Thermal print head
The thermal print head design with a silicon substrate and controlled defect density in the convex portion addresses substrate-related defects, enhancing yield and performance by minimizing shape distortion during manufacturing.
Patent Information
- Application Number
- JP2023068378
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-19
- Publication Date
- 2024-10-31
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Defects in thermal print heads due to the substrate lead to reduced yield, necessitating an improvement in manufacturing processes.
A thermal print head design utilizing a silicon substrate with a convex portion, where the defect density within 200 μm from the apex is controlled to 0.02 pieces/μm², achieved through specific etching and material selection, including DZ-IG treated silicon wafers and low-temperature co-fired ceramic fillers, to minimize shape distortion during manufacturing.
The improved design enhances the yield of thermal print heads by reducing the likelihood of shape distortion in the convex portions, leading to better printing performance and reliability.
Smart Images

Figure 2024154531000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to thermal printheads. [Background technology]
[0002] Japanese Patent Application Laid-Open No. 2022-180152 (Patent Document 1) discloses a thermal printhead including a substrate having a convex portion. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2022-180152 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, defects due to the substrate may occur, and there is room for improvement in the yield of thermal printheads.
[0005] The present disclosure has been made in order to solve the above-mentioned problems, and an object of the present disclosure is to provide a thermal printhead that can improve yield. [Means for solving the problem]
[0006] The thermal printhead of the present disclosure includes a silicon substrate. The silicon substrate has a main surface. The silicon substrate has a protrusion on the main surface. The direction perpendicular to the main surface is defined as the z direction. The protrusion has an apex. The apex is the most distant point in the z direction from the main surface. In a cross section of the silicon substrate along the z direction, the defect density in a region of the silicon substrate within 200 μm in the z direction from the apex is 0.02 defects / μm 2 The following is the result. Effect of the Invention
[0007] According to the present disclosure, a thermal printhead capable of improving yield can be provided. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is a schematic cross-sectional view of a thermal printhead according to a first embodiment. [Diagram 2] FIG. 2 is a schematic plan view of the thermal printhead of the first embodiment. [Diagram 3] FIG. 3 is a schematic partial enlarged plan view of the thermal printhead according to the first embodiment. [Figure 4] FIG. 4 is a schematic enlarged partial cross-sectional view of the thermal printhead of the first embodiment. [Diagram 5] FIG. 5 is a schematic, partially enlarged cross-sectional view showing a step in the method of manufacturing the thermal printhead according to the first embodiment. [Figure 6] FIG. 6 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 5 in the method for manufacturing the thermal printhead according to the first embodiment. [Figure 7] FIG. 7 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 6 in the method for manufacturing the thermal printhead according to the first embodiment. [Figure 8] FIG. 8 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 7 in the method for manufacturing the thermal printhead according to the first embodiment. [Figure 9] FIG. 9 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 8 in the method for manufacturing the thermal printhead according to the first embodiment. [Figure 10] FIG. 10 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 9 in the method for manufacturing the thermal printhead according to the first embodiment. [Figure 11] FIG. 11 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 10 in the method for manufacturing the thermal printhead according to the first embodiment. [Figure 12]FIG. 12 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 11 in the method for manufacturing the thermal printhead according to the first embodiment. [Figure 13] FIG. 13 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 12 in the method of manufacturing the thermal printhead according to the first embodiment. [Figure 14] FIG. 14 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 13 in the method for manufacturing the thermal printhead according to the first embodiment. [Figure 15] FIG. 15 is a schematic partial enlarged cross-sectional view of a thermal printhead according to the second embodiment. [Figure 16] FIG. 16 is a schematic, partially enlarged cross-sectional view showing a step in a method of manufacturing the thermal printhead according to the second embodiment. [Figure 17] FIG. 17 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 16 in the method for manufacturing the thermal printhead according to the second embodiment. [Figure 18] FIG. 18 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 17 in the method for manufacturing the thermal printhead according to the second embodiment. [Figure 19] FIG. 19 is a schematic, partially enlarged cross-sectional view showing a step subsequent to the step shown in FIG. 18 in the method of manufacturing the thermal printhead according to the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The details of the embodiments of the present disclosure will be described with reference to the drawings. In the following drawings, the same or corresponding parts are given the same reference numerals, and the description thereof will not be repeated. At least some of the configurations of the embodiments described below may be arbitrarily combined.
[0010] (Embodiment 1) Fig. 1 is a schematic cross-sectional view of a thermal printhead according to a first embodiment. Fig. 2 is a schematic plan view of the thermal printhead according to the first embodiment. Fig. 3 is a schematic partial enlarged plan view of the thermal printhead according to the first embodiment. Fig. 4 is a schematic partial enlarged cross-sectional view of the thermal printhead according to the first embodiment.
[0011] The thermal printhead 1 is an electronic device that prints on a print medium 47 such as thermal paper by selectively generating heat in multiple heat generating portions 31 (see FIG. 3). The thermal printhead 1 mainly includes a silicon substrate 10, a metal layer 16, an insulating layer 15, a wiring layer 20, a resistor layer 30, a protective layer 33, a drive circuit 35, conductive wires 36 and 37, a connector 40, a sealing member 43, and a heat sink 49.
[0012] As shown in FIG. 4, the silicon substrate 10 has a main surface 11 and a back surface 12 opposite to the main surface 11. The main surface 11 and the back surface 12 each extend in the x direction and the y direction perpendicular to the x direction. The x direction is the longitudinal direction of the silicon substrate 10 and the main scanning direction of the thermal printhead 1. The y direction is the lateral direction of the silicon substrate 10 and the sub-scanning direction of the thermal printhead 1. The z direction is the thickness direction of the silicon substrate 10. The normal direction of the main surface 11 is the z direction perpendicular to the x and y directions. The main surface 11 faces the +z direction. The back surface 12 faces the -z direction.
[0013] As shown in FIG. 3 and FIG. 4, the silicon substrate 10 has a protrusion 14 on the main surface 11. The protrusion 14 is formed by wet etching with, for example, an aqueous solution of potassium hydroxide (KOH), as described below. The height h of the protrusion 14 is, for example, 175 μm. The height h of the protrusion 14 is, for example, 200 μm or less. The height h of the protrusion 14 may be 150 μm or less. The height h of the protrusion 14 may be 50 μm or more. In this specification, the height h of the protrusion 14 is the maximum height of the protrusion 14 from the main surface 11. In a plan view of the main surface 11, the longitudinal direction of the protrusion 14 is the x direction, and the lateral direction of the protrusion 14 is the y direction. The height h direction of the protrusion 14 is the z direction.
[0014] The protrusion 14 has a top surface 14s1 and a pair of inclined surfaces 14s2. The top surface 14s1 is the surface farthest from the main surface 11 in the z direction. The top surface 14s1 has a vertex 14p. The vertex 14p is the point farthest from the main surface 11 in the z direction. The top surface 14s1 may extend in the x direction and the y direction. The shape of the top surface 14s1 may be a curved surface. The pair of inclined surfaces 14s2 are disposed apart from each other in the y direction. The pair of inclined surfaces 14s2 connect the main surface 11 and the top surface 14s1. The pair of inclined surfaces 14s2 are inclined with respect to the main surface 11 so as to approach each other from the main surface 11 to the top surface 14s1. The inclination angle θ of each of the pair of inclined surfaces 14s2 with respect to the main surface 11 is, for example, 54.7°.
[0015] The silicon substrate 10 having the protrusion 14 includes single crystal silicon (Si). In the crystal structure of the silicon substrate 10, the plane orientation of the main surface 11 and the back surface 12 is a (100) plane. The plane orientation of the pair of inclined surfaces 14s2 is a (111) plane.
[0016] As shown in FIG. 4, the metal layer 16 is disposed on the main surface 11 of the silicon substrate 10. The metal layer 16 may cover only the protrusions 14, or may cover the entire protrusions 14 and the main surface 11 as shown in FIG. 4. The material constituting the metal layer 16 may be, for example, aluminum (Al), copper (Cu), or platinum (Pt). The thickness of the metal layer 16 in the z direction is, for example, 0.05 μm or more and 1.5 μm or less. The metal layer 16 is formed by using sputtering or a chemical vapor deposition (CVD) method.
[0017] 3 and 4, the insulating layer 15 is disposed on at least a part of the main surface 11 and the protrusions 14, and covers at least a part of the main surface 11 and the protrusions 14. The insulating layer 15 may cover the entire main surface 11. The material constituting the insulating layer 15 may be, for example, an oxide film (TEOS oxide film) formed using tetraethyl orthosilicate (TEOS). The silicon substrate 10 is electrically insulated from the resistor layer 30 and the wiring layer 20 by the insulating layer 15.
[0018] The insulating layer 15 can be formed by stacking thin films of silicon dioxide multiple times using a plasma CVD method. The silicon dioxide is formed using tetraethyl orthosilicate as a raw material gas. The thickness of the insulating layer 15 in the z direction is, for example, 1 μm or more and 15 μm or less.
[0019] The resistor layer 30 is formed on the insulating layer 15. The resistor layer 30 is connected to the insulating layer. The resistor layer 30 is formed of a material having a higher electrical resistivity than the wiring layer 20 described below. The material constituting the resistor layer 30 is, for example, tantalum nitride (TaN). The resistor layer 30 is formed by sputtering. The thickness of the resistor layer 30 in the z direction is, for example, not less than 0.02 μm and not more than 0.1 μm. The thickness of the resistor layer 30 in the z direction may be 50 nm.
[0020] As shown in FIGS. 2 to 4, the wiring layer 20 is connected to the resistor layer 30. The wiring layer 20 forms a conductive path for passing electricity to the multiple heat generating portions 31 of the resistor layer 30. The wiring layer 20 is electrically connected to the multiple heat generating portions 31. The wiring layer 20 may be made of a conductive material containing at least one of titanium (Ti) and copper (Cu), for example. When the material constituting the wiring layer 20 is titanium, the thickness of the wiring layer 20 in the z direction may be 150 nm. When the material constituting the wiring layer 20 is copper, the thickness of the wiring layer 20 in the z direction may be 800 nm.
[0021] The wiring layer 20 includes a common wiring 21, a plurality of individual wirings 25, and a plurality of lead-out wirings 29. The plurality of individual wirings 25 are separated from the common wiring 21 and the plurality of lead-out wirings 29. In order to selectively cause the plurality of heat generating portions 31 to generate heat, a current flows from the common wiring 21 toward the plurality of individual wirings 25 via the plurality of heat generating portions 31.
[0022] The common wiring 21 is electrically connected to the plurality of heat generating portions 31. Specifically, as shown in Figs. 3 and 4, the common wiring 21 includes a base 22 and a plurality of extension portions 23. In a plan view of the main surface 11, the base 22 is disposed on one side in the y direction (+y side) with respect to the resistor layer 30. The longitudinal direction of the base 22 is the x direction, and the lateral direction of the base 22 is the y direction. The base 22 is separated from the resistor layer 30 in the y direction. The plurality of extension portions 23 extend in the -y direction from the base 22 toward the resistor layer 30. The plurality of extension portions 23 are arranged at equal intervals along the x direction.
[0023] Each of the plurality of individual wirings 25 is electrically connected to a corresponding one of the plurality of heat generating portions 31. Specifically, as shown in Fig. 3 and Fig. 4, the plurality of individual wirings 25 are arranged along the x direction. Each of the plurality of individual wirings 25 includes a terminal portion 28 and an extension portion 26.
[0024] In a plan view of the main surface 11, the terminal portion 28 is disposed on the other side in the y direction (-y side) with respect to the resistor layer 30. The terminal portion 28 is disposed on the opposite side in the y direction to the base portion 22 of the common wiring 21 with respect to the resistor layer 30. As shown in Fig. 1 and Fig. 3, the conductive wire 36 is bonded to the terminal portion 28 and the drive circuit 35. The terminal portion 28 is electrically connected to the drive circuit 35 through the conductive wire 36.
[0025] The extension portion 26 is connected to the terminal portion 28. An end portion 27 of the extension portion 26 opposite the terminal portion 28 is in contact with the resistor layer 30. In a plan view of the main surface 11, the end portion 27 of the extension portion 26 overlaps the protrusion 14.
[0026] 2, in a plan view of the main surface 11, the multiple lead-out wirings 29 are arranged on the other side in the y direction (-y side) with respect to the drive circuit 35. In a plan view of the main surface 11, the multiple lead-out wirings 29 are arranged on the opposite side of the drive circuit 35 to the resistor layer 30 and the multiple individual wirings 25. A conductive wire 37 is bonded to the drive circuit 35 and the multiple lead-out wirings 29. The multiple lead-out wirings 29 are electrically connected to the drive circuit 35 through the conductive wire 37. The multiple lead-out wirings 29 are connected to a connector 40.
[0027] As shown in FIG. 4, the resistor layer 30 is connected onto the insulating layer 15. In the normal direction (z direction) of the main surface 11, the resistor layer 30 is disposed on the opposite side of the insulating layer 15 to the silicon substrate 10. In a plan view of the main surface 11, the longitudinal direction of the resistor layer 30 is the x direction, and the lateral direction of the resistor layer 30 is the y direction. In a plan view of the main surface 11, the resistor layer 30 intersects with the multiple extensions 23 of the common wiring 21 and the ends 27 of the extensions 26 of the multiple individual wirings 25. The resistor layer 30 straddles the multiple extensions 23 of the common wiring 21 and the ends 27 of the extensions 26 of the multiple individual wirings 25.
[0028] The resistor layer 30 includes a plurality of heat generating portions 31. A region of the resistor layer 30 sandwiched between a portion covered by any one of the extension portions 26 of the common wiring 21 and a portion covered by any one of the ends 27 of the individual wirings 25 adjacent to the portion in the x direction is one of the heat generating portions 31. The heat generating portions 31 are connected to the insulating layer 15. The heat generating portions 31 are arranged along the x direction. In a plan view of the main surface 11, the heat generating portions 31 overlap the protrusions 14. In a plan view of the main surface 11, the heat generating portions 31 are arranged inside the protrusions 14 in the short-side direction (y direction) of the resistor layer 30.
[0029] As shown in FIG. 4, the protective layer 33 covers the resistor layer 30, the wiring layer 20, and the plurality of heat generating parts 31. The protective layer 33 is connected to the resistor layer 30, the wiring layer 20, and the plurality of heat generating parts 31. The portions of the wiring layer 20 to which the conductive wires 36, 37 are bonded (e.g., the terminal parts 28, etc.) are exposed from the protective layer 33. The material constituting the protective layer 33 may be at least one of silicon dioxide, silicon nitride (SiN), and silicon carbide (SiC), for example. The protective layer 33 may be formed by a CVD method. The thickness of the protective layer 33 in the z direction may be, for example, 3.2 μm.
[0030] The driving circuit 35 is mounted on the main surface 11. For example, the driving circuit 35 is fixed to the insulating layer 15 using a bonding member (not shown) such as an adhesive. The driving circuit 35 may be mounted on a wiring board (not shown) separated from the silicon substrate 10. The wiring board is, for example, a printed circuit board (PCB). The driving circuit 35 is electrically connected to the wiring layer 20 (specifically, the plurality of individual wirings 25 and the plurality of lead wirings 29). The driving circuit 35 applies current to the plurality of heat generating portions 31 individually through the plurality of individual wirings 25. The heat generating portions 31 to which the current is applied selectively generate heat among the plurality of heat generating portions 31.
[0031] As shown in FIGS. 1 and 2, the connector 40 is disposed on the opposite side of the resistor layer 30 with respect to the driving circuit 35 in the y direction. The connector 40 is attached, for example, to an end of the silicon substrate 10 in the y direction. The connector 40 is electrically connected to the driving circuit 35 through the wiring layer 20 (specifically, a plurality of lead-out wirings 29). For example, the connector 40 includes a plurality of pins (not shown). Some of the plurality of pins are electrically connected to the plurality of lead-out wirings 29. Another portion of the plurality of pins is electrically connected to a wiring (not shown) that is electrically connected to the base 22 of the common wiring 21. The connector 40 is connected to a thermal printer. A constant voltage is applied from the thermal printer to the common wiring 21 through the connector 40.
[0032] 1 and 4, the sealing member 43 covers the drive circuit 35 and seals the drive circuit 35. The sealing member 43 further covers the conductive wires 36, 37 and further seals the conductive wires 36, 37. The sealing member 43 further covers the portions of the individual wirings 25 that are exposed from the protective layer 33 (e.g., the terminal portions 28, etc.). The sealing member 43 has electrical insulation properties. The sealing member 43 is formed of an insulating resin material such as epoxy resin.
[0033] As shown in FIG. 1, the heat sink 49 is disposed on the opposite side of the silicon substrate 10 to the insulating layer 15 and the resistor layer 30 in the z direction. The heat sink 49 is attached to the rear surface 12 of the silicon substrate 10 by a fastening member such as a screw or a joining member (not shown). The heat sink 49 supports the silicon substrate 10. The heat sink 49 is formed of a highly heat conductive material such as aluminum (Al). A part of the heat generated from the multiple heat generating parts 31 of the resistor layer 30 is transferred to the heat sink 49 through the silicon substrate 10. The heat transferred to the heat sink 49 is dissipated to the outside of the thermal printhead 1. The heat sink 49 can prevent an excessive temperature rise of the silicon substrate 10. When the drive circuit 35 is mounted on a wiring board separate from the silicon substrate 10, the heat sink 49 supports the silicon substrate 10 and the wiring board.
[0034] 1 and 4, the thermal printhead 1 includes a protrusion 45 formed on the principal surface 11. The protrusion 45 includes a convex portion 14, an insulating layer 15, a wiring layer 20, a plurality of heat generating portions 31, and a protective layer 33. In the protrusion 45, the protrusion 14, the metal layer 16, the insulating layer 15, the resistor layer 30, the wiring layer 20, the plurality of heat generating portions 31, and the protective layer 33 are laminated on the principal surface 11 in this order in the normal direction (z direction) of the principal surface 11.
[0035] The thermal printhead 1 according to the first embodiment is characterized in that the defect density in the cross section of the silicon substrate 10 is 0.02 / μm 2Specifically, the defect density in the region A1 of the silicon substrate 10 within 200 μm from the vertex 14p in the z direction is 0.02 / μm 2 The defect density is specified for the region A1 within 200 μm in the z direction from the apex 14p as described above because the height of the convex portion 14 is considered to be a maximum of approximately 200 μm. If the defect density in the region A1 is large, for example, when forming the convex portion 14, the shape of the convex portion 14 may become distorted. Specifically, the cross-sectional shape of the inclined surface 14s2 may no longer be linear, and may have an uneven shape. As a result, the printing performance of the thermal printhead 1 is degraded. If the defect density in the region A1 is 0.02 defects / μm 2 If it is equal to or less than this, it is possible to reduce the frequency with which the shape of the protrusions 14 becomes distorted when the protrusions 14 are formed, and as a result, the yield is improved in the manufacture of thermal printheads 1 having the protrusions.
[0036] The defect density in the region A1 should be as small as possible. The defect density in the region A1 is 0.004 / μm 2 It is sufficient that the defect density in the vicinity of the main surface 11 is small. Therefore, the defect density in the center of the silicon substrate 10 in the z direction may be high. The defect density in the center of the silicon substrate 10 in the z direction is 0.004 / μm 2 It may be more than that.
[0037] (Thermal printhead manufacturing method) A method for manufacturing the thermal printhead 1 of this embodiment will now be described.
[0038] First, a step (S1a) of preparing a silicon wafer 10a is performed. In this step (S1a), as shown in FIG. 5, a silicon wafer 10a is prepared as a silicon substrate, which is a semiconductor material. The silicon wafer 10a includes a single crystal of silicon. The thickness of the silicon wafer 10a in the z direction is, for example, 625 μm.
[0039] The silicon wafer 10a may be subjected to a DZ-IG (Denuded Zone-Intrinsic Gettering) process. The silicon wafer 10a subjected to the DZ-IG process has a higher defect density in the center of the silicon wafer 10a in the z direction than in the vicinity of the surface of the silicon wafer 10a. On the other hand, the defect density is extremely low on the front and back surfaces of the silicon wafer 10a subjected to the DZ-IG process. Therefore, the silicon wafer 10a subjected to the DZ-IG process is a suitable silicon wafer because it is less likely to cause shape defects when forming the convex portions 14 described later. By appropriately adjusting the conditions of the DZ-IG process, it is possible to prepare a silicon wafer 10a applicable to the thermal printhead 1 according to this embodiment, in which the defect density on the front and back surfaces is reduced.
[0040] The silicon wafer 10a is subjected to the DZ-IG treatment as follows. The silicon wafer 10a is annealed in an oxygen atmosphere using a lamp annealing device. Specifically, the silicon wafer 10a is annealed at a temperature of 1280°C for 0.2 hours. Then, a ramping heat treatment is performed at 550°C. Then, a precipitation heat treatment is performed at a temperature of 1000°C for 24 hours. In this manner, the silicon wafer 10a is subjected to the DZ-IG treatment. As a result, a defect-free region (DZ layer) is formed on the surface layer (near the main surface 11a and near the back surface 12a) of the silicon wafer 10a.
[0041] The silicon wafer 10a may be a silicon wafer manufactured using the Magnetic Field Applied Chochralski Method (MCZ). By using the MCZ method, it is possible to obtain the silicon wafer 10a with a reduced defect density.
[0042] The silicon wafer 10a may be a silicon wafer manufactured using a floating zone method (FZ). By using the FZ method, it is possible to obtain a silicon wafer 10a with a further reduced defect density.
[0043] The silicon wafer 10a may be a silicon wafer on which an epitaxial layer is formed. By forming an epitaxial layer on the silicon wafer 10a, it is possible to obtain a silicon wafer 10a with a further reduced defect density.
[0044] Next, a step (S2a) of forming a mask layer 2 is performed. In this step (S2a), as shown in Fig. 6, a mask layer 2 is formed in an area of the main surface 11a where the protrusions 14 are to be formed. The material constituting the mask layer 2 is, for example, silicon nitride (SiN) or silicon dioxide (SiO2). The mask layer 2 is formed by using a CVD method or sputtering.
[0045] Next, an etching step (S3a) is performed. In this step (S3a), as shown in FIG. 7, the silicon wafer 10a is wet-etched using the mask layer 2 as a mask. In a plan view seen from the z direction, the silicon wafer 10a in the region where the mask layer 2 is not arranged is etched in the -z direction. For example, a potassium hydroxide (KOH) aqueous solution is used as an etching solution to perform wet etching. The etching is anisotropic. The etching rate in the -z direction may be, for example, 45 μm / hour. At this time, the silicon wafer 10a may be etched by 175 μm in the -z direction. In this way, the silicon substrate 10 is formed. Moreover, the silicon wafer 10a is not etched in the region where the mask layer 2 is formed. Therefore, a protrusion 14 is formed on the main surface 11 of the silicon substrate 10.
[0046] When an alkaline aqueous solution such as a potassium hydroxide (KOH) solution is used as an etching solution, the etching rate of the (111) crystal plane of the silicon wafer 10a is faster than that of the other planes. The (111) plane is inclined at 57.5° with respect to the surface of the silicon wafer 10a. Therefore, the silicon wafer 10a is etched so that the inclination angle θ of the inclined plane 14s2 with respect to the main surface 11 becomes 54.7°. After the protrusion 14 shown in FIG. 7 is formed, the mask layer 2 is removed by wet etching using hydrofluoric acid (HF).
[0047] When the silicon wafer 10a contains defects, the etching rate in the area where the defects exist differs from the etching rate on the (111) plane. This may cause the shape of the protrusion 14 to become distorted. Specifically, the cross-sectional shape of the inclined surface 14s2 may no longer be linear, but may have an uneven shape. As a result, the wiring layer 20 formed on the uneven shape may have a defective shape. This may cause the printing performance of the thermal printhead 1 to deteriorate.
[0048] When the silicon substrate 10 is manufactured using the silicon wafer 10a that has been subjected to the DZ-IG process, the defect density on the main surface 11 and the back surface 12 of the silicon substrate 10 is extremely low. Specifically, the defect density in the region A1 of the silicon substrate 10 within 200 μm in the z direction from the apex 14p is 0.004 / μm 2 On the other hand, defects are concentrated in the center of the silicon substrate 10 in the z direction. Specifically, the defect density outside the region A1 is 0.004 / μm 2 The defect density in the center of the silicon substrate 10 in the z direction is 0.02 / μm 2 More than 0.004 particles / μm 2 It may be more than that.
[0049] When the silicon substrate 10 is manufactured using the silicon wafer 10a manufactured using the MCZ method, the defect density in the silicon substrate 10 is generally low. 2 The result is as follows.
[0050] When the silicon substrate 10 is manufactured using the silicon wafer 10a manufactured using the FZ method, the defect density in the silicon substrate 10 becomes extremely low overall. 2 The result is as follows.
[0051] When the silicon substrate 10 is manufactured using the silicon wafer 10a on which the epitaxial layer is formed, the defect density in the silicon substrate 10 is extremely low overall. 2 The result is as follows.
[0052] Next, a step (S4a) of forming a metal layer 16 is performed. In this step (S4a), as shown in FIG. 8, a metal layer 16 is formed to cover at least a part of the main surface 11 and the protrusions. Specifically, the metal layer 16 is formed by sputtering or CVD. The material constituting the metal layer 16 may be, for example, any one of aluminum (Al), copper (Cu), and platinum (Pt). The metal layer 16 may be patterned by etching. As a result, a part of the main surface 11 is exposed.
[0053] Next, a step (S5a) of forming insulating layer 15 is performed. In this step (S5a), as shown in Fig. 9, insulating layer 15 is formed to cover at least a part of main surface 11 and protrusions 14. Specifically, insulating layer 15 is formed by laminating thin films of silicon dioxide multiple times using a plasma CVD method. The silicon dioxide is formed using tetraethyl orthosilicate as a raw material gas.
[0054] Next, a step (S6a) of forming a resistor layer 30 is performed. In this step (S6a), as shown in FIG. 10, the resistor layer 30 is formed on the insulating layer 15. Specifically, the resistor layer 30 is formed by sputtering. The material constituting the resistor layer 30 is, for example, tantalum nitride (TaN). The resistor layer 30 includes a plurality of heat generating portions 31.
[0055] Next, a step (S7a) of forming the wiring layer 20 is performed. In this step (S7a), as shown in FIG. 11, the wiring layer 20 is formed on the resistor layer 30. Specifically, the wiring layer 20 is formed by sputtering. The wiring layer 20 may be formed, for example, by laminating a thin copper film multiple times using sputtering. The wiring layer 20 may be formed by laminating a thin titanium film on the resistor layer 30 using sputtering, and then laminating a thin copper film multiple times.
[0056] After forming the wiring layer 20, lithography patterning is performed to remove a part of the wiring layer 20. Specifically, a mask layer is formed on the wiring layer 20 by photolithography. The mask layer is used as a mask to partially remove the wiring layer 20 by etching. Wet etching can be used for the wiring layer 20. In the wet etching, a mixed solution of sulfuric acid (H2SO4) and hydrogen peroxide (H2O2) is used. As a result, as shown in FIG. 3, a common wiring 21 and a plurality of individual wirings 25 are formed on the resistor layer 30. As shown in FIG. 11, a part of the resistor layer 30 is exposed from the wiring layer 20. Next, reactive ion etching is used to etch a part of the resistor layer 30. As a result, the insulating layer 15 is exposed on the protrusion 14 as shown in FIG. 3. A plurality of heat generating parts 31 are exposed on the top surface 14s1 of the protrusion 14.
[0057] Next, a step (S8a) of forming protective layer 33 is performed. Specifically, as shown in FIG. 12, protective layer 33 is formed on insulating layer 15, on multiple heat generating portions 31, and on a portion of wiring layer 20 by using plasma CVD. Protective layer 33 is formed by laminating thin films of silicon nitride. Portions of wiring layer 20 to which conductive wires 36, 37 are bonded (e.g., terminal portion 28, etc.) are exposed from protective layer 33.
[0058] Next, a step (S9a) of mounting the drive circuit 35 is performed. In this step (S9a), the drive circuit 35 is mounted on the main surface 11 as shown in FIG. 13. For example, the drive circuit 35 is fixed to the insulating layer 15 using a bonding member (not shown) such as an adhesive. As shown in FIG. 13, the conductive wires 36, 37 are bonded. For example, the conductive wire 36 is bonded to the drive circuit 35 and the terminal portions 28 of the individual wirings 25 using a wire bonder (not shown). The conductive wire 37 is bonded to the drive circuit 35 and the lead-out wirings 29 using a wire bonder (not shown).
[0059] Next, a sealing step (S10a) is performed. In this step (S10a), as shown in Fig. 14, the driving circuit 35 is sealed with a sealing member 43. For example, a sealing resin material is potted on the driving circuit 35. Then, the sealing resin material is cured. In this manner, the sealing member 43 is formed.
[0060] Next, the connector 40 is attached to the silicon substrate 10. The connector 40 includes a plurality of pins (not shown). Some of the plurality of pins are electrically connected to the plurality of lead-out wirings 29. Another portion of the plurality of pins is electrically connected to a wiring (not shown) that is electrically connected to the base 22 of the common wiring 21.
[0061] Next, the heat sink 49 is attached to the silicon substrate 10. Specifically, the heat sink 49 is attached to the rear surface 12 of the silicon substrate 10 by a fastening member such as a screw or a joining member (not shown). In this manner, the thermal printhead 1 of the present embodiment shown in Figures 1 to 4 is obtained.
[0062] The operation of the thermal printhead 1 of this embodiment will now be described.
[0063] 1, the protrusion 45 faces a platen roller 46 included in the thermal printer. The platen roller 46 feeds the print medium 47 towards the thermal printhead 1. As the platen roller 46 rotates, the print medium 47 is fed in the +y direction. The print medium 47 is sandwiched between the protrusion 45 and the platen roller 46.
[0064] The drive circuit 35 applies current to the heat generating portions 31 individually through the individual wirings 25. The heat generating portions 31 to which the current is applied selectively generate heat. The heat generated in the heat generating portions 31 is transferred to the print medium 47. In this manner, printing is performed on the print medium 47 using the thermal printhead 1. A portion of the heat generated in the heat generating portions 31 is transferred to the insulating layer 15. The heat transferred to the insulating layer 15 is reflected by the metal layer 16. In other words, heat dissipation via the silicon substrate 10 can be suppressed. The remainder of the heat generated in the heat generating portions 31 is released to the outside of the thermal printhead 1 through the silicon substrate 10 and the heat sink 49.
[0065] <Action and effect> A thermal printhead 1 according to the present disclosure includes a silicon substrate 10. The silicon substrate 10 has a main surface 11. The silicon substrate 10 has a protrusion 14 on the main surface 11. The direction perpendicular to the main surface 11 is defined as the z direction. The protrusion 14 has an apex 14p. The apex 14p is the farthest point in the z direction from the main surface 11. In a cross section of the silicon substrate 10 taken along the z direction, a region A1 of the silicon substrate 10 within 200 μm in the z direction from the apex 14p has a defect density of 0.02 defects / μm 2 The following is the result.
[0066] In this way, it is possible to reduce the possibility that the shape of the protrusion 14 will be distorted when the protrusion 14 is formed by using wet etching. For example, by using any one of the silicon wafer 10a that has been subjected to the DZ-IG process, the silicon wafer 10a manufactured by the MCZ method, the silicon wafer 10a manufactured by the FZ method, and the silicon wafer 10a on which an epitaxial layer is formed, the defect density in the region A1 of the silicon substrate 10 within 200 μm from the apex 14p in the −z direction can be reduced to 0.02 defects / μm 2 In particular, by using the silicon wafer 10a manufactured by the MCZ method, the defect density in the region A1 is 0.02 / μm 2 In addition, by using the silicon wafer 10a that has been subjected to the DZ-IG process, the defect density in the region A1 is 0.004 / μm 2 In this way, it is possible to reduce the possibility that the shape of the protrusions 14 will be distorted when the silicon wafer 10a is wet-etched, and as a result, the yield in the manufacture of the thermal printheads 1 is improved.
[0067] In the cross section of the thermal printhead 1, the defect density in the area A1 is 0.004 / μm 2 In this way, it is possible to further reduce the possibility that the shape of the protrusions 14 will be distorted when the protrusions 14 are formed by wet etching. For example, by using a silicon wafer 10a that has been subjected to DZ-IG processing, a silicon wafer 10a manufactured by using the FZ method, or a silicon wafer 10a on which an epitaxial layer is formed, the defect density in the region A1 can be reduced to 0.004 defects / μm 2 Therefore, it is possible to further reduce the possibility that the shape of the protrusions 14 will be distorted when the silicon wafer 10a is wet-etched, and as a result, the yield in manufacturing the thermal printhead 1 is further improved.
[0068] In the cross section of the thermal printhead 1, the defect density in the center of the silicon substrate 10 in the z direction is 0.004 / μm 2The defect density in the region other than the region A1 is 0.004 / μm 2 Even in the above cases, when forming the convex portions 14 by wet etching, the defect density in regions other than region A1 does not significantly affect the shape of the convex portions 14. Therefore, if the defect density in region A1 satisfies the above condition, it is possible to reduce the possibility that the shape of the convex portions 14 will be distorted when the silicon wafer 10a is wet etched. For this reason, by using a silicon wafer 10a that has been subjected to DZ-IG processing and that satisfies the defect density condition in region A1, for example, the yield rate in the manufacture of the thermal printhead 1 is improved.
[0069] (Embodiment 2) Fig. 15 is a schematic partially enlarged cross-sectional view of a thermal printhead 1 according to a second embodiment. Fig. 15 corresponds to Fig. 4. The thermal printhead 1 shown in Fig. 15 basically has the same configuration as the thermal printhead 1 shown in Figs. 1 to 4, but differs in that the protrusions 14 are made of a filler. Specifically, the silicon substrate 10 has a recess 14r on the main surface 11. The cross-sectional shape of the recess 14r is, for example, V-shaped. The protrusions 14 are made of a filler that covers the recess 14r.
[0070] The recess 14r has a pair of side surfaces 14s3. The upper ends of the pair of side surfaces 14s3 are connected to the main surface 11. The lower ends of the pair of side surfaces 14s3 are connected to each other. The pair of side surfaces 14s3 are inclined with respect to the main surface 11 so as to approach each other as they move away from the main surface 11. The inclination angle of each of the pair of side surfaces 14s3 with respect to the main surface 11 is 54.7°.
[0071] The filler material is, for example, a low-temperature co-fired ceramic (LTCC ceramic), which is a ceramic material obtained by firing an LTCC slurry containing a ceramic powder, such as alumina, and a glass powder.
[0072] The defect density in the region A1 of the silicon substrate 10 within 200 μm from the vertex 14p in the z direction is 0.02 / μm 2 In this case, for example, when forming the recess 14r by wet etching, the possibility that the shape of the side surface 14s3 of the recess 14r will be distorted due to crystal defects can be reduced. In other words, based on the expected height of the protrusion 14 and the expected depth of the recess 14r, the bottom of the recess 14r is substantially located inside the region A1. Therefore, the recess 14r is formed in a region with a sufficiently low defect density, so that the possibility that the shape of the side surface 14s3 will be distorted as described above is extremely low. As a result, the yield rate is improved in the manufacture of the thermal printhead 1.
[0073] (Thermal printhead manufacturing method) A method for manufacturing the thermal printhead 1 of this embodiment will now be described.
[0074] A step (S1b) of preparing a silicon wafer 10a is performed. In this step (S1b), as shown in FIG. 16, a silicon wafer 10a, which is a semiconductor material, is prepared. The silicon wafer 10a includes a single crystal of silicon. The silicon wafer 10a is any one of a silicon wafer that has been subjected to a DZ-IG process, a silicon wafer manufactured using the MCZ method, a silicon wafer manufactured using the FZ method, and a silicon wafer on which an epitaxial layer is formed.
[0075] Next, a step (S2b) of forming a mask layer 2 is performed. In this step (S2b), as shown in FIG. 17, the mask layer 2 is formed on the main surface 11a in an area other than an area where the recess 14r (see FIG. 15) is to be formed. In other words, the mask layer 2 is not formed in an area where the recess 14r is to be formed. The material constituting the mask layer 2 is, for example, silicon nitride (SiN) or silicon dioxide (SiO2). The mask layer 2 is formed by using a CVD method or sputtering.
[0076] Next, an etching step (S3b) is performed. In this step (S3b), as shown in FIG. 18, the silicon wafer 10a is wet-etched using the mask layer 2 as a mask. In a plan view seen from the z direction, the silicon wafer 10a in an area where the mask layer 2 is not disposed is etched in the -z direction. In this way, a recess 14r having a V-shaped cross section is formed in a part of the main surface 11.
[0077] When an alkaline aqueous solution such as a potassium hydroxide (KOH) solution is used as an etching solution, the etching rate of the (111) crystal plane of the silicon wafer 10a is faster than that of the other planes. The (111) plane is inclined at 57.5° with respect to the surface of the silicon wafer 10a. Here, the plane orientation of the main surface 11 and the back surface 12 of the silicon wafer 10a is the (100) plane. Therefore, the silicon wafer 10a is etched so that the inclination angle of the side surface 14s3 with respect to the main surface 11 is 54.7°. After the recess 14r is formed, the mask layer 2 is removed by wet etching using hydrofluoric acid (HF).
[0078] Next, a step (S4b) of forming the protrusions 14 is carried out. In this step (S4b), as shown in FIG. 19, the protrusions 14 made of low-temperature co-fired ceramic (LTCC semilac) are formed. Specifically, an LTCC slurry is applied to the recesses 14r. The LTCC slurry contains LTCC semilac powder, glass, a binder, and a solvent. The LTCC slurry is fired to form the protrusions 14 made of LTCC. The firing temperature of the LTCC slurry is, for example, 870°C or higher and 900°C or lower.
[0079] After the step (S4b) of forming the protrusions 14, the steps (S4a) of forming the metal layer 16 to the step (S10a) of mounting the drive circuit 35 are carried out in sequence, as shown in Figures 9 to 14. In this manner, the thermal printhead 1 according to the second embodiment is manufactured.
[0080] <Action and effect> In the thermal printhead 1, the silicon substrate 10 has a recess 14r on the main surface 11. The protrusion 14 is formed by a filler that covers the recess 14r. In this way, the defect density in the region A1 of the silicon substrate 10 within 200 μm in the z direction from the apex 14p is reduced to 0.02 defects / μm. 2 If the thickness is equal to or less than this, it is possible to reduce the possibility that the shape of the side surface 14s3 of the recess 14r will be distorted when the recess 14r is formed by wet etching, and as a result, the yield in the manufacture of the thermal printhead 1 is improved.
[0081] (Method of measuring defect density) A method for measuring the defect density will now be described. Crystal defects are observed by performing an etching process using a Zirconium etchant on the cross section of the silicon substrate 10 shown in Fig. 4 or Fig. 15.
[0082] The target area for measuring the defect density is area A1 of the silicon substrate 10 within 200 μm in the z direction from the vertex 14p. In area A1, the defect density of five visual fields is measured. The defect density in each of the five visual fields is measured at a different position in area A1. The area observed as one visual field is an area of 50 μm × 50 μm. The defect density is the arithmetic average of the defect densities in the five visual fields. In the thermal printhead 1 according to the first or second embodiment, the arithmetic average of the defect densities in the five visual fields in area A1 is 0.02 defects / μm 2 The result is as follows.
[0083] Various aspects of the present disclosure are summarized below as appendices. (Appendix 1) a silicon substrate having a main surface; the silicon substrate has a protrusion on the main surface, If the direction perpendicular to the main surface is the z direction, the protrusion has an apex that is the farthest point from the main surface in the z direction, In a cross section of the silicon substrate along the z direction, The defect density in a region of the silicon substrate within 200 μm from the apex in the z direction is 0.02 / μm 2 The following is a thermal print head. (Appendix 2) In the cross section, The defect density in the region is 0.004 / μm 2 2. A thermal printhead as described in claim 1, wherein: (Appendix 3) In the cross section, The defect density in the center of the silicon substrate in the z direction is 0.004 / μm 2 The thermal printhead according to claim 2, (Appendix 4) the silicon substrate has a recess on the main surface, 4. The thermal printhead according to claim 1, wherein the convex portion is formed of a filler that covers the concave portion.
[0084] The first and second embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The basic scope of the present disclosure is indicated by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]
[0085] 1 thermal print head, 2 mask layer, 10 silicon substrate, 10a silicon wafer, 11,11a main surface, 12,12a back surface, 14 convex portion, 14s1 top surface, 14s2 inclined surface, 14s3 side surface, 14p apex, 14r concave portion, 15 insulating layer, 16 metal layer, 20 wiring layer, 21 common wiring, 22 base portion, 23,26 extension portion, 25 individual wiring, 27 end portion, 28 terminal portion, 29 lead wiring, 30 resistor layer, 31 heat generating portion, 33 protective layer, 35 drive circuit, 36,37 conductive wire, 40 connector, 43 sealing member, 45 protrusion, 46 platen roller, 47 printing medium, 49 heat sink, A1 area, h height.
Claims
1. a silicon substrate having a main surface; the silicon substrate has a protrusion on the main surface, If the direction perpendicular to the main surface is the z direction, The protrusion has an apex that is a point farthest from the main surface in the z direction, In a cross section of the silicon substrate along the z direction, The defect density in a region of the silicon substrate within 200 μm from the apex in the z direction is 0.02 / μm 2 The following is a thermal print head.
2. In the cross section, The defect density in the region is 0.004 / μm 2 2. The thermal printhead of claim 1, wherein:
3. In the cross section, The defect density in the center of the silicon substrate in the z direction is 0.004 / μm 2 3. The thermal printhead according to claim 2, wherein:
4. the silicon substrate has a recess on the main surface, 4. The thermal printhead according to claim 1, wherein the protrusions are formed by a filler that covers the recesses.
Citation Information
Patent Citations
Thermal print head and manufacturing method of the same
JP2022180152A