The cushion material addresses the lack of comfort and load distribution in existing materials by incorporating a fiber layer with convex portions between cushion layers, enhancing comfort and load distribution through body-conforming deformation.
Patent Information
- Application Number
- JP2023069081
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-20
- Publication Date
- 2024-10-31
AI Technical Summary
Existing cushioning materials lack high comfort and effective load distribution characteristics.
A cushion material comprising a first cushion layer made of porous polyurethane foam, a second cushion layer, and a fiber layer with convex portions, where the fiber layer is exposed between the cushion layers to enhance comfort and load distribution.
The cushion material provides high comfort and improved load distribution by utilizing a fiber layer with convex portions that deform to follow the body, increasing contact area and dispersing load effectively.
Smart Images

Figure 2024154876000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a cushioning material and bedding including the cushioning material. [Background technology]
[0002] Patent Document 1 discloses a cushioning material having a three-layer structure: an upper cushion layer, an intermediate cushion layer, and a lower cushion layer, all of which are made of urethane foam. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2016-214762 A Summary of the Invention [Problem to be solved by the invention]
[0004] An object of the present disclosure is to provide a cushioning material that is highly comfortable. [Means for solving the problem]
[0005] A cushioning material according to one embodiment of the present disclosure includes a first cushioning layer, a second cushioning layer, and The cushioning material further includes a fiber layer disposed between the first and second cushion layers. Effect of the Invention
[0006] The present disclosure provides a highly comfortable cushioning material. [Brief description of the drawings]
[0007] [Figure 1] FIG. [Diagram 2] Cross section AA of Figure 1. [Diagram 3]FIG. [Figure 4] 5A to 5C are diagrams showing a method for manufacturing the cushioning material. [Diagram 5] FIG. 2 is a diagram of a cushioning material according to another embodiment. [Figure 6] FIG. 1 is a diagram of a cushioning material according to another embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. In each drawing, mutually orthogonal X, Y and Z axes are shown for specifying directions.
[0009] As shown in Fig. 1, the cushion material 1 of this embodiment is used in a mattress, which is an example of bedding. The cushion material 1 is not limited to this, and may be used in pillows and other bedding. In this embodiment, the cushion material 1 may have dimensions corresponding to a bed. For example, the cushion material 1 may correspond to a general single-size bed and have a length of 1800 mm to 2250 mm (direction of arrow Y in Fig. 1) and a width of 850 mm to 1000 mm (direction of arrow X in Fig. 1).
[0010] The cushion material 1 has a support surface 1a that supports the body, and a back surface 1b opposite to the support surface 1a.
[0011] As shown in Fig. 2, the cushion material 1 of this embodiment includes a second cushion layer 3, a fiber layer 4 provided on the second cushion layer 3, and a first cushion layer 2 disposed on the fiber layer 4. The second cushion layer 3 has a flat base 3a and a protruding portion 3b located on the base 3a. The fiber layer 4 is bonded or welded to the second cushion layer 3 (more specifically, the protruding portion 3b). The first cushion layer 2 is bonded or welded to the fiber layer 4.
[0012] In this embodiment, the cushioning material 1 includes a plurality of regularly arranged protrusions 5. The protrusions 5 include the second cushion layer 3 (more specifically, the protrusions 3b), the fiber layer 4, and the first cushion layer 2.
[0013] The first cushion layer 2 is formed of a porous material. The porous material includes polyurethane foam, polyethylene foam, and other resin foams. The polyurethane foam may be a membrane-free urethane foam or a membrane-containing urethane foam, and more preferably, a membrane-free urethane foam is preferable. The membrane-free urethane foam provides high comfort, including high moisture absorption and release, good deodorization, high antibacterial properties, or other high-performance properties. In general, urethane foam contains many cells in the urethane skeleton. These many cells have membranes between adjacent cells. However, by adjusting the material of the urethane foam or its formulation, it is possible to form a skeleton structure in which many of the membranes are not present. Alternatively, it is possible to form a skeleton structure in which many of the membranes are not present by subjecting a molded urethane foam to physical or chemical treatment. In this embodiment, the membrane-free urethane foam refers to a urethane foam in which at least 50% of the membranes defining the cells are not present.
[0014] The first cushion layer 2 may also be made of recycled materials in which polyurethane foam pulverization is compressed with a binder (adhesive). Furthermore, the first cushion layer 2 may be made of materials other than polyurethane foam that are generally used in mattresses, such as feathers, cotton, and resin. In any case, the first cushion layer 2 may be made of any material as long as it is made of a material used in mattresses.
[0015] The first cushion layer 2 of the present embodiment has an apparent density of 12 kg / m according to JIS K 7222. 3 to 300 kg / m 3 The apparent density and hardness according to JIS K 6400-2 are approximately 30N to 500N. Note that the apparent density and hardness shown are values measured according to the measurement methods specified in JIS K7222 and JIS K6400-4, but when international standards or other standards are applied, they are converted appropriately based on the respective standards.
[0016] The first cushion layer 2 has a thickness of, for example, 5 mm or more and 200 mm or less.
[0017] The second cushion layer 3 is made of a porous material. The second cushion layer 3 may be made of the same material as the first cushion layer 2, or may be made of a different material.
[0018] The second cushion layer 3 has a thickness of, for example, 15 mm or more and 200 mm or less. The base portion 3a has a thickness of, for example, 5 mm or more and 295 mm or less.
[0019] The fiber layer 4 is formed of nonwoven fabric, woven fabric, or other fibers. The fibers may include cotton, hemp, wool, silk, polyester, polypropylene, aramid, vinylon, vinylidene, polyvinyl chloride, polyurethane, polychlor, polylactic acid, rayon, nylon, acrylic, and other natural or synthetic fibers. The fiber layer 4 includes a large number of fibers, and a large number of internal spaces are formed between adjacent fibers. The fiber layer 4 absorbs moisture in a high humidity environment and retains it in the internal space, and releases the moisture retained in the internal space in a low humidity environment. Furthermore, the fiber layer 4 provides high comfort, including high moisture absorption and release properties, good deodorizing properties, high antibacterial properties, and other highly functional properties. The fiber layer 4 of this embodiment has a basis weight of 10 g / m 2 ~3000g / m 2 It is.
[0020] The fiber layer 4 has a thickness of, for example, 0.01 mm or more and 10 mm or less.
[0021] The protrusion 5 includes a bottom 5a, a top 5b, and a side surface 5c extending between the bottom 5a and the top 5b. In this embodiment, the side surface 5c is an inclined curved surface. As shown in FIG. 3, in this embodiment, one protrusion 5 includes four bottoms 5a and one top 5b surrounded by the bottoms 5a. The side surfaces 5c extend in all directions from the one top 5b. Adjacent protrusions 5 are continuous at their respective bottoms 5a, and the side surfaces 5c (see FIG. 2) are gently connected to each other. Adjacent protrusions 5 form a space s (see FIG. 2) between them.
[0022] The fiber layer 4 is exposed from the side surface 5c of the protrusions 5 to the space s between adjacent protrusions 5. As shown in Fig. 2, the side surface 5c of the protrusions 5 is inclined obliquely. The inclined side surface 5c increases the area of the fiber layer 4 exposed to the space s compared to a vertical side surface, thereby providing high comfort.
[0023] Furthermore, the fiber layer 4, together with the first cushion layer 2 and the second cushion layer 3, forms the protrusions 5. When the protrusions 5 receive a load from the body, they deform to conform to the body, expanding the contact area with the body and dispersing the load received from the body. The ability of the protrusions 5 to conform to the body affects the load dispersion characteristics of the protrusions 5. In this embodiment, the fiber layer 4 is thinner and more flexible than the first cushion layer 2 and the second cushion layer 3, so it is less likely to adversely affect the ability of the protrusions 5 to conform to the body, and good load dispersion characteristics of the protrusions 5 can be achieved.
[0024] Next, a manufacturing method of the cushioning material 1 will be described with reference to Fig. 4. As shown in Fig. 4, the cushioning material 1 of this embodiment (see Fig. 1) is manufactured using a processing device 10 that performs profile processing. The processing device 10 for the cushioning material 1 includes a pair of drums 12 and a cutter 14.
[0025] The drum 12 has a cylindrical shape and rotates around a rotation axis C. The drum 12 has a peripheral surface 12a and a plurality of protrusions 12b. The protrusions 12b extend a predetermined length from the peripheral surface 12a. The plurality of protrusions 12b are regularly arranged on the peripheral surface 12a.
[0026] The pair of drums 12 are disposed at a predetermined distance from each other with their rotation axes C parallel to each other. These drums 12 are rotated in opposite directions at a constant speed by an actuator (not shown) (see arrow R in FIG. 4).
[0027] The cutter 14 is disposed in a sending direction (see arrow X in FIG. 4) with respect to the rotation direction of the pair of drums 12.
[0028] The manufacturing method of the cushion material 1 includes a bonding step, a profile processing step, and a cutting step.
[0029] In the bonding process, first, two sheets of urethane foam 18a, 18b formed in a sheet shape and nonwoven fabric 19 also in a sheet shape are prepared. In this embodiment, the two sheets of urethane foam 18a, 18b are formed to the same thickness. Next, nonwoven fabric 19 is placed between urethane foam 18a, 18b and bonded with an adhesive. In this way, substrate U is formed. Substrate U has a three-layer structure in which nonwoven fabric 19 is placed in the center in the thickness direction (arrow Z direction in FIG. 4).
[0030] Next, in the profile processing step, the processing device 10 is used to perform profile processing on the base material U. As shown in Fig. 4, the base material U is disposed between a pair of drums 12 of the processing device 10. When the pair of drums 12 rotate in the direction of arrow R about a rotation axis C, the base material U is compressed between the drums 12. At this time, the amount of compression of the base material U at the locations where the protrusions 12b of the drums 12 are disposed is greater than the other locations.
[0031] The base material U, compressed between the pair of drums 12, is pushed toward the cutter 14 as the drums 12 rotate. The cutter 14 cuts the base material U compressed by the drums 12 near the center. As a result, the base material U is processed into two urethane sheets that have been subjected to profile processing.
[0032] As the drum 12 rotates, the substrate U is cut by the cutter 14 in the process of restoring from the compressed state. As a result, the cut surface of the substrate U becomes a curved surface on which the convex portions 5 are repeatedly arranged according to the arrangement of the protrusions 12b of the drum 12. In this embodiment, the nonwoven fabric 19 is arranged in the center in the thickness direction of the substrate U. Therefore, the nonwoven fabric 19 is arranged halfway between the convex portions 5.
[0033] Furthermore, in the cutting process, the urethane sheet formed in the profile processing process is cut to a desired size, thereby forming the cushion material 1.
[0034] As described above, according to the present disclosure, a highly comfortable cushioning material can be provided.
[0035] <Other embodiments> Although the embodiments of the present disclosure have been described above, the present disclosure is not limited to the above embodiments, and various modifications are possible without departing from the spirit of the invention. In particular, the examples described in this specification can be arbitrarily combined as necessary.
[0036] In the above embodiment, as shown in Fig. 2, the side surface 5c of the protrusion 5 is formed by the first cushion layer 2, the fiber layer 4, and the second cushion layer 3. At the boundary between the first cushion layer 2 and the fiber layer 4, the inclination angle of the fiber layer 4 is the same as the inclination angle of the first cushion layer 2. Similarly, at the boundary between the fiber layer 4 and the second cushion layer 3, the inclination angle of the fiber layer 4 is the same as the inclination angle of the second cushion layer 3. The present disclosure is not limited thereto.
[0037] 5, the side surface 205c of the protrusion 205 is formed by the first cushion layer 202, the fiber layer 204, and the second cushion layer 203. At the boundary between the first cushion layer 202 and the fiber layer 204, the inclination angle θ1 of the fiber layer 204 is different from the inclination angle θ2 of the first cushion layer 202. At the boundary between the fiber layer 204 and the second cushion layer 203, the inclination angle θ1 of the fiber layer 204 is different from the inclination angle θ3 of the second cushion layer 203.
[0038] More specifically, on the side surface 205c, the inclination angle θ1 of the fiber layer 204 is smaller than the inclination angle θ2 of the first cushion layer 202 and the inclination angle θ3 of the second cushion layer 203. The fiber layer 204 is exposed to the space s at an angle closer to horizontal. Therefore, the area of the fiber layer 204 exposed to the space s is increased. As a result, the moisture absorption and release properties of the cushion material 201 can be increased.
[0039] In the above embodiment, the protrusion 5 has an inclined side surface 5c, but the present disclosure is not limited thereto. As in the cushion material 301 shown in FIG. 6, the protrusion 305 may have a vertical side surface 305c. Furthermore, the bottom 305a and the top 305b of the protrusion 305 may be flat. The cushion material 301 is preferably formed by contour processing. In the contour processing, the cushion material 301 may be formed by cutting out the protrusion 305 from a block material that has been formed in advance by sandwiching the fiber layer 304 therebetween.
[0040] In the above embodiment, the fiber layer 4, 204, 304 is disposed in the convex portion 5, 205, 305 of the cushion material 1, 201, 301, but is not limited thereto. The fiber layer 4, 204, 304 may be disposed in the base portion 3a instead of in the convex portion 5, 205, 305.
[0041] In the above embodiment, the protrusion 5 is a quadrangular pyramid as shown in Fig. 2 and Fig. 3, but the present disclosure is not limited thereto. The protrusion 5 may be a cone, a pyramid, or a combination thereof. The pyramid includes a triangular pyramid, a quadrangular pyramid, and other polygonal pyramids.
[0042] In the above-mentioned embodiment, the cushion material 1, 201, 301 has the convex portion 5, 205, 305, but is not limited to this.
[0043] In the above embodiment, the fiber layer 4, 204, 304 is exposed, but this is not limited to the above. The fiber layer 4, 204, 304 may be disposed inside the cushion material 1, 201, 301 and may not be exposed to the space around the cushion material 1, 201, 301.
[0044] In the above embodiment, the cushioning material 1, 201, 301 is formed by using profile processing and contour processing, but the present invention is not limited to this. The cushioning material 1, 201, 301 can be formed by a molding process in which finely crushed foam material is bonded with a binder and formed into a desired shape, a bonding process, foam molding in a mold, and various other processing methods. [Explanation of symbols]
[0045] 1,201,301: Cushioning material 2,202,301: First cushion layer 3,203,303: Second cushion layer 4,204,304 : Fiber layer 5,205,305 : Convex
Claims
1. A first cushion layer; A second cushion layer; A cushioning material including a fiber layer provided between the first cushion layer and the second cushion layer.
2. The cushioning material has a protrusion, The cushioning material according to claim 1 , wherein the protrusion includes the first cushion layer, the second cushion layer, and the fiber layer.
3. The cushioning material of claim 1 , wherein the fibrous layer is exposed.
4. The cushioning material according to claim 1 , wherein the fiber layer is formed of a nonwoven fabric.
5. Bedding comprising the cushioning material according to any one of claims 1 to 4.