Inspecting method for semiconductor device and manufacturing method for semiconductor device

The method addresses the issue of reduced current surge resistance in MOSFETs with built-in SBDs by measuring gate voltage differences at varying drain currents, effectively identifying and removing devices with stacking faults to enhance reliability.

JP2024154934AActive Publication Date: 2024-10-31MITSUBISHI ELECTRIC CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023069169
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-20
Publication Date
2024-10-31
Estimated Expiration
2043-04-20

AI Technical Summary

Technical Problem

MOSFETs with built-in SBDs experience reduced current surge resistance due to stacking faults caused by crystal polymorphism, leading to uneven body diode operation and increased risk of device destruction during current surges.

Method used

A method for testing semiconductor devices by measuring the difference in gate voltage at varying drain currents to identify MOSFETs with low I2t tolerance, utilizing the abnormality in drain current-gate voltage characteristics caused by stacking faults.

Benefits of technology

Enables effective detection and removal of MOSFETs with low I2t tolerance, improving the reliability and durability of semiconductor devices by screening out those with stacking faults that affect body diode operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154934000001_ABST
    Figure 2024154934000001_ABST
Patent Text Reader

Abstract

To provide a technique of detecting a SBD-incorporated MOSFET that has low current surge resistance.SOLUTION: An inspecting method for a semiconductor device regarding a technique disclosed herein includes measuring a first gate voltage applied to a gate electrode in accordance with a first drain current flowing from a drain electrode to a source electrode, measuring a second gate voltage applied to the gate electrode in accordance with a second drain current larger than the first drain current, and inspecting whether the difference between the first gate voltage and the second gate voltage is over a predetermined threshold.SELECTED DRAWING: Figure 10
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The technology disclosed in this specification relates to a technology for inspecting semiconductor devices. [Background technology]

[0002] 2. Description of the Related Art In power electronics devices, insulated gate semiconductor devices such as IGBTs (Insulated Gate Bipolar Transistors) or MOSFETs (Metal Oxide Semiconductor Field Effect Transistors) are widely used as switching elements for controlling power supply to loads such as motors.

[0003] On the other hand, MOSFETs or IGBTs using wide band gap semiconductors such as silicon carbide (SiC) are attracting attention as next-generation switching elements, and are expected to be applied to technical fields that handle high voltages of about 1 kV or more. In addition to SiC, other examples of the wide band gap semiconductors mentioned above include gallium nitride (GaN)-based materials and diamond.

[0004] SiC has many crystal polytypes. Crystal polytypes are based on differences in the atomic arrangement that makes up the crystal, and SiC crystals with different atomic arrangements exhibit different physical properties.

[0005] Generally, 4H-SiC is used in semiconductor devices for power control. However, SiC crystals cannot be composed of only one crystal system, and other crystal polytypes may be mixed in during crystal growth. This is called stacking faults.

[0006] A pn diode called a body diode exists parasitically between the drain and source of a power control MOSFET, and in addition to forward operation in which a positive voltage is applied to the drain terminal, it is also possible to operate in the reverse direction in which a positive voltage is applied to the source terminal. By using this body diode, it is possible to eliminate the freewheeling diode placed in parallel with the MOSFET, thereby reducing the number of circuit elements.

[0007] While a MOSFET is a unipolar element in which only electrons or holes flow, a pn diode is a unipolar element in which both flow simultaneously. It is known that when SiC operates in a unipolar manner, the stacking faults mentioned above expand due to the recombination energy of electron-hole pairs. Since stacking faults in 4H-SiC crystals behave as high resistance bodies, the expansion of crystal defects leads to an increase in the element resistance.

[0008] Therefore, when connecting a MOSFET and an SBD (Schottky barrier diode) in parallel, it is necessary to design the SBD so that the body diode of the MOSFET does not operate within the range of the applied current; in other words, so that the generated voltage does not reach the turn-on voltage of the body diode.

[0009] Therefore, SBD-integrated MOSFET technology has been developed, in which an SBD is integrated into a SiC-MOSFET and reverse current flows through the SBD instead of the body diode. Since the SBD is a unipolar element, stacking faults do not expand as they do in the body diode. Unlike normal SBDs, the integrated SBD shares a drift layer with the MOSFET. This makes the voltage applied to the SBD equal to the voltage applied to the body diode, so the turn-on voltage of the body diode in an SBD-integrated MOSFET is higher than the turn-on voltage of the body diode that is parasitic to a normal MOSFET. In other words, an SBD-integrated MOSFET can pass more SBD current than a normal MOSFET and SBD connected in parallel.

[0010] Although defects in semiconductor devices can be inspected by the method shown in Patent Document 1, defects in the drift layer may cause the SBD to behave differently from a normal SBD. For example, if a current surge occurs in the SBD (if a surge current flows), the SBD may heat up and be destroyed.

[0011] To increase the I2t tolerance, which is the resistance against current surges, a structure called JBS (Junction Barrier Schottky) is used, in which a pn diode is arranged in parallel with the SBD. The SBD in a JBS has a low turn-on voltage and high parasitic resistance, while the pn diode is designed to have a high turn-on voltage and low parasitic resistance. This allows the SBD to operate during normal operation, and the pn diode to operate when a large current flows to lower the generated voltage, preventing damage to the element. The difference in these characteristics becomes particularly noticeable at high temperatures, so the JBS has a higher resistance against current surges than a normal SBD. [Prior art documents] [Patent documents]

[0012] [Patent Document 1] JP 2016-23964 A Summary of the Invention [Problem to be solved by the invention]

[0013] In a MOSFET with an SBD, the body diode works in the same way as the pn diode in a JBS. That is, when a certain current surge is applied, the body diode operates, the generated voltage drops, and the SBD current switches to the body diode current.

[0014] However, the inventors found that the histogram of the body diode operating voltage of the SBD-integrated MOSFET has multiple peaks. The cause of this is the above-mentioned crystal polytype. It is considered that some defects have already reached the surface of the drift layer after epitaxial growth, and this high-resistance layer blocks the SBD portion, dissolving the parallel relationship between the body diode and the integrated SBD, lowering the operating voltage of the body diode. In particular, in the case of a module in which many SBD-integrated MOSFET chips are connected in parallel, current concentrates on the SBD-integrated MOSFET chip with a lower body diode operating voltage, causing it to be destroyed quickly, lowering the I2t tolerance of the entire module.

[0015] Generally, methods for inspecting defects in semiconductor devices are disclosed, for example, in Patent Document 1. However, there is no disclosure of an inspection method for the above-mentioned problem (i.e., crystal polytype) of a semiconductor device in which a MOSFET region and a diode region are both formed in an active region.

[0016] The technology disclosed in this specification has been made in consideration of the problems described above, and is a technology for detecting MOSFETs with built-in SBDs that have low resistance to current surges. [Means for solving the problem]

[0017] A method for inspecting a semiconductor device, which is a first aspect of the technology disclosed in the present specification, is a method for inspecting a semiconductor device including an SBD region and a MOSFET region, the SBD region and the MOSFET region being provided on a first main surface side of a semiconductor substrate made of silicon carbide, a drift layer of a first conductivity type being provided on the first main surface of the semiconductor substrate, the MOSFET region including a well region of a second conductivity type provided in a surface layer of the drift layer on the first main surface side, a source region of the first conductivity type provided in a surface layer of the well region, a gate insulating film provided in contact with the well region sandwiched between the source region and the drift layer, a gate electrode provided in contact with the gate insulating film, and an interlayer insulating film covering the gate electrode, a gate electrode connected to the first main surface side of the drift layer and covering the first main surface of the drift layer, and a drain electrode provided on a second main surface side of the semiconductor substrate which is a main surface opposite to the first main surface of the semiconductor substrate, and a method for inspecting the semiconductor device includes measuring a first gate voltage applied to the gate electrode corresponding to a first drain current flowing from the drain electrode to the source electrode, measuring a second gate voltage applied to the gate electrode corresponding to a second drain current having a value larger than the first drain current, and inspecting whether a difference between the first gate voltage and the second gate voltage exceeds a predetermined threshold value. Effect of the Invention

[0018] According to at least the first aspect of the technique disclosed in the present specification, a MOSFET with a built-in SBD having low withstand capability can be detected based on the difference between corresponding gate voltages at different drain current values.

[0019] Furthermore, objects, features, aspects and advantages associated with the technology disclosed in this specification will become more apparent from the detailed description set forth below and the accompanying drawings. [Brief description of the drawings]

[0020] [Figure 1] FIG. 1 is a plan view showing an example of a semiconductor device that is a SiC-MOSFET with an SBD as viewed from above. [Diagram 2] 2 is a plan view mainly showing a silicon carbide semiconductor portion in the structure shown in FIG. [Diagram 3] FIG. 2 is a cross-sectional view illustrating an example of a cross section of a striped unit cell region from a source electrode to a gate wiring in an outer periphery of the silicon carbide semiconductor device, as viewed in a direction perpendicular to the longitudinal direction of the unit cell region, as shown in FIG. [Figure 4] FIG. 11 is a plan view showing another example of the structure of a semiconductor device that is a SiC-MOSFET with an SBD. [Diagram 5] 2 is a cross-sectional view that diagrammatically illustrates an example of a cross section from a source electrode to a gate wiring in an outer periphery of the silicon carbide semiconductor device illustrated in FIG. 1. [Figure 6] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 7] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 8] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 9] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 10] FIG. 1 is a diagram illustrating an example of the relationship between the gate voltage and the drain current of a semiconductor device. [Figure 11] FIG. 1 is a diagram illustrating an example of the relationship between the drain voltage and the drain current of a semiconductor device. [Figure 12] FIG. 1 is a cross-sectional view showing a schematic example of the structure of a SiC-MOSFET with built-in SBD. [Figure 13] FIG. 1 is a plan view showing an example of a part of a semiconductor device that is a SiC-MOSFET with built-in SBD, as viewed from above. [Figure 14] 14 is an enlarged plan view of an active region of the semiconductor device which is the SBD-integrated SiC-MOSFET shown in FIG. 13. [Figure 15]15 is a cross-sectional view of the semiconductor device at a portion of the active region shown in FIG. 14 where a connection region is not formed. [Figure 16] 15 is a cross-sectional view of the semiconductor device at a location where a connection region is formed in the active region shown in FIG. 14. [Figure 17] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 18] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 19] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 20] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 21] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 22] 1 is a cross-sectional view illustrating a method for manufacturing a SiC-MOSFET with built-in SBD. [Figure 23] FIG. 13 is a diagram showing an example of the effect of stacking faults on a gate voltage. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0021] <First embodiment> A method for inspecting a semiconductor device and a method for manufacturing a semiconductor device according to this embodiment will be described.

[0022] First, an example of a silicon carbide semiconductor device incorporating an SBD that is the subject of the inspection method according to the present embodiment will be described.

[0023] In the following description, n and p indicate the conductivity type of the semiconductor. In this disclosure, the first conductivity type is described as n type and the second conductivity type is described as p type, but the first conductivity type may be p type and the second conductivity type may be n type. Also, n- indicates that the impurity concentration is lower than n, and n+ indicates that the impurity concentration is higher than n. Similarly, p- indicates that the impurity concentration is lower than p, and p+ indicates that the impurity concentration is higher than p.

[0024] Hereinafter, the embodiments will be described with reference to the accompanying drawings. Note that the drawings are shown in a schematic manner, and the size and positional relationship of images shown in different drawings are not necessarily described accurately and may be changed as appropriate. In the following description, similar components are illustrated with the same reference numerals, and their names and functions are also the same. Therefore, detailed description thereof may be omitted.

[0025] Fig. 1 is a plan view showing an example of a semiconductor device that is a SiC-MOSFET with an SBD as viewed from the top. In Fig. 1, a gate pad 81 is formed on a part of the top surface of the SiC-MOSFET with an SBD, and a source electrode 80 is formed adjacent to the gate pad 81. In addition, a gate wiring 82 is formed so as to extend from the gate pad 81. The gate wiring 82 is formed on the outer periphery of the silicon carbide semiconductor device, surrounding the source electrode 80 in a plan view.

[0026] <1. Planar type> <1-1. Stripe structure> Fig. 2 is a plan view showing mainly the silicon carbide semiconductor portion in the structure shown in Fig. 1. As shown in Fig. 2, the semiconductor device 100 has unit cell regions, each having a MOSFET region formed on either side of an SBD region, arranged in a stripe pattern, and is called a "stripe type."

[0027] 2, unit cell regions each including an n-type separation region 21 that corresponds approximately to an SBD region where an SBD is formed and a p-type well region 30 that corresponds approximately to a MOSFET region where a MOSFET is formed are repeatedly arranged in one direction in a plan view. Drift layer 20 and separation region 22, which will be described later, are also shown in FIG.

[0028] The region in which the SBD-integrated MOSFET is formed is called the active region, and the region formed on the periphery of the active region is called the termination region. The termination region includes a region in which gate pad 81 in which p-type well region 31 and the like are formed is formed.

[0029] Fig. 3 is a cross-sectional view showing a schematic example of a cross section of a striped unit cell region extending from source electrode 80 to gate wiring 82 at the outer periphery of the silicon carbide semiconductor device, as viewed in a direction perpendicular to the longitudinal direction of the unit cell region, shown in Fig. 1. As described above, an SBD region and a MOSFET region are formed in the unit cell region.

[0030] In FIG. 3, in a semiconductor device 100, a drift layer 20 made of n-type silicon carbide (SiC) is formed on the upper surface of a semiconductor substrate 10 made of n-type low-resistance silicon carbide.

[0031] Further, a well region 31 made of p-type silicon carbide is provided in the surface layer of the drift layer 20 located substantially corresponding to the region in which the gate wiring 82 shown in FIG. 1 is formed.

[0032] 1, a plurality of well regions 30 made of p-type silicon carbide and formed in a stripe pattern are provided in the surface layer of the drift layer 20. The respective well regions 30 formed in a stripe pattern may be connected to each other, or may be a plurality of separated well regions 30.

[0033] In the surface layer of each well region 30, a source region 40 made of n-type silicon carbide is formed at a position a predetermined distance inward from the outer periphery of well region 30.

[0034] In addition, a contact region 35 made of low-resistance p-type silicon carbide is formed in the surface layer of the well region 30. In addition, a separation region 21 made of the same n-type silicon carbide as the drift layer 20 is formed in the striped well region 30 so as to penetrate the well region 30. The separation region 21 is formed in a striped shape along the striped well region 30. The n-type impurity concentration of the separation region 21 may be the same as the n-type impurity concentration of the drift layer 20, or may be higher or lower than the n-type impurity concentration of the drift layer 20. The contact region 35 is formed in the surface layer of the well region 30, closer to the separation region 21 than the source region 40.

[0035] A striped Schottky electrode 71 that is Schottky-connected to the separation region 21 (drift layer 20) is formed on the upper surface of the separation region 21. Here, it is preferable that the Schottky electrode 71 is formed so as to include at least the corresponding separation region 21 in a plan view (in FIG. 3, a part of the Schottky electrode 71 is formed so as to cover the well region 30).

[0036] An ohmic electrode 70 is formed so as to cover a part of the upper surface of the contact region 35 and a part of the upper surface of the source region 40. The ohmic electrode 70, the Schottky electrode 71, and a source electrode 80 connected to the contact region 35 are formed on the upper surfaces thereof.

[0037] The well region 30 can easily transfer electrons and holes between the ohmic electrode 70 and the well region 30 via the low-resistance contact region 35 .

[0038] An n-type separation region 22 is formed in the region where the drift layer 20 is formed between adjacent well regions 30. The n-type impurity concentration of the separation region 22 may be the same as the n-type impurity concentration of the drift layer 20, or may be higher or lower than the n-type impurity concentration of the drift layer 20.

[0039] A gate insulating film 50 made of silicon oxide is formed on a part of the upper surfaces of adjacent well regions 30, on the upper surface of the separation region 22 located therebetween, and on a part of the upper surface of the source region 40 in each well region 30. In addition, a gate electrode 60 made of polycrystalline silicon is formed on at least a portion of the upper surface of the gate insulating film 50 that overlaps with the well region 30 (specifically, the well region 30 sandwiched between the source region 40 and the drift layer 20) in a plan view.

[0040] Here, the surface layer of the well region 30 that overlaps in plan view with the region in which the gate electrode 60 is formed and faces the region via the gate insulating film 50 is called a channel region.

[0041] A well region 31 is formed outside (terminal region) the outermost well region 30 of the semiconductor device 100. In addition, a separation region 23 of the same n-type as the drift layer 20 is formed between the well regions 30 and 31. The n-type impurity concentration of the separation region 23 may be the same as the n-type impurity concentration of the drift layer 20, or may be higher or lower than the n-type impurity concentration of the drift layer 20.

[0042] In addition, a gate insulating film 50 is formed on the upper surface of the well region 31, and a gate electrode 60 electrically connected to the gate electrode 60 formed on the upper surface of the well region 30 is formed on the upper part of the gate insulating film 50.

[0043] A silicon carbide conductive layer 45 made of silicon carbide, which has a lower resistance and a higher n-type impurity concentration than the drift layer 20, is formed in a portion of the surface layer of the well region 31. The silicon carbide conductive layer 45 has a lower sheet resistance than the well region 31, and forms a pn junction with the p-type well region 31. The silicon carbide conductive layer 45 is formed over a width of at least half the lateral width of the well region 31 formed to surround the active region in a plan view. Note that the portion where the silicon carbide conductive layer 45 is formed over a width of at least half the lateral width of the well region 31 does not need to be the entire longitudinal range of the well region 31, and may be only a portion of the longitudinal range.

[0044] Between the gate electrode 60 and the source electrode 80, an interlayer insulating film 55 made of silicon oxide is formed. Furthermore, the gate wiring 82 provided above the well region 31 and the gate electrode 60 are connected via a gate contact hole 95 formed in the interlayer insulating film 55. A p-type JTE (Junction Termination Extension) region 37 made of silicon carbide is formed on the outer periphery of the well region 31, i.e., on the opposite side to the well region 30. The p-type impurity concentration of the JTE region 37 is lower than the p-type impurity concentration of the well region 31. An FLR (Field Limiting Ring) may be formed instead of the JTE region 37. A combination of the JTE region 37 and the FLR may be formed.

[0045] A field insulating film 51 having a thickness thicker than that of the gate insulating film 50 or a gate insulating film 50 is formed on the upper surface of the well region 31 and the upper surface of the silicon carbide conductive layer 45. An opening, i.e., a termination region contact hole 91, is formed in a part of the gate insulating film 50 or the field insulating film 51 on the upper surface of the silicon carbide conductive layer 45, and the silicon carbide conductive layer 45 is ohmically connected to a source electrode 80 formed on its upper surface through the termination region contact hole 91, via a termination portion ohmic electrode 72.

[0046] Termination region contact hole 91 penetrates gate insulating film 50 (or field insulating film 51) and interlayer insulating film 55, and makes an ohmic connection between silicon carbide conductive layer 45 and source electrode 80, but does not connect silicon carbide conductive layer 45 and well region 31. In addition, silicon carbide conductive layer 45 has a width larger than the diameter of termination region contact hole 91. Here, well region 31 is not directly ohmic-connected to source electrode 80.

[0047] In the active region, the ohmic electrode 70, the Schottky electrode 71 and the upper surface of the contact region 35 are connected to the source electrode 80 via an active region contact hole 90 formed through the interlayer insulating film 55 and the gate insulating film 50.

[0048] On the other hand, a drain electrode 84 is formed on the lower surface of the semiconductor substrate 10.

[0049] When the plane orientation of the first main surface of the semiconductor substrate 10 is a (0001) plane having an off-angle in the <11-20> direction, the striped well region 30 may be formed along the <11-20> direction or along a direction perpendicular to the off-direction.

[0050] <1-2. Lattice structure> Fig. 4 is a plan view showing another example of the structure of a semiconductor device that is a SiC-MOSFET with an SBD. As shown in Fig. 4, the semiconductor device 101 has unit cell regions, in which MOSFET regions surrounding an SBD region are formed, repeatedly arranged vertically and horizontally in a plan view, and is called a "lattice type."

[0051] In FIG. 4, unit cell regions each including an n-type isolation region 21A roughly corresponding to an SBD region and a p-type well region 30A roughly corresponding to a MOSFET region are repeatedly arranged lengthwise and widthwise in a plan view.

[0052] The region in which the SBD-integrated MOSFET is formed is called the active region, and the region formed on the periphery of the active region is called the termination region. The termination region includes a region in which gate pad 81 in which p-type well region 31 and the like are formed is formed.

[0053] FIG. 5 is a cross-sectional view that diagrammatically illustrates an example of a cross section from source electrode 80 to gate wiring 82 in the outer periphery of the silicon carbide semiconductor device shown in FIG.

[0054] In FIG. 5, in a semiconductor device 101, a drift layer 20 made of n-type silicon carbide is formed on the upper surface of a semiconductor substrate 10 made of n-type low-resistance silicon carbide.

[0055] Further, a well region 31 made of p-type silicon carbide is provided in the surface layer of the drift layer 20 located substantially corresponding to the region in which the gate wiring 82 shown in FIG. 1 is formed.

[0056] In an active region below the formation region of source electrode 80 shown in FIG. 1, a plurality of well regions 30A made of p-type silicon carbide and formed in a lattice pattern are provided in the surface layer of drift layer 20.

[0057] A source region 40 made of n-type silicon carbide is formed in the surface layer of each well region 30A at a position a predetermined distance inward from the outer periphery of well region 30A.

[0058] A contact region 35 made of low-resistance p-type silicon carbide is formed in the surface layer of the well region 30A. A separation region 21A made of the same n-type silicon carbide as the drift layer 20 is formed in the well region 30A so as to penetrate the well region 30A. The n-type impurity concentration of the separation region 21A may be the same as the n-type impurity concentration of the drift layer 20, or may be higher or lower than the n-type impurity concentration of the drift layer 20. The contact region 35 is formed in the surface layer of the well region 30A, closer to the separation region 21A than the source region 40.

[0059] A Schottky electrode 71 that is Schottky-connected to the separating region 21A is formed on the upper surface of the separating region 21A. Here, it is preferable that the Schottky electrode 71 is formed so as to include at least the corresponding separating region 21A in a plan view (in FIG. 5, a part of the Schottky electrode 71 is formed so as to cover the well region 30A).

[0060] An ohmic electrode 70 is formed so as to cover a part of the upper surface of the contact region 35 and a part of the upper surface of the source region 40. The ohmic electrode 70, the Schottky electrode 71, and a source electrode 80 connected to the contact region 35 are formed on the upper surfaces thereof.

[0061] The well region 30A can easily transfer electrons and holes between the ohmic electrode 70 and the well region 30A via the low-resistance contact region 35.

[0062] In the region where the drift layer 20 is formed between the adjacent well regions 30A, an n-type separation region 22 is formed. The n-type impurity concentration of the separation region 22 may be the same as the n-type impurity concentration of the drift layer 20, or may be higher or lower than the n-type impurity concentration of the drift layer 20.

[0063] A gate insulating film 50 made of silicon oxide is formed on a part of the upper surface of adjacent well regions 30A, on the upper surface of the separation region 22 located therebetween, and on a part of the upper surface of the source region 40 in each well region 30A. In addition, a gate electrode 60 made of polycrystalline silicon is formed on at least a portion of the upper surface of the gate insulating film 50 that overlaps with the well region 30A in a plan view.

[0064] Here, the surface layer of the well region 30A that overlaps in plan view with the region in which the gate electrode 60 is formed and faces the region via the gate insulating film 50 is called a channel region.

[0065] A well region 31 is formed outside (at the termination region) of the outermost well region 30A of the semiconductor device 100. A separation region 23 of the same n-type as the drift layer 20 is formed between the well region 30A and the well region 31. The n-type impurity concentration of the separation region 23 may be the same as the n-type impurity concentration of the drift layer 20, or may be higher or lower than the n-type impurity concentration of the drift layer 20.

[0066] In addition, a gate insulating film 50 is also formed on the upper surface of the well region 31, and a gate electrode 60 is formed on the upper part of the gate insulating film 50, which is electrically connected to the gate electrode 60 formed on the upper surface of the well region 30A.

[0067] A silicon carbide conductive layer 45 made of silicon carbide, which has a lower resistance and a higher n-type impurity concentration than the drift layer 20, is formed in a portion of the surface layer of the well region 31. The silicon carbide conductive layer 45 has a lower sheet resistance than the well region 31, and forms a pn junction with the p-type well region 31. The silicon carbide conductive layer 45 is formed over a width of at least half the lateral width of the well region 31 formed to surround the active region in a plan view. Note that the portion where the silicon carbide conductive layer 45 is formed over a width of at least half the lateral width of the well region 31 does not need to be the entire longitudinal range of the well region 31, and may be only a portion of the longitudinal range.

[0068] An interlayer insulating film 55 made of silicon oxide is formed between the gate electrode 60 and the source electrode 80. The gate electrode 60 and the gate wiring 82 provided above the well region 31 are connected via a gate contact hole 95 formed in the interlayer insulating film 55. A p-type JTE region 37 made of silicon carbide is formed on the outer periphery of the well region 31, i.e., on the opposite side to the well region 30A. The p-type impurity concentration of the JTE region 37 is lower than the p-type impurity concentration of the well region 31. An FLR may be formed instead of the JTE region 37. A combination of the JTE region 37 and the FLR may be formed.

[0069] A field insulating film 51 having a thickness thicker than that of the gate insulating film 50 or a gate insulating film 50 is formed on the upper surface of the well region 31 and the upper surface of the silicon carbide conductive layer 45. An opening, i.e., a termination region contact hole 91, is formed in a part of the gate insulating film 50 or the field insulating film 51 on the upper surface of the silicon carbide conductive layer 45, and the silicon carbide conductive layer 45 is ohmically connected to a source electrode 80 formed on its upper surface through the termination region contact hole 91, via a termination portion ohmic electrode 72.

[0070] Termination region contact hole 91 penetrates gate insulating film 50 (or field insulating film 51) and interlayer insulating film 55, and makes an ohmic connection between silicon carbide conductive layer 45 and source electrode 80, but does not connect silicon carbide conductive layer 45 and well region 31. Silicon carbide conductive layer 45 has a width larger than the diameter of termination region contact hole 91. Here, well region 31 is not directly ohmic-connected to source electrode 80.

[0071] In the active region, the ohmic electrode 70, the Schottky electrode 71 and the upper surface of the contact region 35 are connected to the source electrode 80 via an active region contact hole 90 formed through the interlayer insulating film 55 and the gate insulating film 50.

[0072] On the other hand, a drain electrode 84 is formed on the lower surface of the semiconductor substrate 10.

[0073] <1-3. Supplementary explanation common to stripe type and grid type> Here, a high SBD areal density structure (such as a folded structure) may be formed in the region of the active region closest to the termination region, and a high termination SBD areal density structure (a region with many SBDs such as JBS) may also be formed in the region of the termination region closest to the active region.

[0074] In addition, a sense cell for sensing a current may be provided inside the active region. In addition, by making the n-type impurity concentration of the separation region 22 higher than the n-type impurity concentration of the drift layer 20, the on-resistance can be reduced.

[0075] <1-4. Manufacturing method of planar type (common to stripe type and lattice type)> Next, a method for manufacturing a planar type SiC-MOSFET with built-in SBD, which is a silicon carbide semiconductor device according to this embodiment, will be described with reference to Fig. 6 to Fig. 9. Fig. 6 to Fig. 9 are cross-sectional views for explaining the method for manufacturing a SiC-MOSFET with built-in SBD. Although symbols in a stripe type structure are used in Fig. 6 to Fig. 9, they can be similarly applied to a lattice type structure.

[0076] First, as shown in FIG. 6, a semiconductor substrate 10 made of n-type low-resistance silicon carbide having a first main surface oriented in a (0001) plane having an off-angle and a polytype of 4H is formed on the upper surface of the semiconductor substrate 10 by chemical vapor deposition (CVD). 15 cm -3 Greater than or equal to 1×10 17 cm -3 Drift layer 20 made of n-type silicon carbide having the following impurity concentration and a thickness of 5 μm or more and 50 μm or less is epitaxially grown.

[0077] Next, an implantation mask is formed on a part of the upper surface of the drift layer 20 using photoresist or the like. Then, p-type impurity Al (aluminum) is ion-implanted through the implantation mask. At this time, the depth of the Al ion implantation is set not to exceed the thickness of the drift layer 20, for example, to 0.5 μm or more and 3 μm or less. The impurity concentration of the ion-implanted Al is 1×10 17 cm -3 Greater than or equal to 1×10 19 cm -3 The impurity concentration is in the following range and is set to be higher than the impurity concentration of the drift layer 20. After that, the implantation mask is removed.

[0078] Through the above process, the region into which Al has been ion-implanted becomes well region 30 in the active region, and well region 31 in the termination region.

[0079] Next, an implantation mask is formed on the upper surface of the drift layer 20 in the termination region using photoresist or the like, and Al, which is a p-type impurity concentration, is ion-implanted. At this time, the depth of the Al ion implantation is set not to exceed the thickness of the drift layer 20, for example, to 0.5 μm or more and 3 μm or less. The impurity concentration of the implanted Al is 1×10 16 cm -3 Greater than or equal to 1×10 18 cm -3 The impurity concentration is in the following range, which is higher than the impurity concentration of the drift layer 20 and lower than the impurity concentration of the well region 30. After that, the implantation mask is removed.

[0080] Through the above process, the region into which Al is ion-implanted becomes the JTE region 37.

[0081] Similarly, a predetermined region is provided with an impurity concentration of 1×10 16 cm -3 Greater than or equal to 1×10 18 cm -3 The contact region 35 is formed by ion implantation of Al with an impurity concentration in the following range:

[0082] Next, an implantation mask is formed using photoresist or the like so as to open a predetermined location inside the well region 30 on the upper surface of the drift layer 20, and N (nitrogen) which is an n-type impurity is ion-implanted. The depth of N ion implantation is shallower than the thickness of the well region 30. The impurity concentration of N ion implanted is 1×10 18 cm -3 Greater than or equal to 1×10 21 cm -3 The range is as follows, and exceeds the p-type impurity concentration of the well region 30.

[0083] Through the above steps, the region that exhibits n-type among the regions into which N is implanted becomes the source region 40.

[0084] Similarly, an implantation mask is formed using photoresist or the like so as to open a predetermined location inside the well region 31 of the termination region, and N (nitrogen) which is an n-type impurity is ion-implanted. The ion implantation depth of N is shallower than the thickness of the well region 30. The impurity concentration of N to be ion-implanted is 1×10 18 cm -3 Greater than or equal to 1×10 21 cm -3 The range is as follows, and exceeds the p-type impurity concentration of the well region 30.

[0085] Through the above steps, the region that exhibits n-type among the regions into which N has been implanted becomes silicon carbide conductive layer 45. The thickness of silicon carbide conductive layer 45 only needs to be smaller than the thickness of well region 31.

[0086] Silicon carbide conductive layer 45 and source region 40 may be formed in the same process and with the same thickness and impurity concentration, or silicon carbide conductive layer 45 and source region 40 may be formed in different processes and with different thicknesses and different impurity concentrations.

[0087] Next, annealing is performed in a heat treatment device in an inert gas atmosphere such as argon (Ar) gas at a temperature of, for example, 1300°C or higher and 1900°C or lower for, for example, 30 seconds or higher and 1 hour or lower. This annealing electrically activates the implanted N and Al. The structure at the stage where the ion implantation is completed in this manner is shown in FIG. 6.

[0088] Next, as shown in FIG. 7, a CVD method, photolithography technique, or the like is used to form a field insulating film 51 made of silicon oxide and having a thickness larger than that of the gate insulating film 50, which has a thickness of, for example, 0.5 μm or more and 2 μm or less, on the upper surface of the semiconductor layer (including silicon carbide conductive layer 45, well region 31, JTE region 37, and drift layer 20) except for the active region (the region roughly corresponding to the region in which well region 30 is formed).

[0089] Next, the upper surface of the semiconductor layer (including the silicon carbide conductive layer 45, the well region 31, the drift layer 20, the well region 30, the contact region 35, and the source region 40) that is not covered with the field insulating film 51 is thermally oxidized to form a silicon oxide film which is a gate insulating film 50 of the desired thickness.

[0090] Next, a conductive polycrystalline silicon film is formed on the upper surface of the gate insulating film 50 and the upper surface of the field insulating film 51 by low pressure CVD, and the gate electrode 60 is formed by patterning this.

[0091] Next, an interlayer insulating film 55 made of silicon oxide and having a thickness larger than that of the gate insulating film 50 is formed by low-pressure CVD so as to cover the gate insulating film 50, the field insulating film 51, and the gate electrode 60. The structure at the stage where the steps up to this point are completed is shown in FIG.

[0092] 8, active region contact hole 90A is formed, penetrating interlayer insulating film 55 and gate insulating film 50 and reaching contact region 35 and source region 40 in the active region. Furthermore, termination region contact hole 91 is formed, penetrating interlayer insulating film 55 and gate insulating film 50 and reaching silicon carbide conductive layer 45 in the termination region.

[0093] The active region contact hole 90A is a region of the active region contact hole 90 excluding the portion where the Schottky electrode 71 is to be formed.

[0094] Next, a metal film mainly composed of Ni is formed by a sputtering method or the like, and then heat treatment is performed at a temperature of, for example, 600°C or more and 1100°C or less, to react the metal film mainly composed of Ni with the silicon carbide layer in the active region contact hole 90A to form a silicide between the silicon carbide layer and the metal film, and also to react the metal film mainly composed of Ni with the silicon carbide layer in the termination region contact hole 91 to form a silicide between the silicon carbide layer and the metal film.

[0095] Next, the remaining metal film other than the silicide formed as described above is removed by wet etching. In this manner, ohmic electrode 70 is formed in active region contact hole 90A, and termination ohmic electrode 72 is formed in termination region contact hole 91. The structure at the stage where the process up to this point is completed is shown in FIG.

[0096] Next, as shown in FIG. 9, a metal film mainly composed of Ni is formed on the lower surface (second main surface) of the semiconductor substrate 10, and then heat treatment is performed to form a back surface ohmic electrode (not shown here) on the lower surface of the semiconductor substrate 10.

[0097] Next, a resist mask 99 is formed, and the interlayer insulating film 55 and the gate insulating film 50 on the upper surface of the separation region 21 are removed. Also, a resist mask 99 is formed, and the interlayer insulating film 55 is removed from a position that will become the gate contact hole 95. The removal method is wet etching that does not damage the upper surface of the silicon carbide layer that will become the Schottky interface. The structure at the stage where the steps up to this point have been completed is shown in FIG.

[0098] Next, after removing the resist mask 99, a metal film to be a Schottky electrode is deposited by a method such as sputtering, and then patterned with a photoresist or the like to form a Schottky electrode 71 on the upper surface of the separation region 21 in the active region contact hole 90. The material for the Schottky electrode 71 may be Ti, Mo, or the like.

[0099] Next, a wiring metal such as Al is formed by sputtering or vapor deposition on the upper surface of drift layer 20 that has been processed up to this point (including well region 30, well region 31, contact region 35, source region 40, silicon carbide conductive layer 45, JTE region 37, and interlayer insulating film 55 that have been formed), and the wiring metal is processed into a predetermined shape by photolithography technology to form ohmic electrode 70, termination ohmic electrode 72, and source electrode 80 in contact with Schottky electrode 71. In addition, a gate pad 81 and gate wiring 82 in contact with gate electrode 60 are formed by processing the wiring metal into a predetermined shape.

[0100] In this manner, the semiconductor device according to this embodiment having the structure shown in FIG. 5 can be manufactured.

[0101] <1-5. Operation Description> Next, the operation of the SBD-integrated SiC-MOSFET, which is the semiconductor device according to the present embodiment, will be described. In the following, a semiconductor device whose semiconductor material is 4H-type silicon carbide will be described as an example. In this case, the built-in potential of the pn junction is approximately 2V.

[0102] The operation of the SBD-integrated MOSFET, which is the semiconductor device according to this embodiment, will be briefly described below in three states.

[0103] The first state is when a voltage higher than that applied to the source electrode 80 is applied to the drain electrode 84 and a positive voltage equal to or greater than the threshold is applied to the gate electrode 60, and is hereinafter referred to as the "on state."

[0104] In this on state, an inversion channel is formed in the channel region, and a path is formed through which electrons, which are carriers, flow between n-type source region 40 and n-type separation region 22. On the other hand, no current flows through the Schottky junction formed at the contact portion between separation region 21 and Schottky electrode 71 because an electric field (reverse bias) is applied in a direction that makes it difficult for a current to flow through the Schottky junction, that is, in the reverse direction.

[0105] Electrons flowing from the source electrode 80 to the drain electrode 84 reach the drain electrode 84 from the source electrode 80 through the ohmic electrode 70, the source region 40, the channel region, the separation region 22, the drift layer 20, and the semiconductor substrate 10 in accordance with the electric field formed by the positive voltage applied to the drain electrode 84. Therefore, by applying a positive voltage to the gate electrode 60, an on-current flows from the drain electrode 84 to the source electrode 80.

[0106] The voltage applied between the source electrode 80 and the drain electrode 84 at this time is called the on-voltage, and the value obtained by dividing the on-voltage by the density of the on-current is called the on-resistance. The on-resistance is equal to the total resistance of the above-mentioned paths through which electrons flow. The product of the on-resistance and the square of the on-current is equal to the current loss consumed by the MOSFET when it is conducting, so a low on-resistance is preferable.

[0107] The second state is where a higher voltage is applied to the drain electrode 84 than to the source electrode 80, and a voltage below the threshold is applied to the gate electrode 60, and is hereinafter referred to as the "off state."

[0108] In this off state, since there are no inversion carriers in the channel region, no on current flows, and the high voltage that was applied to the load in the on state is applied between source electrode 80 and drain electrode 84 of the MOSFET. Also, since an electric field in the same direction as in the "on state" is applied to the Schottky junction formed at the contact portion between separation region 21 and Schottky electrode 71, ideally no current flows; however, since an electric field much higher than in the "on state" is applied, a leakage current may occur.

[0109] A large leakage current increases the heat generated by the MOSFET, which can cause thermal destruction of the MOSFET and the module in which it is used. Therefore, in order to reduce the leakage current, it is preferable to keep the electric field applied to the Schottky junction low.

[0110] In the third state, a voltage lower than that applied to the source electrode 80 is applied to the drain electrode 84, i.e., a back electromotive voltage is applied to the MOSFET, and a reflux current flows from the source electrode 80 to the drain electrode 84. Hereinafter, this state will be referred to as the "reflux state."

[0111] In this freewheeling state, a forward electric field (forward bias) is applied to the Schottky junction formed at the contact between separation region 21 and Schottky electrode 71, and a unipolar current consisting of an electron current flows from Schottky electrode 71 to n-type separation region 21. At this time, the freewheeling current component of the freewheeling diode is mainly this unipolar component. Note that source electrode 80 and well region 30 are at the same potential via ohmic electrode 70.

[0112] As a result, a forward bias is also applied to the pn junction between the p-type well region 30 and the drift layer 20. However, since the pn junction is formed in parallel with the Schottky junction, when going from the off state to the reflux state, the Schottky junction, which has a lower threshold voltage, turns on before the pn junction. As a result, the reflux current flows almost entirely through the Schottky junction, and not through the pn junction.

[0113] In this way, by incorporating an SBD, it is possible to prevent a forward current, which is a bipolar current, from flowing through the pn junction even in a reflux state.

[0114] When a bipolar current flows through a pn junction, and a basal plane dislocation or other origin exists at such a location, stacking faults may expand and the breakdown voltage of the transistor may decrease. Specifically, leakage current occurs when the transistor is in the off state, and the element or circuit may be destroyed by heat generated by the leakage current.

[0115] However, by incorporating an SBD as described above, it is possible to prevent a bipolar current from flowing through the pn junction during reflux, thereby improving the reliability of the semiconductor device.

[0116] <1-6. Other structures> In the above, an example has been described in which a unit cell in which an SBD and a MOSFET are integrated is provided in the active region. However, the SBD and the MOSFET may be arranged in parallel in a unit cell formed in the active region.

[0117] Furthermore, the unit cell in the active region may have an n-type channel epitaxial layer 28 formed on the upper surface of the p-type well region 30. Specifically, the n-type channel epitaxial layer 28 may be formed in a portion overlapping with the gate insulating film 50 in a plan view. Fig. 12 is a cross-sectional view showing a schematic example of the structure of a SiC-MOSFET with an SBD.

[0118] As shown in an example in FIG. 12, a MOSFET may be designed such that the channel epitaxial layer 28 operates as a unipolar diode when a gate voltage less than the threshold voltage is applied, and the turn-on voltage of this unipolar diode is lower than the operating voltage of a pn diode formed by a p-type well region 30 and an n-type drift layer 20.

[0119] In this way, even in the case of a MOSFET that causes reverse current to flow through its channel region during freewheeling operation, it is possible to obtain the same effects as in the case of a MOSFET with an SBD.

[0120] <2. Trench type> <2-1. Trench type structure> Fig. 13 is a plan view showing an example of a part of a semiconductor device that is a SiC-MOSFET with built-in SBD, as viewed from the top. As shown in Fig. 13, in an active region of a semiconductor device 102, stripe-shaped gate trenches GT in which transistors are formed and stripe-shaped Schottky trenches ST in which Schottky electrodes are embedded are arranged in parallel to each other and alternately.

[0121] Furthermore, a well region 31 is formed in a termination region provided around the active region.

[0122] FIG. 14 is an enlarged plan view of an active region of the semiconductor device which is the SBD-embedded SiC-MOSFET shown in FIG.

[0123] As shown in the example of Fig. 14, on one side surface of the gate trench GT, connection regions 36 made of p-type silicon carbide are formed at regular intervals. On the other side surface of the gate trench GT, connection regions 38 made of p-type silicon carbide are formed at regular intervals. Similarly, on one side surface of the Schottky trench ST, connection regions 36 made of p-type silicon carbide are formed at regular intervals. On the other side surface of the Schottky trench ST, connection regions 38 made of p-type silicon carbide are formed at regular intervals.

[0124] The termination region of the semiconductor device 102 may be formed in the same manner as a planar type SBD-integrated MOSFET, or may have a different structure to match the trench type. Here, the active region portion of the semiconductor device 102, which is a trench type SBD-integrated SiC-MOSFET, will be described.

[0125] Fig. 15 is a cross-sectional view of the semiconductor device 102 at a portion of the active region shown in Fig. 14 where the connection region 36 and the connection region 38 are not formed. On the other hand, Fig. 16 is a cross-sectional view of the semiconductor device 102 at a portion of the active region shown in Fig. 14 where the connection region 36 and the connection region 38 are formed.

[0126] As shown in FIGS. 14, 15 and 16, in a semiconductor device 102, a drift layer 20 made of n-type silicon carbide is formed on the upper surface of a semiconductor substrate 10 made of n-type low-resistance silicon carbide.

[0127] In addition, in a surface layer portion of the drift layer 20, a well region 30B made of p-type silicon carbide is formed.

[0128] A source region 40B made of n-type silicon carbide is formed in a part of the surface layer of the well region 30B. A low-resistance p-type contact region 35B is formed in a part of the surface layer of the well region 30B adjacent to the source region 40B.

[0129] Furthermore, in the active region, a gate trench GT is formed which penetrates the source region 40B and the well region 30B to reach the drift layer 20. Furthermore, in a location of the active region different from the location where the gate trench GT is formed, a Schottky trench ST is formed which penetrates the source region 40B and the well region 30B to reach the drift layer 20.

[0130] The gate trenches GT and the Schottky trenches ST are arranged alternately and parallel to each other. In Fig. 15 and Fig. 16, the gate trenches GT and the Schottky trenches ST are formed to the same depth, but the depths of the two may be different. In addition, the gate trenches GT and the Schottky trenches ST may be formed to the same width, or the widths of the two may be different.

[0131] A gate electrode 60B is formed in the gate trench GT via a gate insulating film 50B made of silicon oxide. The gate insulating film 50B is provided in contact with a side surface of the well region 30B sandwiched between the source region 40B and the drift layer 20. The gate electrode 60B is made of low-resistance polycrystalline silicon with a high impurity concentration. An interlayer insulating film 55B made of silicon oxide is formed on the upper surface of the gate electrode 60B.

[0132] A Schottky electrode 71B and a source electrode 80 are formed in the Schottky trench ST. The Schottky electrode 71B is formed in contact with the drift layer 20 and is connected to the drift layer 20 via a Schottky connection.

[0133] A p-type protection region 32 is formed on the drift layer 20 side of the lower surface of the gate trench GT. A p-type protection region 33 is formed on the drift layer 20 side of the lower surface of the Schottky trench ST. The protection region 32 and the protection region 33 have the same depth and the same impurity concentration.

[0134] 14 and 16, the protection region 32 and the well region 30B are connected by a p-type connection region 36. Also, in Figures 14 and 16, the protection region 33 and the well region 30B are connected by a p-type connection region 38.

[0135] An ohmic electrode 70 is formed across the upper surfaces of source regions 40B and 35B. In addition, a source electrode 80 connected to the ohmic electrode 70, Schottky electrode 71B, and contact region 35B is formed to cover these.

[0136] The well region 30B can easily transfer electrons and holes between the ohmic electrode 70 and the well region 30B via the low-resistance contact region 35B.

[0137] The source electrode 80 is also connected to the Schottky electrode 71B in the Schottky trench ST.

[0138] A region of the well region 30B facing the gate electrode 60B via the gate insulating film 50B on the side surface of the gate trench GT in which the gate electrode 60B is formed is called a channel region.

[0139] Furthermore, a Schottky diode is formed on the side surface of the Schottky trench ST at a location where the Schottky electrode 71B and the drift layer 20 are in contact with each other.

[0140] On the other hand, a drain electrode 84 is formed on the lower surface of the semiconductor substrate 10.

[0141] The well region 31 in the termination region may be formed to the same depth as the well region 30B in the active region, or may be formed to the same depth as the protection region 32 and the protection region 33 in the active region, that is, to the depth of the bottoms of the gate trench GT and the Schottky trench ST. A low-resistance n-type silicon carbide conductive layer 45 may be formed in a surface layer portion of the well region 31.

[0142] Furthermore, the well region 31 may be formed so as not to be in direct ohmic contact with the source electrode 80 .

[0143] <2-2. Trench type manufacturing method> Next, a method for manufacturing a trench-type SiC-MOSFET with built-in SBD, which is a silicon carbide semiconductor device according to this embodiment, will be described with reference to Fig. 17 to Fig. 22. Fig. 17 to Fig. 22 are cross-sectional views for explaining the method for manufacturing a SiC-MOSFET with built-in SBD. Here, the description will be given using a cross section of a portion where connection region 36 and connection region 38 are not formed.

[0144] First, as shown in FIG. 17, a semiconductor substrate 10 made of n-type low-resistance silicon carbide having a first main surface oriented in a (0001) plane having an off-angle and a polytype of 4H is formed on the upper surface of the semiconductor substrate 10 by chemical vapor deposition (CVD). 15 cm -3 Greater than or equal to 1×10 17 cm -3 Drift layer 20 made of n-type silicon carbide having the following impurity concentration and a thickness of 5 μm or more and 50 μm or less is epitaxially grown.

[0145] Next, p-type impurity Al (aluminum) is ion-implanted into the upper surface of the drift layer 20. At this time, the depth of the Al ion implantation does not exceed the thickness of the drift layer 20, for example, 0.5 μm or more and 3 μm or less. The impurity concentration of the implanted Al is 1×10 17 cm -3 Greater than or equal to 1×10 19 cm-3 The impurity concentration is in the range below and is set higher than the impurity concentration of the drift layer 20.

[0146] Through the above process, the region into which Al is ion-implanted becomes well region 30B in the active region, and becomes well region 31 in the termination region. Note that well region 30B may be formed on the upper surface of drift layer 20 by an epitaxial method.

[0147] Next, a predetermined region of the surface layer of the well region 30B is doped with an impurity concentration higher than that of the well region 30B, for example, 1×10 16 cm -3 Greater than or equal to 1×10 18 cm -3 The contact region 35B is formed by ion implantation of Al with an impurity concentration in the following range:

[0148] In addition, N, which is an n-type impurity, is ion-implanted into a predetermined region of the surface layer of the well region 30B on the upper surface of the drift layer 20. The depth of N ion implantation is shallower than the thickness of the well region 30B. The impurity concentration of the ion-implanted N is 1×10 18 cm -3 Greater than or equal to 1×10 21 cm -3 This is within the following range and exceeds the p-type impurity concentration of the well region 30B.

[0149] Through the above steps, the region that exhibits n-type conductivity among the regions into which N has been implanted becomes source region 40 B. The structure at the stage where the steps up to this point have been completed is shown in FIG.

[0150] 18, a gate trench GT is formed in a portion where the source region 40B is formed, and a Schottky trench ST is formed in a portion where the source region 40B and the contact region 35B are not formed. Then, a protection region 32 is formed in the bottom of the gate trench GT by ion-implanting Al, which is a p-type impurity, into the bottom of the gate trench GT. Similarly, a protection region 33 is formed in the bottom of the Schottky trench ST by ion-implanting Al, which is a p-type impurity, into the bottom of the Schottky trench ST. The impurity concentrations of the protection region 32 and the protection region 33 are, for example, 1×10 17 cm -3 Greater than or equal to 1×10 19 cm -3 The following ranges are acceptable.

[0151] The connection regions 36 and 38 may be formed by obliquely implanting ions of p-type impurities such as Al from a direction perpendicular to the extension direction of the stripe-shaped trench. The impurity concentration of the connection regions 36 and 38 is 1×10 17 cm -3 Greater than or equal to 1×10 19 cm -3 It may be formed by ion implantation of Al with an impurity concentration in the following range.

[0152] Here, when the plane orientation of the first main surface of the semiconductor substrate 10 is a (0001) plane having an off angle in the <11-20> direction, the gate trench GT and Schottky trench ST in the active region may both be formed parallel to the <11-20> direction. In this way, the side surfaces (trench sidewalls) on both sides of the Schottky trench ST are not affected by the off direction of the semiconductor substrate 10. Therefore, it is possible to reduce the variation in the barrier height of the Schottky interface of the Schottky trench ST. In addition, since the threshold voltage of the MOSFET of the gate trench GT is not affected by the off direction of the semiconductor substrate 10, it is possible to reduce the variation in the threshold voltage of the MOSFET.

[0153] Next, annealing is performed in a heat treatment device in an inert gas atmosphere such as Ar gas at a temperature of 1300 to 1900°C for, for example, 30 seconds to 1 hour. This annealing electrically activates the implanted N and Al ions. The structure after completing the process up to this point is shown in FIG. 18.

[0154] Next, as shown in FIG. 19, the inside of the Schottky trench ST is filled with a protective insulating film 52 such as silicon oxide.

[0155] Next, as shown in FIG. 20, a gate insulating film 50B made of silicon oxide is formed in the gate trench GT, and further, inside the gate trench GT surrounded by the gate insulating film 50B, a gate electrode 60B made of a conductive, low-resistance polycrystalline silicon film is formed by low-pressure CVD and patterning.

[0156] Then, on the upper surface of the gate electrode 60B, an interlayer insulating film 55B made of silicon oxide or the like and having a thickness larger than that of the gate insulating film 50B is formed by low pressure CVD.

[0157] Next, the interlayer insulating film 55B and the gate insulating film 50B are removed by wet etching so as to expose the contact region 35B and the source region 40B in the active region. The structure at the stage where the steps up to this point are completed is shown in FIG.

[0158] 21, a metal film mainly composed of Ni is formed by sputtering or the like on the upper surface where the interlayer insulating film 55B and the gate insulating film 50B have been removed to expose the source region 40B and the contact region 35B. Thereafter, a heat treatment is performed at a temperature of, for example, 600° C. or higher and 1100° C. or lower to react the metal film mainly composed of Ni with the silicon carbide layer to form a silicide between the silicon carbide layer and the metal film.

[0159] Next, the remaining metal film other than the silicide formed as described above is removed by wet etching, whereby the remaining silicide becomes the ohmic electrode 70. The structure at the stage where the process up to this point has been completed is shown in FIG.

[0160] 22, protective insulating film 52 in Schottky trench ST is removed with hydrofluoric acid or the like, and Schottky electrode 71B is formed in Schottky trench ST (specifically, on the bottom and side surfaces). The material of Schottky electrode 71B may be Ti, Mo, or the like.

[0161] Next, a source electrode 80 mainly made of Al is formed so as to connect to the Schottky electrode 71B and the ohmic electrode 70. A gate pad 81 and a gate wiring 82 may be formed simultaneously with the source electrode 80. The structure of the active region at the stage where the steps up to this point are completed is shown in FIG.

[0162] Furthermore, a drain electrode 84 made of a metal film is formed on the lower surface of a back surface ohmic electrode (not shown here) formed on the lower surface (back surface) of the semiconductor substrate 10. In this manner, the semiconductor device 102 according to this embodiment shown in FIG. 15 or 16 can be manufactured.

[0163] <2-3. Operation Description> The operation of the trench-type SiC-MOSFET with built-in SBD, which is the semiconductor device according to this embodiment, is similar to that of the planar-type SiC-MOSFET with built-in SBD.

[0164] In the freewheeling state, a freewheeling current flows from the source electrode 80 to the drain electrode 84 when a voltage lower than that applied to the drain electrode 84 is applied to the source electrode 80, that is, when a back electromotive voltage is applied to the MOSFET.

[0165] In this freewheeling state, a forward electric field (forward bias) is applied to the Schottky junction formed at the contact portion between the drift layer 20 and the Schottky electrode 71B, and a unipolar current consisting of an electron current flows from the Schottky electrode 71B toward the n-type drift layer 20. At this time, the freewheeling current component of the freewheeling diode is mainly this unipolar component. The source electrode 80 and the well region 30B are at the same potential via the ohmic electrode 70.

[0166] As a result, a forward bias is also applied to the pn junction between the p-type well region 30B and the drift layer 20. However, since the pn junction is formed in parallel with the Schottky junction, when going from the off state to the reflux state, the Schottky junction, which has a lower threshold voltage, turns on before the pn junction. As a result, the reflux current flows almost entirely through the Schottky junction, and not through the pn junction.

[0167] In this way, by incorporating an SBD, it is possible to prevent a forward current, which is a bipolar current, from flowing through the pn junction even in a reflux state.

[0168] When a bipolar current flows through a pn junction, and a basal plane dislocation or other origin exists at such a location, stacking faults may expand and the breakdown voltage of the transistor may decrease. Specifically, leakage current occurs when the transistor is in the off state, and the element or circuit may be destroyed by heat generated by the leakage current.

[0169] However, by incorporating an SBD as described above, it is possible to prevent a bipolar current from flowing through the pn junction during reflux, thereby improving the reliability of the semiconductor device.

[0170] <3. Supplementary explanation for the whole> In the above embodiment, aluminum (Al) is used as the p-type impurity, but the p-type impurity may be boron (B) or gallium (Ga). Also, the n-type impurity may be phosphorus (P) instead of nitrogen (N).

[0171] In the MOSFETs described in the above embodiments, the gate insulating film 50 does not necessarily have to be an oxide film such as SiO2, but may be an insulating film other than an oxide film, or a combination of an insulating film other than an oxide film and an oxide film. Although silicon oxide obtained by thermally oxidizing silicon carbide is used as the gate insulating film 50, silicon oxide deposited by a CVD method may also be used.

[0172] In addition, in the above embodiment, specific examples of the crystal structure, the plane orientation of the main surface, the off angle, and the respective implantation conditions are used, but the applicable range is not limited to these numerical ranges.

[0173] The semiconductor device may also be one in which an SBD is built into a MOSFET having a superjunction structure.

[0174] <4. Testing Method> The inspection method according to this embodiment will be described below. Analysis by the inventors has revealed that MOSFETs with low I2t tolerance contain stacking faults.

[0175] The SBD built into a semiconductor device shares a drift layer with the MOSFET. Therefore, when a high-resistance layer blocks the SBD due to stacking faults, the parallel relationship between the body diode and the built-in SBD is broken, and as a result, the operating voltage of the body diode drops. Particularly in the case of a module with multiple MOSFET chips connected in parallel, current concentrates in the MOSFET chip with the lowered operating voltage of the body diode, causing it to break down quickly, further reducing the I2t capability of the entire device.

[0176] Therefore, by removing (dropping off) the MOSFET chips that contain stacking faults, it is possible to screen out MOSFET chips with low I2t capability. However, there are many stacking faults in the SiC drift layer, and only a portion of them affect the I2t capability.

[0177] Figure 23 is a diagram showing an example of the effect of stacking faults (SF) on gate voltage. The horizontal axis of Figure 23 shows the gate voltage Vgs value when the drain current Ids = 4.28 μA. The vertical axis of Figure 23 shows the gate voltage Vgs value when the drain current Ids = 4.28 mA for the same element. In Figure 23, MOSFET chips without stacking faults are indicated with white circles, and MOSFET chips with stacking faults are indicated with black circles.

[0178] As shown in Fig. 23, the majority of MOSFET chips with stacking faults do not affect the I2t capability, i.e., the I2t capability is not significantly reduced, so it is unrealistic to reject all MOSFET chips that contain stacking faults.

[0179] It would be ideal if it were possible to operate the body diode and perform screening based on its operating voltage, but by its very nature, MOSFETs with built-in SBDs are designed to prevent the body diode from operating as much as possible, making it difficult to screen based on the electrical characteristics at the chip stage.

[0180] On the other hand, if a module has many MOSFETs with built-in SBDs connected in parallel, it is possible to actually apply a current surge to screen them. However, if any of the parallel-connected MOSFET chips mounted on a module are dropped by screening, all of them will have to be discarded, which will increase costs.

[0181] As a different approach, it is possible to grasp the influence of stacking faults that reduce the operating voltage of the body diode on characteristics other than the body diode, and based on this, to remove MOSFET chips that have stacking faults. According to the analysis by the inventors, it is known that stacking faults that reduce the operating voltage of the body diode cause abnormalities in the drain current-gate voltage characteristics.

[0182] FIG. 10 is a diagram showing an example of the relationship between the gate voltage and the drain current of a semiconductor device. The stacking faults that reduce the operating voltage of the body diode have the effect of lowering the gate voltage in the rising region of the drain current, which is the current flowing from the drain electrode 84 to the source electrode 80. In the example of FIG. 10, the gate voltage Vg1a (see dotted line) at the drain current Id1, which is a low value drain current, is lower than the gate voltage Vg1 (see solid line) at the drain current Id1 of a semiconductor device that does not have stacking faults that reduce the operating voltage of the body diode. This tendency is particularly noticeable when an n-type low-resistance layer (source region) is formed on the surface layer of a p-type well region that contacts the gate insulating film.

[0183] Therefore, by focusing on the amount of change in gate voltage as described above, it is possible to screen MOSFET chips with low body diode operating voltages.

[0184] The above-mentioned decrease in gate voltage occurs in the low current region, and this tendency disappears in the high current region. Therefore, for the MOSFET chip to be inspected, the difference between the gate voltage at the drain current Id1, which is a low drain current, and the gate voltage at the drain current Id2, which is a high drain current, is calculated at a constant drain voltage, and MOSFET chips for which this difference exceeds a threshold are eliminated (i.e., excluded), and MOSFET chips for which this difference does not exceed the threshold are selected.

[0185] Here, the combination of gate voltage and drain current is not limited to the two, low current region and high current region, as described above, but combinations of gate voltage and drain current in three or more regions may be compared. Also, the above effect (i.e., the effect of lowering the gate voltage in the rising region of the drain current) may be detected by a calculation method other than a simple difference.

[0186] The larger the difference between the drain current values ​​used in the test, the better. For example, the ratio of the maximum drain current to the minimum drain current is selected to be 100 times or more.

[0187] As described above, by applying the inspection method according to this embodiment to a semiconductor device incorporating an SBD, it is possible to screen for semiconductor devices with low I2t tolerance.

[0188] <Second embodiment> A method for inspecting a semiconductor device and a method for manufacturing a semiconductor device according to this embodiment will be described.

[0189] According to the analysis by the inventors, it is known that stacking faults that reduce the operating voltage of the body diode of a MOSFET with an SBD also affect the breakdown voltage characteristics (the relationship between the drain voltage and the drain current). Therefore, by focusing on the breakdown voltage characteristics, it is possible to screen MOSFET chips that contain stacking faults that similarly reduce the operating voltage of the body diode.

[0190] Fig. 11 is a diagram showing an example of the relationship between the drain voltage and the drain current of a semiconductor device. Fig. 11 shows an example in which the gate voltage is changed under a drain voltage Vdm3 that is a drain voltage lower than the avalanche voltage. Here, the drain voltage is the voltage applied between the drain electrode 84 and the source electrode 80.

[0191] In the example of FIG. 11, the difference between the drain current Id3 (see solid line) corresponding to the drain voltage Vdm3 in the case of a gate voltage Vg3 that is a low gate voltage and the drain current Id4 (see dotted line) corresponding to the drain voltage Vdm3 in the case of a gate voltage Vg4 that is a high gate voltage is taken, and MOSFET chips for which this difference exceeds a threshold value (i.e., when the gate voltage is increased, the drain current becomes larger than the reference value) are eliminated (i.e., excluded), and MOSFET chips for which this difference does not exceed the threshold value are selected.

[0192] Here, the combination of gate voltage and drain voltage is not limited to the above two, but may be three or more combinations. Also, the above effect (i.e., the effect that the drain current becomes larger than the reference value when the gate voltage becomes large) may be detected by a calculation method other than a simple difference.

[0193] Among the gate voltages used in the inspection, a voltage having a difference between the maximum and minimum voltages of, for example, 1V or more is selected.

[0194] <Effects of the above-described embodiments> Next, examples of effects produced by the above-described embodiments are shown. In the following description, the effects are described based on the specific configurations shown as examples in the above-described embodiments, but may be replaced with other specific configurations shown as examples in this instruction manual to the extent that similar effects are produced. In other words, for convenience, only one of the corresponding specific configurations may be described as a representative below, but the representatively described specific configuration may be replaced with another corresponding specific configuration.

[0195] Furthermore, the replacement may be made across a number of embodiments, that is, configurations shown as examples in different embodiments may be combined to produce the same effect.

[0196] According to the embodiment described above, the SBD region and the MOSFET region are provided on the first main surface side of the semiconductor substrate 10 made of silicon carbide. A drift layer 20 of a first conductivity type is provided on the first main surface of the semiconductor substrate 10. The MOSFET region includes a well region of a second conductivity type, a source region of a first conductivity type, a gate insulating film 50 (or a gate insulating film 50B), a gate electrode 60 (or a gate electrode 60B), and an interlayer insulating film 55 (or an interlayer insulating film 55B). Here, the well region of the second conductivity type corresponds to, for example, a p-type well region 30 or a well region 30B. The source region of the first conductivity type corresponds to, for example, an n-type source region 40 or a source region 40B. The well region 30 is provided in a surface layer of the drift layer 20 on the first main surface side. The source region 40 is provided in a surface layer of the well region 30. The gate insulating film 50 is provided in contact with the well region 30 sandwiched between the source region 40 and the drift layer 20. The gate electrode 60 is provided in contact with the gate insulating film 50. The interlayer insulating film 55 covers the gate electrode 60. The SBD region includes a Schottky electrode 71 (or a Schottky electrode 71B) that forms a Schottky junction with the drift layer 20 on the first main surface side of the drift layer 20. The semiconductor device also includes a source electrode 80 and a drain electrode 84. The source electrode 80 is connected to the Schottky electrode 71. The source electrode 80 covers the interlayer insulating film 55. The drain electrode 84 is provided on the second main surface side, which is the main surface opposite to the first main surface of the semiconductor substrate 10. In a method for testing a semiconductor device including an SBD region and a MOSFET region, a first gate voltage applied to the gate electrode 60 corresponding to a first drain current flowing from the drain electrode 84 to the source electrode 80 is measured. Here, the first drain current corresponds to, for example, a drain current Id1. The first gate voltage corresponds to, for example, a gate voltage Vg1 or a gate voltage Vg1a. Then, a second gate voltage applied to the gate electrode 60 corresponding to a second drain current having a value larger than the drain current Id1 is measured. Here, the second drain current corresponds to, for example, a drain current Id2.The second gate voltage corresponds to, for example, the gate voltage Vg2, etc. Then, it is checked whether or not the difference between the gate voltage Vg1a and the gate voltage Vg2 exceeds a predetermined threshold value (for example, a value based on the difference between the gate voltage Vg1 and the gate voltage Vg2).

[0197] With this configuration, a MOSFET with an SBD having a low I2t capability can be detected based on the difference in corresponding gate voltages at different drain current values ​​by utilizing the fact that a MOSFET with an SBD having a low I2t capability will have an abnormality in its drain current-gate voltage characteristics due to stacking faults.

[0198] Specifically, the above inspection method is for identifying, based on electrical characteristics, stacking faults that have reached the surface layer of the body diode.

[0199] Unless otherwise specified, the order in which the processes are performed may be changed.

[0200] Furthermore, the same effect can be achieved even if other configurations, examples of which are shown in this instruction manual, are added to the above configuration as appropriate, i.e., other configurations in this instruction manual that are not mentioned as the above configuration are added as appropriate.

[0201] Moreover, according to the embodiment described above, the ratio of the drain current Id1 to the drain current Id2 is 100 times or more. With such a configuration, the larger the ratio of the drain current values ​​used in the test, the larger the corresponding gate voltage deviation. Therefore, the test accuracy is improved.

[0202] According to the embodiment described above, in the method for inspecting a semiconductor device, a first drain current flowing from the drain electrode 84 to the source electrode 80 corresponding to a first gate voltage applied to the gate electrode 60 is measured while a first drain voltage applied between the drain electrode 84 and the source electrode 80 is fixed. Here, the first drain voltage corresponds to, for example, a drain voltage Vdm3 or the like. Also, the first gate voltage corresponds to, for example, a gate voltage Vg3 or the like. Also, the first drain current corresponds to, for example, a drain current Id3 or the like. Then, the drain voltage Vdm3 is applied between the drain electrode 84 and the source electrode 80, and a drain current Id4 flowing from the drain electrode 84 to the source electrode 80 corresponding to a gate voltage Vg4 applied to the gate electrode 60 is measured. Here, the second gate voltage corresponds to, for example, a gate voltage Vg4 or the like. Also, the second drain current corresponds to, for example, a drain current Id4 or the like. Here, the gate voltage Vg4 is a voltage different from the gate voltage Vg3. Then, it is checked whether the difference between the drain current Id3 and the drain current Id4 exceeds a predetermined threshold value (for example, a value based on the difference between the drain current corresponding to the gate voltage Vg3 and the drain current corresponding to the gate voltage Vg4 in a MOSFET chip that does not contain stacking faults).

[0203] With this configuration, a MOSFET with an SBD having a low I2t capability can be detected based on the difference in corresponding drain currents at different gate voltage values ​​by utilizing the fact that a MOSFET with an SBD having a low I2t capability will have an abnormality in its drain current-drain voltage characteristics due to stacking faults.

[0204] Specifically, the above inspection method is for identifying, based on electrical characteristics, stacking faults that have reached the surface layer of the body diode.

[0205] Unless otherwise specified, the order in which the processes are performed may be changed.

[0206] Furthermore, the same effect can be achieved even if other configurations, examples of which are shown in this instruction manual, are added to the above configuration as appropriate, i.e., other configurations in this instruction manual that are not mentioned as the above configuration are added as appropriate.

[0207] Moreover, according to the embodiment described above, the difference between the gate voltage Vg3 and the gate voltage Vg4 is 1 V or more. With such a configuration, the difference between the gate voltages used in the test is sufficiently large, and the corresponding difference in drain current is also large. Therefore, the test accuracy is improved.

[0208] According to the embodiment described above, in the manufacturing method of the semiconductor device, a drift layer 20 of a first conductivity type is formed on a first main surface of a semiconductor substrate 10 made of silicon carbide. Then, a well region 30 of a second conductivity type is formed on a surface layer on the first main surface side of the drift layer 20, a source region 40 of a first conductivity type is formed on a surface layer of the well region 30, a gate insulating film 50 is formed in contact with the well region 30 sandwiched between the source region 40 and the drift layer 20, a gate electrode 60 is formed in contact with the gate insulating film 50, and an interlayer insulating film 55 is formed to cover the gate electrode 60, thereby forming a MOSFET region. Also, a Schottky electrode 71 that forms a Schottky junction with the drift layer 20 is formed on the first main surface side of the drift layer 20, thereby forming an SBD region. Then, a source electrode 80 that is connected to the Schottky electrode 71 and covers the interlayer insulating film 55 is formed. Then, a drain electrode 84 is formed on a second main surface side, which is the main surface opposite to the first main surface of the semiconductor substrate 10. Then, a first gate voltage applied to the gate electrode 60 corresponding to the drain current Id1 flowing from the drain electrode 84 to the source electrode 80 is measured. Here, the first gate voltage corresponds to, for example, a gate voltage Vg1. Then, a second gate voltage applied to the gate electrode 60 corresponding to a drain current Id2 having a value larger than the drain current Id1 is measured. Here, the second gate voltage corresponds to, for example, a gate voltage Vg2. Then, a semiconductor device in which the difference between the gate voltages Vg1 and Vg2 does not exceed a predetermined threshold value is selected.

[0209] With this configuration, MOSFETs with built-in SBDs that have low I2t tolerance can cause abnormalities in the drain current-gate voltage characteristics due to stacking faults, and this can be used to detect and remove MOSFETs with built-in SBDs that have low I2t tolerance based on the difference in corresponding gate voltages at different drain current values.

[0210] Unless otherwise specified, the order in which the processes are performed may be changed.

[0211] Furthermore, the same effect can be achieved even if other configurations, examples of which are shown in this instruction manual, are added to the above configuration as appropriate, i.e., other configurations in this instruction manual that are not mentioned as the above configuration are added as appropriate.

[0212] Moreover, according to the embodiment described above, the ratio of the drain current Id1 to the drain current Id2 is 100 times or more. With such a configuration, the larger the ratio of the drain current values ​​used in the test, the larger the corresponding gate voltage deviation. Therefore, the test accuracy is improved.

[0213] According to the embodiment described above, in the manufacturing method of the semiconductor device, the drift layer 20 is formed on the first main surface of the semiconductor substrate 10 made of silicon carbide. Then, the well region 30 is formed on the surface layer of the first main surface side of the drift layer 20, the source region 40 is formed on the surface layer of the well region 30, the gate insulating film 50 is formed in contact with the well region 30 sandwiched between the source region 40 and the drift layer 20, the gate electrode 60 is formed in contact with the gate insulating film 50, and the interlayer insulating film 55 is formed to cover the gate electrode 60, thereby forming a MOSFET region. Also, the Schottky electrode 71 that forms a Schottky junction with the drift layer 20 is formed on the first main surface side of the drift layer 20, thereby forming an SBD region. Then, the source electrode 80 that is connected to the Schottky electrode 71 and covers the interlayer insulating film 55 is formed. Then, the drain electrode 84 is formed on the second main surface side, which is the main surface opposite to the first main surface of the semiconductor substrate 10. Then, a drain current Id3 flowing from the drain electrode 84 to the source electrode 80 corresponding to a gate voltage Vg3 applied to the gate electrode 60 is measured while a drain voltage Vdm3 applied between the drain electrode 84 and the source electrode 80 is kept constant. Furthermore, a drain current Id4 flowing from the drain electrode 84 to the source electrode 80 corresponding to a gate voltage Vg4 applied to the gate electrode 60 is measured while the drain voltage Vdm3 is applied between the drain electrode 84 and the source electrode 80. Here, the gate voltage Vg4 is a voltage different from the gate voltage Vg3. Then, a semiconductor device in which the difference between the drain current Id3 and the drain current Id4 does not exceed a predetermined threshold value is selected.

[0214] With this configuration, a MOSFET with an SBD that has a low I2t capability can be detected and removed based on the difference in corresponding drain currents at different gate voltage values ​​by utilizing the fact that a MOSFET with an SBD that has a low I2t capability can cause an abnormality in the drain current-drain voltage characteristics due to stacking faults.

[0215] Unless otherwise specified, the order in which the processes are performed may be changed.

[0216] Furthermore, the same effect can be achieved even if other configurations, examples of which are shown in this instruction manual, are added to the above configuration as appropriate, i.e., other configurations in this instruction manual that are not mentioned as the above configuration are added as appropriate.

[0217] Moreover, according to the embodiment described above, the difference between the gate voltage Vg3 and the gate voltage Vg4 is 1 V or more. With such a configuration, the difference between the gate voltages used in the test is sufficiently large, and the corresponding difference in drain current is also large. Therefore, the test accuracy is improved.

[0218] <Modifications of the above-described embodiments> In the multiple embodiments described above, the material, composition, dimensions, shape, relative positional relationship, or implementation conditions of each component may be described, but these are merely examples in all aspects and are not limiting.

[0219] Therefore, countless modifications and equivalents not shown as examples are assumed within the scope of the technology disclosed in this specification. For example, the modification, addition or omission of at least one component, and the extraction and combination of at least one component in at least one embodiment with a component in another embodiment are included.

[0220] In addition, in at least one of the embodiments described above, when a material name or the like is stated without being specifically specified, it is understood that the material in question may include other additives, such as alloys, unless a contradiction arises.

[0221] Various aspects of the present disclosure are summarized below as appendices.

[0222] (Appendix 1) A method for testing a semiconductor device having an SBD region and a MOSFET region, comprising the steps of: the SBD region and the MOSFET region are provided on a first main surface side of a semiconductor substrate made of silicon carbide; a drift layer of a first conductivity type is provided on the first main surface of the semiconductor substrate; The MOSFET region is a well region of a second conductivity type provided in a surface layer of the drift layer on the first main surface side; a first conductive type source region provided in a surface layer of the well region; a gate insulating film provided in contact with the well region sandwiched between the source region and the drift layer; a gate electrode provided in contact with the gate insulating film; an interlayer insulating film covering the gate electrode; the SBD region includes a Schottky electrode that forms a Schottky junction with the drift layer on the first principal surface side of the drift layer, The semiconductor device comprises: a source electrode connected to the Schottky electrode and covering the interlayer insulating film; a drain electrode provided on a second main surface side, which is a main surface opposite to the first main surface of the semiconductor substrate; The semiconductor device inspection method includes: measuring a first gate voltage applied to the gate electrode in response to a first drain current flowing from the drain electrode to the source electrode; measuring a second gate voltage applied to the gate electrode corresponding to a second drain current having a value greater than the first drain current; checking whether a difference between the first gate voltage and the second gate voltage exceeds a predetermined threshold; A method for inspecting a semiconductor device.

[0223] (Appendix 2) A method for inspecting a semiconductor device according to claim 1, The ratio of the first drain current to the second drain current is 100 times or more. A method for inspecting a semiconductor device.

[0224] (Appendix 3) A method for testing a semiconductor device having an SBD region and a MOSFET region, comprising the steps of: the SBD region and the MOSFET region are provided on a first main surface side of a semiconductor substrate made of silicon carbide; a drift layer of a first conductivity type is provided on the first main surface of the semiconductor substrate; The MOSFET region is a well region of a second conductivity type provided in a surface layer of the drift layer on the first main surface side; a first conductive type source region provided in a surface layer of the well region; a gate insulating film provided in contact with the well region sandwiched between the source region and the drift layer; a gate electrode provided in contact with the gate insulating film; an interlayer insulating film covering the gate electrode; the SBD region includes a Schottky electrode that forms a Schottky junction with the drift layer on the first principal surface side of the drift layer, The semiconductor device comprises: a source electrode connected to the Schottky electrode and covering the interlayer insulating film; a drain electrode provided on a second main surface side, which is a main surface opposite to the first main surface of the semiconductor substrate; The semiconductor device inspection method includes: a first drain voltage applied between the drain electrode and the source electrode is kept constant, and a first drain current flowing from the drain electrode to the source electrode corresponding to a first gate voltage applied to the gate electrode is measured; applying the first drain voltage between the drain electrode and the source electrode and measuring a second drain current flowing from the drain electrode to the source electrode corresponding to a second gate voltage applied to the gate electrode; the second gate voltage is different from the first gate voltage; checking whether a difference between the first drain current and the second drain current exceeds a predetermined threshold value; A method for inspecting a semiconductor device.

[0225] (Appendix 4) A method for inspecting a semiconductor device according to claim 3, The difference between the first gate voltage and the second gate voltage is 1 V or more. A method for inspecting a semiconductor device.

[0226] (Appendix 5) A method for manufacturing a semiconductor device including an SBD region and a MOSFET region, A drift layer of a first conductivity type is formed on a first main surface of a semiconductor substrate made of silicon carbide; forming a well region of a second conductivity type in a surface layer on the first main surface side of the drift layer, forming a source region of a first conductivity type in a surface layer of the well region, forming a gate insulating film in contact with the well region sandwiched between the source region and the drift layer, forming a gate electrode in contact with the gate insulating film, and forming an interlayer insulating film covering the gate electrode, thereby forming the MOSFET region; forming a Schottky electrode on the first principal surface side of the drift layer to form a Schottky junction with the drift layer, thereby forming the SBD region; forming a source electrode connected to the Schottky electrode and covering the interlayer insulating film; forming a drain electrode on a second main surface side of the semiconductor substrate, the second main surface being the main surface opposite to the first main surface; measuring a first gate voltage applied to the gate electrode in response to a first drain current flowing from the drain electrode to the source electrode; measuring a second gate voltage applied to the gate electrode corresponding to a second drain current having a value greater than the first drain current; selecting the semiconductor device in which a difference between the first gate voltage and the second gate voltage does not exceed a predetermined threshold value; A method for manufacturing a semiconductor device.

[0227] (Appendix 6) A method for manufacturing the semiconductor device according to claim 5, The ratio of the first drain current to the second drain current is 100 times or more. A method for manufacturing a semiconductor device.

[0228] (Appendix 7) A method for manufacturing a semiconductor device including an SBD region and a MOSFET region, A drift layer of a first conductivity type is formed on a first main surface of a semiconductor substrate made of silicon carbide; forming a well region of a second conductivity type in a surface layer on the first main surface side of the drift layer, forming a source region of a first conductivity type in a surface layer of the well region, forming a gate insulating film in contact with the well region sandwiched between the source region and the drift layer, forming a gate electrode in contact with the gate insulating film, and forming an interlayer insulating film covering the gate electrode, thereby forming the MOSFET region; forming a Schottky electrode on the first principal surface side of the drift layer to form a Schottky junction with the drift layer, thereby forming the SBD region; forming a source electrode connected to the Schottky electrode and covering the interlayer insulating film; forming a drain electrode on a second main surface side of the semiconductor substrate, the second main surface being the main surface opposite to the first main surface; a first drain voltage applied between the drain electrode and the source electrode is kept constant, and a first drain current flowing from the drain electrode to the source electrode corresponding to a first gate voltage applied to the gate electrode is measured; applying the first drain voltage between the drain electrode and the source electrode and measuring a second drain current flowing from the drain electrode to the source electrode corresponding to a second gate voltage applied to the gate electrode; the second gate voltage is different from the first gate voltage; selecting the semiconductor device in which a difference between the first drain current and the second drain current does not exceed a predetermined threshold value; A method for manufacturing a semiconductor device.

[0229] (Appendix 8) A method for manufacturing the semiconductor device according to claim 7, The difference between the first gate voltage and the second gate voltage is 1 V or more. A method for manufacturing a semiconductor device. [Explanation of symbols]

[0230] 10 semiconductor substrate, 20 drift layer, 30 well region, 30A well region, 30B well region, 31 well region, 40 source region, 40B source region, 50 gate insulating film, 50B gate insulating film, 55 interlayer insulating film, 55B interlayer insulating film, 60 gate electrode, 60B gate electrode, 71 Schottky electrode, 71B Schottky electrode, 80 source electrode, 84 drain electrode, 100 semiconductor device, 101 semiconductor device, 102 semiconductor device.

Claims

1. A method for testing a semiconductor device including an SBD region and a MOSFET region, the SBD region and the MOSFET region are provided on a first main surface side of a semiconductor substrate made of silicon carbide; a drift layer of a first conductivity type is provided on the first main surface of the semiconductor substrate; The MOSFET region is a well region of a second conductivity type provided in a surface layer on the first main surface side of the drift layer; a first conductive type source region provided in a surface layer of the well region; a gate insulating film provided in contact with the well region sandwiched between the source region and the drift layer; a gate electrode provided in contact with the gate insulating film; an interlayer insulating film covering the gate electrode; the SBD region includes a Schottky electrode that forms a Schottky junction with the drift layer on the first main surface side of the drift layer, The semiconductor device comprises: a source electrode connected to the Schottky electrode and covering the interlayer insulating film; a drain electrode provided on a second main surface side of the semiconductor substrate, the second main surface being the main surface opposite to the first main surface; The semiconductor device inspection method includes: measuring a first gate voltage applied to the gate electrode in response to a first drain current flowing from the drain electrode to the source electrode; measuring a second gate voltage applied to the gate electrode corresponding to a second drain current having a value greater than the first drain current; checking whether a difference between the first gate voltage and the second gate voltage exceeds a predetermined threshold; A method for inspecting a semiconductor device.

2. 2. A method for inspecting a semiconductor device according to claim 1, A ratio of the first drain current to the second drain current is 100 times or more. A method for inspecting a semiconductor device.

3. A method for testing a semiconductor device including an SBD region and a MOSFET region, the SBD region and the MOSFET region are provided on a first main surface side of a semiconductor substrate made of silicon carbide; a drift layer of a first conductivity type is provided on the first main surface of the semiconductor substrate; The MOSFET region is a well region of a second conductivity type provided in a surface layer on the first main surface side of the drift layer; a first conductive type source region provided in a surface layer of the well region; a gate insulating film provided in contact with the well region sandwiched between the source region and the drift layer; a gate electrode provided in contact with the gate insulating film; an interlayer insulating film covering the gate electrode; the SBD region includes a Schottky electrode that forms a Schottky junction with the drift layer on the first main surface side of the drift layer, The semiconductor device comprises: a source electrode connected to the Schottky electrode and covering the interlayer insulating film; a drain electrode provided on a second main surface side of the semiconductor substrate, the second main surface being the main surface opposite to the first main surface; The semiconductor device inspection method includes: a first drain current flowing from the drain electrode to the source electrode corresponding to a first gate voltage applied to the gate electrode is measured while a first drain voltage is applied between the drain electrode and the source electrode. applying the first drain voltage between the drain electrode and the source electrode and measuring a second drain current flowing from the drain electrode to the source electrode corresponding to a second gate voltage applied to the gate electrode; the second gate voltage is different from the first gate voltage; checking whether a difference between the first drain current and the second drain current exceeds a predetermined threshold value; A method for inspecting a semiconductor device.

4. 4. The method for inspecting a semiconductor device according to claim 3, The difference between the first gate voltage and the second gate voltage is 1 V or more. A method for inspecting a semiconductor device.

5. A method for manufacturing a semiconductor device including an SBD region and a MOSFET region, forming a drift layer of a first conductivity type on a first main surface of a semiconductor substrate made of silicon carbide; forming a well region of a second conductivity type in a surface layer on the first main surface side of the drift layer, forming a source region of a first conductivity type in a surface layer of the well region, forming a gate insulating film in contact with the well region sandwiched between the source region and the drift layer, forming a gate electrode in contact with the gate insulating film, and forming an interlayer insulating film covering the gate electrode, thereby forming the MOSFET region; forming a Schottky electrode on the first main surface side of the drift layer to form a Schottky junction with the drift layer, thereby forming the SBD region; forming a source electrode connected to the Schottky electrode and covering the interlayer insulating film; forming a drain electrode on a second main surface side of the semiconductor substrate, the second main surface being the main surface opposite to the first main surface; measuring a first gate voltage applied to the gate electrode in response to a first drain current flowing from the drain electrode to the source electrode; measuring a second gate voltage applied to the gate electrode corresponding to a second drain current having a value greater than the first drain current; selecting the semiconductor device in which a difference between the first gate voltage and the second gate voltage does not exceed a predetermined threshold value; A method for manufacturing a semiconductor device.

6. 6. A method for manufacturing a semiconductor device according to claim 5, A ratio of the first drain current to the second drain current is 100 times or more. A method for manufacturing a semiconductor device.

7. A method for manufacturing a semiconductor device including an SBD region and a MOSFET region, forming a drift layer of a first conductivity type on a first main surface of a semiconductor substrate made of silicon carbide; forming a well region of a second conductivity type in a surface layer on the first main surface side of the drift layer, forming a source region of a first conductivity type in a surface layer of the well region, forming a gate insulating film in contact with the well region sandwiched between the source region and the drift layer, forming a gate electrode in contact with the gate insulating film, and forming an interlayer insulating film covering the gate electrode, thereby forming the MOSFET region; forming a Schottky electrode on the first main surface side of the drift layer to form a Schottky junction with the drift layer, thereby forming the SBD region; forming a source electrode connected to the Schottky electrode and covering the interlayer insulating film; forming a drain electrode on a second main surface side of the semiconductor substrate, the second main surface being the main surface opposite to the first main surface; a first drain current flowing from the drain electrode to the source electrode corresponding to a first gate voltage applied to the gate electrode is measured while a first drain voltage is applied between the drain electrode and the source electrode. applying the first drain voltage between the drain electrode and the source electrode and measuring a second drain current flowing from the drain electrode to the source electrode corresponding to a second gate voltage applied to the gate electrode; the second gate voltage is different from the first gate voltage; selecting the semiconductor device in which a difference between the first drain current and the second drain current does not exceed a predetermined threshold value; A method for manufacturing a semiconductor device.

8. A method for manufacturing a semiconductor device according to claim 7, The difference between the first gate voltage and the second gate voltage is 1 V or more. A method for manufacturing a semiconductor device.

Citation Information

Patent Citations

  • Silicon carbide semiconductor device and power conversion device

    JP2021108396A

  • Method for inspecting silicon carbide semiconductor device and method for manufacturing silicon carbide semiconductor device

    JP2022163866A

  • Silicon carbide semiconductor device and power converter

    WO2019124378A1

  • Inspection method of semiconductor device

    JP2016023964A