Manufacturing method for semiconductor device including diode
A cost-effective method for forming crystal defects in the cathode layer of a diode using common processes like ion implantation and laser irradiation addresses the high-cost issue of helium ion irradiation, achieving high on-characteristics and rapid recovery current attenuation.
Patent Information
- Application Number
- JP2023067962
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-18
- Publication Date
- 2024-10-30
- Estimated Expiration
- 2043-04-18
AI Technical Summary
Forming crystal defects in the cathode layer of a diode using helium ion irradiation increases manufacturing costs due to the need for specialized equipment, and existing methods quickly attenuate the recovery current of the diode.
A manufacturing method that includes semiconductor substrate preparation, anode and cathode layer formation, and laser irradiation to create high-density crystal defects in the cathode layer, using common processes like ion implantation and laser irradiation to form a diode with distinct layers having different impurity concentrations, thereby activating impurities and controlling defect distribution.
The method achieves high on-characteristics and rapid attenuation of recovery current in the diode, reducing manufacturing costs by avoiding specialized helium ion irradiation and maintaining crystal defects only in specific areas of the cathode layer.
Smart Images

Figure 2024154232000001_ABST
Abstract
Description
[Technical field]
[0001] The technology disclosed in this specification relates to a method for manufacturing a semiconductor device having a diode.
[0002] Patent Document 1 discloses a method for manufacturing a semiconductor device having an insulated gate bipolar transistor (hereinafter sometimes referred to as IGBT) and a diode. In this manufacturing method, an n-type cathode layer is formed by ion implantation of n-type impurities. Next, a semiconductor substrate is irradiated with helium ions to form a high density of crystal defects in the cathode layer. By forming crystal defects in the cathode layer, snapback can be suppressed when the IGBT is turned on. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2015-211149 A Summary of the Invention [Problem to be solved by the invention]
[0004] It has been found that forming crystal defects in the cathode layer of a diode makes it possible to quickly attenuate the recovery current of the diode. This effect can be obtained not only in a semiconductor device having an IGBT and a diode, but also in a semiconductor device consisting of a single diode. When forming crystal defects in the cathode layer by irradiating helium ions as in Patent Document 1, a dedicated facility for irradiating helium ions is required, which increases the manufacturing cost. This specification proposes a technology for easily forming a diode having crystal defects in the cathode layer. [Means for solving the problem]
[0005] In the method for manufacturing a semiconductor device disclosed in the present specification, a semiconductor device is manufactured having a diode including a p-type anode layer (42), an n-type cathode layer (48), and a drift layer (44) disposed between the anode layer and the cathode layer. The manufacturing method includes a semiconductor substrate preparation step, an anode layer formation step, a cathode layer formation step, and a laser irradiation step. In the semiconductor substrate preparation step, a semiconductor substrate is prepared that is made of silicon, has a first surface (12a) and a second surface (12b) located on the opposite side of the first surface, and has the drift layer. In the anode layer formation step, the anode layer is formed in a range including the first surface in the semiconductor substrate. In the cathode layer formation step, the cathode layer is formed in a range including the second surface in the semiconductor substrate by implanting an n-type impurity into the second surface. In the laser irradiation step, a laser (92) is irradiated to the second surface after the cathode layer formation step is performed. In the cathode layer forming step, the cathode layer is formed having an n-type first cathode layer (48a) distributed in a range including the second surface, and an n-type second cathode layer (48b) that contacts the first cathode layer from the first surface side and has a lower n-type impurity concentration than the first cathode layer. In the laser irradiation step, a heated range (94) of 950°C or higher is formed in a surface layer portion of the semiconductor substrate near the second surface. In the laser irradiation step, the boundary between the first cathode layer and the second cathode layer is located within the heated range, and the end of the second cathode layer on the first surface side is located closer to the first surface than the heated range.
[0006] The anode layer may be formed by either ion implantation or epitaxial growth. Either the anode layer formation step or the cathode layer formation step may be performed first. In the cathode layer formation step, either the first cathode layer or the second cathode layer may be formed first.
[0007] In this manufacturing method, when the n-type impurity is injected into the first cathode layer and the second cathode layer, crystal defects are formed at a high density inside the first cathode layer and the second cathode layer. Then, in the laser irradiation process, the second surface is irradiated with a laser. In the laser irradiation process, a heating range of 950°C or higher is formed. In the heating range, the silicon is exposed to a temperature of 950°C or higher, so that the impurities are activated and the crystal defects disappear. Since the boundary between the first cathode layer and the second cathode layer is located within the heating range (i.e., the entire first cathode layer is included within the heating range), the entire first cathode layer is activated and most of the crystal defects in the first cathode layer disappear. In this way, a first cathode layer with high crystallinity and high n-type impurity concentration is formed, so that a high on-characteristic of the diode can be realized. In addition, since the end of the second cathode layer on the first surface side is located closer to the first surface side than the heating range (i.e., located outside the heating range), crystal defects are difficult to eliminate at the end of the second cathode layer on the first surface side. Therefore, many crystal defects remain in the second cathode layer. This allows the recovery current of this diode to decay quickly. As described above, this manufacturing method makes it possible to manufacture a diode having crystal defects in the cathode layer. Also, in this manufacturing method, a cathode layer having crystal defects can be formed by the general process of injecting n-type impurities into the cathode layer and irradiating the second surface with a laser. Therefore, a diode having crystal defects in the cathode layer can be manufactured at low cost. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is a cross-sectional view of a semiconductor device 10. [Diagram 2] FIG. 4 is an enlarged cross-sectional view of the cathode layer 48. [Diagram 3] 3A to 3C are explanatory diagrams of a manufacturing method of the semiconductor device 10. [Figure 4] 3A to 3C are explanatory diagrams of a manufacturing method of the semiconductor device 10. [Diagram 5] 3A to 3C are explanatory diagrams of a manufacturing method of the semiconductor device 10. [Figure 6] 3A to 3C are explanatory diagrams of a manufacturing method of the semiconductor device 10. [Figure 7] 3A to 3C are explanatory diagrams of a manufacturing method of the semiconductor device 10. [Figure 8] Graph showing recovery characteristics. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] In one example embodiment disclosed in the present specification, the method may further include, prior to the laser irradiation step, a buffer layer formation step of forming an n-type buffer layer (46) in the semiconductor substrate, in contact with the second cathode layer from the first surface side and having a lower n-type impurity than the second cathode layer.
[0010] In one exemplary embodiment disclosed in the present specification, the semiconductor device may include an insulated gate bipolar transistor adjacent to the diode. The insulated gate bipolar transistor may have a p-type collector layer (30) disposed in a range including the second surface in the semiconductor substrate and adjacent to the cathode layer. In the buffer layer forming step, the buffer layer may be formed so that the buffer layer is distributed across a range of the insulated gate bipolar transistor and a range of the diode.
[0011] In one example embodiment disclosed herein, the laser may be a green laser.
[0012] According to this configuration, even if the cathode layer is thin, a high density of crystal defects can be left in the cathode layer.
[0013] The semiconductor device 10 of the embodiment shown in Fig. 1 has a semiconductor substrate 12, an upper electrode 14, and a lower electrode 16. The semiconductor substrate 12 is made of silicon. The upper electrode 14 is provided on an upper surface 12a of the semiconductor substrate 12. The lower electrode 16 is provided on a lower surface 12b of the semiconductor substrate 12.
[0014] The semiconductor substrate 12 has an IGBT region 20 in which a vertical IGBT is provided, and a diode region 40 in which a vertical diode is provided. The upper electrode 14 serves both as an emitter electrode of the IGBT and an anode electrode of the diode. The lower electrode 16 serves both as a collector electrode of the IGBT and a cathode electrode of the diode.
[0015] A drift layer 44 is provided in the center in the thickness direction of the semiconductor substrate 12. The drift layer 44 is a low-concentration n-type layer. The drift layer 44 is distributed across the IGBT region 20 and the diode region 40.
[0016] A buffer layer 46 is provided below the drift layer 44. The buffer layer 46 is an n-type layer having a higher n-type impurity concentration than the drift layer 44. The buffer layer 46 is distributed across the IGBT region 20 and the diode region 40. The buffer layer 46 contacts the drift layer 44 from below in the IGBT region 20 and the diode region 40.
[0017] In the semiconductor substrate 12 in the IGBT region 20, an emitter layer 22, a body layer 24, and a collector layer 30 are provided.
[0018] The emitter layer 22 is a high-concentration n-type layer, and is disposed in a range exposed on the upper surface 12a of the semiconductor substrate 12. The emitter layer 22 is ohmically connected to the upper electrode .
[0019] The body layer 24 is a p-type layer and is in contact with the emitter layer 22. The body layer 24 is disposed in a range exposed on the upper surface 12a of the semiconductor substrate 12. The body layer 24 extends from the side of the emitter layer 22 to the lower side of the emitter layer 22. The body layer 24 has a body contact layer 24a and a low-concentration body layer 24b. The body contact layer 24a has a high p-type impurity concentration. The body contact layer 24a is disposed in a range exposed on the upper surface 12a of the semiconductor substrate 12, and is ohmic-connected to the upper electrode 14. The low-concentration body layer 24b has a p-type impurity concentration lower than that of the body contact layer 24a. The low-concentration body layer 24b is disposed below the emitter layer 22 and the body contact layer 24a. The low-concentration body layer 24b is in contact with the drift layer 44 from above.
[0020] The collector layer 30 is a high-concentration p-type layer, and is disposed below the buffer layer 46. The collector layer 30 is in contact with the buffer layer 46 from below. The collector layer 30 is separated from the body layer 24 by the drift layer 44 and the buffer layer 46. The collector layer 30 is disposed in an area exposed at the lower surface 12b of the semiconductor substrate 12. The collector layer 30 is ohmic-connected to the lower electrode 16.
[0021] A plurality of trenches are provided on the upper surface 12a of the semiconductor substrate 12 in the IGBT region 20. Each trench is disposed at a position adjacent to the emitter layer 22. Each trench extends to a depth that reaches the drift layer 44. The inner surface of each trench in the IGBT region 20 is covered with a gate insulating film 32. A gate electrode 34 is disposed in each trench. Each gate electrode 34 is insulated from the semiconductor substrate 12 by the gate insulating film 32. Each gate electrode 34 faces the emitter layer 22, the low-concentration body layer 24b, and the drift layer 44 via the gate insulating film 32. An interlayer insulating film 36 is provided on the upper portion of each gate electrode 34. Each gate electrode 34 is insulated from the upper electrode 14 by the interlayer insulating film 36.
[0022] An anode layer 42 and a cathode layer 48 are provided within the semiconductor substrate 12 in the diode region 40 .
[0023] The anode layer 42 is disposed in a range exposed on the upper surface 12a of the semiconductor substrate 12. The anode layer 42 includes an anode contact layer 42a and a low-concentration anode layer 42b. The anode contact layer 42a has a high p-type impurity concentration. The anode contact layer 42a is disposed in a range exposed on the upper surface 12a of the semiconductor substrate 12, and is ohmic-connected to the upper electrode 14. The low-concentration anode layer 42b has a lower p-type impurity concentration than the anode contact layer 42a. The low-concentration anode layer 42b is distributed on the lateral side and the lower side of the anode contact layer 42a. The low-concentration anode layer 42b is in contact with the drift layer 44 from above.
[0024] The cathode layer 48 is an n-type layer having a higher n-type impurity concentration than the buffer layer 46. The cathode layer 48 is disposed below the buffer layer 46. The cathode layer 48 is in contact with the buffer layer 46 from below. The cathode layer 48 is disposed in a range exposed on the lower surface 12b of the semiconductor substrate 12. The cathode layer 48 is ohmic-connected to the lower electrode 16.
[0025] A plurality of trenches are provided on the upper surface 12a of the semiconductor substrate 12 in the diode region 40. Each trench extends to a depth that reaches the drift layer 44. The inner surface of each trench in the diode region 40 is covered with an insulating film 52. A control electrode 54 is disposed in each trench. Each control electrode 54 is insulated from the semiconductor substrate 12 by the insulating film 52. Each control electrode 54 faces the anode layer 42 and the drift layer 44 via the insulating film 52. An interlayer insulating film 56 is disposed on the upper portion of each control electrode 54. Each control electrode 54 is insulated from the upper electrode 14 by the interlayer insulating film 56. Each control electrode 54 may be electrically connected to the gate electrode 34, or may have a different potential from that of the gate electrode 34.
[0026] FIG. 2 is an enlarged cross-sectional view of the cathode layer 48. The cathode layer 48 includes a first cathode layer 48a and a second cathode layer 48b. The second cathode layer 48b has a higher n-type impurity concentration than the buffer layer 46. The first cathode layer 48a has a higher n-type impurity concentration than the second cathode layer 48b. The first cathode layer 48a is disposed in a range exposed to the lower surface 12b of the semiconductor substrate 12. The first cathode layer 48a is ohmically connected to the lower electrode 16. The second cathode layer 48b is disposed between the first cathode layer 48a and the buffer layer 46. The second cathode layer 48b is in contact with the first cathode layer 48a from above and in contact with the buffer layer 46 from below. The collector layer 30 is adjacent to the cathode layer 48 on the lower surface 12b of the semiconductor substrate 12.
[0027] In the second cathode layer 48b, there is provided a high-density defect region 50 having a higher crystal defect density than the surrounding area. The crystal defects act as carrier recombination centers. Therefore, in the high-density defect region 50, the carrier lifetime is short.
[0028] Next, a description will be given of a method for manufacturing the semiconductor device 10. The semiconductor device 10 is manufactured from an unprocessed semiconductor substrate 12 shown in Fig. 3. The entire unprocessed semiconductor substrate 12 is composed of a drift layer 44.
[0029] First, an anode layer forming step is performed. In the anode layer forming step, as shown in FIG. 4, an anode layer 42 is formed in the semiconductor substrate 12 by ion implantation or epitaxial growth. Here, the body layer 24 is formed simultaneously with the anode layer 42. Next, as shown in FIG. 4, an emitter layer 22 is formed. Next, as shown in FIG. 5, a trench, a gate insulating film 32, a gate electrode 34, an interlayer insulating film 36, an insulating film 52, a control electrode 54, an interlayer insulating film 56, and an upper electrode 14 are formed in the semiconductor substrate 12.
[0030] Next, a buffer layer formation step is performed. In the buffer layer formation step, as shown in Fig. 5, a buffer layer 46 is formed so as to extend across the IGBT region 20 and the diode region 40. Here, the buffer layer 46 is formed by ion-implanting n-type impurities into the lower surface 12b of the semiconductor substrate 12. After the buffer layer 46 is formed, the buffer layer 46 is annealed to activate the n-type impurities in the buffer layer 46.
[0031] 5, a collector layer 30 is formed on the semiconductor substrate 12. Here, the collector layer 30 is formed by ion implanting p-type impurities into the lower surface 12b in the IGBT region 20. After the collector layer 30 is formed, the collector layer 30 is annealed to activate the p-type impurities in the collector layer 30.
[0032] Next, as shown in FIG. 6, the cathode layer 48 is formed by injecting n-type impurities into the lower surface 12b in the diode region 40. That is, a first cathode layer 48a and a second cathode layer 48b are formed. In the first cathode layer forming step, the n-type impurities are injected into the lower surface 12b with low energy and a high dose. Therefore, the first cathode layer 48a having a high n-type impurity concentration is formed in the surface layer portion including the lower surface 12b. In the second cathode layer forming step, the n-type impurities are injected into the lower surface 12b with higher energy than in the first cathode layer formation and with a lower dose than in the first cathode layer forming step. For example, the dose amount for the first cathode layer 48a is set to 7×10 14 cm -2 The dose for the second cathode layer 48b is set to 6×10 13 cm -2Therefore, the second cathode layer 48b having a lower n-type impurity concentration than the first cathode layer 48a is formed on the upper side of the first cathode layer 48a. The second cathode layer 48b is formed so as to have a higher n-type impurity concentration than the buffer layer 46. Either the first cathode layer forming step or the second cathode layer forming step may be performed first. Hereinafter, the thickness of the first cathode layer 48a (i.e., the distance from the lower surface 12b to the upper surface of the first cathode layer 48a) is referred to as thickness A. Hereinafter, the thickness of the entire cathode layer 48 (i.e., the combined thickness of the first cathode layer 48a and the second cathode layer 48b) is referred to as thickness B. The thickness B can also be said to be the distance from the lower surface 12b to the upper surface of the second cathode layer 48b. For example, the thickness A can be set to 0.2 μm, and the thickness B can be set to 1.0 μm. The hatched areas in FIG. 6 indicate high-density defect regions 50. In the ion implantation process, crystal defects are formed at a high density in the area where the ions are implanted. Therefore, immediately after the first cathode layer formation process and the second cathode layer formation process are performed, the high-density defect regions 50 are distributed throughout the first cathode layer 48a and the second cathode layer 48b. In the second cathode layer formation process, n-type impurities are ion-implanted at a lower density than in the first cathode layer process, so that crystal defects are formed at a lower density in the second cathode layer 48b than in the first cathode layer 48a. That is, the crystal defect density in the high-density defect region 50 in the second cathode layer 48b is lower than the crystal defect density in the high-density defect region 50 in the first cathode layer 48a.
[0033] Next, a laser irradiation process is performed. In the laser irradiation process, as shown in FIG. 7, the lower surface 12b is irradiated with a green laser 92. Here, by moving the spot of the green laser 92, the entire lower surface 12b within the diode region 40 is irradiated with the green laser 92. In the laser irradiation process, the entire lower surface 12b including the diode region 40 and the IGBT region 20 may be irradiated with the green laser 92. When the lower surface 12b is irradiated with the green laser 92, the surface layer portion near the lower surface 12b of the semiconductor substrate 12 is heated to a temperature of 950° C. or higher. Hereinafter, the range heated to a temperature of 950° C. or higher by the irradiation of the green laser 92 is referred to as a heating range 94. Also, hereinafter, the depth of the heating range 94 is referred to as a depth D. Since the wavelength of the green laser 92 is short, in the laser irradiation process, a very shallow range near the lower surface 12b is heated. For example, when the wavelength of the green laser 92 is 532 nm, the depth D of the heating range 94 can be controlled to 50 to 230 nm. Also, when using a laser with a shorter wavelength, the depth D of the heating range 94 can be made smaller. Here, the depth D is controlled so that the thicknesses A, B, and the depth D satisfy the relationship A < D < B.
[0034] When silicon is heated to 950 °C or higher, impurities inside the silicon are activated. Also, when silicon is heated to 950 °C or higher, crystal defects inside the silicon disappear, resulting in a decrease in the crystal defect density. Therefore, in the laser irradiation process, within the heating range 94, n-type impurities are activated and the high-density defect region 50 disappears. Since A < D is satisfied, the boundary surface between the first cathode layer 48a and the second cathode layer 48b is located within the heating range 94. Therefore, the entire first cathode layer 48a is included within the heating range 94. That is, throughout the entire first cathode layer 48a, n-type impurities are activated and the high-density defect region 50 disappears. Also, since D < B is satisfied, the upper end portion of the second cathode layer 48b (i.e., the boundary surface between the second cathode layer 48b and the buffer layer 46) is located above the heating range 94. Therefore, the lower portion of the second cathode layer 48b is included within the heating range 94, while the upper portion of the second cathode layer 48b is not included within the heating range 94. Therefore, the high-density defect region 50 disappears in the lower portion of the second cathode layer 48b, and the high-density defect region 50 remains in the upper portion of the second cathode layer 48b. In the present embodiment, since the depth D is slightly larger than the thickness A, the high-density defect region 50 remains in a region that is more than half of the thickness of the second cathode layer 48b.
[0035] Next, as shown in FIG. 1, a lower electrode 16 is formed over the entire lower surface 12b. The collector layer 30 and the first cathode layer 48a are ohmically connected to the lower electrode 16. Through the above steps, the semiconductor device 10 is completed.
[0036] Next, the operation of the diode in the diode region 40 will be described. When a potential higher than that of the lower electrode 16 is applied to the upper electrode 14, a forward voltage is applied to the pn junction at the interface between the anode layer 42 and the drift layer 44. Then, electrons flow from the lower electrode 16 to the drift layer 44 through the cathode layer 48 and the buffer layer 46. At the same time, holes flow from the anode layer 42 to the drift layer 44, and the resistance of the drift layer 44 decreases. Therefore, electrons can pass through the drift layer 44 with low loss. The electrons that have passed through the drift layer 44 flow to the upper electrode 14 through the anode layer 42. The flow of electrons from the lower electrode 16 to the upper electrode 14 in this way turns on the diode. As described above, the first cathode layer 48a has a high n-type impurity concentration and high crystallinity. Therefore, the contact resistance of the first cathode layer 48a to the lower electrode 16 is low. Therefore, the loss that occurs when the diode is on (so-called steady-state loss) is small.
[0037] As described above, when the diode is on, holes flow from the anode layer 42 into the drift layer 44. The holes that flow into the drift layer 44 flow to the lower electrode 16 via the buffer layer 46 and the cathode layer 48. Therefore, when the diode is on, holes are present in the drift layer 44, the buffer layer 46, and the cathode layer 48. If the potential of the lower electrode 16 is then increased to a potential higher than the potential of the upper electrode 14, the diode enters a recovery state, and the holes present in the drift layer 44, the buffer layer 46, and the cathode layer 48 are discharged to the upper electrode 14. As a result, a reverse current (so-called recovery current) temporarily flows through the diode.
[0038] FIG. 8 shows a comparison of the recovery characteristics of the diode of the embodiment and the diode of the comparative example. The diode of the comparative example differs from the diode of the embodiment in that it does not have a high-density defect region 50. In FIG. 8, voltage Vak is the voltage between the anode and cathode of the diode, and the higher cathode is shown as positive. Voltage Vak is common to both the embodiment and the comparative example. In FIG. 8, current I Findicates the current flowing through the diode. Positive values indicate forward current and negative values indicate reverse current.
[0039] In Figure 8, the current I F is negative, the recovery state is reached. In the recovery state, the closer the holes in the drift layer 44, the buffer layer 46, and the cathode layer 48 are to the upper electrode 14, the easier they are to be discharged to the upper electrode 14. Therefore, it takes time for the holes in the cathode layer 48 to be discharged to the upper electrode 14. In the diode of the comparative example, the recovery current flows until the holes in the cathode layer 48 are discharged to the upper electrode 14, so the recovery current is unlikely to decay. In contrast, in the diode of the embodiment, the crystal defects in the high-density defect region 50 function as recombination centers, so that many holes disappear in the second cathode layer 48b by recombination with electrons. Therefore, in the diode of the embodiment, the recovery current decays faster than in the diode of the comparative example. Therefore, the diode of the embodiment is unlikely to suffer from recovery loss.
[0040] As described above, the manufacturing method of this embodiment can form the first cathode layer 48a having a high n-type impurity concentration and high crystallinity, and can also form the second cathode layer 48b having the high-density defect region 50. Therefore, the steady loss and recovery loss of the diode can be reduced.
[0041] In addition, in the manufacturing method of this embodiment, the second cathode layer 48b is doped with n-type impurities at a lower density than the first cathode layer 48a, so that the crystal defect density in the second cathode layer 48b can be controlled independently of the n-type impurity concentration in the first cathode layer 48a. This prevents the crystal defect density in the second cathode layer 48b from becoming excessively high, and prevents the steady-state loss of the diode from becoming high.
[0042] Furthermore, in the manufacturing method of this embodiment, the first cathode layer 48a is annealed using a green laser with a short wavelength, so that it is possible to produce, within the thin cathode layer 48, a first cathode layer 48a that does not have high-density defect regions 50 and a second cathode layer 48b that does have high-density defect regions 50.
[0043] Moreover, in the manufacturing method of this embodiment, the first cathode layer 48a having no high-density defect region 50 and the second cathode layer 48b having high-density defect region 50 can be formed by the general process of ion implantation of n-type impurities and laser irradiation. Since a special process such as helium irradiation is not required, the semiconductor device can be manufactured at low cost.
[0044] In the above embodiment, a green laser is used in the laser irradiation process, but a laser having a shorter wavelength than the green laser or a laser having a longer wavelength than the green laser may be used instead of the green laser. However, when the thickness of the cathode layer 48 is thin, it is easier to leave the high-density defect region 50 in the cathode layer 48 by using a green laser or a laser having a shorter wavelength than the green laser.
[0045] In the above-mentioned embodiment, the manufacturing method of the semiconductor device having the diode and the IGBT has been described, but the technology disclosed in this specification may be applied when manufacturing a semiconductor device having a single diode or a semiconductor device having elements other than the diode and the IGBT. Also, the trench, the insulating film 52, the control electrode 54, and the interlayer insulating film 56 may not be provided in the diode region.
[0046] In the above embodiment, the upper surface 12a is an example of a first surface, and the lower surface 12b is an example of a second surface.
[0047] Although the embodiments have been described in detail above, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and changes to the specific examples exemplified above. The technical elements described in this specification or drawings exhibit technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. In addition, the technology exemplified in this specification or drawings achieves multiple objectives simultaneously, and achieving one of the objectives itself has technical utility. [Explanation of symbols]
[0048] 10: semiconductor device, 12: semiconductor substrate, 40: diode region, 42: anode layer, 44: drift layer, 46: buffer layer, 48: cathode layer, 48a: first cathode layer, 48b: second cathode layer, 50: high-density defect region, 92: green laser, 94: heating area
Claims
1. A method for manufacturing a semiconductor device having a diode including a p-type anode layer (42), an n-type cathode layer (48), and a drift layer (44) disposed between the anode layer and the cathode layer, comprising the steps of: providing a semiconductor substrate made of silicon, having a first surface (12a) and a second surface (12b) opposite to the first surface, and having the drift layer; an anode layer forming step of forming the anode layer in an area including the first surface in the semiconductor substrate; a cathode layer forming step of forming the cathode layer in a range including the second surface in the semiconductor substrate by implanting an n-type impurity into the second surface; a laser irradiation step of irradiating the second surface with a laser (92) after the cathode layer formation step is performed; having In the cathode layer forming step, a cathode layer is formed having an n-type first cathode layer (48a) distributed in a range including the second surface, and an n-type second cathode layer (48b) in contact with the first cathode layer from the first surface side and having a lower n-type impurity concentration than the first cathode layer; In the laser irradiation step, a heated area (94) of 950° C. or more is formed in a surface layer portion of the semiconductor substrate near the second surface, In the laser irradiation step, a boundary between the first cathode layer and the second cathode layer is located within the heating range, and an end portion of the second cathode layer on the first surface side is located closer to the first surface than the heating range. Manufacturing method.
2. 2. The manufacturing method according to claim 1, further comprising, prior to the laser irradiation step, a buffer layer formation step of forming an n-type buffer layer (46) in the semiconductor substrate, in contact with the second cathode layer from the first surface side and having a lower n-type impurity than the second cathode layer.
3. the semiconductor device includes an insulated gate bipolar transistor adjacent to the diode; the insulated gate bipolar transistor has a p-type collector layer (30) disposed in a range including the second surface in the semiconductor substrate and adjacent to the cathode layer; In the buffer layer forming step, the buffer layer is formed so as to be distributed across a range of the insulated gate bipolar transistor and a range of the diode. The method according to claim 2 .
4. The method according to any one of claims 1 to 3, wherein the laser is a green laser.
Citation Information
Patent Citations
Semiconductor device and manufacturing method thereof
JP2022136627A
Method for manufacturing semiconductor device
JP2023023918A
Semiconductor device and method for manufacturing same
WO2013069113A1
Semiconductor device manufacturing method