Thin film, in-situ measurement through transparence crystal, and transparence base material in processing chamber wall

By embedding transparent crystals with matching thin films in processing chambers and using interferometric reflectometry, the solution addresses monitoring challenges, ensuring consistent and efficient semiconductor processing.

JP2024156681AActive Publication Date: 2024-11-06APPLIED MATERIALS INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024110618
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2020-06-12
Filing Date
2024-07-10
Publication Date
2024-11-06
Estimated Expiration
2041-06-11

AI Technical Summary

Technical Problem

Current methods for monitoring processing chamber conditions in semiconductor manufacturing are unreliable, leading to non-uniform processing, inefficiencies, and inaccuracies due to variations in chamber surfaces, which affect etch rates and substrate quality.

Method used

Incorporation of transparent crystals embedded within the processing chamber walls with a matching thin film, coupled with a spectrometer and optical coupling device to monitor process film layers using interferometric reflectometry, allowing for real-time detection of optical thin film properties.

Benefits of technology

Provides accurate, real-time monitoring of processing conditions, reducing non-uniformity and inefficiencies by enabling precise control over deposition rates and chamber maintenance, thereby improving substrate quality and throughput.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024156681000001_ABST
    Figure 2024156681000001_ABST
Patent Text Reader

Abstract

To provide a processing system in which at least one part of a transparence crystal is embedded into a wall and a liner of a processing chamber.SOLUTION: A system contains a transparence crystal 120 of which at least one part is embedded into a wall and a liner 124 of a processing chamber. The transparence crystal contains a proximal end having a proximal surface 120A, and a distal end having a distal surface 120B exposed in an inner part of the processing chamber. A transparence thin film 307 is accumulated onto the distal surface, and has a chemical characteristic that is actually matched to a chemical characteristic of the liner. An optical coupling device 204 transmits a light 304A from a light source through the proximal end of the transparence crystal, is returned by being reflected from a combination of a front surface of the transparence thin film and the front surface of a process film layer 309 accumulated onto the transparence thin film to converse a light 304B received into a spectrometer. The spectrometer detects a first spectrum in a focus light expressing a process film layer.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001]

[0001] Embodiments of the present disclosure relate to thin films, in situ measurements through transparent crystals, and transparent substrates within processing chamber walls. [Background technology]

[0002]

[0002] Changes in the surfaces of a processing chamber affect various processing parameters. For example, redeposition of etch by-products on the chamber walls can alter the etch rate of a given process. Thus, as substrates are processed in the chamber, the etch rate (or other processing parameters or conditions) can change, resulting in processing non-uniformity between substrates.

[0003]

[0003] There is currently no reliable method for monitoring surface conditions in a processing chamber, including surfaces such as the liner (or inner wall), lid, electrostatic chuck (ESC), process ring, etc. For example, the chemical, physical, and thermal conditions of the processing chamber liner are known to affect the plasma process by influencing the recombination of outgassing gases near the liner. Although several monitoring methods, such as capacitive monitoring or resonant frequency monitoring, are under development, these methods suffer from thermal or high frequency noise, particularly during processing.

[0004]

[0004] Furthermore, substrate processing is prone to inefficiencies and / or inaccuracies due to lack of information during processing, especially as processing equipment ages. For example, after process shifts over time in a processing chamber, the process may experience changes in deposition amount (e.g., deposition thickness) or changes in deposition composition, either of which may result in unacceptable batches of processed substrates having to be scrapped. Furthermore, knowing when to perform a cleaning process in a processing chamber may be guesswork (e.g., based only on in-process time), and performing the cleaning process too frequently may impact substrate throughput. Other inefficiencies or inaccuracies in processing also exist and are described in more detail below. Summary of the Invention

[0005]

[0005] Some embodiments described herein are directed to a processing system including a transparent crystal, at least a portion of which is embedded within a wall and a liner of a processing chamber. The transparent crystal has a proximal end and a distal end, the distal end having a distal surface exposed to the interior of the processing chamber. A transparent thin film is deposited on the distal surface of the transparent crystal, the transparent thin film having a chemical property substantially matching a chemical property of the liner. The system further includes a spectrometer and an optical coupling device coupled to the spectrometer. The optical coupling device is capable of transmitting light from a light source through the proximal end of the transparent crystal and focusing light received back reflected from a combination of the distal surface, a surface of the transparent thin film, and a surface of a process film layer deposited on the transparent thin film into the spectrometer. The spectrometer is capable of detecting a first spectrum in the focused light, which is representative of the process film layer.

[0006]

[0006] In an additional or related embodiment, the processing chamber includes a wall defining an interior of the processing chamber, a liner attached to an inner surface of the wall, and a transparent crystal, at least a portion of which is embedded within the wall and the liner. The transparent crystal has a proximal end and a distal end, the distal end having a distal surface that is approximately flush with the inner surface of the wall. The processing chamber further includes a transparent thin film deposited on the distal surface of the transparent crystal. The transparent thin film has chemical properties that substantially match chemical properties of the liner. Light from outside the wall can pass through the transparent crystal, reflect off the distal surface, reflect off a surface of the transparent thin film, and return through the proximal end of the transparent crystal.

[0007] In some embodiments, a related method includes embedding at least a portion of a transparent crystal within a wall and a liner of a processing chamber. The transparent crystal has a proximal end and a distal end, the distal end having a distal surface exposed to the interior of the processing chamber. The method further includes depositing a transparent thin film on the distal surface of the transparent crystal, the transparent thin film having chemical properties substantially matching those of the liner. The method further includes depositing a process film layer on the transparent thin film in the processing chamber. The method further includes transmitting light from a light source through the proximal end of the transparent crystal by an optical coupling device. The method further includes focusing light reflected back and received from a combination of the distal end of the liner, the surface of the transparent thin film, and the surface of the process film layer into a fiber optic cable by the optical coupling device. The method further includes receiving the focused light from the fiber optic cable with a spectrometer and detecting a first spectrum representative of the process film layer in the focused light by the spectrometer.

[0008]

[0008] In accordance with these and other aspects of the present disclosure, numerous other features are provided. Other features and aspects of the present disclosure will become more fully apparent from the following detailed description, the claims, and the accompanying drawings.

[0009]

[0009] The present disclosure is illustrated by way of example, and not by way of limitation, in the figures of the accompanying drawings in which like reference numerals denote like elements. It should be noted that different references to "an" or "one" embodiment in the present disclosure are not necessarily to the same embodiment, and such references mean at least one. [Brief description of the drawings]

[0010] [Figure 1] 1 is a top schematic view of an exemplary processing system, according to one embodiment. [Diagram 2] 1 is a simplified side view of a system for monitoring a processing chamber, according to one embodiment. [Diagram 3]3 is an enlarged portion of a side view of the system of FIG. 2 showing transparent crystals embedded in the walls and liner of the processing chamber and a deposited transparent thin film according to one embodiment. [Figure 4A] 11A-11C are simplified side views of a transparent crystal to illustrate angles that may be formed on the proximal and distal surfaces relative to a liner or wall, according to various embodiments. [Figure 4B] FIG. 2 is a simplified side view of a transparent crystal without surface angles, according to one embodiment. [Figure 4C] FIG. 4B is a detailed side view of a transparent crystal with pertinent dimensions including several angles of FIG. 4A, according to one embodiment. [Diagram 5] 1 is a graph of reflectance versus wavelength for several different process film layers compared to a computer model version, according to various embodiments. [Figure 6A] 1 is a flowchart of a method for measuring a first spectrum of a process film layer on a transparent thin film, according to one embodiment. [Figure 6B] 1 is a flowchart of a method for measuring a second spectrum (light not on) of a deposited thin film to determine, along with the first spectrum, one or more optical film properties of a process film layer, according to one embodiment. [Figure 7] 1 is a flow chart of a method of using one or more optical film properties of a thin film deposited on a transparent thin film to improve processing in a processing chamber, according to various aspects of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011]

[0020] The embodiments described herein relate to systems and methods for using interferometric reflectometry on a liner (or inner wall) of a processing chamber to monitor the state and / or process state of the processing chamber. For example, reflectometry can be used to determine one or more optical thin film properties of a thin film layer (e.g., a process film layer) deposited on a liner surface or on a reflector surface proximate to and substantially representative of the liner. Such optical thin film properties include, but are not limited to, thickness, refractive index (n) values, and extinction coefficient (k) values, which may be used to determine compositional materials, as discussed in more detail. In some embodiments, the determination of the process state of the processing chamber is performed during processing of a substrate in the processing chamber, and thus may include adapting to the presence of a plasma in the processing chamber. The plasma includes corrosive gases used to etch the substrate. In other embodiments, the one or more optical thin film properties are determined before or after processing, so there is no need to compensate for the plasma present during an active process.

[0012]

[0021] In various embodiments, determining the condition of the liner of the processing chamber generally indicates the condition of the surface of the processing chamber, including whether there have been any process shifts (or drifts) that need to be corrected, such as, for example, calibration, cleaning, or replacement of the processing equipment or other structures of the processing chamber. Such process shifts may affect the performance and yield of the processed substrate. Additionally, determining the thickness of the layer of the deposited film may be equivalent to a thin film deposited on the substrate being processed (if measured during processing) and therefore can be used to ascertain the appropriate deposition rate, amount, and when and to what extent to clean the processing chamber after processing. The fluorine content in the plasma may also be measured and tracked over time. Further advantages include the ability to perform reflectance measurements with minimal interruption of the plasma space during substrate processing, and reduced risk of hardware-induced skew and particles. This embodiment also requires minimal modifications to existing liner and processing chamber designs.

[0013]

[0022] More specifically, the disclosed systems and methods include a light source (e.g., a broadband light source), a spectrometer (or other apparatus for recording and measuring spectra as an analytical method), and an optical coupling device such as a collimator or mirror. These embodiments, as well as the process chamber that is part of the disclosed system, can further include a transparent crystal, at least a portion of which is embedded within the walls and liner of the process chamber. The transparent crystal can be made of a transparent ceramic material, or can be made of a transparent material such as, for example, sapphire, diamond, quartz, or silicon carbide. A transparent thin film (or substrate) can be formed on the surface of the transparent crystal exposed inside the process chamber. The transparent thin film can be deposited by pre-deposition using atomic layer deposition (ALD), chemical vapor deposition (CVD), or plasma vapor deposition (PVD) of yttrium oxide, aluminum oxide, zirconium oxide, or a similar transparent alloy. In one embodiment, the transparent thin film is approximately flush with the surface of the liner. The transparent thin film can also have a chemical property that substantially matches the chemical property of the liner.

[0014]

[0023] Specifically, a transparent thin film formed on a transparent crystal improves the signal-to-noise ratio (SNR) of the reflected light and the measurement accuracy of the spectrometer. For example, when placed adjacent to or flush with the liner as a separate structure, the transparent thin film can allow for greater control of the film stack created on the transparent thin film. For example, the transparent thin film can be fabricated to obtain desired optical and / or chemical properties. Desired optical properties include producing clearly visible interference fringes when a new process film layer is deposited on top of the transparent thin film. This can increase detection sensitivity and improve SNR. Desired chemical properties include, for example, high chemical resistance to process chemistries, minimizing physical or chemical changes of the transparent thin film to maximize lifetime. Additionally, the chemical properties should mirror those of the liner material to ensure that the deposition on the transparent thin film will be as similar as possible to the deposition on the liner.

[0015]

[0024] In various embodiments, during processing in the chamber, the optical coupling device can direct light from the light source through the transparent crystal, through the transparent thin film, and onto the process film layer deposited on the transparent thin film. In this manner, light passing through both the transparent crystal and the transparent thin film reflects from their respective surfaces and combines with light reflected from the surface of the process film layer deposited on the transparent thin film. This reflected light can include a first spectrum consistent with the condition of the process film layer deposited on the liner.

[0016]

[0025] In these embodiments, the optical coupling device focuses this combination of reflected light into a fiber optic cable that is coupled to a spectrometer. The spectrometer can detect a first spectrum of the focused light that is representative of the process film layer and can be used to determine optical thin film properties. The spectrometer can also detect a second spectrum of the focused light when the light source is turned off during processing in the chamber. This second spectrum corresponds to optical emission spectroscopy (OES) of the plasma at that moment and can be subtracted from the first spectrum to obtain a processable reflectance measurement signal.

[0017]

[0026] For example, embodiments of the system and method may also include a processing device (or controller) coupled to the spectrometer. The processing device may be adapted to receive the first spectrum and the second spectrum and calculate the reflectance measurement data by subtracting (e.g., subtracting) the second spectrum from the first spectrum. The processing device may calculate the reflectance measurement signal by dividing (e.g., dividing) the reflectance measurement data by a reference spectrum that normalizes the reflectance measurement data. The reference spectrum may be obtained under known conditions, such as upon initial installation of the system.

[0018]

[0027] The processing device can then fit the reflectance measurement signal to a thin film optical model to determine information including one or more optical thin film properties of the process film layer. Such optical thin film properties include, but are not limited to, thickness, refractive index (n) value, extinction coefficient (k) value, and compositional material, as discussed in detail. In some embodiments, assumptions can be made about the plasma used, expected deposition thickness, estimated pre-film build-up, and the like, to fit the reflectance measurement signal data to the thin film model to determine the compositional material of the process film layer. The one or more optical thin film properties can then inform certain endpoint decisions associated with the process performed in the processing chamber, such as (but not limited to) whether to adjust the deposition rate, when to stop chemical deposition or plasma, when to start cleaning the processing chamber, when to stop cleaning the processing chamber, and the amount of process drift or consumed chamber life.

[0019]

[0028] In one embodiment, for example, a processing device (or controller) compares the thickness of a process film layer on a transparent thin film to a baseline measurement, e.g., obtained when the processing chamber is first run. If this value fluctuates beyond a threshold variation (e.g., in the thickness of the process film layer), the processing device can trigger a process in the processing chamber to correct the deposition rate of the process film layer. The processing device can also change the process to restore process conditions, or alert a user of the processing chamber of the process shift, or take other actions as described below.

[0020]

[0029] FIG. 1 is a top schematic view of an exemplary processing system 100 according to one aspect of the disclosure. The processing system 100 includes a transfer chamber robot 101 and a factory interface robot 121, each adapted to pick and place a substrate 110 (sometimes referred to as a "wafer" or "semiconductor wafer") from or to a destination within an electronic device processing system, such as the processing system 100 shown in FIG. 1. However, any type of electronic device substrate, mask, or other silica-containing substrate (generally referred to herein as a "substrate") may be transported and transferred by the disclosed robot. For example, the destination of the substrate 110 may be one or more of one or more processing chambers 103 and / or load lock apparatuses 107A, 107B that may be distributed around and coupled to a transfer chamber 114. As shown, the transfer of the substrate may be accomplished, for example, via a slit valve 111.

[0021]

[0030] The processing system 100 may further include a main frame 102 that includes a transfer chamber 114, and at least two processing chambers 103. The housing of the main frame 102 includes the transfer chamber 114 therein. The transfer chamber 114 may include a top wall (not shown), a bottom wall (floor) 139, and side walls, and in some embodiments may be maintained at a vacuum, for example. In the illustrated embodiment, the transfer chamber robot 101 is attached to the bottom wall (floor) 139. However, the transfer chamber robot 101 may be attached elsewhere, such as to the top wall.

[0022]

[0031] In various embodiments, the processing chamber 103 may be adapted to perform any number of processes on the substrate 110. The processes may include deposition, oxidation, nitridation, etching, polishing, cleaning, lithography, metrology, and the like. Other processes may be performed. The load lock apparatus 107A, 107B may be adapted to interface with the factory interface 117 or other system components that may receive the substrate 110, for example, from a substrate carrier 119 (e.g., a front opening integrated pod (FOUP)) that may dock to a load port of the factory interface 117. A factory interface robot 121 (shown in dotted lines) may be used to transfer the substrate 110 between the substrate carrier 119 and each of the load lock apparatuses 107A, 107B. The transfer of the substrate 110 may be performed in any order or direction. The factory interface robot 121 may be the same as (or similar to) the transfer chamber robot 101 in some embodiments, but may further include a mechanism that allows the factory interface robot to move in either lateral direction, as indicated by the arrow 123. Any other suitable robot may also be used as the factory interface robot 121.

[0023]

[0032] In an embodiment, and as an exemplary illustration of any robot, the transfer chamber robot 101 includes at least one arm 113 (e.g., a robot arm) and at least one end effector 115 coupled to the arm 113. The end effector 115 is controllable by the transfer chamber robot 101 to pick up a substrate 110 from a load lock apparatus 107A or 107B, guide the substrate 110 through one of the slit valves 111 of the processing chambers 103, and precisely deposit the substrate 110 on a substrate support of the processing chamber 103.

[0024]

[0033] In various embodiments, one or more of the processing chambers 103 can include a transparent crystal 120, at least a portion of which is embedded in the walls and liner 124 (e.g., an inner wall) of the processing chamber 103. In the disclosed embodiment, light can be collimated and directed through the transparent crystal 120 to generate reflected light. As described in more detail with reference to Figures 2-6, the reflected light can then return through the transparent crystal 120. The reflected light can be focused into a fiber optic cable coupled to a spectrometer 125 for spectral analysis. The spectrometer 125 can perform reflectance measurements to determine one or more spectra of the focused light, which can be used to determine at least one optical property of a process film layer deposited on the transparent thin film of the transparent crystal, whether during or after substrate processing.

[0025]

[0034] The controller 109 (e.g., a tool and equipment controller) can control various aspects of the processing system 100, such as the gas pressure in the processing chamber 103, the individual gas flow rates, spatial flow ratios, the temperature of various chamber components, and the radio frequency (RF) or electrical conditions of the processing chamber 103. The controller 109 can receive signals from and send commands to the factory interface robot 121, the transfer chamber robot 101, one or more sensors, and / or other processing components of the processing system 100. In this manner, the controller 109 can control the start and stop of processing, adjust deposition rates, types or composition ratios of deposition compositions, etc. The controller 109 can further receive and process sensing data from various sensors.

[0026]

[0035] In various embodiments, the controller 109 includes (or is coupled to) a processing device 130 and is coupled to the spectrometer 125. The processing device 130 may be configured to receive and process sensing data including the results of the reflectance measurements performed by the spectrometer 125, including the first and second spectra described above. The processing device 130 may calculate a reflectance measurement signal by subtracting the second spectrum from the first spectrum. The processing device may then fit the reflectance measurement signal to a thin film optical model to determine information including one or more optical thin film properties of the process film layer. Depending on the results of analyzing the one or more optical film properties, the processing device 130 (e.g., the controller 109) may direct the processing chamber 103 to process changes or adjustments. For example, the controller 109 may adjust process parameters or settings, such as, for example, deposition rate, type or composition ratio of deposition composition, timing of performing a cleaning process in the processing chamber, and other operations described in more detail with reference to FIG. 7.

[0027]

[0036] The controller 109 and / or the processing device 130 may be and / or include a computing device, such as a personal computer, a server computer, a programmable logic controller (PLC), a microcontroller, etc. The controller 109 and / or the processing device 130 may include (or be) one or more processing devices, which may be general-purpose processing devices, such as a microprocessor, a central processing unit, etc. More specifically, the processing device may be a complex instruction set computing (CISC) microprocessor, a reduced instruction set computing (RISC) microprocessor, a very long instruction word (VLIW) microprocessor, or a processor implementing other instruction sets, or a processor implementing a combination of instruction sets. The processing device may also be one or more special-purpose processing devices, such as an application specific integrated circuit (ASIC), a field programmable gate array (FPGA), a digital signal processor (DSP), a network processor, etc. The controller 109 and / or the processing device 130 may include a data storage device (e.g., one or more disk drives and / or solid state drives), a main memory, a static memory, a network interface, and / or other components. The processing device 130 may execute instructions to perform any one or more of the methods and / or embodiments described herein. The instructions may be stored in a computer-readable storage medium, which may include a main memory, a static memory, a secondary storage device, and / or a processing device (during execution of the instructions).

[0028]

[0037] FIG. 2 shows a simplified side view of a system 200 for monitoring a process chamber according to one embodiment of the present disclosure. The system 200 can include a process chamber 103 having a liner 124, for example, as shown in FIG. 1. The process chamber 103 can include a wall 222 to which the liner 124 is attached. The liner 124 is specially designed to have high chemical resistance to process chemistries, minimizing physical or chemical changes to the liner to maximize its lifespan. Additionally, as shown, at least a portion of the transparent crystal 120 can be embedded within the wall 222 and the liner 124. The transparent crystal 120 can be made of a transparent ceramic material or a durable transparent material such as sapphire, diamond, quartz, silicon carbide, or a combination thereof.

[0029]

[0038] In an embodiment, the system 200 further includes a light source 201 (e.g., a broadband light source or other electromagnetic radiation source), an optical combining device 204 (e.g., a collimator or mirror), a spectrometer 225, a controller 109, and a processing device 130. The light source 201 and the spectrometer 225 may be optically coupled to the optical combining device 204 via one or more fiber optic cables 232.

[0030]

[0039] In one embodiment, light source 201 is a flash lamp limited to a wavelength range of 200-800 nanometers (nm), is a pulsed xenon light source, and has a flash output variation of less than 0.5% sigma across the entire wavelength range in an open loop. In other embodiments, the wavelength range may vary further, for example, set near near infrared wavelengths. Variable output control of light source 201 may be between 45% and 100%, and output decay over a life of at least one year may be less than 8%, thereby providing over one billion flashes. Additional or different embodiments of light source 201 having various capabilities and wavelengths are envisioned.

[0031]

[0040] In various embodiments, the optical coupling device 204 may be adapted to collimate or otherwise transmit light in two directions along the optical path. The first direction may include light from the light source 201 being collimated and transmitted through the transparent crystal 120 into the processing chamber 103. The second direction may be reflected light from the transparent crystal 120 back into the optical coupling device 204, as described in more detail with reference to FIG. 3. The reflected light may be focused into the fiber optic cable 232 and thus directed to the spectrometer 225 in the second direction along the optical path. Additionally, the fiber optic cable 232 may be coupled between the spectrometer 225 and the light source 201 to efficiently transmit light from the light source 201 to the transparent crystal 120 and back to the spectrometer 225.

[0032]

[0041] In an embodiment, the spectrometer 225 also has a wavelength range of 200-800 nm, a wavelength resolution of less than 2 nm full width at half maximum, a dynamic range of at least 16 bits, a noise floor of less than 32 counts, and a sampling rate of 6 milliseconds (ms) or faster. The spectrometer 225 may require calibration on the same schedule or on a longer schedule compared to the light source 201. The spectrometer 225 may be adapted to detect the spectrum of reflected light received from the optical coupling device 204 (e.g., light reflected back from the transparent crystal 120 and focused by the optical coupling device 204 into the fiber optic cable 232).

[0033]

[0042] In various embodiments, the controller 109 includes or is coupled to the processing device 130 and includes or is coupled to the memory 134 or other computer storage device. The controller 109 may be coupled to both the light source 201, the spectrometer 225, and the process chamber 103. The controller 109 may turn on the flash of the light source 201 and then receive a first spectrum from the spectrometer 225. The controller 109 may also keep the light source off and receive a second spectrum from the spectrometer 225 when the light source 201 is off. The second spectrum may represent the OES of the plasma or chemical process in the process chamber. The processing device 130 may subtract the second spectrum from the first spectrum to determine a reflectance measurement signal at a given moment. The processing device 130 may then mathematically fit the reflectance measurement signal to one or more thin film models to determine one or more optical thin film properties of the process film layer deposited on the transparent thin film of the transparent crystal 120.

[0034]

[0043] In some embodiments, the one or more optical thin film properties include a thickness of the deposited film, as well as values ​​of a refractive index (n) and an extinction coefficient (k). The refractive index is the ratio of the speed of light in a vacuum to the speed of light in the process film layer. The extinction coefficient is a measure of the amount of light absorbed in the process film layer. The processing device 130 can use the n and k values ​​to determine the composition of the process film layer. The processing device 130 can be further configured to analyze the data of the one or more optical film properties and, based on the analysis, trigger a new process or update a current process in the processing chamber 103. Such updates may include alerts and are described in more detail with reference to FIG. 7.

[0035]

[0044] 3 is an enlarged portion of a side view of the system of FIG. 2 showing a transparent crystal 120 embedded within the wall 222 and liner 124 of the processing chamber 303, according to one embodiment. The transparent crystal 120 can have a proximal end and a distal end, where the proximal end has a proximal face 120A that receives light from the optical coupling device 204 and the distal end 120B has a distal face 120B for reflecting light back through the proximal face 120A to the optical coupling device 204. In one embodiment, the distal face 120B of the transparent crystal 120 can be proximal to the processing chamber 303 and can be approximately flush with the inner surface of the wall 222.

[0036]

[0045] In various embodiments, the transparent crystal 120 may be shaped like a plug (e.g., plug-shaped) and may include a shaft 301 and a flange 305 integrally formed with or attached to the shaft 301. The plug may be a sapphire plug, a diamond plug, a quartz plug, or a silicon carbide plug. The shaft 301 and / or the flange 305 may be square, rectangular, cylindrical, or other shapes. For ease of illustration, both the shaft 301 and the flange 305 are illustrated as cylindrical. As described, the transparent crystal 120 may be made from a transparent gemstone, such as sapphire, diamond, quartz, silicon carbide, etc., to provide a hard material that is difficult to change and reflects light. The shaft 301 may be embedded within the wall 222 and the liner 124 such that the distal face is exposed to the interior of the processing chamber 303.

[0037]

[0046] The flange 305 may be adjacent to the outer surface of the wall 222. In one embodiment, a seal 313 is disposed between the flange and the outer surface of the wall 222. The seal 313 may be, for example, an O-ring seal, a rectangular or gasket seal, a valve seal, or the like. The material of the seal 313 may be propylene diene monomer, a fluoroelastomer, or the like. The flange 305 may have an inner surface in physical contact with the seal 313, the inner surface including a surface roughness (Ra) of less than 20 nanometers or a scratch-dig value of at least 80 / 50, which is an optical specification used for surface roughness. The very smooth inner surface of the flange 305 may help provide a hermetic seal between the less clean atmosphere outside the processing system 100, 200 and the highly clean and filtered air of the processing chamber 303, which may be under vacuum.

[0038]

[0047] In various embodiments, a transparent thin film 307 may be deposited on the distal surface 120A of the shaft 301 of the transparent crystal 120, for example by atomic layer deposition (ALD). In some cases, the transparent thin film 307 is deposited on the transparent crystal 120 before the transparent crystal 120 is embedded within the wall 222 and liner 124. The transparent thin film 307 may be exposed inside the processing chamber 303. In some embodiments, as previously described, the transparent thin film 307 is made to be approximately flush with the liner 124 and to have chemical properties that substantially match those of the liner. In various embodiments, the transparent thin film 307 is yttrium oxide, aluminum oxide, zirconium oxide, or combinations thereof that make a similar transparent alloy. In one embodiment, the transparent thin film 307 is yttrium oxide and is deposited to a known thickness that is between 10 nm and 1 micrometer (μm) thick, for example 270 nm thick, and useful for analyzing the reflected light.

[0039]

[0048] In various embodiments, the deposition process (e.g., ALD) of the transparent thin film 307 is carefully controlled to ensure that it is similar to the material of the liner 124 but is in a different physical state, e.g., smoother and flatter, to facilitate light reflection from its surface. In this way, the transparent thin film 307 reflects light to provide an accurate state of the chamber, and the thinness and smoothness increase the signal-to-noise ratio (SNR) of the distal surface, facilitating the ability to test thinner process film layers 309 in the processing chamber 303. The transparent thin film 307 also passivates and protects the material of the transparent crystal 120, allowing the expensive transparent crystal 120 to last longer in the corrosive processing environment of the processing chamber 303.

[0040]

[0049] In some embodiments, a process film layer 309 (e.g., a process thin film layer) is deposited during processing in the processing chamber 303. The process film layer 309 may include a film stack that is measured by the spectrometer 225. The optical coupling device 204 can collimate the light provided by the light source 201 and direct the collimated light 304A through the proximal surface 120A of the transparent crystal 120, e.g., the outer surface of the flange 305. This incident light is then reflected from the distal surface 120B of the transparent crystal, e.g., the shaft 301, from the surface of the transparent thin film 307, and from the surface of the process film layer 309. These three reflected light sources come back together and return into the optical coupling device 204, as shown as reflected light 304B. The optical coupling device 204 can focus the reflected light into the fiber optic cable 232 to enter the spectrometer for measurement (see FIG. 2).

[0041]

[0050] The return optical signals at each interface (e.g., the three surfaces mentioned above) can all be optically combined to result in constructive and destructive interference. The exact nature of this interference depends on the relative thickness of each layer, e.g., the transparent crystal 120, the transparent thin film 307, and the process film layer 309 (or film stack). The final result measured by the spectrometer 225 (and after normalization to an initial reference) is a spectrum with interference fringes. These interference fringes can be fitted with a mathematical thin film model to determine one or more thin film optical parameters of the process film layer 309, such as thickness, n value, and k value. The n value and k value can be used to determine the composition material. Therefore, knowing the exact initial thickness and optical properties of the transparent thin film 307 helps to fit the spectrum to the thin film model.

[0042]

[0051] 4A is a simplified side view of a transparent crystal 420 to illustrate angles that may be formed on a proximal face 420A (or first face) and a distal face 420B (or second face) relative to a liner 122 or wall 222 of a processing chamber 303, according to various embodiments. Note that the lines and angles in FIG. 4A are exaggerated for ease of illustration and are not drawn to scale.

[0043]

[0052] As mentioned above, the distal surface 120B of the transparent crystal 120 may be approximately flush with the wall 222 of the processing chamber 303. Back reflections from the proximal surface 120A may not contribute to the sensor signal and reduce the effective dynamic range of detection by the spectrometer 225. Therefore, the transparent crystal 120 may be designed with a slightly tilted first angle (θ1) with respect to the incident collimated light 404A. The first angle (θ1) may be, for example, between 2 degrees and 5 degrees. In one embodiment, the first angle (θ1) is 3 degrees.

[0044]

[0053] Since the light that passes through is refracted (e.g., refracted light 404B), the optimum angle of the proximal surface 420B for maximum reflection may be perpendicular to this refracted light ray. In one embodiment, this optimum or second angle (θ2) may be between 0.8 and 1.8 degrees. In one embodiment, the second angle (θ2) is 1.3 degrees. Note that θ1 is θ 12 +θ 13 Furthermore, Snell's law, as expressed in Equation 1 and Equation 2, states that: TIFF2024156681000002.tif24170Equation 3 represents the maximum reflection from distal surface 420B. TIFF2024156681000003.tif9170

[0045]

[0054] Thus, by way of example, if the transparent crystal is made of sapphire, the approximate optimum angles can be obtained as follows: TIFF2024156681000004.tif14170Here, assuming θ1=3° and n2=1.8 (sapphire), The result is TIFF2024156681000005.tif9170.

[0046]

[0055] If a different first angle (θ1) is selected, the second angle (θ2) may be different, as determined by Equation 4. In an alternative embodiment, the optical components, e.g., at least the optical coupling device 204, may be tilted by a first angle (θ1) to optimize the incident light with respect to the proximal face 420A. Thus, the proximal face 420A may remain at no angle with respect to the wall of the processing chamber, and the distal face 420B may be slightly angled to maximize reflection from the distal face 420B. Alternatively, the optical coupling device 204 may be tilted by a second angle (θ2), and thus at an optimal angle with respect to the distal face 420B. In this embodiment, the distal face 420A is at no angle with respect to the wall, and then the proximal face 420A may be tilted by a slight angle to reduce back reflection of the incident collimated light 404A.

[0047]

[0056] 4B is a simplified side view of a transparent crystal that does not include surface angles, according to one embodiment. Thus, the proximal and distal faces 420A and 420B are flat and have no angles designed into their respective surfaces. This type of plug for a transparent crystal is easier to manufacture, but may suffer from reduced dynamic range and sensitivity due to back reflections from the proximal face 420A.

[0048]

[0057] FIG. 4C is a detailed side view of a transparent crystal with suitable dimensions including some angles of FIG. 4A, according to one embodiment. In FIG. 4C, the transparent crystal 420 includes a proximal face 420A with a first angle (θ1) of about 3 degrees. The transparent crystal 420 may further include a distal face with a second angle of about 1.3 degrees. Variations in the optimal range of the first and second angles are expected and can be calculated according to Equation 4 once the first angle is selected. The transparent crystal 420 of FIG. 4A and FIG. 4B is more complex to design and manufacture, but has a better dynamic range and sensitivity to film deposition on the distal face 420B.

[0049]

[0058] 5 is a graph of reflectance versus wavelength for several different process film layers compared to a computer model version according to various embodiments. Note that different process film layers have different thicknesses, resulting in correspondingly different reflectance signals. Each experiment (solid curve) includes a corresponding simulation model (dashed curve). This graph shows that the reflectance signal (or reflectometry signal) can be analyzed to determine the thickness of the process film layer.

[0050]

[0059] FIG. 6A is a flow chart of a method 600A for measuring a first spectrum of a process film layer on a transparent thin film, according to one embodiment. The method 600A can be performed using the components described with reference to FIGS. 1-4A, as will become apparent. Although shown in a particular order or sequence, the order of the processes can be changed unless otherwise specified. Thus, the illustrated embodiment should be understood as an example only, and the illustrated processes can be performed in a different order, and some processes can be performed in parallel. Furthermore, in various embodiments, one or more processes can be omitted. Thus, not all processes are required in every embodiment. Other process flows are possible.

[0051]

[0060] In step 610, the method 600A may include providing at least a portion of a transparent crystal 120 embedded within a wall and a liner of a processing chamber. The transparent crystal 120 has a proximal end and a distal end, the distal end having a distal surface exposed to the interior of the processing chamber. The portion of the transparent crystal 120 embedded within the wall and the liner may be a shaft 301, as shown in FIG. 3. The transparent crystal 120 may be one of sapphire, diamond, or other sufficiently hard and sufficiently transparent crystals.

[0052]

[0061] In step 615, the method 600A may further include depositing a transparent thin film having chemical properties substantially matching those of the liner on the distal surface of the transparent crystal 120 using atomic layer deposition (ALD). The transparent thin film may be yttrium oxide, aluminum oxide, or zirconium oxide, or a similar alloy, and may be of a known thickness. The deposition performed in step 615 may occur prior to embedding the transparent crystal 120 within the walls and liner of the processing chamber.

[0053]

[0062] Next, in step 620, the method 600A deposits a process film layer on the transparent thin film in the process chamber. The process film layer may be a chemically or plasma deposited thin film layer, or may include a film stack having a bottom layer of build-up before the process chamber is cleaned.

[0054]

[0063] Next, in step 625, method 600A transmits light from the light source through the proximal end of the transparent crystal by a light coupling device. The light source 201 may be a flash lamp and was described in detail with reference to Figure 2. The light coupling device 204 may be a collimator, a mirror, or a set of mirrors and was described in detail with reference to Figures 2-3.

[0055]

[0064] Next, in step 630, method 600A focuses the light reflected back and received from the combination of the distal surface, the transparent thin film surface, and the process film layer surface into a fiber optic cable by an optical combining device. These three different reflected lights can add constructively and destructively depending on the thicknesses of these three different layers, as described with reference to FIG.

[0056]

[0065] Then, in step 635, method 600A can receive the focused light from the fiber optic cable with a spectrometer, as described in detail with reference to Figure 2. Then, in step 640, method 600A can detect in the focused light with the spectrometer a first spectrum representative of the process film layer.

[0057]

[0066] FIG. 6B is a flow chart of a method 600B for measuring a second spectrum (without light on) of a deposited thin film to determine one or more optical film properties of a process film layer along with the first spectrum, according to one embodiment. Method 600B can be performed using components described with reference to FIGS. 1-4A, as will become apparent. Although shown in a particular order or sequence, the order of processes can be changed unless otherwise specified. Thus, the illustrated embodiment should be understood as an example only, and the illustrated processes can be performed in a different order, and some processes can be performed in parallel. Furthermore, in various embodiments, one or more processes can be omitted. Thus, not all processes are required in every embodiment. Other process flows are possible.

[0058]

[0067] In step 650, the method 600B includes detecting a second spectrum from the focused light with a spectrometer when the light source is off, which may be an OES of the process chamber at the time the first spectrum was measured.

[0059]

[0068] Method 600B may continue with receiving the first spectrum and the second spectrum by a processing device in step 655. The processing device may be processing device 130 or controller 109 shown in FIGS.

[0060]

[0069] Then, in step 660, the method 600B can subtract the second spectrum from the first spectrum by the processing device to generate reflectance measurement data. This reflectance measurement data can also be generated without this step if there is no plasma in the processing chamber and therefore the measurement of the first spectrum is before or after processing with plasma. Then, in step 665, the method 600B can divide the spectroscopic measurement data by a reference spectrum by the processing device to generate a reflectance measurement signal. The reference spectrum can be obtained under known conditions, such as during initial installation of the system. The division can normalize the spectroscopic measurement data to a spectroscopic measurement signal that can be analyzed appropriate for the deposited process film layer.

[0061]

[0070] Subsequently, in step 670, the method 600B can include fitting, by a processing device, the reflectance measurement signals to a thin film optical model to determine information including one or more optical film properties of the process film layer. The one or more optical film properties can be the film thickness, the n and k values, and / or the compositional material of the process film layer.

[0062]

[0071] FIG. 7 is a flow chart of a method 700 of using one or more optical film properties of a process film layer on a transparent thin film to improve processing in a processing chamber, according to various aspects of the present disclosure. Method 700 can be performed by processing logic, which can include hardware (circuitry, dedicated logic, etc.), software (e.g., running on a general purpose computer system or dedicated machine), firmware, or any combination thereof. For example, method 700 may be performed by controller 109 (e.g., processing device 130) as referenced herein. In an embodiment, various baselines or thresholds (such as thickness variations, or n and k variations) may be stored in memory 134 of controller 109 and indexed to specific compositions. These values ​​can be used as a comparison by the various methods 700 just described. Although shown in a particular order or sequence, the order of the processes can be changed unless otherwise specified. Thus, the illustrated embodiment should be understood as an example only, and the illustrated processes can be performed in a different order, and some processes can be performed in parallel. Additionally, in various embodiments, one or more processes can be omitted. Thus, not all processes are required in every embodiment. Other process flows are possible.

[0063]

[0072] Referring to FIG. 7, the method 700 may begin with the processing logic processing the reflectance measurement signal to fit the reflectance measurement signal to a thin film optical model to determine one or more optical film properties (e.g., thickness, n and k values, and / or material composition) of the process film layer 309 deposited on the transparent thin film 307 (710). If the measurements are obtained while processing the substrate in the processing chamber, the method 700 may then determine whether the thickness matches a baseline measurement of the process film layer, for example taking into account the composition of the process film layer 309 (715). If yes, and there is a match, the method 700 may continue to process the substrate in the processing chamber (705). If there is no match, the method 700 may then determine that the variation in the deposition rate of the process film layer 309 exceeds a threshold variation based on the thickness comparison (720).

[0064]

[0073] In various embodiments, the threshold variation may be sufficient to accommodate changes in the deposition process. Such threshold variation may be application specific or may be empirically determined based on the amount of variation required to induce a process shift. Also, the monitored process may be an etch, a deposition, or the like. Subsequently, in method 700, processing logic may trigger a process in the processing chamber to correct the deposition rate of the process film layer (725). This portion of method 700 may thus use differential measurements compared to baseline measurements over time to determine if the process of the processing chamber has shifted (or drifted) over time.

[0065]

[0074] Similarly, method 700 may then include processing logic determining (730) whether the material composition of the process film layer 309 matches the baseline composition expected to be deposited on the transparent thin film. If yes, method 700 may continue to process the substrate in the processing chamber (705). If not, method 700 may then include processing logic sending a feedback signal to the controller 109 (or other computing device with an interface to a processing system operator) to report an error due to a process shift detected in the processing chamber (735). A process shift may be detected by the fact that the detected composition has varied from the expected composition. This portion of method 700 may be performed while the processing system is inactive, in one embodiment.

[0066]

[0075] In some embodiments, the method 700 may then determine (740) whether the process film layer on the transparent thin film has reached a build-up limit (e.g., a limit on the built-up thickness required to be within specifications) during or after processing the substrate in the processing chamber. If not, the method 700 may continue to process the substrate in the processing chamber (705). If yes, the method 700 may then proceed to have the processing logic trigger (745) the processing chamber to start a cleaning process in the processing chamber. This cleaning process may be intended to clean the processing equipment and the surface of the built-up film to improve future processing results and / or to bring the processing equipment back up to a certain specification. The cleaning process may also require a plasma process and therefore may have OES to be subtracted from the spectrum determined with the light source turned on to determine the reflectance measurement signal.

[0067]

[0076] In various embodiments, the method 700 may then determine (750) during such cleaning process triggered by operation 745 whether the process film layer has been removed to a predetermined threshold thickness. Such a determination may be to ascertain whether the process film layer has been sufficiently reduced by the cleaning process. Once the process film layer has been removed to or beyond the predetermined threshold thickness, the method 700 may then include a processing logic triggering the processing chamber to terminate the cleaning process being performed therein (755). Upon completion, the method 700 may continue to process the substrate in the processing chamber (705).

[0068]

[0077] Additional or similar methods to method 700 of Figure 7 are envisioned. For example, during processing of a substrate in a processing chamber, processing logic may detect a moment when a process film layer reaches a threshold level of thickness on the transparent thin film 307. Processing logic may further trigger an end of a deposition process depositing a deposition film layer in the processing chamber. Processing logic may make other decisions similar to this one and update the process or process state of the processing chamber to improve substrate throughput, quality, and / or reduce process shifts.

[0069]

[0078] According to further embodiments, the processing chamber may perform a cleaning process, in some cases after each substrate (or group of substrates) is processed, or at other intervals. The processing logic can determine exactly when the end point of this cleaning is reached on the distal surface 120B or 420B of the transparent membrane 307. The processing logic can then trigger the processing chamber to stop cleaning and proceed to the next step, improving throughput. If the distal surface 120B or 420B is not cleaned at the same rate as the rest of the chamber, this difference can be pre-characterized and compensated for by a look-up table in the controller 109.

[0070]

[0079] The foregoing description sets forth numerous specific details, such as examples of specific systems, components, methods, and the like, to provide a good understanding of some embodiments of the present disclosure. However, it will be apparent to those skilled in the art that at least some embodiments of the present disclosure may be practiced without these specific details. In other instances, well-known components or methods have not been described in detail or have been presented in simple block diagram form to avoid unnecessarily obscuring the present disclosure. Thus, the specific details described are merely illustrative. It may be contemplated that a particular implementation may differ from these illustrative details and still be within the scope of the present disclosure.

[0071]

[0080] References throughout this specification to "one embodiment" or "an embodiment" mean that a particular feature, structure, or characteristic described in connection with that embodiment is included in at least one embodiment. Thus, the appearances of the phrases "in one embodiment" or "in an embodiment" in various places throughout this specification do not necessarily all refer to the same embodiment. Furthermore, the term "or" is intended to mean an inclusive "or" rather than an exclusive "or". When the term "about" or "approximately" is used herein, this is intended to mean that the stated nominal value is accurate to within ±10%.

[0072]

[0081] Although the method steps herein are shown and described in a particular order, the order of each method step may be changed such that certain steps may be performed in reverse order, and certain steps may be performed, at least in part, simultaneously with other steps. In alternative embodiments, the instructions of individual steps or sub-steps may be intermittent and / or alternating.

[0073]

[0082] It is understood that the above description is intended to be illustrative, and not limiting. Many other embodiments will become apparent to those skilled in the art upon reading and understanding the above description. The scope of the present disclosure should therefore be determined with reference to the appended claims, along with the full scope of equivalents to which such claims are entitled.

Claims

1. a transparent crystal, at least a portion of which is embedded within a wall and a liner of a processing chamber, said transparent crystal having a proximal end and a distal end, said distal end having a distal surface exposed to an interior of the processing chamber; a transparent thin film deposited on the distal surface of the transparent crystal, the transparent thin film having chemical properties substantially matching those of the liner; Spectrometers, and an optical coupling device coupled to the spectrometer, transmitting light from a light source through the proximal end of the transparent crystal; focusing light received back from a combination of the distal surface, a surface of the transparent thin film, and a surface of a process film layer deposited on the transparent thin film into the spectrometer; An optical coupling device capable of Equipped with the spectrometer is capable of detecting a first spectrum in the focused light representative of the process film layer; system.

2. The system of claim 1 , wherein the transparent thin film comprises one of yttrium oxide, aluminum oxide, zirconium oxide and is of a known thickness.

3. The system of claim 1 , wherein the transparent crystal is one of a sapphire plug, a diamond plug, a quartz plug, and a silicon carbide plug.

4. The system of claim 1 , wherein the distal surface of the transparent crystal is formed at an angle to the liner, the angle being between 0.8 degrees and 1.8 degrees.

5. and a processing device coupled to the spectrometer, the processing device comprising: receiving the first spectrum from the spectrometer; receiving a second spectrum from the spectrometer when the light source is off; calculating reflectometry data by subtracting the second spectrum from the first spectrum; calculating a reflectometry signal by dividing the reflectometry data by a reference spectrum; fitting the reflectance measurement signals to a thin film optical model to determine information including one or more optical film properties of the process film layer; The system of claim 1 , further comprising:

6. wherein the one or more optical film properties include a thickness, and while processing a substrate in the processing chamber, the processing device further comprises: comparing said thickness to a baseline measurement of said process film layer; using the comparison to determine that a variation in a deposition rate of the process film layer exceeds a threshold variation; triggering a process in the processing chamber to correct the deposition rate of the process film layer; The system according to claim 5, further comprising:

7. wherein the one or more optical film properties include a thickness, after processing the substrate in the processing chamber, the processing device further comprises: detecting when the process film layer on the transparent thin film is removed below a predetermined threshold thickness; triggering the processing device to terminate a cleaning process in the processing chamber in response to the detection; The system according to claim 5, further comprising:

8. wherein the one or more optical film properties include a thickness, and while processing a substrate in the processing chamber, the processing device further comprises: detecting the moment when the process film layer reaches a threshold level of thickness on the transparent thin film; triggering an end of a deposition process depositing the process film layer; The system according to claim 5, further comprising:

9. A processing chamber comprising: a wall for defining an interior of the processing chamber; a liner attached to the inside surface of said wall; a transparent crystal, at least a portion of which is embedded within the wall and the liner, the transparent crystal having a proximal end and a distal end, the distal end having a distal surface that is approximately flush with the inner surface of the wall; and a transparent thin film deposited on the distal surface of the transparent crystal, the transparent thin film having chemical properties substantially matching those of the liner; Equipped with light from outside the wall can pass through the transparent crystal, reflect off the distal surface and off a surface of the transparent membrane, and return through the proximal end of the transparent crystal; Processing chamber.

10. 10. The processing chamber of claim 9, wherein the transparent thin film comprises one of yttrium oxide, aluminum oxide, zirconium oxide and is of a known thickness.

11. 10. The processing chamber of claim 9, wherein the transparent crystal is one of a sapphire plug, a diamond plug, a quartz plug, and a silicon carbide plug.

12. 10. The processing chamber of claim 9, wherein the distal surface of the transparent crystal is formed at an angle to the liner, the angle being between 0.8 degrees and 1.8 degrees.

13. The transparent crystal is in a plug shape, and the transparent crystal is a shaft embedded within the wall and the liner; and a flange attached to the shaft and adjacent an outer surface of the wall; 10. The processing chamber of claim 9, further comprising a seal disposed between the flange and the exterior surface of the wall.

14. 14. The processing chamber of claim 13, wherein the flange comprises an inner surface in physical contact with the seal, the inner surface comprising a surface roughness (Ra) of less than 20 nanometers.

15. 14. The processing chamber of claim 13, wherein a proximal surface at the proximal end of the transparent crystal is formed at an angle to the outer surface of the wall, the angle being between 2 degrees and 5 degrees.

16. providing at least a portion of a transparent crystal embedded within a wall and a liner of a processing chamber, the transparent crystal having a proximal end and a distal end, the distal end having a distal surface exposed to an interior of the processing chamber; depositing a transparent thin film on the distal surface of the transparent crystal, the thin film having chemical properties that substantially match those of the liner; depositing a process film layer on the transparent thin film in the processing chamber; transmitting light from a light source through the proximal end of the transparent crystal by a light coupling device; focusing light reflected back from the combination of the distal surface, the transparent pellicle surface, and the process film layer surface into a fiber optic cable by the optical coupling device; receiving the focused light from the fiber optic cable with a spectrometer; detecting a first spectrum representative of the process film layer within the focused light with the spectrometer; The method includes:

17. detecting a second spectrum from the focused light with the spectrometer when the light source is off; receiving, by a processing device, the first spectrum and the second spectrum; subtracting, by the processing device, the second spectrum from the first spectrum to generate reflectometry data; dividing, by the processing device, the reflectance measurement data by a reference spectrum to generate a reflectance measurement signal; fitting, by the processing device, the reflectance measurement signals to a thin film optical model to determine information including one or more optical film properties of the process film layer; 20. The method of claim 16, further comprising:

18. The one or more optical film properties include a thickness, and the method includes, while processing a substrate in the processing chamber, comparing said thickness to a baseline measurement of said process film layer; using the comparison to determine that a variation in a deposition rate of the process film layer exceeds a threshold variation; triggering a process in the processing chamber to correct the deposition rate of the process film layer; 20. The method of claim 17, further comprising:

19. The one or more optical film properties include thickness, the method comprising: detecting when the thickness of the process film layer on the transparent thin film reaches a build-up limit; triggering the processing chamber to initiate a cleaning process within the processing chamber in response to the detection; 20. The method of claim 17, further comprising:

20. The one or more optical film properties include a thickness, and the method further comprises, after processing the substrate in the processing chamber: Detecting the moment when the process film layer on the transparent thin film is removed by a cleaning process to below a predetermined threshold thickness; triggering the processing device to terminate the cleaning process in the processing chamber in response to the detection; 20. The method of claim 17, further comprising:

21. The one or more optical film properties include a thickness, and the method includes, while processing a substrate in the processing chamber, detecting the moment when the process film layer reaches a threshold level of thickness on the transparent thin film; triggering an end of a deposition process depositing the process film layer; 20. The method of claim 17, further comprising:

Citation Information

Patent Citations

  • Manufacturing method, apparatus, and system of semiconductor device, and cleaning method of semiconductor-manufacturing apparatus

    JP2003077843A

  • Substrate-treating device, deposit monitoring device, and deposit monitoring method

    JP2007258238A

  • Semiconductor device manufacturing method, semiconductor device manufacturing apparatus, semiconductor device manufacturing system, and cleaning method for semiconductor device manufacturing apparatus

    US20030045960A1

  • Substrate processing apparatus, deposit monitoring apparatus, and deposit monitoring method

    US20070215043A1

  • Apparatus and method of treating a substrate

    US20150214016A1