Power module, method for manufacturing power module and power conversion device

The power module design with a resin convex portion and cover jig addresses solder adhesion issues, improving reliability and reducing costs by blocking solder droplets, ensuring efficient and reliable power module manufacturing.

JP2024154108APending Publication Date: 2024-10-30MITSUBISHI ELECTRIC CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023067745
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-30

AI Technical Summary

Technical Problem

Existing power modules face reliability issues due to solder droplets adhering to gate electrodes, which can be exacerbated by the manufacturing process of bending leads, increasing costs and potentially reducing insulation performance.

Method used

A power module design featuring a resin convex portion between the upper main electrode and signal electrode, thicker than the signal electrode, to block solder droplets, combined with a cover jig to prevent solder adhesion during bonding, maintaining reliability and reducing manufacturing costs.

Benefits of technology

The resin convex portion effectively prevents solder droplets from adhering to signal electrodes, enhancing wire bond reliability while avoiding cost increases and performance degradation, thus ensuring reliable power module production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154108000001_ABST
    Figure 2024154108000001_ABST
Patent Text Reader

Abstract

To provide a power module which can suppress increase in manufacturing cost and improves reliability of a wirebond.SOLUTION: A power module includes a substrate, a switching device that has an upper face main electrode provided on the upper face on the side opposite to the substrate and a signal electrode to which a control signal is supplied, and whose lower surface on the side opposite to the upper face is joined to the substrate by a first joint material, a base plate to which the substrate is joined by the first joint material, an electrode plate flowing main current of the switching device therein, a signal terminal to which the control signal of the switching device is supplied and that is connected to the signal electrode through a wire, and a case which is provided so as to surround the substrate and is joined to the top of the base plate. The electrode plate has one end joined to the upper face main electrode of the switching device by a second joint material. The signal terminal has one end connected to the wire. The switching device has a projection that is provided at least between the upper face main electrode and the signal electrode and is composed of a resin thicker than the thickness of the signal electrode.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a power module, and more particularly to a power module with improved wire bond reliability. [Background technology]

[0002] As environmental issues grow, power modules are becoming more and more common in all aspects of power generation, transmission, and regeneration of electrical energy. Power modules used in transportation equipment such as electric vehicles require particularly high reliability, so a structure in which the main circuit of a semiconductor element is soldered using a copper lead frame instead of the conventional wire bond is becoming more common. While solder is used to connect the main terminal and lead of a semiconductor element, wires are often used for gate electrodes of switching elements, etc., because the current flowing through them is small. Therefore, there is a possibility that solder will fly or solder balls will adhere to the gate electrode from the lead joint, hindering wire bonding and causing a decrease in reliability.

[0003] Patent Document 1 discloses a method of suppressing solder skipping by bending the tip of a lead to be soldered to a main terminal of a semiconductor element to form a convex portion. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 6619120 Summary of the Invention [Problem to be solved by the invention]

[0005] The method of Patent Document 1 requires a step of bending the tip of the lead, which increases manufacturing costs, and the provision of the protrusions can reduce insulation performance and hinder the injection of sealing resin.

[0006] The present disclosure has been made to solve the problems described above, and aims to provide a power module that can suppress increases in manufacturing costs, does not degrade the performance of the power module, and improves the reliability of wire bonds without being an obstacle to power module manufacturing. [Means for solving the problem]

[0007] A power module according to the present disclosure includes a substrate, a switching device having a top surface main electrode and a signal electrode to which a control signal is supplied, the bottom surface being joined to the substrate with a first bonding material, a base plate to which the substrate is joined with the first bonding material, an electrode plate through which a main current of the switching device flows, a signal terminal to which the control signal of the switching device is supplied and connected to the signal electrode via a wire, and a case provided to surround the substrate and bonded onto the base plate, one end of the electrode plate being bonded to the top surface main electrode of the switching device with a second bonding material and the other end being inserted into a wall surface of the case, one end of the signal terminal being connected to the wire and the other end being inserted into the wall surface of the case, and the switching device has a protrusion provided at least between the top surface main electrode and the signal electrode, and made of resin that is thicker than the thickness of the signal electrode. Effect of the Invention

[0008] According to the power module of the present disclosure, since there is a protrusion made of resin between the upper main electrode and the signal electrode of the switching device, which is thicker than the signal electrode, even if droplets of the molten second bonding material roll over the switching device when the electrode plate and the upper main electrode of the switching device are bonded, the droplets can be blocked and prevented from adhering to the signal electrode, thereby obtaining a power module with improved reliability of wire bonding to the signal electrode. Furthermore, since the protrusion is made of resin and provided locally, it is possible to suppress an increase in manufacturing costs, and it does not degrade the performance of the power module or become an obstacle to the manufacture of the power module. [Brief description of the drawings]

[0009] [Figure 1] 1 is a plan view showing a configuration of a power module according to a first embodiment of the present disclosure. [Diagram 2] 1 is a cross-sectional view showing a configuration of a power module according to a first embodiment of the present disclosure. [Diagram 3] 1A to 1C are cross-sectional views illustrating a manufacturing process for the power module according to the first embodiment of the present disclosure. [Figure 4] 1A to 1C are cross-sectional views illustrating a manufacturing process for the power module according to the first embodiment of the present disclosure. [Diagram 5] 1A to 1C are cross-sectional views illustrating a manufacturing process for the power module according to the first embodiment of the present disclosure. [Figure 6] 1A to 1C are cross-sectional views illustrating a manufacturing process for the power module according to the first embodiment of the present disclosure. [Figure 7] 1A to 1C are cross-sectional views illustrating a manufacturing process for the power module according to the first embodiment of the present disclosure. [Figure 8] 1 is a plan view showing a configuration of a power module according to a first modification of the first embodiment of the present disclosure. FIG. [Figure 9] 10 is a plan view showing a configuration of a power module according to a second modification of the first embodiment of the present disclosure. FIG. [Figure 10] 6A to 6C are cross-sectional views illustrating a manufacturing process for the power module according to the second embodiment of the present disclosure. [Figure 11] 6A to 6C are cross-sectional views illustrating a manufacturing process for the power module according to the second embodiment of the present disclosure. [Figure 12] 11A to 11C are plan views illustrating a manufacturing process of the power module according to the second embodiment of the present disclosure. [Figure 13] 6A to 6C are cross-sectional views illustrating a manufacturing process for the power module according to the second embodiment of the present disclosure. [Figure 14] FIG. 4 is a diagram showing the results of evaluating the effects of the first and second embodiments according to the present disclosure. [Figure 15]11 is a block diagram showing a configuration of a power conversion system to which a power conversion device according to a third embodiment of the present disclosure is applied. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] <Embodiment 1> <Device configuration> Fig. 1 is a plan view showing a configuration of a power module 202 according to a first embodiment of the present disclosure. In Fig. 1, the sealing resin inside the power module 202 is omitted for convenience, and the power module 202 is viewed from the top side. Fig. 2 is a cross-sectional view taken along line AA in Fig. 1 in the direction indicated by the arrow.

[0011] As shown in FIG. 2, in the power module 202, a ceramic substrate 11 is bonded to the upper surface of a base plate 10 with solder 30 (first bonding material), and a switching device 20 such as an IGBT (Insulated Gate Bipolar Transistor) and a diode 21 are bonded to the upper surface of the ceramic substrate 11 with the solder 30.

[0012] Base plate 10 is adhered to the bottom side wall of case 5 with adhesive 72 so as to cover the opening on the bottom side of case 5 made of PPS (Poly Phenylene Sulfide) resin, which has openings on the top and bottom sides.

[0013] The ceramic substrate 11 has a surface conductor layer 111 provided on the upper surface on which the device is mounted, and a back surface conductor layer 112 provided on the lower surface opposite to the upper surface, and the back surface conductor layer 112 is joined to the base plate 10 by solder 30. In addition, the surface conductor layer 111 is joined to the lower surface main electrodes (not shown) of the switching device 20 and the diode 21 by solder 30.

[0014] The upper surface main electrode 212 of the switching device 20 and the upper surface main electrode 211 of the diode 21 are commonly joined to an electrode plate 65 by solder 31 (second bonding material). The electrode plate 65 is insert-molded into the case 5, and the portion of the electrode plate 65 protruding outside the case 5 serves as a main terminal 62.

[0015] A signal electrode 213 for supplying a control signal to the switching device 20 is provided on the top surface of the switching device 20 near the top surface main electrode 212. The signal electrode 213 is connected to one end of a signal terminal 61 that is insert-molded into the case 5 by an aluminum wire 40. The other end of the signal terminal 61 protrudes to the outside of the case 5.

[0016] The thickness of the upper surface main electrode 212 and the signal electrode 213 of the switching device 20 is 0.01 mm, and the thickness of the upper surface main electrode 211 of the diode 21 is 0.01 mm.

[0017] As shown in FIG. 1, a convex portion 71 is provided to surround the arrangement area of ​​the signal electrode 213 of the switching device 20, and as shown in FIG. 2, the height of the convex portion 71 is formed to exceed the thickness of the signal electrode 213.

[0018] As shown in FIG. 1, an electrode plate 66 is insert-molded into the case 5, one end of the electrode plate 66 is joined to the surface conductor layer 111 by solder (not shown), and the portion of the electrode plate 66 protruding outside the case 5 serves as the main terminal 63.

[0019] 1 and 2 show a 1-in-1 configuration in which one switching device 20 and one diode 21 are housed in the case 5, but this is merely an example in which the present disclosure is applied to a configuration corresponding to one arm of an inverter, and the application of the present disclosure is not limited to this. The present disclosure can also be applied to a 2-in-1 configuration in which switching devices 20 and diodes 21 for one phase of an inverter are housed, and a 6-in-1 configuration in which switching devices 20 and diodes 21 for three phases of an inverter are housed.

[0020] Next, the material of each member of the power module 202 will be described. The ceramic substrate 11 is provided with a front conductor layer 111 in which two copper conductor layers of 17 mm x 37 mm x 0.8 mm are partially connected, and a rear conductor layer 112 made of copper of 37 mm x 37 mm x 0.8 mm, on an aluminum nitride (AlN) base material of 40 mm x 40 mm x 2 mm thickness. The front conductor layer 111 and the rear conductor layer 112 can be formed by metallizing the ceramic substrate 11.

[0021] The switching device 20 is made of silicon and has dimensions of 13 mm×13 mm×0.2 mm thick, and the diode 21 is made of silicon and has dimensions of 13 mm×10 mm×0.2 mm thick. The solder 30 is composed of 96.5% tin, 3% silver, and 0.5% copper, and has a melting point of 217°C.

[0022] The electrode plates 65, 66 and the signal terminal 61 which are insert-molded into the case 5 are made of copper and have a thickness of 0.64 mm.

[0023] The protrusion 71 provided around the signal electrode 213 of the switching device 20 is made of resin such as polyimide, and is 1.0 mm wide and 1.0 mm high. The aluminum wire 40 connecting the signal electrode 213 of the switching device 20 to the copper signal terminal 61 having a thickness of 0.64 mm is made of pure aluminum with a thickness of 0.15 mm.

[0024] The ceramic substrate 11 is not limited to an AlN substrate as long as it has insulating properties and can form a conductive layer that is wettable with solder, such as Cu. The substrate may be an insulating substrate such as alumina (Al2O3), silicon carbide (SiC), or silicon nitride (Si3N4).

[0025] Moreover, the front conductor layer 111 and the back conductor layer 112 may be made of any metal that is wettable by solder, and may not be limited to Cu, but may be made of any metal such as Sn, Au, Ag, etc. Furthermore, the front and back electrodes of the switching device 20 and the diode 21 may be made of any metal that is wettable by solder, and may be made of any metal such as Sn, Au, Ag, etc.

[0026] Although an IGBT and a diode are used as the power semiconductor elements, a MOSFET (Metal Oxide Semiconductor Field Effect Transistor) can also be used, and an IC (Integrated Circuit) can also be mounted.

[0027] Besides being made of silicon, the switching device 20 and the diode 21 may also be made of a wide band gap semiconductor such as silicon carbide or gallium nitride.

[0028] The material of the electrode plates 65, 66 and the signal terminals 61 may be a copper alloy or aluminum with a nickel-plated surface, in addition to copper.

[0029] For the solder 30 and the solder 31, a solder material such as 99.3% tin, 0.7% copper, and a melting point of 224° C. may be used.

[0030] By using the solders 30 and 31, which have relatively low melting points and are easy to handle, as the bonding materials, the manufacturing costs can be reduced.

[0031] The solder 30 and the solder 31, which are the bonding materials in contact with the switching device 20 and the diode 21, can be replaced with a bonding material such as a silver sintered material or a brazing material that has better heat resistance than solder. Also, a bonding material such as a conductive adhesive in which silver (Ag) filler is dispersed in an epoxy resin, or Ag nanopowder or Cu nanopowder in which nanoparticles are baked at a low temperature can be used.

[0032] The wire 40 may be made of aluminum, an aluminum alloy containing a small amount of additive such as iron, a copper wire, an aluminum-coated copper wire, or a gold wire. Also, a ribbon bond may be used.

[0033] Besides PPS resin, LCP (Liquid Crystal Polymer) resin can also be used as the material for case 5. In either case, the heat resistance temperature can be increased by dispersing a filler.

[0034] As the sealing resin 73, an epoxy resin with dispersed silica filler is used, but fillers such as alumina and boron nitride (BN) can also be used, and a resin in which a silicone resin is mixed into an epoxy resin can also be used.

[0035] <Manufacturing method> Next, as a manufacturing method of the first embodiment, a manufacturing method of the power module 202 will be described with reference to cross-sectional views of FIGS. 3 to 7 showing the manufacturing steps in sequence.

[0036] 3, first, the base plate 10 and the ceramic substrate 11 are laminated with unmelted plate-like solder 30 therebetween, the switching device 20 and the diode 21 are laminated on the ceramic substrate 11 with the plate-like solder 30 therebetween, and the laminate is heated to melt the plate-like solder 30. This simultaneously bonds the back surface conductor layer 112 of the ceramic substrate 11 to the base plate 10, and the front surface conductor layer 111 of the ceramic substrate 11 to the switching device 20 and the diode 21. The bonding with the solder 30 is performed by heating the laminate to about 280° C. using a reflow furnace to melt the solder 30 and bond the components.

[0037] 4, a needle 75 provided at the tip of a dispenser (not shown) that supplies liquid resin material is used to draw and form liquid resin material 710 around signal electrode 213 of switching device 20. At this time, the height of resin material 710 is set by calculating shrinkage due to hardening so that convex portion 71 will have a height of 1.0 mm after hardening.

[0038] Next, in the step shown in FIG. 5, adhesive 72 for bonding to case 5 is applied to the edge portion of base plate 10.

[0039] 6, case 5 is mounted on base plate 10 via adhesive 72. At this time, electrode plate 65 is disposed so that the lower surface thereof faces upper main electrode 212 of switching device 20 and upper main electrode 211 of diode 21 via plate-like solder 31 before melting.

[0040] Then, adhesive 72 is heated to bond and fix case 5 and base plate 10, and at the same time, resin material 710 is hardened, and upper surface main electrode 212 of switching device 20 and upper surface main electrode 211 of diode 21 are joined to electrode plate 65 using solder 31. At the same time, electrode plate 66 (not shown) is also joined to surface conductor layer 111 by solder.

[0041] For adhesive fixation, the adhesive 72 and the solder 31 are heated and hardened in a reflow furnace to about 280° C. Although the solders 30 and 31 are in the form of plates, cream solder may also be used.

[0042] Next, in the step shown in FIG. 7, the signal terminal 61 insert-molded into the case 5 and the signal electrode 213 of the switching device 20 are connected by wire bonding using the wire 40.

[0043] Finally, the direct potting sealing resin is heated to 60° C. and poured into the case 5, vacuum degassed, and heated to harden, completing the power module 202 in which the inside of the case 5 is sealed with the sealing resin 73 as shown in Fig. 2. To harden the sealing resin 73, heating is performed at 100° C. for 1.5 hours, and then at 140° C. for 1.5 hours. Note that since the adhesive 72 fills the gap between the base plate 10 and the case 5, leakage of the sealing resin can be prevented when the direct potting sealing resin is poured into the case 5.

[0044] When electrode plate 65 is joined to top main electrode 212 of switching device 20 and top main electrode 211 of diode 21 using plate-shaped solder 31, solder splashes or solder balls are generated from solder 31 at the joint. If such solder splashes roll and adhere to signal electrode 213 of switching device 20, they may impede wire bonding or reduce reliability.

[0045] Therefore, by forming a resin convex portion 71 around the signal electrode 213 of the switching device 20, it is possible to prevent the rolling solder from adhering to the signal electrode 213, and it is possible to obtain a power module 202 with improved wire bond reliability without being an obstacle to the manufacture of the power module.

[0046] Furthermore, since the convex portion 71 is made of resin and is provided locally around the signal electrode 213, an increase in manufacturing costs can be suppressed, and the provision of the convex portion 71 does not result in a decrease in insulation performance, and does not become an obstacle when injecting the sealing resin 73. Therefore, the performance of the power module 202 is not reduced, and the convex portion 71 does not become an obstacle when manufacturing the power module 202.

[0047] The protrusions 71 can also be removed by chemical etching or laser irradiation after the electrode plate 65 is bonded to the upper main electrode 212 of the switching device 20 and the upper main electrode 211 of the diode 21 .

[0048] <Variation 1> Fig. 8 is a plan view showing the configuration of a power module 2021 according to Modification 1 of Embodiment 1. In Fig. 8, the same components as those in power module 202 shown in Fig. 1 are given the same reference numerals, and duplicated explanations will be omitted.

[0049] 8, in the power module 2021, convex portions 711 are provided in front of and behind the signal electrodes 213 of the switching device 20. That is, the convex portions 711 are provided only in front of and behind the arrangement of the signal electrodes 213 so as to block the direction in which the solder rolls from the solder 31 of the joint when the electrode plate 65 is joined using the solder 31. Even with this configuration, the effect of preventing the solder from adhering to the signal electrodes 213 can be obtained.

[0050] The convex portion 711 can be provided between the switching device 20 and the signal electrode 213, that is, only in front of the signal electrode 213. By using such a configuration, the formation area of ​​the convex portion 711 is limited, and the adhesion of solder to the signal electrode 213 can be effectively prevented.

[0051] <Variation 2> Fig. 9 is a plan view showing the configuration of a power module 2022 according to Modification 2 of Embodiment 1. In Fig. 9, the same components as those in power module 202 shown in Fig. 1 are denoted by the same reference numerals, and duplicated explanations will be omitted.

[0052] As shown in FIG. 9, in the power module 2022, the convex portion 712 and the convex portion 713 are provided so as to surround the periphery of the array of the signal electrodes 213 of the switching device 20 in a double manner. That is, the convex portion 713 is provided so as to surround the immediate vicinity of the array of the signal electrodes 213, and the convex portion 712 is provided so as to surround the convex portion 713. By doubly surrounding the periphery of the array of the signal electrodes 213 with the convex portion 712 and the convex portion 713, a higher adhesion prevention effect can be obtained against the solder rolling from the solder 31 at the joint portion when the electrode plate 65 is joined using the solder 31. Note that the configuration is not limited to doubly, but may be multiplexed, such as triple or quadruple, in surrounding the array of the signal electrodes 213.

[0053] <Embodiment 2> 10 to 13, a method for manufacturing the power module 202 will be described below as a manufacturing method of the second embodiment. As described with reference to Figs. 3 to 5, the steps of bonding the back conductor layer 112 of the ceramic substrate 11 to the base plate 10 and simultaneously bonding the switching device 20 and the diode 21 to the front conductor layer 1112 of the ceramic substrate 11, the step of drawing and forming the resin convex portion 71 around the signal electrode 213 of the switching device 20, and the step of applying the adhesive 72 to the base plate 10 are the same as those in the manufacturing method of the first embodiment, and therefore the description thereof will be omitted.

[0054] In the process shown in Fig. 10, when the case 5 and the base plate 10 are bonded and fixed with the adhesive 72 and the electrode plate 65 is bonded to the upper surface main electrode 212 of the switching device 20 and the upper surface main electrode 211 of the diode 21, a cover jig 90 made of a metal such as stainless steel having a spring portion 91 is arranged to cover the upper portion of the opening OP of the case 5. The spring portion 91 of the cover jig 90 protrudes vertically from the lower surface of the cover jig 90 and has a shape in which the tip is horizontally bent, and the horizontally bent portion is a flat plate-like member 911. When the cover jig 90 is placed over the opening OP, the plate-like member 911 is pressed against the protrusions 71 provided around the signal electrode 213, covering the signal electrode 213 and the protrusions 71. Fig. 11 is a cross-sectional view showing this state. Although a stainless steel cover jig 90 is used here, any heat-resistant material that does not get wet with solder and has spring properties can be used. By using titanium alloy, carbon steel, or chrome-plated nickel alloy, it is possible to ensure long-term durability.

[0055] Fig. 12 shows a plan view of power module 202 seen from the top side in the state shown in Fig. 11. As shown in Fig. 12, covering jig 90 does not completely cover opening OP of case 5, but covers above switching devices 20 and diodes 21, above electrode plate 65, above the array of signal electrodes 213, and above the array of signal terminals 61, and is formed to a length and shape that enables it to be fixed to the edge of case 5.

[0056] 11, with plate-like member 911 of spring portion 91 pressed against protrusion 71, case 5 and base plate 10 are bonded and fixed, protrusion 71 is hardened, and electrode plate 65 is joined to top main electrode 212 of switching device 20 and top main electrode 211 of diode 21 at the same time. At this time, heating to about 280° C. is performed using a reflow furnace, as in the first embodiment.

[0057] Thereafter, cover jig 90 is removed, and in the process shown in FIG. 13, signal terminal 61 insert-molded into case 5 and signal electrode 213 of switching device 20 are connected using wire 40. Finally, direct potting sealing resin is heated to 60° C. and poured into case 5, vacuum-degassed, and heated to harden, thereby completing power module 202 in which case 5 is sealed with sealing resin 73 as shown in FIG. 2.

[0058] As explained in the first embodiment, when electrode plate 65 is joined to top main electrode 212 of switching device 20 and top main electrode 211 of diode 21 using plate-shaped solder 31, if solder skips or solder balls occur from solder 31 at the joint, forming resin convex portion 71 around signal electrode 213 of switching device 20 has the effect of preventing such solder from rolling and adhering to signal electrode 213 of switching device 20.

[0059] On the other hand, when the solder melts, air caught in the solder may burst, causing the solder to fly. In the manufacturing method of the second embodiment, the signal electrode 213 and the protrusion 71 are covered by the spring portion 91 of the cover jig 90, so that it is possible to suppress not only the rolling solder but also the adhesion of the flying solder to the signal electrode 213.

[0060] Furthermore, since the spring portion 91 of the covering jig 90 has spring properties in the vertical direction, it is possible to cover the protrusions 71 even if their heights vary slightly.

[0061] 14 is a diagram showing the results of evaluating the effects of the first and second embodiments. In this evaluation, water was dripped onto molten cream solder, the solder was intentionally splashed, and the solder was measured within 1 mm of the metal plate. 2 That is, the number of solder splashes per mm2 of the metal plate was measured in three cases: when the metal plate was not provided with the protrusions 71, when the metal plate was provided with the protrusions 71, and when the metal plate was provided with the protrusions 71 and the protrusions 71 were covered with the cover jig 90. 2 The number of solder splashes per unit was measured.

[0062] 14, the left graph shows the results when no protrusion 71 is provided and no cover jig 90 is arranged, the center graph shows the results when protrusion 71 is provided and no cover jig 90 is arranged, and the right graph shows the results when protrusion 71 is provided and cover jig 90 is arranged. The verification was performed with the verification device in the same state as power module 202, for example, the positional relationship between the metal plate and the cream solder was the same as the positional relationship between signal electrode 213 and plate-shaped solder 51.

[0063] 14, the number of solder splashes was reduced to about 1 / 4 by changing from the embodiment without a cover jig and with a protrusion to the embodiment without a cover jig and with a protrusion. Furthermore, the number of solder splashes was reduced to 1 / 3 or less by changing from the embodiment without a cover jig and with a protrusion to the embodiment with a cover jig and with a protrusion. From these evaluation results, it was confirmed that the manufacturing methods of the first and second embodiments are effective in suppressing solder adhesion to the signal electrode 213 of the switching device 20.

[0064] Although the spring portion 91 of the cover jig 90 has been given spring properties, it may be configured not to have spring properties.

[0065] <Embodiment 3> In this embodiment, the power module according to the above-mentioned embodiment 1 is applied to a power conversion device. Hereinafter, as embodiment 3, a case where embodiment 1 is applied to a three-phase inverter will be described. Note that the power conversion device is not limited to a three-phase inverter.

[0066] Fig. 15 is a block diagram showing a configuration of a power conversion system to which a power conversion device according to this embodiment is applied. The power conversion system shown in Fig. 15 is composed of a power source 100, a power conversion device 200, and a load 300. The power source 100 is a DC power source and supplies DC power to the power conversion device 200. The power source 100 is not particularly limited, and may be composed of, for example, a DC system, a solar cell, or a storage battery, or may be composed of a rectifier circuit or an AC / DC converter connected to an AC system. The power source 100 may also be composed of a DC / DC converter that converts DC power output from a DC system into a predetermined DC power.

[0067] The power conversion device 200 is a three-phase inverter connected between the power source 100 and the load 300, converts DC power supplied from the power source 100 into AC power, and supplies the AC power to the load 300. As shown in Fig. 15, the power conversion device 200 includes a main conversion circuit 201 that converts DC power into AC power and outputs it, and a control circuit 203 that outputs a control signal for controlling the main conversion circuit 201 to the main conversion circuit 201.

[0068] The load 300 is a three-phase motor driven by AC power supplied from the power conversion device 200. The load 300 is, although not limited to, a motor mounted on various electric devices, and is used as, for example, a motor for a hybrid vehicle, an electric vehicle, a railroad car, an elevator, or an air conditioner.

[0069] The power conversion device 200 will be described in detail below. The main conversion circuit 201 includes a switching device (not shown) and a free wheel diode (not shown), and converts DC power supplied from the power source 100 into AC power by switching the switching device, and supplies the AC power to the load 300. There are various specific circuit configurations of the main conversion circuit 201, but the main conversion circuit 201 according to this embodiment is a two-level three-phase full bridge circuit, and can be configured with six switching devices and six free wheel diodes connected inversely in parallel to each switching device. The power module of the main conversion circuit 201 is the power module 202 of the above-mentioned embodiment 1 applied to a 6-in-1 configuration in which the switching devices 20 and diodes 21 for the three phases of the inverter are housed.

[0070] The six switching devices are connected in series in pairs to form upper and lower arms, and each upper and lower arm constitutes one phase (U phase, V phase, and W phase) of the full-bridge circuit. The output terminals of each upper and lower arm, i.e., the three output terminals of the main conversion circuit 201, are connected to a load 300.

[0071] The main conversion circuit 201 also includes a drive circuit (not shown) that drives each switching device, but the drive circuit may be built into the power module 202, or a configuration may be adopted in which the drive circuit is provided separately from the power module 202. The drive circuit generates drive signals that drive the switching devices of the main conversion circuit 201, and supplies the drive signals to the control electrodes of the switching devices of the main conversion circuit 201.

[0072] Specifically, a drive signal for turning on the switching device and a drive signal for turning off the switching device are output to the control electrode of each switching device in accordance with a control signal from the control circuit 203 described later. When maintaining a switching device in the on state, the drive signal is a voltage signal (on signal) equal to or higher than the threshold voltage of the switching device, and when maintaining a switching device in the off state, the drive signal is a voltage signal (off signal) below the threshold voltage of the switching device.

[0073] The control circuit 203 controls the switching devices of the main conversion circuit 201 so that the desired power is supplied to the load 300. Specifically, the control circuit 203 calculates the time (on time) for which each switching device of the main conversion circuit 201 should be in the on state based on the power to be supplied to the load 300. For example, the main conversion circuit 201 can be controlled by pulse width modulation (PWM) control, which modulates the on time of the switching device according to the voltage to be output. Then, a control command (control signal) is output to a drive circuit provided in the main conversion circuit 201 so that an on signal is output to a switching device that should be in the on state at each point in time, and an off signal is output to a switching device that should be in the off state. The drive circuit outputs an on signal or an off signal as a drive signal to the control electrode of each switching device according to this control signal.

[0074] In the power conversion device 200 according to the present embodiment, the power module 202 according to the first embodiment is applied as the power module 202 included in the main conversion circuit 201. Therefore, in the power conversion device 200 according to the present embodiment, the reliability of the wire bond is improved in the manufacture of the power module, and the reliability of the power module 202 is improved, and thus the reliability of the power conversion device is improved.

[0075] In the present embodiment, an example in which the present disclosure is applied to a two-level three-phase inverter has been described, but the present disclosure is not limited thereto and can be applied to various power conversion devices. In the present embodiment, a two-level power conversion device is described, but a three-level or multi-level power conversion device may be used. When the power conversion device supplies power to a single-phase load, the present disclosure may be applied to a single-phase inverter. In addition, when the power conversion device supplies power to a DC load or the like, the present disclosure may be applied to a DC / DC converter or an AC / DC converter.

[0076] Furthermore, the power conversion device of this embodiment is not limited to the case where the above-mentioned load is an electric motor, but can also be used, for example, as a power supply device for an electric discharge machine or a laser processing machine, or an induction heating cooker or a non-contact power supply system, and can also be used as a power conditioner for a solar power generation system, a power storage system, etc.

[0077] In addition, within the scope of the present disclosure, it is possible to freely combine the respective embodiments, and to appropriately modify or omit the respective embodiments.

[0078] The scope of the present disclosure is defined by the claims, rather than the above description, and is intended to include all modifications within the meaning and scope of the claims.

[0079] The present disclosure described above will now be summarized as an appendix.

[0080] (Appendix 1) A substrate; a switching device having an upper surface main electrode and a signal electrode to which a control signal is supplied, the lower surface being bonded to the substrate by a first bonding material; a base plate to which the substrate is bonded by the first bonding material; an electrode plate through which a main current of the switching device flows; a signal terminal to which the control signal of the switching device is supplied and which is connected to the signal electrode via a wire; a case provided to surround the substrate and joined onto the base plate; The electrode plate is one end of the insulating film is bonded to the upper main electrode of the switching device by a second bonding material, and the other end of the insulating film is inserted into a wall surface of the case; The signal terminal is One end is connected to the wire, and the other end is inserted into the wall of the case, The switching device is a protrusion made of resin and having a height greater than a thickness of the signal electrode, the protrusion being provided at least between the upper surface main electrode and the signal electrode.

[0081] (Appendix 2) The protrusion is 2. The power module according to claim 1, wherein the power module is provided so as to surround an area in which the signal electrode is disposed.

[0082] (Appendix 3) The protrusion is 2. The power module according to claim 1, wherein the signal electrode is disposed in a region surrounded by multiple layers.

[0083] (Appendix 4) 2. The power module of claim 1, wherein the first and second bonding materials are made of solder.

[0084] (Appendix 5) A method for manufacturing the power module according to claim 1, (a) stacking the base plate, the substrate, and the switching device with the first bonding material before melting therebetween, and heating the stack to melt the first bonding material; After the step (a), (b) disposing a resin material at least between the top surface main electrode and the signal electrode of the switching device; After the step (b), (d) mounting the case on the base plate with an adhesive therebetween so that a lower surface of the one end of the electrode plate faces the upper surface main electrode of the switching device with the second bonding material before melting therebetween; After the step (d), (e) curing the resin material to form the protrusions and heating the second bonding material to melt the second bonding material; After the step (e), (f) connecting the wire between the signal electrode and the signal terminal.

[0085] (Appendix 6) The step (b) 6. A method for manufacturing a power module according to claim 5, further comprising the step of arranging the resin material so as to surround an area in which the signal electrode is disposed.

[0086] (Appendix 7) The step (b) A method for manufacturing a power module according to claim 5, further comprising the step of arranging the resin material so as to surround an area in which the signal electrode is disposed in multiple layers.

[0087] (Appendix 8) Between the step (d) and the step (e), (g) A method for manufacturing a power module according to claim 5, further comprising the step of covering the resin material and the signal electrode with a plate-shaped member.

[0088] (Appendix 9) The step (g) A method for manufacturing a power module according to claim 8, further comprising the step of pressing the plate-like member against the resin material so that the plate-like member has spring properties in a direction perpendicular to the base plate.

[0089] (Appendix 10) A main conversion circuit having the power module according to any one of Supplementary Note 1 to Supplementary Note 4, which converts input power and outputs the converted power; a control circuit that outputs a control signal for controlling the main conversion circuit to the main conversion circuit. [Explanation of symbols]

[0090] 5 case, 10 base plate, 11 ceramic substrate, 20 switching device, 212 upper main electrode, 213 signal electrode, 21 diode, 30, 31 solder, 40 wire, 61 signal terminal, 65 electrode plate, 71 protrusion, 72 adhesive, 911 plate-shaped member, 100 power supply, 200 power conversion device, 201 main conversion circuit, 202 power module, 203 control circuit, 213 signal electrode.

Claims

1. A substrate; a switching device having an upper surface main electrode and a signal electrode to which a control signal is supplied, the lower surface being bonded to the substrate by a first bonding material; a base plate to which the substrate is bonded by the first bonding material; an electrode plate through which a main current of the switching device flows; a signal terminal to which the control signal of the switching device is supplied and which is connected to the signal electrode via a wire; a case provided to surround the substrate and joined onto the base plate; The electrode plate is one end of the insulating film is bonded to the upper main electrode of the switching device by a second bonding material, and the other end of the insulating film is inserted into a wall surface of the case; The signal terminal is One end is connected to the wire, and the other end is inserted into the wall of the case, The switching device is a protrusion made of resin and having a height greater than a thickness of the signal electrode, the protrusion being provided at least between the upper surface main electrode and the signal electrode.

2. The protrusion is The power module according to claim 1 , wherein the power module is provided so as to surround an area in which the signal electrodes are disposed.

3. The protrusion is 2. The power module according to claim 1, wherein the signal electrodes are arranged in a multi-layer structure so as to surround the area where the signal electrodes are arranged.

4. The power module according to claim 1 , wherein the first and second bonding materials are made of solder.

5. A method for manufacturing the power module according to claim 1, comprising the steps of: (a) stacking the base plate, the substrate, and the switching device with the first bonding material before melting therebetween, and heating the stack to melt the first bonding material; After the step (a), (b) disposing a resin material at least between the top surface main electrode and the signal electrode of the switching device; After step (b), (d) mounting the case on the base plate with an adhesive therebetween so that a lower surface of the one end of the electrode plate faces the upper surface main electrode of the switching device with the second bonding material before melting therebetween; After step (d), (e) curing the resin material to form the protrusions and heating the second bonding material to melt the second bonding material; After step (e), (f) connecting the wire between the signal electrode and the signal terminal.

6. The step (b) The method for producing a power module according to claim 5 , further comprising the step of arranging the resin material so as to surround an area in which the signal electrodes are provided.

7. The step (b) The method for producing a power module according to claim 5 , further comprising the step of arranging the resin material so as to surround in multiple layers an area in which the signal electrodes are provided.

8. Between the step (d) and the step (e), The method for producing a power module according to claim 5 , further comprising the step of: (g) covering the resin material and the signal electrodes with a plate-shaped member.

9. The step (g) The method for producing a power module according to claim 8 , further comprising the step of pressing the plate-like member against the resin material so that the plate-like member has spring properties in a direction perpendicular to the base plate.

10. A main conversion circuit having the power module according to any one of claims 1 to 4, which converts input power and outputs the converted power; a control circuit that outputs a control signal for controlling the main conversion circuit to the main conversion circuit.

Citation Information

Patent Citations

  • Semiconductor device and manufacturing method thereof

    JP6619120B1