Panel molding device and panel molding method

The panel forming apparatus and method address inconsistent flange formation by sequentially compressing and forming panels with multiple constriction portions, ensuring uniform deformation and minimizing wrinkles, while reducing forming time.

JP2024154091AInactive Publication Date: 2024-10-30TOYOTA SHATAI KK
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023067709
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-30
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The cross-sectional shape of recessed flange portions in panels varies along the width direction, leading to inconsistent molding and potential wrinkles during press forming, especially in automobile body panels.

Method used

A panel forming apparatus and method that involves a first constriction portion and a second constriction portion, using a pressing pad, rear and front bending blades, and a holding mechanism to sequentially compress and form the panel into a concave shape, ensuring uniform deformation and minimizing wrinkles.

Benefits of technology

The method effectively suppresses wrinkles on the panel surface by controlling deformation direction, allowing for consistent flange formation despite varying cross-sectional shapes, and reduces forming time through continuous operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154091000001_ABST
    Figure 2024154091000001_ABST
Patent Text Reader

Abstract

To provide a panel molding technique effective for suppressing wrinkles from remaining on a surface when molding an end of a preliminarily drawn panel.SOLUTION: A panel molding device 10 is a device for molding an end 2 of a preliminarily drawn panel 1. The panel molding device includes: a lower die 20 and an upper die 30; a pressing pad 21 which presses the panel 1 to the lower die 20; and a rear bending blade 31 and a front bending blade 32 which move by interlocking with the upper die 30. After a second drawing section 4 is compressed by the front bending blade 32 and the lower die 20 and is molded into a general section 6 by moving the upper die 30 toward the lower die 20 in a state of pressing the panel 1 to the lower die 20 by the pressing pad 21, a first drawing section 3 is compressed by the rear bending blade 31 and the lower die 20 in a state of sandwiching the general section 6 by the front bending blade 32 and the lower die 20 and is molded into a recessed flange section 5.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a panel forming apparatus and a panel forming method. [Background technology]

[0002] Conventionally, when manufacturing an automobile body, a panel made of a steel plate or the like is formed into a predetermined shape by press forming using a forming die. In this type of press forming, first, a primary forming such as drawing described in Patent Document 1 below is performed, and then a secondary forming such as a gathering bending process described in Patent Document 2 below is performed. In the gathering bending process, a panel that has been previously drawn is set on the movable die side, and the end of the panel is pressed against the movable die side by a gathering bending blade, and the end is gathered and bent into a concave flange. This forms the panel into a three-dimensional shape that will become the final product. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-107663 A [Patent Document 2] Japanese Patent Application Publication No. 7-214183 Summary of the Invention [Problem to be solved by the invention]

[0004] In an automobile body, the cross-sectional shape of the recessed flange portion of the panel is not uniform, but differs depending on the position in the width direction of the panel. For example, the cross-sectional shape of the flange portion at the rear end of the roof panel of a hatchback-type automobile is deeper in the recess at both ends than at the center in the width direction of the vehicle. For this reason, when a flange portion is formed by pressing a bending blade against the rear end of a roof panel that has been drawn in advance over the entire length in the width direction of the vehicle, a problem may occur in that wrinkles remain on the surface of the flange portion of the roof panel, which is the final product, due to the difference in the amount of forming and the direction of compressive deformation of the roof panel from one portion to another. Such a problem may occur not only in the manufacture of roof panels for automobile bodies, but also in the manufacture of panels other than roof panels and panels in other fields.

[0005] The present invention has been made in consideration of such problems, and aims to provide a panel molding technology that is effective in preventing wrinkles from remaining on the surface when the edges of a panel that has been pre-drawn and molded are molded. [Means for solving the problem]

[0006] One aspect of the present invention is A panel forming apparatus for forming an edge of a panel that has been previously drawn, comprising: a first drawn portion formed to extend in a panel width direction and a second drawn portion formed to extend along the first drawn portion on the inner side of the first drawn portion at the end portion of the panel; A lower die and an upper die, a pressing pad for pressing the panel against the lower mold; A back bending blade and a front bending blade that move in conjunction with the upper die; Equipped with a panel forming device configured to move the upper die toward the lower die while the panel is pressed against the lower die by the pressing pad, thereby compressing the second drawn portion with the front bending blade and the lower die to form a general portion, and then compressing the first drawn portion with the rear bending blade and the lower die while the general portion is sandwiched between the front bending blade and the lower die to form a concave-shaped flange portion; is located.

[0007] Another aspect of the present invention is A panel forming method for forming an end of a panel that has been previously drawn, comprising the steps of: a first drawn portion formed to extend in a panel width direction and a second drawn portion formed to extend along the first drawn portion on the inner side of the first drawn portion at the end portion of the panel; a pre-bending process in which the second drawn portion is compressed by a pre-bending blade and the lower die in a state in which the panel is pressed against the lower die by a pressing pad to form a general portion; a post-bending process in which the first drawn portion is compressed by a post-bending blade and the lower die in a state in which the general portion formed in the pre-bending process is sandwiched between the pre-bending blade and the lower die, to form a concave-shaped flange portion; A panel forming method comprising: is located. Effect of the Invention

[0008] According to the panel forming device or panel forming method of the above aspect, with the panel pressed against the lower die by the pressing pad, first, the second drawn portion of the end of the panel, which is on the inside of the first drawn portion, is compressed by the leading bending blade and the lower die to be formed into a general portion. Then, with the general portion of the panel sandwiched between the leading bending blade and the lower die, the first drawn portion, which is on the outside of the general portion, is compressed by the bending blade and the lower die to be formed into a concave-shaped flange portion.

[0009] That is, in this embodiment, the second drawn portion on the inside of the first drawn portion located on the free end side (outside) of the end of the panel is bent prior to the first drawn portion, and the first drawn portion is bent after the second drawn portion. By bending the panel in this order, the end of the panel is allowed to deform toward the free end until the end of the panel is bent, so that the compression of the end of the panel toward the inside is suppressed. As a result, even if the cross-sectional shape of the flange portion differs depending on the position in the panel width direction and the molding amount and the compressive deformation direction of the panel differ from part to part, wrinkles are unlikely to remain on the surfaces of the general portion and the flange portion of the panel after the bending. In contrast, if the first drawn portion on the free end side of the panel 1 is bent prior to the second drawn portion, the end of the panel is restricted from deforming toward the free end, and wrinkles are likely to occur on the surfaces of the general portion and the flange portion of the panel.

[0010] As described above, according to the above-described embodiment, it is possible to suppress wrinkles from remaining on the surface when the end portion of a panel that has been previously drawn and shaped is shaped. [Brief description of the drawings]

[0011] [Figure 1] 3A and 3B are perspective views of a panel that has been subjected to drawing and bending after drawing, respectively, with respect to the panel according to the first embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along line II-II in FIG. [Diagram 3] FIG. 3 is a cross-sectional view taken along line III-III in FIG. [Figure 4] FIG. 4 is a cross-sectional view taken along line IV-IV in FIG. [Diagram 5] FIG. 2 is a cross-sectional view showing a cross-sectional structure of a portion of the panel forming apparatus of the first embodiment. [Figure 6] 3 is a flowchart of a panel molding method according to the first embodiment. [Figure 7] 7 is a cross-sectional view showing the panel forming apparatus of FIG. 5 during execution of a third step in FIG. 6. [Figure 8]7 is a cross-sectional view showing the panel forming apparatus of FIG. 5 during execution of a fourth step in FIG. 6. [Figure 9] 7 is a cross-sectional view showing the panel forming apparatus of FIG. 5 during execution of a fifth step in FIG. 6. [Figure 10] 7 is a cross-sectional view showing the panel forming apparatus of FIG. 5 during execution of a fifth step in FIG. 6. [Figure 11] 7 is a cross-sectional view showing the panel forming apparatus of FIG. 5 during execution of a sixth step in FIG. 6. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Preferred embodiments of the above aspects are described below.

[0013] In the panel forming apparatus of the above-mentioned aspect, the leading bending blade is configured to protrude from the rear bending blade toward the lower mold and be movable back and forth between an advanced position and a retracted position, and it is preferable that the rear bending blade is provided with a holding mechanism that elastically holds the leading bending blade in the advanced position so that it can be retracted.

[0014] This panel forming device employs a structure in which a front bending blade is incorporated into the rear bending blade via a holding mechanism. With this structure, by continuing the operation of moving the upper mold toward the lower mold while the panel is pressed against the lower mold by the pressing pad, it is possible to perform a series of continuous operations: compressing the second drawn portion of the panel with the front bending blade and the lower mold to form it into a general portion, and compressing the first drawn portion of the panel with the rear bending blade and the lower mold while the general portion of the panel is sandwiched between the front bending blade and the lower mold to form it into a flange portion. This makes it possible to shorten the forming time required for the panel compression bending process.

[0015] In the panel forming apparatus of the above-mentioned aspect, it is preferable that the holding mechanism portion has a rod attached to the tip bending blade, a piston connected to the rod, and a cylinder that contains the piston and working fluid and elastically biases the rod by utilizing the reaction force generated when the working fluid is compressed by the piston.

[0016] According to this panel molding device, in order to elastically hold the tip bending blade in the forward position so that it can be retracted, a structure is adopted in which the rod is elastically biased by utilizing the reaction force generated when the working fluid is compressed by the piston, thereby simplifying the structure of the holding mechanism.

[0017] Hereinafter, specific embodiments of the panel forming apparatus and the panel forming method according to the above aspects will be described with reference to the drawings.

[0018] In this specification and drawings, unless otherwise specified, the panel width direction is indicated by arrow X, the panel depth direction is indicated by arrow Y, and the panel height direction is indicated by arrow Z.

[0019] (Embodiment 1) FIG. 1 shows a panel 1 after the primary forming process of "drawing" and a panel 1A after the secondary forming process of "gathering" is performed on the panel 1. Both drawing and gathering are types of press forming. In this embodiment, the panels 1 and 1A are exemplified by roof panels of a hatchback type automobile body. The panels 1 and 1A are made of steel plates.

[0020] 1. Panel 1 Structure As shown in Figures 1 and 2, a first drawn portion 3 and a second drawn portion 4 are provided at an end portion 2 on the rear side of a panel 1 after drawing. The first drawn portion 3 is a portion formed so as to extend in a panel width direction X. The second drawn portion 4 is a portion formed so as to extend along the first drawn portion 3, more inward than the first drawn portion 3. In this embodiment, the panel width direction X substantially corresponds to the vehicle width direction.

[0021] 2. Structure of Panel 1A As shown in Fig. 1, after the gathering and bending process, an end portion 2 of the panel 1A is provided with a flange portion 5 and a general portion 6. The flange portion 5 is a portion that is formed by gathering and bending the first drawn portion 3 of the panel 1 so as to have a concave shape. The general portion 6 is a portion that is formed by gathering and bending the second drawn portion 4 of the panel 1.

[0022] As shown in Figs. 3 and 4, the flange portion 5 and the general portion 6 of the end portion 2 of the panel 1A are different in cross-sectional shape between the end portion 2a near the center in the panel width direction X and the end portions 2b on both sides. The flange portion 5 of the panel 1A is configured so that the recess depth is different in the panel width direction X. The flange portions 5 of the end portion 2a and the end portion 2b are the same in that the cross-sectional shape is approximately V-shaped, but are different in that the end portion 2b has a larger recess depth than the end portion 2a. The general portion 6 has a flat surface 6a and an erected surface 6b erected in the panel height direction Z from the flat surface 6a. The general portion 6 is the same in that the flat surface 6a of the end portion 2a and the end portion 2b have the same shape, but is different in that the erected surface 6b of the general portion 6 of the end portion 2a is inwardly recessed. The shape in which the erected surface 6b of the general portion 6 is inwardly recessed is also called, for example, a "shape with a depression angle of the trim".

[0023] 3. Structure of the panel forming device 10 The panel forming apparatus 10 of the first embodiment is an apparatus for forming an end portion 2 of a panel 1 that has been previously drawn. As shown in Fig. 5, the panel forming apparatus 10 of the first embodiment includes, as its main components, a lower die 20, an upper die 30, a pressing pad 21, a rear bending blade 31 and a front bending blade 32 for the gathering bending process, and a holding mechanism unit 40.

[0024] The lower mold 20 is provided with a first molding surface 20a and a second molding surface 20b continuous with the first molding surface 20a. The first molding surface 20a is a molding surface for molding the first drawn portion 3 of the panel 1 into the flange portion 5 of the panel 1A. The second molding surface 20b is a molding surface for molding the second drawn portion 4 of the panel 1 into the general portion 6 of the panel 1A.

[0025] The upper mold 30 is configured to be raised and lowered relative to the lower mold 20 by a drive mechanism (not shown). As the upper mold 30 descends, it approaches the lower mold 20, and as the upper mold 30 ascends, it moves away from the lower mold 20. The pressing pad 21 has the function of pressing the panel 1 against the lower mold 20 and releasing the panel 1 by releasing the pressing of the panel 1 against the lower mold 20.

[0026] 3.1 Structure of the rear bending blade 31 The rear bending blade 31 is a bending blade used after the front bending blade 32. The blade surface of the rear bending blade 31 on the tip side has a shape following the first molding surface 20a of the lower mold 20. The rear bending blade 31 extends in the panel width direction X and is configured to move in conjunction with the upper mold 30. The rear bending blade 31 has a slide member 33 interposed between the rear bending blade 31 and the upper mold 30, and a slide member 34 interposed between the rear bending blade 31 and the lower mold 20. The rear bending blade 31 is configured to move in the molding direction D by the slide member 33 sliding against the upper mold 30 and the slide member 34 sliding against the lower mold 20 by moving the upper mold 30 downward in FIG. 5 relative to the lower mold 20.

[0027] 3.2 Structure of the tip bending blade 32 The leading edge bending blade 32 is a bending blade used prior to the rear bending blade 31. The leading edge bending blade 32 has a blade surface on its tip side that follows the second forming surface 20b of the lower die 20. The leading edge bending blade 32 extends in the panel width direction X and is incorporated into the rear bending blade 31. For this reason, the leading edge bending blade 32 is configured to move in conjunction with the upper die 30, similar to the rear bending blade 31. The leading edge bending blade 32 is configured to protrude from the rear bending blade 31 toward the lower die 20 and to be able to advance and retreat between an advance position P1 and a retreat position P2 (see FIG. 10). That is, the leading edge bending blade 32 is configured to be able to move relative to the rear bending blade 31 between the retreat position P2 and the advance position P1 while protruding from the rear bending blade 31. For example, the leading edge bending blade 32 can advance from the retreat position P2 to the advance position P1, and can retreat from the advance position P1 to the retreat position P2.

[0028] 3.3 Structure of the holding mechanism 40 The holding mechanism 40 has a function of elastically holding the front bending blade 32 at the advanced position P1 so that the front bending blade 32 can be retracted. This holding mechanism 40 is provided in the recess 31a of the rear bending blade 31. In this embodiment, the front bending blade 32 extends in the longitudinal direction (panel width direction X), and in order to stably and elastically hold the front bending blade 32, it is preferable to arrange a plurality of holding mechanisms 40 side by side along the longitudinal direction of the front bending blade 32.

[0029] The holding mechanism 40 has a rod 41, a piston 42, and a cylinder 43. The tip of the rod 41 is attached to the rear end surface of the tip bending blade 32. The piston 42 is connected to the rod 41. The cylinder 43 contains the piston 42 and a working fluid, and is configured to elastically bias the rod 41 by utilizing the reaction force when the working fluid is compressed by the piston 42. With this configuration, the elastic biasing force acting on the tip bending blade 32 via the rod 41 is minimum at the forward position P1 and maximum at the retreated position P2. The working fluid may be a gas or liquid, and the type is not particularly limited, but a gas such as nitrogen, which is typically easy to handle, can be used as the working fluid. The holding mechanism 40 configured in this manner is also generally called a "gas spring."

[0030] In addition, in the holding mechanism portion 40, the structure for elastically biasing the tip bending blade 32 is not limited to one that uses a working fluid, and if necessary, an elastic member such as a spring member can be used in place of or in addition to the working fluid.

[0031] 4.Panel forming method Next, a panel forming method for forming the end portion 2 of the panel 1 that has been previously drawn will be described in detail with reference to Figures 5 to 11. Note that since the overall shape change from panel 1 to panel 1A is substantially the same in the panel width direction X, the following will only describe the change in cross-sectional shape of the end portion 2a toward the center in the panel width direction X, and will omit a description of the change in cross-sectional shape of the end portions 2b on both sides in the panel width direction X.

[0032] 6, the panel forming method of the first embodiment is achieved by sequentially executing the processes from the first step S101 to the sixth step S106. If necessary, another step may be added, at least one of the steps may be divided into multiple steps, or multiple steps may be integrated into one step.

[0033] The first step S101 is a step of setting the panel 1, which has been previously draw-formed, in the lower die 20. Although not specifically shown, the draw-forming is performed using a draw die of known structure. The second step S102 is a step following the first step S101, in which the panel 1 is pressed against the lower die 20 by the pressing pad 21. According to the first step S101 and the second step S102, the panel 1 is temporarily held by the lower die 20 and the pressing pad 21, as shown in FIG. 5.

[0034] The third step S103 is a step in which the second drawn portion 4 of the panel 1 is formed into the general portion 6 by the front bending blade 32. In this third step S103, the upper mold 30 is lowered so as to move the rear bending blade 31 in the forming direction D. As a result, as shown in Fig. 7, first, the front bending blade 32 protruding from the rear bending blade 31 comes into contact with the second drawn portion 4 of the panel 1 and presses the second drawn portion 4. The blade surface of the front bending blade 32 is pressed against the second drawn portion 4 of the panel 1 over the entire length in the panel width direction X.

[0035] Thereafter, as the upper die 30 continues to move downward, the second drawn portion 4 of the panel 1 is compressed by the blade surface of the tip bending blade 32 and the second forming surface 20b of the lower die 20. At this time, the rod 41 of the holding mechanism 40 increases the elastic biasing force applied to the tip bending blade 32 as the tip bending blade 32 receives a reaction force from the second drawn portion 4 and the lower die 20, and moves backward so that the protruding length from the cylinder 43 becomes shorter. Then, as shown in FIG. 8, the lowering operation of the upper die 30 continues until the tip bending blade 32 fits into the second forming surface 20b of the lower die 20 via the panel 1. As a result, the second drawn portion 4 of the panel 1 is formed into the general portion 6 (see FIG. 3) by the gathering bending process by the tip bending blade 32. At this time, the tip bending blade 32 is disposed at an intermediate position between the forward position P1 (see FIG. 7) and the retreated position P2 (see FIG. 10).

[0036] In this way, the third step S103 corresponds to a pre-bending process in which, while the panel 1 is pressed against the lower die 20 by the pressing pad 21, the second drawn portion 4 of the end portion 2 of the panel 1 is compressed by the pre-bending blade 32 and the lower die 20 to form it into the general portion 6.

[0037] The fourth step S104 is a step of sandwiching the general portion 6 between the blade surface of the tip bending blade 32 and the second molding surface 20b of the lower die 20. That is, the fourth step S104 is a step of maintaining the state after the third step S103 is performed. According to the fourth step S104, the general portion 6 of the panel 1 is held by the lower die 20, the pressing pad 21, and the tip bending blade 32, as shown in FIG.

[0038] The fifth step S105 is a step in which the first drawn portion 3 of the panel 1 is formed into the flange portion 5 by the rear bending blade 31. In this fifth step S105, the upper die 30 is lowered so as to move the rear bending blade 31 in the forming direction D. As a result, as shown in Fig. 9, first the rear bending blade 31 comes into contact with the first drawn portion 3 of the panel 1 and presses the first drawn portion 3. The blade surface of the rear bending blade 31 is pressed against the first drawn portion 3 of the panel 1 over the entire length in the panel width direction X.

[0039] Thereafter, as the upper die 30 continues to move downward, the first drawn portion 3 of the panel 1 is compressed by the blade surface of the rear bending blade 31 and the first forming surface 20a of the lower die 20. At this time, the rod 41 of the holding mechanism part 40 increases the elastic biasing force applied to the front bending blade 32 as the front bending blade 32 receives a reaction force from the general part 6 and the lower die 20, and moves backward so that the protruding length from the cylinder 43 becomes shorter. Then, as shown in FIG. 10, the upper die 30 continues to move downward until the rear bending blade 31 fits into the first forming surface 20a of the lower die 20 via the panel 1. As a result, the first drawn portion 3 of the panel 1 is formed into the flange portion 5 (see FIG. 3) by the gathering bending process by the rear bending blade 31. At this time, the front bending blade 32 is disposed at the retreated position P2.

[0040] Thus, the fifth step S105 is a post-bending step in which, while the general portion 6 formed in the third step S103 (pre-bending step) is sandwiched between the pre-bending blade 32 and the lower die 20, the first drawn portion 3 of the panel 1 is compressed by the post-bending blade 31 and the lower die 20 to form a concave flange portion 5. According to this fifth step S105, the panel 1 that has been pre-drawn is subjected to a gather bending process to obtain a panel 1A.

[0041] The sixth step S106 is a step for releasing the panel 1A after the gathering bending process. In this sixth step S106, the upper mold 30 is raised, thereby moving both the rear bending blade 31 and the front bending blade 32 in the opposite direction to the molding direction D. In addition, the pressing by the pressing pad 21 is released. According to the sixth step S106, as shown in FIG. 11, the contact between the flange portion 5 and the rear bending blade 31 is released, the contact between the general portion 6 and the front bending blade 32 is released, and the pressing by the pressing pad 21 is released, thereby releasing the formed panel 1A. Then, the panel 1A is finally removed from the lower mold 20.

[0042] 5. Effects According to the above-mentioned first embodiment, the following advantageous effects can be obtained.

[0043] According to the first embodiment, with the panel 1 pressed against the lower die 20 by the pressing pad 21, first, the second drawn portion 4 of the end portion 2 of the panel 1, which is on the inside of the first drawn portion 3, is compressed by the front bending blade 32 for the gathering bending process and the lower die 20 to form the general portion 6. Next, with the general portion 6 of the panel 1 sandwiched between the front bending blade 32 and the lower die 20, the first drawn portion 3, which is on the outside of the general portion 6, is compressed by the back bending blade 31 for the gathering bending process and the lower die 20 to form the flange portion 5 having a concave shape.

[0044] That is, in this embodiment, the second drawn portion 4 on the inside of the first drawn portion 3 located on the free end side (outside) of the end portion 2 of the panel 1 is bent prior to the first drawn portion 3, and the first drawn portion 3 is bent after the second drawn portion 4. By bending the panel 1 in this order, the end portion 2 of the panel 1 is allowed to deform toward the free end side until the end portion 2 of the panel 1 is bent, and compression of the end portion 2 of the panel 1 toward the inside is suppressed. As a result, even if the cross-sectional shape of the approximately V-shape of the flange portion 5 (the recess depth of the flange portion 5) differs depending on the position in the panel width direction X, and the molding amount and the compressive deformation direction of the panel 1 differ from one portion to another, wrinkles are unlikely to remain on the surfaces of the general portion 6 and the flange portion 5 of the panel 1A after the bending.

[0045] For example, as shown in Figure 3, when the end 2a near the center of the panel 1 is bent so that the upright surface 6b of the general portion 6 has an inwardly concave shape, the panel 1 is deformed inward due to the compressive load received from the bending tip of a conventional structure, and this deformation is likely to cause wrinkles. However, according to this embodiment, even in such a case, by performing the bending of the second drawing portion 4 of the panel 1 prior to the first drawing portion 3, it is possible to prevent this deformation from becoming a cause of wrinkles, even if the second drawing portion 4 is deformed inward due to the compressive load received from the bending tip blade 32.

[0046] 4, when the ends 2b on both sides of the panel 1 are bent together to form a flange portion 5 with a large recession depth, wrinkles are more likely to remain on the surface of the flange portion 5 than when a flange portion 5 with a small recession depth is formed, but according to this embodiment, the occurrence of wrinkles can be suppressed regardless of the recession depth of the flange portion 5. This makes it possible to relax restrictions on the recess depth of the flange portion 5 of the panel 1A.

[0047] In contrast to this embodiment, if the first drawn portion 3 on the free end side of the panel 1 is bent prior to the second drawn portion 4, deformation of the end portion 2 of the panel 1 toward the free end side is restricted, making it easier for wrinkles to form on the surfaces of the general portion 6 and the flange portion 5 of the panel 1.

[0048] Therefore, according to the first embodiment, it is possible to suppress wrinkles from remaining on the surface when the end portion 2 of the panel 1 that has been previously drawn and formed is formed.

[0049] The panel forming apparatus 10 of the first embodiment employs a structure in which the front bending blade 32 is incorporated into the rear bending blade 31 via a holding mechanism unit 40. According to this structure, by continuing the operation of moving the upper die 30 toward the lower die 20 while the panel 1 is pressed against the lower die 20 by the pressing pad 21, it is possible to perform, as a continuous series of operations, the operation of compressing the second drawn portion 4 of the panel 1 with the front bending blade 32 and the lower die 20 to form the general portion 6, and the operation of compressing the first drawn portion 3 of the panel 1 with the rear bending blade 31 and the lower die 20 while the general portion 6 of the panel 1 is sandwiched between the front bending blade 32 and the lower die 20 to form the flange portion 5. This makes it possible to shorten the forming time required for the gathering bending process of the panel 1.

[0050] According to the panel forming apparatus 10 of embodiment 1, in order to elastically hold the tip bending blade 32 in the forward position P1 so that it can be retracted, a structure is adopted in which the rod 41 is elastically biased by utilizing the reaction force generated when the working fluid is compressed by the piston 42, thereby simplifying the structure of the holding mechanism 40.

[0051] The present invention is not limited to the exemplary embodiment described above, and various applications and modifications are possible without departing from the scope of the present invention. For example, the following embodiments can be embodied by applying the above embodiment.

[0052] In the above-described embodiment, a structure in which the front bending blade 32 is incorporated into the rear bending blade 31 via a holding mechanism portion 40 has been exemplified, but instead, a structure in which the rear bending blade 31 and the front bending blade 32 are separate entities and move independently of each other may be adopted.

[0053] The above-described embodiment illustrates the molding of the rear end portion of the roof panel of a hatchback-type automobile body, but this embodiment can also be applied to the molding of panels of an automobile body other than the roof panel, or to the molding of panels of products other than automobile bodies. [Explanation of symbols]

[0054] Explanation of the Reference Numerals 1...panel, 2...end, 3...first drawing section, 4...second drawing section, 5...flange section, 6...general section, 10...panel forming device, 20...lower die, 21...pressing pad, 30...upper die, 31...post bending blade, 32...pre bending blade, 40...holding mechanism, 41...rod, 42...piston, 43...cylinder, P1...forward position, P2...retracted position, S101-S106...panel forming method, S103...third step (pre bending process), S105...fifth step (post bending process), X...panel width direction

Claims

1. A panel forming apparatus for forming an edge of a panel that has been previously drawn, comprising: a first drawn portion formed to extend in a panel width direction and a second drawn portion formed to extend along the first drawn portion on the inner side of the first drawn portion at the end portion of the panel; A lower die and an upper die, a pressing pad for pressing the panel against the lower mold; A back bending blade and a front bending blade that move in conjunction with the upper die; Equipped with The panel forming device is configured to press the panel against the lower die with the pressing pad and move the upper die toward the lower die, thereby compressing the second drawn portion with the front bending blade and the lower die to form a general portion, and then, with the general portion sandwiched between the front bending blade and the lower die, compressing the first drawn portion with the rear bending blade and the lower die to form a concave-shaped flange portion.

2. The panel forming apparatus of claim 1, wherein the leading bending blade is configured to protrude from the rear bending blade toward the lower mold and be movable back and forth between an advanced position and a retracted position, and the rear bending blade is provided with a holding mechanism that elastically holds the leading bending blade in the advanced position so that it can be retracted.

3. 3. The panel forming apparatus of claim 2, wherein the holding mechanism comprises a rod attached to the tip bending blade, a piston connected to the rod, and a cylinder that contains the piston and a working fluid and elastically biases the rod by utilizing a reaction force generated when the working fluid is compressed by the piston.

4. 4. The panel forming apparatus according to claim 1, wherein the flange portion has a substantially V-shaped cross section and a recess depth varies in the width direction of the panel.

5. A panel forming method for forming an end of a panel that has been previously drawn, comprising the steps of: a first drawn portion formed to extend in a panel width direction and a second drawn portion formed to extend along the first drawn portion on the inner side of the first drawn portion at the end portion of the panel; a pre-bending process in which the second drawn portion is compressed by a pre-bending blade and the lower die in a state in which the panel is pressed against the lower die by a pressing pad to form a general portion; a post-bending process in which the first drawn portion is compressed by a post-bending blade and the lower die in a state in which the general portion formed in the pre-bending process is sandwiched between the pre-bending blade and the lower die, to form a concave-shaped flange portion; The panel forming method according to claim 1,

6. 6. The panel forming method according to claim 5, wherein the flange portion has a substantially V-shaped cross section and a recess depth varies in the width direction of the panel.

Citation Information

Patent Citations

  • Draw-back bending method

    JP1995214183A

  • Drawing molding method

    JP2019107663A