are transported to the blast furnace. When the blast furnace charge materials move along this transport path, they may be subjected to impacts, and the properties of the blast furnace charge materials may change due to the impact energy. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-174155 A Summary of the Invention [Problem to be solved by the invention]

[0004] In order to grasp the properties of the blast furnace charge, it is effective to grasp the impact energy given to the blast furnace charge. The present inventors have focused on the circularity of the particles of the blast furnace charge and found that there is a correlation between the circularity and the impact energy, and have completed the present invention. [Means for solving the problem]

[0005] The present invention is a method for estimating impact energy applied to a blast furnace charge, which calculates the circularity of particles of the blast furnace charge based on a photographed image of the blast furnace charge, and calculates the impact energy corresponding to the calculated circularity based on a previously specified correlation between the circularity and the impact energy.

[0006] In the above correlation, the greater the impact energy, the greater the circularity. Meanwhile, the impact energy can be expressed as the number of drum revolutions in a drum testing machine.

[0007] The circularity can be an average value of a plurality of circularities determined from a plurality of particles of the blast furnace charge. When calculating the circularity of the particles of the blast furnace charge, the circularity calculated from the photographed image can be corrected according to the particle diameter based on the correlation between the particle diameter and the circularity of the particles.

[0008] A photographed image can be generated by photographing the blast furnace charge during transportation along the transport path for transporting the blast furnace charge to the blast furnace. Also, a photographed image can be generated by sampling the blast furnace charge along the transport path for transporting the blast furnace charge to the blast furnace and photographing the sampled blast furnace charge. Effect of the Invention

[0009] According to the present invention, by calculating the circularity of particles of a blast furnace charge, it is possible to estimate the impact energy given to the blast furnace charge based on the correlation between the circularity and the impact energy. [Brief description of the drawings]

[0010] [Figure 1] 1 is a flowchart illustrating a process for estimating impact energy (drum rotation speed) received by a blast furnace charge. [Diagram 2] FIG. 2 is a diagram illustrating an example of a coke transport path. [Diagram 3] FIG. 1 illustrates the correlation between circularity and particle size of charge particles. [Figure 4] 11A and 11B are diagrams illustrating a method for correcting circularity. [Diagram 5] FIG. 13 is a diagram showing an example of a depth image obtained by photographing an aggregate of charge particles. [Figure 6] 6 is a diagram showing a binarized image (one example) after discontinuous point detection processing is performed on the image shown in FIG. 5. FIG. [Figure 7] FIG. 7 is a diagram showing an example of an image after thinning processing is performed on the image shown in FIG. 6. [Figure 8]FIG. 6 is a diagram showing an image (one example) in which the contour lines of the finally identified charge particles are superimposed on the depth image shown in FIG. 5. [Figure 9] FIG. 13 is a diagram showing the relationship between the circularity and cumulative frequency of coke particles for each rotation speed. [Figure 10] FIG. 1 is a diagram showing the correlation between the average circularity of coke particles and the drum rotation speed. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] This embodiment is a method for estimating impact energy given to blast furnace charge materials when, for example, the blast furnace charge materials are transported to be charged into the blast furnace. Examples of blast furnace charge materials include coke and iron raw materials (sintered ore, lump ore, pellets). The blast furnace charge materials are transported along a predetermined transport path and charged into the blast furnace. According to this embodiment, for blast furnace charge materials transported to an arbitrary position on the transport path (hereinafter referred to as the "evaluation position"), it is possible to estimate the impact energy received by the blast furnace charge materials while they are transported to the evaluation position. A specific description will be given below.

[0012] FIG. 1 is a flowchart illustrating a method for estimating the impact energy received by a blast furnace charge.

[0013] In step S101, particles of the blast furnace charge material (hereinafter referred to as "charge particles") transported along the transport path are photographed at a predetermined evaluation position. The evaluation position is located on the transport path to the blast furnace and can be appropriately determined.

[0014] As a method for photographing the charge particles, for example, the following two photographing methods can be mentioned.

[0015] In the first photographing method, after collecting charge particles moving on a conveying path at an evaluation position, a photographing device is used to photograph the collected charge particles. Specifically, a collection of collected charge particles is divided into a plurality of groups, and charge particles of each group are placed on a tray. Then, for each group, a plurality of charge particles placed on the tray are photographed. Here, it is preferable to photograph the charge particles so that the plurality of charge particles do not overlap each other, in other words, so that the entire contour of each charge particle can be grasped.

[0016] In the second photographing method, while moving the charge particles along the conveying path, a photographing device is used to photograph the charge particles that have reached the evaluation position. In this case, it is sufficient to install a photographing device so that the evaluation position on the conveying path can be photographed. Here, photographing can be performed multiple times within a predetermined time, and the multiple photographing can be performed at a predetermined time period. When photographing the charge particles while moving them on the conveying path, the multiple charge particles tend to overlap each other, and it may be difficult to grasp the entire contour of the charge particles in the photographed image. Therefore, by photographing multiple times, it is possible to obtain a large number of charge particles whose entire contour can be grasped in the photographed image.

[0017] 2 is a diagram showing an example of a transport path of coke as a blast furnace charge. When estimating the impact energy received by the coke, an evaluation position can be determined on the transport path described below.

[0018] The conveying path 10 is a path from when the coke is pushed out of the coke oven 11 until the coke is conveyed to a stock level (predetermined position) 16a of raw materials inside the blast furnace 16. On the conveying path 10, the coke (red-hot coke) pushed out from the coke oven 11 is conveyed to a coke dry quenching system (CDQ, Coke Dry Quenching) 12 and cooled. The coke cooled in the CDQ 12 is discharged from the CDQ 12 and conveyed to a raw material tub 13. The raw material tub 13 discharges the coke at a predetermined speed so that a predetermined amount of coke is stored. The coke discharged from the raw material tub 13 is conveyed to a relay hopper 14.

[0019] The relay hopper 14 discharges all of the coke when a predetermined amount of coke is delivered thereto. The coke discharged from the relay hopper 14 is delivered to the top hopper 15. The top hopper 15 discharges all of the coke delivered thereto, similar to the relay hopper 14, when a predetermined amount of coke is delivered thereto. The coke discharged from the top hopper 15 falls and is charged into the blast furnace 16, and reaches a stock level 16a of the blast furnace 16. In the conveying path 10, the coke is conveyed by a belt conveyor between the coke oven 11 and the CDQ 12, between the CDQ 12 and the raw material tank 13, between the raw material tank 13 and the relay hopper 14, and between the relay hopper 14 and the top hopper 15.

[0020] The coke may be subjected to an impact during transportation by the belt conveyor described above. Also, the coke may be subjected to an impact when it is stored in any of the CDQ 12, the raw material tank 13, the relay hopper 14, and the top hopper 15. In this embodiment, it is possible to estimate the impact energy received by the coke (blast furnace charge) until it is transported to the evaluation position, including these impacts.

[0021] Here, the evaluation position is preferably a position on the belt conveyor that supplies the blast furnace charge to the furnace top hopper 15. By estimating the impact energy received by the blast furnace charge at this evaluation position, it is possible to grasp the impact energy received by the blast furnace charge immediately before it is charged into the blast furnace 16. Then, based on this impact energy, it is possible to grasp the properties of the blast furnace charge immediately before it is charged into the blast furnace 16.

[0022] In step S102 shown in Fig. 1, the photographed image obtained in the process of step S101 is subjected to image processing described later to calculate the circularity of the burden particle. Specifically, the actual area S and actual perimeter P of the burden particle are calculated by the image processing, and then the circularity C of the burden particle is calculated based on the following formula (1). A method for calculating the actual area S and actual perimeter P of the burden particle will be described later.

[0023]

number

[0024] In the above formula (1), C is the circularity [-], and S is the actual area [mm 2 ], and P is the actual perimeter of the charge particle [mm]. The circularity C can take a value within the range of 0.00 to 1.00 [-]. In this embodiment, the circularity C is calculated for each of a plurality of charge particles whose entire contours have been identified, and the average value of these circularities C (hereinafter referred to as the "average circularity Cave") is calculated.

[0025] The photographed image includes a plurality of burden particles, and these burden particles may include a plurality of burden particles that overlap each other in the photographing direction. When a plurality of burden particles overlap, it becomes impossible to identify at least a part of the contour line of the burden particle, and it becomes impossible to grasp the entire contour line of the burden particle. If the entire contour line of the burden particle cannot be grasped, it becomes impossible to calculate the actual area S and actual perimeter P of the burden particle, and as a result, it becomes impossible to calculate the circularity C of the burden particle.

[0026] Therefore, when calculating the circularity C of the burden particle, only the burden particle whose entire contour can be identified is extracted, and the actual area S and actual perimeter P of the extracted burden particle are calculated. This makes it possible to accurately calculate the circularity C of the burden particle.

[0027] According to the above-mentioned first and second photographing methods, a plurality of photographed images can be obtained, and a plurality of charge particles whose overall contours can be identified can be identified from these photographed images. After calculating the circularity C of each of these charge particles, the average circularity Cave is calculated.

[0028] In step S103, the impact energy given to the charge particles is calculated based on the average circularity Cave calculated in the process of step S102. In this embodiment, the impact energy is defined as the drum rotation speed [rev.], but is not limited to this, and the impact energy can be defined based on a predetermined index. The drum rotation speed is the rotation speed in a drum testing machine used when measuring the drum strength index (DI) (JIS K2151) of the blast furnace charge. The higher the drum rotation speed, the higher the impact energy. In other words, the lower the drum rotation speed, the smaller the impact energy.

[0029] A certain correlation is found between the average circularity Cave and the drum rotation speed (impact energy). This correlation may depend on the initial shape (shape before impact energy is applied) of the blast furnace charge material (coke or iron raw material) and may be specified in advance according to the type of blast furnace charge material. Regarding this correlation, for example, in the case of coke, the higher the drum rotation speed, the higher the average circularity Cave, and, for example, in the case of iron raw material pellets, the higher the drum rotation speed, the lower the average circularity Cave.

[0030] In the case where the average circularity Cave increases as the drum rotation speed increases, there is a positive correlation, which can be expressed by a linear function or a quadratic function. Depending on the type of blast furnace charge, the correlation between the average circularity Cave and the drum rotation speed (impact energy) can be expressed by an N-th order function. If the correlation between the average circularity Cave and the drum rotation speed is specified in advance by an experiment, it is possible to calculate the drum rotation speed (impact energy) corresponding to the average circularity Cave calculated in the process of step S102. In other words, it is possible to estimate the impact energy (here, the drum rotation speed) received by the blast furnace charge while being transported to the evaluation position.

[0031] When estimating the impact energy received by the blast furnace charge, it is preferable to use the same operating conditions as the operating conditions of the blast furnace charge when the correlation between the average circularity Cave and the drum rotation speed (impact energy) was specified. However, the operating conditions do not need to be exactly the same, and as long as the operating conditions are within an allowable range in which they can be considered to be the same, the impact energy received by the blast furnace charge can be estimated based on the correlation between the average circularity Cave and the drum rotation speed (impact energy) specified in advance.

[0032] In this embodiment, the correlation between the average circularity Cave and the impact energy is focused on, but it is clear that a similar correlation is observed between the circularity C and the impact energy. Therefore, the correlation between the circularity C and the impact energy (drum rotation speed, etc.) is specified in advance, and the circularity C of the charge particle is calculated from the captured image, so that the impact energy corresponding to this circularity C can be calculated.

[0033] By estimating the impact energy received by the blast furnace charge according to this embodiment, it is possible to estimate the strength of the blast furnace charge and the particle size distribution of the blast furnace charge. For example, when the blast furnace charge is coke, the drum strength index DI specified in JIS K2151 can be used as the strength of the coke. This drum strength index DI indicates the mass percentage of coke with a particle size of 15 mm or more among the coke after 150 rotations of the drum.

[0034] The number of drum rotations required to apply the estimated impact energy to the coke can be calculated by dividing the estimated impact energy (the impact energy received by the coke before it is moved to the evaluation position) by the impact energy applied to the coke by one rotation of the drum. The estimated impact energy can be applied to the coke by rotating the drum the calculated number of rotations, and the drum strength index DI can be measured for the coke to which the impact energy has been applied. If the correlation between the impact energy and the drum strength index DI is determined in advance, the drum strength index DI can be estimated based on the estimated impact energy.

[0035] The strength of blast furnace charge materials (such as the drum strength index DI described above) can be used as an index for managing the operation of a blast furnace. For example, if the strength of coke (drum strength index DI) is estimated, operational actions such as changing the coke ratio can be taken according to the coke strength. Specifically, the higher the coke strength, the easier it is to reduce the pressure loss in the furnace, so the coke ratio can be reduced. On the other hand, the lower the coke strength, the easier it is to increase the pressure loss in the furnace, so the coke ratio can be increased.

[0036] On the other hand, since the particle size distribution of the blast furnace charge depends on the impact energy received by the blast furnace charge, the particle size distribution of the blast furnace charge can be estimated by estimating the impact energy. Here, the larger the impact energy, the smaller the particle size distribution of the blast furnace charge shifts to the smaller particle size side, and the smaller the impact energy, the larger the particle size distribution of the blast furnace charge shifts to the larger particle size side.

[0037] When estimating the particle size distribution of the blast furnace charge, first, a reference impact energy (hereinafter referred to as "reference impact energy") is determined in advance, and the particle size distribution when the reference impact energy is applied to the blast furnace charge is measured. Then, the particle size distribution of the blast furnace charge is shifted based on the difference between the reference impact energy and the estimated impact energy, so that the particle size distribution corresponding to the estimated impact energy can be estimated. Here, if the relationship between the difference in impact energy and the shift amount of the particle size distribution is obtained in advance, the shift amount of the particle size distribution can be specified from the difference in impact energy. Then, when the estimated impact energy is larger than the reference impact energy, the particle size distribution is shifted to the side with smaller particle sizes, and when the estimated impact energy is smaller than the reference impact energy, the particle size distribution is shifted to the side with larger particle sizes.

[0038] The particle size distribution of the blast furnace charge can be used as an index for managing the operation of the blast furnace. For example, operational actions such as changing the coke ratio can be performed according to the particle size distribution of the blast furnace charge. Specifically, the more the particle size distribution of the coke is shifted to the larger particle size side, the easier it is to reduce the pressure loss in the furnace, so the coke ratio can be reduced. On the other hand, the more the particle size distribution of the coke is shifted to the smaller particle size side, the easier it is to increase the pressure loss in the furnace, so the coke ratio can be increased.

[0039] In this embodiment, the impact energy is calculated from the average circularity Cave (or the circularity C) by focusing on the correlation between the average circularity Cave (or the circularity C) and the impact energy, but the present invention is not limited to this. Specifically, as described below, the circularity C (or the average circularity Cave) is corrected in consideration of the particle size of the charge particles, and the impact energy can be estimated based on the corrected circularity C (or the average circularity Cave). Here, when calculating the average circularity Cave from a plurality of circularities C, each of the plurality of circularities C can be corrected according to the particle size, and then the average circularity Cave can be calculated from the corrected plurality of circularities C, or the average circularity Cave can be calculated from the plurality of circularities C and then corrected according to the particle size.

[0040] Since the circularity C depends on the particle size of the burden particles, if the impact energy is estimated by focusing only on the circularity C, it may deviate from the true impact energy. For example, even if the impact energy is the same, the smaller the particle size of the burden particles, the larger the circularity C, so the impact energy estimated from this circularity C becomes larger than the actual impact energy. Also, even if the impact energy is the same, the larger the particle size of the burden particles, the smaller the circularity C, so the impact energy estimated from this circularity C becomes smaller than the actual impact energy. Therefore, it is preferable to estimate the impact energy after correcting the circularity C (or the average circularity Cave) based on the particle size of the burden particles.

[0041] A correlation (example) L1 shown in FIG. 3 is found between the circularity C of the burden particles and the particle size (here, the minor axis diameter) of the burden particles. In this correlation L1, the larger the particle size, the lower the circularity C, and a negative correlation is established. If this correlation L1 is obtained in advance, the circularity can be corrected according to the particle size by grasping the particle size of the burden particles.

[0042] Specifically, as shown in FIG. 4, a reference particle diameter (hereinafter referred to as "reference particle diameter") Dr is determined in advance, and the circularity C calculated in the process of step S102 shown in FIG. 1 is regarded as the circularity Cr corresponding to the reference particle diameter Dr in the correlation L1 shown in FIG. 4. Then, based on the correlation L1, a difference ΔC in the circularity C corresponding to the difference ΔD between the particle diameter (hereinafter referred to as "measured particle diameter") Dm obtained from the photographed image of the charge particle and the reference particle diameter Dr is obtained. The corrected circularity C can be obtained by adding or subtracting the difference ΔC to the circularity C calculated in the process of step S102 shown in FIG. Here, if the measured particle diameter Dm is smaller than the reference particle diameter Dr, the difference ΔC is subtracted from the calculated circularity C. On the other hand, if the measured particle diameter Dm is larger than the reference particle diameter Dr, the difference ΔC is added to the calculated circularity C.

[0043] Next, a method for calculating the actual area S and actual perimeter P of the burden particle in the process of step S102 described above will be described. The burden particle whose overall contour can be identified can be identified using the technology described in Patent Document 1, and if the overall contour of the burden particle is identified, the actual area S and actual perimeter P of the burden particle can be calculated.

[0044] A method for determining the overall contour of a charge particle is outlined below.

[0045] As the photographed image, an image (hereinafter referred to as a "depth image") is obtained in which the amount of unevenness on the surface of the burden particle is expressed by brightness. There is usually a step at the boundary between the burden particles, and in the depth image, this step appears as a discontinuous change in brightness value, so that the burden particle can be identified based on the change in brightness value.

[0046] The depth image can be generated by a so-called light-section method. In the light-section method, a linear laser beam is irradiated onto the surfaces of multiple overlapping burden particles, and the light-section line (including a state in which the laser beam is displaced from a straight line corresponding to the amount of unevenness) caused by the laser beam reflected on the surface of each burden particle is photographed. The unevenness information is obtained from the multiple light-section images arranged in chronological order, thereby generating one image (depth image). Figure 5 shows an example of a depth image obtained by photographing an aggregate of coke particles, which are burden particles.

[0047] It is possible to perform a gradient correction process on the depth image, in which a reference plane that approximately represents the gradient change in the luminance values ​​in the depth image is calculated, and the gradient change in the luminance values ​​of the pixels included in the depth image is approximated to a plane based on the reference plane and the depth image.

[0048] Next, a discontinuity detection process is performed on the depth image. In the discontinuity detection process, each pixel in the depth image is determined as a pixel of interest, and for each pixel of interest, eight directions are sequentially specified as calculation directions at 45 degree intervals from the pixel of interest. For each of the eight directions, eight adjacent pixels adjacent to the pixel of interest are identified, and the difference in luminance value between the pixel of interest and each adjacent pixel (hereinafter referred to as "luminance difference") is calculated.

[0049] The eight directions include a forward direction and a reverse direction, which are opposite to each other. It is determined whether the luminance difference between the pixel of interest and an adjacent pixel located in the forward direction is equal to or greater than a predetermined threshold A, and it is determined whether the luminance difference between the pixel of interest and an adjacent pixel located in the reverse direction is equal to or less than a predetermined threshold B. For example, when the luminance is expressed in 265 gradations, the threshold A can be set to about 5, and the threshold B can be set to about 2.

[0050] When the luminance difference in the forward direction is equal to or greater than threshold A and the luminance difference in the reverse direction is equal to or less than threshold B, the pixel of interest is determined to be a discontinuity point, and pixels determined to be discontinuity points are set to 1, which has a high luminance value and is displayed in white. The remaining pixels other than the discontinuity points are set to 0, which has a low luminance value and is displayed in black. In this way, a binarized image is obtained. FIG. 6 shows an example of a binarized image after discontinuity detection processing is performed on the image shown in FIG. 5.

[0051] Next, a thinning process is performed on the binarized image after the discontinuous point detection process. The thinning process is a process for reducing the line width of the contour line in the image binarized to white and black to, for example, the line width of one pixel, and a general image processing method can be used. Figure 7 shows an image (one example) after the thinning process is performed on the image shown in Figure 6.

[0052] Next, in the image after the thinning process, a correction process is performed to remove lines with ends (so-called dead-end lines) that cannot be said to be the contour lines of the charge particles as disturbances. This correction process is a process in which the shape of the dead-end line is specified in advance, and the dead-end line is specified and removed from the image using a filter that shows the shape of the dead-end line (for example, a filter of 3 pixels x 3 pixels vertically and horizontally), and a general image processing method can be used.

[0053] In the correction process, in addition to removing the dead end lines described above, the contour lines of the burden particles that are located at a relatively low position are removed. For example, the area of ​​each contour line included in the image is calculated, and when this area is equal to or smaller than the lower limit of the size that the actual burden particle can have, the contour line corresponding to this area is removed. By performing this correction process, the final contour line of the burden particle is identified. FIG. 8 shows an image (one example) in which the contour lines of the finally identified burden particles are superimposed on the depth image shown in FIG. 5. EXAMPLES

[0054] Coke produced in coke oven A and cooled by CDQ was sampled. That is, in FIG. 2, coke was sampled from the transportation route from CDQ 12 to raw material tank 13. Here, the coke was sampled according to the provisions of JIS M8811. The sampled coke was inserted into a drum testing machine specified in JIS K2151, and the drum testing machine was rotated. Here, the rotation speed of the drum testing machine (drum rotation speed) was set to 30, 60, 90, 120, and 150 [rev.], respectively. The higher the drum rotation speed, the greater the impact energy given to the coke.

[0055] Depth images were generated for the coke after rotating at each drum rotation speed (30, 60, 90, 120, 150 [rev.]) and for the coke that was not rotated in the drum test machine (i.e., the coke as collected). Specifically, about 8 to 10 kg of coke was taken out and placed on a tray, and then the coke on the tray was photographed to generate depth images. This process was performed 10 times to generate 10 depth images.

[0056] By performing the above-mentioned image processing on each depth image, approximately 1000 coke particles (burden particles) whose overall contours could be identified were extracted. Then, for each coke particle, the actual area S and actual perimeter P were calculated to calculate the circularity C, and then the average circularity Cave was calculated from the circularity C of all the coke particles.

[0057] Figure 9 shows the relationship between the circularity [-] and cumulative frequency [-] of coke particles for each drum rotation speed (0, 30, 60, 90, 120, 150 [rev.]). When the drum rotation speed is 0 [rev.], no impact energy is applied to the collected coke by the drum testing machine, but it was found that the cumulative distribution shifts toward higher circularity as the drum rotation speed increases.

[0058] FIG. 10 shows the relationship between the rotation speed of the drum test machine (drum rotation speed) and the average circularity Cave at each drum rotation speed. In FIG. 10, circles represent measured values ​​obtained in the above-mentioned test, and the dashed dotted line represents an approximate straight line L2 calculated from the measured values. As can be seen from FIG. 10, the higher the drum rotation speed, the higher the average circularity Cave, and a positive correlation was found between the drum rotation speed and the average circularity Cave. This correlation is the correlation between the drum rotation speed and the average circularity Cave for coke particles.

[0059] In addition, the correlation between the drum rotation speed and the average circularity Cave could be expressed by a linear function (approximation line L2 shown in FIG. 10). In this embodiment, the correlation between the drum rotation speed and the average circularity Cave is expressed by the following formula (2).

[0060]

number

[0061] In the above formula (2), Cave is the average circularity [-] and R is the drum rotation speed [rev.]. It is considered that the higher the drum rotation speed, in other words, the higher the impact energy, the easier it is for the brittle parts on the surface of the coke to peel off, and the outer shape of the coke becomes closer to a sphere.

[0062] If the correlation between the drum rotation speed and the average circularity Cave is obtained in advance, the average circularity Cave of the coke to be evaluated can be calculated based on a depth image obtained at an evaluation position on the transport path, and the drum rotation speed (impact energy) corresponding to this average circularity Cave can be calculated. In other words, the impact energy received by the coke while being transported to the evaluation position can be estimated. Here, it is preferable to estimate the impact energy when the operating conditions of the coke are the same.

[0063] Next, in both cases, the coke produced in the coke oven A was directly transported to the blast furnace A, and the coke produced in the coke oven A was temporarily stored in a yard and then transported to the blast furnace A, and the coke discharged from the raw material bin 13 shown in Fig. 2 was sampled at the same evaluation position. Here, the storage in the yard was performed in the transport route between the CDQ 12 and the raw material bin 13 in Fig. 2.

[0064] The average circularity Cave of the coke transported directly to the blast furnace A was calculated from the depth image to be 0.579 [-]. The average circularity Cave of the coke temporarily stored in the yard was calculated from the depth image to be 0.602 [-]. The drum rotation speed was estimated using the correlation (approximation line L2) shown in Fig. 10. The drum rotation speed was 24 [rev.] for the coke transported directly to the blast furnace A, and 94 [rev.] for the coke temporarily stored in the yard.

[0065] When the coke is temporarily stored in the yard, impact energy associated with storage in the yard is imparted to the coke compared to when the coke is directly transported to blast furnace A. This is evident from the fact that the drum rotation speed (94 [rev.]) for the coke temporarily stored in the yard is greater than the drum rotation speed (24 [rev.]) for the coke directly transported to blast furnace A. The impact energy associated with storage in the yard can be understood as the difference between the two drum rotation speeds mentioned above (24, 94 [rev.]).

[0066] In this embodiment, the impact energy of the coke is focused on, but the impact energy can also be estimated for blast furnace charges other than coke (iron raw materials, etc.). Similar to coke, blast furnace charges other than coke (iron raw materials, etc.) are subjected to impacts during transportation, etc., causing changes in the circularity of the charge particles, so the impact energy can be estimated by a method similar to that of this embodiment. [Explanation of symbols]

[0067] 10: Transport route, 11: Coke oven, 12: CDQ (Coke dry quenching equipment), 13: raw material tank, 14: relay hopper, 15: top hopper, 16: blast furnace, 16a: Stock Level

Claims

1. A method for estimating impact energy imparted to a blast furnace charge, comprising: Calculating the circularity of particles of the blast furnace charge based on the photographed image of the blast furnace charge; A method for estimating the impact energy of a blast furnace charge, comprising: calculating the impact energy corresponding to the calculated circularity based on a correlation between the circularity and the impact energy that is specified in advance.

2. The method for estimating the impact energy of a blast furnace charge according to claim 1, characterized in that, in the correlation, the greater the impact energy, the greater the circularity.

3. The method for estimating the impact energy of a blast furnace charge according to claim 1 or 2, characterized in that the impact energy is expressed as a drum rotation speed in a drum testing machine.

4. The method for estimating the impact energy of blast furnace charge according to claim 1 or 2, characterized in that the circularity is an average value of multiple circularities identified from multiple particles of the blast furnace charge.

5. The method for estimating the impact energy of blast furnace charge material according to claim 1, characterized in that, when calculating the circularity of particles of blast furnace charge material, the circularity calculated from the photographed image is corrected according to the particle size of the particles based on the correlation between the particle size and the circularity of the particles.

6. The method for estimating the impact energy of blast furnace charge as described in claim 1, characterized in that the captured image is generated by photographing the blast furnace charge being transported along a transport path for transporting the blast furnace charge to the blast furnace.

7. The method for estimating the impact energy of blast furnace charge as described in claim 1, characterized in that the blast furnace charge is sampled along a transport path for transporting the blast furnace charge to the blast furnace, and the captured image is generated by photographing the sampled blast furnace charge.

Citation Information

Patent Citations

  • Particle diameter measurement device and particle diameter measurement method

    JP2019174155A