Torch nozzle

The torch nozzle addresses the challenge of cutting thick stainless steel by using a specific gas to move molten material away from the weld pool, enhancing TIG welding efficiency and reducing slag and dust, while maintaining a stable arc and preventing oxidation.

JP2024155271AActive Publication Date: 2024-10-31神野 太郎
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023069867
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-21
Publication Date
2024-10-31
Estimated Expiration
2043-04-21

AI Technical Summary

Technical Problem

Existing TIG welding methods face difficulties in effectively moving and cutting molten base material, particularly in thick stainless steel materials, leading to issues like slag scattering and dust generation, and existing solutions like air arc gouging are inefficient for flat or cylindrical surfaces.

Method used

A torch nozzle with a specific gas inlet and discharge mechanism, allowing the discharge of a specific gas to move molten base material away from the weld pool, utilizing existing TIG welding equipment to form a molten groove by alternating heating and cooling, thereby cutting the material.

Benefits of technology

Enables efficient cutting and melting of base materials using existing TIG welding equipment, reducing slag and dust generation, and maintaining a stable arc while preventing oxidation and nitridation, without the need for additional devices like air arc gouging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024155271000001_ABST
    Figure 2024155271000001_ABST
Patent Text Reader

Abstract

To provide a torch nozzle capable of fusion-cutting a base material by repeating chipping to the base material in order to effectively utilize an existing TIG welding device.SOLUTION: A base material side end part of a torch nozzle 1 is formed with a substantially U-shaped discharge groove 14, and specific gas received from a reception port 13 is discharged from the substantially U-shaped discharge groove 14. Therefore, for example, when a surface diameter of a molten pool reaches a prescribed size, a worker operates a remote controller to discharge the specific gas to the molten pool. As a result, the discharge of the specific gas causes the molten base material in the molten pool to move on the base material. When the molten base material moves on the base material, since there is a large temperature difference with the molten base material, deposition is prevented even if the molten base material solidifies on the base material. Therefore, by repeating the work of moving the molten base material in the molten pool with the specific gas while melting the base material with arc discharge, i.e., the chipping work to the base material, the base material can be finally fusion-cut.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a torch nozzle used in TIG (Tungsten Inert Gas) welding. [Background technology]

[0002] Common methods for cutting stainless steel include cutting with a blade (e.g. grinder, saber saw, hand saw, etc.) and melt cutting (e.g. plasma cutter, etc.). Of these cutting methods, plasma cutting is considered to be superior in terms of work efficiency, but it also has disadvantages such as a rapid decrease in cutting speed as the stainless steel becomes thicker, scattering of slag (dross) during cutting, and generation of a large amount of fumes (dust).

[0003] In order to overcome these disadvantages, a cutting method capable of suppressing scattering of slag and generation of dust has been disclosed (for example, see Patent Document 1). Meanwhile, air arc gouging is one of the methods mainly used in welding to chip away the backside of a weld (chip away the poor penetration part at the bottom of the groove or the first layer part from the backside in butt welding). In air arc gouging, a carbon electrode is attached to an air arc gouging torch, an arc is generated between the electrode and the base material to melt the base material, and compressed air is blown at the base material to blow away the molten base material, thereby creating a groove. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2022-112333 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, in Patent Document 1, when cutting a stainless steel plate, for example, it is difficult to move the molten base material in the molten pool generated by the arc discharge. Even in the case of a cylindrical pipe, it is difficult to move the molten base material in the molten pool generated by the arc discharge near the top of a horizontally installed pipe, just as in the case of cutting a plate.

[0006] Therefore, an object of the present invention is to provide a torch nozzle capable of melt-cutting a base material by repeatedly chipping the base material, in order to effectively utilize existing TIG welding equipment. [Means for solving the problem]

[0007] The torch nozzle is a roughly cylindrical nozzle that houses a tungsten electrode that performs an arc discharge between the electrode and the base material and discharges a shielding gas. The torch nozzle is provided with a receiving port for receiving a specific gas, and the specific gas received from the receiving port is discharged from the end of the roughly cylindrical nozzle on the base material side.

[0008] With this configuration, while the base material is melted by the arc discharge, when the surface diameter of the generated molten pool reaches a predetermined size, the specific gas is discharged, and the molten base material in the molten pool moves over the base material. As the molten base material moves over the base material, the temperature difference between the molten base material in the molten pool and the base material is large, so even if it solidifies on the base material, it will not weld. By repeating this operation of moving the molten base material in the molten pool with the specific gas, i.e., chipping the base material, it is finally possible to melt and cut the base material. Effect of the Invention

[0009] According to the present invention, in order to effectively utilize existing TIG welding equipment, it is possible to provide a torch nozzle capable of melt-cutting a base material by repeatedly chipping the base material. [Brief description of the drawings]

[0010] [Figure 1] FIG. [Diagram 2]FIG. 4 is a side view of the torch nozzle as viewed from the end portion on the base material side. [Diagram 3] FIG. [Figure 4] FIG. [Diagram 5] FIG. 2 is an explanatory diagram showing the configuration of TIG welding. [Figure 6] FIG. 1 is a first explanatory diagram showing the state when chipping the base material. [Figure 7] FIG. 2 is a second explanatory diagram showing the state when chipping the base material. [Figure 8] 4 is an explanatory diagram and a cross-sectional view showing the state after chipping the base material. [Figure 9] FIG. 1 is an explanatory diagram showing the process of chipping a thick base material. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Fig. 1 is a perspective view showing a torch nozzle. As shown in the figure, the torch nozzle 1 is formed in a substantially cylindrical shape made of phosphor bronze. The torch nozzle 1 is formed with a housing portion 12 that houses a tungsten electrode 11 that performs an arc discharge with a base material, and the tungsten electrode 11 is housed therein and a shielding gas is discharged from a gap between the tungsten electrode 11 and the housing portion 12. The upper portion of the torch nozzle 1 is provided with a receiving port 13 that receives a specific gas.

[0012] Further, a substantially U-shaped discharge groove 14 is formed at the end of the torch nozzle 1 on the base material side. This discharge groove 14 is formed on the rear end side in the traveling direction of the torch nozzle 1. The specific gas received from the receiving port 13 is discharged from the substantially U-shaped discharge groove 14.

[0013] FIG. 2 is a side view of the torch nozzle 1 as viewed from the base material side end. As shown in the figure, three communication pipes 15 extending to the back are provided inside the discharge groove 14. FIG. 3 is a plan view of the torch nozzle 1. As shown in the figure, the three communication pipes 15 are provided inside the approximately cylindrical wall constituting the torch nozzle 1. The three communication pipes 15 communicate between the supply port 13 and the discharge groove 14 formed at the base material side end. Therefore, the specific gas received from the supply port 13 is discharged from the discharge groove 14 at the base material side end via the three communication pipes 15.

[0014] FIG. 4 is a right side view of the torch nozzle 1. As shown in the figure, the housing part 12 that houses the tungsten electrode 11 (not shown) is tapered toward the discharge direction of the shielding gas. Therefore, the shielding gas is rectified and the shielding effect against the arc is improved. The communicating tube 15 is inclined toward the housing part 12 as it extends toward the base metal side end of the torch nozzle 1. That is, the communicating tube 15 is inclined with respect to the central axis of the torch nozzle 1 (the dashed line shown in the figure) so as to follow the reduced diameter of the housing part 12. That is, the communicating tube 15 is inclined with respect to the longitudinal direction of the torch nozzle 1. Then, the specific gas received from the receiving port 13 is discharged from the discharge groove 14 through the communicating tube 15. As a result, the specific gas is discharged from an oblique direction with respect to the arc discharge.

[0015] Fig. 5 is an explanatory diagram showing the configuration of TIG welding. As shown in the figure, a gas cylinder 21 is filled with argon gas as a seal gas. The argon gas supplied from the gas cylinder 21 is connected to a welding power source 24 via a pressure regulator 22 and a flowmeter 23. The pressure regulator 22 adjusts the gas pressure of the argon gas filled in the gas cylinders 21 and 28. The flowmeter 23 measures the flow rate of the argon gas supplied from the gas cylinders 21 and 28. The welding power source 24 supplies the power required for TIG welding.

[0016] A remote control 25 that controls the discharge of the seal gas and the specific gas is connected to the welding power source 24. A torch 27 that performs TIG welding on a base material 26 is also connected to the welding power source 24. A torch nozzle 1 is detachably attached to the tip of the torch 27. Argon gas is supplied to the torch 27 as a seal gas via the welding power source 24.

[0017] Gas cylinder 28 is filled with argon gas as a specific gas. The argon gas supplied from gas cylinder 28 is supplied to torch nozzle 1 via pressure regulator 22, flowmeter 23, and solenoid valve 29. When remote control 25 is operated, solenoid valve 29 is opened and closed, and the specific gas is discharged from discharge groove 14 of torch nozzle 1.

[0018] In the TIG welding configuration thus configured, the case of chipping the base material will be described. Fig. 6 is a first explanatory diagram showing the state when chipping the base material. As shown in Fig. 6(a), when the temperature of the base material 26 rises due to the arc discharge while the torch 27 is tilted, the base material 26 melts and a molten pool 31 (double diagonal lines shown in the figure) is generated.

[0019] Then, for example, when the surface diameter of the molten pool 31 reaches a predetermined size, if the operator operates the remote control 25, the specific gas is discharged to the molten pool 31. That is, the specific gas is discharged from the discharge groove 14 formed at the end of the torch nozzle 1 on the base material side. As a result, as shown in FIG. 6(b), the molten base material 32 of the molten pool 31 moves on the base material 26 due to the discharge force of the specific gas and the expansion force caused by the sudden expansion due to the arc heat, and the molten base material 32 moves on the base material 26. When the molten base material 32 moves on the base material 26, the temperature difference between the molten base material 32 and the base material 26 is large, so that even if the molten base material 32 solidifies on the base material 26, it will not be welded. When the molten base material 32 moves from the molten pool 31 in this way, a molten groove 33 is formed behind it.

[0020] FIG. 7 is a second explanatory diagram showing the state when chipping the base material. As shown in FIG. 7(a), the torch 27 moves in the direction indicated by the arrow. When the temperature of the base material 26 rises at the destination, the base material 26 melts, and a molten pool 31 (double diagonal lines in the figure) is generated. For example, when the surface diameter of the molten pool 31 reaches a predetermined size, the operator operates the remote control 25, and a specific gas is discharged. Then, as shown in FIG. 7(b), the molten base material 32 of the molten pool 31 moves on the base material 26. At this time, since the temperature difference between the molten base material 32 and the base material 26 is large, even if the molten base material 32 solidifies on the base material 26, it will not be welded. When the molten base material 32 moves from the molten pool 31 in this way, a molten groove 33 is formed behind it.

[0021] Fig. 8(a) is an explanatory diagram showing the state after chipping the base material. Fig. 8(b) is a cross-sectional view of the part shown by line AA in Fig. 8(a). As shown in Figs. 8(a) and (b), by repeatedly moving the molten base material 32 of the molten pool 31 while moving the torch 27 in the direction of travel shown by the arrow, a molten groove 33 that is long in the direction of travel is formed.

[0022] 9 is an explanatory diagram showing the state when chipping a thick base material. As shown in the figure, when melting a thick base material 26, as shown in the figure (a), by performing the operation of moving the molten base material 32 of the generated molten pool 31 once along the moving direction while tilting the torch 27, a molten groove 33 of a specified depth is formed.

[0023] After that, as shown in (b) to (d) of the same figure, the same operation is repeated again for the molten groove 33 formed in the previous operation. That is, the base material 26 is melted at the same position to generate a molten pool 31 again. Then, the generated molten base material 32 is moved. At this time, the molten groove 33 enhances the effect of the sealing gas. That is, the molten groove 33 can stably maintain the arc discharge and prevent oxidation. By repeating this operation, even in a thick base material 26, the molten groove 33 is gradually formed deeper, and finally the base material 26 can be melted and cut.

[0024] As described above, according to this embodiment, the following actions and effects can be obtained. (1) A substantially U-shaped discharge groove 14 is formed at the end of the torch nozzle 1 on the base material side, and the specific gas received from the receiving port 13 is discharged from the substantially U-shaped discharge groove 14. For this reason, for example, when the surface diameter of the molten pool 31 reaches a predetermined size, if the operator operates the remote control 25, the specific gas is discharged to the molten pool 31. As a result, the molten base material 32 of the molten pool 31 moves on the base material 26 due to the discharge of the specific gas. At this time, the discharge force of the specific gas and the expansion force caused by the sudden expansion due to the arc heat work together to cause the molten base material 32 to move on the base material 26. When the molten base material 32 moves on the base material 26, the temperature difference between the molten base material 32 and the base material 26 is large, so even if the molten base material 32 solidifies on the base material 26, it will not be welded. Therefore, by repeating the process of melting the base material 26 by arc discharge while moving the molten base material 32 in the molten pool 31 that has been generated by a specific gas, i.e., the chipping process on the base material 26, it is possible to eventually melt the base material 26.

[0025] (2) The generation of a molten pool 31 by arc discharge and the movement of the molten base material 32 in the molten pool 31 by the ejection of a specific gas are repeated to form a molten groove 33. At this time, the base material 26 is alternately heated by the arc discharge and momentarily cooled by the ejection of a specific gas. This suppresses the thermal expansion of the base material 26, and reduces unevenness in the molten groove 33. This results in the formation of a molten groove 33 with a smooth surface and an almost straight line pattern.

[0026] (3) The three communication pipes 15 communicate the receiving port 13 with the discharge groove 14 formed at the base metal end. Therefore, the specific gas received from the receiving port 13 is discharged from the discharge groove 14 at the base metal end via the three communication pipes 15. Therefore, even when the specific gas is discharged, it is possible to minimize the entrainment of the surrounding air by the specific gas, and the effect of the shielding gas is not weakened. Therefore, the effect of the shielding gas can be maintained.

[0027] (4) Moreover, the discharge groove 14 is formed in a substantially U-shape at the end of the torch nozzle 1 on the base material side. Therefore, the discharge groove 14 can be moved over the base material 26 so as to envelop the entire molten base material 32 in the molten pool 31, that is, the molten base material 32 can be moved as a single mass. In addition, because the discharge groove 14 is formed in a substantially U-shape, there is an extremely low possibility that it will affect the shielding gas. Therefore, chipping work on the base material 26 and melt-cutting of the base material 26 can be performed while utilizing the TIG welding function.

[0028] (5) The communicating pipe 15 is inclined with respect to the central axis of the torch nozzle 1 so as to follow the reduced diameter of the housing portion 12. In other words, the communicating pipe 15 is inclined with respect to the longitudinal direction of the torch nozzle 1. Therefore, the specific gas received from the receiving port 13 is discharged from the discharge groove 14 via the communicating pipe 15. As a result, the specific gas is discharged from a direction oblique to the arc discharge. Therefore, the molten base material 32 of the molten pool 31 is moved over the base material 26.

[0029] (6) The communication pipes 15 are made up of three pipes. Therefore, the specific gas received through the inlet 13 is discharged from the discharge groove 14 via the three communication pipes 15 without remaining near the inlet 13. Therefore, the specific gas is reliably discharged from the discharge groove 14.

[0030] (7) When the torch nozzle 1 does not receive the specific gas from the receiving port 13, the torch nozzle 1 has a normal TIG welding function. On the other hand, when the specific gas is discharged from the discharge groove 14, the base material 26 can be melted by repeatedly chipping the base material 26. Therefore, the torch nozzle 1 has a TIG welding function, a chipping function, and a melting function. Therefore, according to the torch nozzle 1, since the welded portion can be removed again after TIG welding, there is no need to prepare an air arc gouging device. In addition, since an inert gas is used at that time, oxidation or nitridation of the surface of the base material 26 can be prevented. As a result, there is no need to remove the oxidized or nitrided portion, and the base material 26 can be immediately rewelded.

[0031] (8) For example, when repairing an iron material with a small crack as the base material 26, when cutting the periphery of the crack with a grinder or the like, iron chips get into the crack, making it difficult to grasp the depth of the crack. However, if a method is adopted in which the iron of the base material 26 is melted using a torch nozzle 1 and the molten iron is moved using a specific gas, the molten iron will not get into the crack due to the surface tension of the molten iron, and the periphery of the crack can be reliably removed. In other words, the periphery of the crack can be chipped off using the torch nozzle 1.

[0032] (9) For example, when the surface diameter of the molten pool 31 reaches a predetermined size, the operator operates the remote control 25. This is based on the inventor's empirical rule that the surface diameter of the molten pool 31 is approximately the same as the depth of the molten pool 31. Therefore, the larger the surface diameter of the molten pool 31, the deeper the molten pool 31 can be formed. Therefore, the depth of the molten pool 31, and therefore the depth of the molten groove 33, can be known in advance based on the surface diameter of the molten pool 31 during operation.

[0033] The above embodiment can be modified as follows. The material of the torch nozzle 1 may be ceramic, brass, or alumina (aluminum oxide). The specific gas may be an inert gas containing a small amount of oxygen. For example, the specific gas may be composed of 98% argon and 2% oxygen. The specific gas containing a small amount of oxygen oxidizes the base material and lowers the melting temperature, making the base material more likely to melt. In addition, the viscosity of the molten base material 32 is lowered, making it easier for the molten base material 32 to flow.

[0034] The shielding gas may be an inert gas containing a small amount of hydrogen gas. For example, the shielding gas may be composed of 97% argon and 3% hydrogen. Such a shielding gas containing a small amount of hydrogen gas makes it easier for the arc heat to be transferred to the base material 26, and increases the size and depth of the molten pool 31. As a result, TIG welding and melting of the base material 26 can be performed quickly.

[0035] The torch 27 may be provided with a remote control 25 for allowing the operator to discharge the specific gas from the discharge groove 14. With this configuration, the operator can easily control the timing of discharging the specific gas while still holding the torch 27.

[0036] The specific gas may be discharged from the discharge groove 14 when a temperature sensor or an infrared sensor detects that the temperature of the molten pool 31 has reached a predetermined temperature. With this configuration, the operator does not need to operate a remote control to discharge the specific gas from the discharge groove 14, and the remote control for discharging the specific gas can be omitted.

[0037] A single gas cylinder may be branched into a shielding gas and a specific gas. In other words, if an inert gas similar to the shielding gas is used as the specific gas, gas cylinder 21 may be branched into a shielding gas and a specific gas, eliminating the need to prepare a separate specific gas, making the configuration simpler. The ejection groove 14 may be formed in a substantially V-shape. The ejection groove 14 may be formed with a plurality of small diameters so as to have a generally U-shape or V-shape as a whole.

[0038] The technical ideas grasped from the above-described embodiment will be described below together with their effects. [1] In the torch nozzle according to any one of claims 1 to 5, When the specific gas is not supplied from the receiving port, the torch nozzle functions as a normal TIG welding torch nozzle. With this configuration, it is possible to provide a torch nozzle having a TIG welding function, a chipping function and a melt cutting function.

[0039] [2] A TIG welding device equipped with the torch nozzle according to any one of claims 1 to 5 or the above [1]. With this configuration, it is possible to provide a TIG welding device having a TIG welding function, a chipping function and a melt cutting function. [Explanation of symbols]

[0040] 1...torch nozzle, 11...tungsten electrode, 13...receiving port, 14...discharge groove, 15...connecting pipe, 26...base material.

Claims

1. A torch nozzle having a substantially cylindrical shape that contains a tungsten electrode for performing an arc discharge between the electrode and a base material and that ejects a shielding gas, The torch nozzle is provided with a supply port for receiving a specific gas, A torch nozzle that discharges the specific gas received from the receiving port from the base material side end of the approximately cylindrical body.

2. The torch nozzle according to claim 1, The torch nozzle has a substantially cylindrical wall that defines the substantially cylindrical portion of the torch nozzle and is provided with a communication pipe that connects the supply port to the base material side end portion.

3. The torch nozzle according to claim 2, The torch nozzle has a connecting tube that is inclined so as to follow the reduced diameter of a housing portion that houses a tungsten electrode.

4. The torch nozzle according to claim 3, The torch nozzle has a generally U-shaped ejection groove formed at the end on the base material side.

5. The torch nozzle according to claim 4, The discharge groove is provided on the rear end side of the torch nozzle in the direction in which the welding proceeds.

Citation Information

Patent Citations

  • Gasushiirudoaakuyosetsuho

    JP1976061446A

  • Plasma torch; method for plasma arc welding

    JP2011056546A

  • Cutting method and device used in cutting method

    JP2022112333A

  • Constricting nozzle and tig welding torch using same

    WO2013157036A1